Semiconductor device chip, manufacturing method thereof, semiconductor device and electronic device

By introducing a trench structure in the gate area of ​​semiconductor devices, the problems of slow switching speed, large leakage current and low current tolerance of traditional IGCT devices under high voltage, high frequency and high current conditions are solved, and faster switching is achieved Rate, lower electric field peak and heat loss, and stronger current tolerance.

CN118398657BActive Publication Date: 2024-11-29北京怀柔实验室
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410841865.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-11-29
Estimated Expiration
2044-06-27

AI Technical Summary

Technical Problem

The gate structure of traditional IGCT devices has limitations such as slow switching speed, large leakage current, and low current tolerance under high voltage, high frequency, and high current operating conditions.

Method used

The trench structure is introduced into the gate area of ​​the semiconductor device, and the trench structure is prepared through a patterning process to improve the switching characteristics and current tolerance of the device.

Benefits of technology

By introducing the trench structure, the switching rate of the device is significantly improved, the electric field peak and heat loss are reduced, and the gate convergence capability and safe working area are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118398657B_ABST
    Figure CN118398657B_ABST
Patent Text Reader

Abstract

A semiconductor device chip, a manufacturing method thereof, a semiconductor device and an electronic device, belonging to the field of power semiconductor device manufacturing. The semiconductor device chip includes a gate, and the gate has a groove structure different from a groove gate and an isolation groove; the semiconductor device chip is a bipolar semiconductor device chip in which both electrons and holes are conducted by the diffusion principle, or a thyristor chip. The semiconductor device with a gate groove structure of the present invention can solve at least one technical problem such as slow switching speed, large leakage current, and low current carrying capacity, and has a significant improvement effect in at least one aspect such as switching speed, large current shutdown, gate parasitic parameter optimization, and gate current sharing. The gate turn-off time can be reduced by 10% to 50%, the electric field peak value is reduced by 15%, the parameters of the parasitic inductance in the gate current converging process are also significantly reduced, and the current converging capacity is significantly increased.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor process manufacturing, and in particular to a semiconductor device chip with a gate trench structure, a manufacturing method thereof, and a semiconductor device and electronic equipment using the same. Background Art

[0002] IGCT (Integrated Gate Commutated Thyristor) is a new type of high-voltage and high-power power electronic device with the advantages of high voltage, high current, and low voltage drop. It is widely used in the field of power electronics. As a switching device with gate-controlled shutdown, IGCT has the advantages of both GTO and IGBT. Its shutdown characteristics are like transistors, while its turn-on characteristics are like thyristors. It has the characteristics of high blocking voltage, large power capacity, low conduction loss, no need for shutdown absorption circuit, and easy series and parallel connection. Because of the integrated low-inductance gate drive unit, users only need to configure the corresponding gate drive power supply, complete the heat sink press-fitting and conductive bus connection, and equip the controller with a suitable control strategy to apply it, which can save the development cost of the converter, shorten the development cycle, and facilitate application and maintenance.

[0003] The traditional IGCT device gate structure has some limitations under high voltage, high frequency, and high current working conditions, such as slow switching speed, large leakage current, and low current carrying capacity.

[0004] Chinese patent CN112599587B discloses a semiconductor device with a buffer layer structure, including a first dopant region, a second dopant region, and a third dopant region arranged in sequence, and also including an upper dopant region, a lower dopant region, and a middle dopant region arranged in one or more combinations; the upper dopant region is located between the first dopant region and the second dopant region; the lower dopant region is located between the second dopant region and the third dopant region; the middle dopant region is located in the middle of the second dopant region, thereby achieving a smaller leakage current, improving the device's withstand voltage capability, and the highest junction temperature that can be operated, and increasing the device's current capacity. However, this process requires multiple doping, high preparation cost, complex process, and long processing time.

[0005] Chinese patent application CN108598150A discloses a lateral variable doping-junction terminal extension composite terminal structure. Taking GCT as an example, the terminal area and the active area have a common n-substrate and the n-type FS layer, p+ anode area and anode electrode below it; on the outside of the main junction of the active area, a resistance area, a lateral variable doping area and a junction terminal extension area are arranged in sequence, and the lateral variable doping area and the junction terminal extension area overlap each other, and the surface of the terminal area is covered with two layers of passivation film; the resistance area connects the main junction and the composite terminal area into one. The composite terminal structure of this application can obtain a withstand voltage efficiency of about 91%, a small high-temperature leakage current, high terminal stability, and the manufacturing process is fully compatible with the active area. However, this process mainly solves the problems of leakage current and withstand voltage, and does not involve the problem of switching speed.

[0006] With regard to the current status of the prior art, the inventors have conducted in-depth research and innovatively proposed a semiconductor device chip and a method for manufacturing the same. Summary of the invention

[0007] In view of this, the main purpose of the present invention is to provide a semiconductor device chip, a manufacturing method thereof, and a semiconductor device and electronic device using the same, in order to at least partially solve the above technical problems.

[0008] In order to achieve the above object, as a first aspect of the present invention, a semiconductor device chip is provided, wherein the semiconductor device chip comprises a gate electrode, and the gate electrode has a trench structure;

[0009] The semiconductor device chip is a thyristor, or a chip of a bipolar semiconductor device in which both electrons and holes are conducted according to the diffusion principle.

[0010] As a second aspect of the present invention, a method for manufacturing a semiconductor device chip is also proposed, comprising the following steps:

[0011] After forming the gate, further preparing a desired trench structure on the gate by a patterning process;

[0012] The semiconductor device chip is a thyristor, or a chip of a bipolar semiconductor device in which both electrons and holes are conducted according to the diffusion principle.

[0013] As a third aspect of the present invention, a semiconductor device chip manufactured based on the semiconductor device chip manufacturing method as described above is also proposed.

[0014] As a fourth aspect of the present invention, a semiconductor device including the semiconductor device chip as described above is also proposed.

[0015] As a fifth aspect of the present invention, an electronic device comprising the semiconductor device as described above is also proposed.

[0016] Based on the above technical solutions, it can be seen that the semiconductor device chip and the manufacturing method thereof of the present invention are mainly different from the prior art in the gate trench structure. According to simulation calculations, the prior art chip proposed by the present invention has a significant improvement effect in at least one aspect of switching speed, large current shutdown, gate parasitic parameter optimization, gate current sharing, etc.:

[0017] (1) Through simulation calculation, the gate turn-off time can be reduced by 10% to 50%. The gate trench structure of the present invention reduces the gate turn-off time by 1.3 μs, a reduction of 20%. The present invention can effectively improve the switching rate of the device, and improve the flexibility and operating frequency of the device;

[0018] (2) The electric field concentration effect under the gate when the current is turned off is also significantly improved, and the peak value of the electric field is reduced by 15%, indicating that the avalanche effect is improved and the heat loss can be reduced;

[0019] (3) Due to the presence of the trench gate structure, the thickness of the gate interconnect metal is increased compared to the traditional GCT device, even by several times. Therefore, the parameters of the parasitic inductance during the gate convergence process will be significantly reduced, and the convergence capacity will also be significantly increased, even by several times, which increases the safe working area of ​​the device and improves safety and reliability.

[0020] (4) Due to the introduction of the trench structure, the depth of the gate electrode and the thickness of the interconnection are increased, which significantly improves the current-sharing capability of the device and can more quickly derive the heat accumulation generated by the carrier recombination process at the PN-junction interface, thereby increasing the operating junction temperature of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below.

[0022] Figure 1 It is a roadmap of the control distribution implementation method of the metal-semiconductor contact resistance of the present invention;

[0023] Figure 2 is a schematic cross-sectional view of a GCT chip cell and terminal structure according to a specific embodiment of the present invention;

[0024] FIG3 is a schematic diagram of the cross-sectional structure of a planar junction and a curved junction in the prior art;

[0025] 4 is a cross-sectional view and a top view of a trench structure type of a preferred embodiment of the present invention;

[0026] Figure 5 It is a process flow chart of the preparation of the trench gate integrated gate commutated thyristor of the present invention;

[0027] Figure 6 is a schematic cross-sectional view of a trench structure of a gate according to an embodiment of the present invention;

[0028] Figure 7 is a comparison curve diagram of the turn-off loss of Example 1 of the present invention and Comparative Example 1;

[0029] Figure 8 It is a comparison curve diagram of the turn-off time of Example 1 of the present invention and Comparative Example 1.

[0030] In the above drawings, the meanings of the reference numerals are as follows:

[0031] 1-anode electrode; 2-cathode electrode; 3-gate electrode; 4-red glue; 102-anode side P+ region; 103-anode side P- region; 104-N-drift region; 105-cathode side P- region; 106-cathode side P+ region; 107-PI glue passivation layer; 108-gate cathode dielectric layer; 109-trench gate; 110-gate ring; 111-angled terminal and terminal passivation layer. DETAILED DESCRIPTION

[0032] In order to make the objectives, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments and with reference to the accompanying drawings.

[0033] In this article, some terms have the following meanings:

[0034] Thyristor, also known as silicon controlled rectifier, is a semiconductor device with the characteristics of silicon rectifier devices, which can work under high voltage and high current conditions. Its basic use is controlled rectification, and its working process can be controlled. It has the advantages of small size, light weight, low power consumption, high efficiency, and fast switching.

[0035] GTO, short for Gate-Turn-Off Thyristor, is a gate-turn-off thyristor. When a positive voltage is applied to the anode and a positive trigger current is applied to the gate, the GTO is turned on. When a sufficiently large reverse trigger pulse current is applied to the gate, the GTO switches from on to off. GTO has self-turn-off capability and thyristor characteristics, high voltage resistance, large current capacity, and strong surge resistance. Therefore, it has gradually replaced ordinary thyristors and become the main switching device in large and medium capacity converters.

[0036] IGCT is the abbreviation of Integrated Gate-Commutated Thyristor. It is a power semiconductor device used for current switching in industrial equipment. It is composed of a triode and an anti-parallel diode, and has the advantages of stable turn-off capability and low conduction loss. In the conduction stage, it exerts the performance of a thyristor; in the turn-off stage, it exhibits the characteristics of a transistor. Compared with GTO thyristors, IGCT has higher reliability and lower cost. The cathode surface of IGCT is composed of multiple concentric cathode rings, a concentric gate contact ring and multiple cathode combs.

[0037] GCT cell is the basic structure of IGCT. The vertical structure of each cell from cathode to anode is n+ emitter, p base, n base, n+ buffer layer, p+ emitter, with three PN junctions J1, J2 and J3. The layout, geometry and size of GCT cell and cell density determine the conduction voltage drop of IGCT.

[0038] GTR is the abbreviation of Giant Transistor, which is a power transistor. It is a bipolar junction transistor (BJT) that can withstand high voltage and high current. The names GTR and BJT are equivalent, and their structure and working principle are very similar to those of low-power transistors. GTR consists of three layers of semiconductors and two PN junctions. Like low-power triodes, there are two types, PNP and NPN. GTR usually uses NPN structure. The main characteristics of GTR are high voltage resistance, large current and good switching characteristics.

[0039] MCT, short for MOS-Controlled Thyristor, is a new type of MOS and bipolar composite device. It uses integrated circuit technology to make a large number of MOS devices in an ordinary thyristor structure, and controls the on and off of the thyristor by turning on and off the MOS device. MCT has both the good turn-off and on characteristics of thyristors and the advantages of high input impedance, low driving power and fast switching speed of MOS field effect tubes, overcoming the shortcomings of slow thyristor speed, inability to turn off by itself and large conduction voltage drop of high-voltage MOS field effect tubes. Therefore, MCT is considered to be a new type of power device with great development prospects. MOS controlled thyristors are used in high-power applications, such as high power, high frequency, low conductivity, and in subsequent processes, and are likely to replace high-voltage GTOs. Competition with IGBTs will also begin in the medium-power field.

[0040] MTO, namely GTO thyristor with gate integrated MOS structure.

[0041] Positive photoresist, also known as positive photoresist, is a phenolic formaldehyde called linear phenolic resin, which provides the adhesion and chemical resistance of the photoresist. When there is no dissolution inhibitor, the linear phenolic resin will dissolve in the developer to obtain the desired pattern, wherein the photosensitive agent is a photosensitive compound.

[0042] Negative photoresist, also known as photoresist or negative photoresist, is a light-sensitive mixed liquid composed of three main components: photosensitive resin, sensitizer (spectral sensitizing dye) and solvent. Positive photoresist and negative photoresist are mainly distinguished based on their chemical reaction mechanism and development principle: negative photoresist forms insoluble substances after light exposure; conversely, positive photoresist is insoluble in certain solvents at first, but becomes soluble after light exposure.

[0043] Ohmic contact: When semiconductors come into contact with metals, a potential barrier layer is usually formed. However, when the semiconductor doping concentration is very high, electrons can pass through the potential barrier by tunneling, thus forming a low-resistance ohmic contact. Ohmic contact is very important for semiconductor devices. Forming a good ohmic contact is conducive to the input and output of current. Different alloys with different formulations are often selected as ohmic contact materials for different semiconductor materials.

[0044] Planar junction GCT, when the P of the GCT chip base When the junction formed by the gate region and the drift region is a planar structure, it is called a planar junction GCT.

[0045] Curved junction GCT, when the P of the GCT chip base When the junction formed by the drift zone and the drift zone is a curved structure, it is called a curved junction GCT, a common example of which is the wavy junction GCT structure.

[0046] In view of the limitations of the traditional IGCT device gate structure under high voltage, high frequency, high current and other working conditions, such as slow switching speed, large leakage current, low current carrying capacity and other defects, the present invention proposes to introduce a gate trench structure into the semiconductor device structure, aiming to improve the switching characteristics of the device and reduce the parasitic parameters of the device. The inventors have found that:

[0047] (1) Due to the gate trench structure, the metal electrode can be embedded into the chip gate P base The deep region can improve the carrier injection efficiency of the chip during the opening process, allowing it to be turned on more quickly. i / d t Performance will also be improved;

[0048] (2) Based on the same principle as above, it can effectively improve the carrier extraction efficiency of the chip during the shutdown process, so as to facilitate faster and larger current shutdown, and can significantly improve the electric field under the gate, weaken the avalanche effect, reduce heat loss, and improve the shutdown current capability;

[0049] (3) Due to the presence of the trench gate, the thickness of the gate interconnect metal of the GCT chip can be increased, so the interconnect metal can withstand a larger current, enhance the gate metal current collection capacity of the GCT chip, reduce the parasitic parameters of the gate, increase the safe operating area of ​​the device, and improve the safety control capability of the device.

[0050] (4) The manufacturing process of the gate trench structure is relatively complex and requires precise processing and control to ensure that the geometry and size of the groove meet the design requirements.

[0051] In view of this, the present invention adopts a graphic process to prepare a trench structure in the gate area of ​​a semiconductor device so as to effectively adjust the various electrical indicators of the gate of the device, and thus combines the performance optimization requirements of the semiconductor device to propose a trench structure and develop a preparation process flow of the trench structure that is compatible with upstream and downstream processes.

[0052] Specifically, the present invention provides a semiconductor device chip, the semiconductor device chip includes a gate electrode, and the gate electrode has a groove structure;

[0053] Wherein, the semiconductor device chip is a bipolar semiconductor device chip in which both electrons and holes are conducted according to the diffusion principle, or a thyristor chip.

[0054] The semiconductor device chip is a chip of a GCT, IGCT, GTO, GTR, MCT or MTO type semiconductor device. Different from the prior art, the semiconductor device chip is not a chip of an insulated gate transistor and does not include an IGBT chip.

[0055] Among them, different from the trench gate, virtual trench and other structures in the prior art, the trench structure of the present invention can have at least one of the following functions: shorten the gate turn-off time, reduce the electric field peak, reduce heat loss, reduce the parasitic inductance during the gate convergence process, and increase the working junction temperature of the device.

[0056] Different from the gentle slope groove and isolation groove in the partial gate region in the prior art, the groove structure is located on the gate surface, and if there are multiple groove structures, they are not connected to each other.

[0057] The cross-sectional shape of the groove structure is a figure composed of a number of straight lines or curves, for example, it can be a polygon (triangle, bar / rectangle, square, rhombus, hexagon, cross, etc.), circle, ellipse, racetrack, etc.

[0058] The semiconductor device chip may include a plurality of cells, each of which includes a group of gates, and each group of gates includes only one group of gate trench structures.

[0059] The group of gate trench structures includes a single trench structure or a plurality of trench structures forming an array, such as a plurality of regularly arranged rows of strip trenches, or an array of equally spaced square, circular, hexagonal or cross-shaped trenches.

[0060] Wherein, the substrate material of the semiconductor device chip is, for example, selected from silicon, silicon carbide, gallium nitride, gallium arsenide or III-IV compounds.

[0061] Wherein, the aspect ratio of each of the groove structures is greater than or equal to 1:20, for example, it can be 1:20 to 20:1, such as 1:20, 1:10, 1:5, 1:1, 2:1, etc.

[0062] The depth of each trench structure is, for example, 0.5-30 micrometers, and the depth of the trench structure is less than the depth of the P+ region on the front side (the side where the gate is located).

[0063] Wherein, the sidewall of the groove structure maintains a gradual change.

[0064] The gate electrode may have a planar junction or a curved junction, such as a wavy junction.

[0065] Among them, the inner surface of the groove structure, such as the sidewall and bottom surface of the groove structure, can be metal-doped. The metal doping is achieved, for example, by pre-diffusion or ion implantation, etc., the purpose of which is to alloy the metal, reduce the gold-semiconductor contact resistance between the groove surface and the metal alloy, and enhance its current carrying capacity.

[0066] The groove structure is filled with metal, and the metal filling is achieved by, for example, metal evaporation or sputtering technology.

[0067] The metal used for metal doping or filling can be a conductive metal or alloy, such as a single metal such as gold, silver, copper, titanium, nickel, aluminum, or an alloy such as aluminum-silicon-copper, titanium-nickel-silver, etc.

[0068] Among them, the metal filling void rate of the trench structure is ≤10 / piece, and the void diameter is ≤2μm.

[0069] The metals filled in the trench structures are not interconnected through conductors.

[0070] In which, except for the filling metal, no other structures are designed and arranged in the trench structure, and no other components are filled.

[0071] Wherein, the semiconductor device chip also includes an N-drift region and a P-region and a P+ region formed on both sides of the N-drift region, wherein the P+ region is formed on the side of the P-region facing away from the N-drift region; the semiconductor device chip also includes a cathode and an anode, wherein the gate is formed on the P+ region on one side, the cathode is formed on a high platform structure formed on the P+ region on the same side, and the anode is formed on the P+ region on the other side of the N-drift region.

[0072] The doping concentration of the P-region on both sides ranges from 1E15 to 9.99E17 cm -3 .

[0073] The lateral non-uniformity of the doping concentration of the P-region on both sides is ≤10%.

[0074] The doping elements of the double-sided P-regions may be selected from boron, aluminum, gallium, and indium.

[0075] Among them, the doping concentration of the P+ region on both sides is 1E15-9.99E20 cm -3 .

[0076] The depth of the double-sided P+ regions is, for example, 3-100 μm.

[0077] The doping depth of the P+ region is less than that of the P- region, and the doping concentration of the P+ region is higher than that of the P- region.

[0078] The doping concentration of the P-regions on both sides varies gradually in the longitudinal direction, and the depth range is, for example, 5-200 μm.

[0079] When the doping element of the P- region is aluminum, the doping element of the P+ region is boron.

[0080] The height of the mesa structure forming the cathode is, for example, 0.5-20 μm.

[0081] The shape of the table top of the high table structure forming the cathode may be, for example, cylindrical, strip (including square column) or hexagonal column.

[0082] The high platform structure forming the cathode also includes a cathode N+ region, and the doping concentration of the cathode N+ region is 1E15-9.99E20 / cm 3 The doping depth of the cathode N+ region is greater than the table height of the mesa structure and covers the bottom corner of the side wall of the mesa structure.

[0083] Wherein, the cathode comprises cathode comb bars, and the doping concentration non-uniformity of the cathode comb bars is ≤10%.

[0084] Among them, a high dielectric passivation dielectric layer, namely a gate cathode dielectric layer, is also included between the gate and the cathode; the material for preparing the gate cathode dielectric layer is selected from silicon dioxide, silicon nitride, phosphosilicate glass, borosilicate glass, borophosphosilicate glass, etc.

[0085] Wherein, the gate cathode dielectric layer may have a thickness greater than 0.1 μm, and a thickness non-uniformity of ≤5%.

[0086] Wherein, the gate, cathode and anode respectively include metal electrode layers.

[0087] The material for preparing the metal electrode layer can be selected from gold, silver, copper, titanium, nickel, aluminum, aluminum silicon copper, titanium nickel silver.

[0088] The thickness of the metal electrode layer is, for example, 0.5-60 μm, and the thickness non-uniformity is ≤10%.

[0089] The doping depth of the P+ region is less than that of the P- region, and the doping concentration of the P+ region is higher than that of the P- region.

[0090] When the doping element of the P- region is aluminum, the doping element of the P+ region is boron.

[0091] The height of the cathode platform structure is 0.5-20 μm.

[0092] Among them, the cathode platform structure has a cylindrical, strip (including square column), hexagonal prism and the like shape.

[0093] The cathode platform structure also includes a cathode N+ region, and the doping concentration of the cathode N+ region is 1E15-9.99E20 / cm 3 , the doping depth is greater than the mesa height and covers the bottom corner of the mesa sidewall.

[0094] Among them, the doping concentration non-uniformity of the cathode comb strips of the entire wafer is ≤10%.

[0095] Therein, a layer of high dielectric passivation medium is also included between the gate cathodes, which is called the gate cathode dielectric layer. The material for preparing the gate cathode dielectric layer is silicon dioxide, silicon nitride, phosphosilicate glass, borosilicate glass, borophosphosilicate glass, etc.

[0096] Wherein, the gate cathode dielectric layer has a thickness greater than 0.1 μm and a thickness non-uniformity of ≤5%.

[0097] Wherein, the gate, cathode and anode include metal electrode layers.

[0098] The metal electrode layer is made of gold, silver, copper, titanium, nickel, aluminum and other metals, or aluminum-silicon-copper, titanium-nickel-silver and other alloys.

[0099] Wherein, the thickness of the metal electrode layer is 0.5-60 μm, and the thickness non-uniformity is ≤10%.

[0100] The semiconductor device chip may further include a PI glue passivation layer in the active area, which is used to cover all areas except the metal electrode layer on the high platform structure of the cathode.

[0101] The PI glue passivation layer can be prepared by photosensitive or non-photosensitive PI glue.

[0102] Wherein, when preparing the PI glue passivation layer, the coating thickness of the PI glue is, for example, 0.5-30 μm, and the thickness non-uniformity is ≤10%.

[0103] Wherein, the semiconductor device chip may further include a terminal structure.

[0104] Wherein, the terminal structure includes an angled structure, and the angled structure has a single angle, a double angle, or multiple angles, that is, the angled structure is a single angle, a double angle, or a multiple angle structure.

[0105] The bevel covers and passes through (overlaps) the PN-interface on the front and back sides (both sides), and the bevel angle and shape are determined according to the voltage blocking requirements and terminal structure dimensions of the semiconductor device.

[0106] Wherein, the terminal structure also includes a surface passivation layer, and the material for preparing the surface passivation layer is selected from PI glue, diamond-like carbon (DLC), silicon oxide, silicon nitride, such as DLC film, silicon oxide film, silicon nitride film, etc.

[0107] The present invention also provides a method for manufacturing a semiconductor device chip, comprising the following steps:

[0108] After forming the gate, further preparing a desired trench structure on the gate by a patterning process;

[0109] Wherein, the semiconductor device chip is a bipolar semiconductor device chip in which both electrons and holes are conducted according to the diffusion principle, or a thyristor chip.

[0110] Wherein, the semiconductor device chip is a chip of a GCT, IGCT, GTO, GTR, MCT or MTO type semiconductor device.

[0111] The manufacturing method further comprises the step of performing metal doping on the inner surface of the formed trench structure by pre-diffusion or ion implantation.

[0112] The manufacturing method further comprises the step of filling metal in the formed groove structure by metal evaporation or sputtering technology.

[0113] The metal used for metal doping or filling is selected from gold, silver, copper, titanium, nickel, aluminum, aluminum silicon copper, titanium nickel silver.

[0114] Wherein, the metal filling void ratio of the groove structure is ≤10 per piece, and the void diameter is ≤2 μm.

[0115] Among them, the preparation method also includes other parameter characteristics that are the same as the characteristics of the above-mentioned semiconductor device chip, which will not be repeated here.

[0116] The invention also discloses a semiconductor device chip prepared based on the manufacturing method of the semiconductor device chip.

[0117] The present invention also discloses a semiconductor device comprising the semiconductor device chip, wherein the semiconductor device is, for example, a GCT, an IGCT, a GTO, a GTR, a MCT, a MTO, etc.

[0118] The present invention also discloses an electronic device using the semiconductor device, such as a rectifier, a converter, an inverter, a power switch, a switching circuit device, etc.

[0119] In a preferred embodiment, the present invention proposes a trench gate integrated gate commutated thyristor and a manufacturing method thereof for a GCT device. The specific method roadmap is as follows: Figure 1 As shown, it includes gate trench structure design and terminal structure design based on the GCT device cell structure, as well as process methods and processes for realizing the trench structure, such as trench structure graphics technology, surface doping technology, metallization technology, and other technologies such as dielectric layer and terminal process.

[0120] Implementation method:

[0121] (1) With respect to the trench gate integrated gate commutated thyristor and its manufacturing method of the present invention, its structural design mainly includes the gate trench type design method based on the GCT cell structure, morphology requirements, dimension design basis, etc. The cross-sectional schematic diagram of the GCT cell structure and the terminal structure is shown in FIG. Figure 2 shown.

[0122] The specific process is as follows:

[0123] (I) Figure 3A , 3B The schematic diagrams of the cross-sectional structures of the planar junction and the curved junction of the prior art are shown in the figure. As shown in the figure, the gate trench design method based on the GCT cell structure is specifically based on Figure 2 In the J2 position, you can Figure 3A , Figure 3B , divided into two types: plane knots and curved knots.

[0124] (II) The morphology requirements of the gate trench structure applicable to the GCT chip, specifically, the sidewall morphology requirements of the trench structure based on device performance improvement and the overall adaptability requirements of the cell structure. The morphology described in this step can be a single trench structure or multiple trench structures. Figure 4C is a top view of the groove structure type of the present invention, the morphology described in this step, wherein the structure type can be as follows Figure 4C The structures shown include various types of arrays such as bars, circular holes, squares, hexagons, etc.

[0125] (III) Figures 4A-4B All of them are cross-sectional views of the trench structure type of the present invention. Based on the structural dimension design basis of the trench gate GCT chip, specifically, based on Figure 4A , Figure 4B , including the width and depth of a single groove structure of the groove structure, the width, depth, and spacing of the array groove structure, etc.

[0126] (2) The trench gate integrated gate commutated thyristor and the manufacturing method thereof of the present invention are mainly directed to the structure of the above step (1), and the core processes required for the implementation process thereof include:

[0127] (I) Preparatory work: specifically, it includes edge detection, surface particle and defect detection, and wafer pre-cleaning process for wafers. In addition, it is also necessary to consider the preparation and detection of the layout. The prepared materials include semiconductor substrates and materials for manufacturing metal electrodes. The semiconductor substrates can be silicon, silicon carbide, III-IV compounds, etc.

[0128] Optionally, the size of the semiconductor substrate is, for example, 2, 4, 6, 8, 12, 16 inches, etc.

[0129] (II) Graphical process: specifically, including multiple photolithography processes, etching and etch processes of semiconductor substrates, etching or etch processes of dielectric layers, photolithography of PI glue, and etching or etch processes of metal layers, etc.;

[0130] ① Photolithography process: Specifically, the structure design pattern in step (1) is irradiated with ultraviolet light to the photoresist, and then the design pattern is transferred to the mask layer on the surface of the wafer using the development technology;

[0131] Preferably, the specific steps include: (a) cleaning and processing of the substrate; (b) photoresist coating; (c) photoresist pre-baking; (d) mask exposure; (e) photoresist development; (f) photoresist hardening, thereby forming the desired masking layer pattern.

[0132] Optionally, the thickness of the photoresist produced in the process of coating may be 0.01-10 μm.

[0133] Optionally, the temperature of the photoresist baking may be 80-150°C.

[0134] Optionally, the wavelength of photoresist exposure is determined according to the specific type of photoresist and process requirements. Different photoresists have different responses and sensitivities to light sources of different wavelengths. Ultraviolet (UV) exposure is more commonly used, and common wavelengths are 436nm, 405nm, 365nm, 248nm and 193nm.

[0135] Optionally, the development process requires the use of a developer. The developer of negative photoresist is mainly xylene and butyl acetate, and the developer of positive photoresist is mainly tetramethylammonium hydroxide, etc.

[0136] ② Corrosion and etching process of semiconductor substrate: Specifically, under the protection of the mask prepared by the above-mentioned ① photolithography process, the semiconductor substrate is corroded or etched, and the mask pattern after the photolithography process is further transferred to the surface of the semiconductor substrate;

[0137] Necessarily, in the case where a hard mask layer (such as silicon dioxide, silicon nitride, etc. mask) is required for the corrosion or etching of some semiconductor substrates, it is necessary to first transfer the photolithographic pattern of the hard mask layer, and then, under the protection of the hard mask layer, corrode or etch the semiconductor substrate to further transfer the pattern of the hard mask layer to the metal layer.

[0138] ③ Etching or corrosion process of the dielectric layer: Specifically, under the protection of the mask prepared by the above-mentioned ① photolithography process, the dielectric layer is corroded or etched, and the mask pattern after the photolithography process is further transferred to the dielectric layer. Optionally, the dielectric layer includes an insulating medium with high dielectric capacity such as silicon dioxide, silicon nitride, boron / phosphosilicate glass, etc.;

[0139] ④ Photolithography process of PI glue: Specifically, for photosensitive PI glue, photolithography irradiation and development methods can be directly used to achieve it; for non-photosensitive PI glue, a photoresist mask is coated, and then the photoresist is subjected to photolithography process according to the above method ① to realize the transfer of the designed pattern to the photoresist layer. After that, development, corrosion, etching and other technologies are used to transfer the pattern of the photoresist layer to the underlying non-photosensitive PI glue layer.

[0140] ⑤ Etching or corrosion process of the metal layer: Specifically, under the protection of the mask prepared by the above-mentioned ① photolithography process, the metal layer is corroded or etched, and the mask pattern after the photolithography process is further transferred to the metal layer;

[0141] Optionally, the etching process of the metal film pattern can be wet etching or dry etching. In addition, electron beam exposure and etching, laser etching, etc. can also achieve the patterning of the metal film.

[0142] Preferably, the commonly used gases for dry etching of metals are chlorine-based, fluorine-based and other gases. The specific parameter settings include etching gas and its composition ratio, etching power, etching pressure, etching time, gas flow rate and ambient temperature, etc. These parameters need to be optimized and adjusted according to the specific equipment and etching targets.

[0143] (III) Doping process: specifically, including the implementation methods and process flow of P-type and N-type pre-diffusion, push-diffusion doping, and injection doping in different regions;

[0144] ① For GCT chips, the P-type region refers to the gate Pbase and P+ regions, which are B and Al elements; and the anode Pbase region, which is Al element, is prepared by pre-diffusion (or source deposition diffusion), followed by long-term high-temperature advancement, and diffusion process. The depth requirement is 50-200μm, which can be designed according to the chip performance requirements;

[0145] ② For the trench structure, specifically, a higher concentration of doping is required on its surface. Optional methods include pre-diffusion and ion implantation, which are beneficial to reduce the contact resistance between the trench surface and the metal alloy and enhance its current capacity.

[0146] (IV) Metallization process: specifically, including metal filling of the trench gate 109, metal evaporation or sputtering technology of the gate electrode 3, cathode electrode 2, anode electrode 1, etc., and alloying process of the gate, cathode, anode metal layers and the semiconductor surface;

[0147] In particular, for the metal filling of the trench gate 109 , the effect of the depth-to-width ratio of the trench structure needs to be considered, and the morphology of the trench structure is required to maintain a gradual change at the sidewall.

[0148] Optionally, the evaporation process may be thermal evaporation, electron beam evaporation, pulsed laser source evaporation, multi-component thin film evaporation, etc., preferably electron beam evaporation.

[0149] Optionally, the sputtering process may be direct current sputtering, radio frequency sputtering, magnetron sputtering, reactive sputtering, etc., preferably the magnetron sputtering process.

[0150] Alternatively, the alloying process is usually carried out at high temperatures, the specific temperature depends on the metal used and the alloying method, and the annealing time of the alloying process is generally between a few minutes and a few hours.

[0151] In addition, optionally, when the thickness of the deposited metal layer is small, metal patterning can also be achieved by a metal lift-off process, and the process steps are photolithography-deposition of metal layer-stripping-cleaning.

[0152] (V) Other processes: specifically, including the oxidation process, dielectric layer preparation process, PI glue passivation process, terminal molding process, etc. included in the manufacturing process of trench gate integrated commutation thyristor;

[0153] Optionally, the oxidation process includes wet oxygen technology, dry oxygen technology, etc.

[0154] Specifically, the dielectric layer preparation process includes plasma enhanced chemical vapor deposition (PECVD) technology, low pressure chemical vapor deposition (LPCVD) technology, TEOS technology, oxidation densification technology, etc., preferably oxidation densification technology, especially by passing oxygen to oxidize the surface of the semiconductor substrate to form silicon dioxide, and then high temperature annealing to further densify the oxide layer. The dielectric layer material includes high dielectric insulating materials such as silicon dioxide, silicon nitride, borosilicate glass, phosphosilicate glass, and borophosphosilicate glass.

[0155] Specifically, the PI glue passivation process includes the photolithography and curing technology of the PI glue in the active area, and the coating and curing technology of the PI glue in the terminal area. Optionally, the PI glue includes photosensitive type, non-photosensitive type, etc.

[0156] Specifically, the terminal forming process includes rounding to remove edges, terminal bevel grinding and polishing, terminal surface corrosion to reduce roughness, terminal red glue curing and other processes.

[0157] (3) Figure 5 The present invention is a process flow chart of the preparation of the trench gate integrated gate commutated thyristor. The present invention is mainly aimed at the structure of the above step (1) and based on the key process of the above step (2), the process flow of the implementation process is as follows: Figure 5 shown.

[0158] Based on the above process flow, the implementation steps of the present invention are as follows:

[0159] (I) Wafer inspection and pre-cleaning: Specifically, wafer inspection includes inspection of wafer defects, surface particles, edge cracks, surface flatness, roughness, wafer thickness and uniformity, wafer resistivity and uniformity, etc. Optional inspection methods include visual inspection, optical inspection, electrical inspection, thermal inspection, mechanical inspection, etc.; wafer pre-cleaning includes the removal of pollutants such as wafer surface protective film and dust particles that affect chip performance, making the surface cleaner. Optional cleaning methods include RCA, acid solutions with different ratios, nitrogen chamber purging, deionized water washing, surface grinding, etc.;

[0160] Necessarily, the surface defects must be less than 5 / piece, and the particles and other contaminants must be less than 10 / piece;

[0161] (II) Preparation of double-sided alignment marks: Specifically, photolithography, development, baking, etching, etc. are performed on the surface of the semiconductor wafer by applying glue, carrying out photoresist, forming front and back alignment marks required for subsequent photolithography process for pattern transfer;

[0162] Optionally, the etching process may be wet etching or dry etching.

[0163] Necessarily, the area where the double-sided alignment marks are located is within 0.1-4mm of the wafer edge and has a depth of 0.1-10μm. The specific size is based on the field of view of the photolithography machine used to execute the process to ensure that the alignment marks can be directly removed during the subsequent ring cutting (circle cutting) process to avoid affecting the wafer working area.

[0164] Necessarily, the mask such as the photoresist used to prepare the double-sided mark needs to be removed by an appropriate cleaning process after the mark preparation is completed before the next process can be carried out.

[0165] Necessarily, a photomask with front and back markings is required.

[0166] (III) Preparation of double-sided P-region (anode side P-region 103, cathode side P-region 105): Specifically, for the planar junction P-region, a layer of pre-doped P-type region can be directly prepared on the front and back sides of the wafer by diffusion or injection process, and then advanced to the required depth by high-temperature diffusion technology. The optional temperature range is 1000-1350°C, and the time can be determined according to the required advancement depth. The doping concentration range is 1E15-9.99E17cm -3 The lateral non-uniformity of the doping concentration is required to be ≤10%. Preferably, the doping concentration can change slowly in the longitudinal direction, and the depth range is required to be 5-200μm.

[0167] For the wave junction P-region, it is necessary to first prepare a patterned mask on the front side, and then pre-diffusion of P-type elements is performed on the front side. Under the protection of the patterned mask on the front side, the wafer surface is pre-diffused to form a P-type region in the area without the mask, while there is no P-type pre-diffusion element in the area with the mask. In addition, the entire back side is pre-diffused. Then, high-temperature diffusion technology is continued to be used to push the pre-doped P-type elements on the front and back sides of the wafer to the required depth. The process conditions are consistent with those of the planar junction.

[0168] Specifically, the wave junction P-type pre-doping mask can usually be a medium such as high-density silicon oxide and silicon nitride. The patterning process can be prepared by photolithography plus etching process, and the thickness needs to be ≥0.4μm. Necessarily, the patterning mask needs to be removed by a suitable cleaning process after pre-diffusion doping.

[0169] Optionally, the optional doping elements of the anode side P-region 103 and the cathode side P-region 105 are, for example, trivalent elements, such as boron, aluminum, gallium, indium, and the like.

[0170] Thus, an anode side P-region 103 and a cathode side P-region 105 can be prepared on both sides of the wafer, and the area in the middle of the wafer that has not been diffused or implanted is the N-drift region 104 .

[0171] (IV) Preparation of double-sided P+ region (anode side P+ region 102, cathode side P+ region 106): Specifically, the preparation method of the same plane junction P- region is to first pre-dope a layer of high concentration of P-type elements on the front and back sides of the wafer, and then use high temperature diffusion technology to advance to the required depth;

[0172] Specifically, the process conditions can refer to the above step (III), and the doping concentration of the anode side P+ region 102 and the cathode side P+ region 106 is 1E15~9.99E20 cm -3 , depth of 3-100μm.

[0173] Necessarily, the doping depth of the P+ region 102 on the anode side and the P+ region 106 on the cathode side should be smaller than the doping depth of the P- region 103 on the anode side and the P- region 105 on the cathode side, and the doping concentration of the P+ region 102 on the anode side and the P+ region 106 on the cathode side should be higher than the doping concentration of the P- region 103 on the anode side and the P- region 105 on the cathode side.

[0174] Optionally, the high temperature diffusion processes for preparing the anode side P+ region 102 and the cathode side P+ region 106 and the anode side P− region 103 and the cathode side P− region 105 may be performed simultaneously.

[0175] Preferably, when the doping element of the anode side P- region 103 and the cathode side P- region 105 is aluminum, the doping element of the anode side P+ region 102 and the cathode side P+ region 106 is boron.

[0176] (V) Preparing a cathode platform structure: Specifically, the platform structure design pattern can be transferred to the wafer surface through a patterning process such as photolithography and etching to form a platform structure, wherein one platform structure corresponds to the cathode of one unit cell;

[0177] Necessarily, the specific dimensions of the high platform structure need to refer to the process capability during the preparation process and the cell size design corresponding to the chip performance, where the platform height is 0.5-20μm.

[0178] Optionally, the photolithography mask of the patterning process can be a positive photoresist, a negative photoresist, or a photosensitive PI glue; the etching mask can be a hard mask, such as silicon dioxide, silicon nitride, metal, etc., or it can be a photoresist. If a hard mask is selected, the hard mask needs to be etched to transfer the photoresist mask pattern to the hard mask layer, and then the wafer is subjected to mesa etching under the protection of the patterned hard mask.

[0179] Optionally, the etching technology in the patterning process may be wet etching or dry etching, or a combination of wet etching and dry etching to prepare the desired gradually varying mesa sidewall structure.

[0180] Optionally, the shape of the platform structure can be cylindrical, rectangular, square, hexagonal, etc.

[0181] (VI) Preparation of gate trench structure: Specifically, based on the previous step, the gate trench structure design pattern is further transferred to the wafer surface through patterning processes such as photolithography and etching, and the required trench structure is prepared in the gate region, wherein one cell generally includes one gate trench structure. The gate trench structure of the present invention can be located on the trench gate 109 or on the gate ring 110 with a lead-out structure.

[0182] Necessarily, the specific size of the gate trench structure needs to refer to the process capability during the preparation process and the cell size design corresponding to the chip performance. The depth of the gate trench structure is 0.5-30 microns, and the trench depth is required to be less than the depth of the front P+ region.

[0183] Optionally, the photolithography mask, etching mask, etching technology, etc. in the patterning process are consistent with the previous step.

[0184] Optionally, the groove structure may be a single groove or a plurality of parallel grooves, and the groove shape may be a circular hole, a long strip, a hexagon, a square, or the like.

[0185] (VII) Preparation of cathode N+ region: Specifically, the pre-doped layer of the N+ region is usually prepared before steps (V) and (VI). In the subsequent wafer etching process, only the pre-doped layer on the surface of the cathode platform structure is retained, and the pre-doped layers in other areas are etched away during the patterning process. Then, in this step, the doped N-type element is pushed into all areas of the cathode platform through a high-temperature push-in process;

[0186] Necessarily, the doping concentration of the cathode N+ region is required to be 1E15-9.99E20 / cm 3 The doping depth is required to be greater than the table height and cover the bottom corner of the table side wall. The doping concentration non-uniformity of the comb strips of the entire wafer is ≤10%.

[0187] Optionally, the temperature of the high temperature driving process in the process of preparing the N+ region is 1000-1350° C. and the time is 0.1-5 hours.

[0188] (VIII) Preparing a gate cathode dielectric layer 108: Specifically, a layer of high dielectric passivation dielectric is prepared on the surface between the gate cathodes;

[0189] Optionally, the preparation process may adopt an oxidation process, a LPCVD process, a PECVD process, a TEOS process, etc.

[0190] Optionally, the material of the passivation dielectric layer may be silicon dioxide, silicon nitride, phosphosilicate glass, borosilicate glass, borophosphosilicate glass, or the like.

[0191] Optionally, the thickness of the passivation dielectric layer is greater than 0.1 μm, and the thickness non-uniformity is required to be ≤5%.

[0192] Optionally, the preparation process includes the preparation of a dielectric layer, a patterning process of the dielectric layer, etc., to ensure that there is no dielectric layer on the upper part of the gate trench and the upper part of the cathode platform structure.

[0193] (IX) Preparing gate / cathode / anode metals: Specifically, a metal electrode layer is prepared on the upper part of the trench of the P+ region 102 on the anode side of the gate, the upper part of the N+ region of the cathode platform structure, and the surface of the P+ region 102 on the anode side;

[0194] Optionally, the preparation process may be metal evaporation or sputtering technology, etc.

[0195] Optionally, the metal layer material may be gold, silver, copper, titanium, nickel, aluminum or other metals, or aluminum-silicon-copper, titanium-nickel-silver or other alloys.

[0196] Optionally, the thickness of the metal layer is 0.5-60 μm, and the thickness non-uniformity is required to be ≤10%.

[0197] Essentially, the metal filling void ratio of the trench structure is ≤10 / sheet and the void diameter is ≤2μm.

[0198] Optionally, the gate / cathode / anode metal layer preparation process includes processes such as preparation of the metal layer, patterning of the metal layer, alloying of the gold semi-contact, etc.

[0199] (X) Preparing a PI glue passivation layer 107 in the active area: Specifically, after the above step, a PI glue passivation layer 107 is prepared in the active area, and the passivation layer covers all areas except the metal electrode on the cathode table;

[0200] Optionally, the coating process of PI glue can adopt spin coating, spray coating and other technologies.

[0201] Optionally, PI glue can be photosensitive or non-photosensitive.

[0202] Optionally, the thickness of the PI glue is 0.5-30 μm, and the thickness non-uniformity is required to be ≤10%.

[0203] Optionally, the preparation process of the PI glue passivation layer 107 includes a photolithography process, a curing process, etc., wherein the temperature of the curing process is selected to be 2-15 hours, and the curing temperature is 150-410°C.

[0204] (XI) Preparation of terminal structure: Specifically, the wafer terminal structure is prepared by determining the chip size through circular cutting, preparing an angled terminal, preparing a terminal surface passivation layer, preparing a terminal red glue 4, etc.

[0205] Optionally, the process flow is wafer edge annular cutting - bevel grinding and polishing - bevel surface etching - bevel surface passivation - red glue injection and curing, etc.

[0206] Optionally, the wafer edge is cut in an annular shape, referred to as ring cutting or circle cutting, and laser cutting, wire cutting, water cutting and the like can be selected, and a process with higher cutting accuracy is preferred.

[0207] Optionally, the bevel polishing can be single bevel, double bevel, multi-bevel and other shapes. If necessary, the bevel needs to cover and penetrate the PN-interface on the front and back sides. The bevel angle and shape of the bevel terminal and the terminal passivation layer 111 can be determined according to the voltage blocking requirements and terminal size of the chip.

[0208] Optionally, the terminal surface passivation layer may be PI glue, DLC film, silicon oxide film, silicon nitride film, etc.

[0209] Optionally, the red glue injection 4 and curing process are common processes for thyristors and will not be described in detail here.

[0210] The present invention will be further described below through specific examples. It should be noted that the following examples are only for illustration and are not intended to limit the present invention.

[0211] Example 1 and Comparative Example 1

[0212] Figure 6 is a schematic cross-sectional view of a trench structure of a gate according to an embodiment of the present invention; Figure 6 As shown, the groove structure is a single groove structure with a rectangular cross section, a width of 60 μm, a depth of 45 μm, and a depth-to-width ratio of 3: 4. In contrast, the comparative example 1 does not have the groove structure on the cell. Figure 7 is a comparison curve diagram of the turn-off loss of Example 1 of the present invention and Comparative Example 1; Figure 81 is a comparative curve diagram of the turn-off time of Example 1 of the present invention and Comparative Example 1. As shown in the figure, by calculating the turn-off time and turn-off loss of the two devices, it can be found that the turn-off time of Example 1 of the present invention is improved by 2.3 μs, and the turn-off loss is reduced by 6.18%.

[0213] It can be seen that the groove structure of the present invention can overcome the limitations of traditional gates, reduce the electric field concentration effect, increase the uniformity of electric field distribution, reduce gate resistance, increase the switching speed of the device, reduce leakage current, improve current carrying capacity, etc. It can improve the switching characteristics, current balancing effect, and large current shutdown capability of semiconductor devices including IGCT, GTO, etc., thereby improving the switching safety, control flexibility and long-term reliability of the chip.

[0214] The above description is only a preferred embodiment of the embodiment of the present invention and is not intended to limit the embodiment of the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the embodiment of the present invention should be included in the scope of protection of the embodiment of the present invention.

Claims

1. A semiconductor device chip, characterized in that: The semiconductor device chip comprises a gate, and the gate has a plurality of groove structures; wherein the plurality of groove structures are located on the surface of the gate and are not connected to each other; the depth of each of the plurality of groove structures is 0.5-30 microns, and the depth of the groove structure is less than the depth of the P+ region on the surface where the gate is located; the aspect ratio of each of the plurality of groove structures is greater than or equal to 1:20; the groove structure is filled with metal, and in addition to the metal filling, no other structure is designed and arranged in the groove structure, and no other components are filled; The groove structure has at least one of the following functions: shortening the gate turn-off time, reducing the electric field peak, reducing heat loss, reducing the parasitic inductance during the gate merging process, and increasing the working junction temperature of the device; Wherein, the semiconductor device chip is a bipolar semiconductor device chip in which both electrons and holes are conducted according to the diffusion principle, or a thyristor chip.

2. The semiconductor device chip according to claim 1, characterized in that: The semiconductor device chip is a chip of a GCT, IGCT, GTO, GTR, MCT or MTO type semiconductor device; and / or The gate includes a gate pole piece and a gate lead-out structure.

3. The semiconductor device chip according to claim 1, characterized in that: The cross-sectional shape of the groove structure is a figure composed of a plurality of straight lines or curves.

4. The semiconductor device chip according to claim 3, characterized in that: The groove structure is an array of regularly arranged rectangles, circles, hexagons or crosses in cross section.

5. The semiconductor device chip according to claim 1, characterized in that: The semiconductor device chip includes a plurality of cells, each of which includes a group of gate electrodes, and each group of gate electrodes only includes a group of gate electrode trench structures.

6. The semiconductor device chip according to claim 5, characterized in that: The group of gate trench structures includes a single trench structure or a plurality of trench structures forming an array, wherein the plurality of trench structures forming the array are not connected to each other.

7. The semiconductor device chip according to claim 1, characterized in that: The substrate material of the semiconductor device chip is selected from silicon, silicon carbide, gallium nitride, gallium arsenide or III-IV compounds; and / or The sidewall of the groove structure maintains a gradual change; and / or The gate has a planar junction or a curved junction; and / or The inner surface of the trench structure is doped with metal by pre-diffusion or ion implantation.

8. The semiconductor device chip according to claim 7, characterized in that: When a metal doping or filling operation is performed, the doping or filling metal used is selected from gold, silver, copper, titanium, nickel, aluminum, aluminum silicon copper, titanium nickel silver; and / or The metals filled in the trench structure are not connected to each other through a conductor.

9. The semiconductor device chip according to claim 1, characterized in that: The semiconductor device chip also includes an N-drift region and a P-region and a P+ region formed on both sides of the N-drift region, wherein the P+ region is formed on the side of the P-region facing away from the N-drift region; the semiconductor device chip also includes a cathode and an anode, wherein a gate is formed on the P+ region on one side, a cathode is formed on a high platform structure formed on the P+ region on the same side, and an anode is formed on the P+ region on the other side of the N-drift region.

10. The semiconductor device chip according to claim 9, characterized in that: The doping concentration of the P-region on both sides ranges from 1E15 to 9.99E17 cm -3 ; and / or The lateral non-uniformity of the doping concentration of the P-region on both sides is ≤ 10%; and / or The doping elements of the double-sided P-region are selected from boron, aluminum, gallium, indium; and / or The doping concentration of the P+ region on both sides is 1E15-9.99E20 cm -3 ; and / or The depth of the P+ region on both sides is 3-100 μm; and / or The doping depth of the P+ region is less than the doping depth of the P- region, and the doping concentration of the P+ region is higher than the doping depth of the P- region.

11. The semiconductor device chip according to claim 10, characterized in that: The doping concentration of the P-region on both sides varies gradually in the longitudinal direction, with a depth range of 5-200 μm; and / or When the doping element of the P- region is aluminum, the doping element of the P+ region is boron.

12. The semiconductor device chip according to claim 9, characterized in that: The mesa height of the mesa structure forming the cathode is 0.5-20 μm; and / or The table top of the high table structure forming the cathode is cylindrical, elongated or hexagonal; and / or The high platform structure forming the cathode also includes a cathode N+ region, and the doping concentration of the cathode N+ region is 1E15-9.99E20 / cm 3 , the doping depth of the cathode N+ region is greater than the table height of the mesa structure and covers the bottom corner of the side wall of the mesa structure; The cathode includes cathode comb bars, and the doping concentration non-uniformity of the cathode comb bars is ≤10%.

13. The semiconductor device chip according to claim 9, characterized in that: A passivation dielectric layer, namely a gate cathode dielectric layer, is also included between the gate and the cathode. The material for preparing the gate cathode dielectric layer is selected from silicon dioxide, silicon nitride, phosphosilicate glass, borosilicate glass, and borophosphosilicate glass.

14. The semiconductor device chip according to claim 13, characterized in that: The gate cathode dielectric layer has a thickness greater than 0.1 μm and a thickness non-uniformity of ≤5%.

15. The semiconductor device chip according to claim 9, characterized in that: The gate, cathode and anode respectively include metal electrode layers; The material for preparing the metal electrode layer is selected from gold, silver, copper, titanium, nickel, aluminum, aluminum silicon copper, titanium nickel silver.

16. The semiconductor device chip according to claim 15, characterized in that: The thickness of the metal electrode layer is 0.5-60 μm, and the thickness non-uniformity is ≤10%.

17. The semiconductor device chip according to claim 9, characterized in that: The semiconductor device chip also includes a PI glue passivation layer in the active area, which is used to cover all areas except the metal electrode layer on the high platform structure of the cathode.

18. The semiconductor device chip according to claim 17, characterized in that: The PI glue passivation layer is prepared by photosensitive or non-photosensitive PI glue; When preparing the PI glue passivation layer, the coating thickness of the PI glue is 0.5-30 μm, and the thickness non-uniformity is ≤10%.

19. The semiconductor device chip according to claim 9, characterized in that: The semiconductor device chip also includes a terminal structure.

20. The semiconductor device chip according to claim 19, characterized in that: The terminal structure includes an angled structure, and the angled structure has a single angle, a double angle, or multiple angles.

21. The semiconductor device chip according to claim 20, characterized in that: The bevel covers and passes through the PN-interface on both sides, and the bevel angle and shape are determined according to the voltage blocking requirements and terminal structure dimensions of the semiconductor device.

22. The semiconductor device chip according to claim 19, characterized in that: The terminal structure also includes a surface passivation layer, and the material for preparing the surface passivation layer is selected from PI glue, diamond-like carbon, silicon oxide, and silicon nitride.

23. A method for manufacturing a semiconductor device chip, characterized in that: The steps include: After forming the gate, a plurality of mutually disconnected groove structures are further prepared on the surface of the gate by a graphic process, and metal is filled in the groove structure, and in addition to the metal filling, no other structure is designed and arranged in the groove structure, and no other components are filled; wherein the depth of each of the groove structures is 0.5-30 microns, and the depth of the groove structure is less than the depth of the P+ region on the surface where the gate is located; the aspect ratio of each of the groove structures is greater than or equal to 1:20; Preparing a metal electrode layer on the upper portion of the groove structure; Completing the manufacturing of the semiconductor device chip; The semiconductor device chip is a thyristor, or a chip of a bipolar semiconductor device in which both electrons and holes are conducted according to the diffusion principle.

24. The manufacturing method according to claim 23, characterized in that: The semiconductor device chip is a chip of a GCT, IGCT, GTO, GTR, MCT or MTO type semiconductor device.

25. The manufacturing method according to claim 23, characterized in that: The manufacturing method further comprises the step of performing metal doping on the inner surface of the formed trench structure by pre-diffusion or ion implantation; and / or The manufacturing method further comprises the step of filling the formed trench structure with metal by metal evaporation or sputtering technology.

26. The manufacturing method according to claim 25, characterized in that: The metal used for metal doping or filling is selected from gold, silver, copper, titanium, nickel, aluminum, aluminum silicon copper, titanium nickel silver; and / or The metal filling void ratio of the groove structure is ≤10 per piece, and the void diameter is ≤2 μm.

27. A semiconductor device chip, characterized in that: The semiconductor device chip is manufactured by the method for manufacturing a semiconductor device chip according to any one of claims 23 to 26.

28. A semiconductor device, characterized in that: The semiconductor device comprises a semiconductor device chip as claimed in any one of claims 1-22 and 27.

29. An electronic device, characterized in that: The electronic device includes the semiconductor device according to claim 28.

30. The electronic device according to claim 29, characterized in that The electronic device is a rectifier, a converter, an inverter, a power switch or a switching circuit device.

Citation Information

Patent Citations

  • Transverse varied doped-junction terminal extension composite terminal structure and manufacturing method thereof

    CN108598150A

  • A semiconductor device with a buffer layer structure

    CN112599587B

  • Trench gate MOS-GCT structure and preparation method thereof

    CN110364569A

  • Manufacturing method of power semiconductor device and power semiconductor device

    CN111933705A

  • Gate commutated thyristor GCT device structure and manufacturing method thereof

    CN115692489A