A method for laminating a reinforcement layer without connection points and a circuit board
Through the joint point-free reinforced layer bonding method, laser depth-controlled cutting and peelable cover film are used to partially apply AD epoxy resin pure glue, which solves the auxiliary edge bonding phenomenon and production efficiency in traditional bonding methods. Low problems achieve efficient reinforced layer bonding and circuit board production.
Patent Information
- Application Number
- CN202411171010.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-08-26
AI Technical Summary
The traditional bonding method has AD epoxy resin pure glue on the entire surface of the reinforcement layer, which makes the auxiliary edge prone to bonding, and the inability to batch set bonding leads to low production efficiency.
Using the connection point-free reinforcement layer bonding method, laser depth-controlled cutting is performed by obtaining the FR-4 epoxy resin substrate and peelable cover film, locally bonding AD epoxy resin pure glue, and retaining the connecting bridge on the reinforcement board , multiple reinforcement boards are stacked to form a reinforcement layer, combined with flexible circuit boards for bonding and fast pressing until curing.
The auxiliary edge bonding phenomenon is solved, production efficiency is improved, and the flatness and reliability of the reinforced layer are ensured.
Smart Images

Figure CN118678555B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of flexible circuit boards, and in particular to a method for laminating a reinforcement layer without connection points and a circuit board. Background Art
[0002] Flexible circuit boards, with their excellent bendability and lightweight and precision characteristics, are gradually showing their wide application value in many fields. However, when performing patch or device installation, this type of soft circuit board needs to add a reinforcement layer on the back to ensure the flatness and reliability of the device installation area. The material selection of the reinforcement layer is wide, including but not limited to FR-4 epoxy resin and steel sheet.
[0003] At present, printed circuit board manufacturers mainly use two methods to process steel sheet reinforcement layers: first, through precise etching process, the steel sheet is processed into a set (sheet, meaning PCB board, referred to as set) panel connection form; second, the single steel sheet is arranged on a micro-adhesive film to make a roll, so that the machine can automatically fit it. Similarly, FR-4 epoxy resin reinforced board also has its own unique processing methods: one is to make it into single pcs (pieces, meaning sheets, referred to as pcs) for bonding, and the other is to make it into a set panel connection form.
[0004] However, since it is necessary to add sticky AD epoxy resin pure glue on the back of the reinforcement board, no matter which bonding method is used, it is inevitable to glue the entire back of the reinforcement layer. This phenomenon is particularly obvious during the set bonding process, and during the lamination process, the auxiliary edge of the reinforcement layer connecting the pcs will also be glued to the circuit board. Therefore, when the reinforcement layer of the circuit board is located inside the pattern, in order to avoid the auxiliary edge from bonding with the effective pattern, the traditional set bonding method will not be able to adapt, which brings certain challenges to manual operation and affects the overall production efficiency. Summary of the invention
[0005] Based on this, the purpose of the present invention is to provide a whole board bonding method and circuit board without a connection point reinforcement layer, which is used to solve the technical problems that the traditional bonding method has AD epoxy resin pure glue on the entire surface of the reinforcement layer, which makes the auxiliary edge easy to stick, and cannot be batch-set bonded, resulting in low production efficiency.
[0006] In one aspect, the present invention provides a method for laminating a reinforcement layer without a connection point, comprising:
[0007] Obtain a flexible circuit board and a FR-4 epoxy resin substrate of a size corresponding to the flexible circuit board, and etch the FR-4 epoxy resin substrate to remove copper on both sides of the FR-4 epoxy resin substrate to obtain a reinforcement board with both sides being substrates;
[0008] Obtain a peelable cover film of a size corresponding to the FR-4 epoxy resin substrate, and attach the peelable cover film to the reinforcing plate to obtain a plate-film combination structure, wherein the peelable cover film is a low-viscosity single-sided adhesive PE film;
[0009] The side of the plate-film combination structure that is attached to the peelable cover film faces upward, the plate-film combination structure is cut through the peelable cover film by laser depth control, and a reinforcement area is cut on the reinforcement plate, and the peelable cover film on the reinforcement area is removed to expose the reinforcement plate;
[0010] Obtain an AD epoxy resin glue having a size corresponding to that of the peelable cover film, and attach the entire surface of the AD epoxy resin glue to the cut peelable cover film, and place the peelable cover film attached with the AD epoxy resin glue on a laser cutting machine, and perform depth-controlled cutting of the AD epoxy resin glue by laser so that the AD epoxy resin glue falls off to the reinforcement area without damaging the reinforcement plate, and remove the entire surface of the peelable cover film so that the AD epoxy resin glue is disposed on the reinforcement area, wherein the position of cutting the AD epoxy resin glue is consistent with the position of cutting the peelable cover film;
[0011] A plurality of reinforcing plates are stacked to form a reinforcing layer, the reinforcing layer is cut at a controlled depth and at least two connecting bridges are retained on each reinforcing plate; the cut reinforcing layer is bonded to the flexible circuit board, quickly pressed and baked until the cut reinforcing layer and the flexible circuit board are completely cured, and the connecting bridges are broken so that only the reinforcing layer is retained on the flexible circuit board.
[0012] In addition, the above-mentioned method for laminating a reinforcement layer without connection points according to the present invention may also have the following additional technical features:
[0013] Furthermore, after the step of etching the FR-4 epoxy resin substrate to remove the copper on both sides of the FR-4 epoxy resin substrate to obtain a reinforcing plate with both sides being substrates, the step further includes:
[0014] The reinforcing plate is drilled to obtain positioning holes.
[0015] Further, in the step of cutting the plate-film combination structure by laser depth control to cut through the peelable cover film, and cutting the reinforcement plate to obtain the reinforcement area:
[0016] The depth of the reinforcement area shall not exceed half the thickness of the reinforcement plate;
[0017] The technical parameters of controlled depth cutting include: laser cutting speed is 700 mm / s -850 mm / s; laser frequency is 220KHz; cutting times is 7-9.
[0018] Furthermore, in the step of obtaining an AD epoxy resin pure glue having a size corresponding to the peelable cover film: the AD epoxy resin pure glue has a single-sided release paper, and the thickness of the AD epoxy resin pure glue is 25 μm.
[0019] Furthermore, in the step of cutting the AD epoxy resin pure glue with controlled depth by laser so that the AD epoxy resin pure glue falls off to the reinforcement area without damaging the reinforcement plate: the size of the cut AD epoxy resin pure glue is 0.05 mm smaller than the single side of the peelable cover film.
[0020] Furthermore, in the step of controlling the depth of the AD epoxy resin pure glue by laser so that the AD epoxy resin pure glue falls off to the reinforcement area without damaging the reinforcement plate, the technical parameters of the controlled depth cutting include:
[0021] The laser cutting speed is 750 mm / s -900 mm / s; the laser frequency is 250 KHz; the number of cutting times is 4-5.
[0022] Furthermore, in the step of controlling the depth of cutting the reinforcing layer and retaining at least two connecting bridges on each reinforcing plate: the width of the connecting bridge is 1 mm, and the thickness of the connecting bridge is 2 / 3 of the thickness of the reinforcing plate.
[0023] Furthermore, in the step of laminating, quickly pressing and baking the cut reinforcement layer and the flexible circuit board until the cut reinforcement layer and the flexible circuit board are completely cured: the baking temperature is 150° C. and the baking time is 2 hours.
[0024] Furthermore, after the step of stacking a plurality of reinforcing plates to form a reinforcing layer, the step further includes: using the positioning hole as a reference point, drilling the reinforcing layer to obtain a plurality of functional holes, wherein the functional holes include device mounting holes and mounting auxiliary holes.
[0025] Another aspect of the present invention provides a circuit board, which is prepared by the above-mentioned method for bonding a reinforcement layer without connection points.
[0026] Compared with the prior art, the present invention has the following beneficial effects:
[0027] The above-mentioned method for bonding the reinforcement layer without connection points and the circuit board achieve the purpose of local bonding of AD epoxy resin pure glue by utilizing the micro-stickiness and peelability of the peelable cover film through laser controlled depth cutting, so as to solve the auxiliary edge bonding phenomenon caused by AD epoxy resin pure glue on the entire surface; at the same time, the whole-surface bonding of the reinforcement board with AD epoxy resin pure glue also greatly improves the production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 A method for laminating a reinforcement layer without a connection point in an embodiment of the present invention;
[0029] Figure 2 This is a schematic diagram of the structure of the reinforcing layer after curing in an embodiment of the present invention;
[0030] Description of main structural parts:
[0031]
[0032] The following specific implementation manner will further illustrate the present invention in conjunction with the above-mentioned drawings. DETAILED DESCRIPTION
[0033] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. Several embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive.
[0034] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only.
[0035] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.
[0036] In order to solve the technical problems that the traditional bonding method has AD epoxy resin pure glue on the entire surface of the reinforcement layer, which makes the auxiliary edge easy to stick, and the inability to set the bonding in batches, resulting in low production efficiency, the present application provides a bonding method for the reinforcement layer without connection points and a circuit board. By utilizing the micro-stickiness and peelability of the peelable cover film and laser controlled depth cutting, the purpose of local bonding of AD epoxy resin pure glue is achieved to solve the auxiliary edge bonding problem caused by AD epoxy resin pure glue on the entire surface; at the same time, the whole surface of the reinforcement board bonded with AD epoxy resin pure glue also greatly improves the production efficiency.
[0037] In order to facilitate understanding of the present invention, several embodiments of the present invention are provided below. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thorough and comprehensive.
[0038] Embodiment 1
[0039] See also Figure 1 , which is a method for laminating a reinforcement layer without a connection point in the first embodiment of the present invention, comprising steps S101 to S105:
[0040] S101, obtaining a flexible circuit board and a FR-4 epoxy resin substrate of a size corresponding to the flexible circuit board, etching the FR-4 epoxy resin substrate to remove copper on both sides of the FR-4 epoxy resin substrate to obtain a reinforcement board with both sides being substrates.
[0041] In this embodiment, a flexible circuit board is first obtained, and then a FR-4 epoxy resin substrate of a size corresponding to the flexible circuit board is cut. It should be further explained that the thickness of the FR-4 epoxy resin substrate can be selected according to the actual use. The copper on both sides of the FR-4 epoxy resin substrate is completely removed by etching, and a reinforcement board with both sides as the base material is presented. Then, the reinforcement board is drilled by drilling to obtain the positioning hole 100.
[0042] S102, obtaining a peelable cover film of a size corresponding to the FR-4 epoxy resin substrate, and attaching the peelable cover film to the reinforcing plate to obtain a plate-film combination structure, wherein the peelable cover film is a low-viscosity single-sided adhesive PE film.
[0043] Prepare a peelable cover film 400 of a size corresponding to the FR-4 epoxy resin substrate, and stick the peelable cover film 400 on the reinforcing plate. During the preparation process, it is necessary to ensure that the peelable cover film 400 is flat and free of bubbles, and the positioning holes 100 drilled on the FR-4 epoxy resin substrate need to be exposed. As a specific example, the peelable cover film 400 is a low-viscosity single-sided adhesive PE film.
[0044] S103, with the side of the plate-film combination structure that is attached to the peelable cover film facing upward, cutting the plate-film combination structure by laser depth control to cut through the peelable cover film, cutting the reinforcing plate to obtain a reinforcing area, and removing the peelable cover film on the reinforcing area to expose the reinforcing plate.
[0045] In the actual cutting process, the side with the peelable cover film 400 facing upward is placed on the laser cutting machine, and the laser energy is controlled to cut through the peelable cover film 400. In this embodiment, the depth of the enhanced area obtained by cutting the reinforcing plate is 0.05mm-0.1mm. It should be further explained that in order to prevent the reinforcing plate from breaking, the maximum depth of the enhanced area cannot exceed half of the thickness of the reinforcing plate during the cutting process.
[0046] Specifically, when cutting the plate-film combination structure, the technical parameters for controlled depth cutting include: laser cutting speed of 700 mm / s -850 mm / s; laser frequency of 220 KHz; number of cuts of 7 to 9. As a specific example, the specific values of the cutting speed and number of cuts can be selected according to the actual situation during cutting.
[0047] It should be further explained that, in this embodiment, the pattern of the laser-cut peelable cover film 400 is consistent with the size and position of the reinforcing plate.
[0048] Since the peelable cover film 400 at the reinforcing plate position is cut, it needs to be removed. At this time, the reinforcing area on the reinforcing plate has no peelable cover film 400 and the reinforcing plate is exposed, while other auxiliary areas or waste edges are protected by the peelable cover film 400.
[0049] S104, obtaining an AD epoxy resin pure glue of a size corresponding to the peelable cover film, and attaching the entire surface of the AD epoxy resin pure glue to the cut peelable cover film, placing the peelable cover film with the AD epoxy resin pure glue on a laser cutting machine, and performing controlled depth cutting on the AD epoxy resin pure glue by laser so that the AD epoxy resin pure glue falls off to the reinforcement area without damaging the reinforcement plate, and removing the entire surface of the peelable cover film so that the AD epoxy resin pure glue is provided on the reinforcement area.
[0050] Prepare a sheet of AD epoxy resin pure glue 300, the size of which is consistent with the peelable cover film 400. As a specific example, the AD epoxy resin pure glue 300 has a single-sided release paper, and the thickness of the AD epoxy resin pure glue 300 is 25μm. Furthermore, the entire surface of the AD epoxy resin pure glue 300 on the non-release paper side is attached to the cut peelable cover film 400, and then the four corners of the AD epoxy resin pure glue 300 are fixed with an electric iron, and then pre-pressed on a fast press to ensure that the AD epoxy resin pure glue 300 and the reinforcement plate are reliably adhered. The pre-pressed AD epoxy resin pure glue 300 is placed on a laser cutting machine, and the AD epoxy resin pure glue 300 is deeply cut by laser. During this process, it is necessary to ensure that the AD epoxy resin pure glue 300 can fall off but cannot damage the reinforcement plate.
[0051] Furthermore, the size of the cut AD epoxy resin glue 300 is 0.05 mm smaller than the single side of the peelable cover film 400. In order to ensure the cutting accuracy of the AD epoxy resin glue 300, in this embodiment, the position of cutting the AD epoxy resin glue 300 is consistent with the position of cutting the peelable cover film 400.
[0052] Specifically, when cutting AD epoxy resin pure glue 300, the technical parameters for controlling the cutting depth include:
[0053] The laser cutting speed is 750 mm / s -900 mm / s; the laser frequency is 250 KHz; and the number of cuts is 4 to 5. As a specific example, the specific values of the cutting speed and the number of cuts can be selected according to the actual situation during cutting.
[0054] After the AD epoxy resin pure glue 300 is cut, at this time, except for the reinforced area exposed after the peelable cover film 400 is cut, the AD epoxy resin pure glue 300 in other auxiliary areas or waste edge areas is attached to the peelable cover film 400. At this time, the peelable cover film 400 is completely removed, so that only the reinforced area has the AD epoxy resin pure glue 300, and the other areas are all reinforced boards of the FR-4 epoxy resin substrate.
[0055] S105, stacking a plurality of reinforcing plates to form a reinforcing layer, cutting the reinforcing layer at a controlled depth and retaining at least two connecting bridges on each reinforcing plate; laminating, quickly pressing and baking the cut reinforcing layer and the flexible circuit board until the cut reinforcing layer and the flexible circuit board are completely cured, breaking the connecting bridges so that only the reinforcing layer remains on the flexible circuit board.
[0056] A plurality of reinforcing plates are stacked to form a reinforcing layer. The positioning hole 100 in the reinforcing plate is used as a reference point, and the reinforcing layer is drilled to obtain a plurality of functional holes, including device mounting holes and mounting auxiliary holes.
[0057] like Figure 2 As shown, in this embodiment, the positioning hole 100 in the reinforcing plate is used as the positioning base point to cut the reinforcing plate, and the cutting position and cutting size are consistent with the peelable cover film 400. When cutting, two 1.0 mm connecting bridges 200 are retained on each reinforcing plate; further, the retained 1.0 mm connecting bridge 200 is cut by laser depth control, and the cutting depth is 1 / 3 of the thickness of the reinforcing plate; that is, the width of the connecting bridge 200 is 1 mm, and the thickness of the connecting bridge 200 is 2 / 3 of the thickness of the reinforcing plate. However, it should be noted that at this time, only one side of the reinforcing plate has AD epoxy resin pure glue 300, and the other side is the reinforcing plate, and the side with AD epoxy resin pure glue 300 is selected for depth control cutting. It should be further explained that the laser parameters for depth control cutting of the connecting bridge 200 need to be adjusted for the first time according to the thickness of the reinforcing plate.
[0058] Furthermore, the cut reinforcement layer is bonded to the flexible circuit board. Specifically, the positioning hole 100 of the reinforcement plate is overlapped with the positioning hole 100 of the flexible substrate. Because the positioning holes 100 of the two are consistent, the position of the reinforcement layer and the flexible substrate to be bonded will completely overlap. Secondly, the reinforcement layer and the flexible substrate are fast pressed by fast pressing, and then baked to complete the curing. In this embodiment, the baking temperature is 150°C and the baking time is 2 hours.
[0059] Finally, the auxiliary edge of the reinforcement layer is removed to complete the production of the reinforcement layer. Specifically, the FR-4 reinforcement layer bridge position with controlled depth cutting is broken by utilizing the bending property of the flexible circuit board, and only the required reinforcement layer is retained on the flexible substrate.
[0060] In summary, the method for bonding the reinforcement layer without connection points in the above-mentioned embodiments of the present invention, by utilizing the micro-stickiness and removability of the peelable cover film, achieves the purpose of local bonding of AD epoxy resin pure glue through laser controlled depth cutting, so as to solve the auxiliary edge bonding phenomenon caused by AD epoxy resin pure glue on the entire surface; at the same time, the whole-surface bonding of the reinforcement board with AD epoxy resin pure glue also greatly improves the production efficiency.
[0061] Another aspect of the present invention provides a circuit board, which is prepared by the method for bonding a reinforcement layer without connection points in the above embodiment.
[0062] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.
[0063] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A method for laminating a reinforcement layer without a connection point, characterized in that: include: Obtain a flexible circuit board and a FR-4 epoxy resin substrate of a size corresponding to the flexible circuit board, and etch the FR-4 epoxy resin substrate to remove copper on both sides of the FR-4 epoxy resin substrate to obtain a reinforcement board with both sides being substrates; Obtain a peelable cover film of a size corresponding to the FR-4 epoxy resin substrate, and attach the peelable cover film to the reinforcing plate to obtain a plate-film combination structure, wherein the peelable cover film is a low-viscosity single-sided adhesive PE film; The side of the plate-film combination structure that is attached to the peelable cover film faces upwards, the plate-film combination structure is cut through the peelable cover film by laser depth control, and a reinforcement area is cut on the reinforcement board, and the peelable cover film on the reinforcement area is removed to expose the reinforcement board; wherein, during the cutting process, the maximum depth of the reinforcement area cannot exceed half of the thickness of the reinforcement board to prevent the reinforcement board from breaking; Obtain an AD epoxy resin glue having a size corresponding to that of the peelable cover film, and attach the entire surface of the AD epoxy resin glue to the cut peelable cover film, and place the peelable cover film attached with the AD epoxy resin glue on a laser cutting machine, and perform depth-controlled cutting of the AD epoxy resin glue by laser so that the AD epoxy resin glue falls off to the reinforcement area without damaging the reinforcement plate, and remove the entire surface of the peelable cover film so that the AD epoxy resin glue is disposed on the reinforcement area, wherein the position of cutting the AD epoxy resin glue is consistent with the position of cutting the peelable cover film; Stacking a plurality of reinforcing plates to form a reinforcing layer, cutting the reinforcing layer at a controlled depth and retaining at least two connecting bridges on each reinforcing plate; laminating the cut reinforcing layer with the flexible circuit board, rapidly pressing and baking until the cut reinforcing layer and the flexible circuit board are completely cured, breaking the connecting bridges so that only the reinforcing layer remains on the flexible circuit board; The step of obtaining an AD epoxy resin pure glue having a size corresponding to that of the peelable cover film and laminating the entire surface of the AD epoxy resin pure glue on the cut peelable cover film comprises: AD epoxy resin pure glue has a single-sided release paper. Stick the entire surface of the AD epoxy resin pure glue without the release paper on the cut peelable cover film. Then use an electric iron to fix the four corners of the AD epoxy resin pure glue, and pre-press it on a fast press to ensure that the AD epoxy resin pure glue and the reinforcement board are reliably adhered.
2. The method for laminating a reinforcement layer without connection points according to claim 1, characterized in that: After the step of etching the FR-4 epoxy resin substrate to remove the copper on both sides of the FR-4 epoxy resin substrate to obtain a reinforcement board with both sides being the base material, the step further includes: The reinforcing plate is drilled to obtain positioning holes.
3. The method for laminating a reinforcement layer without connection points according to claim 1, characterized in that: In the step of cutting the sheet-film combination structure by laser depth control to cut through the peelable cover film, and cutting the enhanced area on the reinforcing sheet: The depth of the reinforcement area shall not exceed half the thickness of the reinforcement plate; The technical parameters of controlled depth cutting include: Laser cutting speed is 700mm / s - 850mm / s; laser frequency is 220KHz; The number of cuts is 7-9.
4. The method for laminating a reinforcement layer without connection points according to claim 1, characterized in that: In the step of obtaining an AD epoxy resin pure glue having a size corresponding to the peelable cover film: AD epoxy resin pure glue has single-sided release paper, and the thickness of AD epoxy resin pure glue is 25μm.
5. The method for laminating a reinforcement layer without connection points according to claim 1, characterized in that: In the step of controlling the depth of the AD epoxy resin pure glue by laser so that the AD epoxy resin pure glue falls off to the reinforcement area without damaging the reinforcement plate: The single-side dimension of cutting the pure AD epoxy resin is 0.05mm smaller than the single-side dimension of the peelable cover film.
6. The method for laminating a reinforcement layer without connection points according to claim 1, characterized in that: In the step of controlling the depth of the AD epoxy resin pure glue by laser so that the AD epoxy resin pure glue falls off to the reinforcement area without damaging the reinforcement plate, the technical parameters of the controlled depth cutting include: The laser cutting speed is 750mm / s - 900mm / s; the laser frequency is 250KHz; the number of cutting times is 4-5.
7. The method for laminating a reinforcement layer without connection points according to claim 1, characterized in that: In the step of controlling the depth of cutting the reinforcing layer and retaining at least two connecting bridges on each reinforcing plate: The width of the connecting bridge is 1 mm, and the thickness of the connecting bridge is 2 / 3 of the thickness of the reinforcing plate.
8. The method for laminating a reinforcement layer without connection points according to claim 1, characterized in that: In the step of laminating, quickly pressing and baking the cut reinforcement layer and the flexible circuit board until the cut reinforcement layer and the flexible circuit board are completely cured: The baking temperature is 150°C and the baking time is 2h.
9. The method for laminating a reinforcement layer without connection points according to claim 2, characterized in that: The step of stacking a plurality of reinforcement boards to form a reinforcement layer then includes: The reinforcement layer is drilled with the positioning hole as a reference point to obtain a plurality of functional holes, wherein the functional holes include device mounting holes and mounting auxiliary holes.
10. A circuit board, characterized in that: It is prepared by the method for bonding a reinforcement layer without connection points as described in any one of claims 1 to 9.