Processing method of cold forging star-shaped sleeve

By using the upper and lower top columns of the cold forging molds and the extrusion die core of the eight-petal molding block, the one-time molding of the star sleeve is realized, and the complex cold forging process and rollers in the prior art are solved. The problem of difficulty in groove finishing improves molding accuracy and surface quality.

CN117620052BActive Publication Date: 2024-11-19NINGBO KAIMINSHENG MASCH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311590297.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-27
Publication Date
2024-11-19
Estimated Expiration
2043-11-27

AI Technical Summary

Technical Problem

The existing star sleeve cold forging process is complex. After the cold forging is completed, the roller grooves need to be finished, and the roller grooves with asymmetric structures are difficult to be formed directly, resulting in multiple cold forging and finishing needs.

Method used

Using a cold forging mold including upper die device, lower die device and core device, through the cooperation of the upper top column and the lower top column, the eight-flap forming blocks close together to form a molding cavity, realizing a one-time extrusion forming star sleeve to avoid rollers Secondary processing of the channel groove.

Benefits of technology

The molding accuracy and surface quality of the star sleeve are improved, material waste and process are reduced, and high-precision molding of the roller groove is achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117620052B_ABST
    Figure CN117620052B_ABST
Patent Text Reader

Abstract

The present invention relates to a processing method for cold forging a star-shaped sleeve, and the processing method for cold forging a star-shaped sleeve is used for cold forging a star-shaped sleeve through a cold forging die. The outer peripheral wall of the star-shaped sleeve is provided with eight roller grooves distributed around the center, each of the roller grooves is arc-shaped and concave, and the two ends of the roller grooves are arc-shaped and bent toward the center direction of the star-shaped sleeve. The cold forging die includes an upper die device, a lower die device and a core device installed on the lower die device. Each petal of the extrusion die core is provided with a forming curved surface boss corresponding to one of the roller grooves, and the forming curved surface boss is formed with an integrated roller groove on the surface of the blank, thereby avoiding secondary processing of the roller groove, and the forming precision is high and the surface quality is good.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of forging, and in particular to a processing method for cold forging a star-shaped sleeve. Background Art

[0002] The ball cage type constant velocity universal joint includes an input shaft, a star sleeve, eight steel balls and a bell sleeve. The star sleeve is an important component of the ball cage type constant velocity universal joint. Eight roller grooves distributed around the center are arranged on the outer peripheral wall of the star sleeve. The steel balls are connected to the roller grooves in a rolling manner and connected to the rollers of the bell sleeve to form power transmission.

[0003] The existing star-shaped sleeve can be made by hot forging, which requires a lot of material removal. The star-shaped sleeve is processed by cold forging, and the existing cold forging of the star-shaped sleeve requires multiple cold forging processes. In addition, the roller groove and the outer end surface of the star-shaped sleeve need to be finely processed by cutting, which has a complex processing technology and low processing accuracy of the roller groove.

[0004] Chinese public document CN204842504U discloses a cold forging die for an automobile star-shaped sleeve. The cold forging die uses a two-groove template closing structure to perform cold forging processing on the star-shaped sleeve. Accordingly, there must be an extrusion mark at the closing position of the template. The extrusion mark extends to the roller groove, which will inevitably affect the processing accuracy of the roller groove.

[0005] Especially when the two ends of the roller groove are asymmetrical structures, it is difficult for the existing cold forging die to directly form the roller groove, and to perform secondary processing of the formed star-shaped sleeve on the roller groove. There are technical problems that the star sleeve needs to be cold forged multiple times and the roller groove needs to be finely processed after the cold forging is completed, so improvement is needed. Summary of the invention

[0006] In order to overcome the problems existing in the related art, an embodiment of the present invention provides a processing method for cold forging a star-shaped sleeve, which is used to solve the technical problem that the cold forging process of the star-shaped sleeve is complicated and the roller groove needs to be finely processed after the cold forging is completed.

[0007] According to an embodiment of the present invention, a processing method for cold forging a star-shaped sleeve is provided, which is used for cold forging a star-shaped sleeve by a cold forging die, wherein the outer peripheral wall of the star-shaped sleeve is provided with eight roller grooves distributed around the center, each of the roller grooves is arc-shaped and concave, and the two ends of the roller grooves are arc-shaped and bent toward the center direction of the star-shaped sleeve, and the cold forging die comprises an upper die device, a lower die device and a core device installed on the lower die device;

[0008] The core device comprises a core seat and an extrusion core, the core seat is provided with a conical limiting hole, the extrusion core comprises an eight-petal forming block sliding in the limiting hole, the eight-petal forming block is closed and forms a forming cavity at the center, the forming cavity comprises an extrusion area, an upper guide area and a lower guide area distributed at both ends of the extrusion area; wherein the forming block protrudes toward the extrusion area to form a forming curved surface boss, the shape of the forming curved surface boss is complementary to the corresponding roller groove, and the matching gap of adjacent forming blocks is located between two adjacent forming curved surface bosses;

[0009] The upper die device comprises an upper ejector column aligned with the upper guide area, the size of the upper ejector column is smaller than the size of the upper guide area, and the lower die device comprises a lower ejector column aligned with the lower guide area, the size of the lower ejector column is smaller than the size of the lower guide area;

[0010] The processing method comprises the following steps:

[0011] S101, lubricating the surface of the annealed cylindrical raw material to form a blank;

[0012] S102, placing the blank into the molding cavity, with the lower end of the blank abutting against the top end of the lower ejector column;

[0013] S103, driving the upper mold device to move toward the lower mold device and close, the upper ejector column is inserted into the upper guide area and pushes the top end of the blank, the eight-petal forming block is closed, the lower ejector column is synchronously lifted toward the extrusion area to extrude the blank, the end face spacing between the end face of the lower ejector column and the end face of the upper ejector column is the same as the axial height of the extrusion area, the blank is plastically deformed by the extrusion force to fill the space in the extrusion area, so as to be formed into a star-shaped sleeve;

[0014] S104, driving the upper mold device away from the lower mold device, the lower ejector column pushes the star-shaped sleeve and the eight-petal molding block to move upward, and the star-shaped sleeve is taken out after the eight-petal molding block is unfolded;

[0015] S105, driving the lower ejector column to move downward, and the extrusion die core slides into the limiting hole;

[0016] Steps S101 to S105 are repeated to perform continuous processing.

[0017] In one embodiment, the upper top column includes an upper spline shaft having eight groups of spline ribs, the upper guide area is configured to fit an upper spline hole of the upper spline shaft, and an upper extrusion gap is provided between the upper spline shaft and the upper spline hole.

[0018] In one embodiment, the angle of the spline rib is the same as the angle of the rib of the outer peripheral wall of the star sleeve, and the contour shape of the end face edge of the upper spline shaft is matched with the top contour shape of the star sleeve.

[0019] In one embodiment, an upper center column is formed on the end surface of the upper spline shaft and protrudes in the center. The upper center column pushes and squeezes the blank to plastically deform from the center area toward the forming curved surface boss.

[0020] In one embodiment, the protruding height of the upper center column is less than or equal to one third of the extrusion zone, and the ratio of the axial diameter of the upper center column to the diameter of the inscribed circle of the star sleeve is set to K, wherein 1 / 2≤K≤5 / 7.

[0021] In one embodiment, the lower push column includes a thrust column and a lower spline shaft partially protruding from the end surface of the thrust column, the cross-sectional size of the thrust column is larger than the size of the lower guide area, the outer peripheral wall of the lower spline shaft has eight groups of spline ribs, the lower guide area is configured to adapt to the lower spline hole of the lower spline shaft, and a lower extrusion gap is provided between the lower spline shaft and the lower spline hole.

[0022] In one embodiment, the end surface of the push column is set to be a convex spherical surface, and the eight-petal forming block is configured to match the groove surface of the convex spherical surface.

[0023] In one embodiment, the end surface of the lower spline shaft protrudes in the center to form a lower center column, and the lower center column pushes and squeezes the blank to plastically deform from the center area toward the forming curved surface boss.

[0024] In one embodiment, the molding curved surface boss includes a central curved surface, a first curved surface and a second curved surface distributed at both ends of the central curved surface, the curvature radius of the first curved surface is greater than the curvature radius of the second curved surface, and the molding curved surface bosses of two adjacent molding blocks are distributed in opposite directions.

[0025] In one embodiment, the surface lubrication treatment includes: a phosphorus saponification treatment of the cylindrical raw material; or a lubricating oil immersion treatment of the cylindrical raw material.

[0026] The technical solution provided by the embodiment of the present invention may include the following beneficial effects: each petal of the extrusion die core is provided with a forming curved surface boss corresponding to one of the roller grooves, and the forming curved surface boss forms an integrated roller groove on the surface of the blank, thereby avoiding secondary processing of the roller groove, and having high forming accuracy and good surface quality. The extrusion zone is located inside the extrusion die core, and the blank is abutted by the upper ejector column and the lower ejector column and extruded to fill the entire extrusion zone, thereby extruding a complete star-shaped sleeve at one time, and having high forming accuracy. The excess part of the blank is extruded directionally along the gap between the upper ejector column and the upper guide zone and the gap between the lower ejector column and the lower guide zone, and the forming of the star-shaped sleeve is controllable and the extrusion direction of the excess material is controllable.

[0027] It is to be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.

[0029] Figure 1 It is a block diagram of a processing method for cold forging a star-shaped sleeve according to an exemplary embodiment.

[0030] Figure 2 It is a schematic structural diagram of a cold forging die according to an exemplary embodiment.

[0031] Figure 3 It is a schematic cross-sectional structural diagram of a cold forging die according to an exemplary embodiment.

[0032] Figure 4 It is an enlarged schematic diagram showing an upper ejector column and a lower ejector column abutting against a blank according to an exemplary embodiment.

[0033] Figure 5 It is a schematic structural diagram of a star-shaped sleeve after molding according to an exemplary embodiment.

[0034] Figure 6 It is a schematic structural diagram of an upper mold assembly according to an exemplary embodiment.

[0035] Figure 7 It is a schematic structural diagram showing an extrusion die core being assembled to a die core seat according to an exemplary embodiment.

[0036] Figure 8 is a schematic structural diagram of a forming block according to an exemplary embodiment.

[0037] In the figure, the upper mold device 10; the upper ejector column 11; the spline rib 111; the upper center column 112; the upper spline shaft 113; the upper extrusion gap 114; the hydraulic cylinder 12; the lower mold device 20; the core seat 21; the limiting hole 211; the lower ejector column 22; the lower spline shaft 221; the lower center column 222; the lower mold base 23; the sliding hole 231; the push column 232; the extrusion core 30; the forming cavity 31; the upper guide area 311; the extrusion area 312; the lower guide area 313; the lower extrusion gap 314; the forming curved surface boss 315; the center curved surface 3151; the first arc surface 3152; the second arc surface 3153; the forming block 32; the star sleeve 40; the roller groove 41; the toothed rib 42; the extrusion hole 43. DETAILED DESCRIPTION

[0038] Among them, the drawings are only used for illustrative explanations, and they only represent schematic diagrams rather than actual pictures, and should not be understood as limitations on this patent; in order to better illustrate the embodiments of the present invention, some parts of the drawings may be omitted, enlarged or reduced, and do not represent the size of the actual product; for those skilled in the art, it is understandable that some well-known structures and their descriptions in the drawings may be omitted.

[0039] The same or similar numbers in the drawings of the embodiments of the present invention correspond to the same or similar parts; in the description of the present invention, it should be understood that if the terms "upper", "lower", "left", "right", "inner", "outer", etc. appear, the orientation or position relationship indicated is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. Therefore, the terms describing the position relationship in the drawings are only used for illustrative purposes and cannot be understood as a limitation on this patent. For ordinary technicians in this field, the specific meanings of the above terms can be understood according to specific circumstances.

[0040] In the description of the present invention, unless otherwise clearly specified and limited, if the term "connection" or the like appears to indicate the connection relationship between components, the term should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two components or the interaction relationship between two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0041] like Figures 1 to 5As shown, the present invention provides a processing method for cold forging a star-shaped sleeve, which is used for cold forging a star-shaped sleeve 40 by a cold forging die. The outer peripheral wall of the star-shaped sleeve 40 is provided with eight roller grooves 41 distributed around the center, each roller groove 41 is arc-shaped and concave, and the two ends of the roller groove 41 are arc-shaped and bent toward the center direction of the star-shaped sleeve 40. On the cross section of the star-shaped sleeve 40 perpendicular to the center direction of the star-shaped sleeve 40, the cross section of the roller groove 41 is an arc-shaped concave structure. Optionally, the two ends of the roller groove 41 are bent toward the center direction to form a roller curve that is approximately C-shaped. For example, the two ends of the roller groove 41 have the same structure to form a symmetrical structure. Alternatively, the arc lengths of the two ends of the roller groove 41 are different to form a directional curved groove. Preferably, the arc lengths of the two ends of the roller groove 41 are different, and the arc directions of the two adjacent roller grooves 41 are relatively cross-arranged.

[0042] The cold forging die comprises an upper die device 10, a lower die device 20 and a core device installed on the lower die device 20. The upper die device 10 and the lower die device 20 move relatively to form a die closing posture and a die opening posture.

[0043] The core device includes a core seat 21 and an extrusion core 30, and the core seat 21 is installed on the lower mold device 20. The core seat 21 is provided with a conical limiting hole 211, and the extrusion core 30 is slidably inserted in the limiting hole 211. Among them, the outer peripheral wall of the extrusion core 30 is a conical structure adapted to the limiting hole 211, and the extrusion core 30 can be aligned and arranged along the limiting hole 211. The extrusion core 30 includes an eight-petal forming block 32 that slides in the limiting hole 211, and the limiting hole 211 limits and positions the outer peripheral wall of the extrusion core 30. The eight-petal forming block 32 can automatically close and align under the action of the extrusion force.

[0044] The eight-petal forming block 32 is closed and forms a forming cavity 31 at the center. The forming cavity 31 includes an extrusion area 312, an upper guide area 311 and a lower guide area 313 distributed at both ends of the extrusion area 312. The extrusion area 312 is located in the forming cavity 31, and the shape of the extrusion area 312 is substantially the same as that of the star-shaped sleeve 40. The upper guide area 311 and the lower guide area 313 are located at the upper and lower ends of the extrusion area 312, respectively. The upper mold device 10 includes an upper ejector column 11 aligned with the upper guide area 311, and the size of the upper ejector column 11 is smaller than the size of the upper guide area 311. The lower mold device 20 includes a lower ejector column 22 aligned with the lower guide area 313, and the size of the lower ejector column 22 is smaller than the size of the lower guide area 313. The upper ejector column 11 is inserted into the forming cavity 31 along the upper guide area 311, and the lower ejector column 22 is inserted into the forming cavity 31 along the lower guide area 313, so that the material is extruded into the forming cavity 31.

[0045] Among them, the forming block 32 protrudes toward the extrusion area 312 to form a forming curved surface boss 315, the shape of the forming curved surface boss 315 is complementary to the corresponding roller groove 41, and the matching gap between adjacent forming blocks 32 is located between two adjacent forming curved surface bosses 315. The protruding shape and protruding angle of the forming curved surface boss 315 are the same as the shape of the roller groove 41. The surface of the forming curved surface boss 315 is a smooth curved surface structure, and the metal material is extruded and fitted on the surface of the forming curved surface boss 315 to form a matching roller groove 41. The eight-petal forming block 32 is unfolded after the star-shaped sleeve 40 is formed, so as to facilitate the removal of the star-shaped sleeve 40 from the forming cavity 31.

[0046] The cold forging method of the star sleeve 40 comprises the following steps:

[0047] Step S101, lubricate the surface of the annealed cylindrical raw material to form a blank. The cylindrical raw material adopts a solid cylindrical material such as a steel column, and the cylindrical raw material is annealed to reduce the hardness and improve the plasticity. The surface of the cylindrical raw material is lubricated to improve the extrusion molding effect and reduce damage to the extrusion die core 30. Optionally, the surface lubrication treatment includes: 1. Phosphorus saponification treatment of the cylindrical raw material, which can improve the surface sliding flexibility of the blank and improve the plasticity. 2. The cylindrical raw material is immersed in lubricating oil, and the lubricating oil can lubricate the blank and the molding cavity 31 to reduce indentation and wear, and maintain the controllability and molding quality of the extrusion die core 30.

[0048] Step S102, the blank is placed in the molding cavity 31, and the lower end of the blank is against the top of the lower ejector 22. The axial diameter of the blank is smaller than the aperture of the upper guide area 311, so that the blank can be directly placed in the molding cavity 31. The lower ejector 22 partially extends into the upper guide area 311, so that the blank is symmetrically arranged on both sides of the extrusion area 312.

[0049] Step S103, drive the upper mold device 10 to move toward the lower mold device 20 and close, the upper ejector 11 is inserted into the upper guide area 311 and pushes the top of the blank, and the eight-petal forming block 32 is closed. The lower ejector 22 synchronously lifts the extruded blank in the direction of the extrusion area 312, and the end face spacing between the end face of the lower ejector 22 and the end face of the upper ejector 11 is the same as the axial height of the extrusion area 312. The blank is plastically deformed by the extrusion force to fill the space in the extrusion area 312 to form a star-shaped sleeve 40. Each petal of the extrusion die core 30 is provided with a forming curved surface boss 315 corresponding to one of the roller grooves 41, and the forming curved surface boss 315 is formed with an integrated roller groove 41 on the surface of the blank, thereby avoiding secondary processing of the roller groove 41, and the forming precision is high and the surface quality is good.

[0050] The upper die device 10 moves and closes toward the lower die device 20 under the drive of the stamping machine. The upper ejector 11 is inserted into the upper guide area 311 and pushes the blank to compress and deform. The lower ejector 22 is lifted and cooperates with the upper ejector 11 to synchronously extrude the two ends of the blank to achieve axial compression deformation of the blank so that the blank expands radially. At the same time, the eight-petal forming block 32 slides along the conical surface of the limiting hole 211 and closes toward the center to clamp the outer peripheral wall of the extruded blank to achieve the roller groove 41 of the star sleeve 40. The extrusion and deformation of the blank are both located in the forming cavity 31. The outer shape of the star sleeve 40 is formed in one step, and only the excess extrusion edge material needs to be cut off. There is no need to process the roller groove 41 and the outer peripheral wall, which reduces material waste and saves process costs.

[0051] Step S104, the upper mold device 10 is driven away from the lower mold device 20, the lower ejector column 22 pushes the star-shaped sleeve 40 and the eight-petal molding block 32 upward, and the star-shaped sleeve 40 is taken out after the eight-petal molding block 32 is unfolded. The upper mold device 10 moves upward and resets, and the upper ejector column 11 is separated from the molding cavity 31. The lower ejector column 22 continues to rise and pushes the star-shaped sleeve 40, and the extrusion mold core 30 moves upward and gradually unfolds, thereby facilitating the removal of the star-shaped sleeve 40.

[0052] Step S105 , driving the lower ejector pin 22 to move downward, and the extrusion die core 30 slides into the limiting hole 211 .

[0053] Steps S101 to S105 are repeated to perform continuous processing.

[0054] The extrusion area 312 is located inside the extrusion die core 30. The blank is abutted by the upper ejector pin 11 and the lower ejector pin 22 and extruded to fill the entire extrusion area 312, thereby extruding a complete star-shaped sleeve 40 at one time with high molding precision. The excess portion of the blank is extruded along the gap between the upper ejector pin 11 and the upper guide area 311 and the gap between the lower ejector pin 22 and the lower guide area 313, and the molding of the star-shaped sleeve 40 is controllable and the extrusion direction of the excess material is controllable.

[0055] like Figures 4 to 6 As shown, the upper ejector 11 squeezes and pushes the upper end of the blank to deform, wherein the upper ejector 11 can be configured as a columnar structure, such as a cylindrical, prism or spline shaft. Preferably, the upper ejector 11 includes an upper spline shaft 113 having eight groups of spline ribs 111. The star sleeve 40 has tooth-shaped ribs 42 between two adjacent roller grooves 41. The spline ribs 111 are arranged in eight groups and protrude at intervals around the outer peripheral wall of the upper spline shaft 113. The positions of the eight groups of spline ribs 111 coincide with the positions of the tooth-shaped ribs 42.

[0056] The upper guide area 311 is configured to fit the upper spline hole of the upper spline shaft 113, and an upper extrusion gap 114 is provided between the upper spline shaft 113 and the upper spline hole. The upper spline hole is used to guide the upper spline shaft 113 to slide, and to guide and support the upper spline shaft 113. The upper extrusion gap 114 is used to guide the directional extrusion of the remainder of the blank, thereby avoiding the reservation of machining allowance on the outer dimensions of the star sleeve 40, so that the star sleeve 40 can be formed in one step. Preferably, the upper extrusion gap 114 extends from the end of the upper spline shaft 113 to a preset length in the opening direction of the upper guide area 311, so as to avoid excessive metal remainder from squeezing into the upper extrusion gap 114. For example, the axial length of the upper extrusion gap 114 is configured to be 5 mm to 20 mm, and the maximum gap width of the upper extrusion gap 114 is 0.1 mm to 0.5 mm.

[0057] Preferably, the angle of the spline rib 111 is the same as the angle of the rib of the outer peripheral wall of the star sleeve 40, and the edge contour of the end face of the upper spline shaft 113 is adapted to the top contour of the star sleeve 40. During the cold forging process, the spline rib 111 supports the part of the toothed rib 42 and compacts the end face to improve the forming strength of the end surface. The shape of the spline rib 111 is slightly smaller than the end face shape of the toothed rib 42, so that the metal residue enters the upper extrusion gap 114 from the end edge of the toothed rib 42. The extruded edge material formed by the metal residue is concentrated on the end face of the star sleeve 40, which is convenient for removal by grinding or cutting, avoiding processing at the roller groove 41. Preferably, the star sleeve 40 is heat treated or tempered after the metal residue grinding process to improve the structural strength.

[0058] Preferably, the shape of the upper extrusion gap 114 is larger than the shape of the upper spline shaft 113, and the shape of the upper extrusion gap 114 is smaller than the size of the top contour shape of the star sleeve 40, which can facilitate the insertion of the upper spline shaft 113 into the upper guide area 311 and concentrate the metal residue on the end face of the star sleeve 40, thereby facilitating smooth cutting.

[0059] Similar to the structure of the upper spline shaft 113, the lower top column 22 is provided with a lower spline shaft 221, the outer peripheral wall of the lower spline shaft 221 has eight groups of spline ribs 111, the lower guide area 313 is provided as a lower spline hole adapted to the lower spline shaft 221, and a lower extrusion gap 314 is provided between the lower spline shaft 221 and the lower spline hole. The cooperation between the lower spline shaft 221 and the lower guide area 313 can refer to the upper spline shaft 113 and the upper guide area 311, and the lower extrusion gap 314 can realize that the metal excess enters the lower extrusion gap 314 from the end edge of the tooth-shaped rib 42.

[0060] In one embodiment, the end surface of the upper spline shaft 113 protrudes in the center to form an upper center column 112, and the upper center column 112 pushes the extruded blank to plastically deform from the center area to the direction of the formed curved surface boss 315. The upper center column 112 is a boss structure protruding from the end surface of the upper spline shaft 113. Optionally, the upper center column 112 can be set as a cylindrical, frustum-shaped, or prismatic protrusion structure to form a local protrusion. The center line of the upper center column 112 coincides with the axis of the upper spline shaft 113 to form a central boss.

[0061] When the upper spline shaft 113 extrude the end face of the blank, the upper center column 112 is embedded in the blank until the end face of the upper spline shaft 113 abuts against the top face of the blank. The upper center column 112 can extrude the metal part material in the middle of the blank to deform and fill the entire extrusion area 312, so as to reduce the shaft diameter requirement of the blank and improve the utilization rate of the material. The upper center column 112 provides support for the outer peripheral wall of the star sleeve 40 from the center, and combines with the eight-petal forming block 32 to realize the synchronous extrusion of metal materials inside and outside, achieve high extrusion performance, and ensure that the forming surface of the star sleeve 40 is flat and smooth with high density.

[0062] Preferably, the end of the upper center column 112 is provided with an arc-shaped chamfer, which makes the end of the upper center column 112 gradually tilted, making demoulding easier. In addition, the upper center column 112 is formed with a countersunk extrusion hole 43 at the center position of the star-shaped sleeve 40, which can easily locate and process the center hole of the star-shaped sleeve 40.

[0063] Optionally, the protruding height of the upper center column 112 is less than or equal to one third of the extrusion area 312, so as to avoid eccentricity caused by the large amount of extrusion on one side of the star sleeve 40, and to achieve an effective center extrusion effect. Preferably, the lower top column 22 is provided with a lower center column 222, and the lower center column 222 pushes the extruded blank to plastically deform from the center area to the forming curved surface boss 315. The structure and function of the lower center column 222 and the upper center column 112 are similar, and can be understood by reference, and will not be repeated here.

[0064] The upper center column 112 and the lower center column 222 move relative to each other to jointly extrude the two ends of the blank, and both ends of the blank are squeezed into the groove, so that the middle area of ​​the blank is extruded toward the cavity wall direction of the extrusion zone 312, avoiding extrusion defects caused by insufficient metal extrusion in the roller groove 41. The structure of the upper center column 112 and the lower center column 222 is combined with the upper extrusion gap 114 and the lower extrusion gap 314 between the lower top column 22 and the lower guide zone 313 to achieve complete extrusion filling of the extrusion zone 312.

[0065] In one embodiment, the ratio of the shaft diameter of the upper center column 112 to the diameter of the inscribed circle of the star sleeve 40 is set to K, where 1 / 2≤K≤5 / 7. The upper center column 112 is set to a frustum-shaped boss structure, and the diameter of the middle height of the upper center column 112 is used as the shaft diameter, where the shaft diameter of the upper center column 112 is adjusted according to the size specification of the extruded star sleeve 40, and the inscribed circle diameter of the star sleeve 40 is the minimum inscribed diameter of the roller groove 41. K can be set to a ratio of 1 / 2, 2 / 3, 5 / 7, etc.

[0066] Preferably, the upper die device 10 includes an upper die plate, a plurality of guide pillars connected to the upper die plate, and a hydraulic cylinder 12 installed on the upper die plate, and an upper ejector pillar 11 is fixed to the output shaft of the hydraulic cylinder 12. Driven by the machine tool, the upper die plate slides along the guide pillars to the top of the lower die device 20 until the upper ejector pillar 11 abuts against the end of the blank, and the upper die plate pushes the extrusion die core 30 to move into the limiting hole 211 to cooperate with the lower ejector pillar 22 to extrude the lower end of the blank until the extrusion die core 30 is embedded in the limiting hole 211 and the eight-petal forming block 32 is completely closed. The hydraulic cylinder 12 drives the upper ejector pillar 11 to radially pressurize the upper ejector pillar 11 for a second time, and pressurizes the upper ejector pillar 11 at a second speed. The upper ejector pillar 11 gradually pressurizes the blank to form a multi-stage cold forging setting to improve the forming quality. Preferably, the upper push column 11 includes a top plate portion, and the upper spline shaft 113 protrudes from the top plate portion. The hydraulic cylinder 12 drives the upper push column 11 to abut against the end of the blank, and gradually extrude the blank until the top plate portion abuts against the end of the extrusion die core 30, so that the eight-petal forming block 32 is completely closed, and the planetary sleeve gradually fills the extrusion area 312, and the extrusion effect is good and the extrusion is comprehensive. In this extrusion method, the extrusion area 312 is a gradually reduced space. In addition to the extrusion effect of the blank from the center to the periphery, the eight-petal forming block 32 pushes the extrusion die core 30 from the outside to the inside under the action of the top plate portion to close and extrude the outer peripheral wall of the star sleeve, thereby forming internal and external synchronous extrusion, better extrusion filling effect, and higher surface forming density of the roller groove.

[0067] like Figure 2 , Figure 3 , Figure 7 and Figure 8 As shown, preferably, the lower die device 20 further includes a lower die base 23, the lower die base 23 is provided with a sliding hole 231, and the lower spline shaft 221 is slidably connected to the sliding hole 231. The sliding clearance between the lower spline shaft 221 and the sliding hole 231 is smaller than the lower extrusion clearance 314 between the lower spline shaft 221 and the lower guide area 313, and there is a movable space between the lower end surface of the extrusion die core 30 and the top surface of the lower die base 23. The movable space can not only meet the activity requirements of the extrusion die core 30, but also carry the excess metal residue.

[0068] Furthermore, the lower push column 22 also includes a push column 232, and the lower spline shaft 221 is partially protruded from the end surface of the push column 232, and the cross-sectional size of the push column 232 is larger than the size of the lower guide area 313. The length of the lower spline shaft 221 is greater than or equal to the depth of the lower guide area 313. When the star sleeve 40 completes the cold forging process, the lower push column 22 continues to rise under the power drive, and the push column 232 pushes the extrusion mold core 30 to rise and expand the extrusion mold core 30 to facilitate the removal of the star sleeve 40. Optionally, the push column 232 is located in the activity space. On the contrary, the extrusion mold core 30 is in an extended state when the blank is received, and the push of the upper mold device 10 is cooperated to achieve closing and extrusion.

[0069] Preferably, the end surface of the push column 232 is set as a convex spherical surface, and the eight-petal forming block 32 is configured with a groove surface matching the convex spherical surface. The mating surface between the push column 232 and the extrusion mold core 30 is a spherical mating surface. When the push column 232 pushes the extrusion mold core 30 upward, the eight-petal forming block 32 unfolds along the convex spherical surface, thereby facilitating the removal of the star-shaped sleeve 40.

[0070] Each forming block 32 is provided with a forming curved surface boss 315, which is used to form the roller groove 41 to form a complete roller groove 41 structure. In one embodiment, the forming curved surface boss 315 includes a central curved surface 3151, a first curved surface 3152 and a second curved surface 3153 distributed at both ends of the central curved surface 3151. The central surface of the central curved surface 3151 of the eight-petal forming block 32 is at the same height, and the forming curved surface is curved from the central surface to the two ends. Among them, the central surface is perpendicular to the center line of the star sleeve 40, and the central curved surface 3151, the first curved surface 3152 and the second curved surface 3153 are all convex curved surfaces.

[0071] The first arc surface 3152 and the second arc surface 3153 are respectively located at the two ends of the central curved surface 3151. When the arc radius of the first arc surface 3152 and the second arc surface 3153 are the same, the roller groove 41 is a symmetrical structure. When the arc radius of the first arc surface 3152 is greater than the arc radius of the second arc surface 3153, the curvature of the two ends of the roller groove 41 is different, and accordingly, the forming of the roller groove 41 has directionality. Optionally, the first arc surface 3152 is located at the same end of the star sleeve 40, and the second arc surface 3153 is located at the other end of the star sleeve 40. Preferably, the forming curved surface bosses 315 of two adjacent forming blocks 32 are distributed in opposite directions, and the first arcuate surfaces 3152 are alternately arranged on the star sleeve 40, that is, at the same end of the star sleeve 40, the first arcuate surface 3152 is located between the second arcuate surfaces 3153 of two adjacent roller grooves 41, and the second arcuate surface 3153 is located between the first arcuate surfaces 3152 of two adjacent roller grooves 41. The roller groove 41 is arranged in a three-positive and three-negative layout, and the processing difficulty of the existing cutting processing of the star sleeve 40 is extremely great. However, the present application adopts a cold forging process, which can realize the roller groove 41 without processing, with high processing accuracy and low cost.

[0072] Preferably, the overlapping surfaces of two adjacent forming blocks 32 are provided with overflow grooves, which are chamfers of the forming blocks 32 in the extrusion area 312. The overflow grooves extend from one end of the extrusion area 312 to the other end. The setting of the overflow grooves can allow the metal material to be completely extruded, filled and covered with the entire surface of the forming curved boss 315 and the concave areas on both sides, thereby reducing the forming defects of the tooth-shaped convex ribs 42. The part of the metal material in the overflow groove is correspondingly formed with convex ribs on the star-shaped sleeve 40, and the convex ribs are located at the top of the tooth-shaped convex ribs 42, which are convenient for grinding or cutting.

[0073] Those skilled in the art will readily appreciate other embodiments of the present invention after considering the specification and practicing the disclosure disclosed herein. This application is intended to cover any variations, uses or adaptations of the present invention that follow the general principles of the present invention and include common knowledge or customary techniques in the art that are not disclosed by the present invention. The description and examples are to be considered exemplary only, and the true scope and spirit of the present invention are indicated by the following claims.

[0074] It should be understood that the present invention is not limited to the exact construction that has been described above and shown in the drawings and that various modifications and changes may be made without departing from the scope thereof. The scope of the present invention is limited only by the appended claims.

Claims

1. A processing method for cold forging a star-shaped sleeve, which is used for cold forging a star-shaped sleeve by a cold forging die, wherein the outer peripheral wall of the star-shaped sleeve is provided with eight roller grooves distributed around the center, each of the roller grooves is arc-shaped and concave, and the two ends of the roller grooves are arc-shaped and bent toward the center direction of the star-shaped sleeve, and the cold forging die comprises an upper die device, a lower die device and a core device installed on the lower die device; characterized in that: The core device comprises a core seat and an extrusion core, the core seat is provided with a conical limiting hole, the extrusion core comprises an eight-petal forming block sliding in the limiting hole, the eight-petal forming block is closed and forms a forming cavity at the center, the forming cavity comprises an extrusion area, an upper guide area and a lower guide area distributed at both ends of the extrusion area; wherein the forming block protrudes toward the extrusion area to form a forming curved surface boss, the shape of the forming curved surface boss is complementary to the corresponding roller groove, and the matching gap of adjacent forming blocks is located between two adjacent forming curved surface bosses; The upper die device comprises an upper ejector column aligned with the upper guide area, the size of the upper ejector column is smaller than the size of the upper guide area, and the lower die device comprises a lower ejector column aligned with the lower guide area, the size of the lower ejector column is smaller than the size of the lower guide area; The processing method comprises the following steps: S101, lubricating the surface of the annealed cylindrical raw material to form a blank; S102, placing the blank into the molding cavity, with the lower end of the blank abutting against the top end of the lower ejector column; S103, driving the upper mold device to move toward the lower mold device and close, the upper ejector column is inserted into the upper guide area and pushes the top end of the blank, the eight-petal forming block is closed, the lower ejector column is synchronously lifted toward the extrusion area to extrude the blank, the end face spacing between the end face of the lower ejector column and the end face of the upper ejector column is the same as the axial height of the extrusion area, the blank is plastically deformed by the extrusion force to fill the space in the extrusion area, so as to be formed into a star-shaped sleeve; S104, driving the upper mold device away from the lower mold device, the lower ejector column pushes the star-shaped sleeve and the eight-petal molding block to move upward, and the star-shaped sleeve is taken out after the eight-petal molding block is unfolded; S105, driving the lower ejector column to move downward, and the extrusion die core slides into the limiting hole; Steps S101 to S105 are repeated to perform continuous processing.

2. The processing method according to claim 1, characterized in that: The upper top column comprises an upper spline shaft having eight groups of spline ribs, the upper guide area is configured to fit an upper spline hole of the upper spline shaft, and an upper extrusion gap is provided between the upper spline shaft and the upper spline hole.

3. The processing method according to claim 2, characterized in that: The angle of the spline rib is the same as the angle of the outer peripheral wall rib of the star sleeve, and the contour shape of the end face edge of the upper spline shaft is matched with the top contour shape of the star sleeve.

4. The processing method according to claim 2, characterized in that: The end surface of the upper spline shaft protrudes in the center to form an upper center column, and the upper center column pushes and squeezes the blank to plastically deform from the center area toward the forming curved surface boss.

5. The processing method according to claim 4, characterized in that: The protruding height of the upper center column is less than or equal to one third of the extrusion zone, and the ratio of the axial diameter of the upper center column to the diameter of the inscribed circle of the star sleeve is set to K, wherein 1 / 2≤K≤5 / 7.

6. The processing method according to claim 1, characterized in that: The lower push column includes a thrust column and a lower spline shaft partially protruding from the end surface of the thrust column, the cross-sectional size of the thrust column is larger than the size of the lower guide area, the outer peripheral wall of the lower spline shaft has eight groups of spline ribs, the lower guide area is configured to fit the lower spline hole of the lower spline shaft, and a lower extrusion gap is provided between the lower spline shaft and the lower spline hole.

7. The processing method according to claim 6, characterized in that: The end surface of the push column is set as a convex spherical surface, and the eight-petal forming block is configured to match the groove surface of the convex spherical surface.

8. The processing method according to claim 6, characterized in that: The end surface of the lower spline shaft protrudes in the center to form a lower center column, and the lower center column pushes and squeezes the blank to plastically deform from the center area toward the forming curved surface boss.

9. The processing method according to claim 1, characterized in that: The forming curved surface boss includes a central curved surface, a first curved surface and a second curved surface distributed at both ends of the central curved surface, the curvature radius of the first curved surface is greater than the curvature radius of the second curved surface, and the forming curved surface bosses of two adjacent forming blocks are distributed in opposite directions.

10. The processing method according to claim 1, characterized in that: The surface lubrication treatment includes: a phosphorus saponification treatment of the cylindrical raw material; or a lubricating oil immersion treatment of the cylindrical raw material.