Quinazoline-containing organic room temperature phosphorescent scintillator and preparation method and application thereof
Through the binding of quinazoline groups with halogen and heteroaryl groups and the introduction of anicyclic groups, the X-ray absorption and phosphorescence luminescence efficiency of organic scintillators are improved, and the low absorption of organic scintillator materials in the prior art is solved. and low conversion efficiency issues, high-performance, low-toxic phosphorescent scintillators are prepared, suitable for X-ray imaging and extreme environments.
Patent Information
- Application Number
- CN202410734286.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-07
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing organic scintillator materials exhibit low X-ray absorption and low high-energy photon conversion efficiency under high-energy X-rays, and low exciton utilization, resulting in weak scintillation performance and complex preparation methods.
The quinazoline group is used to combine with halogen and heteroaryl groups to improve the phosphorescence luminescence efficiency through charge transfer, and the introduction of nitrogen heterocyclic groups to enhance the intermolecular interactions to prepare high-performance organophosphorescence scintillator materials and combine with polymer matrix. Prepare flexible X-ray scintillation film.
It realizes efficient X-ray luminescence, improves scintillation performance and stability, and provides high-performance, low-biotoxic organic phosphorescent crystal scintillators, suitable for extreme environments and X-ray imaging fields.
Smart Images

Figure CN118561833B_ABST
Abstract
Description
Technical field:
[0001] The invention belongs to the technical field of organic room temperature phosphorescent scintillators, and in particular relates to a quinazoline-containing organic room temperature phosphorescent scintillator and a preparation method and application thereof. Background technology:
[0002] X-ray scintillators can convert high-energy X-rays into low-energy visible light, and have important applications in medical detection, non-destructive testing, safety testing, space detection, and high-energy physics. Current X-ray scintillators are mainly divided into two categories: inorganic scintillators and organic scintillators. Scintillators based on organic materials can be mainly divided into organic crystal scintillators, plastic scintillators, and liquid scintillators. Plastic scintillators and liquid scintillators require aromatic matrices during preparation. After repeated exposure to X-rays, these matrices may degrade, cross-link, or deteriorate, affecting the performance of the scintillator. In contrast, crystal scintillating materials have orderly molecular stacking, high chemical purity, and a rigid crystal environment, resulting in low scattering, light loss, and fewer lattice defects, showing better radiant luminescence, radiation resistance, and good mechanical strength.
[0003] Compared with inorganic scintillators, organic crystal scintillators still have relatively weak scintillation performance. The main reasons for the above results are the low X-ray absorption and low high-energy photon conversion efficiency of organic scintillators. In order to solve the low X-ray absorption of organic materials, researchers have introduced halogen atoms with high atomic numbers into organic materials to improve the low X-ray absorption of organic scintillators. In addition, the large number of triplet excitons generated by traditional fluorescent scintillator materials under high-energy X-ray irradiation are dissipated in a non-radiative transition manner, which is the main reason for the low visible light conversion efficiency of organic scintillators. The development of high-performance room temperature phosphorescent crystal scintillator materials is a current key research issue with important commercial value. Summary of the invention:
[0004] In view of the deficiencies in the prior art, the low utilization rate of excitons in existing organic scintillating crystals, the single type, and the complex synthesis and preparation methods, the purpose of the present invention is to provide a novel organic compound, a phosphorescent scintillator material, and a preparation method and application thereof. The phosphorescent group quinazoline and the electron-donating group form a charge transfer, further improving the phosphorescent luminescence efficiency and ensuring the utilization rate of triplet excitons of high-energy rays. In addition, the introduction of the nitrogen heterocyclic group provides more hydrogen bonds and intermolecular interactions, which not only protects the triplet excitons but also ensures that the crystal has rigid characteristics, thereby obtaining an organic phosphorescent crystal scintillator with high performance, high stability and low biotoxicity. In addition, the phosphorescent scintillator material is applied to the field of X-ray imaging.
[0005] The present invention specifically adopts the following technical solutions:
[0006] The first aspect of the present invention provides a quinazoline-containing organic room temperature phosphorescent scintillator, wherein the organic room temperature phosphorescent scintillator has the following molecular structure:
[0007]
[0008] Wherein, R1 is selected from any one of -H, -F, -Cl or -Br, and R2 is selected from any one of substituted or unsubstituted heteroaryl.
[0009] Furthermore, the structural formula of R2 is any one of the following structures
[0010] .
[0011] Furthermore, the scintillator takes the quinazoline group as the core, and realizes efficient phosphorescence emission under ultraviolet light and X-ray by modifying different halogen atoms and heteroaryl groups.
[0012] The second aspect of the present invention provides a method for preparing the quinazoline-containing organic room temperature phosphorescent scintillator described in any one of the above items, the method comprising:
[0013] Quinazoline compounds respectively carrying out a nucleophilic substitution reaction with a substituted or unsubstituted heteroaryl to obtain the quinazoline-containing organic room temperature phosphorescent scintillator;
[0014] Wherein, R1 is any one of -H, -F, -Cl or -Br.
[0015] Furthermore, the method specifically comprises:
[0016] Under nitrogen atmosphere at 0°C, dissolve the substituted or unsubstituted heteroaryl in anhydrous tetrahydrofuran, then add n-butyl lithium solution to react by stirring;
[0017] The solution obtained above is added to a solution of a quinazoline compound dissolved in anhydrous tetrahydrofuran, stirred at 0°C for sufficient reaction, and then the solvent is removed, followed by column chromatography separation and purification to obtain the quinazoline-containing organic room temperature phosphorescent scintillator.
[0018] Furthermore, the method specifically comprises any one of the following reactions:
[0019] .
[0020] The third aspect of the present invention provides the use of the above-mentioned quinazoline-containing organic room temperature phosphorescent scintillator in large-area and flexible X-ray imaging.
[0021] Furthermore, the quinazoline-containing organic room temperature phosphorescent scintillator material is combined with a polymer matrix to prepare a flexible X-ray scintillating film.
[0022] Furthermore, the polymer matrix is any one of polymethylsiloxane, polystyrene or polymethyl methacrylate.
[0023] Compared with the prior art, the present invention has the following beneficial technical effects:
[0024] The organic room temperature phosphorescent scintillating crystal material provided by the present invention utilizes the quinazoline group itself to have efficient phosphorescence. In addition, the introduction of halogen into the quinazoline derivative can improve the absorption of X-rays by the material. Then, the electron-withdrawing quinazoline group and the electron-donating phosphorescent group form a charge transfer, further improving the phosphorescent luminescence efficiency and ensuring efficient X-ray radiation luminescence. In addition, the introduction of the nitrogen heterocyclic group provides more hydrogen bonds and intermolecular interactions, which not only protects triplet excitons but also ensures that the crystal has rigid characteristics, thereby obtaining an organic phosphorescent crystal scintillator with high performance, high stability and low biotoxicity.
[0025] Since the crystal material has the characteristics of high light yield, strong radiation resistance and structural rigidity, the organic room temperature phosphorescent scintillation crystal provided by the present invention exhibits more excellent scintillation performance and is more suitable for various extreme environments in practical applications.
[0026] In order to more clearly illustrate the technical solutions of the embodiments of the present disclosure, the drawings of the embodiments will be briefly described below. It should be noted that the drawings described below only relate to some embodiments of the present disclosure, but are not intended to limit the present disclosure, wherein:
[0027] Figure 1 The single crystal XRD diagram of the organic compound provided in Example 1 of the present invention illustrates the structure and purity of the material.
[0028] Figure 2 The steady-state emission spectrum and delayed emission spectrum of the organic compound provided in Example 1 of the present invention under ultraviolet light excitation. The embedded photos in the picture are photos under ultraviolet excitation; it shows that the material has good optical properties and ensures high-performance scintillation luminescence.
[0029] Figure 3 The luminescence lifetime at 560 nm of the organic compound provided in Example 1 of the present invention under the excitation of a 350 nm ultraviolet lamp indicates that the material has a short luminescence decay time, proving the high radiation recombination rate of the material and ensuring a high-performance scintillator.
[0030] Figure 4 This is the steady-state emission spectrum of the organic compound under X-ray irradiation provided in Example 1 of the present invention; it indicates that the material has good stability under X-rays.
[0031] Figure 5The stability of the organic compound provided in Example 1 of the present invention under high-dose X-ray radiation of 278 μGy / s indicates that the material has good stability under X-rays.
[0032] Figure 6 The detection limit diagram of the organic compound provided in Example 1 of the present invention shows that the material has a sensitive response characteristic to X-rays. A low detection limit is an important indicator of the excellent performance of the scintillator.
[0033] Figure 7 This is an X-ray image of the spring inside the capsule and the metal iron sheet obtained by using the scintillator film prepared in Example 2 of the present invention. Specific implementation method:
[0034] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0035] Example 1: Preparation of organic room temperature phosphorescent material:
[0036]
[0037] Compound 1: Preparation of quinazoline phenothiazine QZP (10-(7-bromo-2-chloroquinazolin-4-yl)-10H-phenothiazine)
[0038] Under nitrogen atmosphere, anhydrous tetrahydrofuran (80 mL) was injected into a 250 mL round-bottom flask containing phenothiazine (2 g; 10.04 mmol). The above solution was placed in an ice-water bath and stirred for 10 minutes, and then a 1.6 M solution of n-butyl lithium (6.8 mL; 10.04 mmol) dissolved in n-hexane was added. After the mixture solution was stirred at 273 K for 20 minutes, the solution was slowly added to a quinazoline derivative (2.79 g; 10.04 mmol) dissolved in anhydrous tetrahydrofuran (20 mL). Finally, the solution was stirred at 273 K for 5 hours. The solvent was removed by rotary evaporation, and the residue was purified by column chromatography to obtain a white solid QZP (3.5 g). Finally, the obtained product was separated and purified by column chromatography and dried in vacuo to obtain the final product. The structure of the compound was characterized by single crystal XRD, and the results Figure 1 As shown, the experimental results confirmed the structure and purity of the obtained QZP compound.
[0039] Example 2: Preparation of a flexible scintillator film that can be prepared over a large area
[0040] (1) 100 mg of the organic phosphorescent scintillator material provided in Example 1 was dissolved in 2 ml of THF solvent to obtain a saturated solution.
[0041] (2) Add the main agent of polydimethylsiloxane and the curing agent to the precursor solution of step 1 in sequence, and then ultrasonicate the obtained mixed solution for one hour to make the phosphorescent scintillator material and polydimethylsiloxane uniformly mixed. Finally, heat the mixed solution in a forced air oven at 50 degrees Celsius for 10 hours to obtain a QZP@PDMS scintillator film.
[0042] Structural characterization, spectroscopy and imaging results:
[0043] Test methods: Steady-state photoluminescence, phosphorescence spectra and lifetime decay spectra were measured on an Edinburgh FLS1000 fluorescence spectrophotometer equipped with a xenon arc lamp and a microsecond flash lamp, respectively. Single crystal X-ray diffraction was performed using a Bruker SMARTAPEX-II CCD diffractometer. RL spectra were measured using an Edinburgh FS5 fluorescence spectrophotometer (Edinburgh Instruments Ltd.) and a micro X-ray source (AMPEK). Photos were taken with a Canon EOS850D digital camera.
[0044] Experimental study on X-ray response characteristics and photostability
[0045] The X-ray response characteristics and photostability of the room temperature phosphorescent crystal scintillator materials are investigated. When ultraviolet light or X-rays irradiate the scintillator material, the material exhibits bright visible light, indicating that the scintillator material has sensitive X-ray response characteristics (such as Figure 2 and Figure 4 Most importantly, the present invention measures the luminescence lifetime (as shown in Figure 3 As shown in FIG. 1 ), it is proved that the luminescence decay of the scintillator material provided by the present invention is only 26.5 microseconds. The short lifetime decay indicates the efficient radiation recombination rate, which ensures the high performance of the phosphorescent scintillator. Figure 5 As shown, at high dose rate X-rays (278 mGy s -1 ), the luminescence intensity of the polymer remained basically unchanged under the continuous excitation of Figure 6 As shown in the figure, by measuring the X-ray luminescence intensity at different doses, the detection limit of the room temperature phosphorescent crystal scintillator material was calculated to be 208 nGy s -1 , which is much lower than the standard medical X-ray detection limit of 5.5 mGy s -1 , indicating that our room temperature phosphorescent crystal scintillator material has excellent scintillation luminescence properties.
[0046] Application research experiment of polymer phosphorescent scintillator
[0047] The X-ray phosphorescent scintillator film prepared in Example 2 was used as an imaging plate, and then the sample to be detected was placed between the X-ray source and the imaging plate. The different absorption of the X-ray source by the different structures of the sample was utilized, and then the light signal was collected by a digital camera to obtain the X-ray imaging of the internal structure of the sample. The obtained results are shown in FIG. Figure 7 As shown in the figure, it can be seen that the spring structure and the metal iron sheet inside the capsule can be clearly presented, indicating that the organic phosphorescent scintillator provided by the present invention has great application potential in the field of X-ray imaging.
[0048] It should be noted that, in this article, terms such as "comprises", "includes" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or apparatus that includes a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or apparatus.
[0049] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A quinazoline-containing organic room temperature phosphorescent scintillator, characterized in that: The organic room temperature phosphorescent scintillator has the following molecular structure: 。 2. A method for preparing the quinazoline-containing organic room temperature phosphorescent scintillator according to claim 1, characterized in that: The method is specifically the following reaction: 。 3. Use of the quinazoline-containing organic room temperature phosphorescent scintillator according to claim 1 in the preparation of X-ray imaging materials.
4. Use of the quinazoline-containing organic room temperature phosphorescent scintillator according to claim 3 in the preparation of X-ray imaging materials, characterized in that: The quinazoline-containing organic room temperature phosphorescent scintillator material is combined with a polymer matrix to prepare a flexible X-ray scintillating film.
5. Use of the quinazoline-containing organic room temperature phosphorescent scintillator according to claim 4 in the preparation of X-ray imaging materials, characterized in that: The polymer matrix is any one of polymethylsiloxane, polystyrene or polymethyl methacrylate.
Citation Information
Patent Citations
Organic compound, scintillator material and preparation method and application thereof
CN112174941A
Molecular glass scintillator material and preparation method and application thereof
CN116218520A