Intelligent submerged arc welding method and system for stainless steel composite plate
By adjusting the arc length and linear speed in real time during the welding process of stainless steel composite plates, and using automated wire management and filling materials, welding problems caused by differences in the properties of base and cladding materials are solved, and welding quality and efficiency are improved.
Patent Information
- Application Number
- CN202410057809.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-16
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-01-16
AI Technical Summary
During the welding process, stainless steel composite plates are prone to defects such as thermal stress, lack of fusion, and slag inclusion due to the differences in physical and chemical properties of the base layer and cladding materials, resulting in unstable welding quality and low efficiency.
The intelligent submerged arc welding method is adopted, by setting a reference point at the end of the groove, using a laser tracker or a high-precision three-dimensional scanner to adjust the arc length and linear speed in real time, generating a weld temperature distribution cloud map, and using a welding wire replacement and distribution device to automatically Replacement and delivery, and root filler material shoveled on the back to improve weld quality.
It improves welding accuracy and efficiency, reduces defects and fluctuations, provides flexibility and efficiency in the welding process, and ensures the stability of welding quality.
Smart Images

Figure CN117680796B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of welding, and in particular to an intelligent submerged arc welding method and system for stainless steel composite plates. Background Art
[0002] Stainless steel composite plate is a metal material composed of two or more materials and has the characteristics of stainless steel. For example, the base material is carbon steel or low alloy steel, and the composite material is stainless steel. Through specific processing technology, such as blasting, rolling or explosive rolling, the base and the composite are combined together to form a new type of metal material. Stainless steel composite plate has good tolerance to corrosive media such as acid, alkali, and salt, and its price is relatively low. Stainless steel composite plate is widely used in petroleum, chemical, salt, food processing, medicine, environmental protection and other fields.
[0003] In the field of welding technology, the selection of welding methods and welding materials is crucial to welding quality and welding efficiency. There are many welding methods for different materials and processes. Among them, submerged arc welding is a widely used welding technology. By covering the flux around the arc and using the high temperature of the arc to melt the welding wire and the parent material for welding, it has the advantages of high efficiency and low cost. However, stainless steel composite plates are composed of two or more materials, and there are large differences in their physical and chemical properties, so various problems are prone to occur during the welding process. For example, due to the different thermal expansion coefficients of the base layer and the composite layer, thermal stress is prone to occur during the welding process, resulting in cracking or deformation of the weld. In addition, due to the difference in the chemical composition of the base layer and the composite layer, defects such as incomplete fusion and slag inclusion are prone to occur during the welding process.
[0004] The current welding method for stainless steel composite plates is usually to perform submerged arc welding on the base layer and then repair welding on the composite layer. Although the influence of thermal stress and chemical composition differences on welding quality can be reduced, this method still has some problems. For example, due to the different melting points of the base layer and the composite layer, poor fusion or lack of fusion is prone to occur. At the same time, this method requires a lot of time and manpower for welding operations, and the welding quality is unstable. Due to human factors and mechanical processing accuracy, there are differences in the dimensions of different groove positions, resulting in different arc lengths at different groove positions during welding and differences in welding quality. Due to the complex groove shape and weld process parameters, it is impossible to achieve accurate control of the welding process, which seriously affects the welding efficiency and quality.
[0005] Therefore, a new intelligent submerged arc welding method for stainless steel clad plates is needed to improve welding quality and efficiency. Summary of the invention
[0006] In view of the above problems, the present invention is proposed to provide an intelligent submerged arc welding method and system for stainless steel composite plates that overcome all or at least part of the above problems.
[0007] According to one aspect of the present invention, there is provided a method for intelligent submerged arc welding of a stainless steel composite plate, comprising:
[0008] Step 1. Processing a groove at the welding position of the stainless steel composite plate to be welded, and setting two reference points at the end of the groove, wherein the width of the groove is set according to the electrode diameter, the penetration depth, the density of the molten metal and the welding energy;
[0009] Step 2. Use a laser tracker or a high-precision 3D scanner to detect the groove to obtain 3D data, and adjust the arc length and line speed in real time during the welding process to reduce defects and fluctuations in the welding process, wherein the arc length is adjusted according to the arc voltage, arc current and welding wire parameters;
[0010] Step 3. Perform interpolation calculation on the weld temperature data obtained by the infrared detector to generate a weld temperature distribution cloud map and mark the locations with large temperature deviations;
[0011] Step 4. Use the pre-designed welding wire replacement and delivery device to automatically replace and deliver welding materials;
[0012] Step 5. First weld the base weld of the groove on one side of the composite layer, then shovel the root from the back to fill the back groove, and finally weld the transition layer and composite layer weld until the front base part between the two stainless steel composite plates is welded.
[0013] Furthermore, in step 1, the setting expression of the width of the groove is:
[0014]
[0015] Among them, W is the groove width, d is the electrode diameter, H is the penetration depth, ρ is the density of the molten metal, g is the gravitational acceleration, P is the welding energy, and α is the empirical coefficient.
[0016] Furthermore, in step 2, the adjustment expression of the arc length is:
[0017]
[0018] Wherein, L is the length of the arc, U is the arc voltage, I is the arc current, π is the circumference, D is the diameter of the welding wire, and R is the resistivity of the welding wire;
[0019] The linear velocity is expressed as:
[0020]
[0021] Among them, V is the linear velocity, β is the empirical coefficient, D is the wire diameter, π is the circumference, n is the wire feeding speed, and r is the rotation radius.
[0022] Furthermore, in step 3, the expression of the temperature distribution cloud map is:
[0023]
[0024] Where, T is the temperature, E is the emissivity of the object, t is the response time of the thermal imager, A is the mirror area of the thermal imager, and I is the emissivity of the radiation source.
[0025] Furthermore, in step 3, the formula for interpolating the weld temperature data obtained by the infrared detector is:
[0026] T interp =Interpolation(T ori ,ΔT,α,T amb ,T base ,R update ,autoWeight)
[0027] Among them, T interp is the temperature value obtained by interpolation, Interpolation(.) is the interpolation function, T ori is the original temperature data, ΔT is the temperature difference, α is the temperature correction coefficient, T amb is the ambient temperature, T base is the reference temperature value, R update To dynamically update the neighborhood radius, autoWeight is the adaptive weight.
[0028] Furthermore, in step 5, the step of first welding the base weld of the groove on one side of the composite layer, then shoveling the root from the back side to fill the back groove, and finally welding the transition layer and the composite layer weld further comprises:
[0029] Use titanium alloy or nickel-based alloy filling materials to fill the back groove. After the front base part is welded, spray anti-corrosion coating around the transition layer weld for strengthening.
[0030] Furthermore, the distance from the end of the welding wire to the root of the groove is automatically detected by a laser radar device, and the distance is used as the initial arc length;
[0031] Perform adaptive analysis based on the initial arc length and preset welding control parameters to generate a welding gun height adjustment strategy;
[0032] According to the welding gun height adjustment strategy, an instruction is issued to the welding gun motion mechanism to adaptively adjust the welding gun height to ensure that the arc length between the welding wire and the workpiece is always maintained within a preset range during the welding process.
[0033] Furthermore, the welding gun height adjustment strategy is specifically as follows:
[0034]
[0035] Where D is the arc length monitored in real time, D preset is the preset arc length, and the tolerance is the acceptable range of the arc length, which is used to determine whether the arc length is within the ideal range. When the real-time monitored arc length D is greater than the preset arc length D preset When the arc length is greater than or equal to the preset arc length D preset The difference with the tolerance and less than or equal to the preset arc length D preset When the arc length D is less than the preset arc length D preset If the difference is within the tolerance, raise the height of the welding gun.
[0036] Furthermore, according to the three-dimensional coordinates of the groove root and the vertical distance between the bottom of the welding gun and the groove root, the Z-direction coordinates of the bottom of the welding gun at each welding point are calculated, and the Z-direction coordinates of the welding point are:
[0037] Z i =Zp i +ΔZ
[0038] Among them, Zq i is the Z coordinate of the bottom of the welding gun at the ith welding point, Zp i is the Z coordinate of the root of the i-th groove, ΔZ is the fixed vertical distance between the bottom of the welding gun and the root of the groove;
[0039] A corresponding relationship curve is drawn between the Z-axis coordinate of the welding point and the corresponding groove root coordinate, and the groove position coordinates that need to be adjusted for the welding gun position are determined according to the corresponding relationship curve.
[0040] According to another aspect of the present invention, there is provided a stainless steel composite plate intelligent submerged arc welding system, comprising:
[0041] A welding preparation module is used to process a groove at the welding position of the stainless steel composite plate to be welded, and set two reference points at the end of the groove, wherein the width of the groove is set according to the electrode diameter, the penetration depth, the density of the molten metal and the welding energy;
[0042] An arc length adjustment module is used to use a laser tracker or a high-precision 3D scanner to perform groove detection to obtain 3D data, and to adjust the arc length and line speed in real time during the welding process to reduce defects and fluctuations in the welding process, wherein the arc length is adjusted according to the arc voltage, arc current and welding wire parameters;
[0043] The temperature distribution cloud map generation module is used to interpolate the weld temperature data obtained by the infrared detector, generate the weld temperature distribution cloud map, and mark the positions with large temperature deviations;
[0044] A welding material handling module, which is used to automatically change and distribute welding materials using a pre-designed welding wire changing and distribution device;
[0045] The weld filling module is used to first weld the base weld of the groove on one side of the composite layer, then shovel the root from the back to fill the back groove, and finally weld the transition layer and composite layer weld until the front base part between the two stainless steel composite plates is welded.
[0046] According to the scheme provided by the present invention, step 1. processing a groove at the welding position of the stainless steel composite plate to be welded, and setting two reference points at the end position of the groove, wherein the width of the groove is set according to the electrode diameter, the penetration depth, the density of the molten metal and the welding energy; step 2. using a laser tracker or a high-precision three-dimensional scanner to detect the groove to obtain three-dimensional data, and adjusting the length and line speed of the arc in real time during the welding process to reduce defects and fluctuations in the welding process, wherein the length of the arc is adjusted according to the arc voltage, the arc current and the welding wire parameters; step 3. interpolating the weld temperature data obtained by the infrared detector to generate a weld temperature distribution cloud map, and marking the position with a large temperature deviation; step 4. using a pre-designed welding wire replacement and delivery device to automatically replace and deliver welding materials; step 5. first weld the base weld of the groove on one side of the composite layer, then shovel the root from the back to fill the back groove, and finally weld the transition layer and the composite layer weld until the front base part between the two stainless steel composite plates is welded. The present invention improves welding accuracy by adjusting the length and line speed of the arc in real time, provides welding guidance by marking positions with large temperature deviations, and makes the entire welding process more flexible and efficient. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:
[0048] Figure 1 A schematic diagram showing a flow chart of an intelligent submerged arc welding method for a stainless steel composite plate according to an embodiment of the present invention;
[0049] Figure 2 A schematic diagram showing the structure of an intelligent submerged arc welding system for stainless steel composite plates according to an embodiment of the present invention DETAILED DESCRIPTION
[0050] The exemplary embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present invention are shown in the accompanying drawings, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present invention and to enable the scope of the present invention to be fully communicated to those skilled in the art.
[0051] Figure 1 The schematic diagram of the process of the intelligent submerged arc welding method of the stainless steel composite plate according to the embodiment of the present invention is shown. Specifically, the following steps are included:
[0052] Step S101, processing a groove at a welding position of a stainless steel composite plate to be welded, and setting two reference points at the end position of the groove.
[0053] In this embodiment, two stainless steel composite plates to be welded are selected to ensure that their surfaces are clean and free of impurities. For example, a cutting machine or a plasma cutting machine is used to process a groove at the welding position, and the depth and width of the groove can be adjusted according to actual needs. At the end of the groove, two reference points are set using a marking pen or drilling, and the function of the reference points is to determine the position and angle of the welding gun to ensure the accuracy and stability of the welding process. Then, the two stainless steel composite plates are assembled as needed, and fixed on the workbench using a fixture or bracket or other fixing device to ensure that the position and angle of the composite plate are accurate. Place the welding gun at the end of the groove so that the wire outlet of the welding gun is aligned with the two reference points. By adjusting the angle and position of the welding gun, the welding wire can smoothly fill the groove.
[0054] The width of the groove is set according to the electrode diameter, penetration, density of molten metal and welding energy. Among them, the size of the electrode diameter directly affects the distribution and conduction of the welding current, which in turn affects the penetration and flow of the molten metal. The penetration is the depth to which the molten metal diffuses on the parent material during welding. The required penetration can be set by adjusting parameters such as welding current, welding time, and electrode pressure. The density of the molten metal affects its fluidity and filling effect during welding. Therefore, when setting the groove width, it is necessary to consider the density of the material used and its changes during welding. Welding energy refers to the total energy input into the welding zone during welding. It can be determined by calculating arc heat, resistance heat, etc. The calculation of welding energy helps to better control the welding process and weld quality. The width of the groove is set by the electrode diameter, penetration, density of molten metal and welding energy to obtain better welding results.
[0055] Furthermore, the setting expression of the width of the groove is:
[0056]
[0057] Among them, W is the groove width, d is the electrode diameter, H is the penetration depth, ρ is the density of the molten metal, g is the gravitational acceleration, P is the welding energy, and α is the empirical coefficient.
[0058] Too large groove width leads to increased processing difficulty and material waste, while too small groove width affects welding quality and reliability. The groove width needs to consider the interaction between multiple factors to obtain better welding results. Substituting the collected or measured electrode diameter, penetration, molten metal density, and welding energy into the above formula can calculate the groove width.
[0059] Step S102, using a laser tracker or a high-precision 3D scanner to perform groove detection to obtain 3D data, and adjusting the arc length and line speed in real time during the welding process to reduce defects and fluctuations in the welding process.
[0060] Specifically, according to the shape and size of the groove to be inspected, install the laser tracker or 3D scanner in a suitable position to ensure that the equipment can capture the complete groove surface and cover the required measurement range. According to the material, size and accuracy requirements of the groove, set the relevant parameters of the laser tracker or 3D scanner. For example, measurement range, resolution, measurement accuracy, etc. Start the laser tracker or 3D scanner to scan and measure the groove, which will automatically collect the surface point cloud data of the groove and generate a 3D model.
[0061] According to the three-dimensional data or model of the groove detection, the initial arc length and line speed parameters are set. During the welding process, the arc length and line speed are monitored in real time using sensors or monitoring systems. When defects or fluctuations are detected, the arc length and line speed are automatically adjusted to reduce defects and fluctuations in the welding process and maintain the stability and consistency of the welding process.
[0062] In this embodiment, the length of the arc is adjusted according to the arc voltage, arc current and welding wire parameters. During the welding process, real-time monitoring of the arc voltage and current can reflect the burning state and energy distribution of the arc. Parameters such as the diameter and material of the welding wire will also affect the length of the arc. The best combination of arc voltage, current and welding wire parameters can be determined through experiments and verification. By continuously adjusting and optimizing these parameters, the arc length adjustment scheme that best suits specific materials and process conditions can be found.
[0063] Furthermore, the adjustment expression of the arc length is:
[0064]
[0065] Among them, L is the length of the arc, U is the arc voltage, I is the arc current, π is pi, D is the wire diameter, and R is the resistivity of the wire. The length L of the arc refers to the distance between the two ends of the arc (between the electrode and the welding material) when the arc is burning, which is an important factor in the stability of arc burning and welding quality. The arc voltage U refers to the voltage difference between the two ends of the arc, which has a certain relationship with the arc length and usually increases with the increase of the arc length. The arc current I is the current value flowing through the arc, and its size directly affects the heat input of welding, thereby affecting the quality and efficiency of welding. The wire diameter D is the cross-sectional diameter of the welding wire. The size of the wire diameter affects the heat input, penetration depth and weld width during welding. The resistivity R of the welding wire is used to measure the conductive performance of the welding wire, expressed in Ω·mm 2 / m is the unit, which affects the combustion and thermal efficiency of the arc, thus affecting the welding process and results. The above parameters are interrelated and jointly affect the welding process and results.
[0066] The linear velocity is expressed as:
[0067]
[0068] Where V is the wire speed, β is the empirical coefficient, D is the wire diameter, π is the circumference, n is the wire feeding speed, and r is the rotation radius. The wire speed V refers to the speed at which the wire moves along the welding direction, which determines the welding efficiency and is an important parameter for controlling welding quality and efficiency. The empirical coefficient β is used to adjust and optimize other parameters in the welding process and is determined based on actual welding experience. The wire diameter D is the cross-sectional diameter of the wire, which determines the heat input, penetration depth, and weld width during welding. The wire feeding speed n is the speed at which the wire is fed into the arc, which is related to the wire speed and can be controlled by adjusting the wire feeding speed. The rotation radius r refers to the distance from the center of the wire to the axis of rotation when the welding torch is rotated or swung, which determines parameters such as penetration depth and weld width. An appropriate wire speed can help maintain the stability of the welding process and reduce the occurrence of defects and problems. By controlling the wire speed, the length and shape of the weld can be accurately controlled, thereby reducing the use and waste of materials and helping to reduce production costs.
[0069] Step S103, interpolating the weld temperature data acquired by the infrared detector to generate a weld temperature distribution cloud map, and marking the positions with large temperature deviations.
[0070] Specifically, an infrared detector is used to scan around the weld to obtain temperature data at various locations of the weld. The infrared detector generates a two-dimensional array containing temperature data, in which each element represents the temperature value of a pixel. The acquired temperature data is preprocessed, including removing outliers and smoothing, to improve the accuracy of subsequent interpolation calculations. An appropriate interpolation algorithm (such as linear interpolation, polynomial interpolation, spline interpolation, etc.) is used to interpolate the preprocessed temperature data to generate a more accurate temperature distribution cloud map. The goal of the interpolation calculation is to estimate the temperature distribution of the entire weld area based on known temperature data points. The temperature data obtained by the interpolation calculation is visualized to generate a weld temperature distribution cloud map. The temperature distribution cloud map can be displayed in two-dimensional or three-dimensional form, where color or grayscale indicates the temperature, and different colors or grayscale levels correspond to different temperature ranges. In the temperature distribution cloud map, the location with large temperature deviation is identified by the difference in color or grayscale level. According to the identified location with large temperature deviation, combined with the temperature distribution cloud map, the temperature distribution of the weld is analyzed. For areas with large temperature deviations, adjust welding process parameters (such as current, voltage, welding speed, etc.) to optimize the welding process and improve welding quality.
[0071] Furthermore, the expression of the temperature distribution cloud map is:
[0072]
[0073] Where, T is the temperature, E is the emissivity of the object, t is the response time of the thermal imager, A is the mirror area of the thermal imager, and I is the emissivity of the radiation source.
[0074] In this embodiment, temperature T represents the physical quantity of the thermal state or heat of the object, reflecting the heat distribution of the weld and its surrounding areas. The emissivity E of the object represents the ability of the surface of the object to radiate energy. Different materials have different emissivities, and the emissivity of the same material may also change at different temperatures and surface conditions. The response time t of the thermal imager is the time interval from the thermal imager receiving radiation to outputting the measurement results. The response time affects the thermal imager's ability to capture rapid temperature changes. The mirror area A of the thermal imager is the area where the thermal imager receives radiation, which affects the total amount of radiation received and thus affects the measured temperature value. The emissivity I of the radiation source represents the energy intensity radiated outward by the radiation source, which is related to the temperature and emissivity.
[0075] Furthermore, the formula for interpolating the weld temperature data obtained by the infrared detector is:
[0076] T interp =Interpolation(T ori ,ΔT,α,T amb ,T base ,R update,autoWeight)
[0077] Among them, T interp is the temperature value obtained by interpolation, Interpolation(.) is the interpolation function, T ori is the original temperature data, ΔT is the temperature difference, α is the temperature correction coefficient, T amb is the ambient temperature, T base is the reference temperature value, R update To dynamically update the neighborhood radius, autoWeight is the adaptive weight. interp The result obtained by processing the weld temperature data through the interpolation algorithm is used to estimate the temperature distribution in the weld area. Interpolation(.) is used to interpolate the temperature data to generate a more accurate temperature distribution cloud map. Common interpolation algorithms include linear interpolation, polynomial interpolation, spline interpolation, etc. ori The original temperature data obtained by the infrared detector can be represented in the form of a two-dimensional array, where each element represents the temperature value of a pixel. The temperature difference ΔT represents the difference between the temperatures at two different times or different locations, and is used to evaluate temperature changes or analyze the unevenness of temperature distribution. The temperature correction coefficient α is used to correct the original temperature data to eliminate the influence of environmental factors, instrument errors, etc. on the measurement results, and improve the accuracy and reliability of the temperature data. Ambient temperature value T amb It indicates the temperature of the surrounding environment during measurement, which affects the measurement results of the infrared detector. The ambient temperature can be used as a reference value for correction. base Indicates the temperature of a fixed reference point. In weld temperature analysis, the reference temperature value is used to evaluate whether the temperature distribution of the weld meets the process requirements. Dynamically update the neighborhood radius R update It can be dynamically adjusted according to actual needs and algorithm logic to achieve more accurate temperature analysis. Adaptive weight autoWeigh t To more accurately estimate the temperature distribution of the weld to process temperature data at different locations.
[0078] Step S104, using the pre-designed welding wire replacement and delivery device to automatically replace and deliver welding materials.
[0079] Specifically, first, a device capable of automatically replacing and distributing welding wire is designed, for example, a storage device for storing welding wire, a material taking device for taking out welding wire from the storage device, and a distributing device for distributing welding wire to welding equipment. The above device can be realized by using existing technology through the automatic operation of the control system control device, which is not limited in this article. For example, the welding wire is placed in the storage device so that the welding wire can be continuously supplied during the continuous welding process. When the welding wire needs to be replaced, the material taking device automatically takes out new welding wire from the storage device. The material taking device should ensure that the welding wire can be continuously and stably supplied. The distributing device automatically distributes the taken welding wire to the welding equipment. The distributing device ensures that the welding wire can be accurately delivered to the welding position. The control system ensures the continuity and stability of the welding process by setting the time interval and quantity for automatically replacing and distributing the welding wire. The above device can improve welding efficiency, reduce manual intervention, and ensure the stability of welding quality.
[0080] Step S105, first weld the base weld of the groove on one side of the composite layer, then scrape the root from the back to fill the back groove, and finally weld the transition layer and the composite layer weld until the front base part between the two stainless steel composite plates is welded.
[0081] Specifically, ensure that the two stainless steel composite plates are butted flat and without gaps. If there are gaps, they need to be filled or adjusted to ensure the welding quality. Starting from the composite side, the base part can be welded using the welding process of the base weld (such as submerged arc welding, gas shielded welding, etc.). After the base weld is welded, the root is shoveled from the back. The purpose of shoveling is to remove the weld root of the base weld so that the base and the composite can be better combined. After the root is shoveled, the back groove is filled with suitable filling materials (such as welding wire, welding rod, etc.). During the filling process, ensure that the filling material is well fused with the base and composite materials, without defects such as pores and slag inclusions. After the back groove is filled, start welding the transition layer and the composite weld. The purpose of the transition layer is to make a smooth transition between the base and the composite and reduce stress concentration. After the transition layer and the composite weld are welded, the welding of the front base part is completed. The above steps can ensure the welding quality of the stainless steel composite plate and improve its overall performance and service life.
[0082] Furthermore, the method of first welding the base weld of the groove on one side of the composite layer, then shoveling the root from the back side to fill the back groove, and finally welding the transition layer and the composite layer weld further includes:
[0083] Use titanium alloy or nickel-based alloy filling materials to fill the back groove. After the front base part is welded, spray anti-corrosion coating around the transition layer weld for strengthening.
[0084] In this embodiment, since titanium alloy and nickel-based alloy have excellent welding performance and corrosion resistance, they are used as filling materials. According to the material and welding requirements of the stainless steel composite plate, suitable titanium alloy or nickel-based alloy filling materials are selected. When filling the back groove, an appropriate welding process (such as tungsten inert gas arc welding, metal arc gas shielded welding, etc.) can be used to melt the titanium alloy or nickel-based alloy filling material into the back groove. Ensure that the filling material is well fused with the base and the composite material, without defects such as pores and slag inclusions. According to the order of welding the base weld first, shoveling the root, filling the back groove, welding the transition layer and the composite weld, the welding of the front base part is completed to ensure that the entire welding area is defect-free and leak-free. After the welding of the front base part is completed, an anti-corrosion coating is sprayed around the transition layer weld. Select suitable anti-corrosion coating materials, such as anti-rust paint, galvanizing, etc., to ensure that the coating is uniform and continuous, and can effectively isolate the base and the composite material to prevent the intrusion of corrosive media. After spraying the anti-corrosion coating, the transition layer weld is strengthened around the weld, such as local heat treatment, machining or adding reinforcing ribs, to improve the fatigue resistance and structural stability of the weld.
[0085] Furthermore, the distance from the end of the welding wire to the root of the groove is automatically detected by a laser radar device, and the distance is used as the initial arc length;
[0086] Perform adaptive analysis based on the initial arc length and preset welding control parameters to generate a welding gun height adjustment strategy;
[0087] According to the welding gun height adjustment strategy, an instruction is issued to the welding gun motion mechanism to adaptively adjust the welding gun height to ensure that the arc length between the welding wire and the workpiece is always maintained within a preset range during the welding process.
[0088] Specifically, an adaptive analysis is performed based on the initial arc length and preset welding control parameters. The adaptive analysis includes the evaluation of arc stability, the analysis of the relationship between wire feeding speed and current and voltage, etc., and a welding gun height adjustment strategy is generated based on the results of the adaptive analysis. For example, if the arc length becomes shorter, the welding gun height needs to be increased, and vice versa, the welding gun height needs to be lowered. The generated welding gun height adjustment strategy is converted into a specific instruction and sent to the welding gun motion mechanism through the control system. The welding gun motion mechanism can be a mechanical arm, an electric slide, or other forms of motion devices.
[0089] Furthermore, the welding gun height adjustment strategy is specifically as follows:
[0090]
[0091] Where D is the arc length monitored in real time, D presetis the preset arc length, and the tolerance is the acceptable range of the arc length, which is used to determine whether the arc length is within the ideal range. When the real-time monitored arc length D is greater than the preset arc length D preset When the arc length is greater than or equal to the preset arc length D preset The difference with the tolerance and less than or equal to the preset arc length D preset When the arc length D is less than the preset arc length D preset When the difference between the welding gun and the tolerance is exceeded, the height of the welding gun is raised to increase the arc length. During the entire welding process, by monitoring the change in arc length, the height of the welding gun can be adjusted in real time according to the adjustment strategy.
[0092] Furthermore, according to the three-dimensional coordinates of the groove root and the vertical distance between the bottom of the welding gun and the groove root, the Z-direction coordinates of the bottom of the welding gun at each welding point are calculated, and the Z-direction coordinates of the welding point are:
[0093] Z i =Zp i +ΔZ
[0094] Among them, Zq i is the Z coordinate of the bottom of the welding gun at the ith welding point, Zp i is the Z coordinate of the root of the i-th groove, ΔZ is the fixed vertical distance between the bottom of the welding gun and the root of the groove;
[0095] A corresponding relationship curve is drawn between the Z-axis coordinate of the welding point and the corresponding groove root coordinate, and the groove position coordinates that need to be adjusted for the welding gun position are determined according to the corresponding relationship curve.
[0096] Specifically, a measuring tool or sensor is used to obtain the X, Y, and Z coordinate values of the root of the groove at the i-th welding point, and the coordinate value is the position of the groove on the workpiece. According to preset or known parameters, a fixed vertical distance between the bottom of the welding gun and the root of the groove is determined to ensure that the relative position of the welding gun and the workpiece is stable during welding. The height of the welding gun is adjusted according to the calculated Z-direction coordinate of the bottom of the welding gun to ensure that the arc length is within a preset range, thereby improving the welding quality. The Z-direction coordinate of the bottom of the welding gun and the corresponding Z-direction coordinate of the root of the groove are collected at each welding point. The collected data are plotted into a scatter plot or a curve graph using a drawing tool or software. According to the distribution of the data points, a suitable curve function (such as a linear equation, a quadratic equation, etc.) is selected for fitting to describe the corresponding relationship between the Z-direction coordinates of the bottom of the welding gun and the root of the groove. According to the standard or preset threshold of the fitting curve, it is judged whether each welding point deviates from the expected corresponding relationship. For example, if the actual Z-direction coordinate of the bottom of the welding gun is significantly different from the coordinate value predicted by the fitting curve, it is considered that the point deviates from the expected position. According to the deviation, determine the groove position coordinates where the welding gun position needs to be adjusted. These coordinate points may be the positions where the actual Z-axis coordinates of the bottom of the welding gun differ greatly from the expected values. According to the determined groove position coordinates, adjust the height of the welding gun or other related parameters to correct the deviation. For example, recalculate the Z-axis coordinates of the bottom of the welding gun and adjust the welding gun position accordingly. Among them, Zq i is the Z-coordinate of the bottom of the welding gun at the ith welding point, indicating the vertical position of the bottom of the welding gun at the ith welding point. It determines the vertical position of the welding gun. By adjusting Zq i The length of the arc can be precisely controlled. i is the Z-axis coordinate of the root of the i-th groove, which indicates the Z-axis coordinate value of the groove root at the i-th welding point, that is, the position on the workpiece where welding is to begin. The groove root is where welding begins, so its Z-axis coordinate determines the relative position of the arc and the workpiece, thereby affecting the welding quality. By adjusting Zp i It can ensure that the arc is correctly aligned with the groove, improving the reliability and strength of the welded joint. ΔZ is the fixed vertical distance between the bottom of the welding gun and the root of the groove, indicating the fixed vertical distance between the bottom of the welding gun and the root of the groove. It is used to ensure that the relative position between the welding gun and the workpiece remains unchanged during the welding process, providing stable welding conditions. By maintaining a fixed vertical distance, the arc length during the welding process can be ensured to be consistent, improving welding quality and efficiency.
[0097] According to the scheme provided by the present invention, step 1. processing a groove at the welding position of the stainless steel composite plate to be welded, and setting two reference points at the end position of the groove, wherein the width of the groove is set according to the electrode diameter, the penetration depth, the density of the molten metal and the welding energy; step 2. using a laser tracker or a high-precision three-dimensional scanner to detect the groove to obtain three-dimensional data, and adjusting the length and line speed of the arc in real time during the welding process to reduce defects and fluctuations in the welding process, wherein the length of the arc is adjusted according to the arc voltage, the arc current and the welding wire parameters; step 3. interpolating the weld temperature data obtained by the infrared detector to generate a weld temperature distribution cloud map, and marking the position with a large temperature deviation; step 4. using a pre-designed welding wire replacement and delivery device to automatically replace and deliver welding materials; step 5. first weld the base weld of the groove on one side of the composite layer, then shovel the root from the back to fill the back groove, and finally weld the transition layer and the composite layer weld until the front base part between the two stainless steel composite plates is welded. The present invention improves welding accuracy by adjusting the length and line speed of the arc in real time, provides welding guidance by marking positions with large temperature deviations, and makes the entire welding process more flexible and efficient.
Claims
1. An intelligent submerged arc welding method for stainless steel composite plates, characterized in that: include: Step 1: Processing a groove at the welding position of the stainless steel composite plate to be welded, and setting two reference points at the end of the groove, wherein the width of the groove is set according to the electrode diameter, the penetration depth, the density of the molten metal and the welding energy; The setting expression of the width of the groove is: Where W is the groove width, d is the electrode diameter, H is the penetration depth, ρ is the density of the molten metal, g is the gravitational acceleration, P is the welding energy, and α is the empirical coefficient; Step 2: Use a laser tracker or a high-precision 3D scanner to detect the groove to obtain 3D data, and adjust the arc length and line speed in real time during the welding process to reduce defects and fluctuations in the welding process, wherein the arc length is adjusted according to the arc voltage, arc current and welding wire parameters; The adjustment expression of the arc length is: Wherein, L is the length of the arc, U is the arc voltage, I is the arc current, π is the circumference, D is the diameter of the welding wire, and R is the resistivity of the welding wire; The linear velocity is expressed as: Wherein, V is the linear velocity, β is the empirical coefficient, D is the wire diameter, π is the circumference, n is the wire feeding speed, and r is the rotation radius; Step 3: Perform interpolation calculation on the weld temperature data obtained by the infrared detector to generate a weld temperature distribution cloud map and mark the locations with large temperature deviations; The expression of the temperature distribution cloud diagram is: Where, T is temperature, E is the emissivity of the object, t is the response time of the thermal imager, A is the mirror area of the thermal imager, and I is the emissivity of the radiation source; The formula for interpolating the weld temperature data obtained by the infrared detector is: T interp =Interpolation(T ori ,ΔT,α,T amb ,T base ,R update ,autoWeight) Among them, T interp is the temperature value obtained by interpolation, Interpolation(.) is the interpolation function, T ori is the original temperature data, ΔT is the temperature difference, α is the temperature correction coefficient, T amb is the ambient temperature, T base is the reference temperature value, R update To dynamically update the neighborhood radius, autoWeight is the adaptive weight, T interp The result obtained by processing the weld temperature data through the interpolation algorithm is used to estimate the temperature distribution in the weld area; Step 4: Use the pre-designed welding wire replacement and delivery device to automatically replace and deliver welding materials; Step 5: First weld the base weld of the groove on one side of the composite layer, then shovel the root from the back to fill the back groove, and finally weld the transition layer and composite layer weld until the front part between the two stainless steel composite plates is welded; In step 5, the step of first welding the base weld of the groove on one side of the composite layer, then shoveling the root from the back side to fill the back groove, and finally welding the transition layer and the composite layer weld further comprises: Use titanium alloy or nickel-based alloy filler materials to fill the back groove. After the front part is welded, spray anti-corrosion coating around the transition layer weld for strengthening treatment. The distance from the end of the welding wire to the root of the groove is automatically detected by a laser radar device, and the distance is used as the initial arc length; Perform adaptive analysis based on the initial arc length and preset welding control parameters to generate a welding gun height adjustment strategy; Sending instructions to the welding gun motion mechanism according to the welding gun height adjustment strategy to adaptively adjust the welding gun height to ensure that the arc length between the welding wire and the workpiece is always within a preset range during welding; The welding gun height adjustment strategy is specifically as follows: Where D is the arc length monitored in real time, D preset is the preset arc length, and the tolerance is the acceptable range of the arc length, which is used to determine whether the arc length is within the ideal range. When the real-time monitored arc length D is greater than the preset arc length D preset When the arc length is greater than or equal to the preset arc length D preset The difference with the tolerance and less than or equal to the preset arc length D preset When the arc length D is less than the preset arc length D preset If the difference is within the tolerance, raise the height of the welding gun.
2. An intelligent submerged arc welding system for stainless steel composite plates, the system is based on the intelligent submerged arc welding method for stainless steel composite plates according to claim 1, characterized in that: include: A welding preparation module is used to process a groove at the welding position of the stainless steel composite plate to be welded, and set two reference points at the end of the groove, wherein the width of the groove is set according to the electrode diameter, the penetration depth, the density of the molten metal and the welding energy; An arc length adjustment module is used to use a laser tracker or a high-precision 3D scanner to perform groove detection to obtain 3D data, and to adjust the arc length and line speed in real time during the welding process to reduce defects and fluctuations in the welding process, wherein the arc length is adjusted according to the arc voltage, arc current and welding wire parameters; The temperature distribution cloud map generation module is used to perform interpolation calculation on the weld temperature data obtained by the infrared detector, generate a weld temperature distribution cloud map, and mark the positions with large temperature deviations; A welding material handling module for automatically changing and dispensing welding materials using a pre-designed welding wire changing and dispensing device; The weld filling module is used to first weld the base weld of the groove on one side of the composite layer, then shovel the root from the back to fill the back groove, and finally weld the transition layer and composite layer weld until the front part between the two stainless steel composite plates is welded.