Chips and electronic devices

By segmenting field oxygen and adding auxiliary field oxygen in the power semiconductor chip to form a buffer structure, the cracking problem caused by stress mismatch between the metal layer and the passivation layer is solved, thereby improving the reliability of the chip and the functional stability of the device.

CN116799042BActive Publication Date: 2026-11-10HUAWEI DIGITAL POWER TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202210262835.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-17
Publication Date
2026-11-10
Estimated Expiration
2042-03-17

AI Technical Summary

Technical Problem

During temperature cycling or thermal shock testing of power semiconductor chips, excessive stress caused by the mismatch in the thermal expansion coefficients of the metal layer and the passivation layer can lead to cracks in the passivation layer at the step of the metal layer, allowing moisture to enter the chip and affecting device reliability.

Method used

The field oxygen is divided into main field oxygen and auxiliary field oxygen, or auxiliary field oxygen is added on the basis of main field oxygen to form a buffer structure, which reduces the stress between the metal layer and the passivation layer, and reduces the risk of cracking of the passivation layer by adjusting the thickness and shape of the metal layer.

Benefits of technology

It effectively reduces the risk of passivation layer cracking, prevents moisture from entering the chip, and improves chip reliability and device functional stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116799042B_ABST
    Figure CN116799042B_ABST
Patent Text Reader

Abstract

This application provides a chip and electronic device, relating to the field of chip technology, which can reduce the risk of passivation layer cracking and improve chip reliability. The chip is divided into a main functional region, a transition region, and a protection region, with the transition region located between the main functional region and the protection region. The chip includes a field oxide layer, a metal layer, and a passivation layer sequentially stacked on a semiconductor substrate. The field oxide layer and the passivation layer are located in the transition region and the protection region, while the metal layer is located in the main functional region and the transition region. In the transition region, the field oxide layer includes a main field oxide layer and at least one auxiliary field oxide layer spaced apart, with the auxiliary field oxide layer located on the side of the main field oxide layer facing the main functional region. In the transition region, the metal layer extends from the main functional region to the side of the main field oxide layer facing away from the semiconductor substrate. The passivation layer extends from the side of the metal layer facing away from the semiconductor substrate to the side of the metal layer facing away from the main functional region, covering the surface of the metal layer facing away from the semiconductor substrate and the side of the metal layer facing away from the main functional region.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of chip technology, and more particularly to a chip and an electronic device. Background Technology

[0002] Power semiconductor devices, as core components in electronic circuits, can be used to achieve efficient transmission and conversion of electrical energy, and to realize efficient utilization of electrical energy.

[0003] Power semiconductor devices can be integrated into power semiconductor chips. To prevent external moisture and mobile ions (e.g., sodium) from affecting the power semiconductor devices inside the power semiconductor chip, a passivation layer is usually covered on the portion of the metal layer located in the terminal region of the power semiconductor chip to block moisture.

[0004] However, in some scenarios, when performing reliability tests such as temperature cycle test (TCT) or thermal shock (TS) on semiconductor devices, the mismatch in the thermal expansion coefficients of the metal layer and the passivation layer causes stress to be generated between the metal layer and the passivation layer due to mutual compression. Excessive stress causes cracks to form in the passivation layer at the step of the metal layer, which in turn allows moisture to enter the active region of the power semiconductor chip through the cracks in the passivation layer and corrode the power semiconductor device, affecting the reliability of the power semiconductor device. Summary of the Invention

[0005] To address the aforementioned technical problems, this application provides a chip and electronic device that can reduce the risk of passivation layer cracking and improve chip reliability.

[0006] In a first aspect, this application provides a chip divided into a main functional region, a transition region, and a protection region, with the transition region located between the main functional region and the protection region. The chip includes a field oxide layer, a metal layer, and a passivation layer sequentially stacked on a semiconductor substrate. The field oxide layer and the passivation layer are located in the transition region and the protection region, respectively, while the metal layer is located in the main functional region and the transition region. In the transition region, the field oxide layer includes a main field oxide layer and at least one auxiliary field oxide layer spaced apart, with the auxiliary field oxide layer located on the side of the main field oxide layer facing the main functional region. In the transition region, the metal layer extends from the main functional region to the side of the main field oxide layer facing away from the semiconductor substrate. The passivation layer extends from the side of the metal layer facing away from the semiconductor substrate to the side of the metal layer facing away from the main functional region, covering the surface of the metal layer facing away from the semiconductor substrate and the side of the metal layer facing away from the main functional region.

[0007] In this application, the existing field oxygen is divided into a main field oxygen and at least one auxiliary field oxygen in the transition region, or at least one auxiliary field oxygen is added to the existing main field oxygen, with the main field oxygen and at least one auxiliary field oxygen spaced apart. In this way, at least one auxiliary field oxygen can act as a buffer, preventing stress from the metal layer extending from the main functional region to the side of the main field oxygen away from the semiconductor substrate from being transmitted to the passivation layer. This effectively reduces the stress between the large-size metal layer and the passivation layer, reduces the risk of passivation layer cracking, and prevents moisture from entering the main functional region of the chip through cracks in the passivation layer, thus affecting the function of the devices in the main functional region.

[0008] In some possible implementations, to prevent moisture from entering the main functional region through the field oxygen, the passivation layer can extend from the side of the metal layer away from the main functional region to the side of the main field oxygen away from the main functional region. In this case, the metal layer can cover a portion of the surface of the main field oxygen away from the semiconductor substrate; or, the metal layer can completely cover the surface of the main field oxygen away from the semiconductor substrate.

[0009] Optionally, in the transition region, the metal layer covers a portion of the surface of the main field oxygen on the side facing away from the semiconductor substrate. In this way, along the direction from the semiconductor substrate to the metal layer, the passivation layer can first ascend from the side facing away from the main field oxygen to the side facing away from the semiconductor substrate; then ascend from the side facing away from the main functional region of the metal layer to the side facing away from the semiconductor substrate of the metal layer. This avoids the passivation layer simultaneously ascending at the steps of the main field oxygen and the metal layer, increasing the total height of the steps required for the passivation layer to ascend, thereby reducing the risk of cracking of the passivation layer.

[0010] In some possible implementations, the number of auxiliary field oxygen atoms can be one; or, the number of auxiliary field oxygen atoms can be multiple. The number of auxiliary field oxygen atoms is related to the size of the auxiliary field oxygen atoms, the size of the primary field oxygen atoms, the spacing between the auxiliary and primary field oxygen atoms, the spacing between adjacent auxiliary field oxygen atoms, and the size of the chip. Specifically, when there are multiple auxiliary field oxygen atoms, they are spaced apart.

[0011] Optionally, there can be three auxiliary oxygen fields. Along the direction from the main functional area to the protected area, the length of each auxiliary oxygen field ranges from [0.2 μm to 100 μm], and the spacing between adjacent auxiliary oxygen fields ranges from [0.2 μm to 100 μm].

[0012] For example, taking a distance of 100 μm between the side of the auxiliary oxygen field closest to the main functional area and the side of the main oxygen field away from the main functional area, the length of the main oxygen field along the direction from the main functional area to the protected area can be 50 μm, the length of each auxiliary oxygen field can be 10 μm, and the spacing between adjacent auxiliary oxygen fields, as well as the spacing between the main oxygen field and auxiliary oxygen fields, can be 5 μm. In this case, the number of auxiliary oxygen fields can be three.

[0013] In some possible implementations, the metal layer includes a first portion and a second portion, the first portion being located at least in the main functional region and the second portion being located in the transition region; the thickness of the first portion is greater than the thickness of the second portion along the direction from the metal layer to the semiconductor substrate.

[0014] By reducing the thickness of the second part, this application can reduce the stress transmitted from the larger first part to the second part, thereby reducing the stress between the metal layer (or the second part) and the passivation layer, reducing the risk of passivation layer cracking, and preventing moisture from entering the main functional area of ​​the chip through cracks in the passivation layer, thus affecting the function of each device in the main functional area.

[0015] In some possible implementations, the first part, in addition to being located in the main functional region, can also extend from the main functional region to the transition region. In other words, besides the portion located in the main functional region, a portion of the first part is also located in the transition region. This prevents misalignment during the fabrication of the device in the main functional region due to process limitations, which could prevent the first part from forming a good contact relationship with other parts of the main functional region, thus affecting the performance of the device located in the main functional region. Furthermore, by placing the portion of the first part located in the transition region on the side of the auxiliary field oxygen facing the main functional region, in addition to utilizing at least one auxiliary field oxygen to buffer stress, it also prevents a large amount of stress from being transmitted to the passivation layer even after the thick metal layer has passed through at least one auxiliary field oxygen.

[0016] In some possible ways, the first and second parts of the metal layer can be prepared in the following manner:

[0017] In the first scenario, a first metal layer is formed on the side of the semiconductor substrate away from the field oxide layer using the same semiconductor process. The thickness of the first metal layer is the same as the thickness of the second portion, and the first metal layer is located in both the main functional region and the transition region. Next, a second metal layer is formed on the side of the first metal layer away from the semiconductor substrate using photolithography. The second metal layer is located at least in the main functional region. In this case, the materials of the first and second metal layers can be the same or different. For example, the thickness range of the first portion is [1 μm, 7 μm], and the thickness range of the second portion is [0.1 μm, 4 μm].

[0018] In the second scenario, photolithography is used to first form the second portion in the transition region. Then, photolithography is used to form the first portion in the main functional region (or the main functional region and the transition region). In this case, the materials of the first and second metal layers can be the same or different.

[0019] Of course, the first part can be formed in the main functional area (or the main functional area and the transition area) first, and the second part can be formed in the transition area later. This application does not limit this.

[0020] In the third scenario, a metal thin film and a second photoresist can be sequentially formed on the side of the field oxide layer away from the semiconductor substrate. The second photoresist is then partially exposed and developed to obtain a second photoresist pattern. This second photoresist pattern includes fully retained areas, partially retained areas, and fully exposed areas. The fully retained areas correspond to the metal layer to be formed, the partially retained areas correspond to the second portion to be formed, and the fully exposed areas correspond to other areas. Next, under the protection of the second photoresist pattern, the metal thin film is etched for the first time to obtain a metal pattern. Then, the second photoresist pattern is further exposed and developed to obtain a third photoresist pattern, which corresponds to the first portion to be formed. Finally, under the protection of the third photoresist pattern, the metal pattern is etched to obtain the first and second portions of the metal layer. In this case, the material of the first metal layer is the same as the material of the second metal layer.

[0021] In some possible implementations, for chips with a field-limiting ring structure for the transition and protection regions, the chip also includes an electrode layer located in the protection region. In the protection region, the electrode layer extends from the side of the main field oxygen away from the semiconductor substrate to the side of the main field oxygen adjacent to the main field oxygen away from the semiconductor substrate; the passivation layer extends from the side of the electrode layer away from the semiconductor substrate to the side of the electrode layer adjacent to the electrode layer away from the semiconductor substrate.

[0022] The electrode layer can be formed with the first part or the second part of the metal layer through the same semiconductor process. That is, the electrode layer can be formed at the same time as the first part is formed; or the electrode layer can be formed at the same time as the second part is formed.

[0023] In some possible implementations, the side of the metal layer away from the main functional region can also be a slope; along the direction from the metal layer to the semiconductor substrate, the distance between the slope and the main functional region gradually increases.

[0024] In this application, by setting the side of the metal layer away from the main functional area as an inclined surface, the inclined surface can act as a buffer for the passivation layer while keeping the height of the step of the passivation layer unchanged. This improves the problem of the passivation layer being prone to cracking at the step and prevents moisture from entering the active area of ​​the power semiconductor chip from the cracks in the passivation layer and corroding the power semiconductor device, thus affecting the reliability of the power semiconductor device.

[0025] In some possible implementations, the chip also includes a main junction that extends from the main functional region to the transition region and is in contact with at least one auxiliary field oxygen and a main field oxygen.

[0026] Secondly, this application also provides an electronic device, which includes a circuit board and the chip described in the first aspect, the chip being disposed on the circuit board.

[0027] The implementation method of the second aspect corresponds to any implementation method of the first aspect. The technical effects corresponding to the implementation method of the second aspect can be found in the first aspect and the technical effects corresponding to any implementation method of the first aspect mentioned above, and will not be repeated here. Attached Figure Description

[0028] Figure 1 A structural block diagram of the electronic device provided in the embodiments of this application;

[0029] Figure 2a A top-view diagram of a chip provided for related technologies;

[0030] Figure 2b for Figure 2a Enlarged view and cross-sectional diagram of region A in the middle;

[0031] Figure 2c A schematic diagram of the main junction of the terminal extension structure;

[0032] Figure 2d This is a schematic diagram of the main junction of a lateral doped structure.

[0033] Figure 3 A schematic diagram of the chip structure provided for related technologies;

[0034] Figure 4a A schematic diagram of the structure of a chip provided in an embodiment of this application;

[0035] Figure 4b This is a schematic diagram of another chip structure provided in an embodiment of this application;

[0036] Figure 4c This is another schematic diagram of the structure of the chip provided in the embodiments of this application;

[0037] Figure 5 This is another schematic diagram of the structure of the chip provided in the embodiments of this application;

[0038] Figure 6 This is another schematic diagram of the structure of the chip provided in the embodiments of this application;

[0039] Figure 7 for Figure 6 Enlarged view of the intermediate transition zone;

[0040] Figure 8 This is another schematic diagram of the structure of the chip provided in the embodiments of this application;

[0041] Figure 9aA process diagram illustrating the fabrication of the metal layer provided in the embodiments of this application;

[0042] Figure 9b A process diagram illustrating the fabrication of the metal layer provided in the embodiments of this application;

[0043] Figure 10a A process diagram illustrating the fabrication of the metal layer provided in the embodiments of this application;

[0044] Figure 10b A process diagram illustrating the fabrication of the metal layer provided in the embodiments of this application;

[0045] Figure 11 A process diagram illustrating the fabrication of the metal layer provided in the embodiments of this application;

[0046] Figure 12 This is another schematic diagram of the chip structure provided in the embodiments of this application.

[0047] Figure label:

[0048] 10-Semiconductor substrate; 11-Field plate; 12-Field oxide; 121-Main field oxide; 122-Secondary field oxide; 13-Passivation layer; 14-Main junction; 21-Metal layer; 211-First metal layer; 212-Second metal layer; 201-First part; 202-Second part. Detailed Implementation

[0049] To make the objectives, technical solutions, and advantages of this application clearer, the technical solutions of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.

[0050] The terms "first," "second," etc., used in the specification, embodiments, claims, and drawings of this application are for descriptive purposes only and should not be construed as indicating or implying relative importance or order. "And / or" describes the relationship between related objects, indicating that three relationships can exist. For example, "A and / or B" can mean: only A exists, only B exists, and both A and B exist simultaneously, where A and B can be singular or plural. The character " / " generally indicates that the preceding and following related objects are in an "or" relationship. "Installation," "connection," "linking," etc., should be interpreted broadly, for example, as a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, an indirect connection through an intermediate medium, or a connection within two elements. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion, such as including a series of steps or units. A method, system, product, or device is not necessarily limited to those steps or units explicitly listed, but may include other steps or units not explicitly listed or inherent to these processes, methods, products, or devices. Terms such as “up,” “down,” “left,” and “right” are used only in relation to the orientation of the components in the accompanying drawings. These directional terms are relative concepts used for relative description and clarification, and they can change accordingly depending on the orientation of the components in the accompanying drawings.

[0051] This application provides an electronic device, which can be a mobile phone, computer, tablet computer, automobile, wearable device, or other electronic device that requires a chip. Of course, the electronic device can also be other devices, and this application does not limit the specific form of the terminal. The chip mentioned can be any chip, including but not limited to power semiconductor chips. For ease of explanation, unless otherwise stated, the following description uses power semiconductor chips as examples.

[0052] Whether it is hydropower, thermoelectric power, wind power, or electrical energy generated by chemical batteries, most of it cannot be directly used in electronic devices. More than 75% of electrical energy must be converted by power semiconductor devices before it can be used in electronic devices.

[0053] like Figure 1 As shown, taking a car as an example, a car integrates a battery, switches, and DC / AC devices. The battery can provide DC voltage to the car, but the car needs AC voltage to start. Therefore, power semiconductor devices can act as switches to turn on the DC / AC devices, which then convert the received DC voltage into AC voltage, thereby starting the car under the control of the AC voltage.

[0054] As mentioned earlier, the passivation layer located in the terminal region is prone to cracking under stress, which can cause moisture to enter the active region and affect the reliability of power semiconductor devices.

[0055] Specifically, such as Figure 2a As shown, the chip may include a main functional region, a transition region, and a protection region. The transition region and protection region are located outside the main functional region, with the transition region situated between the main functional region and the protection region. The main functional region of the chip can correspond to the active region of a power semiconductor chip, and the transition region and protection region can correspond to the termination region of the power semiconductor chip. The termination region can be a field-limiting ring (FLR) structure, a junction termination extension (JTE) structure, a variation lateral doping (VLD) structure, and various derived composite termination structures, etc.

[0056] Taking the structure of the transition zone and the protected zone as an example of the FLR structure, such as Figure 2b As shown, in the main functional region, the power semiconductor chip includes power semiconductor devices disposed on a semiconductor substrate. For example, the power semiconductor devices may include diodes, transistors, thyristors, etc., disposed on the semiconductor substrate 10. The power semiconductor devices include a metal layer 21, which extends from the main functional region to the transition region. In addition, the power semiconductor chip includes a main junction 14, a field oxide layer 12, an electrode layer 11, and a passivation layer 13 sequentially stacked on the semiconductor substrate 10. The main junction 14 may be located in the main functional region, the transition region, and the protection region. The field oxide layer 12 is located in the transition region and the protection region. The electrode layer 11 is located in the protection region. The passivation layer is located in the transition region and the protection region, and may cover the portion of the metal layer 21 located in the transition region and the electrode layer 11 to block moisture and prevent moisture from entering the main functional region. The metal layer 21 and the electrode layer 11 disposed in the transition region and the protection region can play a role in modulating the electric field distribution, etc.

[0057] The pattern of the main junction 14 can be fabricated using the same semiconductor process as some of the film layers in the power semiconductor device. For example, the pattern of the main junction 14 can be fabricated using the same semiconductor process as the active layer in the power semiconductor device, and the pattern of the electrode layer 11 can be fabricated using the same semiconductor process as the metal layer 21 in the power semiconductor device. This simplifies the chip fabrication process.

[0058] Furthermore, in the transition region, field oxide 12 is disposed between the metal layer 21 and the adjacent electrode layer 11, with the metal layer 21 extending from the main functional region to the side of the field oxide 12 facing away from the semiconductor substrate 10. In the protection region, field oxide 12 is also disposed between adjacent electrode layers 11, each electrode layer 11 extending from the surface of the field oxide 12 facing away from the semiconductor substrate 10, passing through the exposed surface of the main junction 14 facing away from the semiconductor substrate 10, to the surface of the field oxide 12 adjacent to that field oxide 12 facing away from the semiconductor substrate 10. Adjacent electrode layers 11 are spaced apart along the direction from the main functional region to the protection region.

[0059] In the transition region, a passivation layer 13 is disposed between an adjacent metal layer 21 and an adjacent electrode layer 11, extending from the metal layer 21 away from the surface of the semiconductor substrate 10 to the surface of the electrode layer 11 adjacent to the metal layer 21 away from the surface of the semiconductor substrate 10. In the protection region, passivation layers 13 are also disposed between adjacent electrode layers 11, each passivation layer 13 extending from the electrode layer 11 away from the surface of the semiconductor substrate 10 to the surface of the electrode layer 11 adjacent to the electrode layer 11 away from the surface of the semiconductor substrate 10. Adjacent passivation layers 13 are spaced apart along the direction from the main functional region to the protection region.

[0060] For chips with JTE and VLD structures in the transition and protection regions, the power semiconductor chip in the terminal region also includes a main junction 14, a field oxide 12, and a passivation layer 13 sequentially stacked on the semiconductor substrate 10. In addition, the metal layer 21 can extend from the main functional region to the transition region. However, chips with JTE and VLD structures may not include the field plate 11.

[0061] For JTE structures, such as Figure 2c As shown, the protection zone may include multiple junction terminal extension regions, and multiple main junctions 14 are located in multiple junction terminal extension regions. Along the direction away from the main functional region, the doping concentration of the multiple main junctions 14 gradually decreases, and the doping depth gradually becomes shallower.

[0062] For VLD structures, such as Figure 2d As shown, the main junction 14 can extend from the main functional region to the protection zone, but along the direction away from the main functional region, the doping concentration of the main junction 14 gradually decreases, and the thickness of the main junction 14 also gradually decreases.

[0063] like Figure 3As shown, in the transition region, the metal layer 21 has a certain pattern, and the thickness of the portion of the metal layer 21 located in the transition region is, for example, the same as the thickness of the portion of the metal layer 21 located in the main functional region. However, in order to meet the design requirements for bonding or soldering of power semiconductor devices, the thickness of the metal layer 21 is usually relatively thick, with a thickness range of [0.1μm, 7μm]. When performing reliability tests such as TCT or TS on semiconductor devices, the stress on the large metal layer 21 is transmitted to the passivation layer 13. It is possible that the stress on the passivation layer 13 at the step ramp of the metal layer 21 is too large, causing the passivation layer 13 to crack. This allows moisture to enter the main functional region of the power semiconductor chip from the cracks in the passivation layer 13, and erode the power semiconductor device, affecting the reliability of the power semiconductor device.

[0064] Furthermore, it should be noted that the material of the passivation layer 13 is not limited in the embodiments of this application. Optionally, a material with good waterproof effect can be selected as the material of the passivation layer 13. For example, the material of the passivation layer 13 may include inorganic insulating material, which may be silicon nitride (SiN).

[0065] For the semiconductor substrate 10, the semiconductor substrate 10 may include a substrate. If the material of the substrate includes silicon (Si), then the semiconductor substrate 10 may only include the substrate. If the material of the semiconductor substrate 10 includes silicon carbide (SiC), then the semiconductor substrate 10 may also include an epitaxial layer disposed between the substrate and a structure such as field oxygen 12.

[0066] Based on the above problems, this application improves the structure of the field oxygen 12 to reduce the stress transmitted from the metal layer 21 to the passivation layer 13 and reduce the risk of cracking of the passivation layer 13.

[0067] The specific structure of the chip will be described in detail below with reference to the accompanying drawings.

[0068] like Figure 4a and Figure 4b As shown, for chips with JTE and VLD structures in the transition and protection regions, the chip includes field oxides 12, a metal layer 21, and a passivation layer 13 sequentially stacked on a semiconductor substrate 10. Field oxides 12 and passivation layer 13 are located in the transition and protection regions, respectively; metal layer 21 is located in the main functional region and the transition region. In the transition region, field oxides 12 include a main field oxide 121 and at least one auxiliary field oxide 122 spaced apart, with the auxiliary field oxide 122 located on the side of the main field oxide 121 facing the main functional region. Metal layer 21 extends from the main functional region to the side of the main field oxide 121 facing away from the semiconductor substrate 10. Passivation layer 13 extends from the side of metal layer 21 facing away from the semiconductor substrate 10 to the side of metal layer 21 facing away from the main functional region.

[0069] It should be noted here that, as Figure 4a and Figure 4bAs shown, the metal layer 21 extends from the main functional region to the side of the main field oxygen 121 facing away from the semiconductor substrate 10. That is, the metal layer 21 extending from the main functional region to the side of the main field oxygen 121 facing away from the semiconductor substrate 10 is a continuous structure. Since the auxiliary field oxygen 122 is located on the side of the main field oxygen 121 facing the main functional region, the continuous metal layer 21 not only covers the surface of the main field oxygen 121 facing away from the semiconductor substrate 10, but also covers all the surfaces of the auxiliary field oxygen 122 facing away from the semiconductor substrate 10.

[0070] In some possible implementations, this application may divide the existing field oxygen 12 into a main field oxygen 121 and at least one auxiliary field oxygen 122; or, this application may add at least one auxiliary field oxygen 122 to the existing field oxygen 12.

[0071] In the scheme of this application, in the transition region, the existing field oxygen 12 is divided into a main field oxygen 121 and at least one auxiliary field oxygen 122, or at least one auxiliary field oxygen 122 is added to the existing main field oxygen 121, and the main field oxygen 121 and at least one auxiliary field oxygen 122 are spaced apart. In this way, at least one auxiliary field oxygen 122 can play a buffering role, blocking the stress on the metal layer 21 extending from the main functional region to the side of the main field oxygen 121 away from the semiconductor substrate 10 from being transmitted to the passivation layer 13, thereby effectively reducing the stress between the large-sized metal layer 21 and the passivation layer 13, reducing the risk of cracking of the passivation layer 13, and preventing moisture from entering the main functional region of the chip through cracks in the passivation layer 13, affecting the function of each device in the main functional region.

[0072] In some possible ways of implementation, such as Figure 4b As shown, to prevent moisture from entering the main functional region through the field oxygen 121, the passivation layer 13 can also extend from the side of the metal layer 21 away from the main functional region to the side of the main field oxygen 121 away from the main functional region. In this case, as Figure 4b As shown, the metal layer 21 can cover a portion of the surface of the main field oxygen 121 on the side facing away from the semiconductor substrate 10; or, as... Figure 4c As shown, the metal layer 21 can also completely cover the surface of the main field oxygen 121 facing away from the semiconductor substrate 10.

[0073] Optional, such as Figure 4bAs shown, in the transition region, the metal layer 21 covers a portion of the surface of the main field oxygen 121 on the side facing away from the semiconductor substrate 10. In this way, along the direction from the semiconductor substrate 10 to the metal layer 21, the passivation layer 13 can first ascend from the side of the main field oxygen 121 facing away from the main functional region to the side of the main field oxygen 121 facing away from the semiconductor substrate 10; then ascend from the side of the metal layer 21 facing away from the main functional region to the side of the metal layer 21 facing away from the semiconductor substrate 10. This avoids the passivation layer 13 simultaneously ascending at the steps of the main field oxygen 121 and the metal layer 21, increasing the total height of the steps required for the passivation layer 13 to ascend, thereby reducing the risk of cracking of the passivation layer 13.

[0074] In some possible ways of implementation, such as Figure 4b and Figure 4c As shown, the number of auxiliary field oxygen 122 can be one; or, as... Figure 5 As shown, the number of auxiliary field oxygen 122 can also be multiple. The number of auxiliary field oxygen 122 is related to the size of the auxiliary field oxygen 122, the size of the main field oxygen 121, the spacing between the auxiliary field oxygen 122 and the main field oxygen 121, the spacing between adjacent auxiliary field oxygen 122, and the size of the chip. This application embodiment does not limit this.

[0075] It should be noted that when there are multiple auxiliary oxygen fields 122, they are spaced apart.

[0076] Optional, such as Figure 5 As shown, there can be three auxiliary oxygen fields 122. Along the direction from the main functional area to the protected area, the length of each auxiliary oxygen field 122 ranges from [0.2 μm to 100 μm], and the spacing between adjacent auxiliary oxygen fields 122 ranges from [0.2 μm to 100 μm].

[0077] For example, such as Figure 5 As shown, taking a distance L of 100 μm between the auxiliary oxygen field closest to the main functional area and the main oxygen field away from the main functional area, along the direction from the main functional area to the protected area, the length L1 of the main oxygen field 121 can be 50 μm, the length L2 of each auxiliary oxygen field 122 can be 10 μm, and the spacing between adjacent auxiliary oxygen fields 122, as well as the spacing between the main oxygen field 121 and the auxiliary oxygen field 122, can be 5 μm. In this case, the number of auxiliary oxygen fields 122 can be three.

[0078] In some possible implementations, regardless of whether there is one or more auxiliary field oxygen 122, the main field oxygen 121 and at least one auxiliary field oxygen 122 located in the transition region can be fabricated using the same semiconductor process.

[0079] For example, the primary field oxygen 121 and at least one secondary field oxygen 122 can be formed by the following steps: First, a thin film and a first photoresist are sequentially formed on a semiconductor substrate 10. The first photoresist is exposed and developed to obtain a first photoresist pattern. The first photoresist pattern covers the primary field oxygen 121 and at least one secondary field oxygen 122 to be formed, exposing areas in the thin film other than the primary field oxygen 121 and at least one secondary field oxygen 122. Then, under the protection of the first photoresist pattern, the thin film is etched to obtain the primary field oxygen 121 and at least one secondary field oxygen 122. The thin film can be, for example, a silicon dioxide (SiO2) thin film.

[0080] Of course, other processes can also be used to form the main field oxygen 121 and at least one auxiliary field oxygen 122. This application does not limit this process. As long as the structural relationship between the final main field oxygen 121 and at least one auxiliary field oxygen 122 is as described above, the processes for forming the main field oxygen 121 and at least one auxiliary field oxygen 122 are all within the protection scope of this application. Furthermore, the field oxygen 12 located in the protected area can also be prepared using the same semiconductor process as the field oxygen 12 located in the transition region.

[0081] The foregoing embodiments describe chips with JTE and VLD structures for the transition and protection regions. For chips with FLR structures for the transition and protection regions, the chip may further include an electrode layer 11. Figure 6 As shown, electrode layer 11 is located in the protection zone. In the protection zone, electrode layer 11 extends from the side of the main field oxygen 121 away from the semiconductor substrate 10 to the side of the main field oxygen 121 adjacent to the semiconductor substrate 10. Passivation layer 13, in addition to covering metal layer 21, also extends from the side of electrode layer 11 away from the semiconductor substrate 10 to the side of electrode layer 11 adjacent to the semiconductor substrate 10. In this way, not only can electrode layer 11 provide an equipotential effect, but passivation layer 13 can also cover electrode layer 11 to prevent moisture from entering the main functional area.

[0082] As mentioned earlier, the thickness of the portion of metal layer 21 located in the main functional area is the same as the thickness of the portion of metal layer 21 located in the transition area. However, in order to meet the design requirements of metal layer 21, the thickness of metal layer 21 is usually relatively thick, which results in a large step height required for passivation layer 13 to climb at metal layer 21. Under stress, passivation layer 13 is prone to cracking at the step.

[0083] Based on this, in some embodiments, such as Figure 7 As shown, the metal layer 21 may include a first portion 201 and a second portion 202. The first portion 201 is located at least in the main functional region, and the second portion 202 is located in the transition region. Along the direction from the metal layer 21 to the semiconductor substrate 10, the thickness of the first portion 201 is greater than the thickness of the second portion 202.

[0084] By reducing the thickness of the second part 202, this application can reduce the stress transmitted from the larger first part 201 to the second part 202, thereby reducing the stress between the metal layer 21 (or the second part) and the passivation layer 13, reducing the risk of cracking of the passivation layer 13, and preventing moisture from entering the main functional area of ​​the chip through the cracks in the passivation layer 13, thus affecting the function of each device in the main functional area.

[0085] In some possible implementations, the embodiments of this application do not limit the thickness range of the first part 201 and the second part 202, as long as the second part 202 can play an equipotential role and the first part 201 can meet the design requirements of the device located in the main functional area.

[0086] Optionally, the thickness of the second portion 202 can be in the range of [0.1μm, 4μm]. For example, the thickness of the second portion 202 can be 0.1μm, 0.6μm, 2μm, or 4μm. The thickness of the first portion 201 can be in the range of [0.1μm, 7μm]. For example, the thickness of the metal layer 21 can be 1μm, 2.5μm, 3.2μm, 4μm, 5μm, or 7μm.

[0087] In some possible ways of implementation, such as Figure 8 As shown, the first part 201, in addition to being located in the main functional region, can also extend from the main functional region to the transition region. In other words, besides the portion located in the main functional region, a portion of the first part 201 is also located in the transition region. This prevents misalignment during the fabrication of the device in the main functional region due to process limitations, which could prevent the first part 201 from forming a good contact relationship with other parts of the main functional region, thus affecting the performance of the device located in the main functional region. Furthermore, by placing the portion of the first part 201 located in the transition region on the side of the auxiliary field oxygen 122 facing the main functional region, in addition to utilizing at least one auxiliary field oxygen 122 to buffer stress, it also prevents the thicker metal layer 21 from still transmitting significant stress to the passivation layer 13 after passing through at least one auxiliary field oxygen 122.

[0088] In some possible implementations, the present application embodiments do not limit the preparation process of the first part 201 and the second part 202. For example, the first part 201 and the second part 202 of the metal layer 21 can be prepared in the following ways:

[0089] The first case, such as Figure 9aAs shown, a first metal layer 211 is formed on the side of the field oxide 12 away from the semiconductor substrate 10 using the same semiconductor process. The thickness of the first metal layer 211 is the same as the thickness of the second portion 202, and the first metal layer 211 is located in the main functional region and the transition region. Next, as... Figure 9b As shown, a second metal layer 212 is formed on the side of the first metal layer 211 away from the semiconductor substrate 10 using a photolithography process. The second metal layer 212 is located at least in the main functional region. In this case, the materials of the first metal layer 211 and the second metal layer 212 can be the same or different.

[0090] For the region where the first metal layer 211 and the second metal layer 212 are stacked, the first metal layer 211 and the second metal layer 212 can constitute a first portion 201 of the metal layer 21. The thickness range of the first metal layer 211 can be [0.1μm, 4μm], and the thickness range of the second metal layer 212 can be [0.1μm, 4μm], to ensure that the total thickness range of the first portion 201 is [0.1μm, 7μm].

[0091] The second scenario, such as Figure 10a As shown, using photolithography, the second part 202 is first formed in the transition region. Then, as... Figure 10b As shown, a first portion 201 is formed in the main functional region (or the main functional region and the transition region) using photolithography. In this case, the material of the first metal layer 211 and the material of the second metal layer 212 may be the same or different.

[0092] Of course, the first part 201 can be formed first in the main functional area (or the main functional area and the transition area), and the second part 202 can be formed in the transition area. This application embodiment does not limit this.

[0093] In the third scenario, a metal thin film and a second photoresist can be sequentially formed on the side of the field oxide 12 away from the semiconductor substrate 10. Then, the second photoresist is subjected to half-exposure, and after development, a second photoresist pattern is obtained. The second photoresist pattern includes a fully retained area, a half-retained area, and a fully exposed area. The fully retained area corresponds to the metal layer 21 to be formed, the half-retained area corresponds to the second portion 202 to be formed, and the fully exposed area corresponds to the other areas. Then, as... Figure 11 As shown, under the protection of the second photoresist pattern, the metal film is etched for the first time to obtain the metal pattern 213. Then, the second photoresist pattern is further exposed and developed to obtain the third photoresist pattern, which corresponds to the first portion 201 to be formed. Next, under the protection of the third photoresist pattern, the metal pattern 213 is etched to obtain... Figure 7 or Figure 8The metal layer 21 shown has a first portion 201 and a second portion 202. In this case, the material of the first metal layer 211 is the same as the material of the second metal layer 212.

[0094] Of course, other processes can also be used to form the first part 201 and the second part 202 of the metal layer 21. This application does not limit this. As long as the structural relationship between the first part 201 and the second part 202 is as described above, the processes for forming the first part 201 and the second part 202 of the metal layer 21 are all within the protection scope of this application.

[0095] Furthermore, for chips with an FLR structure for the transition region and protection region, the electrode layer 11 can be formed with the first part 201 or the second part 202 of the metal layer 21 through the same semiconductor process. That is, the electrode layer 11 can be formed at the same time as the first part 201 is formed; or the electrode layer 11 can be formed at the same time as the second part 202 is formed.

[0096] In some embodiments, such as Figure 12 As shown, the side of the metal layer 21 away from the main functional region can also be a slope; along the direction from the metal layer 21 to the semiconductor substrate 10, the distance between the slope and the main functional region gradually increases.

[0097] In this application, by setting the side of the metal layer 21 away from the main functional area as an inclined surface, the inclined surface can play a buffering role on the passivation layer 13 without changing the height of the step of the passivation layer 13. This improves the problem that the passivation layer 13 is prone to cracking at the step and prevents moisture from entering the active area of ​​the power semiconductor chip from the crack of the passivation layer 13 and corroding the power semiconductor device, thus affecting the reliability of the power semiconductor device.

[0098] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.

Claims

1. A chip, characterized in that, The system is divided into an active zone and a terminal zone. The active zone includes a main functional area, and the terminal zone includes a transition zone and a protection zone. The transition zone is located between the main functional area and the protection zone. The chip includes a field oxide layer, a metal layer, and a passivation layer sequentially stacked on a semiconductor substrate, wherein the field oxide layer and the passivation layer are located in the transition region and the protection region; and the metal layer is located in the main functional region and the transition region. In the transition region, the field oxygen includes a primary field oxygen and at least one secondary field oxygen spaced apart, the secondary field oxygen being located on the side of the primary field oxygen facing the primary functional region; the metal layer extends from the primary functional region to the side of the primary field oxygen away from the semiconductor substrate; The passivation layer extends from the side of the metal layer away from the semiconductor substrate to the side of the metal layer away from the main functional region.

2. The chip according to claim 1, characterized in that, In the transition region, the passivation layer also extends from the metal layer away from the main functional region to the main field oxygen away from the main functional region. The metal layer covers a portion of the surface of the semiconductor substrate on the side where the primary oxygen field is away from the semiconductor substrate. The passivation layer extends from the side of the metal layer away from the semiconductor substrate, through the side of the main field oxygen away from the semiconductor substrate, to the side of the main field oxygen away from the main functional region.

3. The chip according to claim 1, characterized in that, The number of auxiliary oxygen fields is multiple, and the multiple auxiliary oxygen fields are arranged at intervals.

4. The chip according to claim 3, characterized in that, The number of auxiliary oxygen fields is three; along the direction from the main functional area to the protected area, the length of each auxiliary oxygen field ranges from [0.2μm to 100μm], and the spacing between adjacent auxiliary oxygen fields ranges from [0.2μm to 100μm].

5. The chip according to any one of claims 1-4, characterized in that, The metal layer includes a first portion and a second portion, wherein the first portion is located at least in the main functional area and the second portion is located in the transition area; Along the direction from the metal layer to the semiconductor substrate, the thickness of the first portion is greater than the thickness of the second portion.

6. The chip according to claim 5, characterized in that, The first part extends from the main functional area to the transition area.

7. The chip according to claim 5, characterized in that, The metal layer includes a first metal layer and a second metal layer, wherein the first metal layer is located between the semiconductor substrate and the second metal layer; the thickness of the first metal layer is the same as the thickness of the second portion. The first metal layer is located in the main functional area and the transition area, and the second metal layer is located at least in the main functional area.

8. The chip according to claim 5, characterized in that, The thickness range of the first part is [1μm, 7μm], and the thickness range of the second part is [0.1μm, 4μm].

9. The chip according to claim 1, characterized in that, The chip also includes an electrode layer located in the protected area; In the protected area, the electrode layer extends from the side of the main field oxygen away from the semiconductor substrate to the side of the main field oxygen away from the semiconductor substrate adjacent to the main field oxygen; the passivation layer extends from the side of the electrode layer away from the semiconductor substrate to the side of the electrode layer away from the semiconductor substrate adjacent to the electrode layer.

10. The chip according to claim 9, characterized in that, In the case where the metal layer includes a first metal layer and a second metal layer, The electrode layer and the metal layer are made of the same material.

11. The chip according to any one of claims 1-4 and 6-10, characterized in that, The side of the metal layer facing away from the main functional area is a slope; Along the direction from the metal layer to the semiconductor substrate, the distance between the inclined surface and the main functional region gradually increases.

12. The chip according to any one of claims 1-4 and 6-10, characterized in that, The chip also includes a main junction that extends from the main functional region to the transition region and is in contact with at least one auxiliary field oxygen and the main field oxygen.

13. An electronic device, characterized in that, It includes a circuit board and a chip as described in any one of claims 1-12, wherein the chip is disposed on the circuit board.

Citation Information

Patent Citations

  • Switching device

    US20170263739A1

  • Semiconductor device and method of manufacturing semiconductor device

    US20200127082A1