A rapid repair process for bridge pavement
By cutting cracks, opening holes on the bridge pavement, spraying airflow and water mist, and filling concrete repair liquid, the problem of poor bonding strength between the repair slurry and the crack wall in the prior art is solved, and the repair effect is significantly improved.
Patent Information
- Application Number
- CN202310324128.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2043-03-30
AI Technical Summary
In the existing bridge pavement repair process, the bonding strength between the repair slurry and the crack wall is poor, resulting in the problem of cracks being prone to reappearance after repair.
A bridge pavement rapid repair process is adopted, forming grooves by cutting the edges of cracks, using stamping blocks and chisels to open holes in the groove wall, and spray airflow and water mist to reduce dust and wetting, and then fill with concrete repair liquid to Improve bond strength.
It improves the bonding strength after repair, reduces the reappearance of cracks, and enhances the repair effect.
Smart Images

Figure CN116289463B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of bridge pavement repair, in particular to a bridge pavement rapid repair process. Background Art
[0002] A bridge pavement is a structure built for roads to cross natural or artificial obstacles, allowing vehicles and pedestrians to pass smoothly. Bridge pavements can be roughly divided into beam bridges, arch bridges, steel frame bridges and cable-stayed bridges. During the long-term use of bridge pavements, cracks will appear in the bridge pavement due to the influence of vehicle running over, etc., and maintenance personnel are required to repair the cracks in time.
[0003] When repairing cracks on bridge pavement, direct repair methods are often used, where repair slurry is injected into the cracks and the repair slurry is rolled and scraped flat using scraping and rolling tools. However, the bonding strength between the repair slurry and the crack wall in this repair method is relatively poor, and cracks are prone to reappear at the repaired area after a period of use.
[0004] In response to existing problems, it is urgent to innovate based on the original repair technology. Summary of the invention
[0005] The purpose of the present invention is to provide a rapid bridge pavement repair process to solve the problem raised in the above-mentioned background technology that when repairing cracks on bridge pavements, a direct repair method is often used, in which a repair slurry is injected into the cracks, and the repair slurry at the cracks is rolled and scraped flat by a scraping tool and a rolling tool. However, the bonding strength between the repair slurry and the crack wall in this repair method is relatively poor. After a period of use, cracks are likely to appear again at the repaired area.
[0006] To achieve the above object, the present invention provides the following technical solution: a rapid repair process for a bridge pavement, comprising the following steps:
[0007] S1: First, push the handrail to drive the support base to move on the ground, and control the engine to drive the cutting machine to rotate, cut the crack edge of the bridge pavement, cut the cracked pavement into pieces, and use tools to clean and remove the pieces, forming a regular groove on the bridge pavement;
[0008] S2: Control the hydraulic rod on the support frame to drive the mounting seat and the docking seat to move up and down, so that the punching shell and the chisel head are embedded in the groove, and the end of the chisel head fits with the groove wall;
[0009] S3: Then, the motor in the docking seat is controlled to move, driving the first push block and the second push block to reciprocate in the connecting shell, so that the punching block impacts the impact head, so that the docking rod and the chisel head can reciprocate, impact the groove wall to open a hole, and densely form a plurality of slots on the groove wall;
[0010] S4: When the chisel head makes reciprocating motion, the air intake mechanism and the nozzle cooperate with each other to realize that the chisel head sprays airflow to the slot hole while hitting the hole, blowing out the debris in the slot hole. At the same time, the liquid storage mechanism will open the channel to allow water to enter the punching shell and spray out with the airflow, achieving the effect of dust reduction and wetting the slot hole wall;
[0011] S5: Finally, use a cleaning tool to clean and remove the debris in the groove, pour the pre-mixed concrete repair slurry into the groove, and use a vibrating tool to treat the concrete repair liquid. At this time, the concrete repair liquid will flow into the groove hole and fill the groove hole. When the concrete repair liquid solidifies, it will increase the contact surface between the concrete repair liquid and the bridge pavement, thereby increasing the repair bonding strength.
[0012] As an optional solution to the bridge pavement rapid repair process described in the present invention, the liquid storage mechanism includes a liquid storage shell, a sealing head, a sealing block, a sealing gasket, a positioning block and an airbag, and a sealing head is arranged inside the liquid storage shell, and the end of the sealing head is fixedly connected to the sealing block, and the end of the liquid storage mechanism is connected to a connecting pipe.
[0013] As an optional solution to the rapid repair process for bridge pavement described in the present invention, a sealing gasket is adhesively connected to the outer surface of the sealing block, and the top of the sealing gasket fits with the bottom of the liquid storage shell, and positioning blocks are arranged on both sides of the sealing block, and an airbag is fit-connected to the bottom of the sealing block, and through holes are symmetrically opened inside the sealing block.
[0014] As an optional solution of the rapid repair process for bridge pavement of the present invention, the end of the connecting pipe is connected to a water tank, and the water tank is interconnected with the liquid storage mechanism through the connecting pipe.
[0015] As an optional scheme for the rapid repair process for bridge pavement described in the present invention, the air intake mechanism includes an air intake shell, an extrusion column, an extrusion block, a limit column and a compression spring, and the extrusion column is nested inside the air intake shell, and the end of the extrusion column is fixedly connected to the extrusion block, and the extrusion columns are arranged at equal angles, and the end of the air intake mechanism is connected to a filter head.
[0016] As an optional solution to the rapid repair process for bridge pavement described in the present invention, the interior of the extrusion block is penetrated by a limiting column, and the limiting column and the air intake shell are welded together, and a compression spring is arranged at the bottom of the extrusion block, and the compression spring is nested on the outside of the limiting column.
[0017] As an optional solution to the rapid bridge pavement repair process described in the present invention, the output end of the motor is provided with a connecting gear, and the side of the connecting gear is meshingly connected with a transmission gear, and the diameter of the connecting gear is smaller than the diameter of the transmission gear, and a rotating disk is provided at the end of the transmission gear, and the outer wall of the rotating disk is fixedly connected with a connecting column, and the outside of the connecting column is movably connected with a movable rod.
[0018] As an optional solution to the rapid repair process for bridge pavement described in the present invention, the end of the movable rod is movably connected to a docking block, and the outer wall of the docking block is fixedly connected to a first pushing block, and a second pushing block is arranged on the side of the first pushing block, and a connecting groove is provided on the surface of the second pushing block, a stamping block is arranged on the right side of the second pushing block, and the outer wall of the stamping block is integrally provided with a docking outer edge.
[0019] As an optional scheme for the rapid repair process of bridge pavement described in the present invention, the outer surface of the punching block is in contact with the outer surface of the punching shell, and a first channel is opened inside the punching shell, and a second channel is arranged on the side of the first channel, and at the same time, a connecting seat is fixedly connected to the inner wall of the punching shell, an impact head is movably installed on the inner side of the connecting seat, and the end of the impact head is fixedly connected to a connecting disk, and the end of the connecting disk is fixedly connected to a docking rod, and at the same time, a first spring is nested outside the docking rod.
[0020] As an optional solution to the bridge pavement rapid repair process described in the present invention, the connection seat is provided with connection channels at equal angles inside, and a limiting rod is provided inside the connection channel, and a blocking block is fixedly connected to the end of the limiting rod, and a second spring is provided on the side of the blocking block.
[0021] Compared with the prior art, the present invention has the following beneficial effects:
[0022] 1. The bridge pavement rapid repair process is provided with a chisel head, and the punching block is used to collide with the impact head by reciprocating motion, thereby driving the docking rod and the chisel head to move. When the docking rod moves, the connecting plate squeezes the first spring. The punching block and the first spring cooperate with each other to make the chisel head reciprocate and open a hole on the inner wall of the crack groove, so that the concrete repair liquid is filled in the hole, the contact surface between the concrete repair liquid and the bridge pavement at the crack is increased, and the bonding strength after repair is increased;
[0023] 2. The rapid repair process for the bridge pavement is provided with a blocking block. When the chisel head and the punching block move to the right, the punching block will squeeze the space between the chisel head and the punching block at the same time, allowing the gas in the space to enter the connecting channel, and squeeze the blocking block to move the blocking block, and compress the second spring to open the flow channel, so that the gas can be ejected from the nozzle, so that the chisel head can eject airflow while opening a hole, and the debris generated during the excavation process can be blown out, so as to avoid a large amount of debris accumulating in the slot and affecting the subsequent opening of the chisel head;
[0024] 3. The rapid repair process for the bridge pavement is provided with a liquid storage mechanism. When the punching block is reset from the rightmost end, as the punching block moves to the left, suction is generated in the punching shell, and the sealing block is reset to seal the connecting channel to prevent the air with a large amount of dust at the chisel head from entering the punching shell through the connecting channel, which affects the service life of the internal components. When the punching shell is in a negative pressure state, the extrusion block on the compression spring is adsorbed, and the extrusion block drives the extrusion column to move downward to open the air intake channel. As the punching block moves to expose the first channel, the sealing block is sucked at the same time to make the sealing block move downward to open the flow channel in the liquid storage shell, so that the water in the liquid storage shell can enter the punching shell, so that when the punching block reciprocates in the later stage, water can be sprayed out from the nozzle along with the air flow, and the sprayed water mist can be used to reduce the dust generated in the hole opening process. At the same time, the water mist will be sprayed on the crack wall to moisten the crack wall. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a schematic diagram of the repair process of the present invention;
[0026] Figure 2 It is a schematic diagram of the three-dimensional structure of the present invention;
[0027] Figure 3 It is a schematic diagram of the connection structure between the support frame and the mounting seat of the present invention;
[0028] Figure 4 It is a schematic diagram of the cross-sectional structure of the docking seat and the punching shell of the present invention;
[0029] Figure 5 It is a schematic diagram of the connection structure between the rotating disk and the movable rod of the present invention;
[0030] Figure 6 It is a schematic diagram of the connection structure between the impact head and the connection seat of the present invention;
[0031] Figure 7 For the present invention Figure 6 The enlarged structural diagram at A in the middle;
[0032] Figure 8 For the present invention Figure 6Enlarged structural diagram at B in the middle.
[0033] In the figure: 1, support base; 2, handrail frame; 3, engine; 4, cutting machine; 5, water tank; 6, support frame; 7, hydraulic rod; 8, mounting seat; 9, docking seat; 10, punching shell; 11, liquid storage mechanism; 1101, liquid storage shell; 1102, sealing head; 1103, sealing block; 1104, sealing gasket; 1105, positioning block; 1106, air bag; 12, connecting pipe; 13, air intake mechanism; 1301, air intake shell; 1302, extrusion column; 1303, extrusion block; 1304, limit column; 1305, compression spring; 1 4. Filter head; 15. Motor; 16. Connecting gear; 17. Transmission gear; 18. Rotating disk; 19. Connecting column; 20. Movable rod; 21. Docking block; 22. First push block; 23. Second push block; 24. Connecting groove; 25. Punching block; 26. Docking outer edge; 27. Connecting seat; 28. Impact head; 29. Connecting disk; 30. Docking rod; 31. Chisel head; 32. First spring; 33. Connecting channel; 34. Limit rod; 35. Blocking block; 36. Second spring; 37. Spray nozzle; 38. First channel; 39. Second channel. DETAILED DESCRIPTION
[0034] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0035] Example 1
[0036] The present invention provides a technical solution: a rapid repair process for a bridge pavement, comprising the following steps:
[0037] S1: First, the handrail frame 2 is pushed to drive the support base 1 to move on the ground, and the engine 3 is controlled to drive the cutting machine 4 to rotate, so as to cut the crack edge of the bridge pavement, cut the pavement at the crack into fragments, and use tools to clean and remove the fragments, so as to form a regular groove on the bridge pavement;
[0038] S2: Control the hydraulic rod 7 on the support frame 6 to drive the mounting seat 8 and the docking seat 9 to move up and down, so that the punching shell 10 and the chisel head 31 are embedded in the groove, and the end of the chisel head 31 is in contact with the groove wall;
[0039] S3: Then, the motor 15 in the docking seat 9 is controlled to move, driving the first push block 22 and the second push block 23 to reciprocate in the connection housing, and then the punching block 25 impacts the impact head 28, so that the docking rod 30 and the chisel head 31 can reciprocate, impact and open holes in the groove wall, and densely form a plurality of slots on the groove wall;
[0040] S4: When the chisel head 31 makes a reciprocating motion, the air intake mechanism 13 and the nozzle 37 cooperate with each other to realize that the chisel head 31 sprays airflow to the slot hole while striking the hole, so as to blow out the debris in the slot hole. At the same time, the liquid storage mechanism 11 will open the channel to allow water to enter the punching shell 10 and be sprayed out along with the airflow, so as to achieve the effect of dust reduction and wetting the slot hole wall.
[0041] S5: Finally, use a cleaning tool to clean and remove the debris in the groove, pour the pre-mixed concrete repair slurry into the groove, and use a vibrating tool to treat the concrete repair liquid. At this time, the concrete repair liquid will flow into the groove hole and fill the groove hole. When the concrete repair liquid solidifies, it will increase the contact surface between the concrete repair liquid and the bridge pavement, thereby increasing the repair bonding strength.
[0042] Example 2
[0043] This embodiment is intended to promote the solution of the problem of how to reduce the impact of the recoil force generated by the collision on the movement of the second push block 23. This embodiment is an improvement made on the basis of embodiment 1. For details, please refer to Figures 1 to 5 , a connecting gear 16 is provided at the output end of the motor 15, and a transmission gear 17 is meshedly connected to the side of the connecting gear 16, and the diameter of the connecting gear 16 is smaller than the diameter of the transmission gear 17, and a rotating disk 18 is provided at the end of the transmission gear 17, and a connecting column 19 is fixedly connected to the outer wall of the rotating disk 18, and a movable rod 20 is movably connected to the outside of the connecting column 19, and a docking block 21 is movably connected to the end of the movable rod 20, and a first push block 22 is fixedly connected to the outer wall of the docking block 21, and a second push block 23 is provided on the side of the first push block 22, and a connecting groove 24 is provided on the surface of the second push block 23, and a stamping block 25 is provided on the right side of the second push block 23, and a docking outer edge 26 is integrally provided on the outer wall of the stamping block 25;
[0044] The engine 3 is controlled to drive the cutting machine 4 to rotate, the cracked ground is cut, and the ground at the crack is cut into pieces, and the crack debris is shoveled away with a cleaning tool, and then the mounting seat 8 is driven by the hydraulic rod 7 to move on the support frame 6 to adjust the position of the docking seat 9 and the punching shell 10, and the chisel head 31 is connected to the crack groove wall after the cutting process, and the motor 15 is controlled to drive the connecting gear 16 and the transmission gear 17 to rotate, so that the rotating disk 18 drives the connecting column 19 to rotate, and the connecting column 19 is movably connected with a movable rod 20, and the end of the movable rod 20 is movably connected with a docking block 21, and the rotating disk 18 is used to drive the movable rod 20 to reciprocate by rotating, and when the docking block 21 moves, it will simultaneously drive the first push block 22 and the second push block 23 to move, so that the first push block 22 and the second push block 23 reciprocate in the punching shell 10;
[0045] A stamping block 25 is arranged on the side of the second pushing block 23, and there is a gap between the two. When the second pushing block 23 moves, the air between the gap will be squeezed, thereby driving the stamping block 25 to move in the punching shell 10. When the subsequent stamping block 25 collides with the impact head 28, the air between the stamping block 25 and the second pushing block 23 is used to buffer the impact rebound force to avoid the rebound force directly acting on the second pushing block 23. A docking outer edge 26 is provided on the stamping block 25 to increase the contact surface with the punching shell 10, so as to facilitate the subsequent blocking of the entrance of the first channel 38. The groove on the second pushing block 23 is used to maintain the relative distance between the stamping block 25 and the docking outer edge 26 on the second pushing block 23 to effectively avoid the collision between the two.
[0046] Example 3
[0047] This embodiment is intended to help solve the problem of how to blow out the debris generated by the opening when opening the crack groove wall. This embodiment is an improvement made on the basis of embodiment 1. For details, please refer to Figures 4 to 7 The outer surface of the punching block 25 is fitted with the outer surface of the punching shell 10, and a first channel 38 is opened inside the punching shell 10, and a second channel 39 is arranged on the side of the first channel 38, and the inner wall of the punching shell 10 is fixedly connected with a connecting seat 27, and a collision head 28 is movably installed on the inner side of the connecting seat 27, and the end of the collision head 28 is fixedly connected with a connecting disk 29, and the end of the connecting disk 29 is fixedly connected with a docking rod 30, and a first spring 32 is nested outside the docking rod 30, and a connecting channel 33 is opened at an equal angle inside the connecting seat 27, and a limiting rod 34 is arranged inside the connecting channel 33, and a blocking block 35 is fixedly connected to the end of the limiting rod 34, and a second spring 36 is arranged on the side of the blocking block 35;
[0048] When the punch block 25 moves and contacts the impact head 28, the impact head 28 is squeezed to make it slide in the connection seat 27. When the punch block 25 moves, the connection plate 29 and the docking rod 30 are driven to move. The end of the docking rod 30 is fixedly connected with a chisel head 31, so that the chisel head 31 can move. At the same time, the first spring 32 can be squeezed. The reciprocating motion of the punch block 25 and the first spring 32 is used to realize the telescopic motion of the chisel head 31, so as to impact and open a hole in the crack groove wall.
[0049] When the punching block 25 moves toward the impact head 28, the punching block 25 will squeeze the space between the two to allow air to enter the connecting channel 33. As the punching block 25 and the impact head 28 approach each other, the pressure in the connecting channel 33 will increase, and then the blocking block 35 in the connecting channel 33 will be pushed up, allowing the blocking block 35 to drive the limit rod 34 to move and squeeze the second spring 36 to open the through holes on both sides of the limit rod 34, allowing the air flow to be ejected from the nozzle 37 through the through holes, thereby achieving the goal of ejecting air at the opening while opening the hole, blowing out the debris generated by the opening, and avoiding the accumulation of a large amount of debris in the hole that affects the subsequent opening of the hole.
[0050] Example 4
[0051] This embodiment is intended to promote the solution of the problem of how to automatically block the connection channel 33 during suction to prevent the air with a large amount of dust from entering the interior and affecting the service life of the device. This embodiment is an improvement made on the basis of embodiment 1. For details, please refer to Figure 6 and Figure 8 The air intake mechanism 13 includes an air intake housing 1301, an extrusion column 1302, an extrusion block 1303, a limiting column 1304 and a compression spring 1305, and the extrusion column 1302 is nested inside the air intake housing 1301, and the end of the extrusion column 1302 is fixedly connected to the extrusion block 1303, and the extrusion column 1302 is arranged at an equal angle, and the end of the air intake mechanism 13 is connected to the filter head 14, the interior of the extrusion block 1303 passes through the limiting column 1304, and the limiting column 1304 and the air intake housing 1301 are welded, and the bottom of the extrusion block 1303 is provided with a compression spring 1305, and the compression spring 1305 is nested outside the limiting column 1304;
[0052] When the punching block 25 moves to the left from the impact head 28, a suction negative pressure will be generated on the right side of the punching block 25. The generated negative pressure cooperates with the return elastic force of the second spring 36 to allow the blocking block 35 to block the flow channel. Regarding the air outlet flow channel, it is prevented that the air with a high dust content at the opening will flow back into the punching shell 10 through the connecting channel during the suction process, affecting the normal operation and service life of the internal components. The return elastic force of the first spring 32 will drive the docking rod 30 and the chisel head 31 to reset, so that the docking rod 30 and the connecting plate 29 are both provided with gaskets and contact the connecting seat 27, further improving its sealing performance.
[0053] When the punching block 25 drives the docking outer edge 26 to continue to move to the left, the suction negative pressure in the punching shell 10 will increase accordingly, and the suction negative pressure will suck the extrusion block 1303 through the second channel 39, so that the extrusion block 1303 drives the extrusion column 1302 to move downward and separate the air intake of the air intake shell 1301. The internal nesting of the extrusion block 1303 is provided with a limiting column 1304 to limit the movement of the extrusion block 1303. When the extrusion block 1303 moves, it will squeeze the compression spring 1305 and finally open the air intake hole, allowing the external gas to be filtered through the filter head 14 and then enter the punching shell 10 through the second channel 39 to relieve the suction negative pressure generated during the suction process.
[0054] Example 5
[0055] This embodiment is intended to promote the solution of the problem of how to reduce dust and wet the hole wall while punching. This embodiment is an improvement made on the basis of embodiment 1. For details, please refer to Figure 6 and Figure 8 The liquid storage mechanism 11 includes a liquid storage shell 1101, a sealing head 1102, a sealing block 1103, a sealing gasket 1104, a positioning block 1105 and an airbag 1106, and the sealing head 1102 is arranged inside the liquid storage shell 1101, and the end of the sealing head 1102 is fixedly connected with the sealing block 1103, and the end of the liquid storage mechanism 11 is connected with a connecting pipe 12, the outer surface of the sealing block 1103 is bonded with the sealing gasket 1104, and the top of the sealing gasket 1104 and the bottom of the liquid storage shell 1101 are fitted with each other, and positioning blocks 1105 are arranged on both sides of the sealing block 1103, and the bottom of the sealing block 1103 is fitted with the airbag 1106, and the inside of the sealing block 1103 is symmetrically provided with through holes, the end of the connecting pipe 12 is connected with the water tank 5, and the water tank 5 is connected with the liquid storage mechanism 11 through the connecting pipe 12;
[0056] When the punch block 25 continues to move to the left, the punch block 25 will expose the entrance of the first channel 38. As the punch block 25 continues to move, the suction negative pressure opens the air inlet channel of the air inlet mechanism 13, and at the same time, the suction negative pressure sucks the sealing block 1103, so that the sealing block 1103 drives the sealing head 1102 to move downward, and positioning blocks 1105 are provided on both sides of the sealing block 1103 to position the movement of the sealing block 1103, so that the sealing gasket 1102 on the sealing block 1103 can be moved downward. 04 is separated from the liquid storage shell 1101, and the air bag 1106 is squeezed to open the liquid circulation channel, so that the water in the water tank 5 enters the punching shell 10 through the connecting pipe 12 and the liquid storage mechanism 11, so that when the punching block 25 reciprocates, the water will follow the gas and be sprayed out through the nozzle 37 at the connecting channel 33. The nozzle 37 is an atomizing nozzle, so that the sprayed water mist can reduce the dust generated by the punching, and the sprayed water mist is sprayed on the hole wall, which can have the effect of wetting the hole wall;
[0057] It should be noted that when the punching block 25 moves to the rightmost end and collides and squeezes the impact head 28, the docking outer edge 26 on the punching block 25 will still block the entrance of the first channel 38 to prevent the air between the second push block 23 and the punching block 25 from being connected to the first channel 38. When the punching block 25 moves from right to left, the flow channel of the air intake mechanism 13 will be opened first, and then the flow channel of the liquid storage mechanism 11 will be opened. By staggered opening of the two channels, the air entering the punching shell 10 is much larger than the water intake, avoiding the problem of a large amount of water spraying and the need to deal with the accumulated water later. When the filter head 14 on the air intake mechanism 13 is slightly blocked (the filter head 14 is composed of a pipe and a filter element), the suction force at the liquid storage mechanism 11 will be too large, causing the air bag 1106 to be over-extruded and deformed, thereby reducing the water flow channel, thereby relatively increasing the suction force at the air intake mechanism 13, and again achieving the effect of the air intake being greater than the water intake, so that it has an automatic regulation effect.
[0058] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0059] The contents not described in detail in this specification belong to the prior art known to professional and technical personnel in this field.
[0060] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A rapid repair process for a bridge pavement, characterized in that: The steps include: S1: First, the handrail frame (2) is pushed to drive the support base (1) to move on the ground, and the engine (3) is controlled to drive the cutting machine (4) to rotate, so as to cut the crack edge of the bridge pavement, cut the pavement at the crack into fragments, and use tools to clean and remove the fragments, so as to form a regular groove on the bridge pavement; S2: controlling the hydraulic rod (7) on the support frame (6) to drive the mounting seat (8) and the docking seat (9) to move up and down, so that the punching shell (10) and the chisel head (31) are embedded in the groove, and the end of the chisel head (31) is in contact with the groove wall; S3: Then, the motor (15) in the docking seat (9) is controlled to move, driving the first push block (22) and the second push block (23) to reciprocate in the connection housing, thereby causing the punching block (25) to impact the impact head (28), so that the docking rod (30) and the chisel head (31) can reciprocate, impacting and opening the groove wall, and densely forming a plurality of slots on the groove wall; The output end of the motor (15) is provided with a connecting gear (16), and the side of the connecting gear (16) is meshingly connected with a transmission gear (17), and the diameter of the connecting gear (16) is smaller than the diameter of the transmission gear (17), and a rotating disk (18) is provided at the end of the transmission gear (17), and the outer wall of the rotating disk (18) is fixedly connected with a connecting column (19), and the outside of the connecting column (19) is movably connected with a movable rod (20); The end of the movable rod (20) is movably connected to a docking block (21), and the outer wall of the docking block (21) is fixedly connected to a first push block (22), and a second push block (23) is provided on the first push block (22), and a connecting groove (24) is provided on the surface of the second push block (23), and a punching block (25) is provided on the right side of the second push block (23), and a docking outer edge (26) is integrally provided on the outer wall of the punching block (25); The outer surface of the punching block (25) is in contact with the outer surface of the punching shell (10), and a first channel (38) is provided inside the punching shell (10), and a second channel (39) is provided at the junction of the first channel (38), and a connecting seat (27) is fixedly connected to the inner wall of the punching shell (10), a collision head (28) is movably mounted inside the connecting seat (27), and a connecting plate (29) is fixedly connected to the end of the collision head (28), and a docking rod (30) is fixedly connected to the end of the connecting plate (29), and a first spring (32) is nested outside the docking rod (30); The connection seat (27) has connection channels (33) formed at equal angles inside, and a limit rod (34) is provided inside the connection channel (33), and a blocking block (35) is fixedly connected to the end of the limit rod (34), and a second spring (36) is provided on the side of the blocking block (35); S4: When the chisel head (31) makes a reciprocating motion, the air intake mechanism (13) and the nozzle (37) cooperate with each other to achieve the chisel head (31) to spray airflow at the slot hole while striking the hole, thereby blowing out the debris in the slot hole. At the same time, the liquid storage mechanism (11) opens the channel to allow water to enter the punching shell (10) and be sprayed out along with the airflow, thereby achieving the effect of dust reduction and wetting the slot hole wall. S5: Finally, use a cleaning tool to clean and remove the debris in the groove, pour the pre-mixed concrete repair slurry into the groove, and use a vibrating tool to treat the concrete repair liquid. At this time, the concrete repair liquid will flow into the groove hole and fill the groove hole. When the concrete repair liquid solidifies, it will increase the contact surface between the concrete repair liquid and the bridge pavement, thereby increasing the repair bonding strength.
2. A rapid bridge pavement repair process according to claim 1, characterized in that: The liquid storage mechanism (11) comprises a liquid storage housing (1101), a sealing head (1102), a sealing block (1103), a sealing gasket (1104), a positioning block (1105) and an airbag (1106); the sealing head (1102) is arranged inside the liquid storage housing (1101), and the end of the sealing head (1102) is fixedly connected to the sealing block (1103); and the end of the liquid storage mechanism (11) is connected to a connecting tube (12).
3. A rapid bridge pavement repair process according to claim 2, characterized in that: The outer surface of the sealing block (1103) is bonded to a sealing gasket (1104), and the top of the sealing gasket (1104) is in contact with the bottom of the liquid storage shell (1101), and positioning blocks (1105) are provided on both sides of the sealing block (1103). At the same time, the bottom of the sealing block (1103) is in contact with an air bag (1106), and through holes are symmetrically provided inside the sealing block (1103).
4. The rapid repair process for a bridge pavement according to claim 2 is characterized by: The end of the connecting pipe (12) is connected to a water tank (5), and the water tank (5) is in communication with the liquid storage mechanism (11) via the connecting pipe (12).
5. The rapid repair process for a bridge pavement according to claim 1 is characterized by: The air intake mechanism (13) comprises an air intake housing (1301), an extrusion column (1302), an extrusion block (1303), a limiting column (1304) and a compression spring (1305), wherein the air intake housing (1301) is provided with an extrusion column (1302) nested inside, and the end of the extrusion column (1302) is fixedly connected to the extrusion block (1303), and the extrusion column (1302) is arranged at an equal angle, and the end of the air intake mechanism (13) is connected to a filter head (14).
6. A rapid bridge pavement repair process according to claim 5, characterized in that: The interior of the extrusion block (1303) passes through the limiting column (1304), and the limiting column (1304) and the air intake housing (1301) are welded together. A compression spring (1305) is provided at the bottom of the extrusion block (1303), and the compression spring (1305) is nested on the outside of the limiting column (1304).