Memory and method for manufacturing the same

By controlling the difference in the spacing and dielectric constant between the word line and the end face in the memory, the problem of signal interference in the memory is solved and the signal transmission performance is improved.

CN116113237BActive Publication Date: 2024-11-15CHANGXIN MEMORY TECH INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310234943.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-08-18
Publication Date
2024-11-15
Estimated Expiration
2040-08-18

AI Technical Summary

Technical Problem

With the shrinking of process nodes, the signal interference problem caused by the row hammer effect in memory is becoming more and more serious. How to reduce signal interference between word lines has become an important direction for memory process optimization.

Method used

By designing an active region extending in the first direction and a word line extending in the second direction in the memory, the word line includes a gate conductive layer, ensuring that the spacing between the end surface and the gate conductive layer is within a preset range and at a certain In some embodiments, gate dielectric layers are used, with the dielectric constant of the material greater than or equal to the dielectric constant of the isolated structure to reduce signal interference.

Benefits of technology

By controlling the difference in spacing and dielectric constant between the end surface and gate conductive layer, electron migration and signal interference are reduced, and the signal transmission performance of word lines is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116113237B_ABST
    Figure CN116113237B_ABST
Patent Text Reader

Abstract

An embodiment of the present invention provides a memory and a manufacturing method thereof, wherein the memory comprises: an active region extending along a first direction and a word line extending along a second direction, wherein the word line portion is located between adjacent active regions, wherein the word line comprises a gate conductive layer, and wherein in parallel with the first direction, the active region has an end face facing the word line, and the extreme difference in spacing between the end face and the gate conductive layer is within a preset range. The present invention is conducive to reducing signal interference between adjacent active regions caused by the word line.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present invention relate to the semiconductor field, and in particular to a memory and a manufacturing method thereof. Background Art

[0002] Memory is a memory component used to store programs and various data information. It can be divided into read-only memory and random access memory according to the type of memory used. Memory usually includes capacitors and transistors connected to the capacitors. The capacitors are used to store charges representing stored information, and the transistors are switches that control the flow and release of charges in the capacitors. Among them, the transistors are formed with a source, a drain, and a gate, and the gate is connected to the word line.

[0003] However, as the process nodes continue to shrink, the signal interference problem caused by the row hammer effect in the memory is becoming more and more serious. How to solve this problem has become an important direction for memory process optimization. Summary of the invention

[0004] The embodiment of the present invention provides a memory and a manufacturing method thereof, which is beneficial to reducing signal interference between word lines.

[0005] To solve the above problems, an embodiment of the present invention provides a memory, comprising: an active area extending along a first direction and a word line extending along a second direction, wherein a portion of the word line is located between adjacent active areas, the word line comprises a gate conductive layer, and in parallel with the first direction, the active area has an end face facing the word line, and the extreme difference in the spacing between the end face and the gate conductive layer is within a preset range.

[0006] In some embodiments, in parallel with the first direction, the maximum difference of the spacing between the end surface and the word line is within the preset range.

[0007] In some embodiments, in parallel with the first direction, a maximum difference in the spacing between the end surface and the word line is greater than the preset range.

[0008] In some embodiments, the word line further includes a gate dielectric layer located between the gate conductive layer and the active region, and in parallel with the first direction, the maximum thickness of the gate dielectric layer is 3nm to 5nm, and the minimum thickness is 1nm to 3nm.

[0009] In some embodiments, the preset range is 0 nm to 0.4 nm.

[0010] In some embodiments, the memory further includes: an isolation structure located between adjacent active areas, the word line is located within the isolation structure, the word line includes a gate dielectric layer located between the isolation structure and the gate conductive layer, and the dielectric constant of the material of the gate dielectric layer is greater than or equal to the dielectric constant of the material of the isolation structure.

[0011] In some embodiments, the gate conductive layer includes adjacent straight portions and bent portions, the straight portions are located within the active regions and extend along the second direction, and the bent portions are located between adjacent active regions and have a portion extending perpendicular to the first direction.

[0012] Correspondingly, an embodiment of the present invention also provides a method for manufacturing a memory, comprising: providing an active area extending along a first direction; forming a word line extending along a second direction, wherein a portion of the word line is located between adjacent active areas, the word line includes a gate conductive layer, and in parallel with the first direction, the active area has an end face facing the word line, and the extreme difference in the spacing between the end face and the gate conductive layer is within a preset range.

[0013] In some embodiments, in parallel with the first direction, the maximum difference of the spacing between the end surface and the word line is within the preset range.

[0014] In some embodiments, there is an isolation structure between adjacent active areas; the process steps for forming the word line include: forming a groove for filling the word line, the groove passing through the active area and the isolation structure, and in parallel with the first direction, the extreme difference in thickness of the isolation structure between the end face and the groove in the isolation structure is within the preset range.

[0015] In some embodiments, in parallel with the first direction, a maximum difference in the spacing between the end surface and the word line is greater than the preset range.

[0016] In some embodiments, there is an isolation structure between adjacent active areas; the process steps for forming the word line include: forming a groove for filling the word line, the groove passing through the active area and the isolation structure; performing an in-situ growth process to use the material in the active area to form a gate dielectric layer covering the sidewalls and bottom of the groove; filling the groove to form the gate conductive layer.

[0017] In some embodiments, the in-situ growth process includes an oxidation process or a nitridation process.

[0018] In some embodiments, the oxidation process includes a thermal oxidation process, and a process temperature of the thermal oxidation process is 900° C. to 1100° C.

[0019] Compared with the prior art, the technical solution provided by the embodiment of the present invention has the following advantages:

[0020] In the above technical solution, the extreme difference in the spacing between the end face and the gate conductive layer is within a preset range, and a position on the end face closer to the gate conductive layer has a larger spacing from the gate conductive layer. This helps to avoid excessive electric field applied by the gate conductive layer to a certain position on the end face, thereby avoiding the electrons at that position from being actuated and undergoing electron migration, thereby reducing signal interference between adjacent active areas.

[0021] In addition, when there is a difference in the dielectric constant between different positions on the end surface and the gate conductive layer in parallel to the first direction, using a gate dielectric layer material with a larger or equal dielectric constant to compensate for the difference is beneficial to thinning the thickness of the gate dielectric layer, reserving more space for the gate conductive layer, thereby reducing the resistance of the gate conductive layer and improving the signal transmission performance of the word line. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] One or more embodiments are exemplarily described by pictures in the corresponding drawings, and these exemplifications do not constitute limitations on the embodiments. Unless otherwise stated, the pictures in the drawings do not constitute proportional limitations.

[0023] Figure 1 and Figure 2 A schematic diagram of the structure of a memory;

[0024] Figures 3 to 9 A schematic structural diagram corresponding to each step of the method for manufacturing a memory provided in the first embodiment of the present invention;

[0025] Figures 10 to 16 This is a schematic structural diagram corresponding to each step of the method for manufacturing a memory provided in the second embodiment of the present invention. DETAILED DESCRIPTION

[0026] refer to Figure 1 and Figure 2 , Figure 1 is a top view of the memory. Figure 2 for Figure 1 Schematic diagram of the cross-sectional structure along the cross-sectional direction AA.

[0027] The memory includes: an active area 11 extending along a first direction X, an isolation structure 12 located between adjacent active areas 11, and a word line 13 extending along a second direction Y and partially located in the isolation structure 12; in parallel to the first direction X, the active area 11 has an end surface 11c facing the word line 13.

[0028] Since the first direction X and the second direction Y are usually not perpendicular, when the word line 13 located between adjacent active areas 11 is a straight line, the spacing between different positions on the end surface 11c and the word line 13 is different in parallel to the first direction X, that is, the extreme difference of the spacing between the end surface 11c and the word line 13 is not zero.

[0029] Specifically, in parallel to the first direction X, the end surface 11c has a first position 11a closest to the word line 13 and a second position 11b farthest from the word line 13, a first spacing d1 is provided between the first position 11a and the word line 13, a second spacing d2 is provided between the second position 11b and the word line 13, and the difference between the first spacing d1 and the second spacing d2 is the range. When the first direction X is not perpendicular to the second direction Y, the range is not zero, and the range increases as the angle between the first direction X and the second direction Y decreases.

[0030] Since the active areas 11 located on both sides of the word line 13 are usually symmetrically distributed, and the spacing between adjacent active areas 11 is fixed, the greater the difference in the spacing between the end surface 11c and the word line 13, the smaller the first spacing d1 and the larger the second spacing d2. When the thickness of the gate dielectric layer 131 remains unchanged, since the gate conductive layer 132 in the isolation structure 12 is closer to the first position 11a of the active area 11, the stronger the electric field applied by the gate conductive layer 132 in the isolation structure 12 to the first position 11a, the easier it is for the electrons in the drain area of ​​the active area 11 (i.e., the area between two adjacent word lines 13 in the active area 11) to be actuated. When the number of electrons actuated and gathered under the word line 13 in the active area 11 is large, a channel will be formed under the word line 13. At this time, the electrons will migrate from the drain area of ​​the active area 11 to the source area of ​​the active area 11 (i.e., the area close to the gate conductive layer 132 in the isolation structure 12) through the channel, thereby causing signal interference.

[0031] It should be noted that, since the first position 11 a is closer to the word line 13 in the isolation structure 12 , the electron crosstalk usually occurs between the first position 11 a of the active region 11 and the isolation structure 12 .

[0032] According to the above analysis, when the extreme difference in the distance between the end face 11c and the gate conductive layer 132 is greater than the preset range, the gate conductive layer 132 in the isolation structure 12 is closer to the first position 11a, and the gate conductive layer 132 in the isolation structure 12 is more likely to activate the electrons in the active area 11, so that the electrons in the active area 11 gather under the word line 13 in the active area 11 close to the isolation structure 12 and form a channel, thereby causing signal interference.

[0033] To solve the above problems, the present invention provides a memory and a method for manufacturing the same, in which the extreme difference in the spacing between the end face and the gate conductive layer is within a preset range, and a position on the end face closer to the gate conductive layer has a larger spacing from the gate conductive layer, and the electric field applied by the gate conductive layer to this position is smaller, which is beneficial to reducing the number of electrons that can be activated by the gate conductive layer, thereby inhibiting the formation of channels and reducing signal interference.

[0034] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the embodiments of the present invention will be described in detail below with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the embodiments of the present invention, many technical details are provided to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can be implemented.

[0035] refer to Figures 3 to 9 , Figures 3 to 9 The schematic diagram of the structure corresponding to each step of the manufacturing method of the memory provided by the first embodiment of the present invention. For the sake of clarity, each step provides a top view of the memory and a schematic diagram of the cross-sectional structure of the memory along the cross-sectional direction AA.

[0036] refer to Figure 3 and Figure 4 , providing an active area 21 extending along a first direction X and a groove 23 extending along a second direction Y.

[0037] In this embodiment, there is an isolation structure 22 between adjacent active areas 21, and the groove 23 is located in the active area 21 and the isolation structure 22, and the groove 23 is used to fill the word line; in other embodiments, there may be other structures or empty grooves between adjacent active areas. When there are empty grooves between adjacent active areas, a gate dielectric layer with a specific shape can be formed subsequently through other processes such as deposition process.

[0038] In this embodiment, in parallel to the first direction X, the active region 21 has an end surface 21 c facing the groove 23 , and the material of the active region 21 includes single crystal silicon; in other embodiments, the material of the active region may also be semiconductor materials such as polycrystalline silicon and germanium.

[0039] In this embodiment, the groove 23 between adjacent active regions 21 is a straight groove, the first direction X is not perpendicular to the second direction Y, and the end surface 21c has a first position 21a closest to the groove 23 and a second position 21b farthest from the groove 23 in parallel to the first direction X. There is a first spacing d1 between the first position 21a and the groove 23, and there is a second spacing d2 between the second position 21b and the groove 23, and the first spacing d1 is smaller than the second spacing d2. It can be seen from the cross-sectional schematic diagram in the cross-sectional direction AA that the groove 23 in the isolation structure 22 is closer to one active region 21 and farther from another active region 21.

[0040] In this embodiment, the difference between the first spacing d1 and the second spacing d2 is greater than the preset range, that is, the range difference of the spacing between the end face 21c and the word line is greater than the preset range. In order to make the range difference of the spacing between the end face 21c and the gate conductive layer formed subsequently within the preset range, it is necessary to form a gate dielectric layer with different thicknesses to adjust the spacing between the end face 21c and the gate conductive layer, thereby adjusting the electric field isolation capability of the dielectric layer located between the end face 21c and the gate conductive layer, and the dielectric layer includes an isolation structure 22 and a gate dielectric layer located between the end face 21c and the gate conductive layer.

[0041] refer to Figure 5 and Figure 6 , an in-situ growth process is performed to form a gate dielectric layer 241 using the material in the active region 21 .

[0042] For simplicity of expression, the groove 23 located in the isolation structure 22 is defined as a first groove 231 , and the groove 23 located in the active area 21 is defined as a second groove 232 .

[0043] In this embodiment, since the gate dielectric layer 241 needs to be formed by the material in the active region 21, the time required for the material in the active region 21 to diffuse to the surface of the first groove 231 during the formation of the gate dielectric layer 241 will determine the formation rate of the gate dielectric layer 241 and the thickness of the gate dielectric layer 241. Specifically, under the same atomic diffusion rate, since the first position 21a is closer to the first groove 231, the material at the first position 21a can diffuse to the surface of the first groove 231 faster to form the gate dielectric layer 241, and finally the thickness of the gate dielectric layer 241 on the surface of the first groove 231 corresponding to the first position 21a is greater than the thickness of the gate dielectric layer 241 on the surface of the first groove 231 corresponding to the second position 21a.

[0044] The following is a principle description using an example of using an oxidation process to form the gate dielectric layer 241 made of silicon oxide.

[0045] During the oxidation process, since the first position 21a is closer to the first groove 231, more silicon atoms can diffuse from the first position 21a to the surface of the first groove 231 per unit time, thereby forming a thicker gate dielectric layer 241 on the surface of the first groove 231; correspondingly, since the second position 21b is farther from the first groove 231, only fewer silicon atoms can diffuse from the second position 21b to the surface of the first groove 231 per unit time, so the gate dielectric layer 231 on the surface of the first groove 231 corresponding to the second position 21b is thinner.

[0046] Accordingly, since the second groove 232 is directly located in the active area 21 , there is no need to consider the effect of atomic diffusion time on the thickness of the gate dielectric layer 241 during the formation of the gate dielectric layer 241 , and the gate dielectric layer 241 covering the sidewall of the second groove 232 is relatively uniform.

[0047] By utilizing the positional relationship between the first position 21a and the second position 21b relative to the first groove 231, an in-situ generation process is used to form a gate dielectric layer 241 with different thicknesses, which is beneficial to reducing the extreme difference in the spacing between the end face 21c and the subsequently formed gate conductive layer, so that the extreme difference in the spacing between the end face 21c and the gate conductive layer is within a preset range, that is, the position on the end face 21c that is closer to the gate conductive layer has a larger spacing with the gate conductive layer, and the electric field applied by the gate conductive layer to this position is smaller, thereby reducing the number of electrons that can be actuated in the gate conductive layer, inhibiting the formation of channels and reducing signal interference. This embodiment only uses an oxidation process to form silicon oxide as the gate dielectric layer 241 as an example; in other embodiments, a nitridation process can also be used to form silicon nitride or germanium nitride as the gate dielectric layer, and the material of the gate dielectric layer is related to the material of the active area.

[0048] In this embodiment, in parallel to the first direction X, the gate dielectric layer 241 at the surface position of the first groove 231 corresponding to the first position 21a is the thickest, and the maximum thickness is 3nm~5nm, for example, 3.5nm, 4nm or 4.5nm; the gate dielectric layer 241 at the surface position of the first groove 231 corresponding to the second position 21b is the thinnest, and the minimum thickness is 1nm~3nm, for example, 1.5nm, 2nm or 2.5nm.

[0049] In this embodiment, the preset range of the distance between the end surface 21c and the gate conductive layer is 0nm-0.4nm, such as 0.1nm, 0.2nm or 0.3nm. If the preset range is too large, the distance between the subsequently formed gate conductive layer and the first position 21a may be too small, thereby causing signal interference problems.

[0050] In this embodiment, a thermal oxidation process is used to form the gate dielectric layer 241. Since the thermal oxidation process has a relatively high process temperature, and a high temperature environment is conducive to accelerating the diffusion movement of atoms, the use of a thermal oxidation process to form the gate dielectric layer 241 is conducive to shortening the process time. The temperature of the thermal oxidation process is 900°C to 1100°C, for example, 950°C, 1000°C or 1500°C.

[0051] It should be noted that, as the gate dielectric layer 241 is formed, the time for silicon atoms in the active region 21 to diffuse to the surface of the current gate dielectric layer 241 will gradually increase, and the thickness of the gate dielectric layer 241 grown per unit time will become smaller and smaller.

[0052] In other words, as the oxidation process proceeds, the formation rate of the gate dielectric layer 241 on the surface of the first groove 231 corresponding to the first position 21a and the formation rate of the gate dielectric layer 241 on the surface of the first groove 231 corresponding to the second position 21b will tend to be equal. At this time, in parallel to the first direction X, the difference in thickness of the dielectric layer between the first position 21a and the gate conductive layer and the thickness of the dielectric layer between the second position 21b and the gate conductive layer is also small, and the electric field isolation of the dielectric layers corresponding to different positions can be less different.

[0053] In this embodiment, the process time of the thermal oxidation process is 10 minutes to 60 minutes, for example, 20 minutes, 40 minutes or 50 minutes. If the process time is too short, it is not conducive to making the extreme difference of the distance between the end face 21c and the gate conductive layer within the preset range; if the process time is too long, an overly thick gate dielectric layer 241 will be formed, which will lead to too small a reserved space for the gate conductive layer, a large resistance of the gate conductive layer, and an excessively large threshold voltage of the word line located in the active area 21, which will increase the required operating voltage and reduce the sensitivity of the memory.

[0054] In other embodiments, the oxidation process further includes an in-situ steam generation process, a wet oxidation process, and a dry oxidation process.

[0055] In this embodiment, the dielectric constant of the material of the gate dielectric layer 241 is greater than or equal to the dielectric constant of the material of the isolation structure 22. In this way, a thinner gate dielectric layer 241 can be used to compensate for the thickness difference of the isolation structure 22 corresponding to different positions of the end surface 21c, reserving a larger space for the gate conductive layer, thereby reducing the resistance of the gate conductive layer.

[0056] In this embodiment, after the in-situ generation process, the gate dielectric layer 241 on the side where the thickness of the isolation structure 22 is thinner is thicker, and the gate dielectric layer 241 on the side where the thickness of the isolation structure 22 is thicker is thinner. The extreme difference in the spacing between the end face 21c and the gate conductive layer is within a preset range, and the groove reserved for the gate conductive layer can be regarded as being in the center position of the adjacent active area 21.

[0057] refer to Figure 7 and Figure 8 , a gate conductive layer 242 is filled into the first groove 231 and the second groove 232, the gate dielectric layer 241 and the gate conductive layer 242 constitute a word line 24, the width of the gate conductive layer 242 is 5nm to 15nm, and the material of the gate conductive layer 242 includes tungsten; reference Fig. 9 A dielectric layer 25 for electrical isolation or support is formed on the word line 24. In addition, a barrier layer (not shown) may be formed between the gate dielectric layer 241 and the gate conductive layer 242. The material of the barrier layer includes titanium nitride.

[0058] In this embodiment, since the thickness of the gate dielectric layer 241 at different positions in the first groove 231 is different, and the thickness of the gate dielectric layer 242 at different positions in the second groove 231 is the same, the gate conductive layer 242 filled in the first groove 231 and the second groove 232 will also present different shapes. Specifically, the gate conductive layer 242 includes a bending portion 242a located between adjacent active regions 21 and a straight portion located in the active region 21. The straight portion extends along the second direction Y, and the bending portion 242a has a portion extending perpendicular to the first direction X.

[0059] In the present embodiment, the extreme difference in the spacing between the end face and the gate conductive layer is within a preset range, and a position on the end face that is closer to the gate conductive layer has a larger spacing therebetween. This helps to prevent the gate conductive layer from applying an excessively large electric field to a certain position on the end face, thereby preventing the electrons at that position from being actuated and undergoing electron migration, thereby reducing signal interference between adjacent word lines.

[0060] Another embodiment of the present invention further provides a method for manufacturing a memory. Different from the previous embodiment, in this embodiment, the range difference between the end surface and the first groove is within a preset range. Figures 10 to 15 For detailed explanation, Figures 10 to 15 This is a schematic diagram of the structure corresponding to each step of the manufacturing method of the memory provided by the second embodiment of the present invention. For the same or corresponding steps as the previous embodiment, reference can be made to the corresponding description of the previous method embodiment, and no further description will be given below.

[0061] refer to Fig.10 and Fig.11 , providing an active area 31 extending along a first direction X and a groove 33 extending along a second direction Y.

[0062] In this embodiment, the groove 33 includes a first groove 331 located between adjacent active regions 31 and a second groove located in the active region 31 . In a direction parallel to the first direction X, the range difference between the end surface 31 c and the first groove 331 is within a preset range.

[0063] In this embodiment, an etching process can be used to etch the isolation structure 32 to form a groove 33. Since the shape of the first groove 231 needs to be adjusted according to the position of the end surface 31c, it can be seen from the top view that the first groove 331 is in a bent state and the second groove 332 is in a straight state. The groove 33 with a special shape is formed by etching through a special mask plate, which is conducive to improving the structural stability of the groove 33, and then improving the structural stability of the word line.

[0064] refer to Fig.12 and Fig.13 , forming a gate dielectric layer 341.

[0065] In this embodiment, an in-situ formation process or a deposition process may be used to form the gate dielectric layer 341. When the in-situ formation process is used, since the difference in the distance between the end surface 31c and the first groove 331 is within a preset range, the thickness difference of the gate dielectric layer 341 at different positions is also small.

[0066] refer to Fig.14 and Fig.15 , a gate conductive layer 342 is filled into the first groove 331 and the second groove 332, the gate dielectric layer 341 and the gate conductive layer 342 constitute a word line 34, the width of the gate conductive layer 342 is 5nm to 15nm, and the material of the gate conductive layer 342 includes tungsten; reference Fig.16 A dielectric layer 35 is formed on the word line 34, and the dielectric layer 35 plays the role of electrical isolation and support. In addition, a barrier layer (not shown in the figure) can be formed between the gate dielectric layer 341 and the gate conductive layer 342, and the material of the barrier layer includes titanium nitride.

[0067] In this embodiment, grooves with special shapes are directly formed through a special mask plate, which is conducive to ensuring that the grooves at different positions and the word lines formed by filling the grooves have good structural stability, thereby making the memory have good performance stability.

[0068] Correspondingly, an embodiment of the present invention further provides a memory, which can be manufactured using the above-mentioned memory manufacturing method.

[0069] refer to Figures 7 and 8 The memory includes: an active area 21 extending along a first direction X and a word line 24 extending along a second direction Y, wherein a portion of the word line 24 is located between adjacent active areas 21, and the word line 24 includes a gate conductive layer 242. In parallel with the first direction X, the active area 21 has an end face 21c facing the word line 24, and the extreme difference in the spacing between the end face 21c and the gate conductive layer 242 is within a preset range.

[0070] In this embodiment, in parallel to the first direction X, the difference in the distance between the end surface 21c and the word line 24 is greater than a preset range; in other embodiments, refer to Fig.10 , in parallel with the first direction, the maximum difference of the distance between the end surface 31c and the first groove 331 is within a preset range.

[0071] In this embodiment, the word line 24 also includes a gate dielectric layer 241 located between the gate conductive layer 242 and the active area 21. In the direction parallel to the first direction X, the maximum thickness of the gate dielectric layer 241 is 3nm to 5nm, for example, 3.5nm, 4nm or 4.5nm, and the minimum thickness is 1nm to 3nm, for example, 1.5nm, 2nm or 2.5nm.

[0072] In this embodiment, the preset range is 0 nm to 0.4 nm.

[0073] In this embodiment, the memory also includes: an isolation structure 22 located between adjacent active areas 21, a word line 24 located within the isolation structure 22, the word line 24 includes a gate dielectric layer 241 located between the isolation structure 22 and the gate conductive layer 242, and the dielectric constant of the material of the gate dielectric layer 241 is greater than or equal to the dielectric constant of the material of the isolation structure 22.

[0074] In this embodiment, the gate conductive layer 242 includes adjacent bending portions 242 a and straight portions 242 b . The straight portion 242 b is located in the active region 21 , and the bending portion 242 a is located between adjacent active regions 21 .

[0075] In the present embodiment, the extreme difference in the spacing between the end face and the gate conductive layer is within a preset range, and a position on the end face that is closer to the gate conductive layer has a larger spacing from the gate conductive layer. This helps to avoid excessive electric field applied by the gate conductive layer to a certain position on the end face, thereby preventing the electrons at that position from being actuated and undergoing electron migration, thereby reducing signal interference between adjacent active areas.

[0076] Those skilled in the art will appreciate that the above embodiments are specific examples of the present invention, and in practical applications, various changes may be made to the embodiments in form and detail without departing from the spirit and scope of the present invention. Any person skilled in the art may make changes and modifications without departing from the spirit and scope of the present invention, and therefore the scope of protection of the present invention shall be subject to the scope defined in the claims.

Claims

1. A memory, It is characterized in that include: a plurality of active regions extending along a first direction; An isolation structure between the active regions; a plurality of word lines extending along a second direction, wherein the first direction is not perpendicular to the second direction; The word line comprises a gate conductive layer and a gate dielectric layer; Wherein, the gate conductive layer includes a bent portion located within the isolation structure; In the first direction, the thickness of the gate dielectric layer on the sidewalls on the same side of the section where the bent portion is located between two ends of adjacent active regions is uneven.

2. The memory according to claim 1, It is characterized in that An angle between an extension direction of a section of the bending portion located between two ends of adjacent active regions and the first direction is greater than an angle between the second direction and the first direction.

3. The memory according to claim 2, It is characterized in that An extension direction of a section of the bent portion located between two ends of adjacent active regions is perpendicular to the first direction.

4. The memory according to claim 1, It is characterized in that A first groove is formed in the isolation structure, a second groove is formed in the active area, and the first groove is connected to the second groove; The gate dielectric layer is located on the inner walls of the first groove and the second groove; The gate conductive layer is located in the first groove and the second groove.

5. The memory according to claim 4, It is characterized in that The bent portion of the gate conductive layer is located in the first groove, and the gate conductive layer further includes a straight portion located in the second groove, and the straight portion is connected to the bent portion.

6. The memory according to claim 4, It is characterized in that In the first direction, the first groove is located in a section between two ends of the adjacent active regions, and the thickness of the gate dielectric layer located on the inner wall on the same side is uneven.

7. The memory according to claim 6, It is characterized in that In the cross section along the first direction, the cross section is perpendicular to the plane formed by the first direction and the second direction, and the thickness of the gate dielectric layer between two ends of adjacent active regions is greater at the thinner side close to the isolation structure than at the thicker side close to the isolation structure.

8. The memory according to claim 7, It is characterized in that The gate dielectric layer between two adjacent active regions has a thickness range of 3nm to 5nm near the thinner side of the isolation structure, and the gate dielectric layer between two adjacent active regions has a thickness range of 1nm to 3nm near the thicker side of the isolation structure.

9. The memory according to claim 4, It is characterized in that An angle between an extension direction of a section of the first groove located between two ends of adjacent active regions and a normal to the first direction is smaller than an angle between the second direction and a normal to the first direction.

10. The memory according to claim 4, It is characterized in that An extension direction of a section of the first groove located between two ends of adjacent active regions is perpendicular to the first direction.

11. A method for manufacturing a memory, It is characterized in that include: Providing active areas extending along a first direction and grooves extending along a second direction, with isolation structures between adjacent active areas, and the grooves being located within the active areas and the isolation structures; forming a word line in the groove, the word line comprising a gate dielectric layer and a gate conductive layer, wherein the gate dielectric layer is formed on the inner wall of the groove by an in-situ generation process, and the thickness of the gate dielectric layer on the inner wall on the same side of the groove in a section between two ends of the adjacent active area is uneven; Wherein, the gate conductive layer includes a bending portion located in the isolation structure.

12. The method for manufacturing a memory according to claim 11, It is characterized in that An angle between an extension direction of a section of the bending portion located between two ends of adjacent active regions and the first direction is greater than an angle between the second direction and the first direction.

13. The method for manufacturing a memory according to claim 11, It is characterized in that The in-situ generation process includes an oxidation process or a nitridation process.

14. The method for manufacturing a memory according to claim 13, It is characterized in that The oxidation process includes a thermal oxidation process, and the temperature range of the thermal oxidation process includes 900° C. to 1100° C.

15. The method for manufacturing a memory according to claim 11, It is characterized in that The gate dielectric layer is formed on the inner wall of the groove by using a deposition process, and the thickness of the gate dielectric layer on the inner wall on the same side in the section of the groove between the two ends of the adjacent active areas is the same; the angle between the extension direction of the section of the groove between the two ends of the adjacent active areas and the first direction is greater than the angle between the second direction and the first direction.