Laser lift-off device
By setting up an eddy current induction area and an eddy current heater in the laser stripping device, combined with laser heating, the problem of cracks during the peeling of the transparent polyimide film layer in the production of flexible display screens is solved, achieving a more efficient peeling process and more efficient Good glowing effect.
Patent Information
- Application Number
- CN202410946323.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2044-07-16
AI Technical Summary
During the production process of flexible display screens, when the transparent polyimide film layer is peeled off from the glass substrate, severe local cracking occurs due to thermal mismatch, affecting the luminous effect and yield.
Design a laser peeling device. The first and second eddy current sensing areas are set on the top surface of the glass substrate. The eddy current heater heats the eddy current sensing area and uses the laser to heat the peeling point to eliminate the temperature difference between the peeling point and the surrounding area. Poor, combined with the breakage of dangling keys by eddy current heaters, uniform heating is achieved.
It effectively reduces the local cracking phenomenon during the peeling process, guarantees the luminous effect and yield of the flexible display, and allows peeling along the curve to avoid cracking and improve the peeling efficiency.
Smart Images

Figure CN118492640B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of flexible display screen processing, and in particular to a laser peeling device. Background Art
[0002] In the production process of flexible display screens, the transparent polyimide film layer needs to be peeled off from the glass substrate. Usually, laser irradiation is used to irradiate the peeling point, and the irradiated area is heated to break the dangling bonds between the glass substrate and the transparent polyimide film layer, so that the two are separated. However, there is a large temperature difference between the irradiated area and the surrounding area. Due to thermal mismatch, local cracking is very likely to occur during the peeling process, which seriously affects the luminous effect and yield of the flexible display screen. Summary of the invention
[0003] The invention provides a laser stripping device for reducing the problem of local cracking when a transparent polyimide film layer is stripped from a glass substrate.
[0004] The present invention provides a laser lift-off device, comprising:
[0005] A glass substrate, wherein a first eddy current induction zone is arranged in the middle of the top surface, and second eddy current induction zones are arranged at four corners of the top surface respectively;
[0006] a transparent polyimide film layer, located above the top surface of the glass substrate;
[0007] An eddy current heater is disposed below the glass substrate and is capable of heating the first eddy current induction area and the second eddy current induction area;
[0008] The laser is movably arranged above the transparent polyimide film layer and can emit laser toward the transparent polyimide film layer.
[0009] In some embodiments, a plurality of first graphite rings are disposed in the first eddy current induction zone; the plurality of first graphite rings are distributed in an array;
[0010] A second graphite ring is arranged in each second eddy current induction area.
[0011] In some embodiments, the first graphite ring has a diameter of 2 μm-2 mm and a thickness of 20 μm-2 mm;
[0012] The diameter of the second graphite ring is larger than that of the first graphite ring.
[0013] In some of the embodiments, the eddy current frequency of the eddy current heater is 20 Hz-60 Hz;
[0014] The wavelength of the laser emitted by the laser is 193.5nm-395nm, and the spot size is 8μm-32μm.
[0015] In some of these embodiments, the laser can move up and down, left and right, forward and backward, and can swing back and forth.
[0016] In some embodiments, the transparent polyimide film layer has a thickness of 50 μm-2 mm.
[0017] In some embodiments, it also includes:
[0018] a lower periodic anti-oxidation layer, located above the top surface of the glass substrate;
[0019] a transparent flexible layer, located above the top surface of the lower periodic anti-oxidation layer;
[0020] an upper periodic anti-oxidation layer, located above the top surface of the transparent flexible layer;
[0021] The transparent polyimide film layer is located above the top surface of the upper periodic anti-oxidation layer.
[0022] In some embodiments, the material of the lower periodic anti-oxidation layer and the upper periodic anti-oxidation layer is silicon oxide or silicon nitride;
[0023] The material of the flexible layer is polydimethylsiloxane or polymethyl methacrylate.
[0024] In some embodiments, it also includes:
[0025] an anode electrode layer, located above the top surface of the transparent polyimide film layer;
[0026] A light emitting layer, located above the top surface of the anode electrode layer;
[0027] The cathode electrode layer is located above the top surface of the light-emitting layer.
[0028] The beneficial effects of the present invention are as follows: The laser stripping device of the present invention is provided with a glass substrate, and a first eddy current induction zone is provided in the middle of the top surface of the glass substrate, and second eddy current induction zones are provided at the four corners of the top surface. When the transparent polyimide film layer is stripped from the glass substrate, the first eddy current induction zone and the second eddy current induction zone of the glass substrate are first heated by means of an eddy current heater, and the first eddy current induction zone and the second eddy current induction zone heat the transparent polyimide film layer as a whole to a temperature of 180°C-260°C. Then, the stripping point is irradiated with the help of a laser, and the stripping point is heated by a laser. Since the temperature difference between the stripping point and the surrounding area is eliminated, cracking is not easy to occur locally during the stripping process, which is conducive to ensuring the luminous effect and yield of the flexible display screen. Moreover, the stripping process is no longer limited to stripping along a straight line, and even if stripping is performed along a curve, cracking is not easy to occur locally. In addition, the heated first eddy current induction zone and the second eddy current induction zone are conducive to the breaking of the hanging bond, which is helpful for the stripping process. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is a schematic structural diagram of some specific embodiments of a laser lift-off device of the present invention;
[0030] Figure 2 yes Figure 1 Schematic diagrams of structures of some specific embodiments of glass substrates in the laser lift-off device shown;
[0031] Figure 3 yes Figure 1 The schematic diagrams of the structures of some specific embodiments of the laser in the laser lift-off device shown;
[0032] Figure 4 yes Figure 3 Left view of .
[0033] In the accompanying drawings, 110, glass substrate; 111, first eddy current induction zone; 1111, first graphite ring; 112, second eddy current induction zone; 1121, second graphite ring; 120, transparent polyimide film layer; 130, eddy current heater; 140, laser; 151, lower periodic anti-oxidation layer; 152, transparent flexible layer; 153, upper periodic anti-oxidation layer; 154, anode layer; 155, light-emitting layer; 156, cathode layer; 160, posture adjustment mechanism; 161, first support seat; 162, second support seat; 163, third support seat; 164, first driving gear; 165, first driven gear; 166, second driving gear; 167, second driven gear; 170, carrier; 180, tray. DETAILED DESCRIPTION
[0034] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0035] As mentioned in the background technology, in the production process of flexible display screens, it is necessary to peel the transparent polyimide film layer from the glass substrate. Usually, laser irradiation is used to irradiate the peeling point, and the irradiated area is heated to break the dangling bonds on the surface of the glass substrate and the transparent polyimide film layer, so as to separate the two. However, there is a large temperature difference between the irradiated area and the surrounding area. Due to thermal mismatch, local cracking is very likely to occur during the peeling process, which seriously affects the luminous effect and yield of the flexible display screen.
[0036] To solve the above problems, refer to Figure 1 , Figure 2 , Figure 3 and Figure 4 The present invention provides a laser lift-off device, comprising a glass substrate 110, a transparent polyimide film layer 120, an eddy current heater 130 and a laser 140. A first eddy current induction zone 111 is provided in the middle of the top surface of the glass substrate 110, and second eddy current induction zones 112 are provided at the four corners of the top surface. The transparent polyimide film layer 120 is located above the first eddy current induction zone 111 and the second eddy current induction zone 112 of the glass substrate 110. The eddy current heater 130 is provided below the glass substrate 110, and can heat the first eddy current induction zone 111 and the second eddy current induction zone 112. The laser 140 is movably provided above the transparent polyimide film layer 120, and can emit laser toward the transparent polyimide film layer 120. When the transparent polyimide film layer 120 is peeled off from the glass substrate 110, the first eddy current induction zone 111 and the second eddy current induction zone 112 of the glass substrate 110 are first heated by the eddy current heater 130, and the first eddy current induction zone 111 and the second eddy current induction zone 112 heat the transparent polyimide film layer 120 as a whole, so that its temperature reaches 180°C-260°C. Then, the peeling point is irradiated with the help of the laser 140, and the peeling point is heated by the laser. Since the temperature difference between the peeling point and the surrounding area is eliminated, cracking is not easy to occur locally during the peeling process, which is conducive to ensuring the luminous effect and yield of the flexible display screen. Moreover, the peeling process is no longer limited to peeling only along a straight line. Even if peeling is performed along a curve, cracking is not easy to occur locally. In addition, the heated first eddy current induction zone 111 and the second eddy current induction zone 112 are conducive to the breaking of the hanging bond and help the peeling process.
[0037] Preferably, the glass substrate 110 may be deformation-free glass or flexible ultra-thin glass.
[0038] Specifically, in the exemplary embodiment, a plurality of first graphite rings 1111 are arranged in the first eddy current induction zone 111. The plurality of first graphite rings 1111 are arranged in an array. A second graphite ring 1121 is arranged in each second eddy current induction zone. The diameter of the first graphite ring 1111 is 2 μm-2 mm, and the thickness is 20 μm-2 mm. The diameter of the second graphite ring 1121 is larger than the first graphite ring 1111. That is, a plurality of smaller graphite rings are arranged in the middle of the glass substrate 110, and are arranged in a square, circular or triangular array. Compared with the form of setting a single large graphite ring, the middle of the transparent polyimide film layer 120 is heated very uniformly, which is more conducive to eliminating cracking. Since the temperature uniformity requirements at the four corners of the transparent polyimide film layer 120 are not particularly high, a larger graphite ring can be arranged at the four corners of the glass substrate 110 to heat the four corners of the transparent polyimide film layer 120 respectively.
[0039] Preferably, each first graphite ring 1111 and each second graphite ring 1121 is circular, annular, elliptical, rectangular or polygonal.
[0040] To meet the heating temperature requirement, the eddy current frequency of the eddy current heater 130 is 20Hz-60Hz. To meet the glass requirement, the wavelength of the laser emitted by the laser 140 is 193.5nm-395nm, the spot can be a circular spot or an elliptical spot, and the size of the spot is 8μm-32μm.
[0041] It should be noted that the laser 140 may be an excimer laser 140, a nonlinear optical multi-stage frequency doubling laser 140, a pulse laser 140 or a continuous laser 140, and the emitted wavelength may be a single wavelength or multiple wavelengths. When the laser 140 is a pulse laser 140, it can emit pulse laser light with a pulse frequency of 10 Hz-10 KHz.
[0042] Preferably, the laser stripping device is suitable for stripping a transparent polyimide film layer 120 with a thickness of 50 μm-2 mm from a glass substrate 110, and the size of the polyimide film layer is 10 mm×10 mm-1600 mm×800 mm. The stripped flexible display screen can be a monochrome display screen or a three-primary color display screen. A circuit is provided on the surface of the polyimide film layer, the circuit line width of the display area is less than 20 μm, and the overall light transmittance is greater than 85%.
[0043] Specifically, in the exemplary embodiment, the laser lift-off device further includes a lower periodic anti-oxidation layer 151, a transparent flexible layer 152, an upper periodic anti-oxidation layer 153, an anode electrode layer 154, a light-emitting layer 155, and a cathode electrode layer 156. The lower periodic anti-oxidation layer 151 is located above the top surface of the glass substrate 110, has an anti-oxidation function, and is made of silicon oxide or silicon nitride, etc. The transparent flexible layer 152 is located above the top surface of the lower periodic anti-oxidation layer 151, and is made of polydimethylsiloxane or polymethyl methacrylate. The upper periodic anti-oxidation layer 153 is located above the top surface of the transparent flexible layer 152, has an anti-oxidation function, and is made of silicon oxide or silicon nitride, etc. The transparent polyimide film layer 120 is located above the top surface of the upper periodic anti-oxidation layer 153. The anode electrode layer 154 is located above the top surface of the transparent polyimide film layer 120. The light-emitting layer 155 is located above the top surface of the anode electrode layer 154, and is capable of emitting light. The cathode layer 156 is located above the top surface of the light emitting layer 155 .
[0044] Specifically, in the example, Figure 1 , Figure 3 and Figure 4As shown, the laser stripping device also includes a tray 180, a carrier 170 and a posture adjustment mechanism 160. The tray 180 is arranged below the glass substrate 110 and is used to carry the glass substrate 110. The carrier 170 is equipped with a posture adjustment mechanism 160, and the laser 140 is installed on the posture adjustment mechanism 160. Assume that the front and rear direction is defined as the X-axis direction, the left and right direction is defined as the Y-axis direction, and the up and down direction is defined as the Z-axis direction. Driven by the driver, the carrier 170 can move up and down, left and right, and forward and backward to drive the posture adjustment mechanism 160 and the laser 140 to move up and down, left and right, and forward and backward, so that the laser 140 can move in a straight line along the X-axis, Y-axis or Z-axis, and can also move in a curve in space or a plane. The posture adjustment mechanism 160 can swing the laser 140 around the X-axis and Y-axis, so that the emitting head of the laser 140 can swing back and forth, left and right, and the irradiation angle of the laser 140 can be adjusted according to the actual working conditions.
[0045] Preferably, the posture adjustment mechanism 160 includes a first support seat 161, a second support seat 162, a third support seat 163, a first driving gear 164, a first driven gear 165, a first servo motor, a second driving gear 166, a second driven gear 167, and a second servo motor. The first support seat 161 is fixedly mounted on the carrier 170. The second support seat 162 is mounted on the first support seat 161 so as to be swingable around the Y-axis direction. The third support seat 163 is mounted on the third support seat 163 so as to be swingable around the X-axis direction. The laser 140 is mounted on the third support seat 163. The first driving gear 164 is rotatably mounted on one side of the first support seat 161. The first driven gear 165 is sleeved on one end of the rotating shaft of the second support seat 162, and the side wall is meshed and connected with the first driving gear 164. The first servo motor is mounted on one side of the first support seat 161, and the first driving gear 164 is sleeved on the output shaft. The first servo motor drives the first driving gear 164 to rotate, and then the second support seat 162 is swung around the Y-axis direction through the first driven gear 165 and the rotating shaft. The second driving gear 166 is rotatably mounted on the second support seat 162. The second driven gear 167 is mounted on the third support seat 163, and the side wall is meshed and connected with the second driving gear 166. The second servo motor is mounted on the second support seat 162, and the second driving gear 166 is sleeved on the output shaft. The second driving gear 166 is driven by the second servo motor to rotate, and then the third support seat 163 is driven to swing around the X-axis direction through the second driven gear 167.
[0046] On the other hand, the present invention also provides a laser lift-off process, comprising the following steps: first, the first eddy current induction zone 111 and the second eddy current induction zone 112 are heated by means of an eddy current heater 130, the first eddy current induction zone 111 heats the middle of the transparent polyimide film layer 120 to 180°C-260°C, and the second eddy current induction zones 112 at the four corners heat the four corners of the transparent polyimide film layer 120 to 180°C-260°C respectively. Then, the laser 140 moves in a straight line or curve above the transparent polyimide film layer 120, and emits laser light to the transparent polyimide film layer 120. The laser and heat break the hanging bonds between the glass substrate 110 and the surface of the transparent polyimide film layer 120, so as to peel the transparent polyimide film layer 120 from the glass substrate 110. Since the temperature difference between the peeling point and the surrounding area is eliminated, local cracking is not easy to occur during the peeling process, which is conducive to ensuring the luminous effect and yield of the flexible display screen. Moreover, the peeling process is no longer limited to peeling along a straight line, and even if peeling along a curve, local cracking is not easy to occur. At the same time, the heating of the first eddy current induction area 111 and the second eddy current induction area 112 is conducive to the breaking of the dangling bonds, which helps the peeling process.
[0047] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0048] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0049] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0050] In the present invention, the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. mean that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the described specific features, structures, materials or characteristics may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.
[0051] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.
Claims
1. A laser lift-off device, characterized in that: include: A glass substrate, wherein a first eddy current induction zone is arranged in the middle of the top surface, and second eddy current induction zones are arranged at four corners of the top surface respectively; A transparent polyimide film layer is located above the top surface of the glass substrate; An eddy current heater is arranged below the glass substrate, and can make the first eddy current induction area and the second eddy current induction area generate heat; the first eddy current induction area heats the middle of the transparent polyimide film layer to 180° C.-260° C., and the second eddy current induction areas at the four corners heat the four corners of the transparent polyimide film layer to 180° C.-260° C. respectively; A laser is movably disposed above the transparent polyimide film layer and is capable of emitting laser light toward the transparent polyimide film layer; A plurality of first graphite rings are arranged in the first eddy current induction area; the plurality of first graphite rings are distributed in an array; A second graphite ring is disposed in each of the second eddy current induction zones; The first graphite ring has a diameter of 2 μm-2 mm and a thickness of 20 μm-2 mm; The diameter of the second graphite ring is larger than that of the first graphite ring; The eddy current frequency of the eddy current heater is 20Hz-60Hz; The wavelength of the laser emitted by the laser is 193.5nm-395nm, and the spot size is 8μm-32μm; The laser can move up and down, left and right, forward and backward, and can swing forward and backward and left and right; The laser stripping device also includes a carrier and a posture adjustment mechanism; the posture adjustment mechanism is installed on the carrier, and the laser is installed on the posture adjustment mechanism; the carrier can move up, down, left, right, forward, and backward under the drive of the driver, so as to drive the posture adjustment mechanism and the laser to move up, down, left, right, forward, and backward, so that the laser can move in a straight line along the X-axis, Y-axis or Z-axis, and can move in a curve in space or a plane; the posture adjustment mechanism can swing the laser around the X-axis and the Y-axis, so that the laser's emitting head can swing back, forth, left, and right, so as to adjust the irradiation angle of the laser; The posture adjustment mechanism includes a first support seat, a second support seat, a third support seat, a first driving gear, a first driven gear, a first servo motor, a second driving gear, a second driven gear and a second servo motor; the first support seat is fixedly mounted on the carrier; the second support seat can be mounted on the first support seat so as to swing around the Y-axis direction; the third support seat can be mounted on the third support seat so as to swing around the X-axis direction; the laser is mounted on the third support seat; the first driving gear is rotatably mounted on one side of the first support seat; the first driven gear is sleeved on one end of the rotating shaft of the second support seat, and the side wall is meshed and connected with the first driving gear; the first servo The motor is installed on one side of the first support seat, and the first driving gear is sleeved on the output shaft; the first driving gear is driven to rotate by the first servo motor, and then the second support seat is swung around the Y-axis direction through the first driven gear and the rotating shaft; the second driving gear is rotatably installed on the second support seat; the second driven gear is installed on the third support seat, and the side wall is meshed and connected with the second driving gear; the second servo motor is installed on the second support seat, and the second driving gear is sleeved on the output shaft; the second driving gear is driven to rotate by the second servo motor, and then the third support seat is driven to swing around the X-axis direction through the second driven gear.
2. The laser lift-off device according to claim 1, characterized in that: The thickness of the transparent polyimide film layer is 50 μm-2 mm.
3. The laser lift-off device according to claim 1, characterized in that: Also includes: a lower periodic anti-oxidation layer, located above the top surface of the glass substrate; a transparent flexible layer, located above the top surface of the lower periodic anti-oxidation layer; an upper periodic anti-oxidation layer, located above the top surface of the transparent flexible layer; The transparent polyimide film layer is located above the top surface of the upper periodic anti-oxidation layer.
4. The laser lift-off device according to claim 3, characterized in that: The material of the lower periodic anti-oxidation layer and the upper periodic anti-oxidation layer is silicon oxide or silicon nitride; The material of the transparent flexible layer is polydimethylsiloxane or polymethyl methacrylate.
5. The laser lift-off device according to claim 3, characterized in that: Also includes: an anode electrode layer, located above the top surface of the transparent polyimide film layer; A light-emitting layer, located above the top surface of the anode electrode layer; The cathode electrode layer is located above the top surface of the light-emitting layer.
Citation Information
Patent Citations
Method for reducing injury caused by laser peeling
CN101924065A
Laser spiral perforating device and device adopting eddying effect for assisting in heating
CN107695543A
Laser lift-off equipment and preparation method of flexible display device
CN115394711A
Method for stripping organic light-emitting diode substrate