A heterogeneous bonding three-dimensional integrated packaging structure

Through heterobonding, the three-dimensional integrated packaging structure is used to utilize the metal bonding and TGV structure of the overall layer of EMC and Glass, the warping problem in EWLB packaging technology is solved, high integration and stability are achieved, and the overall packaging structure is improved. Performance and reliability.

CN118571858BActive Publication Date: 2024-11-15QUANZHOU YUNJIAN MEASUREMENT CONTROL & SENSING TECH INNOVATION RES INST +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411054577.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-15
Estimated Expiration
2044-08-02

AI Technical Summary

Technical Problem

Traditional EWLB packaging technology is prone to warping when temperature changes, affecting the stability and reliability of the packaging structure, and it is difficult to achieve high-integration stacking and RDL layer preparation.

Method used

Adopt a hetero-bonded three-dimensional integrated packaging structure, through metal bonding between the EMC overall layer and the Glass overall layer, combining the TGV structure and the RDL layer, high-strength connection and electrical interconnection are achieved, and precise metal bonding technology and material adaptation are used. The overall strength of the package structure is enhanced.

Benefits of technology

It effectively solves the warping problem, ensures the stability and reliability of the packaging structure, improves the compactness and functional integration of the packaging structure, improves space utilization, and provides an effective solution for multi-layer integration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118571858B_ABST
    Figure CN118571858B_ABST
Patent Text Reader

Abstract

The present invention introduces a heterogeneous bonding three-dimensional integrated packaging structure, which is composed of an EMC overall layer, a Glass overall layer, an RDL wiring layer, a connection component, a semiconductor chip and a passivation layer. The semiconductor chip is embedded in a cavity formed by wet etching of the EMC resin and the Glass layer through wafer reconstruction technology, thereby realizing a high-integration design. The TGV structure used by the connection component and the Glass layer connects the EMC and the Glass layers through high-precision metal alignment bonding technology to ensure electrical conduction and structural stability. The RDL structure provides electrical lead-out and has the integrated expandability of the adapter board. Due to the EMC material characteristics and the warping deformation generated during its packaging process, the EMC wafer-level packaging faces difficulties in the subsequent multi-layer integrated wiring preparation process. While having high integration and mechanical strength, the present structure is stretched by the thermal expansion coefficient adaptation and bonding force between the EMC and Glass materials, effectively reducing the warping and meeting the subsequent higher-density wiring requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of semiconductor packaging, and in particular relates to a heterogeneous bonding three-dimensional integrated packaging structure. Background Art

[0002] With the rapid development of microelectronics technology, especially its wide application in high-performance computing, wireless communications, and military and aerospace fields, packaging technology is rapidly evolving towards miniaturization, high integration, and high reliability. Traditional two-dimensional packaging technology has gradually failed to meet the stringent requirements of modern packaging technology due to its size and integration limitations. EWLB (embedded wafer-level ball grid array) packaging technology has become the current mainstream advanced packaging solution due to its unique advantages, such as thinner package size, excellent RF (radio frequency) performance, high I / O (input / output) density, and low thermal resistance. It not only supports fan-out electrical I / O, but also can flexibly realize multi-chip integration. However, the inherent characteristics of epoxy resin materials make EWLB packaging prone to warping when facing temperature changes. This problem poses a challenge to the stability and reliability of the packaging structure, and thus affects the possibility of achieving a higher integration stacking structure. Therefore, how to effectively deal with and solve the warping problem has become the key to the further development of EWLB packaging technology.

[0003] The EWLB stress warping problem is mainly caused by differences in material properties, improper packaging process control, design factors and the accumulation of internal stress. The difference in thermal expansion coefficient between different materials causes stress when the temperature changes. The heat treatment steps in the packaging process, such as improper temperature control or uneven heating / cooling rates, can also cause uneven stress distribution. Unreasonable design, such as epoxy resin thickness, size, chip arrangement and improper material selection, may also aggravate the warping phenomenon. In addition, if the internal stress generated during the packaging process is not properly released or balanced, it will further cause warping problems. These problems not only affect the appearance of the packaging structure, but more importantly, they may have a negative impact on the performance and reliability of the components inside the package, thereby affecting the stability and reliability of the entire system. Moreover, the generation of warping in the EWLB structure will make it difficult to implement a higher-integration stacking structure and the preparation of subsequent RDL layers, and may also lead to an increase in heat dissipation problems, affecting the performance and life of the product. Summary of the invention

[0004] In view of the deficiencies in the prior art, the present invention provides a heterogeneous bonding three-dimensional integrated packaging structure, which has a high degree of integration and solves the problems of difficult stacking and integration due to stress warping and difficult preparation of RDL layers in the existing EWLB packaging structure.

[0005] In order to achieve the above object, the technical solution of the present invention is as follows:

[0006] A heterogeneous bonding three-dimensional integrated packaging structure is composed of an EMC overall layer (100), a Glass overall layer (200), an upper RDL layer (700), a lower RDL layer (500), an upper passivation layer (800), and a lower passivation layer (600); the EMC overall layer includes a connection component (110), a first semiconductor chip (120), and an epoxy resin (130); the Glass overall layer includes glass (210), a second semiconductor chip (220), and a TGV structure (400); the EMC overall layer (100) adopts a wafer reconstruction method to mount and The glass overall layer (200) is a wet etching layer, and the second semiconductor chip (220) is placed in the etching cavity through a mounting process; the two overall layers need to ensure that the through holes connecting the component (110) and the TGV structure (400) are exposed and have a flat surface, and metal bonding is performed between the through holes to form a metal bonding structure (300), thereby achieving electrical interconnection between the two overall layers; the upper RDL layer (700) and the lower RDL layer (500) are electrically connected and redistributed, and the upper passivation layer (800) and the lower passivation layer (600) are used for RDL layer surface protection.

[0007] The connection component (110) is a core particle through-hole structure, the through-hole is filled with metal, and the front and back sides have metal structures.

[0008] The connection component (110) is made of silicon (Si) and glass (Glass).

[0009] The TGV structure (400) is a blind hole structure, and metal copper is filled into the glass deep hole by electroplating technology to achieve metallization of the deep hole.

[0010] The thickness of the EMC overall layer (100) is the same as that of the first semiconductor chip (120); the thickness of the connection component (110) is the same as that of the first semiconductor chip (120); and the thickness of the Glass overall layer (200) is the same as that of the second semiconductor chip (220).

[0011] The number of mounted chips is expanded and adjusted according to actual design requirements.

[0012] The materials of the first semiconductor chip (120) and the second semiconductor chip (220) include silicon (Si), gallium nitride (GaN), silicon carbide (SiC), gallium phosphide (GaP), and gallium arsenide (GaAs).

[0013] The metal bonding structure (300) achieves high-strength connection between the EMC overall layer (100) and the Glass overall layer (200) by precisely controlling bonding temperature and pressure, and the metal bonding includes Au-Au bonding and Au-Sn bonding.

[0014] The number and thickness of the wiring layers of the upper RDL layer (700) and the lower RDL layer (500) are designed according to the actual number of chips and wiring requirements.

[0015] Beneficial Effects

[0016] Through the above scheme, the beneficial effects obtained by the present invention are as follows: (1) The bonding force after the glass overall layer is bonded to the EMC overall layer, as well as the material adaptability, are used to enhance the overall strength of the packaging structure, and the warping deformation problem caused by the stress of the epoxy resin is effectively solved, thereby ensuring the stability and reliability of the packaging structure under various working environments. (2) The precise metal bonding technology is adopted to ensure the stable connection between the EMC layer and the glass layer and the electrical interconnection between the semiconductor chips, thereby improving the compactness and high functional integration of the packaging structure and effectively improving the space utilization rate. (3) Epoxy resin is different from glass and silicon wafers, and it is difficult to achieve electrical interconnection in the material through process technology similar to TSV / TGV, resulting in EMC fan-out packaging to be multi-layer interconnected through an adapter board, which greatly increases the packaging cost and packaging size. The connection component in the present invention solves the problem of electrical interconnection in epoxy resin by making a core particle similar to TSV / TGV structure and using chip mounting, providing an effective solution for multi-layer integration. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 A front view schematic diagram of an embodiment of the present invention is disclosed;

[0018] Figure 2 This is a schematic diagram of the EMC overall layer of the present invention before thinning;

[0019] Figure 3 This is a schematic diagram of the warping of the EMC material of the present invention;

[0020] Figure 4 This is a schematic diagram of the EMC overall layer after thinning of the present invention;

[0021] Figure 5 It is a schematic diagram of the overall layer of Glass after etching of the present invention;

[0022] Figure 6 It is a schematic diagram of the glass overall layer chip after mounting and deep hole electroplating filling of the present invention;

[0023] Figure 7 It is a schematic diagram of the glass layer after thinning after metal bonding of the present invention;

[0024] Figure 8 A schematic diagram of the preparation of the upper redistribution layer of the present invention;

[0025] Fig. 9 A schematic diagram of the preparation of the lower redistribution layer of the present invention;

[0026] Fig.10 It is a schematic diagram of further three-dimensional stacking of the present invention.

[0027] The meanings of some of the figure marks are as follows: 100-EMC overall layer; 200-Glass overall layer; 110-connection component; 120-first semiconductor chip; 130-epoxy resin; 210-glass; 220-second semiconductor chip; 230-chip placement cavity; 240-TGV cavity; 300-metal bonding structure; 400-TGV structure; 700-upper RDL layer; 800-upper passivation layer; 500-lower RDL layer; 600-lower passivation layer; 900-substrate; 1000-third semiconductor chip. DETAILED DESCRIPTION

[0028] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0029] like Figure 1 As shown, a heterogeneous bonding three-dimensional integrated packaging structure of the present invention is disclosed, wherein the EMC overall layer 100 is an epoxy resin layer, and the first semiconductor chip 120 is embedded therein in a wafer reconstruction packaging form; the Glass overall layer 200 is a glass layer, and the glass 210 is laser punched and then HF wet etched to form corresponding deep holes and cavities, the deep holes are used for electroplating filling to form upper and lower electrical connection channels, and the cavity is used for mounting the second semiconductor chip 220, and the second semiconductor chip 220 is precisely embedded and mounted in the Glass overall layer 200; the electrical connection components in the EMC overall layer 100 can be TSV / TGV structures made of Si or Glass materials, and the metal bonding structure 300 adopts metal alignment bonding to ensure electrical connection and mechanical stability between the upper and lower layers. Furthermore, the upper and lower RDL layer wiring is prepared to achieve electrical connection and redistribution, and multi-layer stacking can be performed based on this structure; a passivation layer is coated on top of the RDL layer, leaving only the metal PAD connection position to protect the packaging structure from the external environment and improve the weather resistance and stability of the device.

[0030] like Figure 2As shown, the EMC overall layer 100 adopts a wafer reconstruction method to mount the connection component 110 and the first semiconductor chip 120 on a carrier covered with a pyrolytic tape by flip-chip mounting (the PAD surface faces the pyrolytic tape surface), and then molds them with epoxy resin. After molding, the bottom is heated, and the bottom carrier is removed by using the characteristics of the pyrolytic adhesive film, and finally baked and cured.

[0031] like Figure 3 As shown, after the EMC overall layer 100 is completed, the epoxy resin 130, the first semiconductor chip 120, and the connection component 110 have different thermal expansion coefficients, causing the EMC layer to present a warping state of "crying face" or "smiling face" to varying degrees.

[0032] like Figure 4 As shown, the chip PAD surface of the EMC overall layer 100 is protected by a resin film, and the excess epoxy resin on the back is ground and thinned by CMP (chemical mechanical polishing). Finally, the thickness of the epoxy resin layer is consistent with the thickness of the first semiconductor chip 120.

[0033] like Figure 5 As shown, the glass overall layer 200 is formed into a chip placement cavity 230 and a TGV cavity 240 by laser induced drilling and HF wet etching, and the depth of these two cavities is consistent with the thickness of the second semiconductor chip 220. The deep cavity ratio of the glass overall layer 200 opening to depth should be considered whether it meets the existing process capabilities to avoid the deep cavity PVD being unable to adhere to the inner wall and the existence of voids in the electroplating filling, resulting in electrical connection failure.

[0034] like Figure 6 As shown, the second semiconductor chip 220 is mounted in the chip placement cavity 230 of the Glass overall layer 200 in the form of a flip chip, and the deep hole is filled with Cu by PVD deposition and electroplating, and then the metal Cu-Ti etching and surface metal CMP technology are used to improve the surface flatness. Finally, annealing treatment is performed to reduce the stress between the glass and Cu.

[0035] like Figure 7 As shown, the bonding points of the Glass overall layer 200 and the EMC overall layer 100 are subjected to metallization plating, and then the through holes of the connection component 110 and the TGV structure 400 are aligned and permanently bonded to form a metal bonding structure 300 .

[0036] Furthermore, the metallization process is not limited to a certain metal. According to specific application requirements, cost considerations and material availability, metals or metal alloys can be flexibly selected for post-plating bonding, including Au-Au bonding or Au-Sn bonding.

[0037] Furthermore, by aligning and bonding with the Glass overall layer 200, a tensile bonding force is provided for the EMC overall layer 100, effectively solving the warping of the EMC overall layer 100. During bonding, pressure and temperature are mainly required to avoid wafer breakage or relative displacement.

[0038] Furthermore, the front side of the EMC overall layer 100 is protected by a resin film, and the back side glass is ground and thinned by CMP (chemical mechanical polishing) until the thickness of the glass is consistent with the thickness of the second semiconductor chip 220, and then the resin film is torn off.

[0039] The thickness of the EMC overall layer 100 and the Glass overall layer 200 may be different, but the adaptability of materials of different thicknesses and the thickness of the chip must be considered. Generally, the larger the wafer size and the thicker the epoxy resin, the greater the stress and the more severe the warping; the larger the glass size and the thicker the thickness, the stronger the bonding tensile force.

[0040] like Figure 8 As shown, the upper RDL layer 700 and the upper passivation layer 800 are prepared by coating and edge washing, exposure and development, PVD, and electroplating and etching processes. It should be noted that when the EMC overall layer 100 is deposited by PVD, the thickness of the PVD seed layer Ti-Cu should be increased to avoid erosion of the EMC material after wet etching, resulting in PVD faults, electroplating failure, and electrical connection failure.

[0041] like Fig. 9 As shown, the upper RDL layer 700 and the upper passivation layer 800 are prepared, the upper surface is temporarily protected by a temporary bonding carrier, and then the lower RDL layer 500 and the lower passivation layer 600 are prepared. After completion, a debonding process is performed by laser debonding, and cleaning is performed after the process is completed.

[0042] like Fig.10 As shown, the EMC overall layer 100 and the Glass overall layer 200 are respectively led out with RDL redistribution layers, which can be mounted on the substrate 900 to form a transfer board. By further mounting the third semiconductor chip 1000, three-dimensional stacking is achieved to improve integration and performance density.

[0043] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any technical personnel in this field can make corresponding changes and modifications to the technical solution of the present invention by using the methods and technical contents disclosed above without departing from the spirit and scope of the present invention. Therefore, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention shall fall within the protection scope of the technical solution of the present invention.

Claims

1. A heterogeneous bonding three-dimensional integrated packaging structure, characterized in that: The invention is composed of an EMC overall layer (100), a Glass overall layer (200), an upper RDL layer (700), a lower RDL layer (500), an upper passivation layer (800), and a lower passivation layer (600); the EMC overall layer comprises a connection component (110), a first semiconductor chip (120), and an epoxy resin (130); the Glass overall layer comprises glass (210), a second semiconductor chip (220), and a TGV structure (400); the EMC overall layer (100) adopts a wafer reconstruction method, and the first semiconductor chip (120) and the connection component (110) are embedded in the epoxy resin by mounting and molding; the Glass overall layer (200) is a wet etching layer, and the second semiconductor chip (220) is placed in a cavity formed by etching of the Glass overall layer (200) by a mounting process; The back of the glass (210) is then ground and thinned by a thinning process, so that the thickness of the glass (210) is consistent with the thickness of the second semiconductor chip (220); the EMC overall layer (100) and the Glass overall layer (200) need to ensure that the through holes of the connection component (110) and the TGV structure (400) are exposed and the surface is flat, and metal bonding is performed between the through holes to form a metal bonding structure (300), thereby realizing electrical interconnection between the two overall layers; the upper RDL layer (700) and the lower RDL layer (500) are electrically connected and redistributed, and the upper passivation layer (800) and the lower passivation layer (600) are used for RDL layer surface protection; the connection component (110) is a core particle through hole structure, the through hole is filled with metal, and the front and back sides have a metal structure, the thickness of the connection component (110) is the same as the thickness of the first semiconductor chip (120), and the material of the connection component (110) includes silicon or glass.

2. According to the heterogeneous bonding three-dimensional integrated packaging structure described in claim 1, the TGV structure (400) is a blind hole structure, and metal copper is filled into the glass deep hole by electroplating technology to achieve metallization of the deep hole.

3. The heterogeneous bonding three-dimensional integrated packaging structure according to claim 1, characterized in that: The thickness of the EMC overall layer (100) is the same as that of the first semiconductor chip (120); and the thickness of the Glass overall layer (200) is the same as that of the second semiconductor chip (220).

4. The heterogeneous bonding three-dimensional integrated packaging structure according to claim 1, characterized in that: The materials of the first semiconductor chip (120) and the second semiconductor chip (220) include silicon, gallium nitride, silicon carbide, gallium phosphide or gallium arsenide.

5. The heterogeneous bonding three-dimensional integrated packaging structure according to claim 1, characterized in that: The metal bonding structure (300) achieves high-strength connection between the EMC overall layer (100) and the Glass overall layer (200) by precisely controlling bonding temperature and pressure, and the metal bonding includes Au-Au bonding and Au-Sn bonding.