Manual TIG (Tungsten Inert Gas) welding method for high-fragment-rate steel plug welding head
Through the manual TIG welding method, the problems of non-fusion of the inner corner root and weld cracks during plug welding are solved, a high-quality welded joint is achieved, and the weld is ensured to be well formed. It is suitable for high-fragment rate steel and high-strength steel materials. Preheat welding.
Patent Information
- Application Number
- CN202411128444.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-10-01
AI Technical Summary
During the plug welding process of steel materials with a high fragmentation rate, defects such as lack of fusion of the inner corner roots and weld cracks during plug welding are common, resulting in poor welding quality and difficulty in meeting the mechanical performance requirements of product design.
Use manual TIG welding methods, including heat treatment of the sleeve and base, processing of plug weld holes, detailed operation of welding steps, including bottom welding, filler welding and cap welding, using tungsten electrodes and specific welding wires, controlling the welding environment and arc The moving sequence, slow cooling treatment and inspection steps ensure the integrity and mechanical properties of the weld.
It achieves high-quality welded joints, avoids defects of root failure and weld cracks, ensures good weld formation, meets the welding performance requirements of steel materials with high fragmentation rate, and is suitable for high-strength steel materials without preheating.
Smart Images

Figure CN118720665A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of missile welding, and in particular to a manual TIG welding method for a high-fragmentation rate steel plug welding joint. Background Art
[0002] With the upgrading of ammunition products, a series of high-strength steel materials such as 58SiMn and 50SiMnVB have been put into use to meet the characteristics of high hardness, high strength and high fragmentation rate of the products. These have caused great difficulties in material welding. At the same time, in order to reduce production costs, welding without preheating is also required, which has higher requirements for welding specifications. However, there are few records of the use of 50SiMnVB and 58SiMn materials in welding structures in domestic and foreign literature, especially there is not much mature experience to learn from in the welding technology of plug welding without preheating.
[0003] In order to improve the plug welding with high hardness, high strength and high restraint after heat treatment, the low matching joint form is generally adopted, and the actual operation of the fillet weld position is carried out according to the welding method of the fillet weld at the vertical angle joint position. The welding sequence is to start the arc at the 12 o'clock or 6 o'clock position at the root of the inner angle of the hole, turn to the 3 o'clock position after starting the arc, then turn to the 6 o'clock or 12 o'clock position, then turn to the 9 o'clock position, then turn to the 12 o'clock or 6 o'clock position, and finally turn to the middle of the weld. After filling the weld, the arc is closed to fill the arc pit. But in fact, the plug welding hole diameter is small, and the arc is difficult to reach the root of the joint, resulting in the arc growth and the arc column temperature reduction; the welding speed is fast, the weld cooling crystallization speed is different, etc., causing welding problems such as unfused weld root, weld cracks (weld center cracks, weld heat affected zone cracks).
[0004] How to solve the defects such as unfused inner corner root and weld cracks during plug welding is of practical significance for meeting production requirements. Summary of the invention
[0005] The purpose of the present invention is to provide a manual TIG welding method for a high fragmentation rate steel plug weld joint to solve the defects such as unfused inner corner root and weld cracks during plug weld hole welding, so that the weld joint is well formed, free of welding defects, has good mechanical properties, and meets product design requirements.
[0006] The technical solution adopted by the present invention to solve the above technical problems is: a manual TIG welding method for a high fragmentation rate steel plug welding joint, the welding method is based on the TIG welding method for a high fragmentation rate steel plug welding joint, and adopts manual TIG welding, comprising the following steps: ⑴ Heat treatment of the socket and the substrate: first quenching and tempering, the yield strength of the socket after heat treatment is Rp0.2 ≥ 1250MPa, and the shrinkage rate is A ≥ 10%; the tensile strength of the substrate material 58SiMn after heat treatment is RM ≥ 920MPa, and the cross-sectional shrinkage rate is Z ≥ 15% or the yield strength of the material 50SiMnVB after heat treatment is Rp0.2 ≥ 1050MPa, and the cross-sectional shrinkage rate is Z ≥ 16%; (2) Processing the plug welding holes of the socket parts: Process the cone-shaped through holes on the cylindrical surface of the socket parts, evenly distribute two groups, a total of 12 to 16 plug welding holes; then socket them on the base, and make the inner circle of the welded part and the outer circle of the base form a transition fit; ⑶ Welding: Place the assembled and cleaned workpiece on the welding tooling, and use TIG welding for base welding. First, ignite the arc. You can also use the arc-starting plate to start the arc to the joint in the groove, lower the arc and move slowly, first melt the joint with a short arc without filling wire, the welding current is 180A~200A, the gas flow is 10L / min~13L / min, the argon purity is 99.95%, direct current is positive, and then intermittent wire feeding is performed; for filling welding, continuous wire feeding is performed to ensure fusion with the edge of the previous weld; for cap welding, intermittent wire feeding is performed; thoriated tungsten electrode should be used, the tungsten electrode diameter is φ2.4mm, the tungsten end head is a cone shape, the angle is 45°, and the minimum end diameter is 1.1mm; welding environment: room temperature is not lower than 10℃, relative humidity is not higher than 70%, and wind speed is not higher than 2m / s; ⑷ Slow cooling: After welding, put it into the furnace immediately, the furnace temperature is 150℃~180℃, the insulation time is 300±10 minutes, then take it out of the furnace and air cool it to room temperature, or cover the welded joint with aluminum silicate insulation cotton to slowly cool it to room temperature; ⑸ Inspection: After welding, visual inspection should be conducted to check for defects such as pits and undercuts. After machining, the weld should be inspected by magnetic particle inspection. No cracks or pores are allowed on the weld surface.
[0007] Furthermore, in step (1), the socket is made of 35CrMnSiA.
[0008] In step (2), the thickness of the socket is 5mm-12mm, the thickness of the base is 10mm-18mm, the diameter of the large end of the plug welding hole is φ15mm-φ25mm, and the diameter of the small end is φ12mm-φ20mm.
[0009] In step (3), for cold welding, the arc is stretched to preheat the welded parts without filling wire at the melting joint, the temperature is between 150°C and 200°C, the interlayer temperature is maintained between 180°C and 200°C, and the temperature is measured at a distance of 50mm from the groove.
[0010] In step (3), jet transition is adopted, the tungsten electrode extension length is 5mm-6mm, short arc welding, arc length is 2mm-3mm, TIG welding is adopted for base welding, welding wire is H18CrMoA, welding wire diameter is φ1.2mm, gas flow rate is 10L / min-13L / min, argon purity is 99.95%, welding current is 180A-220A, welding voltage is 20V-22V, DC positive connection; TIG welding is adopted for filling welding, welding wire is HS-80, welding wire diameter is The diameter of the welding wire is φ1.2mm, the gas flow rate is 10L / min~13L / min, the purity of argon is 99.95%, the welding current is 200A~230A, the welding voltage is 20V~22V, and the DC is connected positively; TIG welding is used for cap welding, HS-80 welding wire is selected, the welding wire diameter is φ1.2mm, the gas flow rate is 10L / min~15L / min, the purity of argon is 99.95%, the welding current is 230A~250A, the welding voltage is 20V~22V, and the DC is connected positively.
[0011] In step (3), after the arc stabilizes, start welding from the 6 o'clock or 12 o'clock position in the plug weld hole toward the 3 o'clock direction, with the welding gun and the socket at 55º~60º and the welding direction at about 75º~80º to ensure fusion at the root of the entry point, and then adjust the welding gun angle, with the welding gun and the substrate at 75º~80º, quickly move along the diameter direction of the plug weld hole to the 9 o'clock position, and then start welding quickly toward the 12 o'clock or 6 o'clock direction, and then quickly move along the diameter direction of the plug weld hole to the 6 o'clock or 12 o'clock position, and then start welding toward the 9 o'clock direction, and finally quickly move along the diameter direction of the plug weld hole to the 3 o'clock position, and then start welding toward the 12 o'clock or 6 o'clock direction. During this period, pay attention to the rapid change of the welding gun angle to fill the entire plug weld hole, and close the arc, and pay attention to delayed gas protection.
[0012] Compared with the prior art, the beneficial effects of the present invention are: TIG welding of plug welding joints without preheating after heat treatment of high fragmentation rate steel is realized. It can ensure that the weld is well fused, no defects such as root incomplete fusion and weld cracks are found, and the weld is well formed. The plug welding sequence of TIG welding is reasonable and reliable welding can be achieved. Low-strength matching without preheating can achieve high-quality welded joints. The method of the present invention is suitable for manual TIG welding of plug welding joints of high fragmentation rate steel, and can be extended to welding of heterogeneous high-strength steel materials without preheating. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 Schematic diagram of plug welding of socket parts and base parts. Figure 2 yes Figure 1 Top view of the . DETAILED DESCRIPTION Embodiment 1:
[0014] like Figure 1 As shown, a manual TIG welding method for a high fragmentation rate steel plug welding joint is provided. This embodiment is based on the TIG welding method for a high fragmentation rate steel plug welding joint, and adopts manual TIG welding, including the following steps: Step (1) heat-treating the socket 1 and the substrate 2: first quenching and tempering, the yield strength of the socket material 35CrMnSiA steel after heat treatment is Rp0.2≥1250MPa, and the shrinkage rate is A≥10%; the tensile strength of the substrate material 58SiMn after heat treatment is RM≥920MPa, and the cross-sectional shrinkage rate is Z≥15%; Step (2) Processing the plug welding holes of the socket: Processing the cone-shaped through holes on the cylindrical surface of the socket with a thickness of 5 mm, evenly distributing two groups, a total of 16 plug welding holes 3, the large end diameter of the plug welding hole is φ15 mm, and the small end diameter is φ12 mm; then socketing on the substrate 2 with a thickness of 10 mm, so that the inner circle of the socket to be welded and the outer circle of the substrate form a transition fit; Step ⑶ Welding: Place the assembled and cleaned workpiece on the welding tool. Use jet transition and TIG welding for base welding. First, ignite the arc. You can also use an arc starting plate to start the arc to the joint in the groove. Lower the arc and move slowly. First, use a short arc without filling the wire to melt the joint. The welding current is 180A~200A, the gas flow rate is 10L / min~13L / min, the argon purity is 99.95%, and the direct current is positive. The arc is stretched for preheating. The temperature is between 150℃ and 200℃. The interlayer temperature is maintained between 180℃ and 200℃. The temperature is measured at a distance of 50mm from the groove, followed by intermittent wire feeding. The tungsten electrode extends to a length of 5mm~6mm. Short arc welding has an arc length of 2mm~3mm. The welding wire is H18CrMoA, the welding wire diameter is φ1.2mm, and the gas flow rate is 10L / min~13L / min. , argon purity is 99.95%, welding current is 180A~220A, welding voltage is 20V~22V, and DC is positively connected; for filling welding, continuous wire feeding is carried out, the welding wire is HS-80, the welding wire diameter is φ1.2mm, the gas flow rate is 10L / min~13L / min, the argon purity is 99.95%, the welding current is 200A~230A, the welding voltage is 20V~22V, and DC is positively connected to ensure fusion with the edge of the previous weld; for cap welding, intermittent wire feeding is carried out, the welding wire is HS-80, the welding wire diameter is φ1.2mm, the gas flow rate is 10L / min~15L / min, the argon purity is 99.95%, the welding current is 230A~250A, the welding voltage is 20V~22V, and DC is positively connected. The tungsten electrode should be thoriated tungsten electrode with a diameter of φ2.4mm. The tungsten electrode tip is frustum-shaped with an angle of 45° and a minimum end diameter of 1.1mm. Welding environment: room temperature not lower than 10°C, relative humidity not higher than 70%, and wind speed not higher than 2m / s. The welding sequence is: after the arc is stable, start welding from the 6 o'clock or 12 o'clock position in the plug weld hole toward the 3 o'clock direction, with the welding gun and the socket at 55º~60º and about 75º~80º to the welding direction to ensure fusion at the root of the entry point, and then adjust the welding gun angle, with the welding gun and the substrate at 75º~80º, quickly move along the diameter direction of the plug weld hole to the 9 o'clock position, and then start welding quickly toward the 12 o'clock or 6 o'clock direction, and then quickly move along the diameter direction of the plug weld hole to the 6 o'clock or 12 o'clock position, and then start welding toward the 9 o'clock direction, and finally quickly move along the diameter direction of the plug weld hole to the 3 o'clock position, and then start welding toward the 12 o'clock or 6 o'clock direction. During this period, pay attention to the rapid change of the welding gun angle to fill the entire plug weld hole, and close the arc, and pay attention to delayed gas protection.
[0015] Step (4) Slow cooling: After welding, put the welded joint into the furnace immediately, the furnace temperature is 150℃~180℃, the heat preservation time is 300±10 minutes, then take it out of the furnace and air cool it to room temperature, or cover the welded joint with aluminum silicate insulation cotton to slowly cool it to room temperature; Step ⑸ Inspection: After welding, visually inspect to ensure there are no defects such as pits and undercuts. After machining, use magnetic particle inspection to inspect the weld. No cracks or pores are allowed on the weld surface.
[0016] This implementation method can provide stable welding quality, and the performance of the welding joint meets the requirements of safe use, etc.; at the same time, the welding joint can withstand the influence of chamber pressure, inertia force and other forces, meeting the actual use requirements of the product. Embodiment 2:
[0017] like Figure 1 As shown, this embodiment is based on a TIG welding method for high fragmentation rate steel 50SiMnVB and 35CrMnSiA steel plug welding joints, using manual TIG welding, and includes the following steps: Step (1) heat-treating the socket 1 and the substrate 2: first quenching and tempering, the yield strength of the socket material 35CrMnSiA steel after heat treatment is Rp0.2≥1250MPa, and the shrinkage rate is A≥10%; the yield strength of the substrate material 50SiMnVB after heat treatment is Rp0.2≥1050MPa, and the cross-sectional shrinkage rate is Z≥16%; Step (2) Processing the plug welding holes of the socket: Processing the cone-shaped through holes on the cylindrical surface of the socket with a thickness of 10 mm, evenly distributing two groups of 12 plug welding holes in total, with the large end diameter of the plug welding holes being 25 mm and the small end diameter being 20 mm; then socketing on a substrate with a thickness of 18 mm so that the inner circle of the socket to be welded forms a transition fit with the outer circle of the substrate; Step (3) Welding: Place the assembled and cleaned workpiece on the welding tool. Use jet transition and TIG welding for base welding. First, ignite the arc. You can also use an arc-starting plate to start the arc to the joint inside the groove. Press down the arc and move it slowly. First, melt the joint with a short arc without filling wire. The welding current is 180A~200A, the gas flow rate is 10L / min~13L / min, the argon purity is 99.95%, and the direct current is positive. The arc is stretched for preheating. The temperature is between 150℃ and 200℃. The interlayer temperature is maintained between 180℃ and 200℃. When measuring the temperature, the distance from the groove is 50mm. Then, intermittent wire feeding is performed. The tungsten electrode extension length is 5mm~6mm. Short arc welding has an arc length of 2mm~3mm. The welding wire is H18CrMoA, the welding wire diameter is φ1.2mm, and the gas flow rate is 10L / min~13L / min. , argon purity is 99.95%, welding current is 180A~220A, welding voltage is 20V~22V, and DC is positively connected; for filling welding, continuous wire feeding is carried out, the welding wire is HS-80, the welding wire diameter is φ1.2mm, the gas flow rate is 10L / min~13L / min, the argon purity is 99.95%, the welding current is 200A~230A, the welding voltage is 20V~22V, and DC is positively connected to ensure fusion with the edge of the previous weld; for cap welding, intermittent wire feeding is carried out, the welding wire is HS-80, the welding wire diameter is φ1.2mm, the gas flow rate is 10L / min~15L / min, the argon purity is 99.95%, the welding current is 230A~250A, the welding voltage is 20V~22V, and DC is positively connected. The tungsten electrode should be thoriated tungsten electrode with a diameter of φ2.4mm. The tungsten electrode tip is frustum-shaped with an angle of 45° and a minimum end diameter of 1.1mm. Welding environment: room temperature not lower than 10°C, relative humidity not higher than 70%, and wind speed not higher than 2m / s. The welding sequence is: after the arc is stable, start welding from the 6 o'clock or 12 o'clock position in the plug weld hole toward the 3 o'clock direction, with the welding gun and the socket at 55º~60º and about 75º~80º to the welding direction to ensure fusion at the root of the entry point, and then adjust the welding gun angle, with the welding gun and the substrate at 75º~80º, quickly move along the diameter direction of the plug weld hole to the 9 o'clock position, and then start welding quickly toward the 12 o'clock or 6 o'clock direction, and then quickly move along the diameter direction of the plug weld hole to the 6 o'clock or 12 o'clock position, and then start welding toward the 9 o'clock direction, and finally quickly move along the diameter direction of the plug weld hole to the 3 o'clock position, and then start welding toward the 12 o'clock or 6 o'clock direction. During this period, pay attention to the rapid change of the welding gun angle to fill the entire plug weld hole, and close the arc, and pay attention to delayed gas protection.
[0018] Step (4) slow cooling: after welding is completed, the welded joint is immediately put into a furnace at a temperature of 150°C to 180°C for 300±10 minutes, then removed from the furnace and air-cooled to room temperature, or the welded joint is covered with aluminum silicate insulation cotton to allow it to slowly cool to room temperature; Step (5) Inspection: After welding, visual inspection is performed to ensure that there are no defects such as pits and undercuts. After machining, the weld is inspected by magnetic particle inspection. No cracks or pores are allowed on the weld surface.
[0019] This implementation method can provide stable welding quality, and the performance of the welding joint meets the requirements of safe use, etc.; at the same time, the welding joint can withstand the influence of chamber pressure, inertia force and other forces, meeting the actual use requirements of the product.
Claims
1. A manual TIG welding method for a high fragmentation rate steel plug welding joint, the welding method is based on the TIG welding method for a high fragmentation rate steel plug welding joint, adopts manual TIG welding, and is characterized in that: The following steps are involved: ⑴ Heat treatment of the socket and the substrate: first quenching and tempering, the yield strength of the socket after heat treatment is Rp0.2 ≥ 1250MPa, and the shrinkage rate is A ≥ 10%; the tensile strength of the substrate material 58SiMn after heat treatment is RM ≥ 920MPa, and the cross-sectional shrinkage rate is Z ≥ 15% or the yield strength of the material 50SiMnVB after heat treatment is Rp0.2 ≥ 1050MPa, and the cross-sectional shrinkage rate is Z ≥ 16%; (2) Processing the plug welding holes of the socket parts: Process the cone-shaped through holes on the cylindrical surface of the socket parts, evenly distribute two groups, a total of 12 to 16 plug welding holes; then socket them on the base, and make the inner circle of the welded part and the outer circle of the base form a transition fit; ⑶ Welding: Place the assembled and cleaned workpiece on the welding tooling, and use TIG welding for base welding. First, ignite the arc. You can also use the arc-starting plate to start the arc to the joint in the groove, lower the arc and move slowly, first melt the joint with a short arc without filling wire, the welding current is 180A~200A, the gas flow is 10L / min~13L / min, the argon purity is 99.95%, direct current is positive, and then intermittent wire feeding is performed; for filling welding, continuous wire feeding is performed to ensure fusion with the edge of the previous weld; for cap welding, intermittent wire feeding is performed; thoriated tungsten electrode should be used, the tungsten electrode diameter is φ2.4mm, the tungsten end head is a cone shape, the angle is 45°, and the minimum end diameter is 1.1mm; welding environment: room temperature is not lower than 10℃, relative humidity is not higher than 70%, and wind speed is not higher than 2m / s; ⑷ Slow cooling: After welding, put it into the furnace immediately, the furnace temperature is 150℃~180℃, the insulation time is 300±10 minutes, then take it out of the furnace and air cool it to room temperature, or cover the welded joint with aluminum silicate insulation cotton to slowly cool it to room temperature; ⑸ Inspection: After welding, visual inspection should be conducted to check for defects such as pits and undercuts. After machining, the weld should be inspected by magnetic particle inspection. No cracks or pores are allowed on the weld surface.
2. According to the manual TIG welding method of high fragmentation rate steel plug welding joint according to claim 1, it is characterized in that: In step (1), the socket is made of 35CrMnSiA.
3. The manual TIG welding method for high fragmentation rate steel plug welding joint according to claim 1 is characterized in that: In step (2), the thickness of the socket is 5mm-12mm, the thickness of the base is 10mm-18mm, the diameter of the large end of the plug welding hole is φ15mm-φ25mm, and the diameter of the small end is φ12mm-φ20mm.
4. According to claim 1, the manual TIG welding method for high fragmentation rate steel plug welding joint is characterized in that: In step (3), for cold welding, the arc is stretched to preheat the welded parts without filling wire at the melting joint, the temperature is between 150°C and 200°C, the interlayer temperature is maintained between 180°C and 200°C, and the temperature is measured at a distance of 50mm from the groove.
5. The manual TIG welding method for high fragmentation rate steel plug welding joint according to claim 1, 2, 3 or 4, characterized in that: In step (3), jet transition is adopted, the tungsten electrode extension length is 5mm-6mm, short arc welding, arc length is 2mm-3mm, TIG welding is adopted for base welding, welding wire is H18CrMoA, welding wire diameter is φ1.2mm, gas flow rate is 10L / min-13L / min, argon purity is 99.95%, welding current is 180A-220A, welding voltage is 20V-22V, DC positive connection; TIG welding is adopted for filling welding, welding wire is HS-80, welding wire diameter is The diameter of the welding wire is φ1.2mm, the gas flow rate is 10L / min~13L / min, the purity of argon is 99.95%, the welding current is 200A~230A, the welding voltage is 20V~22V, and the DC is connected positively; TIG welding is used for cap welding, HS-80 welding wire is selected, the welding wire diameter is φ1.2mm, the gas flow rate is 10L / min~15L / min, the purity of argon is 99.95%, the welding current is 230A~250A, the welding voltage is 20V~22V, and the DC is connected positively.
6. The manual TIG welding method for high fragmentation rate steel plug welding joint according to claim 5 is characterized in that: In step (3), after the arc stabilizes, start welding from the 6 o'clock or 12 o'clock position in the plug weld hole toward the 3 o'clock direction, with the welding gun and the socket at 55º~60º and the welding direction at about 75º~80º to ensure fusion at the root of the entry point, and then adjust the welding gun angle, with the welding gun and the substrate at 75º~80º, quickly move along the diameter direction of the plug weld hole to the 9 o'clock position, and then start welding quickly toward the 12 o'clock or 6 o'clock direction, and then quickly move along the diameter direction of the plug weld hole to the 6 o'clock or 12 o'clock position, and then start welding toward the 9 o'clock direction, and finally quickly move along the diameter direction of the plug weld hole to the 3 o'clock position, and then start welding toward the 12 o'clock or 6 o'clock direction. During this period, pay attention to the rapid change of the welding gun angle to fill the entire plug weld hole, and close the arc, and pay attention to delayed gas protection.
Citation Information
Patent Citations
13 Cr oil well-pipe test material object preparation method
CN101149319A
Conical tip argon tungsten-arc welding method adopting 4d tungsten electrode
CN103386537A
Deep-fuze-hole-provided thin-wall shell warhead composite powder charging method
CN108955426A
Welding method of plug welding hole
CN109940246A
Partial multidirectional corner joint TIG welding method of thin-walled ultrahigh-strength steel
CN110315173A