A personalized customized planting base and a manufacturing method thereof
By collecting and judging the humidity and temperature data on the surface of the planting base, spraying and re-spraying adjustments, the problem of uneven coating spray thickness is solved, the mechanical performance and stability of the planting base are improved, and product quality is ensured. Security.
Patent Information
- Application Number
- CN202410496715.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-24
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-04-24
AI Technical Summary
During the manufacturing process of planting abutment, the uniformity and qualification rate of the spray thickness cannot be guaranteed during the coating spraying process, which affects the service life and safety of the abutment.
By designing the base, processing the base, surface treatment, chemical treatment and inspection and testing methods, the humidity and temperature data of the base surface are collected, and whether it meets the spraying standards are met, spraying treatment is carried out, and spraying thickness is ensured through re-spraying and data adjustment. Improve uniformity and consistency of spraying within the preset range.
The uniformity and qualification rate of the surface spraying thickness of the planting abutment are achieved, the mechanical properties and stability of the abutment are improved, and the quality and safety of the product are ensured.
Smart Images

Figure CN118304023B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of manufacturing a planting base, and in particular to a personalized customized planting base and a manufacturing method thereof. Background Art
[0002] The implant abutment is the basic structure that connects the external crown and the implant, and has the function of retention and stability. It is a very important component in the dental implant system, which can provide stability and support for the implant, improve chewing function, and increase the aesthetics of the oral cavity;
[0003] Patients with missing teeth require not only functional restoration, but also aesthetic and convenience. Implant restoration has become a common restoration method for patients with missing teeth due to its good retention, high chewing efficiency, and aesthetic and comfortable appearance. The abutment is an important part of the implant restoration system, which plays the role of connecting the implant and the upper restoration;
[0004] During the manufacturing process of the implant abutment, it is necessary to ensure the stability and safety of the implant abutment during use. Therefore, the surface of the implant abutment needs to be sprayed with a coating during the production process to ensure the service life and safety and stability of the implant abutment during subsequent use. However, during the coating spraying process, the uniformity of the spraying thickness and the pass rate cannot be guaranteed. Summary of the invention
[0005] The purpose of the present invention is to provide a method for manufacturing a personalized customized implant base to solve the above-mentioned problems.
[0006] The purpose of the present invention can be achieved through the following technical solutions:
[0007] A method for manufacturing a personalized customized planting base, comprising:
[0008] Step 1: Design the abutment: determine the abutment material and design the abutment size according to the implant plan and tooth model;
[0009] Step 2: Processing the abutment: cutting, grinding and polishing the abutment material;
[0010] Step 3: Surface treatment: spray the surface of the base;
[0011] The method comprises: S1: collecting data on the state value of the surface of the base platform to obtain a surface humidity value Sd and a surface temperature value Wd of the surface of the base platform;
[0012] S2: Compare the surface humidity value Sd with the humidity threshold Sdy;
[0013] And determine whether the surface temperature value Wd is within the temperature value range [Wdx, Wdy];
[0014] Obtain a base platform whose surface state value meets the spraying standard, and spray the coating through the surface spraying equipment;
[0015] S3: Obtain the spraying thickness value Hp of the base surface; and make a judgment;
[0016] If Hp<Hpx, it means the spraying fails to meet the standard;
[0017] If Hpy<Hp, it means overspray;
[0018] If the spraying thickness value Hp is within the preset spraying thickness range [Hpx, Hpy], it means that the spraying is qualified;
[0019] S4: If the spraying fails to meet the standard, the surface of the base is sprayed again to obtain a base with qualified surface spraying; and the spraying data is stored and adjusted;
[0020] If the amount of spraying is excessive, it indicates that the base is unqualified;
[0021] Step 4: Chemical treatment: Surface treatment such as oxidation and melting is performed to improve its biocompatibility and wear resistance;
[0022] Step 5: Inspection and testing: Conduct quality inspection and performance testing on the base to ensure that it meets the design requirements and is safe to use.
[0023] As a further solution of the present invention: in said S2;
[0024] If the surface humidity value Sd is greater than or equal to the humidity threshold Sdy, it means that the surface humidity is too high and humidity intervention adjustment is required;
[0025] If the surface humidity value Sd is less than the humidity threshold Sdy, it means that the surface humidity meets the standard, and it is determined whether the surface temperature value Wd is within the temperature range [Wdx, Wdy].
[0026] As a further solution of the present invention: in S2:
[0027] If the surface temperature value Wd is not within the temperature range [Wdx, Wdy], it means that the surface temperature is unqualified and temperature intervention adjustment is required;
[0028] If the surface temperature value Wd is within the temperature value range [Wdx, Wdy], it means that the temperature meets the standard.
[0029] As a further solution of the present invention: in S4, the step of performing supplementary spraying on the surface of the base comprises:
[0030] V1: Calculate the difference in thickness Hpc of the spray coating on the base surface;
[0031] V2: Get the spraying time value Tp of the base surface; calculate the supplementary spraying time Tbp based on the difference of the spraying thickness on the base surface;
[0032] V3: Perform re-spraying on the surface of the base platform based on the re-spraying time Tbp; after the re-spraying is completed, obtain the re-spraying value Hbp of the spraying thickness on the surface of the base platform; and then execute S3.
[0033] As a further solution of the present invention: in the V1, the calculation method of the difference Hpc of the spraying thickness on the surface of the base is: Hpc=Hpx-Hp.
[0034] As a further solution of the present invention: in V2, the calculation method of the base surface spraying time Tbp is:
[0035] As a further solution of the present invention: in S4, the step of adjusting the spraying data includes:
[0036] W1: Get the final value of surface spraying thickness Hzp and the final value of surface spraying time Tzp;
[0037] W2: Based on the spraying rate value Ls and the spraying temperature value Wd; the final value of the surface spraying thickness Hzp and the final value of the surface spraying time Tzp are inserted into k=Hzp-Ls×Tzp to calculate the correction coefficient k;
[0038] W3: Calculate the relationship between the surface spray thickness value Hp and the spray time value Tp when the spray temperature value Wd is obtained;
[0039] Hp=Ls×Tp+k; wherein k is the correction coefficient.
[0040] As a further solution of the present invention: in S4, if it is indicated that the base is unqualified, the coating sprayed on the surface is removed and re-sprayed.
[0041] As a further solution of the present invention: a personalized customized planting base, the personalized customized planting base is prepared by the above-mentioned manufacturing method.
[0042] Beneficial effects of the present invention:
[0043] In the present invention, in the process of spraying the surface of the planting base, the spraying time of the coating is obtained based on the preset thickness of the spray coating, and then the spraying is carried out. After the spraying is completed, the thickness of the spray coating is detected to obtain the surface coating thickness value, and it is determined whether the surface coating thickness value is within the surface spraying thickness value range. If the surface spraying thickness is unqualified, the surface of the planting base is reprocessed to ensure that the surface thickness of the planting base meets the standard spraying thickness. In addition, in the working process, according to the surface spraying data of the completed planting base, the surface spraying data that does not meet the standard in the initial spraying can be updated, that is, the preset spraying time in the system is updated to ensure that in the subsequent surface spraying process of the planting base, a planting base with qualified surface spraying can be obtained quickly and effectively. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] The present invention will be further described below in conjunction with the accompanying drawings.
[0045] Figure 1 It is a schematic flow chart of the method of the present invention;
[0046] Figure 2 It is a system block diagram of the surface spraying system in the present invention. DETAILED DESCRIPTION
[0047] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0048] See also Figure 1 As shown, the present invention is a method for manufacturing a personalized customized planting base, comprising:
[0049] Step 1: Design the abutment: determine the abutment material and design the abutment size according to the implant plan and tooth model;
[0050] Step 2: Processing the abutment: cutting, grinding and polishing the abutment material;
[0051] Step 3: Surface treatment: spray the surface of the abutment; during the spraying process, the surface of the abutment needs to be cleaned and degreased, and the surface needs to be kept dry and free of foreign matter, and then the surface of the abutment needs to be sprayed. The thickness of the coating needs to be ensured during the spraying process, because the coating thickness has an important influence on the performance and service life of the abutment. Too thick a coating will cause cracking, falling off and other problems, while too thin a coating may not achieve the desired protective effect. Therefore, it is extremely important to control the thickness of the coating and ensure uniformity and consistency during the spraying process;
[0052] In addition, it should be noted that during the spraying process, the spraying temperature, spraying humidity and spraying rate will have a certain impact on the spraying effect;
[0053] During the spraying process, the spraying data is acquired and the spraying results are tested to improve the subsequent spraying time to meet the design requirements of the spraying;
[0054] Step 4: Chemical treatment: Surface treatment such as oxidation and melting is performed to improve its biocompatibility and wear resistance;
[0055] Step 5: Inspection and testing: Conduct quality inspection and performance testing on the base to ensure that it meets the design requirements and is safe to use.
[0056] In the process of making customized planting bases, the planting base is first designed, and then machined to obtain a planting base base with qualified structure. The surface characteristics and performance of the planting base are improved by surface spraying, thereby improving the mechanical properties and stability of the planting base. The sprayed coating is then oxidized and melted to better ensure the stability between the soil layer and the planting base. Finally, it can be inspected and tested.
[0057] The implant base prepared by the above method has good surface stability and better adaptability, which improves the safety of the preparation process and ensures the quality and stability of the product.
[0058] Embodiment 2
[0059] Based on the above embodiments, this embodiment provides a surface spraying method based on the spraying process of the planting base surface, which solves the qualified rate of the surface coating during the coating process and further ensures the stability of the planting base surface coating;
[0060] The figure is as follows:
[0061] S1: Collect data on the state value of the base surface to obtain the surface humidity value Sd and the surface temperature value Wd of the base surface;
[0062] S2: Compare the surface humidity value Sd with the humidity threshold Sdy;
[0063] If the surface humidity value Sd is greater than or equal to the humidity threshold Sdy, it means that the surface humidity is too high and humidity intervention adjustment is required;
[0064] Since the humidity of the planting base surface has a certain influence on the adhesion of the coating, if the humidity of the planting base surface is too high during the coating spraying process, the spray coating will easily flow and cause uneven spraying, which will have a certain impact on the quality of the planting base.
[0065] Adjust the humidity of the planting base surface by drying or air drying to reduce the humidity of the planting base surface so that the surface humidity meets the spraying standard.
[0066] If the surface humidity value Sd is less than the humidity threshold Sdy, it means that the surface humidity meets the standard; and determine whether the surface temperature value Wd is within the temperature range [Wdx, Wdy].
[0067] If the surface temperature value Wd is not within the temperature range [Wdx, Wdy], it means that the surface temperature is unqualified and temperature intervention adjustment is required;
[0068] The surface temperature value has a certain influence on the curing speed of the spray coating, which in turn affects the coating efficiency of the surface spray coating and the production time of the entire process. Therefore, it is necessary to ensure the surface temperature of the base during the surface coating spraying process;
[0069] If the surface temperature value Wd is within the temperature range [Wdx, Wdy], it means that the temperature meets the standard;
[0070] S3: Obtain a base platform whose surface state value meets the spraying standard, and spray the coating through the surface spraying equipment;
[0071] During spraying, the spraying rate and spraying time in the spraying system at a preset temperature are obtained, and then spraying is performed through the spraying equipment; after the spraying is completed, S4 is executed;
[0072] S4: Obtain the spraying thickness value Hp of the base surface; and make a judgment;
[0073] S41: If Hp<Hpx, it means that the spraying fails to meet the standard; the surface of the base is sprayed again to obtain a base with qualified surface spraying; and the spraying data is stored and adjusted;
[0074] The surface of the base is sprayed again. The steps of spraying are as follows:
[0075] S:411: Calculate and obtain the difference value Hpc of the spraying thickness on the surface of the base; the calculation method of the difference value Hpc of the spraying thickness on the surface of the base is: Hpc=Hpx-Hp;
[0076] S412: Obtain the base surface spraying time value Tp; calculate the supplementary spraying time Tbp based on the base surface spraying thickness difference; the calculation method of the base surface supplementary spraying time Tbp is:
[0077] S413: Perform supplementary spraying on the surface of the base platform based on the supplementary spraying time Tbp; after the supplementary spraying is completed, obtain the supplementary spraying value Hbp of the spraying thickness on the surface of the base platform; then execute S4;
[0078] S414: Obtaining a final value Hzp of the surface spraying thickness and a final value Tzp of the surface spraying time;
[0079] S415: Based on the spraying rate value Ls and the spraying temperature value Wd; the final value of the surface spraying thickness Hzp and the final value of the surface spraying time Tzp are inserted into k=Hzp-Ls×Tzp to calculate and obtain the correction coefficient k;
[0080] S416: Calculate the relationship between the surface spraying thickness value Hp and the spraying time value Tp when the spraying temperature value Wd is obtained;
[0081] Hp=Ls×Tp+k; wherein k is the correction coefficient.
[0082] S42: If Hpy is less than Hp, it indicates that the spraying is excessive, and the base is unqualified; the relationship between the surface spraying thickness value Hp and the spraying time value Tp under the spraying temperature value Wd is calculated;
[0083] Hp=Ls×Tp+k; wherein k is the correction coefficient.
[0084] S43: If the spraying thickness value Hp is within the preset spraying thickness value range [Hpx, Hpy], it means that the spraying is qualified;
[0085] During the process of spraying the surface of the implant base, the spraying time of the coating is obtained based on the preset thickness of the spray coating, and then the spraying is carried out. After the spraying is completed, the thickness of the spray coating is detected to obtain the surface coating thickness value, and it is determined whether the surface coating thickness value is within the surface spraying thickness range. If the surface spraying thickness is unqualified, the surface of the implant base is reprocessed to ensure that the surface thickness of the implant base meets the standard spraying thickness. In addition, during the working process, according to the surface spraying data of the completed implant base, the surface spraying data that does not meet the standard in the initial spraying can be updated, that is, the preset spraying time in the system is updated to ensure that in the subsequent surface spraying process of the implant base, a implant base with qualified surface spraying can be obtained quickly and effectively.
[0086] Embodiment 3
[0087] Based on the above embodiments, this embodiment provides a personalized customized planting base, which is prepared by the above manufacturing method.
[0088] Embodiment 4
[0089] like Figure 2 As shown, a surface spraying system for a method of making a personalized customized implant base:
[0090] It includes: a data acquisition module: used to collect data on the state value of the base surface, and obtain the surface humidity value Sd and the surface temperature value Wd of the base surface;
[0091] Data determination module: used to compare the surface humidity value Sd with the humidity threshold Sdy;
[0092] And determine whether the surface temperature value Wd is within the temperature value range [Wdx, Wdy];
[0093] Data processing module: used to obtain the spraying thickness value Hp on the surface of the base and make a judgment;
[0094] If Hp<Hpx, it means the spraying fails to meet the standard;
[0095] If Hpy<Hp, it means overspray;
[0096] If the spraying thickness value Hp is within the preset spraying thickness range [Hpx, Hpy], it means that the spraying is qualified;
[0097] Control module: used to re-spray the surface of the base; obtain a base with qualified surface spraying; and store and adjust the spraying data; used to remove the sprayed coating on the surface for re-spraying.
[0098] Working principle of the present invention:
[0099] Determine the abutment material and design the abutment size according to the implant plan and tooth model; Process the abutment: cut, grind and polish the abutment material;
[0100] The surface of the base is sprayed. Specifically, the surface humidity value Sd is compared with the humidity threshold value Sdy; and it is determined whether the surface temperature value Wd is in the temperature value range [Wdx, Wdy]; a base whose surface state value meets the spraying standard is obtained, and the coating is sprayed through the surface spraying equipment; the spraying thickness value Hp of the base surface is obtained; and a judgment is made; if Hp<Hpx; it means that the spraying does not meet the standard; if Hpy<Hp; it means that the spraying is excessive; if the spraying thickness value Hp is in the preset spraying thickness value range [Hpx, Hpy], it means that the spraying is qualified; if the spraying does not meet the standard; the surface of the base is sprayed again; a base with qualified surface spraying is obtained; and the spraying data is stored and adjusted; if the spraying is excessive; it is prompted that the base is unqualified;
[0101] Then, the surface is subjected to surface treatments such as oxidation and melting to improve its biocompatibility and wear resistance, and the base is subjected to quality inspection and performance testing to ensure that it meets the design requirements and is safe to use.
[0102] The above is a detailed description of an embodiment of the present invention, but the content is only a preferred embodiment of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the scope of the patent coverage of the present invention.
Claims
1. A method for making a personalized customized planting base, characterized in that: include: Step 1: Design the abutment: determine the abutment material and design the abutment size according to the implant plan and tooth model; Step 2: Processing the abutment: cutting, grinding and polishing the abutment material; Step 3: Surface treatment: spray the surface of the base; The method comprises: S1: collecting data on the state value of the surface of the base platform to obtain a surface humidity value Sd and a surface temperature value Wd of the surface of the base platform; S2: Compare the surface humidity value Sd with the humidity threshold Sdy; And determine whether the surface temperature value Wd is within the temperature value range [Wdx, Wdy]; Obtain a base platform whose surface state value meets the spraying standard, and spray the coating through the surface spraying equipment; S3: Obtain the spraying thickness value Hp of the base surface; and make a judgment; If Hp<Hpx, it means the spraying fails to meet the standard; If Hpy<Hp, it means overspray; If the spraying thickness value Hp is within the preset spraying thickness range [Hpx, Hpy], it means that the spraying is qualified; S4: If the spraying fails to meet the standard, the surface of the base is sprayed again to obtain a base with qualified surface spraying; and the spraying data is stored and adjusted; If the amount of spraying is excessive, it indicates that the base is unqualified; Step 4: Chemical treatment: oxidation and melting of the surface to improve its biocompatibility and wear resistance; Step 5: Inspection and testing: Conduct quality inspection and performance testing on the base to ensure that it meets the design requirements and is safe to use.
2. The method for making a personalized customized planting base according to claim 1, characterized in that: In said S2; If the surface humidity value Sd is greater than or equal to the humidity threshold Sdy, it means that the surface humidity is too high and humidity intervention adjustment is required; If the surface humidity value Sd is less than the humidity threshold Sdy, it means that the surface humidity meets the standard, and it is determined whether the surface temperature value Wd is within the temperature range [Wdx, Wdy].
3. The method for making a personalized customized planting base according to claim 2, characterized in that: In S2: If the surface temperature value Wd is not within the temperature range [Wdx, Wdy], it means that the surface temperature is unqualified and temperature intervention adjustment is required; If the surface temperature value Wd is within the temperature value range [Wdx, Wdy], it means that the temperature meets the standard.
4. The method for making a personalized customized planting base according to claim 1, characterized in that: In S4, the step of performing supplementary spraying on the surface of the base includes: V1: Calculate the difference in thickness Hpc of the spray coating on the base surface; V2: Get the spraying time value Tp of the base surface; calculate the supplementary spraying time Tbp based on the difference of the spraying thickness on the base surface; V3: Perform re-spraying on the surface of the base platform based on the re-spraying time Tbp; after the re-spraying is completed, obtain the re-spraying value Hbp of the spraying thickness on the surface of the base platform; and then execute S3.
5. The method for making a personalized customized planting base according to claim 4, characterized in that: In V1, the calculation method of the difference Hpc of the spraying thickness on the surface of the base is: Hpc=Hpx-Hp.
6. The method for making a customized planting base according to claim 5, characterized in that: In V2, the calculation method of the base surface spraying time Tbp is:
7. The method for making a personalized customized planting base according to claim 1, characterized in that: In said S4, the step of adjusting the spraying data comprises: W1: Get the final value of surface spraying thickness Hzp and the final value of surface spraying time Tzp; W2: Based on the spraying rate value Ls and the spraying temperature value Wd; the final value of the surface spraying thickness Hzp and the final value of the surface spraying time Tzp are inserted into k=Hzp-Ls×Tzp to calculate the correction coefficient k; W3: Calculate the relationship between the surface spray thickness value Hp and the spray time value Tp when the spray temperature value Wd is obtained; Hp=Ls×Tp+k; wherein k is the correction coefficient.
8. The method for making a customized planting base according to claim 1, characterized in that: In S4, if it is indicated that the base is unqualified, the coating already sprayed on the surface is removed and re-sprayed.