Processing control method of semiconductor device and high energy particle beam lithography equipment
Directly engraving semiconductor devices through high-energy particle beam lithography equipment solves the problem of mask making in traditional technology, improves processing efficiency and accuracy, achieves cost saving and flexible modification, and improves the processing effect of semiconductor devices.
Patent Information
- Application Number
- CN202280017326.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-11
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2042-10-11
AI Technical Summary
In traditional semiconductor processing technology, the production and lithography of integrated circuit mask plates are difficult to meet the requirements of high precision and small size, resulting in high manufacturing costs and low processing efficiency. Especially when modifying the layout, the mask plate needs to be remade. Inefficient.
Using high-energy particle beam lithography equipment, by obtaining the integrated circuit layout, converting it into grayscale pictures and performing color reversal, the high-energy particle beam engraving target substrates according to the correspondence between the high-energy particle beam processing parameters and grayscale values, the high-energy particle beam engraving target substrates are controlled to realize semiconductors. Direct processing of the device avoids the production of multiple mask plates.
It improves the processing efficiency and accuracy of semiconductor devices, saves costs, and can flexibly modify the integrated circuit layout, reducing manufacturing costs. At the same time, the negative chip processing of grayscale pictures further improves the processing effect.
Smart Images

Figure CN117157731B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to the field of semiconductor processing technology, and in particular to a processing control method for a semiconductor device and a high-energy particle beam lithography device. Background Art
[0002] In the field of traditional semiconductor processing technology, it is often based on the combination of integrated circuit mask and photolithography technology to achieve the transfer of integrated circuit layout to silicon substrate, thereby completing the manufacture of semiconductor devices.
[0003] However, as the requirements for the size of semiconductor devices become higher and higher, the manufacture of light source systems that support lithography technology (such as EUV lithography machines) and the production of integrated circuit masks have become increasingly difficult. The use of integrated circuit masks will also make the manufacturing cost of semiconductor devices huge. Moreover, if the integrated circuit layout is modified or fine-tuned, the mask needs to be remade, resulting in low processing efficiency.
[0004] The high-energy particle beam in this application can be an ion beam, electron beam, laser beam, X-ray, etc., among which the high-energy focused ion beam is used in the experiment. High-energy particle beams have a smaller wavelength than ordinary optical systems, which can improve the resolution of layout transfer and are suitable for making smaller devices. For example, due to wavelength limitations, DUV lithography machines are only suitable for making devices with feature sizes greater than 7nm; for the production of devices below 7nm, EUV must be introduced. High-energy particle beams have a smaller wavelength than EUV. Summary of the invention
[0005] The embodiment of the present application provides a method for controlling the processing of a semiconductor device and a high-energy particle beam lithography device, which can complete the processing of the semiconductor device without making an integrated circuit mask, thereby improving the processing efficiency. The technical solution is as follows:
[0006] In a first aspect, an embodiment of the present application provides a method for controlling a process of a semiconductor device, comprising:
[0007] Acquire an integrated circuit layout corresponding to a target semiconductor device; wherein the integrated circuit layout includes a plurality of layers of integrated circuit sub-layouts, each layer of the integrated circuit sub-layout corresponds to a pattern of one or more material layers of the target semiconductor device;
[0008] Converting the integrated circuit sub-layouts of the plurality of layers into grayscale images of a preset format respectively;
[0009] Performing hue inversion on the grayscale image to obtain a grayscale negative film corresponding to the grayscale image;
[0010] According to the correspondence between the preset high-energy particle beam processing parameters and the grayscale value, the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film are obtained;
[0011] Each corresponding material layer is sequentially manufactured on the target substrate, and according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam and act on the corresponding material layer on the target substrate, and the pattern corresponding to the integrated circuit sub-layout is engraved on the corresponding material layer on the target substrate to obtain the target semiconductor device.
[0012] In a second aspect, an embodiment of the present application provides a high-energy particle beam lithography device, comprising: a processor, a memory, and a computer program stored in the memory and executable on the processor, wherein when the processor executes the computer program, the steps of the semiconductor device processing control method as described in the first aspect are implemented.
[0013] In an embodiment of the present application, an integrated circuit layout corresponding to a target semiconductor device is obtained; wherein the integrated circuit layout includes several layers of integrated circuit sub-layouts, each layer of the integrated circuit sub-layout corresponds to a pattern of one or more material layers of the target semiconductor device; the several layers of the integrated circuit sub-layouts are respectively converted into grayscale images of a preset format; the grayscale images are color-converted to obtain a grayscale negative film corresponding to the grayscale image; according to the correspondence between the preset high-energy particle beam processing parameters and the grayscale value, the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film are obtained; each corresponding material layer is sequentially made on the target substrate, and the corresponding grayscale values of each pixel point in the grayscale negative film are respectively obtained. The high-energy particle beam processing parameters corresponding to the target substrate are controlled to emit the high-energy particle beam and act on the corresponding material layer on the target substrate, and the pattern corresponding to the integrated circuit sub-layout is engraved on the corresponding material layer on the target substrate to obtain the target semiconductor device. This method does not need to make multiple mask plates, and the high-energy particle beam processing parameters can be automatically adjusted according to the grayscale value of each pixel point in the grayscale negative film corresponding to the integrated circuit sub-layout to complete the pattern engraving and obtain the semiconductor device. This method can not only greatly save costs, but also flexibly modify the integrated circuit layout and improve processing efficiency. In addition, the negative film conversion process of the grayscale image can further improve the processing effect of the target semiconductor device.
[0014] For better understanding and implementation, the technical solution of the present application is described in detail below with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 A schematic flow chart of a method for controlling a semiconductor device process provided by one embodiment of the present application;
[0016] Figure 2 A schematic diagram of the process of S105 in a method for controlling a semiconductor device processing according to an embodiment of the present application;
[0017] Figure 3 A schematic flow chart of a method for controlling a semiconductor device process according to another embodiment of the present application;
[0018] Figure 4 A schematic diagram of the flow of S208 in a method for controlling a semiconductor device processing according to another embodiment of the present application;
[0019] Figure 5 A schematic flow chart of a semiconductor device processing control method provided in other embodiments of the present application;
[0020] Figure 6 A schematic diagram of the process of S306 in the semiconductor device processing control method provided in other embodiments of the present application;
[0021] Figure 7 A schematic diagram of the process of S308 in the semiconductor device processing control method provided in other embodiments of the present application;
[0022] Figure 8 A schematic diagram of the structure of a high-energy particle beam lithography device provided in one embodiment of the present application. DETAILED DESCRIPTION
[0023] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, the same numbers in different drawings represent the same or similar elements unless otherwise indicated. The implementations described in the following exemplary embodiments do not represent all implementations consistent with the present application. Instead, they are merely examples of devices and methods consistent with some aspects of the present application as detailed in the appended claims.
[0024] The terms used in this application are for the purpose of describing specific embodiments only and are not intended to limit this application. The singular forms of "a", "said" and "the" used in this application and the appended claims are also intended to include plural forms unless the context clearly indicates other meanings. It should also be understood that the term "and / or" used herein refers to and includes any or all possible combinations of one or more associated listed items.
[0025] It should be understood that, although the terms first, second, third, etc. may be used in the present application to describe various information, these information should not be limited to these terms. These terms are only used to distinguish the same type of information from each other. For example, without departing from the scope of the present application, the first information may also be referred to as the second information, and similarly, the second information may also be referred to as the first information. Depending on the context, the words "if" / "if" as used herein may be interpreted as "at the time of" or "when" or "in response to determination".
[0026] See also Figure 1 , is a flow chart of a method for controlling a semiconductor device according to an embodiment of the present application, the method comprising the following steps:
[0027] S101: Obtain an integrated circuit layout corresponding to a target semiconductor device; wherein the integrated circuit layout includes several layers of integrated circuit sub-layouts, and each layer of the integrated circuit sub-layout corresponds to a pattern of one or more material layers of the target semiconductor device.
[0028] In an optional embodiment, the executor of the semiconductor device processing control method may be a high-energy particle beam lithography device, or a component in the high-energy particle beam lithography device, such as a processor or microprocessor inside the device; in another optional embodiment, the executor of the semiconductor device processing control method may be an external device that establishes a data connection with the high-energy particle beam lithography device, or a component in the external device.
[0029] In an embodiment of the present application, the execution body of the semiconductor device processing control method is a high-energy particle beam lithography device.
[0030] Specifically, the high-energy particle beam lithography equipment obtains the integrated circuit layout corresponding to the target semiconductor device.
[0031] The target semiconductor device may be any type of semiconductor device, and its specific type is not limited herein.
[0032] The integrated circuit layout refers to mapping the circuit design circuit diagram or circuit description language to the physical description level. The integrated circuit layout includes relevant physical information such as the device type, device size, relative position between devices, and connection relationship between each device of the integrated circuit.
[0033] The integrated circuit layout includes several layers of integrated circuit sub-layouts, and each layer of the integrated circuit sub-layout corresponds to the pattern of a material layer of the target semiconductor device.
[0034] In the embodiment of the present application, the material layer includes but is not limited to an active layer, an insulating layer, a polysilicon gate layer, a metal layer, and the like.
[0035] S102: Converting the integrated circuit sub-layouts of the plurality of layers into grayscale images of a preset format respectively.
[0036] The high-energy particle beam lithography equipment converts the integrated circuit sub-layouts of the plurality of layers into grayscale images of a preset format. In an optional embodiment, the preset format is a TIF format, and in other optional embodiments, the preset format may be other image formats that can be recognized and processed by the high-energy particle beam.
[0037] The grayscale value of the pixel in the grayscale image is 0 to 255, where a grayscale value of 0 indicates that the pixel has a lower brightness, and the human body subjectively perceives it as black, and a grayscale value of 255 indicates that the pixel has a higher brightness, and the human body subjectively perceives it as white.
[0038] S103: Perform hue inversion on the grayscale image to obtain a grayscale negative film corresponding to the grayscale image.
[0039] A negative film is an image obtained after exposure and development. The brightness and darkness of a grayscale negative film are opposite to those of the original grayscale image. Converting a grayscale image into a grayscale negative film can highlight the white details or gray details in the dark area of the image, thereby improving the processing effect of semiconductor devices when subsequent semiconductor device processing is performed based on the grayscale negative film.
[0040] There are many ways to invert the color phase of an image and obtain a negative film, which are not specifically limited here.
[0041] S104: According to the preset correspondence between the high-energy particle beam processing parameter and the gray value, the high-energy particle beam processing parameter corresponding to each pixel point in the gray negative film is obtained.
[0042] In an optional embodiment, the correspondence between the preset high-energy particle beam processing parameters and the grayscale values can be preset and stored in the high-energy particle beam lithography equipment. In another optional embodiment, the correspondence between the preset high-energy particle beam processing parameters and the grayscale values can be preset and stored in the cloud or host computer, and then downloaded to the high-energy particle beam lithography equipment when used.
[0043] Depending on the type of semiconductor device or the material difference of the material layer, the corresponding relationship between the high-energy particle beam processing parameters and the grayscale value is also different. In the high-energy particle beam lithography equipment, cloud or host computer, the corresponding relationship between the high-energy particle beam processing parameters and the grayscale value can be found according to the identification of the semiconductor device, or the corresponding relationship between the high-energy particle beam processing parameters and the grayscale value can be found according to the material identification of the material layer.
[0044] In an optional embodiment, a third-party semiconductor device design manufacturer can upload the designed semiconductor device identification or material identification to the cloud, and configure the corresponding relationship between the high-energy particle beam processing parameters and the grayscale value, so that the high-energy particle beam lithography equipment can control the high-energy particle beam lithography equipment to complete the processing of more types of semiconductor devices and meet more third-party customer needs.
[0045] In the embodiment of the present application, the high-energy particle beam processing parameters include the high-energy particle beam acceleration voltage and / or the high-energy particle beam action time. In order to process the semiconductor device more accurately, the high-energy particle beam lithography equipment obtains the high-energy particle beam processing parameters corresponding to each pixel in the grayscale negative film according to the correspondence between the preset high-energy particle beam processing parameters and the grayscale value, which are as follows:
[0046] The high-energy particle beam lithography equipment obtains the high-energy particle beam acceleration voltage corresponding to each pixel point in the grayscale negative film according to the grayscale value of the pixel point in the grayscale negative film. When the grayscale value of the pixel point in the grayscale negative film is smaller, the high-energy particle beam acceleration voltage of the high-energy particle beam lithography equipment is lower. When the grayscale value of the pixel point in the grayscale negative film is larger, the high-energy particle beam acceleration voltage of the high-energy particle beam lithography equipment is higher. The higher the high-energy particle beam acceleration voltage, the higher the kinetic energy of the emitted high-energy particle beam, so that in the same time, more materials can be engraved to obtain deeper material grooves.
[0047] Alternatively, the high-energy particle beam lithography device obtains the high-energy particle beam action time corresponding to each pixel point in the grayscale negative film according to the grayscale value of the pixel point in the grayscale negative film. When the grayscale value of the pixel point in the grayscale negative film is smaller, the high-energy particle beam action time of the high-energy particle beam lithography device is shorter. When the grayscale value of the pixel point in the grayscale negative film is larger, the high-energy particle beam action time of the high-energy particle beam lithography device is longer. The longer the high-energy particle beam action time, the more material can be engraved and deeper material grooves can be obtained when other control conditions remain unchanged.
[0048] Alternatively, the high-energy particle beam lithography device obtains the grayscale mean value of all pixels in the grayscale negative film. When the grayscale mean value is smaller, the high-energy particle beam acceleration voltage of the high-energy particle beam lithography device is lowered, and according to the grayscale value of the pixel in the grayscale negative film, the high-energy particle beam action time corresponding to each pixel in the grayscale negative film is obtained when the high-energy particle beam acceleration voltage remains unchanged. When the grayscale value of the pixel in the grayscale negative film is smaller, the high-energy particle beam action time of the high-energy particle beam lithography device is shorter, and when the grayscale value of the pixel in the grayscale negative film is larger, the high-energy particle beam action time of the high-energy particle beam lithography device is longer. By coordinating the high-energy particle beam acceleration voltage and the high-energy particle beam action time, the manufacturing process of semiconductor devices can be further accelerated and the manufacturing efficiency can be improved.
[0049] S105: each corresponding material layer is manufactured on the target substrate in sequence, and according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam and act on the corresponding material layer on the target substrate, and the pattern corresponding to the integrated circuit sub-layout is engraved on the corresponding material layer on the target substrate to obtain the target semiconductor device.
[0050] In an optional embodiment, the material layer is a pre-processed material layer, and each corresponding material layer is placed on the target substrate in sequence by controlling a mechanical device.
[0051] In another optional embodiment, the material layer is a material layer deposited by controlling a high energy particle beam lithography device. For details, see Figure 2 The step of sequentially manufacturing each corresponding material layer on the target substrate includes steps S1051 to S1052, as follows:
[0052] S1051: Acquire the material gas corresponding to the material layer and the deposition area corresponding to the material layer on the target substrate.
[0053] The material gas may be one gas or multiple gases, which may be different according to the differences of the material layers.
[0054] In some embodiments, in order to enable the high-energy particle beam to engrave better graphics effects on the material layer, each material layer includes multiple materials. For example, a layer of silicon oxide is first plated on the surface of single crystal silicon, and then a layer of tantalum is plated on the surface of the silicon oxide. Accordingly, multiple material gases are also required when preparing such material layers.
[0055] S1052: Control the high-energy particle beam lithography equipment to spray the material gas in the deposition area, so that the material gas is decomposed and deposited in the deposition area, thereby completing the production of the material layer.
[0056] Since high-energy particle beams can decompose metal vapor or gas-phase insulating materials, etc., the material gas is sprayed in the deposition area through the gas injection device in the high-energy particle beam lithography equipment, and the high-energy particle beam is emitted to decompose the material gas at the same time, so that the decomposed material gas is deposited in the deposition area to complete the production of the material layer.
[0057] The above method can complete the laying of material layers and the engraving of graphics by controlling a high-energy particle beam lithography device, thereby realizing the processing of semiconductor devices, which can not only reduce costs but also have a higher degree of automation.
[0058] In an optional embodiment, after each layer of the material is produced on the target substrate, the high-energy particle beam lithography equipment can also control the high-energy particle beam to polish the material layer according to a preset optimized thickness range and / or a preset optimized flatness range, so that the current thickness and / or current flatness of the material layer are respectively within the preset optimized thickness range and the preset optimized flatness range, thereby further improving the subsequent engraving effect and optimizing the processing of semiconductor devices.
[0059] Optionally, the preset optimized thickness range is 1 nm to 500 nm, and the preset optimized flatness range is 0.5 nm to 5 nm.
[0060] In another optional embodiment, due to the different properties and uses of different devices, different requirements for engraving processing accuracy are required. Before controlling the high-energy particle beam lithography equipment to emit a high-energy particle beam and act on the corresponding material layer on the target substrate, the high-energy particle beam lithography equipment can control the electromagnetic lens to perform the high-energy particle beam miniaturization according to a preset engraving size threshold, so that the pixel size of the high-energy particle beam engraving is smaller than the engraving size threshold.
[0061] In an embodiment of the present application, an integrated circuit layout corresponding to a target semiconductor device is obtained; wherein the integrated circuit layout includes several layers of integrated circuit sub-layouts, each layer of the integrated circuit sub-layout corresponds to a pattern of one or more material layers of the target semiconductor device; the several layers of the integrated circuit sub-layouts are respectively converted into grayscale images of a preset format; the grayscale images are color-converted to obtain a grayscale negative film corresponding to the grayscale image; according to the correspondence between the preset high-energy particle beam processing parameters and the grayscale value, the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film are obtained; each corresponding material layer is sequentially made on the target substrate, and the corresponding grayscale values of each pixel point in the grayscale negative film are respectively obtained. The high-energy particle beam processing parameters corresponding to the target substrate are controlled to emit the high-energy particle beam and act on the corresponding material layer on the target substrate, and the pattern corresponding to the integrated circuit sub-layout is engraved on the corresponding material layer on the target substrate to obtain the target semiconductor device. This method does not need to make multiple mask plates, and the high-energy particle beam processing parameters can be automatically adjusted according to the grayscale value of each pixel point in the grayscale negative film corresponding to the integrated circuit sub-layout to complete the pattern engraving and obtain the semiconductor device. This method can not only greatly save costs, but also flexibly modify the integrated circuit layout and improve processing efficiency. In addition, the negative film conversion process of the grayscale image can further improve the processing effect of the target semiconductor device.
[0062] To improve semiconductor device processing efficiency, please refer to Figure 3 , which is a flow chart of a semiconductor device processing control method provided by another embodiment of the present application, including steps S201 to S208, wherein steps S201 to S203 and S207 are respectively the same as steps S101 to S103 and S104, and are specifically as follows:
[0063] S201: Acquire an integrated circuit layout corresponding to a target semiconductor device; wherein the integrated circuit layout includes several layers of integrated circuit sub-layouts, and each layer of the integrated circuit sub-layout corresponds to a pattern of one or more material layers of the target semiconductor device.
[0064] S202: Converting the integrated circuit sub-layouts of the plurality of layers into grayscale images of a preset format respectively.
[0065] S203: Perform hue inversion on the grayscale image to obtain a grayscale negative film corresponding to the grayscale image.
[0066] S204: Obtain target pixel points in the grayscale negative film corresponding to each layer of the integrated circuit sub-layout and the coordinates of the target pixel points in the grayscale negative film; wherein the target pixel points are pixel points whose grayscale values are higher than a preset threshold.
[0067] In the grayscale negative film corresponding to the integrated circuit sub-layout, there may be some target pixels whose grayscale values are higher than a preset threshold, indicating that the coordinates of the target pixels in the corresponding material layer need to be penetrated by the high-energy particle beam.
[0068] The preset threshold is related to the corresponding relationship between the preset high-energy particle beam processing parameters and the grayscale value, and can be set according to actual conditions, and is not limited here.
[0069] S205: When there are target pixel points with the same coordinates in the grayscale negative films corresponding to the integrated circuit sub-layouts of the i-j layers, the pixel points to be adjusted in the grayscale negative films corresponding to the integrated circuit sub-layouts of the i-j layers are obtained.
[0070] If there are target pixels with the same coordinates in the grayscale negative films corresponding to the integrated circuit sub-layouts described in layers i to j, then these target pixels are the pixels to be adjusted. By adjusting the grayscale values of the pixels to be adjusted, engraving is not performed at the coordinates of the pixels to be adjusted when engraving the corresponding material layer.
[0071] The integrated circuit sub-layout has a total of n layers, 1≤i <j≤n。
[0072] S206: reset the grayscale values of the pixels to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layouts of the i-th to j-th layers according to a preset adjustment strategy.
[0073] In an optional embodiment, the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the i-j layers is set to the lowest value, i.e., 0, so that when engraving the pattern corresponding to the integrated circuit sub-layout of the i-j layers, the pattern composed of the pixel to be adjusted will not be engraved.
[0074] In another optional embodiment, the high-energy particle beam lithography equipment first obtains a first grayscale value corresponding to the lowest high-energy particle beam processing parameter.
[0075] The high-energy particle beam processing parameters include the high-energy particle beam acceleration voltage and / or the high-energy particle beam action time. In the embodiment of the present application, the grayscale value corresponding to the high-energy particle beam acceleration voltage being 0 or the high-energy particle beam action time being 0 is the first grayscale value.
[0076] Due to the different corresponding relationships between the high-energy particle beam processing parameters and the grayscale values, the first grayscale value will also be different and is not necessarily 0, and its specific value is not limited here.
[0077] Afterwards, the high-energy particle beam lithography equipment sets the grayscale values at the same pattern in the grayscale negative film corresponding to the integrated circuit sub-layout of the i-th to j-th layers to the first grayscale value, so that when engraving the pattern corresponding to the integrated circuit sub-layout of the i-th to j-th layers, the pattern composed of the pixel points to be adjusted will not be engraved.
[0078] S207: According to the preset correspondence between the high-energy particle beam processing parameter and the gray value, the high-energy particle beam processing parameter corresponding to each pixel point in the gray negative film is obtained.
[0079] S208: Making each corresponding material layer on the target substrate in sequence, and controlling the high-energy particle beam lithography equipment to emit a high-energy particle beam and act on the corresponding material layer on the target substrate according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film, and engraving the pattern corresponding to the integrated circuit sub-layout to the corresponding material layer on the target substrate to obtain the target semiconductor device.
[0080] Step S208 is performed in the same manner as step S105, that is, each time a material layer is provided, a pattern corresponding to the integrated circuit sub-layout is engraved on the material layer, and finally a target semiconductor device is obtained.
[0081] However, in this embodiment, when engraving the i-th to j-th material layers, no pattern composed of pixels to be adjusted is engraved, so this step is different from step S105. Figure 4 , step S208 includes steps S2081 to S2082, and the specific distinction process is as follows:
[0082] S2081: sequentially fabricating i-j material layers on the target substrate, and controlling the high-energy particle beam lithography equipment to emit a high-energy particle beam to act on the i-j material layers according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film corresponding to the i-j integrated circuit sub-layout, respectively, to engrave all patterns corresponding to the i-j integrated circuit sub-layout except the pattern composed of the pixel points to be adjusted onto the corresponding i-j material layers.
[0083] After laying down each material layer (the i-th to j-th layers) by the high-energy particle beam lithography equipment, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam to act on the material layer according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film corresponding to the integrated circuit sub-layout of the layer, so as to engrave all patterns corresponding to the integrated circuit sub-layout of the layer except the pattern composed of the pixel points to be adjusted onto the material layer.
[0084] The engraving of the layers other than the i-th to j-th material layers is the same as the engraving in step S105 and will not be described in detail.
[0085] S2082: According to the coordinates of the pixel point to be adjusted, control the high-energy particle beam lithography equipment to emit a high-energy particle beam to act on the coordinates of the pixel point to be adjusted in the j-th material layer, and penetrate the i-j-th material layer at the coordinates of the pixel point to be adjusted.
[0086] After the high-energy particle beam lithography equipment has engraved all patterns corresponding to the j-th layer of the integrated circuit sub-layout except the pattern composed of the pixel points to be adjusted to the j-th layer of the material layer, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam to act on the coordinates of the pixel points to be adjusted in the j-th layer of the material layer according to the coordinates of the pixel points to be adjusted, and penetrate the i-j layers of the material layer at the coordinates of the pixel points to be adjusted.
[0087] Among them, the high-energy particle beam processing parameters that penetrate each material layer can be obtained according to experiments and pre-stored in the high-energy particle beam lithography equipment. The corresponding high-energy particle beam processing parameters can be found according to the identification of the material layer, thereby obtaining the high-energy particle beam processing parameters that penetrate the i-th to j-th layers.
[0088] In this embodiment, by obtaining the target pixel points in the grayscale negative film corresponding to each layer of the integrated circuit sub-layout and the coordinates of the target pixel points, the target pixel points with the same coordinates that exist in the grayscale negative films corresponding to the integrated circuit sub-layouts from the i to j layers, that is, the pixel points to be adjusted, are obtained, and then the grayscale values of the pixel points to be adjusted are reset through the adjustment strategy, so that when the patterns corresponding to the integrated circuit sub-layouts from the i to j layers are engraved to the i to j material layers respectively, the patterns composed of the pixel points to be adjusted will not be engraved. Finally, after engraving the j material layer, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam to act on the coordinates of the pixel points to be adjusted in the j material layer according to the coordinates of the pixel points to be adjusted, and penetrate the i to j material layers at the coordinates of the pixel points to be adjusted, so as to realize combined engraving, thereby effectively improving the processing efficiency of semiconductor devices.
[0089] To further improve the processing efficiency of semiconductor devices, please refer to Figure 5 , which is a flow chart of a semiconductor device processing control method provided in other embodiments of the present application, including steps S301 to S308, wherein steps S301 to S304 and S307 are respectively the same as steps S201 to S204 and S207, and are specifically as follows:
[0090] S301: Obtain an integrated circuit layout corresponding to a target semiconductor device; wherein the integrated circuit layout includes several layers of integrated circuit sub-layouts, and each layer of the integrated circuit sub-layout corresponds to a pattern of one or more material layers of the target semiconductor device.
[0091] S302: Converting the integrated circuit sub-layouts of the plurality of layers into grayscale images of a preset format respectively.
[0092] S303: Perform hue inversion on the grayscale image to obtain a grayscale negative film corresponding to the grayscale image.
[0093] S304: Obtain target pixel points in the grayscale negative film corresponding to each layer of the integrated circuit sub-layout and the coordinates of the target pixel points in the grayscale negative film; wherein the target pixel points are pixel points whose grayscale values are higher than a preset threshold.
[0094] S305: When there are target pixel points with the same coordinates in the grayscale negative films corresponding to the integrated circuit sub-layouts of the i-j layers, the pixel points to be adjusted in the grayscale negative films corresponding to the integrated circuit sub-layouts of the i-j layers are obtained.
[0095] S306: reset the grayscale values of the pixels to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layouts of the i-th to j-th layers according to a preset adjustment strategy.
[0096] The adjustment strategy preset in step S306 is different from the adjustment strategy preset in step S206. Specifically:
[0097] In step S306, when the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the i-th to j-1th layers is set, it is the same as step S206, except that the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the jth layer is set separately. Figure 6 , step S306 includes steps S3061 to S3064:
[0098] S3061: Set the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the i to j-1 layers to the lowest value, or obtain the first grayscale value corresponding to the lowest high-energy particle beam processing parameter, and set the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the i to j-1 layers to the first grayscale value.
[0099] S3062: Obtain target high-energy particle beam processing parameters that penetrate the i-th to j-th material layers.
[0100] The high-energy particle beam processing parameters penetrating each material layer can be obtained according to experiments and pre-stored in the high-energy particle beam lithography equipment. The corresponding high-energy particle beam processing parameters can be found according to the identification of the material layer, thereby obtaining the high-energy particle beam processing parameters penetrating the i-j layers.
[0101] S3063: Obtain a second grayscale value according to the corresponding relationship between the target high-energy particle beam processing parameter and the preset high-energy particle beam processing parameter and the grayscale value.
[0102] The high-energy particle beam lithography equipment obtains the second grayscale value according to the corresponding relationship between the preset high-energy particle beam processing parameters and the grayscale value and the target high-energy particle beam processing parameters.
[0103] S3064: Setting the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the j-th layer to the second grayscale value.
[0104] The high-energy particle beam lithography equipment sets the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the jth layer to the second grayscale value. This makes it possible for the high-energy particle beam equipment to, when engraving the jth material layer, determine that the grayscale value of a certain pixel is the second grayscale value, and then, based on the target high-energy particle beam processing parameters corresponding to the second grayscale value, control the high-energy particle beam to act on the coordinates of the pixel in the jth material layer, thereby allowing the high-energy particle beam to penetrate the i to jth material layers at the coordinates of the pixel.
[0105] By separately setting the grayscale value of the pixel points to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the jth layer, when engraving the pattern corresponding to the integrated circuit sub-layout of the jth layer, the pattern composed of the pixel points to be adjusted can be engraved to the i-j material layers at the same time, thereby reducing the engraving steps and further improving the processing efficiency.
[0106] S307: According to the preset correspondence between the high-energy particle beam processing parameter and the gray value, the high-energy particle beam processing parameter corresponding to each pixel point in the gray negative film is obtained.
[0107] S308: Each corresponding material layer is manufactured on the target substrate in sequence, and according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam and act on the corresponding material layer on the target substrate, and the pattern corresponding to the integrated circuit sub-layout is engraved on the corresponding material layer on the target substrate to obtain the target semiconductor device.
[0108] In the embodiments of this application, please refer to Figure 7 Step S308 includes steps S3081 to S3082, which are specifically as follows:
[0109] S3081: fabricate i to j-1th material layers on the target substrate in sequence, and control the high-energy particle beam lithography equipment to emit a high-energy particle beam to act on the i to j-1th material layers according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film corresponding to the i to j-1th integrated circuit sub-layout, and engrave all patterns corresponding to the i to j-1th integrated circuit sub-layout except the pattern composed of the pixel points to be adjusted to the corresponding i to j-1th material layers.
[0110] After laying down each material layer (the i-th to j-1-th layers) by the high-energy particle beam lithography equipment, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam to act on the material layer according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film corresponding to the integrated circuit sub-layout of the layer, so as to engrave all patterns corresponding to the integrated circuit sub-layout of the layer except the pattern composed of the pixel points to be adjusted onto the material layer.
[0111] S3082: Arrange the jth material layer on the target substrate, control the high-energy particle beam lithography equipment to emit a high-energy particle beam to act on the jth material layer, engrave the pattern corresponding to the jth integrated circuit sub-layout to the jth material layer, and penetrate the j to i material layers at the coordinates of the pixel point to be adjusted.
[0112] Since the grayscale value of the pixel to be adjusted is set to the second grayscale value in the grayscale negative film corresponding to the j-th layer of the integrated circuit sub-layout, when the high-energy particle beam lithography equipment is engraving the coordinates of the pixel to be adjusted in the j-th layer of the material layer, it will emit a high-energy particle beam to act on the coordinates of the pixel to be adjusted according to the target high-energy particle beam processing parameters corresponding to the second grayscale value, so that the high-energy particle beam penetrates the j to i layers of the material layer at the coordinates.
[0113] The engraving of the layers other than the i-th to j-th material layers is the same as the engraving in step S105 (or S208), and will not be described in detail.
[0114] In this embodiment, by obtaining the target pixel points and the coordinates of the target pixel points in the grayscale negative film corresponding to each layer of the integrated circuit sub-layout, the target pixel points with the same coordinates that exist in the grayscale negative films corresponding to the integrated circuit sub-layouts of the i to j layers, that is, the pixel points to be adjusted, are obtained, and then the grayscale values of the pixel points to be adjusted in the i to j-1 layers and the grayscale values of the pixel points to be adjusted in the j layer are reset respectively through the adjustment strategy, so that when the patterns corresponding to the integrated circuit sub-layouts of the i to j-1 layers are engraved to the i to j-1 layers of the material layer respectively, the patterns composed of the pixel points to be adjusted will not be engraved. Finally, when the j layer of the material layer is engraved, according to the coordinates and grayscale values of the pixel points to be adjusted, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam to act on the coordinates of the pixel points to be adjusted, and penetrate the i to j layers of the material layer at the coordinates of the pixel points to be adjusted, so as to realize the combined engraving of the pattern corresponding to the j layer of the integrated circuit sub-layout and the pattern composed of the pixel points to be adjusted in the i to j-1 layers, thereby further improving the processing efficiency of the semiconductor device.
[0115] See also Figure 8 , which is a schematic diagram of the structure of a high-energy particle beam lithography device provided by an embodiment of the present application. Figure 8 As shown, the high-energy particle beam lithography device 8 may include: a processor 80, a memory 81, and a computer program 82 stored in the memory 81 and executable on the processor 80, such as a semiconductor device processing control program; when the processor 80 executes the computer program 82, the steps in the above-mentioned method embodiments are implemented, such as Figure 1 Steps S101 to S105 are shown.
[0116] Wherein, the processor 80 may include one or more processing cores. The processor 80 uses various interfaces and lines to connect the various parts in the high-energy particle beam lithography device 8, and executes various functions and processes data of the high-energy particle beam lithography device 8 by running or executing instructions, programs, code sets or instruction sets stored in the memory 81, and calling the data in the memory 81. Optionally, the processor 80 can be implemented in at least one hardware form of digital signal processing (Digital Signal Processing, DSP), field programmable gate array (Field-Programmable Gate Array, FPGA), and programmable logic array (Programble Logic Array, PLA). The processor 80 can integrate one or more combinations of a central processing unit (Central Processing Unit, CPU), a graphics processing unit (Graphics Processing Unit, GPU) and a modem. Among them, the CPU mainly processes the operating system, user interface and application programs; the GPU is responsible for rendering and drawing the content to be displayed on the touch display; the modem is used to process wireless communications. It can be understood that the above-mentioned modem may not be integrated into the processor 80, and it can be implemented by a single chip.
[0117] Among them, the memory 81 may include a random access memory (RAM) or a read-only memory (Read-Only Memory). Optionally, the memory 81 includes a non-transitory computer-readable storage medium. The memory 81 can be used to store instructions, programs, codes, code sets or instruction sets. The memory 81 may include a program storage area and a data storage area, wherein the program storage area may store instructions for implementing an operating system, instructions for at least one function (such as touch instructions, etc.), instructions for implementing the above-mentioned various method embodiments, etc.; the data storage area may store data involved in the above-mentioned various method embodiments, etc. The memory 81 may also be optionally at least one storage device located away from the aforementioned processor 80.
[0118] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described or recorded in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.
[0119] Those skilled in the art will appreciate that the units and algorithm steps of each example described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are performed in hardware or software depends on the specific application and design constraints of the technical solution. Professional and technical personnel can use different methods to implement the described functions for each specific application, but such implementation should not be considered to be beyond the scope of the present invention.
[0120] The present invention is not limited to the above-mentioned embodiments. If various changes or modifications to the present invention do not depart from the spirit and scope of the present invention, and if these changes and modifications fall within the scope of the claims and equivalent technologies of the present invention, the present invention is also intended to include these changes and modifications.
Claims
1. A method for controlling the processing of a semiconductor device, characterized in that: Includes steps: Acquire an integrated circuit layout corresponding to a target semiconductor device; wherein the integrated circuit layout includes a plurality of layers of integrated circuit sub-layouts, each layer of the integrated circuit sub-layout corresponds to a pattern of one or more material layers of the target semiconductor device; Converting the integrated circuit sub-layouts of the plurality of layers into grayscale images of a preset format respectively; Performing hue inversion on the grayscale image to obtain a grayscale negative film corresponding to the grayscale image; According to the correspondence between the preset high-energy particle beam processing parameters and the grayscale value, the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film are obtained; Each corresponding material layer is sequentially manufactured on the target substrate, and according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam and act on the corresponding material layer on the target substrate, and the pattern corresponding to the integrated circuit sub-layout is engraved on the corresponding material layer on the target substrate to obtain the target semiconductor device.
2. The method for controlling the processing of a semiconductor device according to claim 1, wherein: The high-energy particle beam processing parameters include the high-energy particle beam acceleration voltage and / or the high-energy particle beam action time. According to the correspondence between the preset high-energy particle beam processing parameters and the grayscale values, the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film are obtained, including the steps of: According to the grayscale value of the pixel point in the grayscale negative film, the high-energy particle beam acceleration voltage corresponding to each pixel point in the grayscale negative film is obtained, when the grayscale value of the pixel point in the grayscale negative film is smaller, the high-energy particle beam acceleration voltage of the high-energy particle beam lithography device is lower, and when the grayscale value of the pixel point in the grayscale negative film is larger, the high-energy particle beam acceleration voltage of the high-energy particle beam lithography device is higher; or, According to the grayscale value of the pixel point in the grayscale negative film, the high-energy particle beam action time corresponding to each pixel point in the grayscale negative film is obtained, when the grayscale value of the pixel point in the grayscale negative film is smaller, the high-energy particle beam action time of the high-energy particle beam lithography device is shorter, and when the grayscale value of the pixel point in the grayscale negative film is larger, the high-energy particle beam action time of the high-energy particle beam lithography device is longer; or, The grayscale mean of all the pixels in the grayscale negative film is obtained. When the grayscale mean is smaller, the high-energy particle beam acceleration voltage of the high-energy particle beam lithography device is lowered. According to the grayscale value of the pixel in the grayscale negative film, the high-energy particle beam action time corresponding to each pixel in the grayscale negative film is obtained when the high-energy particle beam acceleration voltage remains unchanged. When the grayscale value of the pixel in the grayscale negative film is smaller, the high-energy particle beam action time of the high-energy particle beam lithography device is shorter. When the grayscale value of the pixel in the grayscale negative film is larger, the high-energy particle beam action time of the high-energy particle beam lithography device is longer.
3. The method for controlling the processing of a semiconductor device according to claim 1, wherein: After the grayscale image is hue-converted to obtain a grayscale negative film corresponding to the grayscale image, the method includes the following steps: Obtaining target pixel points in the grayscale negative film corresponding to each layer of the integrated circuit sub-layout and the coordinates of the target pixel points in the grayscale negative film; wherein the target pixel points are pixel points whose grayscale values are higher than a preset threshold; When there are target pixel points with the same coordinates in the grayscale negative films corresponding to the integrated circuit sub-layouts of the i-th to j-th layers, the pixel points to be adjusted in the grayscale negative films corresponding to the integrated circuit sub-layouts of the i-th to j-th layers are obtained; The grayscale values of the pixels to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layouts of the i-th to j-th layers are reset according to a preset adjustment strategy.
4. The method for controlling the processing of a semiconductor device according to claim 3, wherein: The method of resetting the grayscale values of the pixels to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layouts of the i-th to j-th layers according to a preset adjustment strategy comprises the following steps: Setting the grayscale value of the pixel to be adjusted in the grayscale negative corresponding to the integrated circuit sub-layout of the i-th to j-th layers to the lowest value; or, Obtaining a first grayscale value corresponding to the lowest high-energy particle beam processing parameter; The grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the i-th to j-th layers is set as the first grayscale value.
5. The method for controlling the processing of a semiconductor device according to claim 4, wherein: The method comprises the steps of sequentially manufacturing each corresponding material layer on the target substrate, and controlling the high-energy particle beam lithography equipment to emit a high-energy particle beam and act on the corresponding material layer on the target substrate according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film, and engraving the pattern corresponding to the integrated circuit sub-pattern to the corresponding material layer on the target substrate to obtain the target semiconductor device, including the steps of: Sequentially fabricating i-th to j-th material layers on the target substrate, and controlling the high-energy particle beam lithography equipment to emit a high-energy particle beam to act on the i-th to j-th material layers according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film corresponding to the i-th to j-th integrated circuit sub-layout, respectively, to engrave all patterns corresponding to the i-th to j-th integrated circuit sub-layout except the pattern composed of the pixel points to be adjusted onto the corresponding i-th to j-th material layers; According to the coordinates of the pixel to be adjusted, the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam to act on the coordinates of the pixel to be adjusted in the jth material layer, and penetrate the i to jth material layers at the coordinates of the pixel to be adjusted.
6. The method for controlling the processing of a semiconductor device according to claim 3, wherein: The method of resetting the grayscale values of the pixels to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layouts of the i-th to j-th layers according to a preset adjustment strategy comprises the following steps: Setting the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the i-th to j-1-th layers to the lowest value, or obtaining the first grayscale value corresponding to the lowest high-energy particle beam processing parameter, and setting the grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the i-th to j-1-th layers to the first grayscale value; Obtaining target high-energy particle beam processing parameters that penetrate the i-th to j-th material layers; Acquire a second grayscale value according to a correspondence between the target high-energy particle beam processing parameter and the preset high-energy particle beam processing parameter and the grayscale value; The grayscale value of the pixel to be adjusted in the grayscale negative film corresponding to the integrated circuit sub-layout of the j-th layer is set to the second grayscale value.
7. The method for controlling the processing of a semiconductor device according to claim 6, wherein: The method comprises the steps of sequentially manufacturing each corresponding material layer on the target substrate, and controlling the high-energy particle beam lithography equipment to emit a high-energy particle beam and act on the corresponding material layer on the target substrate according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film, and engraving the pattern corresponding to the integrated circuit sub-pattern to the corresponding material layer on the target substrate to obtain the target semiconductor device, including the steps of: Sequentially fabricating the i-th to j-1-th material layers on the target substrate, and controlling the high-energy particle beam lithography equipment to emit a high-energy particle beam to act on the i-th to j-1-th material layers according to the high-energy particle beam processing parameters corresponding to each pixel point in the grayscale negative film corresponding to the i-th to j-1-th integrated circuit sub-layout, respectively, to engrave all patterns corresponding to the i-th to j-1-th integrated circuit sub-layout except the pattern composed of the pixel points to be adjusted onto the corresponding i-th to j-1-th material layers; A j-th material layer is arranged on the target substrate, and the high-energy particle beam lithography equipment is controlled to emit a high-energy particle beam to act on the j-th material layer, and a pattern corresponding to the j-th integrated circuit sub-layout is engraved to the j-th material layer, and the j-th to i-th material layers are penetrated at the coordinates of the pixel point to be adjusted.
8. The method for controlling the processing of a semiconductor device according to claim 1, wherein: The step of sequentially manufacturing each corresponding material layer on the target substrate comprises the following steps: Acquire a material gas corresponding to the material layer and a deposition area corresponding to the material layer on the target substrate; The high-energy particle beam lithography equipment is controlled to spray the material gas in the deposition area, so that the material gas is decomposed and deposited in the deposition area, thereby completing the production of the material layer.
9. The method for controlling the processing of a semiconductor device according to claim 1, wherein: The step of sequentially manufacturing each corresponding material layer on the target substrate comprises the following steps: According to a preset optimized thickness range and / or a preset optimized flatness range, the high-energy particle beam is controlled to polish the material layer so that the current thickness and / or the current flatness of the material layer are respectively within the preset optimized thickness range and the preset optimized flatness range.
10. A high energy particle beam lithography device, characterized in that: include: A processor, a memory, and a computer program stored in the memory and executable on the processor, wherein the processor implements the steps of the method according to any one of claims 1 to 9 when executing the computer program.
Citation Information
Patent Citations
Processing control method and device of semiconductor device and high-energy particle beam photoetching equipment
CN114927410A
Manufacturing method for cylinder lens, gray scale mask, manufacturing method for integrator, integrator, illumination optical system and projection aligner
JP2004317678A