A ceramic ferrule and a test jumper for high-speed optical modules

By opening rubber-repellent holes on the ceramic ferrule, the area length of the hard glue bonding between the bare optical fiber and the ceramic ferrule is shortened, and the problem of bare optical fibers being easily damaged in low-temperature and high-temperature tests is solved, and the high-speed optical module is improved test yield.

CN118655662BActive Publication Date: 2024-11-15武汉钧恒科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411142757.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-15
Estimated Expiration
2044-08-20

AI Technical Summary

Technical Problem

The difference in thermal expansion coefficient between traditional ceramic ferrules and bare optical fibers causes bare optical fibers to be easily damaged or unable to effectively contact the high-speed optical module during low and high temperature tests, increasing light reflection and insertion loss.

Method used

Open a rubber-repellent hole on the ceramic ferrule to shorten the area length of the hard rubber bond between the bare optical fiber and the ceramic ferrule, prevent the hard rubber from flowing into the inner hole, and reduce the convex or concave of the bare optical fiber caused by thermal expansion and contraction.

Benefits of technology

It reduces the probability of bare optical fiber damage and light reflection, and improves the test yield of high-speed optical modules, especially under high and low temperature conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118655662B_ABST
    Figure CN118655662B_ABST
Patent Text Reader

Abstract

The present invention relates to a ceramic ferrule, comprising: a ferrule body, an inner hole for inserting a bare optical fiber in an optical fiber is formed through the ferrule body along the axis, a glue avoidance hole intersecting with the inner hole is formed through the ferrule body at a predetermined distance from its front end face in the radial direction, and the inner hole is completely cut off by the glue avoidance hole. A test jumper for a high-speed optical module comprises: an optical fiber and a ceramic ferrule, the bare optical fiber of the optical fiber is inserted into the inner hole of the ceramic ferrule and its front end face is flush with the front end face of the ceramic ferrule, the inner hole is located in the section between the front end face of the ceramic ferrule and the glue avoidance hole and filled with hard glue for fixing the bare optical fiber, and the inner hole is located in the section between the rear end face of the ceramic ferrule and the glue avoidance hole and filled with soft glue for fixing the bare optical fiber. The beneficial effect is: without changing the outer dimensions and material of the ceramic ferrule and the outer dimensions and material of the bare optical fiber, by forming a specific glue avoidance hole on the ceramic ferrule, the high and low temperature test yield of the high-speed optical module can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of optical module testing, and in particular to a ceramic ferrule and a test jumper for a high-speed optical module. Background Art

[0002] High-speed optical modules are usually tested at room temperature, low temperature, and high temperature. For example, room temperature is 25°C, low temperature is -40°C, and high temperature is 85°C. At this time, the temperature difference between high temperature and room temperature, as well as the temperature difference between low temperature and room temperature, is basically above 60°C.

[0003] High-speed optical modules use test jumpers during normal temperature, low temperature, and high temperature testing. Traditional test jumpers include: ceramic ferrules, optical fibers, and tail handles. The ceramic ferrule structure used is as follows: Figure 1 As shown, the bare optical fiber of the optical fiber is inserted into the inner hole of the ceramic ferrule and its front end face is flush with the front end face of the ceramic ferrule. The gap between the inner hole and the bare optical fiber is filled with hard glue to fix the bare optical fiber. The length of the area where the bare optical fiber and the ceramic ferrule are bonded with the hard glue is the same as the length of the inner hole, that is, the same as the length of the ceramic ferrule. A tail handle is set at the tail end of the ceramic ferrule, and the ceramic ferrule and the tail handle are bonded with hard glue. The area with the plastic cladding of the optical fiber is in the tail handle, and the plastic cladding of the optical fiber is bonded with the tail handle with hard glue. The structure of the test jumper finally formed is as shown in the figure. Figure 2 As shown, the bare optical fiber of the optical fiber is made of quartz glass, whose thermal expansion coefficient is 0.5ppm / ℃, that is, 0.5×0.000001 / ℃, and the ceramic ferrule is made of zirconium dioxide, whose thermal expansion coefficient is 11.7ppm / ℃, that is, 11.7×0.000001 / ℃.

[0004] Taking the SC test patch cord as an example, the total length of the ceramic ferrule is about 10.6mm, and the length of the area where the bare fiber and the ceramic ferrule are bonded with the hard glue is 10.6mm. Due to the large difference in thermal expansion coefficients between the ceramic ferrule and the bare fiber, the thermal expansion and contraction lengths are inconsistent. Figure 3 As shown in the figure, when this type of test jumper is used with a high-speed optical module for low-temperature testing, the bare optical fiber will protrude beyond the front end of the ceramic ferrule, which can easily damage the optical fiber end face of the high-speed optical module being tested. Figure 4 As shown in the figure, when this type of test patch cord is used with a high-speed optical module for high-temperature testing, the bare fiber will be concave, resulting in a large gap between the end face of the bare fiber and the end face of the high-speed optical module being tested. This makes it difficult for the end face of the bare fiber to align well with the end face of the high-speed optical module being tested, which will increase additional light reflection (Fresnel reflection) and insertion loss.

[0005] Taking low temperature as an example, the temperature difference is 25℃-(-40℃)=65℃, the shrinkage of bare fiber = 10.6mm×65℃×0.5×0.000001 / ℃=344.5×0.000001mm=344.5×0.001um=0.3445um, the shrinkage of ceramic ferrule = 10.6mm×65℃×11.7×0.000001 / ℃=8061.3×0.000001mm=8061.3×0.001 mm = 8.613 μm. A rough calculation using the center point of the ceramic ferrule's total length as the origin of contraction shows that the bare fiber protrusion is theoretically calculated to be (8.613 μm - 0.3445 μm) / 2 = 3.9 μm. This 3.9 μm protrusion is relatively large, making it sufficient for the bare fiber to damage the fiber end face of the high-speed optical module being tested. Similarly, at high temperatures, excessive fiber indentation creates a large gap between the bare fiber and the fiber end face of the module being tested, increasing additional light reflection (Fresnel reflection) and insertion loss. Summary of the Invention

[0006] The technical problem to be solved by the present invention is to provide a ceramic ferrule and a test jumper for a high-speed optical module, so as to overcome the deficiencies in the above-mentioned prior art.

[0007] The technical solution of the present invention to solve the above-mentioned technical problems is as follows: a ceramic ferrule, comprising: a ferrule body, an inner hole for passing a bare optical fiber in an optical fiber is formed through the ferrule body along the axis, and a glue avoidance hole intersecting with the inner hole is formed through the ferrule body along the radial direction at a predetermined distance from its front end face, and the inner hole is completely cut off by the glue avoidance hole.

[0008] The beneficial effects of the present invention are:

[0009] The present invention provides a specific glue avoidance hole on the ceramic ferrule without changing its external dimensions and material. When the ceramic ferrule is used in a test jumper, due to the presence of the glue avoidance hole, after the hard glue is filled in the section between the front end face of the ceramic ferrule and the glue avoidance hole, the capillary flow of the hard glue will stop in the glue avoidance hole, thereby preventing it from flowing into the section between the rear end face of the ceramic ferrule and the glue avoidance hole. Compared with the prior art, the total length of the area where the bare optical fiber and the ceramic ferrule are bonded with the hard glue is shortened. Taking the SC test jumper as an example, the total length of the area where the bare optical fiber and the ceramic ferrule are bonded with the hard glue is smaller than 10.6 mm. When the test jumper having the ceramic ferrule is When testing high-speed optical modules at low temperatures, the total length of the area where the bare fiber and the ceramic ferrule are bonded together is shortened, so the length of the bare fiber protruding from the ceramic ferrule is also shortened. This reduces the probability of damage to the fiber end face of the tested high-speed optical module, significantly reducing the defect rate of the tested high-speed optical module's fiber end face. Similarly, when a test patch cord with this ceramic ferrule is used to test high-speed optical modules at high temperatures, the total length of the area where the bare fiber and the ceramic ferrule are bonded together is shortened, so the amount of bare fiber recessed is also reduced. This reduces the gap variation between the end face of the bare fiber and the end face of the tested high-speed optical module, and correspondingly optimizes light reflection and insertion loss, effectively improving the high-temperature test yield.

[0010] On the basis of the above technical solution, the present invention can also be improved as follows.

[0011] Furthermore, the distance between the glue avoidance hole on the ferrule body and the front end surface thereof is 1 mm to 1.5 mm.

[0012] The above method has the following further beneficial effects: the total length of the area where the bare optical fiber and the ceramic ferrule are bonded with hard glue can be shortened to 1mm~1.5mm, that is, the total length of the thermal expansion and contraction area is changed from 10.6mm to 1mm~1.5mm. A theoretical estimate shows that at low temperature of 10.6mm, the protruding length of the bare optical fiber is 3.9um, while at 1mm~1.5mm, the protruding length of the bare optical fiber is 3.9um×(1mm~1.5mm) / 10.6mm=0.37um~0.55um, that is, the protruding length of the bare optical fiber at low temperature is greatly optimized from the original 3.9um to 0.37um~0.55um, which greatly reduces the defective rate of the optical fiber end face of the tested high-speed optical module.

[0013] Furthermore, the distance between the glue-avoiding hole on the ferrule body and the front end surface thereof is 1.5 mm.

[0014] The above further beneficial effect is that in actual process, the shorter the distance, the better the effect. However, the bonding strength of the bare optical fiber will become worse, resulting in a reduction in the number of tests and affecting the use. Therefore, 1.5mm is preferred.

[0015] Furthermore, the outer diameter of the ferrule body is 2.5 mm, the inner diameter of the inner hole is 0.127 mm, and the glue-avoiding hole is a circular hole with an inner diameter of 0.5 mm to 1 mm.

[0016] Furthermore, the inner diameter of the glue-avoiding hole is 1 mm.

[0017] Furthermore, the outer diameter of the ferrule body is 1.25 mm, the inner diameter of the inner hole is 0.127 mm; the glue-avoiding hole is a circular hole with an inner diameter of 0.4 mm to 0.6 mm.

[0018] Furthermore, the inner diameter of the glue-avoiding hole is 0.5 mm.

[0019] Furthermore, a tapered groove is provided at the opening of the inner hole at the rear end of the ferrule body.

[0020] Based on the above technical solution, the present invention also provides a test jumper for a high-speed optical module, comprising: an optical fiber and a ceramic ferrule, wherein the bare optical fiber of the optical fiber is inserted into the inner hole of the ceramic ferrule and its front end face is flush with the front end face of the ceramic ferrule, the inner hole is located in a section between the front end face of the ceramic ferrule and the glue avoidance hole and is filled with hard glue for fixing the bare optical fiber, and the inner hole is located in a section between the rear end face of the ceramic ferrule and the glue avoidance hole and is filled with soft glue for fixing the bare optical fiber.

[0021] The above-mentioned method has the following further beneficial effects: without changing the overall dimensions and material of the ceramic ferrule or the bare fiber, the total length of the adhesive bond between the bare fiber and the ceramic ferrule is shortened. Taking the SC test patch cord as an example, the total length of the adhesive bond between the bare fiber and the ceramic ferrule is reduced to less than 10.6 mm. When the test patch cord with this ceramic ferrule is used in conjunction with a high-speed optical module for low-temperature testing, the shortened total length of the adhesive bond between the bare fiber and the ceramic ferrule shortens the length of the bare fiber protruding from the ceramic ferrule, thereby reducing the probability of damage to the fiber end face of the tested high-speed optical module and significantly reducing the defective rate of the tested high-speed optical module. Similarly, when the test patch cord with this ceramic ferrule is used to test a high-speed optical module at high temperature, the shortened total length of the adhesive bond between the bare fiber and the ceramic ferrule reduces the amount of bare fiber recessed. This reduces the gap variation between the end face of the bare fiber and the end face of the tested high-speed optical module, resulting in optimized light reflection and insertion loss, effectively improving the high-temperature test yield.

[0022] Furthermore, a tail handle is mounted on the tail end of the ceramic ferrule, the area of ​​the optical fiber with the plastic cladding is located inside the tail handle, and the plastic cladding of the optical fiber and the tail handle are bonded with soft glue. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a structural diagram of a ceramic ferrule in the prior art;

[0024] Figure 2This is a structural diagram of a test jumper at room temperature in the prior art;

[0025] Figure 3 This is a structural diagram of a test jumper at low temperature in the prior art;

[0026] Figure 4 This is a structural diagram of a test jumper at high temperature in the prior art;

[0027] Figure 5 This is a structural diagram of the ceramic ferrule in the present invention;

[0028] Figure 6 This is a structural diagram of the test jumper in the present invention.

[0029] In the accompanying drawings, the components represented by the reference numerals are as follows:

[0030] 1. Ceramic ferrule, 110. Ferrule body, 111. Inner hole, 112. Tapered groove, 120. Glue-avoiding hole, 2. Optical fiber, 210. Bare optical fiber, 220. Plastic cladding, 3. Hard glue, 4. Soft glue, 5. Tail handle. DETAILED DESCRIPTION

[0031] The principles and features of the present invention are described below with reference to the accompanying drawings. The examples given are only used to explain the present invention and are not used to limit the scope of the present invention.

[0032] Example 1

[0033] like Figure 5 As shown, a ceramic ferrule includes: a ferrule body 110, the material used for the ferrule body 110 remains unchanged, that is, the zirconium dioxide material in the prior art, and an inner hole 111 is formed along the axis of the ferrule body 110, and the inner hole 111 is used to pass the bare optical fiber 210 in the optical fiber 2;

[0034] A glue avoidance hole 120 is radially formed on the ferrule body 110 at a predetermined distance from the front end thereof and intersects with the inner hole 111. The inner hole 111 is completely cut off by the glue avoidance hole 120. The glue avoidance hole 120 may be perpendicular to the axis of the ferrule body 110 or may not be perpendicular to the axis of the ferrule body 110.

[0035] The present invention provides a specific glue avoidance hole 120 on the ceramic ferrule 1 without changing its external dimensions and material. When the ceramic ferrule 1 is used in a test jumper, due to the presence of the glue avoidance hole 120, after the hard glue 3 is filled in the section between the front end face of the ceramic ferrule 1 and the glue avoidance hole 120 at the inner hole 111, the capillary flow of the hard glue 3 will stop in the glue avoidance hole 120, and thus will not flow into the section between the rear end face of the ceramic ferrule 1 and the glue avoidance hole 120 at the inner hole 111. Compared with the prior art, the total length of the area where the bare optical fiber 210 and the ceramic ferrule 1 are bonded with the hard glue 3 is shortened. Taking the SC test jumper as an example, the total length of the area where the bare optical fiber 210 and the ceramic ferrule 1 are bonded with the hard glue 3 is smaller than 10.6 mm. When the ceramic ferrule 1 is provided with the present invention, the hard glue 3 is filled in the section between the front end face of the ceramic ferrule 1 and the glue avoidance hole 120. When a test jumper with core 1 is used in conjunction with a high-speed optical module for low-temperature testing, the total length of the area where the bare fiber 210 and the ceramic ferrule 1 are bonded to the hard adhesive 3 is shortened. As a result, the length of the bare fiber 210 protruding from the ceramic ferrule 1 is shortened, thereby reducing the probability of damaging the end face of the optical fiber of the tested high-speed optical module, that is, significantly reducing the defect rate of the optical fiber end face of the tested high-speed optical module. Similarly, when a test jumper with this ceramic ferrule 1 is used to test a high-speed optical module at high temperature, the total length of the area where the bare fiber 210 and the ceramic ferrule 1 are bonded to the hard adhesive 3 is shortened, so the amount of indentation of the bare fiber 210 is also reduced. In other words, the change in the gap between the end face of the bare fiber 210 and the end face of the optical fiber of the tested high-speed optical module is reduced, and the corresponding light reflection and insertion loss are also optimized, effectively improving the high-temperature test yield.

[0036] Example 2

[0037] like Figure 5 As shown, this embodiment is a further improvement on the basis of embodiment 1, specifically as follows:

[0038] The distance between the glue-avoiding hole 120 on the ferrule body 110 and its front end face is 1mm to 1.5mm, thereby shortening the total length of the area where the bare optical fiber 210 and the ceramic ferrule 1 are bonded with the hard glue 3 to 1mm to 1.5mm. That is, the total length of the thermal expansion and contraction area is reduced from 10.6mm to 1mm to 1.5mm. According to theoretical estimation, at low temperature of 10.6mm, the protruding length of the bare optical fiber 210 is 3.9um, while at 1mm to 1.5mm, the protruding length of the bare optical fiber 210 is 3.9um × (1mm to 1.5mm) / 10.6mm = 0.37um to 0.55um. That is, the protruding length of the bare optical fiber 210 at low temperature is greatly optimized from the original 3.9um to 0.37um to 0.55um, which greatly reduces the defective rate of the optical fiber end face of the tested high-speed optical module.

[0039] Furthermore, the distance between the glue-avoiding hole 120 on the ferrule body 110 and its front end face is 1.5 mm. In actual practice, the shorter the distance, the better the effect. However, the bonding strength of the bare optical fiber 210 will be weakened, resulting in a reduction in the number of tests and affecting the use. Therefore, 1.5 mm is preferred.

[0040] like Figure 5 As shown, this embodiment is a further improvement on the basis of embodiment 1 or 2, specifically as follows:

[0041] Taking a 2.5mm SC ceramic ferrule as an example, the outer diameter of the ferrule body 110 is 2.5mm, the inner diameter of the inner hole 111 is 0.127mm, and the glue avoidance hole 120 is a circular hole with an inner diameter of 0.5mm to 1mm. Preferably, the inner diameter of the glue avoidance hole 120 is 1mm.

[0042] Taking a 1.25mm LC ceramic ferrule as an example, the outer diameter of the ferrule body 110 is 1.25mm, the inner diameter of the inner hole 111 is 0.127mm, and the glue avoidance hole 120 is a circular hole with an inner diameter of 0.4mm to 0.6mm. Preferably, the inner diameter of the glue avoidance hole 120 is 0.5mm.

[0043] Other types of jumpers can be processed similarly as long as they use ceramic ferrules. However, no matter how they are changed, it is always necessary to ensure that the glue-avoiding hole 120 completely cuts off the inner hole 111, while also making the ceramic ferrule 1 less likely to break.

[0044] In addition, the shape of the glue avoidance hole 120 may not be circular, but other shapes, such as polygonal, elliptical, etc. In this embodiment, a circular shape is preferred because: the circular shape is easier to process, has the least stress, and is not likely to cause the ceramic ferrule 1 to break.

[0045] Example 4

[0046] like Figure 5 As shown, this embodiment is a further improvement on the basis of embodiment 1, 2 or 3, and the details are as follows:

[0047] A tapered groove 112 is provided at the rear end of the ferrule body 110 at the opening of the inner hole 111 .

[0048] Example 5

[0049] like Figure 5 、 Figure 6As shown, a test jumper for a high-speed optical module comprises: an optical fiber 2 and a ceramic ferrule 1 as described in any one of Examples 1 to 4, the material used for the bare optical fiber 210 remains unchanged, that is, quartz glass in the prior art, the bare optical fiber 210 of the optical fiber 2 is inserted into the inner hole 111 of the ceramic ferrule 1, and the front end face of the bare optical fiber 210 inserted into the inner hole 111 of the ceramic ferrule 1 is flush with the front end face of the ceramic ferrule 1, the section of the inner hole 111 between the front end face of the ceramic ferrule 1 and the glue avoidance hole 120 is filled with a hard glue 3 for fixing the bare optical fiber 210, and the section of the inner hole 111 between the rear end face of the ceramic ferrule 1 and the glue avoidance hole 120 is filled with a soft glue 4 for fixing the bare optical fiber 210. Compared with the prior art, without changing the outer dimensions, material of the ceramic ferrule 1 and the outer dimensions and material of the bare optical fiber 210, the total length of the area where the bare optical fiber 210 and the ceramic ferrule 1 are bonded with the hard glue 3 is shortened, so as to S Taking the C test patch cord as an example, the total length of the area where the bare optical fiber 210 and the ceramic ferrule 1 are bonded with the hard adhesive 3 is made smaller than 10.6 mm. When the test patch cord with this ceramic ferrule 1 is used in conjunction with a high-speed optical module for low-temperature testing, the total length of the area where the bare optical fiber 210 and the ceramic ferrule 1 are bonded with the hard adhesive 3 is shortened, and therefore the length of the bare optical fiber 210 protruding from the ceramic ferrule 1 is shortened, thereby reducing the probability of damaging the optical fiber end face of the tested high-speed optical module, that is, significantly reducing the defective rate of the optical fiber end face of the tested high-speed optical module. Similarly, when the test patch cord with this ceramic ferrule 1 is used to test the high-speed optical module at high temperature, the total length of the area where the bare optical fiber 210 and the ceramic ferrule 1 are bonded with the hard adhesive 3 is shortened, so the amount of indentation of the bare optical fiber 210 is also reduced. In other words, the change in the gap between the end face of the bare optical fiber 210 and the end face of the optical fiber of the tested high-speed optical module is reduced, and the corresponding light reflection and insertion loss are also optimized, effectively improving the high-temperature test yield.

[0050] In this embodiment, the hard glue 3 is still the same type as that used in the prior art, such as 353ND glue, and the soft glue 4 used is also a common glue on the market, so it is not clearly defined here. Since the soft glue 4 is very soft, the bare optical fiber 210 will not be restrained by the soft glue 4. The bare optical fiber 210 can freely expand and contract relative to the ceramic ferrule 1. The soft glue 4 can be regarded as air. The purpose of the soft glue 4 is to act as a buffer to prevent the bare optical fiber 210 from being torn when external force is applied to bend the optical fiber 2.

[0051] In addition, a tail handle 5 is mounted on the tail end of the ceramic ferrule 1 , and the area of ​​the optical fiber 2 with the plastic cladding 220 is located inside the tail handle 5 , and the plastic cladding 220 of the optical fiber 2 and the tail handle 5 are bonded with soft glue 4 .

[0052] Although the embodiments of the present invention have been shown and described above, it will be understood that the above embodiments are illustrative and are not to be construed as limitations on the present invention. A person skilled in the art may change, modify, replace and modify the above embodiments within the scope of the present invention.

Claims

1. A test jumper for a high-speed optical module, characterized in that: include: An optical fiber (2) and a ceramic ferrule (1), wherein the ceramic ferrule (1) comprises: a ferrule body (110), wherein an inner hole (111) for inserting a bare optical fiber (210) in the optical fiber (2) is formed through the ferrule body (110) along the axis, wherein a glue avoidance hole (120) intersecting the inner hole (111) is formed through the ferrule body (110) along the radial direction at a predetermined distance from the front end surface thereof, and wherein the inner hole (111) is completely cut off by the glue avoidance hole (120), and the glue avoidance hole (120) formed on the ferrule body (110) is 1.5 meters in diameter. The distance between the front end faces is 1 mm to 1.5 mm. The bare optical fiber (210) of the optical fiber (2) is inserted into the inner hole (111) of the ceramic ferrule (1) and its front end face is flush with the front end face of the ceramic ferrule (1). The section of the inner hole (111) between the front end face of the ceramic ferrule (1) and the glue avoidance hole (120) is filled with hard glue (3) for fixing the bare optical fiber (210). The section of the inner hole (111) between the rear end face of the ceramic ferrule (1) and the glue avoidance hole (120) is filled with soft glue (4) for fixing the bare optical fiber (210).

2. A test jumper for a high-speed optical module according to claim 1, characterized in that: The distance between the glue avoidance hole (120) opened on the insert body (110) and the front end surface thereof is 1.5 mm.

3. A test jumper for a high-speed optical module according to claim 1, characterized in that: The outer diameter of the insert body (110) is 2.5 mm, and the inner diameter of the inner hole (111) is 0.127 mm; the glue avoidance hole (120) is a circular hole, and its inner diameter is 0.5 mm to 1 mm.

4. A test jumper for a high-speed optical module according to claim 3, characterized in that: The inner diameter of the glue-avoiding hole (120) is 1 mm.

5. A test jumper for a high-speed optical module according to claim 1, characterized in that: The outer diameter of the insert body (110) is 1.25 mm, and the inner diameter of the inner hole (111) is 0.127 mm; the glue avoidance hole (120) is a circular hole, and its inner diameter is 0.4 mm to 0.6 mm.

6. A test jumper for a high-speed optical module according to claim 5, characterized in that: The inner diameter of the glue-avoiding hole (120) is 0.5 mm.

7. A test jumper for a high-speed optical module according to claim 1, characterized in that: A tapered groove (112) is provided at the rear end of the insert body (110) at the opening of the inner hole (111).

8. A test jumper for a high-speed optical module according to claim 1, characterized in that: A tail handle (5) is mounted on the tail end of the ceramic ferrule (1); the region of the optical fiber (2) having the plastic cladding (220) is located within the tail handle (5); and the plastic cladding (220) of the optical fiber (2) and the tail handle (5) are bonded with soft glue (4).