A UV-resistant and environmentally friendly color paste and preparation method thereof

By using components such as imidazole-based polyphenylene sulfide, modified crown ether, diatomaceous earth and barium stearate in the color paste, a UV-resistant and environmentally friendly color paste is prepared, which solves the failure of existing color pastes under UV exposure. problem, achieving good ultraviolet absorption and anti-UV effects, and is suitable for a variety of industries.

CN118374189BActive Publication Date: 2024-10-18GUANGZHOU SIQI POLYMER MATERIAL TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410615335.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-17
Publication Date
2024-10-18
Estimated Expiration
2044-05-17

AI Technical Summary

Technical Problem

Existing color pastes fail under ultraviolet (UV) exposure and cannot effectively protect the human body, especially in the toy industry, silicone medical devices, plexiglass and other industries, posing safety risks.

Method used

Using components such as imidazole-based polyphenylene sulfide, modified crown ether, diatomaceous earth, barium stearate and polyvinyl alcohol, a UV-resistant and environmentally friendly color paste is prepared through modification reaction and mixing process. The hydroxyl group in the crown ether and the carboxyl group in the diatomite form an ester group. The conjugated structure of the imidazole system absorbs ultraviolet rays and synergistically resists UV rays.

Benefits of technology

The UV-resistant effect of the color paste is significantly improved. Through the synergistic effect of the modified crown ether and imidazole groups, it can effectively absorb and resist ultraviolet rays, significantly reducing the damage of UV to the human body.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the technical field of color pastes, and discloses a UV-resistant and environment-friendly color paste and a preparation method thereof. The invention provides a UV-resistant and environment-friendly color paste by adding imidazole polyphenylene sulfide, modified crown ether, diatomaceous earth, barium stearate and polyvinyl alcohol into a high-speed mixing pot for uniform mixing, then continuously adding pigment and deionized water, stirring, and grinding after completion to obtain the UV-resistant and environment-friendly color paste; in the process of stirring and mixing, the hydroxyl group in the modified crown ether forms an ester group with a benzene ring with the carboxyl group in the diatomaceous earth, which can effectively absorb ultraviolet rays; the imidazole group in the modified crown ether and the imidazole group in the imidazole polyphenylene sulfide form an imidazole system, the five-membered ring in the imidazole has a conjugated system, which can effectively absorb ultraviolet rays, and the crown ether, polyphenylene sulfide and phenolic resin themselves can also resist ultraviolet rays, and the synergistic effect can achieve a better ultraviolet resistance effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of color pastes, in particular to a UV-resistant and environment-friendly color paste and a preparation method thereof. Background Art

[0002] The color paste contains pigments and plasticizers, and has good stability and dispersibility. Except for a few inorganic pigments containing lead, other pigments are strictly selected for low toxicity. There are many types of color pastes. The colorants made by machinery are suitable for the toy industry, silicone medical devices, organic glass and other industries. Ultraviolet rays can cause harm to the body, so color pastes with good UV resistance are needed to be better used in real life; cardanol has a good ability to absorb ultraviolet rays and can effectively protect the human body from damage by ultraviolet rays. In the present invention, cardanol and other substances with ultraviolet resistance are synergistically anti-ultraviolet to prepare a UV-resistant and environmentally friendly color paste. Summary of the invention

[0003] 1. Technical issues to be resolved

[0004] In view of the deficiencies in the prior art, the present invention provides a UV-resistant and environmentally friendly color paste and a preparation method thereof, which has good UV-resistant effect.

[0005] (II) Technical solution

[0006] To achieve the above object, the present invention provides the following technical solution: a UV-resistant and environmentally friendly color paste, comprising the following components by weight: 8-15 parts by weight of imidazole polyphenylene sulfide, 5-10 parts by weight of modified crown ether, 15-20 parts by weight of diatomaceous earth, 12-16 parts by weight of barium stearate, 6-12 parts by weight of polyvinyl alcohol, 4-10 parts by weight of pigment, and 20-30 parts by weight of deionized water;

[0007] The preparation method of the imidazole polyphenylene sulfide is:

[0008] (1) Under nitrogen protection, acetylated polyphenylene sulfide powder is added to anhydrous toluene solvent, and then 3-aminopropyltriethoxysilane is slowly added dropwise, and acetic acid and 4A molecular sieve are continuously added, and the reaction is carried out at 80-100° C. for 8-12 hours. After the reaction, the mixture is filtered, washed, and subjected to Soxhlet extraction with ethanol solution for 22-24 hours, and dried to constant weight to obtain organosilicon-grafted modified polyphenylene sulfide;

[0009] (2) adding organosilicon-grafted polyphenylene sulfide and trichlorosilane to N,N-dimethylformamide solvent under nitrogen protection, stirring evenly, and then adding chloroplatinic acid catalyst, reacting at 40-70° C. for 20-40 min, and then performing reduced pressure distillation after reaction, filtering and drying to obtain intermediate 1;

[0010] (3) Add intermediate 1, cardanol, and 5-hydroxy-1H-imidazole-4-carboxamide to N,N-dimethylformamide solvent, stir evenly, and react at 50-70° C. for 6-10 hours. After reaction, wash, filter, and dry to obtain imidazole polyphenylene sulfide.

[0011] Preferably, the mass ratio of acetylated polyphenylene sulfide, 3-aminopropyltriethoxysilane, acetic acid and 4A molecular sieve in (1) is 1.5-2.2:1:0.02-0.03:0.6-0.9.

[0012] Preferably, the mass ratio of the organosilicon grafted modified polyphenylene sulfide, trichlorosilane and chloroplatinic acid catalyst in (2) is 1:1.1-1.4:0.02-0.04.

[0013] Preferably, the mass ratio of the intermediate 1, cardanol and 5-hydroxy-1H-imidazole-4-carboxamide in (3) is 0.7-1.2:1:1.1-1.5.

[0014] Preferably, the preparation method of the modified crown ether is:

[0015] S1. 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4, KI and N,N-dimethylformamide solvent are added to a reactor, and in a microwave reactor, the microwave power is controlled to be 550-650 W, the reaction time is 20-40 min, and then ethyl acetate and water are added for extraction, the organic phase is dried to remove water, and the solid crude product is recrystallized in ethanol to obtain an imidazolyl crown ether;

[0016] S2. The phenolic resin and epichlorohydrin are mixed uniformly, reacted at 60-80 ° C for 8-12 hours, and then concentrated under reduced pressure and washed to obtain an epoxidized phenolic resin;

[0017] S3. Add imidazolyl crown ether and epoxidized phenolic resin to a mixed solvent of distilled water and N,N-dimethylformamide, stir evenly, add triethylamine catalyst, pass nitrogen protection, react at 80-100°C for 20-32h, filter the solvent after reaction, wash with distilled water and ethanol, filter and dry to obtain modified crown ether.

[0018] Preferably, the mass ratio of 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4 and KI in S1 is 1:1.1-1.3:0.1-0.2:0.06-0.08.

[0019] Preferably, the mass ratio of phenolic resin to epichlorohydrin in S2 is 1:0.9-1.2.

[0020] Preferably, the mass ratio of the imidazolyl crown ether, the epoxidized phenolic resin and the triethylamine catalyst in S3 is 1:1.1-1.3:0.02-0.03.

[0021] Preferably, it is characterized in that the preparation method of the UV-resistant and environmentally friendly color paste comprises the following steps: adding imidazole polyphenylene sulfide, modified crown ether, diatomaceous earth, barium stearate, and polyvinyl alcohol into a high-speed mixing pot and uniformly mixing, and then continuing to add pigment and deionized water, stirring at 40-50°C for 30-40 minutes, and grinding after completion to obtain the UV-resistant and environmentally friendly color paste.

[0022] (III) Beneficial technical effects

[0023] The invention adds imidazole polyphenylene sulfide, modified crown ether, diatomaceous earth, barium stearate and polyvinyl alcohol into a high-speed mixing pot for uniform mixing, then continues to add pigment and deionized water, stirs, and grinds to obtain UV-resistant and environmentally friendly color paste.

[0024] During the stirring and mixing process, the hydroxyl group in the modified crown ether will form an ester group with a benzene ring with the carboxyl group in the diatomaceous earth, which can effectively absorb ultraviolet rays; the imidazole group in the modified crown ether and the imidazole group in the imidazole-based polyphenylene sulfide constitute an imidazole system, and the five-membered ring in the imidazole has a conjugated system, which can effectively absorb ultraviolet rays, and the crown ether, polyphenylene sulfide, and phenolic resin themselves can also resist ultraviolet rays, and the synergistic effect has a better ultraviolet resistance effect. DETAILED DESCRIPTION

[0025] Reference "Organic Silicone Grafted Modified Polyphenylene Sulfide" Preparation of Acetylated Polyphenylene Sulfide: Dried PPS powder was suspended and dispersed in 200ml dichloromethane (purified after dehydration) for pre-swelling for 12 hours, and then poured into a 500ml flask equipped with a thermometer, a constant pressure dropping funnel, a condenser and a stirrer, and the upper end of the condenser was connected to a gas absorption device. After nitrogen was passed through for a while, 32.52g of anhydrous aluminum chloride powder was quickly added, and then 15ml of acetyl chloride was added to the constant pressure dropping funnel. In order to prevent the reaction from being too intense, the drop rate was controlled to 1 drop / 3S, and the mixture was stirred evenly. After all the materials were added, the mixture was first reacted in an ice water bath for 1.5r, then the temperature was raised to 38℃ and reacted for 3.5 hours until no HCl gas escaped, and then cooled to room temperature. The entire reaction solution was transferred into glacial hydrochloric acid (50 ml hydrochloric acid + 50 g ice) for decomposition, filtered, washed with 5% NaOH solution, then repeatedly washed with deionized water and ethanol solution, and vacuum dried at 80°C for 24 hours to obtain acetylated polyphenylene sulfide.

[0026] Example 1

[0027] (1) Under nitrogen protection, acetylated polyphenylene sulfide powder is added to anhydrous toluene solvent, and then 3-aminopropyltriethoxysilane is slowly added dropwise, and acetic acid and 4A molecular sieve are continuously added, wherein the mass ratio of acetylated polyphenylene sulfide, 3-aminopropyltriethoxysilane, acetic acid, and 4A molecular sieve is 1.5:1:0.02:0.6, and the reaction is carried out at 80° C. for 8 hours. After the reaction is completed, the mixture is filtered, washed, and subjected to Soxhlet extraction with ethanol solution for 22 hours, and dried to constant weight to obtain organosilicon-grafted modified polyphenylene sulfide;

[0028] (2) adding organosilicon-grafted modified polyphenylene sulfide and trichlorosilane to N,N-dimethylformamide solvent under nitrogen protection, stirring evenly, and then adding chloroplatinic acid catalyst, wherein the mass ratio of organosilicon-grafted modified polyphenylene sulfide, trichlorosilane, and chloroplatinic acid catalyst is 1:1.1:0.02, reacting at 40° C. for 20 min, and then performing reduced pressure distillation after completion, filtering and drying to obtain intermediate 1;

[0029] (3) adding intermediate 1, cardanol, and 5-hydroxy-1H-imidazole-4-carboxamide to N,N-dimethylformamide solvent, wherein the mass ratio of intermediate 1, cardanol, and 5-hydroxy-1H-imidazole-4-carboxamide is 0.7:1:1.1, stirring evenly, reacting at 50° C. for 6 hours, and after completion, washing, filtering, and drying to obtain imidazole polyphenylene sulfide;

[0030] (4) adding 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4, KI and N,N-dimethylformamide solvent into a reactor, wherein the mass ratio of 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4 and KI is 1:1.1:0.1:0.06, and in a microwave reactor, the microwave power is controlled to be 550 W, the reaction time is 20 min, and ethyl acetate and water are added for extraction, the organic phase is dried to remove water, and the solid crude product is recrystallized in ethanol to obtain an imidazolyl crown ether;

[0031] (5) mixing phenolic resin and epichlorohydrin uniformly, wherein the mass ratio of phenolic resin to epichlorohydrin is 1:0.9, reacting at 60° C. for 8 h, and then concentrating under reduced pressure and washing to obtain epoxidized phenolic resin;

[0032] (6) adding an imidazolyl crown ether and an epoxidized phenolic resin to a mixed solvent of distilled water and N,N-dimethylformamide, stirring evenly, adding a triethylamine catalyst, wherein the mass ratio of the imidazolyl crown ether, the epoxidized phenolic resin, and the triethylamine catalyst is 1:1.1:0.02, passing nitrogen protection, reacting at 80° C. for 20 h, filtering the solvent after the reaction, washing with distilled water and ethanol, filtering and drying to obtain a modified crown ether;

[0033] (7) 8 parts by weight of imidazole polyphenylene sulfide, 5 parts by weight of modified crown ether, 15 parts by weight of diatomaceous earth, 12 parts by weight of barium stearate, and 6 parts by weight of polyvinyl alcohol are added to a high-speed mixing pot and uniformly mixed, and then 4 parts by weight of pigment and 20 parts by weight of deionized water are added, and stirred at 40° C. for 30 minutes. After completion, the mixture is ground to obtain a UV-resistant and environmentally friendly color paste.

[0034] Example 2

[0035] (1) under nitrogen protection, acetylated polyphenylene sulfide powder was added to anhydrous toluene solvent, and then 3-aminopropyltriethoxysilane was slowly added dropwise, and acetic acid and 4A molecular sieve were continuously added, wherein the mass ratio of acetylated polyphenylene sulfide, 3-aminopropyltriethoxysilane, acetic acid and 4A molecular sieve was 2.2:1:0.03:0.9, and the mixture was reacted at 100° C. for 12 h. After the reaction, the mixture was filtered, washed, and subjected to Soxhlet extraction with ethanol solution for 24 h, and dried to constant weight to obtain organosilicon-grafted modified polyphenylene sulfide;

[0036] (2) adding organosilicon-grafted modified polyphenylene sulfide and trichlorosilane to N,N-dimethylformamide solvent under nitrogen protection, stirring evenly, and then adding chloroplatinic acid catalyst, wherein the mass ratio of organosilicon-grafted modified polyphenylene sulfide, trichlorosilane, and chloroplatinic acid catalyst is 1:1.4:0.04, reacting at 70° C. for 40 min, and then performing reduced pressure distillation after the reaction, filtering and drying to obtain intermediate 1;

[0037] (3) adding intermediate 1, cardanol, and 5-hydroxy-1H-imidazole-4-carboxamide to N,N-dimethylformamide solvent, wherein the mass ratio of intermediate 1, cardanol, and 5-hydroxy-1H-imidazole-4-carboxamide is 1.2:1:1.5, stirring evenly, reacting at 70° C. for 10 hours, and after completion, washing, filtering, and drying to obtain imidazole polyphenylene sulfide;

[0038] (4) adding 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4, KI and N,N-dimethylformamide solvent into a reactor, wherein the mass ratio of 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4 and KI is 1:1.3:0.2:0.08, and in a microwave reactor, the microwave power is controlled to be 650 W, the reaction time is 40 min, and ethyl acetate and water are added for extraction, the organic phase is dried to remove water, and the solid crude product is recrystallized in ethanol to obtain an imidazolyl crown ether;

[0039] (5) mixing phenolic resin and epichlorohydrin uniformly, wherein the mass ratio of phenolic resin to epichlorohydrin is 1:1.2, reacting at 80° C. for 12 h, and then concentrating under reduced pressure and washing to obtain epoxidized phenolic resin;

[0040] (6) adding an imidazolyl crown ether and an epoxidized phenolic resin to a mixed solvent of distilled water and N,N-dimethylformamide, stirring evenly, adding a triethylamine catalyst, wherein the mass ratio of the imidazolyl crown ether, the epoxidized phenolic resin, and the triethylamine catalyst is 1:1.3:0.03, passing nitrogen protection, reacting at 100° C. for 32 hours, filtering the solvent after the reaction, washing with distilled water and ethanol, filtering and drying to obtain a modified crown ether;

[0041] (7) 15 parts by weight of imidazole polyphenylene sulfide, 10 parts by weight of modified crown ether, 20 parts by weight of diatomaceous earth, 16 parts by weight of barium stearate, and 12 parts by weight of polyvinyl alcohol are added to a high-speed mixing pot and uniformly mixed, and then 10 parts by weight of pigment and 30 parts by weight of deionized water are added, stirred at 50° C. for 40 minutes, and then ground to obtain a UV-resistant and environmentally friendly color paste.

[0042] Example 3

[0043] (1) Under nitrogen protection, acetylated polyphenylene sulfide powder is added to anhydrous toluene solvent, and then 3-aminopropyltriethoxysilane is slowly added dropwise, and acetic acid and 4A molecular sieve are continuously added, wherein the mass ratio of acetylated polyphenylene sulfide, 3-aminopropyltriethoxysilane, acetic acid, and 4A molecular sieve is 1.85:1:0.025:0.75, and the reaction is carried out at 90° C. for 10 hours. After the reaction is completed, the mixture is filtered, washed, and subjected to Soxhlet extraction with ethanol solution for 23 hours, and dried to constant weight to obtain organosilicon-grafted modified polyphenylene sulfide;

[0044] (2) adding organosilicon-grafted modified polyphenylene sulfide and trichlorosilane to N,N-dimethylformamide solvent under nitrogen protection, stirring evenly, and then adding chloroplatinic acid catalyst, wherein the mass ratio of organosilicon-grafted modified polyphenylene sulfide, trichlorosilane, and chloroplatinic acid catalyst is 1:1.25:0.03, reacting at 55° C. for 30 minutes, and then performing reduced pressure distillation after the reaction, filtering and drying to obtain intermediate 1;

[0045] (3) adding intermediate 1, cardanol, and 5-hydroxy-1H-imidazole-4-carboxamide to N,N-dimethylformamide solvent, wherein the mass ratio of intermediate 1, cardanol, and 5-hydroxy-1H-imidazole-4-carboxamide is 0.95:1:1.3, stirring evenly, reacting at 60° C. for 8 h, and after completion, washing, filtering, and drying to obtain imidazole polyphenylene sulfide;

[0046] (4) adding 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4, KI and N,N-dimethylformamide solvent into a reactor, wherein the mass ratio of 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4 and KI is 1:1.2:0.15:0.07, and in a microwave reactor, the microwave power is controlled to be 600 W, the reaction time is 30 min, and ethyl acetate and water are added for extraction, the organic phase is dried to remove water, and the solid crude product is recrystallized in ethanol to obtain an imidazolyl crown ether;

[0047] (5) mixing phenolic resin and epichlorohydrin uniformly, wherein the mass ratio of phenolic resin to epichlorohydrin is 1:1.05, reacting at 70° C. for 10 h, and then concentrating under reduced pressure and washing to obtain epoxidized phenolic resin;

[0048] (6) adding an imidazolyl crown ether and an epoxidized phenolic resin to a mixed solvent of distilled water and N,N-dimethylformamide, stirring uniformly, adding a triethylamine catalyst, wherein the mass ratio of the imidazolyl crown ether, the epoxidized phenolic resin, and the triethylamine catalyst is 1:1.2:0.025, passing nitrogen protection, reacting at 90° C. for 26 hours, filtering the solvent after the reaction, washing with distilled water and ethanol, filtering and drying to obtain a modified crown ether;

[0049] (7) 11.5 parts by weight of imidazole polyphenylene sulfide, 7.5 parts by weight of modified crown ether, 17.5 parts by weight of diatomaceous earth, 14 parts by weight of barium stearate, and 9 parts by weight of polyvinyl alcohol are added to a high-speed mixing pot and uniformly mixed, and then 7 parts by weight of pigment and 25 parts by weight of deionized water are added, and stirred at 45° C. for 35 minutes. After completion, the mixture is ground to obtain a UV-resistant and environmentally friendly color paste.

[0050] Comparative Example 1

[0051] The difference between this comparative example and Example 3 is that no imidazole polyphenylene sulfide is added.

[0052] Comparative Example 2

[0053] Compared with Example 3, this comparative example is characterized in that no modified crown ether is added.

[0054] The UV test is as follows: by irradiating with UVB at a wavelength of 313nm, at 55°C for 45h, the color difference before and after UVB changes △E. The test results are shown in Table 1.

[0055] Table 1: UV resistance test.

[0056] project △E Example 1 0.7 Example 2 1.2 Example 3 0.9 Comparative Example 1 2.8 Comparative Example 2 2.9

[0057] As can be seen from Table 1, the UV-resistant and environmentally friendly color pastes prepared in Examples 1-3 of the present invention have better UV-resistant effects than those prepared in Comparative Examples 1-2.

[0058] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.

Claims

1. A UV-resistant and environmentally friendly color paste, characterized in that: The invention comprises the following components by weight: 8-15 parts by weight of imidazole polyphenylene sulfide, 5-10 parts by weight of modified crown ether, 15-20 parts by weight of diatomaceous earth, 12-16 parts by weight of barium stearate, 6-12 parts by weight of polyvinyl alcohol, 4-10 parts by weight of pigment, and 20-30 parts by weight of deionized water; The preparation method of the imidazole polyphenylene sulfide is: (1) Under nitrogen protection, acetylated polyphenylene sulfide powder is added to anhydrous toluene solvent, and then 3-aminopropyltriethoxysilane is slowly added dropwise, and acetic acid and 4A molecular sieve are continuously added, and the reaction is carried out at 80-100° C. for 8-12 hours. After the reaction, the mixture is filtered, washed, and subjected to Soxhlet extraction with ethanol solution for 22-24 hours, and dried to constant weight to obtain organosilicon-grafted modified polyphenylene sulfide; (2) adding organosilicon-grafted polyphenylene sulfide and trichlorosilane to N,N-dimethylformamide solvent under nitrogen protection, stirring evenly, and then adding chloroplatinic acid catalyst, reacting at 40-70° C. for 20-40 min, and then performing reduced pressure distillation after reaction, filtering and drying to obtain intermediate 1; (3) adding intermediate 1, cardanol, and 5-hydroxy-1H-imidazole-4-carboxamide to N,N-dimethylformamide solvent, stirring evenly, reacting at 50-70° C. for 6-10 hours, and after completion, washing, filtering, and drying to obtain imidazole polyphenylene sulfide; The mass ratio of acetylated polyphenylene sulfide, 3-aminopropyltriethoxysilane, acetic acid and 4A molecular sieve in (1) is 1.5-2.2:1:0.02-0.03:0.6-0.9; The mass ratio of organosilicon grafted modified polyphenylene sulfide, trichlorosilane and chloroplatinic acid catalyst in (2) is 1:1.1-1.4:0.02-0.04; The mass ratio of intermediate 1, cardanol and 5-hydroxy-1H-imidazole-4-carboxamide in (3) is 0.7-1.2:1:1.1-1.5; The preparation method of the modified crown ether is: S1. 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4, KI and N,N-dimethylformamide solvent are added to a reactor, and in a microwave reactor, the microwave power is controlled to be 550-650 W, the reaction time is 20-40 min, and then ethyl acetate and water are added for extraction, the organic phase is dried to remove water, and the solid crude product is recrystallized in ethanol to obtain an imidazolyl crown ether; S2. The phenolic resin and epichlorohydrin are mixed uniformly, reacted at 60-80 ° C for 8-12 hours, and then concentrated under reduced pressure and washed to obtain an epoxidized phenolic resin; S3. The imidazolyl crown ether and the epoxidized phenolic resin are added to a mixed solvent of distilled water and N,N-dimethylformamide, stirred evenly, triethylamine catalyst is added, nitrogen is introduced, and the reaction is carried out at 80-100 ° C for 20-32h. After the reaction, the solvent is filtered, washed with distilled water and ethanol, filtered and dried to obtain a modified crown ether; The mass ratio of 4-formylbenzo-15-crown-5, 3,4-diaminobenzoic acid, anhydrous Na2SO4, and KI in S1 is 1:1.1-1.3:0.1-0.2:0.06-0.08; The mass ratio of phenolic resin to epichlorohydrin in S2 is 1:0.9-1.2; The mass ratio of the imidazolyl crown ether, the epoxidized phenolic resin and the triethylamine catalyst in S3 is 1:1.1-1.3:0.02-0.

03.

2. A method for preparing the UV-resistant and environmentally friendly color paste as claimed in claim 1, characterized in that: The preparation method of the UV-resistant and environmentally friendly color paste comprises the following steps: adding imidazole polyphenylene sulfide, modified crown ether, diatomaceous earth, barium stearate, and polyvinyl alcohol into a high-speed mixing pot and uniformly mixing, then continuously adding pigment and deionized water, stirring at 40-50° C. for 30-40 minutes, and grinding after completion to obtain the UV-resistant and environmentally friendly color paste.

Citation Information

Patent Citations

  • Organic silicon grafted and modified polyphenylene sulphide material and preparation method thereof

    CN102504256A

  • Photocrosslinkable Materials