Welding method using temperature and gas molecule quantity adjustment in chamber

By adjusting the temperature and the number of gas molecules in the chamber, the problem of bubbles during the welding process is solved, achieving high coverage and low bubble rate, and improving heat dissipation performance.

CN118081014BActive Publication Date: 2024-10-22ELEAD TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410479780.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-22
Publication Date
2024-10-22
Estimated Expiration
2044-04-22

AI Technical Summary

Technical Problem

The volatilization of flux in existing welding technology results in a large number of bubbles at the welding interface, which affects the heat dissipation efficiency.

Method used

By adjusting the temperature and the number of gas molecules in the chamber, controlled changes in heat and pressure are achieved, bubbles in the welding medium are removed, and high coverage and low bubble rates are achieved.

Benefits of technology

It effectively removes bubbles in the welding medium, improves the heat dissipation effect and product yield, improves the coverage of the welding medium and the heat dissipation performance of the components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118081014B_ABST
    Figure CN118081014B_ABST
Patent Text Reader

Abstract

The present application discloses a welding method using the temperature and the number of gas molecules in a chamber to be adjusted. The welding method may include: arranging a first component and a second component to be welded in a chamber, wherein the first component and the second component are pre-connected using a welding medium; adjusting the temperature and the number of gas molecules in the chamber to achieve a heat change in the chamber and a cyclic change in the number of gas molecules to solidify the welding medium to complete the welding of the first component and the second component; wherein the heat change causes the temperature in the chamber to continuously change between rising and falling, and the cyclic change causes the pressure in the chamber to change between positive pressure and negative pressure at intervals.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of industrial manufacturing, and in particular to a welding method and a packaged chip utilizing the adjustment of the temperature in a chamber and the number of gas molecules. Background Art

[0002] In recent years, with the high development of chip integration, chip power consumption and power density have also become higher and higher. The accompanying heat problem has gradually become the main reason limiting chip performance and life. In order to enable the chip to have good heat dissipation, the prior art often uses heat dissipation interface materials to coat the chip surface and then bond the heat dissipation cover. This process can be called welding. At present, flux is usually added during welding, and the volatilization of the solvent contained in the flux will cause a large number of bubbles to exist at the welding interface, which will eventually affect the heat dissipation efficiency.

[0003] Therefore, a new welding method is urgently needed to solve the bubble problem during the welding process. Summary of the invention

[0004] In order to solve the above technical problems, the present application provides a welding method by adjusting the temperature and the number of gas molecules in the chamber, and a packaged chip prepared based on the method. The welding method can achieve high coverage and low bubble rate of the welding medium, and obtain excellent heat dissipation performance.

[0005] In one aspect, the present application provides a welding method by adjusting the temperature and the number of gas molecules in a chamber. The welding method may include: arranging a first component and a second component to be welded in a chamber, wherein the first component and the second component are pre-connected using a welding medium; adjusting the temperature and the number of gas molecules in the chamber to achieve a heat change in the chamber and a cyclic change in the number of gas molecules to solidify the welding medium to complete the welding of the first component and the second component; wherein the heat change causes the temperature in the chamber to continuously change between rising and falling, and the cyclic change causes the pressure in the chamber to change between positive pressure and negative pressure at intervals.

[0006] In some feasible implementations, the continuous change of the temperature in the chamber between rising and falling may include the temperature first rising and then falling over time; wherein the temperature rising process includes a constant temperature stage.

[0007] In some possible implementations, the pressure in the chamber varying between positive pressure and negative pressure at intervals may include varying the pressure between positive pressure and negative pressure over time.

[0008] In some feasible implementations, when the pressure in the chamber is at a negative pressure, the vacuum degree in the chamber may change continuously in multiple stages.

[0009] In some feasible implementations, the multiple continuous changes may cause the vacuum degree to continuously increase and then decrease; the continuous changes that cause the vacuum degree to increase may include decreasing the initial vacuum degree to an intermediate vacuum degree and then increasing to a target vacuum degree.

[0010] In some feasible implementations, when the pressure in the chamber is at the last time of the interval change, it may include maintaining a predetermined positive pressure until the welding is completed.

[0011] In some feasible implementations, the pressure in the chamber maintains a predetermined positive pressure until the welding is completed, and the temperature may include a process of continuously decreasing until the welding is completed.

[0012] In some feasible implementations, when the pressure in the chamber is positive pressure, the positive pressure may be no less than 2 atm.

[0013] In some feasible implementations, the first component may include a chip, the second component may include a heat dissipation cover plate, and the welding medium may include flux and a heat dissipation interface material.

[0014] On the other hand, the present application further provides a packaged chip, which can be prepared by the above-mentioned welding method.

[0015] The implementation of this application has the following beneficial effects:

[0016] The welding method provided in the present application utilizes adjusting the temperature and the number of gas molecules in the chamber to achieve regulated changes in the heat and pressure in the chamber by adjusting the temperature and the number of gas molecules in the chamber, thereby being able to effectively remove bubbles generated by the welding medium during the welding process, thereby achieving high coverage and low bubble rate of the components, improving the heat dissipation effect, and increasing the product yield. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The present application will be further described in the form of exemplary embodiments, which will be described in detail by way of the accompanying drawings. These embodiments are not restrictive, and in these embodiments, the same number represents the same structure, wherein:

[0018] Figure 1 is an exemplary flow chart of a welding method using adjustment of the number of gas molecules in a chamber according to some embodiments of the present application;

[0019] Figure 2 is an exemplary waveform diagram of temperature and pressure changes according to some embodiments of the present application;

[0020] Figure 3 is a scanned image of a welding interface according to some embodiments of the present application;

[0021] Figure 4 is another scanned image of a welding interface according to some embodiments of the present application;

[0022] Figure 5 A scanning diagram of the welding interface obtained by the prior art is shown;

[0023] Figure 6 Another scan of the welding interface obtained by the prior art is shown. DETAILED DESCRIPTION

[0024] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation of the present application is described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present application, so the present application is not limited by the specific embodiments disclosed below.

[0025] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.

[0026] In the prior art, vacuum reflow soldering equipment is often used to solder components. Vacuum reflow soldering equipment can be equipped with multiple chambers. Each chamber has a preset temperature, which can also be called a temperature zone. Different vacuum reflow equipment has different numbers of temperature zones, which can be roughly divided into 7-13 temperature zones, including a vacuum temperature zone and a cooling temperature zone set after the vacuum temperature zone). The products to be soldered will be placed on a chain conveyor belt and enter each temperature zone in turn. By controlling the conveyor belt chain speed, the residence time of the product in each temperature zone can be indirectly controlled. After the product enters the vacuum temperature zone, the chamber door of the vacuum temperature zone is closed to form a closed space to achieve the purpose of vacuum extraction. After the vacuum stage ends, the chamber door opens and the product continues to flow to the next temperature zone. After solidification is completed in the cooling temperature zone, the product flows out from the discharge port of the equipment and the welding is completed.

[0027] At present, the products prepared by vacuum reflow soldering equipment have a bubble rate of more than 6%, and cannot achieve the heat dissipation function of the product well.

[0028] On the one hand, the present application provides a welding method by adjusting the number of gas molecules in a chamber, which can achieve high coverage and low bubble rate of welding products. Figure 1 ,like Figure 1As shown, the welding method may include the following steps.

[0029] Step 110 , placing a first component and a second component to be welded in a chamber.

[0030] In some feasible implementations, the chamber can be airtight, and the temperature and pressure in the chamber can be adjusted. Exemplarily, the chamber can have an openable and closable door panel. Opening or closing the door panel can make the chamber communicate with the outside world, or be airtight. The chamber can have and / or be externally connected to a heating / cooling component and / or a gas flow path. The temperature in the chamber can be adjusted by the heating / cooling component, and the pressure in the chamber can be adjusted by the gas flow path. Alternatively, the gas flow path can be provided with a circulation pipeline, and a cooling device such as a condenser and a power device such as a fan or a pump are provided on the circulation pipeline. The gas in the chamber circulates in the circulation pipeline under the action of the power device, and the cooling device cools down the circulating gas.

[0031] In some feasible implementations, the first element and the second element may be pre-connected using a welding medium. Exemplarily, the first element may include a chip, and the second element may include a heat dissipation cover plate. The heat dissipation cover plate may be made of metal materials with excellent thermal conductivity such as copper, aluminum, iron, zinc, nickel, titanium, etc. or alloys, ceramic materials such as alumina, zirconium oxide, etc., polymer materials such as polyimide, polyamic acid ester, etc., carbon materials such as graphite, carbon fiber, etc. By welding the heat dissipation cover plate to the top of the chip, rapid heat conduction of the chip is achieved to reduce the temperature of the chip. The welding medium may include a heat dissipation interface material, for example, a silicone-type thermal conductive material such as thermal conductive silicone grease, a metal heat sink such as an indium sheet, etc. These heat dissipation interface materials can fix the first element and the second element in certain circumstances, and at the same time serve as a heat dissipation bridge between the two.

[0032] In a feasible implementation, the welding medium may include flux. The flux may be contained in or coated on the heat dissipation interface material. Exemplarily, when a metal heat sink is used as the heat dissipation interface material, the flux may be coated on the surface of the metal heat sink. A method of using the welding medium to achieve a pre-connection between the first component and the second component may be to first coat the surface of the chip with flux to form a first flux layer. Subsequently, the heat dissipation interface material is coated or mounted on the first flux layer, and after completion, flux is coated on the surface of the heat dissipation interface material to form a second flux layer. The heat dissipation cover plate will be installed on the second flux layer to complete the pre-connection between the first component and the second component. In this way, after the curing of the welding medium is completed in the subsequent process, the welding of the components can be achieved, which effectively improves the heat dissipation efficiency of the first component, such as a chip.

[0033] Step 120, adjusting the temperature and the number of gas molecules in the chamber to achieve heat changes in the chamber and cyclic changes in the number of gas molecules to solidify the welding medium to complete welding of the first component and the second component.

[0034] In some feasible implementations, the temperature in the chamber can be adjusted by adjusting the heating / cooling components of the chamber, thereby achieving heat changes in the chamber. For example, the heating coil or hot water pipe surrounding the chamber can apply heat to the chamber by heat conduction to achieve an increase in the temperature in the chamber. At the same time, a cooling component such as a cooling water circulation device or a gas flow path can absorb and dissipate the heat in the chamber to achieve a decrease in the temperature in the chamber. In some feasible implementations, the heat change in the chamber can cause the temperature in the chamber to continuously change between rising and falling. Exemplarily, during the entire welding process, the temperature in the chamber may first rise and then fall over time. The rise in temperature can cause the welding medium to reach a suitable melting point to form a co-metal interface and bond more tightly, and the drop in temperature can cause the welding medium to begin to cool and solidify, thereby achieving a fixed connection between components.

[0035] It is understandable that the solvent of the flux will volatilize during the heating process to generate gas, thus forming bubbles inside the welding medium. The generation of bubbles will affect the final welding quality and thermal conductivity. In short, the more bubbles there are, the lower the thermal conductivity. In the present application, the removal of bubbles can be achieved by adjusting the temperature inside the chamber and the number of gas molecules. In some feasible implementations, the number of gas molecules in the chamber can be changed cyclically by filling a predetermined amount of gas molecules into the chamber and / or extracting gas molecules from the chamber through a gas flow path. The cyclic change can make the number of gas molecules in the chamber change between increase and decrease. That is, over time, the number of gas molecules in the chamber can increase first, then decrease, then increase again, and then decrease in such a pattern. Reflected in the pressure in the chamber, the pressure can change between positive pressure and negative pressure over time. In the positive pressure stage, the number of gas molecules introduced can make the pressure of the chamber not less than 2atm. For example, 2atm, 3atm, 5atm, 8atm, etc. The increase in the number of gas molecules in the chamber can squeeze the welding medium, thereby squeezing out the bubbles from the welding medium. On the other hand, smaller bubbles can be dissolved in the welding medium under the squeezing of a large number of gas molecules, thereby achieving the purpose of ablation. The reduction in the number of gas molecules in the chamber can reduce the obstruction of gas molecules in the environment, making it easier for the gas molecules that constitute the bubbles to be taken away. The purpose of bubble removal is achieved in two aspects.

[0036] refer to Figure 2 , Figure 2is an exemplary waveform diagram of the temperature and pressure changes inside the chamber according to some embodiments of the present application. Figure 2 As shown, Pc represents the pressure curve in the chamber, Tc represents the temperature curve in the chamber, and P0 represents the ambient atmospheric pressure. Exemplarily, as time t passes, the temperature in the chamber may rise over time. The temperature rise process may include a stage in which the temperature is maintained stable. The gas molecules in the chamber may be extracted from the chamber through the gas flow path in the chamber. For example, when the pre-connected first component and the second component are placed in the chamber, oxygen molecules will enter the chamber. If deoxidation is not performed, these oxygen molecules will have an adverse effect on the welding process, such as the welding metal will be oxidized to form oxides, which will affect the welding quality. Therefore, the process of extracting the gas molecules in the chamber and then extracting them after the gas molecules are introduced can achieve effective removal of oxygen molecules. In some feasible implementations, the gas molecules introduced into the chamber may be protective gas molecules, such as nitrogen molecules, argon molecules, etc.

[0037] The increase in temperature can preheat the welding medium. For example, the heat dissipation interface material is preheated and the soldering flux is activated. The activation of the soldering flux will volatilize the solvent, which will be removed from the chamber during the step of adjusting the number of gas molecules (for example, extracting gas molecules to cause the pressure in the chamber to drop). For example, the regulation of the heat in the chamber can be first adjusted so that the temperature in the chamber rises to T1, and T1 can be higher than or equal to the activation starting point of the soldering flux to activate the soldering flux. At the same time, T1 is lower than the melting point of the heat dissipation interface material. In this way, the solvent begins to volatilize while the soldering flux is activated, while the heat dissipation interface material remains in a solid state. As a result, no bubbles will enter the heat dissipation medium, which is convenient for removal in the process of reducing the gas molecules in the chamber.

[0038] Return to reference Figure 2 , the heat applied to the interior of the chamber can continue to increase over time, so that the temperature inside the chamber continues to rise. For example, the temperature is raised to T2. T2 can exceed the melting point of the heat dissipation interface material, so that the heat dissipation interface material can be transformed into a molten state to better connect the components. For example, the indium sheet is wetted in a molten state, thereby forming a co-metal interface to achieve a good welding effect in the subsequent process.

[0039] In this process, the number of gas molecules inside the chamber can still be varied at intervals, so that the pressure inside the chamber changes between positive pressure and negative pressure, achieving better bubble removal. In some feasible implementations, when the number of gas molecules in the chamber causes the chamber to be in a negative pressure state, the vacuum degree in the chamber can be a multi-stage continuous change. The multi-stage continuous change can be a change in the vacuum degree between two values, or it can be a change in the vacuum degree that maintains the same trend in each stage of change, for example, decreases, increases, and / or maintains. In some feasible implementations, the multi-stage continuous change can cause the vacuum degree in the chamber to continue to increase and then decrease. For example, the vacuum degree can increase in each stage of change other than the final stage, and decrease in the final stage of change. In some feasible implementations, the continuous increase in the vacuum degree can be a decrease from the initial vacuum degree to the intermediate vacuum degree and then increase to the target vacuum degree. The pressure in the chamber is expressed in Torr. Obviously, 760Torr is the ambient atmospheric pressure. In one variation, assuming that the initial vacuum is 300Torr, some gas molecules can be introduced first to reduce the vacuum to an intermediate vacuum of 350Torr. The intermediate vacuum can be maintained or not maintained, and then the gas molecules can be extracted outside the chamber to increase the vacuum to 250Torr to reach the target vacuum. In the present application, the number of gas molecules that causes the pressure in the chamber to be negative is adjusted. On the one hand, it is avoided that the continuous extraction of gas molecules causes the overflow of the heat dissipation interface material to cause contamination. On the other hand, the reduction of the vacuum can realize the function of "backfilling of thermal conductive materials" through the principle of pressure difference, so that bubbles escape from the heat dissipation interface material and are subsequently removed during the extraction of gas molecules.

[0040] In some feasible implementations, the last time the interval change of the pressure in the chamber caused by the regulation of the number of gas molecules in the chamber can include a stage in which the positive pressure in the chamber is achieved and maintained, and continues until the end of welding. Correspondingly, the regulation of the heat in the chamber can cause the temperature in the chamber to include a process of continuous decrease until the end of welding. That is, in the process of temperature drop to solidify the molten heat dissipation interface material, the positive pressure is still maintained inside the chamber. While maintaining high pressure, if there are still bubbles in the heat dissipation interface material, these bubbles will be compressed to a very small size. Then they are confined in the solid structure during the cooling and solidification process. On the other hand, under the action of high pressure, the bubbles can also be compressed to move in the molten heat dissipation interface material, and then escape from the boundary to further remove bubbles.

[0041] Another aspect of the present application provides a packaged chip, which can be prepared by the above-mentioned welding method.

[0042] The welding method disclosed in the present application utilizes the method of adjusting the temperature and the number of gas molecules in the chamber, and the packaged chip prepared by the welding method, which is used for connecting components, can achieve a high heat conduction welding medium with a high surface coverage rate on the component and a low bubble rate, and can achieve excellent heat dissipation performance.

[0043] refer to Figures 3 to 6 , Figure 3 and Figure 4 is a scanned image of a welding interface according to some embodiments of the present application, Figure 5 and Figure 6 FIG. 1 shows a scanning diagram of the welding interface obtained by the prior art. Figure 3 As shown in the figure, it shows the bubble rate of the welding interface. The bubble rates of the three examples are 0.01%, 0.65% and 0.20 respectively. All are less than 1%. This is much smaller than Figure 5 The soldering interface of the product prepared by the vacuum reflow soldering equipment shown has a bubble rate of less than 10%. Figure 4 The coverage of the welding interface of the three examples is 98.2%, 96.71% and 98.7%, which is much higher than Figure 6 The prior art shown results in products with less than 90% coverage of the weld interface.

[0044] It can be seen that compared with the prior art, the welding process provided by the present application can effectively remove the bubbles generated by the solvent of the flux during the welding process, and improve the coverage rate of the heat dissipation medium.

[0045] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0046] The above-described embodiments only express several implementations of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be noted that, for a person of ordinary skill in the art, several variations and improvements may be made without departing from the concept of the present application, and these all fall within the scope of protection of the present application. Therefore, the scope of protection of the present patent application shall be subject to the attached claims.

[0047] The basic concepts have been described herein. It is obvious to those skilled in the art that the above detailed disclosure is merely an example and does not constitute a limitation of this specification. Although not explicitly stated herein, those skilled in the art may make various modifications, improvements and amendments to this specification. Such modifications, improvements and amendments are suggested in this specification, so such modifications, improvements and amendments still fall within the spirit and scope of the exemplary embodiments of this specification.

[0048] It should be noted that in order to simplify the description disclosed in this specification and thus help understand one or more application embodiments, in the above description of the embodiments of this specification, multiple features are sometimes combined into one embodiment, figure or description thereof. However, this disclosure method does not mean that the features required by the object of this specification are more than the features mentioned in the claims. In fact, the features of the embodiments are less than all the features of the single embodiment disclosed above.

[0049] In some embodiments, numbers describing the number of components and attributes are used. It should be understood that such numbers used in the description of the embodiments are modified by the modifiers "about", "approximately" or "substantially" in some examples. Unless otherwise specified, "about", "approximately" or "substantially" indicate that the numbers are allowed to vary by ±20%. Accordingly, in some embodiments, the numerical parameters used in the specification and claims are approximate values, which may change according to the required features of individual embodiments. In some embodiments, the numerical parameters should take into account the specified significant digits and adopt the general method of retaining the digits. Although the numerical domains and parameters used to confirm the breadth of the range in some embodiments of this specification are approximate values, in specific embodiments, the setting of such numerical values ​​is as accurate as possible within the feasible range.

[0050] Finally, it should be understood that the embodiments described in this specification are only used to illustrate the principles of the embodiments of this specification. Other variations may also fall within the scope of this specification. Therefore, as an example and not a limitation, alternative configurations of the embodiments of this specification may be considered consistent with the teachings of this specification. Accordingly, the embodiments of this specification are not limited to the embodiments explicitly introduced and described in this specification.

Claims

1. A welding method utilizing the adjustment of the temperature in the chamber and the number of gas molecules, characterized in that: The welding method comprises: Disposing a first component and a second component to be welded in a chamber, wherein the first component and the second component are pre-connected using a welding medium; The temperature and the number of gas molecules in the chamber are adjusted to achieve heat changes in the chamber and cyclic changes in the number of gas molecules so that the welding medium is solidified to complete the welding of the first component and the second component; wherein the heat changes cause the temperature in the chamber to continuously change between rising and falling, and the cyclic changes cause the pressure in the chamber to change between positive pressure and negative pressure at intervals; the pressure in the chamber changes between positive pressure and negative pressure at intervals, including: the pressure changes between positive pressure and negative pressure over time; and when the pressure in the chamber is at negative pressure, the vacuum degree in the chamber changes continuously in multiple stages; the multiple continuous changes cause the vacuum degree to increase continuously and then decrease; the continuous changes that cause the vacuum degree to increase include: decreasing from an initial vacuum degree to an intermediate vacuum degree and then increasing to a target vacuum degree.

2. The welding method according to claim 1, characterized in that: The temperature in the chamber changes continuously between rising and falling, including: the temperature first rises and then falls over time; wherein the temperature rising process includes a constant temperature stage.

3. The welding method according to claim 1, characterized in that: When the pressure in the chamber is at the last time of the interval change, the pressure is maintained at a predetermined positive pressure until the welding is completed.

4. The welding method according to claim 3, characterized in that: The pressure in the chamber maintains a predetermined positive pressure until the welding is finished, and the temperature includes a process of continuously decreasing until the welding is finished.

5. The welding method according to claim 1, characterized in that: When the pressure in the chamber is positive pressure, the positive pressure is not less than 2 atm.

6. The welding method according to any one of claims 1 to 5, characterized in that: The first component includes a chip, the second component includes a heat dissipation cover plate, and the welding medium includes soldering flux and heat dissipation interface material.

7. A packaged chip, characterized in that: The welding method is prepared by adjusting the temperature in the chamber and the number of gas molecules as described in any one of claims 1 to 6.