Pole thickness grouping adjustment method, device and battery
By matching the thickness of the pole sheet in intervals, we ensure that the total thickness of the cathode sheet, anode sheet and separator meets the standard specifications, solving the problem of pole ear dislocation, reducing the pole sheet scrap rate, and improving battery performance.
Patent Information
- Application Number
- CN202410899140.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-07-05
AI Technical Summary
During the battery manufacturing process, the thickness of the pole plate cannot be consistent, resulting in the dislocation of the pole ears during the winding process, increasing the scrap rate of the pole plate and affecting the battery performance.
By obtaining the thickness of the cathode sheet and anode sheet to be wound, dividing the thickness intervals of the same length, and matching them by interval, ensuring that the total thickness of the matching cathode sheet, anode sheet and diaphragm meets the standard specifications, thereby reducing pole ear dislocation.
It effectively reduces the pole ear misalignment caused by the winding process, reduces the pole scrap rate, and enhances battery performance.
Smart Images

Figure CN118448695B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of battery manufacturing, and in particular to a method, a device and a battery for adjusting the thickness of pole pieces by grouping. Background Art
[0002] The manufacturing process of multi-tab battery cells generally includes: reserving an empty foil area on the pole piece, forming the pole tab by die cutting, and forming a bare battery cell by winding the pole piece after die cutting. The winding core is formed by winding the cathode sheet, the diaphragm and the anode sheet together; in order to align the pole tabs after winding, the distance between the pole tabs is arranged in equal distances.
[0003] However, in the actual production process of batteries, since the thickness of the electrode sheets cannot be kept consistent, the total thickness of the cathode and anode sheets and the separator between two adjacent tabs is different from the preset thickness, which leads to the inconsistency between the winding circumference and the preset circumference, resulting in misalignment of the tabs. Figure 1 As shown in the figure, the misalignment of the tabs is as follows Figure 2 shown. Figure 2 (a) to (f) show the cathode and anode ears, with the left ear representing the cathode and the right ear representing the anode. Figure 2 (a)~(d) are schematic cross-sectional views of the battery. Figure 2 (a) shows that one side of the pole ear is misaligned. Figure 2 (b) shows the state where the tabs on both sides are misaligned in the same direction. Figure 2 (c) in the middle shows that both sides of the pole ears are displaced inwards. Figure 2 Middle (d) indicates that the tabs on both sides are displaced outward. Figure 2 (e) and (f) are top views of the battery. Figure 2 (e) in the middle shows that the tab has a C-type misalignment. Figure 2 (f) in the middle indicates that the pole ear has tailing misalignment.
[0004] Due to the influence of the winding core manufacturing method, if the thickness error of a pole piece is 1μm, then winding 40 turns will cause the pole ear to be misaligned by 4mm. However, the production and manufacturing of pole pieces inevitably have thickness errors, and it is impossible to ensure that the thickness of the pole pieces is completely consistent; and when the existing pole pieces are delivered to the winding machine for production, the thickness matching degree of the positive and negative pole pieces is poor, which further aggravates the pole ear misalignment in the winding process, increases the pole piece scrap rate, and affects the battery performance. Summary of the invention
[0005] To this end, the technical problem to be solved by the present invention is to overcome the deficiencies in the prior art and provide a method, device and battery for grouping and adjusting the thickness of a pole piece, which can reduce the misalignment of the pole lugs caused by the winding process, reduce the pole piece scrap rate and enhance battery performance.
[0006] In order to solve the above technical problems, the present invention provides a method for adjusting the thickness of pole pieces by groups, comprising:
[0007] Obtaining the thickness of the cathode sheet and the anode sheet to be wound, wherein the cathode sheet and the anode sheet to be wound are both provided with tabs;
[0008] Dividing a plurality of thickness intervals with the same interval length based on the standard thickness of the cathode sheet and the anode sheet, and classifying the cathode sheet and the anode sheet to be wound into the thickness intervals according to the thickness;
[0009] The cathode sheets and anode sheets to be wound within each thickness range are matched, and the diaphragms of corresponding thickness are matched according to the total thickness of the matched cathode sheets and anode sheets to be wound, so that the total thickness of the matched cathode sheets, anode sheets and diaphragms to be wound meets the standard specifications.
[0010] Furthermore, the thickness intervals of the cathode sheet and the anode sheet are divided into a plurality of intervals of the same length based on the standard thickness of the cathode sheet and the anode sheet, specifically:
[0011] Set the interval length to x, and take the standard thickness of the cathode sheet as the reference, and divide the thickness intervals of the cathode sheet into [d1-nx,d1-(n-1)x), …, [d1-ix,d1-(i-1)x), …, [d1-x,d1), (d1,d1+x], …, (d1+(i-1)x,d1+ix], …, (d1+(n-1)x,d1+nx]; where d1 represents the standard thickness of the cathode sheet, [d1-ix,d1-(i-1)x) represents the i-th thickness interval that is less than the standard thickness of the cathode sheet, (d1+(i-1)x,d1+ix] represents the i-th thickness interval that is greater than the standard thickness of the cathode sheet, and n is the total number of intervals divided on one side of the reference;
[0012] Based on the standard thickness of the anode sheet, the thickness intervals of the anode sheet are divided into [d2-nx, d2-(n-1)x), …, [d2-ix, d2-(i-1)x), …, [d2-x, d2), (d2, d2+x], …, (d2+(i-1)x, d2+ix], …, (d2+(n-1)x, d2+nx]; wherein d2 represents the standard thickness of the anode sheet, [d2-ix, d2-(i-1)x) represents the i-th thickness interval that is less than the standard thickness of the anode sheet, and (d2+(i-1)x, d2+ix] represents the i-th thickness interval that is greater than the standard thickness of the anode sheet.
[0013] Furthermore, the cathode sheets and anode sheets to be wound within the respective thickness ranges are matched, specifically:
[0014] Match the cathode sheet belonging to the thickness interval [d1-ix, d1-(i-1)x) with the anode sheet belonging to the thickness interval (d2+(i-1)x, d2+ix], and match the cathode sheet belonging to the thickness interval (d1+(i-1)x, d1+ix] with the anode sheet belonging to the thickness interval [d2-ix, d2-(i-1)x).
[0015] Furthermore, the cathode sheets and anode sheets to be wound within each thickness range are matched so that the total thickness of the matched cathode sheets and anode sheets to be wound meets the first standard specification; and the separators of standard thickness are matched so that the total thickness of the matched cathode sheets, anode sheets and separators to be wound meets the standard specification.
[0016] Furthermore, if there are at least two areas on the cathode sheet to be wound or the anode sheet to be wound whose thickness is not within a range, the anode sheet to be wound whose thickness is not within a range or the cathode sheet to be wound whose thickness is at least two areas is not within a range is used for matching, so that the thickness of each location on the cathode sheet to be wound and the anode sheet after matching meets the first standard specification.
[0017] Furthermore, the cathode sheets and anode sheets to be wound within each thickness range are matched, and the first thickness of the cathode sheets and anode sheets to be wound after matching does not meet the first standard specification; and the diaphragms with corresponding thickness ranges are matched, so that the total thickness of the cathode sheets, anode sheets and diaphragms to be wound after matching meets the standard specification.
[0018] Furthermore, the cathode sheets and anode sheets to be wound within each thickness range are matched, and the first thicknesses of the cathode sheets and anode sheets to be wound after matching are equal at each location and the first thicknesses do not meet the first standard specifications; then the diaphragms in the corresponding thickness ranges are matched, so that the total thicknesses of the cathode sheets, anode sheets and diaphragms to be wound after matching meet the standard specifications.
[0019] Furthermore, the cathode sheets and anode sheets to be wound within each thickness range are matched. If the first thickness of at least two regions of the matched cathode sheets and anode sheets to be wound are not within a range, the diaphragms of the corresponding thickness ranges are matched so that the total thickness of the matched cathode sheets, anode sheets and diaphragms to be wound meets the standard specifications.
[0020] The present invention also provides a device for adjusting the thickness of pole pieces by groups, comprising:
[0021] A laser thickness gauge is used to measure the thickness of the cathode sheet and the anode sheet to be wound, wherein the cathode sheet and the anode sheet to be wound are both provided with tabs;
[0022] The manufacturing operation management system divides a plurality of thickness intervals with the same length based on the standard thickness of the cathode sheet and the anode sheet, and classifies the cathode sheet and the anode sheet to be wound into the thickness intervals according to the thickness;
[0023] The logistics information management system receives information of cathode sheets and anode sheets of different thicknesses to be wound from the manufacturing operation management system, and generates tasks for transporting the cathode sheets and anode sheets to be wound;
[0024] An AGV module, including an AGV and an AGV scheduling system, wherein the AGV scheduling system receives tasks issued by the logistics information management system and notifies the AGV to transport cathode sheets and anode sheets to be wound;
[0025] The winding module includes a winding machine and a winding scheduling management system; the winding scheduling management system receives the cathode sheets and anode sheets to be wound transported by the AGV, matches the cathode sheets and anode sheets to be wound within each thickness range, matches the diaphragm of corresponding thickness according to the total thickness of the matched cathode sheets and anode sheets to be wound, so that the total thickness of the matched cathode sheets, anode sheets and diaphragm to be wound meets the standard specifications; the winding machine winds the matched cathode sheets and anode sheets to be wound to obtain a winding core.
[0026] The present invention also provides a battery, including a winding core, wherein the winding core is formed by winding cathode sheets and anode sheets, and the cathode sheets and anode sheets used during winding are selected using the electrode sheet thickness grouping and deployment method.
[0027] The above technical solution of the present invention has the following advantages compared with the prior art:
[0028] The present invention classifies the thickness of cathode sheets and anode sheets, and on this basis matches anode sheets, cathode sheets and separators according to different thicknesses, so that the total thickness of the matched cathode sheets, anode sheets and separators meets the standard specifications during winding, thereby reducing the misalignment of the pole lugs caused by the winding process, reducing the pole sheet scrap rate, and enhancing battery performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to make the content of the present invention more clearly understood, the present invention is further described in detail below according to specific embodiments of the present invention in conjunction with the accompanying drawings, wherein:
[0030] Figure 1 This is a schematic diagram of the tab in normal conditions.
[0031] Figure 2 This is a schematic diagram of the tab being misaligned.
[0032] Figure 3 is a flow chart of the method of the present invention.
[0033] Figure 4 It is the work flow chart of the device of the present invention.
[0034] Figure 5 It is a logic diagram for mixing materials during winding in the present invention. DETAILED DESCRIPTION
[0035] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention. Embodiment 1
[0036] Reference Figure 3 As shown, the present invention discloses a method for adjusting the thickness of pole pieces by groups, comprising the following steps:
[0037] S1: Obtaining the thickness of the cathode sheet and the anode sheet to be wound, both of which are provided with tabs. In this embodiment, a laser thickness gauge or other measuring device is used to obtain the thickness of the cathode sheet and the anode sheet to be wound.
[0038] S2: Divide the cathode sheet and the anode sheet into a plurality of thickness intervals of the same length based on the standard thickness of the cathode sheet and the anode sheet, and classify the cathode sheet and the anode sheet to be wound into the thickness intervals according to the thickness.
[0039] S2-1: Set the interval length to x, and take the standard thickness of the cathode sheet as the reference, and divide the thickness intervals of the cathode sheet into [d1-nx, d1-(n-1)x), …, [d1-ix, d1-(i-1)x), …, [d1-x, d1), (d1, d1+x], …, (d1+(i-1)x, d1+ix], …, (d1+(n-1)x, d1+nx]; wherein d1 represents the standard thickness of the cathode sheet, [d1-ix, d1-(i-1)x) represents the i-th thickness interval that is less than the standard thickness of the cathode sheet, (d1+(i-1)x, d1+ix] represents the i-th thickness interval that is greater than the standard thickness of the cathode sheet, and n is the total number of intervals divided on one side of the reference;
[0040] Based on the standard thickness of the anode sheet, the thickness intervals of the anode sheet are divided into [d2-nx, d2-(n-1)x), ..., [d2-ix, d2-(i-1)x), ..., [d2-x, d2), (d2, d2+x], ..., (d2+(i-1)x, d2+ix], ..., (d2+(n-1)x, d2+nx]; wherein d2 represents the standard thickness of the anode sheet, [d2-ix, d2-(i-1)x) represents the i-th thickness interval less than the standard thickness of the anode sheet, and (d2+(i-1)x, d2+ix] represents the i-th thickness interval greater than the standard thickness of the anode sheet. The value of the interval length x is determined according to the actual situation. In this embodiment, x is 1 μm, and the value of n is determined according to the thickness of the cathode sheet and the anode sheet actually produced.
[0041] S2-2: Cathode sheets and anode sheets to be wound having different thicknesses are classified into thickness ranges according to the thicknesses of the cathode sheets and anode sheets to be wound obtained by actual measurement.
[0042] S3: Match the cathode sheets and anode sheets to be wound in each thickness range. Specifically, match the cathode sheets in the thickness range [d1-ix, d1-(i-1)x) with the anode sheets in the thickness range (d2+(i-1)x, d2+ix], and match the cathode sheets in the thickness range (d1+(i-1)x, d1+ix] with the anode sheets in the thickness range [d2-ix, d2-(i-1)x).
[0043] Furthermore, according to whether the thickness of the matched cathode sheet and anode sheet to be wound is uniform at various locations, it can be divided into two situations:
[0044] The first situation is that the thickness of the matched cathode sheet and anode sheet to be wound is uniform everywhere. In this case, the total thickness of the matched cathode sheet and anode sheet to be wound meets the first standard specification.
[0045] The second situation is that the thickness of the cathode sheet or anode sheet to be wound after matching is uneven, that is, if the thickness of at least two regions on the cathode sheet or anode sheet to be wound is not within a range. In this case, the anode sheet to be wound or the cathode sheet to be wound with at least two regions whose thickness is not within a range is used for matching, so that the thickness of each region on the matched cathode sheet or anode sheet meets the first standard specification.
[0046] The thickness of each part of the matched cathode sheet and anode sheet meets the first standard specification. At this time, the separator of standard thickness is matched in S4 to ensure that the total thickness of the matched cathode sheet, anode sheet and separator to be wound meets the standard specification, which can avoid the problem of misalignment of the tabs caused by uneven thickness. Among them, the standard specification refers to the standard total thickness of the matched cathode sheet, anode sheet and separator to be wound.
[0047] However, in the actual production process, the difference in thickness of the cathode and anode sheets is caused by processing errors and has a certain degree of randomness, so the number of cathode sheets belonging to the thickness interval [d1-ix, d1-(i-1)x) and the number of anode sheets belonging to the thickness interval (d2+(i-1)x, d2+ix], or the number of cathode sheets belonging to the thickness interval (d1+(i-1)x, d1+ix] and the number of anode sheets belonging to the thickness interval [d2-ix, d2-(i-1)x) may be different. At this time, the electrode sheets with a thickness smaller than that of the adjacent thickness interval of the current thickness interval among the electrode sheets with a small number are used as compensation electrodes, and then a diaphragm of corresponding thickness is used for compensation. At this time, after matching the cathode sheets and anode sheets to be wound in each thickness interval, the first thickness of the matched cathode sheets and anode sheets to be wound will not meet the first standard specification.
[0048] Furthermore, according to whether the thickness of the cathode sheet and anode sheet to be wound is uniform, it is further divided into three cases:
[0049] The first situation is that the cathode sheet and the anode sheet to be wound after matching are uniform at all locations, that is, the first thicknesses at all locations of the cathode sheet and the anode sheet to be wound after matching are equal and do not meet the first standard specification.
[0050] The second situation is that there is unevenness in various parts of the cathode sheet and anode sheet to be wound after matching (that is, there are at least two areas of the first thickness of the cathode sheet and anode sheet after matching that are not in the same range), and the first thickness of various parts of the cathode sheet and anode sheet to be wound after matching are equal and the first thickness does not meet the first standard specification.
[0051] The third situation is that there are unevenness in various parts of the cathode sheet and anode sheet to be wound after matching (that is, there are at least two areas of the first thickness of the cathode sheet and anode sheet after matching that are not within the same range), and the first thickness of various parts of the cathode sheet and anode sheet to be wound after matching are not equal and do not meet the first standard specifications.
[0052] Furthermore, in S4, the cathode sheets and anode sheets matched in the above three cases are matched with the separators of corresponding thicknesses to ensure that the total thickness of the matched cathode sheets, anode sheets and separators to be wound meets the standard specifications, thereby avoiding the problem of misalignment of the tabs caused by uneven thickness.
[0053] Specifically, it includes the following situations:
[0054] In the first and second cases, the diaphragm of the corresponding thickness range is first matched according to the difference between the first thickness and the first standard specification, so that the total thickness of the cathode sheet, the anode sheet and the diaphragm meets the first standard specification; then the diaphragm of the corresponding thickness range is matched, so that the total thickness of the matched cathode sheet, the anode sheet and the diaphragm meets the standard specification.
[0055] In the third case, the diaphragms of different thickness ranges are first matched according to the gaps between the different first thicknesses at various locations and the first standard specifications, so that the total thickness of the cathode sheet, anode sheet and diaphragm meets the first standard specifications; and then the diaphragms of corresponding thickness ranges are matched, so that the total thickness of the matched cathode sheet, anode sheet and diaphragm meets the standard specifications.
[0056] In order to further illustrate the process of the method of the present invention, this embodiment takes the standard specifications of cathode sheet thickness of 30 μm, anode sheet thickness of 35 μm, and separator thickness of 10 μm as an example for illustration. When winding, there are four layers of cathode sheet, separator, anode sheet, and separator in sequence between two adjacent layers of pole ears. Therefore, the standard specification of the total thickness when winding is cathode sheet thickness + separator thickness + anode sheet thickness + separator thickness, that is, the total thickness of the standard specification is 85 μm.
[0057] Due to manufacturing errors, the actual thickness of the cathode and anode sheets produced will fluctuate around the standard thickness. The cathode and anode sheets are classified into thickness ranges according to the thickness difference, and the following is obtained:
[0058] The cathode sheet thickness is classified as: ..., 28μm, 29μm, 30μm, 31μm, 32μm, ...
[0059] The thickness of the anode sheet is classified as follows: ..., 33μm, 34μm, 35μm, 36μm, 37μm, ...
[0060] The cathode and anode sheets are matched and wound according to the difference from the standard thickness: that is, the sum of the difference between the cathode and anode sheets and their standard thickness is 0. The 31μm cathode sheet, 34μm anode sheet, and two 10μm separators are matched and wound, and the thickness of adjacent pole ears is: 31+34+10+10=85μm, which meets the standard specifications for total thickness.
[0061] For cathode and anode plates with uneven thickness:
[0062] If the 31μm anode sheet includes regions 1 and 2 of different thicknesses, the thickness of region 1 is 31.5μm, and the thickness of region 2 is 30.5μm; if the 34μm anode sheet has uniform thickness, a 10μm diaphragm with uniform thickness and a diaphragm with uneven thickness are selected for compensation. The compensation diaphragm includes regions A and B of different thicknesses, the thickness of region A is 10.5μm, and the thickness of region B is 9.5μm. Region A corresponds to region 2, and region B corresponds to region 1. On this basis, a 34μm anode sheet with uniform thickness and a 10μm diaphragm are used for matching winding. At this time, the thickness of the adjacent pole ears is 85μm, which meets the standard specifications of the total thickness.
[0063] If the 31μm anode sheet includes regions 1 and 2 with different thicknesses, the thickness of region 1 is 31.5μm, and the thickness of region 2 is 30.5μm; if the 34μm anode sheet includes regions A and B with different thicknesses, the thickness of region A is 33.4μm, and the thickness of region B is 34.5μm. Then region A corresponds to region 1, and region B corresponds to region 2, and then a 10μm diaphragm with uniform thickness and a diaphragm with uneven thickness are selected for compensation. The compensation diaphragm includes regions a and b with different thicknesses, and the thickness of region a is 10.1μm, and the thickness of region b is 10μm. Match regions A, region 1, and region a, and match regions B, region 2, and region b. On this basis, a 10μm diaphragm with uniform thickness is used for matching winding. At this time, the thickness of the adjacent pole ears is 85μm, which meets the standard specifications for the total thickness.
[0064] If the 31μm anode sheet includes regions 1 and 2 of different thicknesses, the thickness of region 1 is 31.5μm, and the thickness of region 2 is 30.5μm; if the 34μm anode sheet includes regions A and B of different thicknesses, the thickness of region A is 33.5μm, and the thickness of region B is 34.5μm. Then region A corresponds to region 1, and region B corresponds to region 2. On this basis, two 10μm separators are used for matching winding. At this time, the thickness of the adjacent tabs is 85μm, which meets the standard specification of the total thickness.
[0065] If the number of cathode sheets and anode sheets with corresponding thicknesses are not equal, there are 80 cathode sheets with a thickness of 31μm and 100 anode sheets with a thickness of 33μm, then there will be 20 anode sheets with a thickness of 33μm without corresponding cathode sheets. At this time, a diaphragm is used for compensation: the 20 unpaired 33μm anode sheets are matched with 30μm cathode sheets and matched with a 11μm thick diaphragm, and the total thickness is: 33+30+11+11=85μm, which meets the standard specifications for total thickness.
[0066] The cathode sheets, anode sheets and separators of different thicknesses are matched and wound to make the total thickness 85μm, thereby avoiding the problem of pole ear misalignment caused by different pole sheet thicknesses. This can reduce the pole ear misalignment caused by the winding process, reduce the pole sheet scrap rate, and enhance battery performance. Embodiment 2
[0067] The present invention also discloses a device for adjusting the thickness of a pole piece by grouping. The working process is as follows: Figure 4 As shown, it includes a laser thickness gauge, a manufacturing operation management system (MOM), a logistics information management system, an AGV module and a winding module.
[0068] The laser thickness gauge measures the thickness of each roll of cathode and anode sheets to be wound. Both the cathode and anode sheets to be wound are provided with pole ears. The laser thickness gauge measures the thickness of the pole sheet when it is rolled and wound. The thickness data recorded includes the thickness of the transverse and longitudinal regions. The longitudinal region is the width region of the pole sheet, and the thickness of the middle and both sides is measured respectively. The thickness of the transverse region is measured every predetermined length of 1μm. To reduce the error, each thickness value is measured multiple times and the average value is taken.
[0069] The manufacturing operation management system divides the cathode sheet and the anode sheet into a plurality of thickness intervals of the same length based on the standard thickness of the cathode sheet and the anode sheet, and classifies the cathode sheet and the anode sheet to be wound into the thickness intervals according to the thickness.
[0070] The logistics information management system receives information of cathode sheets and anode sheets of different thicknesses to be wound from the manufacturing operation management system, and generates tasks for transporting the cathode sheets and anode sheets to be wound.
[0071] The AGV module includes AGV (Automated Guided Vehicle) and AGV scheduling system. The AGV scheduling system receives tasks issued by the logistics information management system and notifies the AGV to transport the cathode sheets and anode sheets to be wound; the AGV transfers the pallet to the conveyor line connection port, and the conveyor line and stacker transfer the pallet to the stereoscopic warehouse for storage.
[0072] The winding module includes a winding machine and a winding scheduling management system. The winding scheduling management system receives the cathode and anode sheets to be wound from the AGV, and matches the cathode and anode sheets within the same thickness range on both sides of the reference (configure the thickness group, material model and other material calling information). The cache racks next to the winding module are configured in even numbers to store the cathode and anode sheets in pairs. The diaphragms of different thicknesses are matched according to the total thickness of the matched cathode and anode sheets, so that the total thickness of the matched cathode, anode and diaphragms meets the standard specifications during winding; the winding machine winds the matched cathode, anode and diaphragms to obtain a winding core, and the total thickness of the cathode and anode sheets and diaphragms formed by winding is consistent with the standard specifications of the total thickness, thereby avoiding misalignment of the tabs.
[0073] The electrode thickness grouping and allocation device in this embodiment may also include a roller press, a marking machine and a die-cutting machine. The roller press is used to produce the cathode and anode sheets to be wound, and is connected to a laser thickness gauge; the laser thickness gauge measures the thickness of each roll of cathode and anode sheets to be wound and transmits the thickness data to the main machine of the roller press, and the main machine of the roller press uploads the thickness data to the manufacturing operation management system. The marking machine prints the thickness values of the cathode and anode sheets to be wound on the delivery card under the control of the manufacturing operation management system. The manufacturing operation management system traces the thickness information of a single roll of electrode sheets according to the inbound and outbound parent-child number information of the cathode and anode sheets, and the manufacturing operation management system controls the die-cutting machine to die-cut the cathode and anode sheets to be wound to form the pole ears according to the thickness values of the cathode and anode sheets to be wound. The pole ear die-cutting size is based on the target thickness, and the pole ear die-cutting size includes the pole ear size and the pole ear spacing size, wherein the pole ear spacing size is set according to the target specification size and is an arithmetic progression.
[0074] The electrode thickness grouping and adjustment device in this embodiment may also include a power-assisting arm and a handheld device, and the handheld device may specifically be a PAD. Two rolls of materials (cathode sheets and anode sheets) are placed on a tray of the die-cutting machine. A person operates the power-assisting arm to transfer the electrodes with the same thickness range to a tray for storage. The handheld device is bound to the cache rack number, the pallet code, and the barcode information on the electrode shipping tag. The manufacturing operation management system verifies the barcode information scanned and transmitted by the handheld device. If the thickness group requirements are met, the electrode production time, model, material code, length, thickness group and other information will be sent back to the logistics information management system. If the thickness group requirements are not met, the manufacturing operation management system will send back an error message, and the information management system will pop up an error prompt on the handheld device.
[0075] The electrode thickness grouping and allocation device in this embodiment may also include a three-dimensional warehouse and a warehouse management system (WMS), and the three-dimensional warehouse is used to store the cathode sheets and anode sheets to be wound. When the cathode sheets and anode sheets to be wound need to be taken out of the three-dimensional warehouse, for example, when the winding scheduling management system matches the cathode sheets and anode sheets and there is a shortage of materials, the caller next to the buffer rack is manually pressed to trigger the winding material call signal.
[0076] The logic of the material allocation during winding is as follows: Figure 5 In this embodiment, when the thickness is grouped into intervals, the thickness ±1 μm from the standard thickness is taken as the middle group, the thickness +1 to +3 μm from the standard thickness is taken as the middle-upper group, and the thickness -1 to -3 μm from the standard thickness is taken as the middle-lower group, and the cathode sheet middle group (abbreviated as "yin middle"), cathode sheet middle-upper group (abbreviated as "yin middle-upper"), cathode sheet middle-lower group (abbreviated as "yin middle-lower"), anode sheet middle group (abbreviated as "yang middle"), anode sheet middle-upper group (abbreviated as "yang middle-upper"), and anode sheet middle-lower group (abbreviated as "yang middle-lower") are obtained. When matching the cathode sheets and anode sheets within the thickness interval with the same length from both sides of the reference, the matching grouping logic includes: ① the middle group of the cathode sheets matches the middle group of the anode sheets (referred to as "yin middle matches yang middle"), ② the middle and lower groups of the cathode sheets match the middle and lower groups of the anode sheets (referred to as "yin middle and lower matches yang middle and lower"), ③ the middle and upper groups of the cathode sheets match the middle and lower groups of the anode sheets (referred to as "yin middle and upper matches yang middle and lower"), ④ the middle and lower groups of the cathode sheets match the middle groups of the anode sheets (referred to as "yin middle and lower matches yang middle and lower"), The middle and upper groups of the anode sheet match the middle group of the anode sheet (referred to as "yang middle and upper match yang middle"); the middle and lower groups of the anode sheet match the middle group of the cathode sheet (referred to as "yang middle and lower match yin middle"); the middle and upper groups of the anode sheet match the middle group of the cathode sheet (referred to as "yang middle and upper match yin middle"); the middle and upper groups of the anode sheet match the middle and upper groups of the cathode sheet (referred to as "yang middle and upper match yin middle"); the middle and upper groups of the anode sheet match the middle and upper groups of the cathode sheet (referred to as "yang middle and upper match yin middle"); and the middle and upper groups of the anode sheet match the middle and lower groups of the cathode sheet (referred to as "yang middle and upper match yin middle").
[0077] According to the material call signal of the buffer rack, the warehouse management system matches the cathode and anode sheets of the corresponding thickness range according to the shortage of materials, and dispatches the cathode and anode sheets of the corresponding thickness according to the first-in-first-out principle. After the sheets are dispatched, the logistics information management system is notified, and the logistics information management system dispatches the AGV module to transport the cathode and anode sheets dispatched. The AGV transfers the materials to the buffer rack for storage, and the manually operated power arm winds the electrodes onto the machine. Embodiment 3
[0078] The present invention also discloses a battery, wherein a winding core is formed by winding cathode sheets and anode sheets. The cathode sheets and anode sheets used in the winding are selected using the electrode sheet thickness grouping and adjusting method in the first embodiment. After the winding core is hot-pressed and connected to the top cover, it is placed in a shell and injected with liquid for packaging to form a battery.
[0079] In the embodiments of the present application, the battery may be a secondary battery, which refers to a battery that can be used continuously by activating the active material by charging after the battery is discharged. The battery may be a lithium ion battery, a sodium ion battery, a sodium lithium ion battery, a lithium metal battery, a sodium metal battery, a lithium sulfur battery, a magnesium ion battery, a nickel hydrogen battery, a nickel cadmium battery, a lead storage battery, etc., and the embodiments of the present application are not limited thereto. Embodiment 4
[0080] The present invention also discloses a computer-readable storage medium on which a computer program is stored. When the computer program is executed by a processor, the method for grouping and allocating the thickness of the pole pieces in the first embodiment is implemented. Embodiment 5
[0081] The present invention also discloses a device, including a memory, a processor, and a computer program stored in the memory and executable on the processor. When the processor executes the computer program, the method for grouping and allocating the thickness of the pole piece in the first embodiment is implemented.
[0082] Those skilled in the art will appreciate that the embodiments of the present application may be provided as methods, systems, or computer program products. Therefore, the present application may adopt the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present application may adopt the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.
[0083] The present application is described with reference to the flowcharts and / or block diagrams of the methods, devices (systems), and computer program products according to the embodiments of the present application. It should be understood that each process and / or box in the flowchart and / or block diagram, as well as the combination of the processes and / or boxes in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0084] These computer program instructions may also be stored in a computer-readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer-readable memory produce an article of manufacture comprising an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1A function specified in one or more boxes.
[0085] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 A step that specifies a function in one or more boxes.
[0086] Obviously, the above embodiments are merely examples for clear explanation and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived from these are still within the protection scope of the invention.
Claims
1. A method for adjusting the thickness of pole pieces by groups, characterized in that: include: Obtaining the thickness of the cathode sheet and the anode sheet to be wound, wherein the cathode sheet and the anode sheet to be wound are both provided with tabs; Dividing a plurality of thickness intervals with the same interval length based on the standard thickness of the cathode sheet and the anode sheet, and classifying the cathode sheet and the anode sheet to be wound into the thickness intervals according to the thickness; Matching the cathode sheets and anode sheets to be wound within each thickness range, and matching the separators of corresponding thicknesses according to the total thickness of the matched cathode sheets and anode sheets to be wound, so that the total thickness of the matched cathode sheets, anode sheets and separators to be wound meets the standard specifications; The method of dividing the thickness intervals with the same length into multiple intervals based on the standard thickness of the cathode sheet and the anode sheet is as follows: Set the interval length to x, and take the standard thickness of the cathode sheet as the reference, and divide the thickness intervals of the cathode sheet into [d1-nx,d1-(n-1)x), …, [d1-ix,d1-(i-1)x), …, [d1-x,d1), (d1,d1+x], …, (d1+(i-1)x,d1+ix], …, (d1+(n-1)x,d1+nx]; where d1 represents the standard thickness of the cathode sheet, [d1-ix,d1-(i-1)x) represents the i-th thickness interval that is less than the standard thickness of the cathode sheet, (d1+(i-1)x,d1+ix] represents the i-th thickness interval that is greater than the standard thickness of the cathode sheet, and n is the total number of intervals divided on one side of the reference; Based on the standard thickness of the anode sheet, the thickness intervals of the anode sheet are divided into [d2-nx, d2-(n-1)x), …, [d2-ix, d2-(i-1)x), …, [d2-x, d2), (d2, d2+x], …, (d2+(i-1)x, d2+ix], …, (d2+(n-1)x, d2+nx]; wherein d2 represents the standard thickness of the anode sheet, [d2-ix, d2-(i-1)x) represents the i-th thickness interval that is less than the standard thickness of the anode sheet, and (d2+(i-1)x, d2+ix] represents the i-th thickness interval that is greater than the standard thickness of the anode sheet; Match the cathode sheets and anode sheets to be wound within each thickness range, specifically: Match the cathode sheet belonging to the thickness interval [d1-ix, d1-(i-1)x) with the anode sheet belonging to the thickness interval (d2+(i-1)x, d2+ix], and match the cathode sheet belonging to the thickness interval (d1+(i-1)x, d1+ix] with the anode sheet belonging to the thickness interval [d2-ix, d2-(i-1)x).
2. The method for grouping and adjusting the thickness of the electrode piece according to claim 1, characterized in that: The cathode sheets and anode sheets to be wound within each thickness range are matched so that the total thickness of the matched cathode sheets and anode sheets to be wound meets the first standard specification; and the separators of standard thickness are matched so that the total thickness of the matched cathode sheets, anode sheets and separators to be wound meets the standard specification.
3. The method for grouping and adjusting the thickness of the electrode pieces according to claim 2, characterized in that: If there are at least two areas on the cathode sheet to be wound or the anode sheet to be wound whose thickness is not in a range, then the anode sheet to be wound or the cathode sheet to be wound whose thickness is not in a range is used for matching, so that the thickness of each location on the cathode sheet to be wound and the anode sheet after matching meets the first standard specification.
4. The method for grouping and adjusting the thickness of the electrode pieces according to claim 1, characterized in that: The cathode sheets and anode sheets to be wound within each thickness range are matched, so that the first thickness of the cathode sheets and anode sheets to be wound after matching does not meet the first standard specification; and the diaphragms with corresponding thickness ranges are matched, so that the total thickness of the cathode sheets, anode sheets and diaphragms to be wound after matching meets the standard specification.
5. The method for grouping and adjusting the thickness of the electrode pieces according to claim 4, characterized in that: The cathode sheets and anode sheets to be wound within each thickness range are matched, and the first thicknesses of the matched cathode sheets and anode sheets to be wound are equal at each place and the first thicknesses do not meet the first standard specifications; then the diaphragms in the corresponding thickness ranges are matched, so that the total thicknesses of the matched cathode sheets, anode sheets and diaphragms to be wound meet the standard specifications.
6. The method for adjusting the thickness of pole pieces by groups according to claim 4, characterized in that: Match the cathode sheets and anode sheets to be wound within each thickness range. If the first thickness of at least two regions of the matched cathode sheets and anode sheets to be wound are not within the same range, match the diaphragm of the corresponding thickness range so that the total thickness of the matched cathode sheets, anode sheets and diaphragm to be wound meets the standard specifications.
7. A device for adjusting the thickness of pole pieces by groups, characterized in that: include: A laser thickness gauge is used to measure the thickness of the cathode sheet and the anode sheet to be wound, wherein the cathode sheet and the anode sheet to be wound are both provided with tabs; The manufacturing operation management system divides a plurality of thickness intervals with the same length based on the standard thickness of the cathode sheet and the anode sheet, and classifies the cathode sheet and the anode sheet to be wound into the thickness intervals according to the thickness; The logistics information management system receives information of cathode sheets and anode sheets of different thicknesses to be wound from the manufacturing operation management system, and generates tasks for transporting the cathode sheets and anode sheets to be wound; An AGV module, including an AGV and an AGV scheduling system, wherein the AGV scheduling system receives tasks issued by the logistics information management system and notifies the AGV to transport cathode sheets and anode sheets to be wound; Winding module, including a winder and a winding scheduling management system; The winding scheduling management system receives the cathode sheets and anode sheets to be wound that are transported by the AGV, matches the cathode sheets and anode sheets to be wound within each thickness range, matches the diaphragm of corresponding thickness according to the total thickness of the matched cathode sheets and anode sheets to be wound, so that the total thickness of the matched cathode sheets, anode sheets and diaphragm to be wound meets the standard specifications; the winding machine winds the matched cathode sheets and anode sheets to be wound to obtain a winding core; The method of dividing the thickness intervals with the same length into multiple intervals based on the standard thickness of the cathode sheet and the anode sheet is as follows: Set the interval length to x, and take the standard thickness of the cathode sheet as the reference, and divide the thickness intervals of the cathode sheet into [d1-nx,d1-(n-1)x), …, [d1-ix,d1-(i-1)x), …, [d1-x,d1), (d1,d1+x], …, (d1+(i-1)x,d1+ix], …, (d1+(n-1)x,d1+nx]; where d1 represents the standard thickness of the cathode sheet, [d1-ix,d1-(i-1)x) represents the i-th thickness interval that is less than the standard thickness of the cathode sheet, (d1+(i-1)x,d1+ix] represents the i-th thickness interval that is greater than the standard thickness of the cathode sheet, and n is the total number of intervals divided on one side of the reference; Based on the standard thickness of the anode sheet, the thickness intervals of the anode sheet are divided into [d2-nx, d2-(n-1)x), …, [d2-ix, d2-(i-1)x), …, [d2-x, d2), (d2, d2+x], …, (d2+(i-1)x, d2+ix], …, (d2+(n-1)x, d2+nx]; wherein d2 represents the standard thickness of the anode sheet, [d2-ix, d2-(i-1)x) represents the i-th thickness interval that is less than the standard thickness of the anode sheet, and (d2+(i-1)x, d2+ix] represents the i-th thickness interval that is greater than the standard thickness of the anode sheet; Match the cathode sheets and anode sheets to be wound within each thickness range, specifically: Match the cathode sheet belonging to the thickness interval [d1-ix, d1-(i-1)x) with the anode sheet belonging to the thickness interval (d2+(i-1)x, d2+ix], and match the cathode sheet belonging to the thickness interval (d1+(i-1)x, d1+ix] with the anode sheet belonging to the thickness interval [d2-ix, d2-(i-1)x).
8. A battery, comprising a winding core, characterized in that: The winding core is formed by winding cathode sheets and anode sheets, and the cathode sheets and anode sheets used in the winding are selected using the electrode sheet thickness grouping and deployment method described in any one of claims 1-6.