A silicon wafer anodic bonding device and bonding method thereof

By using heating disks, bonding trays and connecting springs in the anode bonding device of the silicon wafer, combined with the electric field, the problem of low success rate of silicon wafer anode bonding in the prior art is solved, and efficient silicon wafer bonding is achieved. Reduces equipment modification costs.

CN117963836BActive Publication Date: 2024-12-06SUZHOU SENWAN ELECTRONICS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410152349.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-02-03
Publication Date
2024-12-06
Estimated Expiration
2044-02-03

AI Technical Summary

Technical Problem

In the prior art, the anode bonding success rate of silicon wafers is low and the equipment modification cost is high, making it difficult to achieve side lead connection of silicon wafers, especially when the thickness of the intermediate silicon wafer is less than 100um.

Method used

Design an anode bonding device for silicon wafers, including a heating plate, a bonding tray and a connecting spring. By setting holes on the first glass sheet, the connecting spring comes into contact with the silicon wafer, and a second time is achieved under the action of heating and electric field. The bonding of glass sheets and silicon wafers increases the bonding success rate.

Benefits of technology

It improves the success rate of the second bonding of the silicon wafer, reduces the equipment transformation cost, and has a simple structure, which is suitable for the anode bonding operation of thin silicon wafers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117963836B_ABST
    Figure CN117963836B_ABST
Patent Text Reader

Abstract

The present invention discloses an anode bonding device and a bonding method for a silicon wafer, belonging to the technical field of silicon wafer bonding. A first glass sheet has been bonded to one surface of the silicon wafer, and the bonding device bonds a second glass sheet to the other surface of the silicon wafer. The second glass sheet is connected to a cathode, and a hole is provided on the first glass sheet. The bonding device includes a heating plate, a bonding tray, and a connecting spring. The bonding tray is connected to the anode, and the connecting spring is installed on the bonding tray. The connecting spring extends into the hole and contacts the silicon wafer. After power is turned on, the silicon wafer, the connecting spring, and the bonding tray form a bonding path. The present invention uses a bonding tray as an intermediate piece, and a hole is provided on the first glass sheet, so that the silicon wafer and the bonding tray are in a connected state under the action of the connecting spring, and the bonding tray is connected to the anode, and the second glass sheet is connected to the cathode, which is conducive to the smooth progress of the second bonding operation of the silicon wafer and greatly improves the bonding efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of silicon wafer bonding, and in particular relates to an anodic bonding device for a silicon wafer and a bonding method thereof. Background Art

[0002] At present, glass-silicon-glass three-layer anodic bonding is used in microfluidic chips, MEMS, inertial sensors and pressure devices. The glass-silicon-glass three-layer structure needs to undergo two anodic bondings. The first bonding is to bond a piece of glass to one side of the silicon wafer, and the second bonding is to bond another piece of glass to the other side of the silicon wafer. At this time, the anodic bonding of the glass-silicon-glass structure is completed.

[0003] For the anodic bonding of glass-silicon wafer-glass structure, the current existing technology is to achieve it through the common anode method, that is, the middle silicon wafer lead is connected to the anode, and the upper and lower glass wafers are connected to the cathode to achieve common anode one-time bonding. There is currently no ready-made equipment for this method, and the thickness of the middle silicon wafer is 100um or even less than 50um, so it is extremely difficult to set the lead connection on the side of the silicon wafer, and it is impossible to use equipment to achieve the anodic bonding operation of the silicon wafer. Its bonding success rate is extremely low. If the equipment is modified, the modification cost is extremely high, and its bonding success rate cannot be guaranteed. Summary of the invention

[0004] The present invention overcomes the deficiencies of the prior art and provides an anodic bonding device for a silicon wafer and a bonding method thereof to solve the problems existing in the prior art.

[0005] To achieve the above-mentioned purpose, the technical solution adopted by the present invention is: an anode bonding device for a silicon wafer, a first glass sheet has been bonded to one surface of the silicon wafer, the bonding device bonds a second glass sheet to the other surface of the silicon wafer, the second glass sheet is connected to the cathode, the first glass sheet is provided with a hole, the bonding device includes a heating plate, a bonding tray and a connecting spring, the bonding tray is connected to the anode, the connecting spring is installed on the bonding tray, the connecting spring extends into the hole and contacts the silicon wafer, after power is turned on, the silicon wafer, the connecting spring and the bonding tray form a bonding path.

[0006] In a preferred embodiment of the present invention, the heating plate is connected to the bonding tray.

[0007] In a preferred embodiment of the present invention, the bonding tray and the connecting spring are both conductive metal parts.

[0008] In a preferred embodiment of the present invention, the connecting spring is fixedly mounted on the bonding tray.

[0009] In a preferred embodiment of the present invention, the number of the holes is at least two, and they are located at two ends of the first glass sheet.

[0010] In a preferred embodiment of the present invention, the diameter of the hole is larger than the diameter of the connecting spring.

[0011] The present invention also discloses a method for anodic bonding of a silicon wafer, comprising the following steps:

[0012] S1, drilling a hole in the ineffective area of ​​the first glass sheet, wherein the position of the hole corresponds to the position of the connecting spring;

[0013] S2, anodically bonding the first glass sheet to the silicon sheet to complete the first bonding process of the silicon sheet. At this time, the first glass sheet is bonded to one surface of the silicon sheet;

[0014] S3, performing metal patterning on the non-bonded surface of the first glass sheet, so that the metal structure formed at the hole position of the first glass sheet is connected to the silicon sheet to form a circuit conduction structure;

[0015] S4, thinning the silicon wafer after the metal patterning process, and performing deep silicon etching on the silicon wafer after thinning to make a sensitive structure layer;

[0016] S5. Attach the second glass sheet to the other side of the silicon wafer, connect the fixture of the bonding device to the metal structure after the metal patterning process, make the circuit conductive, and perform a second bonding on the silicon wafer.

[0017] In a preferred embodiment of the present invention, the metal structure is a conductive metal member.

[0018] The present invention solves the defects existing in the background technology and has the following beneficial effects:

[0019] (1) The present invention uses a bonding tray as an intermediate piece, and sets a hole on the first glass sheet so that the silicon wafer and the bonding tray are connected under the action of a connecting spring, and the bonding tray is connected to the anode, and the second glass sheet is connected to the cathode. Under the heating action of the heating plate and the action of the electric field, the anodic bonding process is completed, which is conducive to the smooth progress of the second bonding operation of the silicon wafer and greatly improves the bonding success rate;

[0020] (2) The present invention has a simple structure and low cost, and does not require large-scale modification of the equipment, thereby effectively reducing costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] The present invention is further described below in conjunction with the accompanying drawings and embodiments;

[0022] Figure 1 It is a schematic diagram of the overall structure of a preferred embodiment of the present invention;

[0023] Figure 2 A cross-sectional view of a preferred embodiment of the present invention;

[0024] Figure 3 This is a schematic structural diagram of a first glass sheet in a preferred embodiment of the present invention;

[0025] Figure 4 This is a schematic structural diagram of a bonding tray according to a preferred embodiment of the present invention;

[0026] Figure 5 A flowchart of a preferred embodiment of the present invention;

[0027] In the figure: 10, silicon wafer; 20, first glass sheet; 21, hole position; 30, second glass sheet; 40, heating plate; 50, bonding tray; 60, connecting spring. DETAILED DESCRIPTION

[0028] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention.

[0029] Embodiment 1

[0030] The present embodiment provides an anodic bonding device for a silicon wafer. A first glass sheet 20 has been bonded to one surface of the silicon wafer 10. The bonding device bonds a second glass sheet 30 to the other surface of the silicon wafer 10, thereby completing the anodic bonding process of the silicon wafer 10. The present device can make the second bonding operation of the silicon wafer 10 proceed more smoothly, greatly improving the bonding success rate of the silicon wafer 10.

[0031] Combination Figures 1 to 4 As shown, the second glass sheet 30 of this embodiment is connected to the cathode, and a hole 21 is provided on the first glass sheet 20. The bonding device includes a heating plate 40, a bonding tray 50 and a connecting spring 60. The bonding tray 50 is connected to the anode, and the connecting spring 60 is installed on the bonding tray 50. The connecting spring 60 extends into the hole 21 and contacts the silicon wafer 10. After power is turned on, the silicon wafer 10, the connecting spring 60 and the bonding tray 50 form a bonding path. This embodiment uses the bonding tray 50 as an intermediate piece, and a hole 21 is provided on the first glass sheet 20, so that the silicon wafer 10 and the bonding tray 50 are connected under the action of the connecting spring 60, and the bonding tray 50 is connected to the anode, and the second glass sheet 30 is connected to the cathode, so as to ensure that the second bonding operation of the silicon wafer 10 is carried out smoothly and improve the bonding efficiency of the silicon wafer 10.

[0032] In this embodiment, the first glass sheet 20 is firstly punched before the first bonding. The hole 21 is located in the ineffective area of ​​the first glass sheet 20 and will not affect the bonding quality of the silicon wafer 10 .

[0033] Furthermore, the heating plate 40 is connected to the bonding tray 50. In this embodiment, the heating plate 40 is connected to the bonding tray 50. The heating plate 40 can heat the silicon wafer 10 through the bonding tray 50, further promoting the bonding of the second glass sheet 30, and having a high-temperature bonding effect on the bonding of the silicon wafer 10, thereby ensuring the bonding success of the silicon wafer 10.

[0034] In this embodiment, the bonding tray 50 and the connecting spring 60 are both conductive metal parts. After power is turned on, the silicon wafer 10, the connecting spring 60, and the bonding tray 5 form a bonding path. Through the action of the electric field and high temperature, the second bonding operation of the silicon wafer 10 is realized. In this embodiment, copper parts are used as the bonding tray 50 and the connecting spring 60 to ensure that the silicon wafer 10, the connecting spring 60, and the bonding tray 5 form a bonding path after power is turned on.

[0035] like Figure 4 As shown, the connection spring 60 is fixedly mounted on the bonding tray 50 , so that the connection spring 60 stably connects the bonding tray 50 and the silicon wafer 10 to form a stable bonding path.

[0036] In this embodiment, there are at least two holes 21, which are arranged at both ends of the first glass sheet 20. The hole diameter of the hole 21 is larger than the diameter of the connecting spring 60. The number of the holes 21 corresponds to the connecting spring 60 one by one. The connecting spring 60 passes through the hole 21 and contacts the silicon sheet 10 to form a stable bonding path.

[0037] In actual use, the anodic bonding device for silicon wafers of this embodiment has completed the first bonding of the first glass sheet 20 on one side of the silicon wafer 10, and the first glass sheet 20 has completed the punching operation before the first bonding, and a hole 21 has been formed in the invalid area of ​​the first glass sheet 20. Then, the second glass sheet 30 needs to be bonded to the other side of the silicon wafer 10. First, the second glass sheet 30 is attached to the other side of the silicon wafer 10, and at the same time, the connecting spring 60 on the bonding tray 50 is extended into the hole 21 of the first glass sheet 20, so that the silicon wafer 10, the connecting spring 60, and the bonding tray 50 form a bonding path, and the bonding tray 50 is connected to the anode, and the second glass sheet 30 is connected to the cathode. After power is turned on, the bonding operation of the second glass sheet 30 is performed under the action of the electric field and the high temperature generated by the heating plate 40. After the bonding is completed, the heating plate 40, the bonding tray 50 and the connecting spring 60 can be removed.

[0038] In this embodiment, the sizes of the heating plate 40 and the bonding tray 50 can be adjusted according to the sizes of the silicon wafer 10 , the first glass wafer 20 , and the second glass wafer 30 , so as to improve the adaptability of the bonding device.

[0039] Embodiment 2

[0040] like Figure 5As shown, this embodiment discloses a method for anodic bonding of a silicon wafer, comprising the following steps:

[0041] S1. Punch a hole in the invalid area of ​​the first glass sheet 20. The formed hole position 21 corresponds to the position of the connecting spring 60. In this embodiment, laser punching is used to form the hole position 21 in the invalid area of ​​the first glass sheet 20. The hole diameter of the hole position 21 is larger than the diameter of the connecting spring 60, and the coordinates of the hole position 21 and the connecting spring 60 are consistent;

[0042] S2, anodically bonding the first glass sheet 20 and the silicon wafer 10 to complete the first bonding process of the silicon wafer 10. At this time, the first glass sheet 20 is bonded to one surface of the silicon wafer 10. Specifically, the first glass sheet 20 and the silicon wafer 10 are placed on an anodic bonding device, the first glass sheet 20 is connected to the negative electrode, and the silicon wafer 10 is connected to the positive electrode. Under the heating action of the heating plate 40 and the action of the electric field, the anodic bonding process of the first glass sheet 20 and the silicon wafer 10 is completed, so that the first glass sheet 20 is bonded to one surface of the silicon wafer 10;

[0043] S3, performing metal patterning on the non-bonded surface of the first glass sheet 20, so that the metal structure formed at the hole position 21 of the first glass sheet 20 is connected to the silicon sheet 10, forming a circuit conduction structure, so that the subsequent second bonding operation can be smoothly carried out;

[0044] S4, thinning the silicon wafer 10 after the metal patterning process, and performing deep silicon etching on the silicon wafer 10 after thinning to make a sensitive structure layer. In this embodiment, CMP thinning is performed on the silicon wafer 10 after the first bonding to be less than 100 um;

[0045] S5. Attach the second glass sheet 30 to the other side of the silicon wafer 10, connect the fixture of the bonding device to the metal structure after the metal patterning process, make the circuit conductive, and perform the second bonding on the silicon wafer 10. In this embodiment, the second glass sheet 30 is connected to the negative electrode, and the bonding tray 50 is connected to the positive electrode, so that the silicon wafer 10, the connecting spring 60, and the bonding tray 50 form a bonding path, and the anodic bonding process of the second glass sheet 30 is completed under the heating action of the heating plate 40 and the action of the electric field.

[0046] In this embodiment, the metal structure used in step S3 is a conductive metal member, which may be copper or silver.

[0047] Obviously, the above embodiments are merely examples for clear explanation and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived from these are still within the protection scope of the invention.

Claims

1. A method for anodic bonding of silicon wafers, using an anodic bonding device for silicon wafers, characterized in that: After the first glass sheet (20) is bonded to one surface of the silicon wafer (10), the bonding device bonds the second glass sheet (30) to the other surface of the silicon wafer (10), the second glass sheet (30) is connected to the cathode, the first glass sheet (20) is provided with a hole (21), the bonding device comprises a heating plate (40), a bonding tray (50) and a connecting spring (60), the bonding tray (50) is connected to the anode, the connecting spring (60) is installed on the bonding tray (50), the connecting spring (60) extends into the hole (21) and contacts the silicon wafer (10), after power is turned on, the silicon wafer (10), the connecting spring (60) and the bonding tray (50) form a bonding path, and the anode bonding method of the silicon wafer comprises the following steps: S1, drilling a hole in the ineffective area of ​​the first glass sheet (20), wherein the position of the formed hole (21) corresponds to the position of the connecting spring (60); S2, anodically bonding the first glass sheet (20) to the silicon sheet (10), completing the first bonding process of the silicon sheet (10), wherein the first glass sheet (20) is bonded to one surface of the silicon sheet (10); S3, performing metal patterning on the non-bonded surface of the first glass sheet (20), so that the metal structure formed at the hole position (21) of the first glass sheet (20) is connected to the silicon sheet (10), thereby forming a circuit conduction structure; S4, thinning the silicon wafer (10) after the metal patterning process, and after thinning, performing deep silicon etching on the silicon wafer (10) to form a sensitive structure layer; S5, attaching the second glass sheet (30) to the other surface of the silicon wafer (10), connecting the fixture of the bonding device to the metal structure after the metal patterning process, making the circuit conductive, and performing a second bonding on the silicon wafer (10).

2. The method for anodic bonding of silicon wafers according to claim 1, characterized in that: The heating plate (40) is connected to the bonding tray (50).

3. The method for anodic bonding of silicon wafers according to claim 1, characterized in that: The bonding tray (50) and the connecting spring (60) are both conductive metal parts.

4. The method for anodic bonding of silicon wafers according to claim 1, characterized in that: The connecting spring (60) is fixedly mounted on the bonding tray (50).

5. The method for anodic bonding of silicon wafers according to claim 1, characterized in that: The number of the holes (21) is at least two, and they are arranged at two ends of the first glass sheet (20).

6. The method for anodic bonding of silicon wafers according to claim 1, characterized in that: The hole diameter of the hole (21) is larger than the diameter of the connecting spring (60).

7. The method for anodic bonding of silicon wafers according to claim 1, characterized in that: In step S3, the metal structure is a conductive metal part.