A method and system for comprehensive utilization of sulfur dioxide tail gas
By reacting sulfur dioxide in the exhaust gas with fluorine gas to generate sulfuryl fluorine, and absorbing water and hydrolyzing it into mixed acid, the problems of low removal efficiency and by-product treatment in the existing exhaust gas treatment are solved, and efficient and low-cost exhaust gas treatment and Resource recycling.
Patent Information
- Application Number
- CN202310488605.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-28
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2043-04-28
AI Technical Summary
In the existing exhaust gas treatment process, the removal efficiency of sulfur dioxide is low and there are problems with by-product treatment. The existing methods have high energy consumption and high cost, and the exhaust gas after treatment may exceed the standard, which requires further neutralization treatment.
The exhaust gas containing sulfur dioxide is reacted with fluorine gas to form sulfuryl fluorine, and the mixed acid that is hydrolyzed into sulfuric acid and hydrofluoric acid is absorbed by water. The mixed acid is used in the washing process in the hydrogen fluoride process to achieve efficient removal of sulfur dioxide and complete recycling of resources.
The efficient removal of sulfur dioxide is achieved. The sulfur dioxide concentration in the treated exhaust gas can reach below 100mg/m3, and there is no need for neutralization treatment, which reduces energy consumption and operating costs, and improves resource utilization.
Smart Images

Figure CN116495708B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of tail gas treatment, and in particular relates to a comprehensive utilization method of sulfur dioxide tail gas. Background Art
[0002] In the current preparation process of hydrogen fluoride, whether it is the fluorite method, the fluorosilicic acid method or other methods, due to the influence of raw materials, process control, etc., it is inevitable that sulfur dioxide will be contained in the process exhaust gas.
[0003] The current industrial waste gas desulfurization processes mainly include limestone / lime-gypsum method, ammonia method, double alkali method, etc.
[0004] The limestone / lime-gypsum method uses limestone or lime as a desulfurization absorbent, which reacts with sulfur dioxide in the flue gas to form calcium sulfite, which then contacts oxygen in the air to form calcium sulfate. The process is simple and does not require high equipment. The problem is that the process is difficult to control and the absorption efficiency is not high.
[0005] Ammonia desulfurization uses ammonia as a sulfur dioxide absorbent. Ammonia reacts with sulfur dioxide to form ammonium sulfite, which then reacts with oxygen to form ammonium sulfate. Due to the volatility of ammonia, the tail gas after desulfurization contains ammonia, causing secondary pollution.
[0006] Patent CN201811290654.7 provides a process for treating sulfur dioxide in tail gas by a double alkali method. The process is to react sodium alkali in the form of dry powder or slurry with sulfur-containing flue gas to generate sodium sulfate, which is then mixed with water to form a slurry. The obtained slurry is reacted with a mixture of ammonium bicarbonate and ammonium sulfate to regenerate, and the regenerated sodium bicarbonate crystals are returned to the desulfurization unit to continue to be used as a desulfurizer. The remaining mother liquor reacts with calcium oxide or calcium hydroxide to generate calcium sulfate precipitation, and the mother liquor is regenerated and reused in the regeneration process of the desulfurizer. The calcium sulfate generated in this process is difficult to recycle, and stacking treatment is prone to secondary pollution.
[0007] The above schemes all utilize the acid-base neutralization principle to absorb sulfur dioxide in the tail gas, and there is a problem of handling by-products.
[0008] In addition, patent CN202221533834.5 discloses a treatment device for tail gas generated during the production of hydrogen fluoride, which is to oxidize the sulfur dioxide tail gas generated by the hydrogen fluoride production terminal to generate sulfur trioxide, which is absorbed by 93.8% sulfuric acid to make 98% sulfuric acid. 98% sulfuric acid can be used in the production system, realizing the comprehensive utilization of sulfur dioxide tail gas. However, this method is to react sulfur dioxide with oxygen, which needs to be carried out under heating and catalyst conditions. The heating temperature is 400-500°C, which has high energy consumption, high investment and operation costs. Moreover, the sulfur dioxide in the tail gas treated by this method may still exceed the standard, and further alkali neutralization treatment is required. Summary of the invention
[0009] In view of the above-mentioned defects in the prior art, the present invention provides a method for comprehensive utilization of sulfur dioxide tail gas, and the specific scheme is:
[0010] A method for comprehensive utilization of sulfur dioxide tail gas comprises the following steps:
[0011] 1) reacting tail gas containing sulfur dioxide with an oxidizing gas to obtain a mixed gas, wherein the tail gas is produced by a hydrogen fluoride production process, and the oxidizing gas is a mixture of fluorine gas and an inert carrier gas;
[0012] 2) absorbing water into the mixed gas obtained in step 1) to obtain a mixed acid;
[0013] 3) The mixed acid in step 2) is recycled for washing hydrogen fluoride in the hydrogen fluoride production process.
[0014] In the present invention, fluorine gas is reacted with sulfur dioxide to generate sulfuryl fluoride, and then the mixed gas after the reaction is absorbed by water, and the sulfuryl fluoride is hydrolyzed to generate mixed acid. The reaction formula is as follows:
[0015] SO2+F2→SO2F2
[0016] SO2F2+2H2O→H2SO4+2HF
[0017] The reaction between sulfur dioxide and fluorine gas can be carried out violently at room temperature and pressure, with fast reaction speed and high conversion rate. Therefore, the removal rate of sulfur dioxide is high, and the sulfur dioxide concentration in the treated tail gas can directly reach the required 100mg / m 3 No neutralization treatment is required below.
[0018] The generated sulfuryl fluoride water is hydrolyzed into a mixed acid of sulfuric acid and hydrofluoric acid after absorption. The mixed acid can be used as a washing acid for hydrogen fluoride in the hydrogen fluoride production process. During the washing process, hydrogen fluoride can be desorbed to improve resource utilization.
[0019] Preferably, in step 1), the tail gas is the tail gas generated in the process of producing hydrogen fluoride. In the process of producing hydrogen fluoride, processes such as condensation and degassing will generate tail gas containing sulfur dioxide and hydrogen fluoride.
[0020] Preferably, the inert carrier gas is nitrogen, and the volume fraction of fluorine gas in the oxidizing gas is 1-50%. Since the reaction between fluorine gas and sulfur dioxide is too violent, it is necessary to use an inert gas for dilution to control the concentration of fluorine gas to control the reaction rate. Using nitrogen as an inert carrier gas is relatively low in cost. When the volume fraction of fluorine gas in the oxidizing gas is higher than 50%, the reaction rate is too fast, and there is a safety hazard.
[0021] Preferably, the molar ratio of fluorine gas in the oxidizing gas to sulfur dioxide in the tail gas is 1.0-1.05: 1. Fluorine gas can be slightly excessive to ensure the conversion rate of sulfur dioxide, and unreacted fluorine gas reacts with water to generate hydrogen fluoride when absorbed by water, thereby achieving complete recovery.
[0022] Preferably, the reaction temperature in step 1) is 10-25° C. The reaction of sulfur dioxide and fluorine gas can be carried out at room temperature without heating.
[0023] Preferably, the absorption temperature in step 2) is 20-50° C. Increasing the temperature is beneficial to the absorption and hydrolysis efficiency of sulfuryl fluoride.
[0024] In order to realize the method of the present invention, the present invention further discloses a comprehensive utilization system of sulfur dioxide tail gas, comprising a primary reactor and a secondary reactor connected in sequence, the primary reactor is provided with a tail gas inlet and an oxidizing gas inlet, the secondary reactor is provided with an absorption water inlet and a mixed acid outlet, and the mixed acid outlet is connected to a hydrogen fluoride washing tower of a hydrogen fluoride production system.
[0025] The tail gas inlet is connected to the tail gas outlet of the hydrogen fluoride production system, and the oxidizing gas inlet is used to introduce a fluorine-nitrogen mixed gas. The sulfur dioxide in the tail gas reacts with the fluorine gas in the primary reactor to generate a mixed gas containing sulfuryl fluoride. The mixed gas enters the secondary reactor, and the water entering from the absorption water inlet is absorbed, and the sulfuryl fluoride undergoes a hydrolysis reaction to generate a mixed acid of sulfuric acid and hydrofluoric acid. The mixed acid is then transported to the hydrogen fluoride washing tower of the hydrogen fluoride production system to wash the hydrogen fluoride and recover the hydrogen fluoride in the mixed acid.
[0026] Specifically, the primary reactor is a microchannel reactor or a continuous flow reactor. Both the microchannel reactor and the continuous flow reactor can realize the continuous chemical reaction. Among them, the microchannel reactor is more conducive to the mixing efficiency of the reactants, and can improve the reaction speed and conversion rate. In the present invention, it is conducive to improving the removal rate of sulfur dioxide.
[0027] Specifically, the secondary reactor is a microchannel reactor or a spray absorption tower. Similarly, the use of a microchannel reactor is conducive to improving the absorption and hydrolysis efficiency of sulfuryl fluoride.
[0028] Preferably, both the primary reactor and the secondary reactor are microchannel reactors.
[0029] When the method of the present invention is used to treat tail gas from a hydrogen fluoride production process, the process flow is simple, the operation cost is low, and it is easy to implement. The sulfur dioxide concentration in the tail gas after treatment according to the method of the present invention can reach 100 mg / m 3 The following emission standards are not required for neutralization treatment. The present invention can also achieve complete recycling of resources. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] The present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0031] Figure 1 It is a schematic flow chart of the method of the present invention;
[0032] Figure 2 It is a system schematic diagram of Example 4. DETAILED DESCRIPTION
[0033] The present invention is described clearly below in conjunction with the drawings and specific embodiments in the embodiments of the present invention. The description herein is only used to explain the present invention, but is not intended to limit the present invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work, any modifications, equivalent substitutions, improvements, etc., should be included in the protection scope of the present invention.
[0034] Example
[0035] like Figure 1 As shown, the technical solutions in the embodiments of the present invention will be clearly and completely described below in combination with the embodiments of the present invention.
[0036] Embodiment 1:
[0037] A comprehensive utilization method of sulfur dioxide tail gas:
[0038] (1) reacting the hydrogen fluoride process tail gas with a fluorine-nitrogen mixed gas containing 1% fluorine gas at a ratio of n (fluorine gas): n (sulfur dioxide in the tail gas) = 1.05:1 at 25° C. to obtain a mixed gas;
[0039] (2) spraying and absorbing the mixed gas in step (1) with water at 25° C. until the sulfuric acid content in the mixed acid reaches 30%;
[0040] (3) The mixed acid containing 30% sulfuric acid in step (2) is recycled to the hydrogen fluoride process for washing hydrogen fluoride.
[0041] Embodiment 2:
[0042] (1) reacting the hydrogen fluoride process tail gas with a fluorine-nitrogen mixed gas containing 25% fluorine gas at a ratio of n (fluorine gas): n (sulfur dioxide in the tail gas) = 1.02:1 at 15° C. to obtain a mixed gas;
[0043] (2) spraying and absorbing the mixed gas in step (1) with water at 40° C. until the sulfuric acid content in the water reaches 40%;
[0044] (3) 40% of the sulfuric acid in step (2) is recycled to the hydrogen fluoride process for washing hydrogen fluoride.
[0045] Embodiment 3:
[0046] (1) reacting the hydrogen fluoride process tail gas with a fluorine-nitrogen mixed gas containing 50% fluorine gas at a ratio of n (fluorine gas): n (sulfur dioxide in the tail gas) = 1:1 at 10° C. to obtain a mixed gas;
[0047] (2) spraying and absorbing the mixed gas in step (1) with water at 50° C. until the sulfuric acid content in the water reaches 50%;
[0048] (3) 50% of the sulfuric acid in step (2) is recycled to the hydrogen fluoride process for washing the hydrogen fluoride.
[0049] The content of sulfur dioxide in the tail gas of Example 1-3 before and after treatment was tested, and the results are shown in the following table:
[0050]
[0051] It can be seen from the table that the sulfur dioxide content of the tail gas treated by this method is reduced to 100 mg / m 3 Below, meet the emission standards.
[0052] In Examples 1-3, the reaction of tail gas and fluorine is carried out in a continuous flow reactor, and the mixed gas is subjected to water absorption in a spray tower.
[0053] Example 4
[0054] According to the process parameters of Example 1, the tail gas treatment of this embodiment is as follows Figure 2 The system shown in the figure is carried out, the system includes a primary reactor 1 and a secondary reactor 2 connected in sequence, the primary reactor is provided with a tail gas inlet 3 and an oxidizing gas inlet 4, the secondary reactor is provided with an absorption water inlet 5 and a mixed acid outlet 6, the mixed acid outlet is connected to the hydrogen fluoride washing tower of the hydrogen fluoride production system, and the primary reactor and the secondary reactor are both microchannel reactors. The reaction of tail gas and fluorine is carried out in the microchannel reactor, and the water absorption of the mixed gas is also carried out in the microchannel reactor. In Example 1, the removal rate of sulfur dioxide is 98.5%, and in this embodiment, the removal rate of sulfur dioxide is increased to 99.0%.
Claims
1. A method for comprehensive utilization of sulfur dioxide tail gas, characterized in that: The following steps are involved: 1) reacting the tail gas containing sulfur dioxide with an oxidizing gas to obtain a mixed gas, wherein the oxidizing gas is a mixture of fluorine gas and an inert carrier gas; 2) absorbing water into the mixed gas obtained in step 1) to obtain a mixed acid; 3) The mixed acid in step 2) is recycled for washing hydrogen fluoride in the hydrogen fluoride production process.
2. The method for comprehensive utilization of sulfur dioxide tail gas according to claim 1, characterized in that: In step 1), the tail gas is the tail gas generated in the process of preparing hydrogen fluoride.
3. The method for comprehensive utilization of sulfur dioxide tail gas according to claim 1, characterized in that: In step 1), the inert carrier gas is nitrogen, and the volume fraction of fluorine gas in the oxidizing gas is 1-50%.
4. The method for comprehensive utilization of sulfur dioxide tail gas according to claim 1, characterized in that: In step 1), the molar ratio of fluorine gas in the oxidizing gas to sulfur dioxide in the tail gas is 1.0-1.05:
1.
5. The method for comprehensive utilization of sulfur dioxide tail gas according to claim 1, characterized in that: Step 1) The reaction temperature is 10-25°C.
6. The method for comprehensive utilization of sulfur dioxide tail gas according to claim 1, characterized in that: The absorption temperature in step 2) is 20-50°C.
7. A comprehensive utilization system of sulfur dioxide tail gas, characterized in that: The invention comprises a primary reactor and a secondary reactor which are connected in sequence. The primary reactor is provided with a tail gas inlet and an oxidizing gas inlet. The secondary reactor is provided with an absorption water inlet and a mixed acid outlet. The mixed acid outlet is connected to a hydrogen fluoride washing tower of a hydrogen fluoride production system.
8. The comprehensive utilization system of sulfur dioxide tail gas according to claim 7, characterized in that: The primary reactor is a microchannel reactor or a continuous flow reactor.
9. The comprehensive utilization system of sulfur dioxide tail gas according to claim 7, characterized in that: The secondary reactor is a microchannel reactor or a spray absorption tower.