A method for online quality detection of packaging plastic film blow molding production
Through online inspection methods, the multi-faceted quality of packaging plastic film is evaluated and optimized, which solves the problems of incomplete monitoring of production process parameters and incomplete quality assessment in the existing technology, and improves the stability and consistency of product quality.
Patent Information
- Application Number
- CN202411178604.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-08-27
AI Technical Summary
The existing packaging plastic film blow molding production process fails to fully monitor and optimize parameters such as temperature, pressure, and extrusion speed, resulting in product consistency and reliability issues, and the quality of plastic films such as thickness and transparency cannot be comprehensively evaluated. Affects the stability of product quality.
The quality of blow molding of packaging plastic film is online, including raw material detection, extrusion mass analysis, blown mass testing, cooling shaping mass testing, traction mass analysis and winding mass analysis, through infrared spectrometer, temperature sensor, laser thickness measuring instrument , transparency tester and force sensor equipment, monitor and evaluate various parameters in real time, calculate the production quality evaluation index for feedback.
It realizes multi-faceted quality inspection and optimization of packaging plastic film, improves product consistency and stability, timely adjusts airflow and process parameters, and improves product pass rate and quality stability.
Smart Images

Figure CN118700507B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of material science, in particular to an online detection method for production quality of packaging plastic film blow molding. Background Art
[0002] With the rapid development of modern industry, the packaging industry has an increasing demand for high-quality plastic films. Packaging plastic films play a vital role in protecting products, improving the appearance of goods, and facilitating transportation.
[0003] Packaging plastic film blow molding is an important plastic product production process. It is mainly used to produce various types of packaging plastic films. The plastic raw materials are heated and melted, and then blown into films of specific shapes and thicknesses using air pressure. This process has the advantages of relatively low cost, high production efficiency, and large-scale production. Packaging plastic films are widely used in packaging in many fields such as food, daily necessities, and industrial products. They can protect products, block external factors, and maintain product freshness. They occupy an important position in the modern packaging industry.
[0004] For example, the existing Chinese patent with application number CN202110135342.4 discloses a method for continuous blow molding of degradable plastic bags. This scheme uses a pressure sensor to monitor the air pressure in the cylindrical plastic film ejected from the blow molding die in real time. When a momentary pressure loss is detected in the cylindrical plastic film, it indicates that a hole has appeared. An annular air curtain device is used to blow an annular air curtain around it to keep it upright and prevent it from swinging. At the same time, a sealing device is used to separate the hole area from the cylindrical plastic film below, and a reinforcement pattern is ironed in the hole area to prevent tearing. The system can automatically monitor and process holes, reduce manual intervention, improve production efficiency, and help improve the quality and stability of the plastic film.
[0005] However, the above patent has the following problems: First, the solution improves the quality of plastic film by automatically monitoring and processing holes, but does not involve other factors in the plastic production process, such as temperature, pressure, extrusion speed and other parameters in the production process. It may not be possible to fully understand and optimize the plastic production process, resulting in problems in the production process and affecting the consistency and reliability of the product.
[0006] Second, this solution mainly focuses on monitoring holes in plastic films, but ignores other quality tests, such as thickness and transparency. It is unable to comprehensively evaluate the quality of plastic films, which may affect the accurate judgment of product quality and lead to unstable product quality. Summary of the invention
[0007] In order to overcome the shortcomings of the background technology, an embodiment of the present invention provides an online detection method for the production quality of packaging plastic film blow molding, which can effectively solve the problems involved in the above-mentioned background technology.
[0008] The purpose of the present invention can be achieved by the following technical scheme: A method for online detection of the production quality of packaging plastic film blow molding, the method comprising the following steps: S1. Raw material detection and analysis: the purity and moisture content of the plastic resin particles are detected, and the raw material quality evaluation coefficient of the packaging plastic film is obtained by analysis. .
[0009] S2. Extrusion quality analysis: Test the extrusion temperature fluctuation and extrusion pressure stability of the extruder, and analyze and obtain the extrusion process evaluation coefficient of the packaging plastic film. .
[0010] S3. Blowing quality inspection: The blowing quality parameters of the packaging plastic film are inspected, including the degree of compliance of the blowing ratio and the uniformity of the wall thickness.
[0011] S4. Blowing quality analysis: According to the blowing quality parameter analysis of the packaging plastic film, the blowing quality evaluation coefficient of the packaging plastic film is obtained. , and use this to control the airflow at each measuring point of the packaging plastic film.
[0012] S5. Cooling and shaping test: The cooling and shaping parameters of the packaging plastic film are tested. The cooling and shaping parameters include the transparency of each measuring point, the temperature of each abnormal measuring point at each testing time point, and the cooling time.
[0013] S6. Cooling and shaping analysis: According to the cooling and shaping parameters of the packaging plastic film, the cooling and shaping quality evaluation coefficient of the packaging plastic film is obtained. .
[0014] S7. Traction quality analysis: Detect the traction force of the packaging plastic film, and then analyze the fluctuation degree of the traction force of the packaging plastic film. .
[0015] S8. Rewinding quality analysis: Check the rewinding size data of the packaging plastic film and analyze the conformity of the rewinding size of the packaging plastic film. , where the dimension data includes diameter and length.
[0016] S9. Comprehensive evaluation of production quality: Based on the raw material quality evaluation coefficient, inflation quality evaluation coefficient, cooling and shaping quality evaluation coefficient, traction force fluctuation degree and winding size compliance degree of the packaging plastic film, the blow molding production quality evaluation index of the packaging plastic film is obtained and feedback is provided.
[0017] Preferably, the specific analysis method for the raw material detection and analysis is as follows: in the first step, a set amount of resin particles are selected and carefully ground into a uniform powder, which is recorded as a resin particle powder sample, and the resin particle powder sample is placed in a sample cell of an infrared spectrometer, the spectrometer is started, infrared light is irradiated to the resin particle powder sample, and the absorption degree of the resin particle powder sample to infrared light of different wavelengths is recorded to generate a spectrum, which is recorded as a resin particle spectrum. At the same time, a resin particle standard spectrum is read from a management database, the peak position of each characteristic peak in the resin particle standard spectrum is marked, and the resin particle spectrum is overlapped and compared with the resin particle standard spectrum, and the number of overlapping characteristic peaks in the resin particle spectrum and the resin particle standard spectrum is obtained by counting, which is recorded as , read the intensity of each overlapping characteristic peak in the resin particle spectrum and the resin particle standard spectrum respectively, and record it as , Indicates The number of overlapping characteristic peaks, , substituting it into the formula Get the purity of plastic resin particles , They represent the weight factors corresponding to the number of overlapping characteristic peaks and the intensity similarity of overlapping characteristic peaks, respectively. It represents the proportional constant of the similarity and purity of the set resin particle spectrum. Indicates the number of overlapping characteristic peaks, Indicates the total number of characteristic peaks in the preset resin particle standard spectrum.
[0018] In the second step, a set amount of resin particles is weighed and placed in a dry reaction container, and the standard colorimetric value of the reagent fully reacted is read from the management database, and the reagent is slowly injected into the reaction container, and the colorimetric value displayed by the injection instrument when the reagent reacts is recorded in real time. The reagent injection is stopped when the colorimetric value displayed by the instrument is the same as the standard colorimetric value of the reagent fully reacted. The total amount of reagent injected at this time is recorded as the resin particle reagent amount, and the quantitative relationship between the reagent amount and the moisture content of the resin particles is read from the management database. The moisture content of the resin particles is obtained by calculation and recorded as .
[0019] Step 3: Read the purity of plastic resin particles , moisture content , substituting it into the formula Get the raw material quality evaluation coefficient of packaging plastic film , They represent the weight factors of the purity and moisture content of the set resin particles respectively. Indicates the set standard moisture content.
[0020] Preferably, the specific analysis method of the extrusion quality analysis is: a temperature sensor is set at each part of the extruder, and a time point is selected according to a set time interval, and the temperature of each part of the extruder at each time point is measured, and recorded as the temperature of each part of the extruder at each time point , Indicates The number of the part, , Indicates The number of the time point, , and the temperature of each part of the extruder is obtained by taking the average value, which is recorded as , substituting it into the formula Get the extrusion temperature fluctuation of the extruder , represents the number of time points, Indicates the number of parts of the extruder. At the same time, the pressure sensor is used to detect the pressure of the extruder outlet at each time point, which is recorded as , the average pressure of the extruder is obtained by taking the average value, which is recorded as , substituting it into the formula Get the extrusion pressure stability of the extruder , substituting it into the formula Get the extrusion process evaluation coefficient of packaging plastic film , The weight factor that represents the set extrusion temperature fluctuation degree and extrusion pressure stability degree.
[0021] Preferably, the specific analysis method of the inflation quality detection is as follows: in the first step, a plurality of diameter measurement points with equal distances are taken on the bubble tube according to the set distance, the diameters of the diameter measurement points of the bubble tube are measured respectively, and the average value is calculated to obtain the diameter of the bubble tube, which is recorded as At the same time, the diameter of the extrusion die is obtained according to the measurement method of the bubble tube diameter, which is recorded as , through the formula Get the degree of compliance of the blowing ratio of the packaging plastic film ,in , Indicates the preset inflation ratio design value.
[0022] In the second step, several measuring points are selected on the packaging plastic film according to the set interval, and the thickness of each measuring point of the packaging plastic film is detected by a laser thickness gauge, which is recorded as , Indicates The number of the measuring point, , through the formula Get the uniformity of the wall thickness of the packaging plastic film , Indicates the number of measurement points.
[0023] Preferably, the specific analysis method of the inflation quality analysis is as follows: the first step is to read the inflation ratio compliance of the packaging plastic film. , wall thickness uniformity , substituting it into the formula Get the inflation quality evaluation coefficient of packaging plastic film , The weight factors respectively represent the set blowing ratio compliance degree and wall thickness uniformity degree, and the blowing quality evaluation coefficient of the packaging plastic film is compared with the preset blowing quality evaluation coefficient threshold. If the blowing quality evaluation coefficient of the packaging plastic film is greater than or equal to the preset blowing quality evaluation coefficient threshold, it means that the blowing quality evaluation coefficient of the packaging plastic film is qualified, otherwise it means that the blowing quality evaluation coefficient of the packaging plastic film is unqualified, and the second step is executed.
[0024] The second step is to monitor the airflow size at each measuring point of the packaging plastic film through the wind speed sensor, and read the thickness of each measuring point of the packaging plastic film at the same time. , and compare the two to get the proportional constant of the airflow size and thickness of the packaging plastic film , through the formula Get the adjusted airflow size at each measuring point of the packaging plastic film , Indicates the number of measuring points, which is used to control the airflow at each measuring point of the packaging plastic film.
[0025] Preferably, the specific analysis method of the cooling and setting detection is: the transparency of each measuring point of the packaging plastic film is monitored by a transparency tester, and recorded as , according to the set time interval, several time points are taken from the cooling process of the packaging plastic film, recorded as the detection time points, the temperature of each measurement point of the packaging plastic film at each detection time point is detected, and it is compared with the preset temperature, and the measurement points at which the packaging plastic film temperature is greater than the preset temperature at each detection time point are obtained, which are recorded as abnormal measurement points at each detection time point, and the temperature of each abnormal measurement point of the packaging plastic film at each detection time point is recorded as , Indicates The number of the detection time point, , Indicates The number of the abnormal measurement point, , and record the time taken for the packaging plastic film to cool down, which is recorded as the packaging plastic film cooling time .
[0026] Preferably, the specific analysis method of the cooling setting analysis is: reading the transparency of each measuring point of the packaging plastic film , the temperature of each abnormal measurement point at each detection time point , Cooling time , substituting it into the formula Get the cooling and shaping quality evaluation coefficient of the packaging plastic film , Respectively represent the weight factors of the set transparency, temperature, and cooling time. Indicates the reference value of the set cooling time. represents the number of measurement points, represents the number of detection time points, Indicates the number of abnormal measurement points.
[0027] Preferably, the specific analysis method of the traction quality analysis is: install a force sensor at the traction force application position of the packaging plastic film, measure the traction force at each time point in real time, and analyze the traction force of the packaging plastic film at each time point according to the method of analyzing the extrusion temperature fluctuation degree of the extruder, and obtain the traction force fluctuation degree of the packaging plastic film, which is recorded as .
[0028] Preferably, the specific analysis method of the winding quality analysis is: when the packaging plastic film drives the roller of the meter to rotate during the winding process, the number of rotations of the meter roller is counted, and the circumference of the roller is measured at the same time, and the winding length of the packaging plastic film is calculated and recorded as , and use a caliper to detect the diameter of the rolled packaging plastic film, recorded as , substituting it into the formula Get the degree of conformity of the reel size of the packaging plastic film , They represent the weight factors of the set winding length and diameter respectively. They respectively represent the design values of the preset winding length and diameter.
[0029] Preferably, the specific analysis method for the comprehensive evaluation of production quality is: respectively reading the raw material quality evaluation coefficient of the packaging plastic film , Extrusion process evaluation coefficient , Blowing quality evaluation coefficient , Cooling and shaping quality evaluation coefficient , traction force fluctuation degree , the degree of conformity of the reel size , substituting it into the formula Get the blow molding production quality evaluation index of packaging plastic film , They respectively represent the weight factors of the set raw material quality evaluation coefficient, extrusion process evaluation coefficient, inflation quality evaluation coefficient, cooling and shaping quality evaluation coefficient, traction force fluctuation degree, and winding size compliance degree. It represents a natural constant. The blow molding production quality evaluation index of the packaging plastic film is compared with the preset blow molding production quality production index threshold. If the blow molding production quality evaluation index of the packaging plastic film is greater than or equal to the preset blow molding production quality production index threshold, it means that the blow molding production quality of the packaging plastic film is qualified. Otherwise, it means that the blow molding production quality of the packaging plastic film is unqualified, and feedback is given.
[0030] Compared with the prior art, the embodiments of the present invention have at least the following advantages or beneficial effects: 1. The present invention obtains the inflation quality evaluation coefficient of the packaging plastic film based on the thickness and transparency of the packaging plastic film, and controls the airflow at each measuring point of the packaging plastic film. The airflow can be adjusted in time to improve the inflation quality, avoid further expansion of quality problems, and improve the product qualification rate.
[0031] 2. The present invention obtains the blow molding production quality evaluation index of the packaging plastic film according to the raw material quality evaluation coefficient, the blowing quality evaluation coefficient, the cooling and setting quality evaluation coefficient, the traction force fluctuation degree, and the winding size compliance degree of the packaging plastic film, and provides feedback, which is helpful to optimize a certain link in a targeted manner, promote the continuous improvement and optimization of the production process, and enhance the stability and consistency of product quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] The present invention is further described using the accompanying drawings, but the embodiments in the accompanying drawings do not constitute any limitation to the present invention. A person skilled in the art can obtain other drawings based on the following drawings without creative work.
[0033] Figure 1 It is a schematic diagram of the method flow of the present invention.
[0034] Figure 2 for Figure 1 Conditional flow chart of step S4 in FIG.
[0035] Figure 3 The present invention provides a processing technology process. DETAILED DESCRIPTION
[0036] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0037] See also Figure 1As shown, the present invention provides an online detection method for the production quality of packaging plastic film blow molding, the method comprising the following steps: S1. Raw material detection and analysis: the purity and moisture content of plastic resin particles are detected, and the raw material quality evaluation coefficient of the packaging plastic film is obtained by analysis. .
[0038] The specific analysis method of the raw material detection and analysis is as follows: the first step is to select a set amount of resin particles and grind them carefully into a uniform powder, which is recorded as a resin particle powder sample, and the resin particle powder sample is placed in a sample cell of an infrared spectrometer, the spectrometer is started, infrared light is irradiated to the resin particle powder sample, and the absorption degree of the resin particle powder sample to infrared light of different wavelengths is recorded to generate a spectrum, which is recorded as a resin particle spectrum. At the same time, a resin particle standard spectrum is read from a management database, the peak position of each characteristic peak in the resin particle standard spectrum is marked, and the resin particle spectrum is overlapped and compared with the resin particle standard spectrum, and the number of overlapping characteristic peaks in the resin particle spectrum and the resin particle standard spectrum is obtained by counting, which is recorded as , read the intensity of each overlapping characteristic peak in the resin particle spectrum and the resin particle standard spectrum respectively, and record it as , Indicates The number of overlapping characteristic peaks, , substituting it into the formula Get the purity of plastic resin particles , They represent the weight factors corresponding to the number of overlapping characteristic peaks and the intensity similarity of overlapping characteristic peaks, respectively. It represents the proportional constant of the similarity and purity of the set resin particle spectrum. Indicates the number of overlapping characteristic peaks, It indicates the total number of characteristic peaks in the preset standard spectrum of resin particles. By comparing with the standard spectrum, it can quickly determine whether the resin particles meet the standard requirements, accurately detect and analyze the composition and purity of the resin particles, and ensure the stability and reliability of product quality.
[0039] It should be noted that the peak position refers to the position of the characteristic peak appearing in the spectrum, and the number of overlapping characteristic peaks refers to the number of characteristic peaks at the same position in the resin particle spectrum and the resin particle standard spectrum.
[0040] It should be noted that It can be set to 0.5. It can be set to 0.5. The number of overlapping characteristic peaks can reflect the number of similar peaks in the spectrum. A larger number of overlapping characteristic peaks may mean that there are more similarities between the two spectra. However, relying solely on the number of overlapping characteristic peaks may not be able to fully and accurately describe the degree of similarity, because the intensity of the peak may also affect the similarity. The intensity similarity of overlapping characteristic peaks pays more attention to the intensity change of the peaks. If the intensity similarity of the overlapping characteristic peaks in the two spectra is high, it means that the intensity distribution of the peaks is similar, which further increases the similarity of the spectra. Therefore, the weights corresponding to the number of overlapping characteristic peaks and the similarity of overlapping characteristic peak intensity are equal.
[0041] In the second step, a set amount of resin particles is weighed and placed in a dry reaction container, and the standard colorimetric value of the reagent fully reacted is read from the management database, and the reagent is slowly injected into the reaction container, and the colorimetric value displayed by the injection instrument when the reagent reacts is recorded in real time. The reagent injection is stopped when the colorimetric value displayed by the instrument is the same as the standard colorimetric value of the reagent fully reacted. The total amount of reagent injected at this time is recorded as the resin particle reagent amount, and the quantitative relationship between the reagent amount and the moisture content of the resin particles is read from the management database. The moisture content of the resin particles is obtained by calculation and recorded as It can accurately measure the moisture content in resin particles, provide key data for product quality control, ensure the stability of resin particle quality, and timely discover abnormal moisture content by precisely controlling the reagent volume and comparing colorimetric values, thereby improving the accuracy and reliability of detection. It can also use standard colorimetric values and the quantitative relationship in the database for calculation, reduce errors, and clarify whether the moisture index of the resin particles meets the requirements.
[0042] It should be noted that the specific analysis method for calculating the moisture content of the resin particles is: the calculation formula for the moisture content of the resin particles is: ,in Indicates the amount of resin particle reagent, Indicates the set reagent concentration. represents the molar mass of water, Indicates the set amount of resin pellets.
[0043] Step 3: Read the purity of plastic resin particles , moisture content , substituting it into the formula Get the raw material quality evaluation coefficient of packaging plastic film , They represent the weight factors of the purity and moisture content of the set resin particles respectively. Indicates the set standard moisture content; can accurately understand the influence of the purity and moisture content of plastic resin particles on the quality of raw materials, facilitate comparison and analysis of different batches of raw materials, timely discover quality differences and take corresponding measures, and provide strong guarantee for the stability and improvement of product quality.
[0044] It should be noted that, in a specific embodiment, It can be set to 0.6. It can be set to 0.4. Purity has an important influence on the performance and quality of the final packaging plastic film. High purity usually means more stable and reliable product performance. The importance of moisture content is relatively smaller, but it cannot be ignored. Because too high moisture content may affect some processing processes and certain characteristics of the product, the weight corresponding to the purity of the resin particles is slightly higher.
[0045] S2. Extrusion quality analysis: Test the extrusion temperature fluctuation and extrusion pressure stability of the extruder, and analyze and obtain the extrusion process evaluation coefficient of the packaging plastic film. .
[0046] The specific analysis method of the extrusion quality analysis is: set a temperature sensor at each part of the extruder, select a time point according to the set time interval, measure the temperature of each part of the extruder at each time point, and record it as the temperature of each part of the extruder at each time point , Indicates The number of the part, , Indicates The number of the time point, , and the temperature of each part of the extruder is obtained by taking the average value, which is recorded as , substituting it into the formula Get the extrusion temperature fluctuation of the extruder , represents the number of time points, Indicates the number of parts of the extruder. At the same time, the pressure sensor is used to detect the pressure of the extruder outlet at each time point, which is recorded as , the average pressure of the extruder is obtained by taking the average value, which is recorded as , substituting it into the formula Get the extrusion pressure stability of the extruder , substituting it into the formula Get the extrusion process evaluation coefficient of packaging plastic film , The weight factor represents the set extrusion temperature fluctuation degree and extrusion pressure stability degree. Accurately grasping the temperature changes of various parts of the extruder at different times is conducive to timely detection of temperature anomalies and ensuring the stability and consistency of the production process. At the same time, real-time monitoring of the extruder nozzle pressure can ensure the smoothness and safety of the extrusion process, help optimize process parameters, and maintain a good production state.
[0047] It should be noted that, in a specific embodiment, It can be set to 0.6. It can be set to 0.4. The extrusion temperature has a critical impact on the molding quality and performance (such as mechanical properties, transparency, etc.) of the plastic film. Large temperature fluctuations may cause product defects, uneven thickness and other problems. Stable extrusion pressure helps to ensure uniform extrusion and good shape of the plastic film, but compared with temperature, its impact may not be so direct and significant. Therefore, the weight corresponding to the degree of extrusion temperature fluctuation is slightly higher.
[0048] S3. Blowing quality inspection: The blowing quality parameters of the packaging plastic film are inspected, including the degree of compliance of the blowing ratio and the uniformity of the wall thickness.
[0049] The specific analysis method of the inflation quality detection is as follows: the first step is to take a number of diameter measurement points at equal distances on the bubble tube according to the set distance, measure the diameters of the diameter measurement points of the bubble tube respectively, and obtain the average value of the diameters to obtain the bubble tube diameter, which is recorded as At the same time, the diameter of the extrusion die is obtained according to the measurement method of the bubble tube diameter, which is recorded as , through the formula Get the degree of compliance of the blowing ratio of the packaging plastic film ,in , It indicates the preset design value of the blowing ratio. It can accurately understand the dimensions of each part of the bubble tube, ensure the consistency and uniformity of the product dimensions, and clarify the degree of compliance with the blowing ratio, which is helpful to judge whether the production process meets the design requirements, find problems in time and adjust the process, which is conducive to ensuring the final quality of the packaging plastic film, so that it has good physical properties and dimensional accuracy.
[0050] In the second step, several measuring points are selected on the packaging plastic film according to the set interval, and the thickness of each measuring point of the packaging plastic film is detected by a laser thickness gauge, which is recorded as , Indicates The number of the measuring point, , through the formula Get the uniformity of the wall thickness of the packaging plastic film , Indicates the number of measuring points; can accurately determine the thickness of each measuring point, fully grasp the thickness distribution of the packaging plastic film, help to promptly discover areas with uneven thickness, so that measures can be taken to make adjustments and improvements, ensuring the consistency and stability of the overall quality of the packaging plastic film.
[0051] S4. Blowing quality analysis: According to the blowing quality parameter analysis of the packaging plastic film, the blowing quality evaluation coefficient of the packaging plastic film is obtained. , and use this to control the airflow at each measuring point of the packaging plastic film.
[0052] See also Figure 2 As shown, the specific analysis method of the inflation quality analysis is as follows: the first step is to read the inflation ratio compliance of the packaging plastic film. , wall thickness uniformity , substituting it into the formula Get the inflation quality evaluation coefficient of packaging plastic film , The weight factors respectively represent the set blowing ratio compliance degree and wall thickness uniformity degree, and the blowing quality evaluation coefficient of the packaging plastic film is compared with the preset blowing quality evaluation coefficient threshold value. If the blowing quality evaluation coefficient of the packaging plastic film is greater than or equal to the preset blowing quality evaluation coefficient threshold value, it means that the blowing quality evaluation coefficient of the packaging plastic film is qualified, otherwise it means that the blowing quality evaluation coefficient of the packaging plastic film is unqualified, and the second step is executed; the two important factors of the blowing ratio compliance degree and the wall thickness uniformity degree are comprehensively considered to make the evaluation more comprehensive and accurate. The clear qualified judgment standard is helpful to quickly judge the quality status of the packaging plastic film, so as to timely discover quality problems and take targeted measures to improve them, thereby improving the stability of product quality.
[0053] It should be noted that, in a specific embodiment, It can be set to 0.5. It can be set to 0.5. The blowing ratio has a direct and critical impact on the final size and mechanical properties of the plastic film. If the blowing ratio does not meet the requirements, it may cause the key dimensions of the plastic film, such as thickness and width, to fail to meet the standards, thereby affecting its adaptability and use effect in packaging applications. A suitable blowing ratio is an important factor in ensuring the basic performance and specifications of the plastic film. The uniformity of the wall thickness is directly related to the quality consistency and appearance of the plastic film. Uneven wall thickness may cause local weakness or excessive thickness during use, affecting its strength, barrier properties and other properties. It will also affect the appearance of the product. In some application scenarios with high quality requirements, the importance of wall thickness uniformity will be more prominent. Therefore, the weights corresponding to the degree of compliance with the blowing ratio and the uniformity of the wall thickness are equal.
[0054] The second step is to monitor the airflow size at each measuring point of the packaging plastic film through the wind speed sensor, and read the thickness of each measuring point of the packaging plastic film at the same time. , and compare the two to get the proportional constant of the airflow size and thickness of the packaging plastic film , through the formula Get the adjusted airflow size at each measuring point of the packaging plastic film , Indicates the number of measuring points, so as to control the size of the airflow at each measuring point of the packaging plastic film; can accurately monitor and control the size of the airflow at each measuring point, ensure the stability of the airflow conditions during the production process, adjust the airflow size according to the thickness, help to achieve more accurate production process control, ensure product quality, and help improve the consistency and qualified rate of packaging plastic film production.
[0055] It should be noted that the specific analysis method of the proportional constant of the airflow size and thickness of the packaging plastic film is: the size of the airflow at each measuring point of the packaging plastic film is recorded as , and read the thickness of each measuring point of the packaging plastic film at the same time , substituting it into the formula Get the proportional constant of the airflow size and thickness of the packaging plastic film , Indicates the number of measurement points.
[0056] S5. Cooling and shaping test: The cooling and shaping parameters of the packaging plastic film are tested. The cooling and shaping parameters include the transparency of each measuring point, the temperature of each abnormal measuring point at each testing time point, and the cooling time.
[0057] The specific analysis method of the cooling and setting test is: the transparency of each measuring point of the packaging plastic film is monitored by a transparency tester, and is recorded as , according to the set time interval, several time points are taken from the cooling process of the packaging plastic film, recorded as the detection time points, the temperature of each measurement point of the packaging plastic film at each detection time point is detected, and it is compared with the preset temperature, and the measurement points at which the packaging plastic film temperature is greater than the preset temperature at each detection time point are obtained, which are recorded as abnormal measurement points at each detection time point, and the temperature of each abnormal measurement point of the packaging plastic film at each detection time point is recorded as , Indicates The number of the detection time point, , Indicates The number of the abnormal measurement point, , and record the time taken for the packaging plastic film to cool down, which is recorded as the packaging plastic film cooling time Monitoring of transparency helps ensure that the product appearance quality meets the requirements, identify abnormal measurement points and their temperatures, facilitate targeted adjustments to the cooling process, improve the cooling effect and product quality stability, and facilitate better control of the entire production process, improving the overall quality and performance of the product.
[0058] It should be noted that the specific analysis method of the preset temperature is: reading the temperature of each measuring point of the packaging plastic film at each detection time point, recorded as , the average temperature of the packaging plastic film at each detection time point is obtained by taking the average value, which is recorded as At the same time, the temperatures of each measuring point of the packaging plastic film at each detection time point are grouped according to the detection time point, and the temperatures of each measuring point are sorted in order from large to small and the median value is screened out to obtain the median value of the temperature of the packaging plastic film at each detection time point, which is recorded as , substituting it into the formula Get the preset temperature , Indicates the number of detection time points.
[0059] S6. Cooling and shaping analysis: According to the cooling and shaping parameters of the packaging plastic film, the cooling and shaping quality evaluation coefficient of the packaging plastic film is obtained. .
[0060] The specific analysis method of the cooling setting analysis is: reading the transparency of each measuring point of the packaging plastic film , the temperature of each abnormal measurement point at each detection time point , Cooling time , substituting it into the formula Get the cooling and shaping quality evaluation coefficient of the packaging plastic film , Respectively represent the weight factors of the set transparency, temperature, and cooling time. Indicates the reference value of the set cooling time. represents the number of measurement points, represents the number of detection time points, Indicates the number of abnormal measurement points; by comprehensively considering key factors such as transparency, temperature and cooling time, it can comprehensively and objectively evaluate the cooling and shaping quality, which helps to promptly discover problems in the cooling and shaping process so that targeted measures can be taken to improve and optimize, thereby improving the overall quality level of the product.
[0061] It should be noted that, in a specific embodiment, It can be set to 0.4. It can be set to 0.4. It can be set to 0.2. Transparency directly affects the appearance and visibility of the packaging plastic film, which is crucial to the product display effect. If the transparency is not good, it may reduce the attractiveness and market competitiveness of the product, and affect the observation of the items in the package. Good transparency can improve the overall quality of the package, so it occupies an important position in quality evaluation. The control of cooling temperature has a profound impact on the performance and quality of the plastic film. Inappropriate temperature may cause stress concentration, deformation, abnormal crystallinity and other problems in the plastic film, thereby affecting its mechanical properties, barrier properties and other key indicators. Accurate temperature control is one of the key factors to ensure good cooling and shaping effects. Appropriate cooling time can ensure that the plastic film is fully shaped and avoid undesirable phenomena such as rebound. If the cooling time is insufficient, the plastic film may have problems such as dimensional instability in subsequent use. However, compared with transparency and temperature, its impact may not be so direct and critical, so the weights corresponding to transparency and temperature are higher.
[0062] S7. Traction quality analysis: Detect the traction force of the packaging plastic film, and then analyze the fluctuation degree of the traction force of the packaging plastic film. .
[0063] The specific analysis method of the traction quality analysis is: install a force sensor at the traction force application position of the packaging plastic film, measure the traction force at each time point in real time, and analyze the traction force of the packaging plastic film at each time point according to the method of analyzing the extrusion temperature fluctuation degree of the extruder, and obtain the traction force fluctuation degree of the packaging plastic film, which is recorded as ; Clarifying the degree of traction force fluctuation helps to determine the stability of the production process and promptly detect abnormal traction force fluctuations.
[0064] S8. Rewinding quality analysis: Check the rewinding size data of the packaging plastic film and analyze the conformity of the rewinding size of the packaging plastic film. , where the dimension data includes diameter and length.
[0065] The specific analysis method of the winding quality analysis is: when the packaging plastic film drives the roller of the meter counter to rotate during the winding process, the number of rotations of the meter counter roller is counted, and the circumference of the roller is measured at the same time, and the winding length of the packaging plastic film is calculated and recorded as , and use a caliper to detect the diameter of the rolled packaging plastic film, recorded as , substituting it into the formula Get the degree of conformity of the reel size of the packaging plastic film , They represent the weight factors of the set winding length and diameter respectively. They respectively represent the preset design values of the winding length and diameter; the winding length is calculated by counting the number of roller rotations and measuring the circumference. The data acquisition is relatively accurate and direct, and can effectively reflect the actual winding situation. The final winding size compliance degree can intuitively reflect the winding quality, which is convenient for quality control and comparison. At the same time, it is helpful to promptly discover problems with the winding size, so as to adjust the winding process or equipment parameters in a targeted manner and improve the stability of the winding quality.
[0066] It should be noted that, in a specific embodiment, It can be set to 0.5. It can be set to 0.5. The winding length is directly related to the effective utilization and applicability of the plastic film in subsequent use. If the winding length does not meet the requirements, it may lead to insufficient length or waste in actual application, affecting production efficiency and cost. In addition, accurate winding length is also very important to ensure the continuity and consistency of the product. The appropriate winding diameter helps to ensure the stability and neatness of the winding, which is of certain significance in storage, transportation and use. If the diameter does not meet the standard, the winding may be loose and easy to loosen, or in some cases affect the normal operation of the equipment, so the corresponding weights are equal.
[0067] S9. Comprehensive evaluation of production quality: Based on the raw material quality evaluation coefficient, inflation quality evaluation coefficient, cooling and shaping quality evaluation coefficient, traction force fluctuation degree and winding size compliance degree of the packaging plastic film, the blow molding production quality evaluation index of the packaging plastic film is obtained and feedback is provided.
[0068] The specific analysis method of the comprehensive evaluation of production quality is: respectively reading the raw material quality evaluation coefficient of the packaging plastic film , Extrusion process evaluation coefficient , Blowing quality evaluation coefficient , Cooling and shaping quality evaluation coefficient , traction force fluctuation degree , the degree of conformity of the reel size , substituting it into the formula Get the blow molding production quality evaluation index of packaging plastic film , They respectively represent the weight factors of the set raw material quality evaluation coefficient, extrusion process evaluation coefficient, inflation quality evaluation coefficient, cooling and shaping quality evaluation coefficient, traction force fluctuation degree, and winding size compliance degree. It represents a natural constant, and compares the blow molding production quality evaluation index of the packaging plastic film with the preset blow molding production quality production index threshold. If the blow molding production quality evaluation index of the packaging plastic film is greater than or equal to the preset blow molding production quality production index threshold, it means that the blow molding production quality of the packaging plastic film is qualified, otherwise it means that the blow molding production quality of the packaging plastic film is unqualified, and feedback is given to it; by comparing with the preset threshold, it can quickly and accurately determine whether the product quality is qualified, improve the efficiency and accuracy of quality judgment, and timely feedback helps production personnel to quickly understand the quality situation, take corresponding measures to improve the production process, improve product quality, facilitate better quality control, and ensure the consistency and stability of product quality.
[0069] It should be noted that, in a specific embodiment, It can be set to 0.2. It can be set to 0.2. It can be set to 0.2. It can be set to 0.2. Can be set to 0.1, It can be set to 0.1. High-quality raw materials are the basis for producing high-quality plastic film. If there are problems with the raw materials, no matter how hard the subsequent links try, it is difficult to completely make up for it. The extrusion process directly affects the key indicators of the plastic film such as thickness uniformity and melt quality, and has a great impact on the quality of the final product. The inflation quality evaluation coefficient is related to the stretching uniformity and bubble stability of the plastic film, and has a direct effect on the performance of the plastic film. The cooling and shaping quality evaluation coefficient is of great significance to the final shape and performance stability of the plastic film. Although the degree of traction fluctuation will affect the flatness of the plastic film, it may be slightly less important than the previous factors. The degree of compliance with the winding size mainly affects the subsequent convenience of use, but it may not be as prominent as the previous factors in terms of the impact on the performance of the plastic film itself. Therefore, the raw material quality evaluation coefficient, extrusion process evaluation coefficient, inflation quality evaluation coefficient, and cooling and shaping quality evaluation coefficient have higher corresponding weights.
[0070] See also Figure 3 As shown, the processing process of the present invention includes: raw material preparation, extrusion molding, blow molding, cooling and shaping, traction and stretching, slitting and winding, quality inspection, and packaging and warehousing.
[0071] The present invention obtains a blowing quality evaluation coefficient of a packaging plastic film according to the blowing quality parameter analysis, and controls the size of the airflow at each measuring point of the packaging plastic film based on this, and then comprehensively analyzes the raw material quality evaluation coefficient of the packaging plastic film, the cooling and shaping quality evaluation coefficient, the degree of traction force fluctuation, and the degree of compliance with the winding size to obtain the blow molding production quality evaluation index of the packaging plastic film, and provides feedback, which is helpful to optimize a certain link in a targeted manner, promote continuous improvement and optimization of the production process, and enhance the stability and consistency of product quality.
[0072] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations on the present invention. A person skilled in the art may make changes, modifications, substitutions and variations to the above embodiments within the scope of the present invention and they are still covered by the protection scope of the present invention.
Claims
1. A packaging plastic film blow molding production quality online detection method, characterized in that, The steps include: S1. Raw material testing and analysis: Test the purity and moisture content of plastic resin particles and analyze to obtain the raw material quality evaluation coefficient of packaging plastic film ; S2. Extrusion quality analysis: The extrusion temperature fluctuation and extrusion pressure stability of the extruder are tested to obtain the extrusion process evaluation coefficient of the packaging plastic film. ; S3. Blowing quality testing: Testing the blowing quality parameters of the packaging plastic film, including the degree of compliance with the blowing ratio and the uniformity of the wall thickness; S4. Blowing quality analysis: According to the blowing quality parameters of the packaging plastic film, the blowing quality evaluation coefficient of the packaging plastic film is obtained. , and use this to control the airflow at each measuring point of the packaging plastic film; S5. Cooling and setting test: The cooling and setting parameters of the packaging plastic film are tested, including the transparency of each measuring point, the temperature of each abnormal measuring point at each detection time point, and the cooling time. S6. Cooling and shaping analysis: According to the cooling and shaping parameters of the packaging plastic film, the cooling and shaping quality evaluation coefficient of the packaging plastic film is obtained. ; S7. Traction quality analysis: Detect the traction of the packaging plastic film and analyze the fluctuation of the traction of the packaging plastic film. ; S8. Rewinding quality analysis: Check the rewinding size data of the packaging plastic film and analyze the degree of compliance of the rewinding size of the packaging plastic film. , where the size data includes diameter and length; S9. Comprehensive Production Quality Evaluation: Calculate the blow molding production quality evaluation index for the packaging plastic film based on the raw material quality evaluation coefficient, inflation quality evaluation coefficient, cooling and setting quality evaluation coefficient, traction force fluctuation, and winding size compliance, and provide feedback. The specific analysis method for the raw material detection and analysis is: In the first step, a set amount of resin particles are selected and carefully ground into a uniform powder, which is recorded as a resin particle powder sample. The resin particle powder sample is placed in a sample cell of an infrared spectrometer, the spectrometer is started, infrared light is irradiated on the resin particle powder sample, and the absorption degree of the resin particle powder sample to infrared light of different wavelengths is recorded to generate a spectrum, which is recorded as a resin particle spectrum. At the same time, a resin particle standard spectrum is read from a management database, the peak position of each characteristic peak in the resin particle standard spectrum is marked, and the resin particle spectrum is overlapped and compared with the resin particle standard spectrum, and the number of overlapping characteristic peaks in the resin particle spectrum and the resin particle standard spectrum is obtained by counting, which is recorded as , respectively read the intensity of each overlapping characteristic peak in the resin particle spectrum and the resin particle standard spectrum, and record it as , Indicates the The number of overlapping characteristic peaks, , substitute it into the formula Obtain the purity of plastic resin particles , They represent the weight factors corresponding to the set number of overlapping characteristic peaks and the similarity of the overlapping characteristic peak intensities, The proportional constant that represents the similarity between the set resin particle spectrum and the purity. Indicates the number of overlapping characteristic peaks, Indicates the total number of characteristic peaks in the preset resin particle standard spectrum; In the second step, a set amount of resin particles is weighed and placed in a dry reaction container, and the standard colorimetric value of the reagent fully reacted is read from the management database. The reagent is slowly injected into the reaction container, and the colorimetric value displayed by the injection instrument when the reagent reacts is recorded in real time. The injection of the reagent is stopped when the colorimetric value displayed by the instrument is the same as the standard colorimetric value of the reagent fully reacted. The total amount of reagent injected at this time is recorded as the resin particle reagent amount. The quantitative relationship between the reagent amount and the moisture content of the resin particles is read from the management database. The moisture content of the resin particles is obtained by calculation and recorded as ; The third step is to read the purity of plastic resin particles , moisture content , substitute it into the formula Get the raw material quality evaluation coefficient of packaging plastic film , Respectively represent the weight factors of the purity and moisture content of the set resin particles, Indicates the set standard moisture content; The specific analysis method of the extrusion quality analysis is: Temperature sensors are set at various parts of the extruder, and time points are selected according to the set time intervals to measure the temperature of each part of the extruder at each time point, which is recorded as the temperature of each part of the extruder at each time point. , Indicates the The number of the part, , Indicates the The number of the time point, , and the temperature of each part of the extruder is obtained by taking the average value, which is recorded as , substitute it into the formula Get the extrusion temperature fluctuation degree of the extruder , represents the number of time points, Indicates the number of parts of the extruder. At the same time, the pressure sensor is used to detect the pressure of the extruder outlet at each time point, which is recorded as , the average pressure of the extruder is obtained by taking the average value, which is recorded as , substitute it into the formula Get the extrusion pressure stability of the extruder , substitute it into the formula Get the extrusion process evaluation coefficient of packaging plastic film , The weight factor that represents the set extrusion temperature fluctuation degree and extrusion pressure stability degree; The specific analysis method of the inflation quality detection is: In the first step, several diameter measurement points with equal distances are taken on the bubble tube according to the set distance, and the diameter of each diameter measurement point of the bubble tube is measured respectively. The average value is obtained to obtain the diameter of the bubble tube, which is recorded as At the same time, the diameter of the extrusion die is obtained according to the measurement method of the bubble tube diameter, which is recorded as , through the formula Obtain the degree of compliance of the blowing ratio of the packaging plastic film ,in , Indicates the preset inflation ratio design value; In the second step, several measuring points are selected on the packaging plastic film according to the set interval, and the thickness of each measuring point of the packaging plastic film is measured by a laser thickness gauge, which is recorded as , Indicates the The number of the measuring point, , through the formula Get the uniformity of the wall thickness of the packaging plastic film , Indicates the number of measurement points; The specific analysis method of the inflation quality analysis is: The first step is to read the degree of compliance of the blowing ratio of the packaging plastic film , wall thickness uniformity , substitute it into the formula Get the inflation quality evaluation coefficient of packaging plastic film , The weight factors respectively represent the set blowing ratio compliance degree and wall thickness uniformity degree, and the blowing quality evaluation coefficient of the packaging plastic film is compared with the preset blowing quality evaluation coefficient threshold. If the blowing quality evaluation coefficient of the packaging plastic film is greater than or equal to the preset blowing quality evaluation coefficient threshold, it means that the blowing quality evaluation coefficient of the packaging plastic film is qualified; otherwise, it means that the blowing quality evaluation coefficient of the packaging plastic film is unqualified, and the second step is executed; The second step is to monitor the airflow at each measuring point of the packaging plastic film through the wind speed sensor, and read the thickness of each measuring point of the packaging plastic film at the same time. Comparing the two, we can get the proportional constant of the airflow size and thickness of the packaging plastic film. , through the formula Get the adjusted airflow size at each measuring point of the packaging plastic film , Indicates the number of measuring points, so as to control the airflow at each measuring point of the packaging plastic film; The specific analysis method of the cooling setting test is: The transparency of each measuring point of the packaging plastic film is monitored by a transparency tester and recorded as , according to the set time interval, several time points are taken from the cooling process of the packaging plastic film, which are recorded as detection time points. The temperature of each measurement point of the packaging plastic film at each detection time point is detected and compared with the preset temperature. The measurement points at which the packaging plastic film temperature is greater than the preset temperature at each detection time point are recorded as abnormal measurement points at each detection time point. The temperature of each abnormal measurement point of the packaging plastic film at each detection time point is recorded as , Indicates the The number of the detection time point, , Indicates the The number of the abnormal measurement point, At the same time, the time it takes for the packaging plastic film to cool down is recorded as the cooling time of the packaging plastic film. ; The specific analysis method of the cooling setting analysis is: Read the transparency of each measuring point of the packaging plastic film , the temperature of each abnormal measurement point at each detection time point , Cooling time , substitute it into the formula Get the cooling and shaping quality evaluation coefficient of the packaging plastic film , Respectively represent the weight factors of the set transparency, temperature, and cooling time, Indicates the set cooling time reference value, represents the number of measurement points, represents the number of detection time points, Indicates the number of abnormal measurement points; The specific analysis method of the traction quality analysis is: A force sensor is installed at the traction force application part of the packaging plastic film to measure the traction force at each time point in real time. The traction force of the packaging plastic film at each time point is analyzed according to the method of analyzing the extrusion temperature fluctuation degree of the extruder, and the fluctuation degree of the traction force of the packaging plastic film is obtained, which is recorded as ; The specific analysis method of the winding quality analysis is: When the packaging plastic film drives the meter roller to rotate during the winding process, the number of revolutions of the meter roller is counted, and the circumference of the roller is measured at the same time to calculate the winding length of the packaging plastic film, which is recorded as , and use a caliper to detect the diameter of the rolled packaging plastic film, which is recorded as , substitute it into the formula Get the degree of compliance of the reel size of the packaging plastic film , Respectively represent the weight factors of the set winding length and diameter, Respectively represent the design values of the preset winding length and diameter; The specific analysis method for the comprehensive evaluation of production quality is: Read the raw material quality evaluation coefficient of the packaging plastic film respectively , Extrusion process evaluation coefficient , inflation quality evaluation coefficient , Cooling setting quality evaluation coefficient , traction force fluctuation degree , the degree of compliance of the winding size , substitute it into the formula Get the blow molding production quality evaluation index of packaging plastic film , They represent the weight factors of the set raw material quality evaluation coefficient, extrusion process evaluation coefficient, inflation quality evaluation coefficient, cooling and shaping quality evaluation coefficient, traction force fluctuation degree, and winding size compliance degree, respectively. It represents a natural constant, and compares the blow molding production quality evaluation index of the packaging plastic film with the preset blow molding production quality index threshold. If the blow molding production quality evaluation index of the packaging plastic film is greater than or equal to the preset blow molding production quality index threshold, it means that the blow molding production quality of the packaging plastic film is qualified; otherwise, it means that the blow molding production quality of the packaging plastic film is unqualified, and feedback is given.