Efficient preparation method of fluorine-containing compound intermediate fluorobenzene

By using PVDF pervaporation membranes for water removal in the preparation of fluorobenzene, the problems of high-temperature heating and difficulty in catalyst selection are solved, high-purity and efficient preparation of fluorobenzene is achieved, meeting the purity requirements in the high-tech field and reducing production costs. .

CN118724672APending Publication Date: 2024-10-01NINGXIA KUNZHENG BIOTECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410751340.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-12
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Existing fluorobenzene preparation methods have problems such as potential problems caused by high-temperature heating, difficulty in catalyst selection, complex separation and purification technology, and low water removal efficiency, making it difficult to achieve high-purity and efficient fluorobenzene preparation.

Method used

PVDF pervaporation membrane is used for moisture removal of fluorobenzene, by heating to 80±5℃ and pressurizing into the membrane shell at a pressure of 0.20-0.25Mpa, using the TGTG' spiral structure of PVDF and appropriate thickness (300-450μm). Moisture removal, ensuring a hold time of 15-40 minutes for efficient removal.

Benefits of technology

It achieves high purity (more than 99.999%) and low moisture content (≤10ppm) of fluorobenzene, improves the service life of the pervaporation membrane, reduces production costs and energy consumption, and ensures the application needs of the product in high-tech fields.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides an efficient preparation method of fluorine-containing compound intermediate fluorobenzene, which comprises the following steps: treating fluorobenzene in a raw material intermediate tank by a filter, a heat exchanger and a heater, heating to 80 + / -5 DEG C by a steam system, and pressurizing to enter a membrane shell of a permeable membrane; the pervaporation membrane active layer is made of PVDF; and keeping for a specific time in the membrane shell of the permeable membrane to remove moisture in the fluorobenzene. According to the method, the service life of the pervaporation membrane is prolonged, and the production cost of fluorobenzene is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for manufacturing a chemical product, and in particular to a method for preparing high-purity fluorobenzene. Background Art

[0002] Fluorobenzene is a colorless liquid with an aromatic smell similar to benzene. It is often used as a fluorination agent for aromatic compounds in organic synthesis, and can be used to prepare other organofluorine compounds, such as fluorobenzoates, fluorobenzyl alcohols, and fluorophenyl borate esters. These compounds have broad application prospects in the fields of medicine, dyes, and coatings. Fluorobenzene can be used to prepare phenyl fluoride compounds and fluorinated substituted benzene rings. These fluorinated aromatic hydrocarbons are key building blocks for many drugs, pesticides, and other bioactive molecules, so fluorobenzene is widely used in the pharmaceutical and agricultural chemical fields. In addition, fluorobenzene can also be used to synthesize organic compounds containing fluorine atoms, which also have important application prospects in the fields of medicine, materials science, and optoelectronic technology.

[0003] CN117263765A discloses a process for preparing high-purity electronic-grade fluorobenzene by an aniline synthesis method, comprising the following steps: step 1: filtering fluorobenzene from a synthesis workshop; step 2: heating the product of step 1 to a first temperature; step 3: transferring the product of step 2 to a pervaporation membrane and heating it to a second temperature; step 4: maintaining the second temperature for a period of time, cooling the fluorobenzene in the atmospheric pressure region of the pervaporation membrane to obtain electronic-grade fluorobenzene.

[0004] CN116751103A discloses a method for preparing electronic grade fluorobenzene, which belongs to the field of fluorine chemical industry, wherein aniline and hydrogen fluoride are used as raw materials to form salt, and then nitrosyl fluoride is used as a diazo reagent to perform diazotization reaction to prepare fluorobenzene. The method for preparing fluorobenzene provided by the present invention uses aniline hydrogen fluoride salt solution and nitrosyl fluoride for diazotization thermal decomposition reaction to obtain fluorobenzene, without introducing sodium ions and without aniline residue, and has simple process, high reaction efficiency and good selectivity. Summary of the invention

[0005] In view of the deficiencies in the prior art, the present invention provides a method for efficiently preparing fluorinated intermediate fluorobenzene. To achieve the above purpose, the present invention adopts the following scheme:

[0006] The fluorobenzene in the raw material intermediate tank is processed by the filter, heat exchanger and heater, and then heated to 80±5℃ by the steam system, and then pressurized into the membrane shell of the permeation membrane;

[0007] The material of the active layer of the pervaporation membrane is PVDF;

[0008] Keep the water in the fluorobenzene in the permeation membrane shell for a specific time.

[0009] Furthermore, the pressure is applied to the membrane shell of the permeable membrane at a pressure of 0.15-0.45 MPa.

[0010] Furthermore, the preferred pressure is 0.20-0.25 MPa.

[0011] Furthermore, the spatial structure of the PVDF is a TGTG' helical structure.

[0012] Furthermore, the thickness of the PVDF is between 200-550 μm.

[0013] Furthermore, the thickness of the PVDF is between 300-450 μm.

[0014] Furthermore, the specific maintaining time is 15-40 minutes.

[0015] Compared with the prior art, the present invention has the following advantages and beneficial effects:

[0016] 1. The present invention directly removes water from high-temperature fluorobenzene, avoiding potential problems caused by heating the pervaporation membrane. 2. The present invention uses a PVDF pervaporation membrane to remove water from fluorobenzene. The membrane has a TGTG' spiral structure and an efficient permeation flux, and can efficiently remove water. 3. The method of the present invention increases the service life of the pervaporation membrane and reduces the production cost of fluorobenzene. DETAILED DESCRIPTION

[0017] In order to make the technical problems solved by the present invention, the technical solutions adopted and the technical effects achieved clearer, the technical solutions of the embodiments of the present invention are further described in detail below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.

[0018] The preparation of electronic-grade fluorobenzene is very difficult. The first is the high purity requirements of the raw materials. Electronic-grade fluorobenzene has extremely high requirements for the purity of the raw materials, because any impurities may affect the performance and quality of the final product. Secondly, the reaction conditions are strictly controlled. Reaction temperature, pressure and time are key factors affecting the preparation of fluorobenzene. For example, the reaction temperature usually needs to be controlled below -20°C to avoid further substitution reactions of the benzene ring. Accurate control of these conditions is essential to ensure the purity and yield of the product. The choice of catalyst is also very important. Catalysts play a key role in the preparation of fluorobenzene, which can accelerate the reaction rate and improve product selectivity. Selecting a catalyst with high activity, good stability and reasonable price is a major challenge in the preparation process. The last and most important step is the complex separation and purification technology. Due to the similarity and proximity between fluorobenzene and raw materials such as styrene and hydrofluoric acid, the separation and purification process needs to adopt appropriate methods to ensure product purity and yield. Common separation methods include extraction, distillation, crystallization, etc. These technologies require precise control of operating conditions to ensure the quality and purity of the product.

[0019] The present invention conducts a detailed exploration of the water removal process in fluorobenzene.

[0020] Pervaporation membranes are usually composed of one or more layers of materials with specific selectivity, which can be polymers, inorganic materials, or their composites. These materials are selected and designed to achieve specific separation goals, such as removing water from organic solvents, separating organic matter from mixtures, etc. The thickness of the active layer of polyvinylidene fluoride (PVDF) as a pervaporation membrane is one of the key factors affecting its separation performance. The thickness of the active layer determines the path length and resistance of the substance through the membrane, thereby affecting the permeation flux and selectivity. When selecting PVDF as the thickness of the active layer of the pervaporation membrane, multiple factors need to be considered comprehensively. First, a thinner active layer usually has a higher permeation flux because the path through which the substance passes is shorter and the resistance is smaller. However, an active layer that is too thin may result in reduced selectivity because the shorter path may weaken the separation effect between different molecules. On the other hand, a thicker active layer can provide higher selectivity because the longer path and greater resistance help to better separate different molecules. However, an overly thick active layer may reduce the permeation flux because the path through which the substance passes is longer and the resistance is greater. Therefore, when selecting PVDF as the thickness of the active layer of the pervaporation membrane, the relationship between permeation flux and selectivity needs to be weighed. The specific thickness should be considered comprehensively based on factors such as the properties of the target separation material, operating conditions, and economic costs.

[0021] Under low pressure or normal pressure conditions, the structure of the pervaporation membrane usually includes the following parts:

[0022] Active Layer: This is the most important part of the pervaporation membrane, which determines the selectivity and separation performance of the membrane. The active layer is usually made of highly selective materials that allow the target components (such as water molecules) to pass through while blocking the passage of other components.

[0023] Support Layer: The support layer provides the mechanical strength and stability of the membrane and supports the active layer. It is usually made of porous materials such as porous polymers, ceramics or metal meshes. The pore size and porosity of the support layer can be adjusted as needed to optimize the permeability and selectivity of the membrane.

[0024] Protective Layer: In some cases, a protective layer can be added on top of the active layer to protect it from contamination or mechanical damage. The protective layer is usually made of a thin and tough material such as polytetrafluoroethylene (PTFE).

[0025] Under low pressure or normal pressure conditions, the working principle of pervaporation membrane is: when the mixture contacts the membrane, the target component (such as water molecules) passes through the active layer and permeates to the other side of the membrane driven by the chemical potential difference on both sides of the membrane. Due to the high selectivity of the active layer, other components are prevented from passing through, thereby achieving the separation of the target component.

[0026] Although there is no direct relationship between the structure of the pervaporation membrane and the operating pressure, the operating pressure may affect the permeability and selectivity of the membrane. Therefore, in practical applications, it is necessary to select a suitable pervaporation membrane according to the specific separation goals and operating conditions.

[0027] The structure of the pervaporation membrane has no direct relationship with its operating pressure (low pressure or normal pressure), because the working principle of the pervaporation membrane is based on the molecular transfer process driven by the chemical potential difference of the components on both sides of the membrane, rather than a simple pressure difference. However, low pressure or normal pressure operating conditions may affect the performance and selectivity of the pervaporation membrane.

[0028] The invention aims at solving the problems existing in the prior art and proposes a new method for preparing electronic-grade fluorobenzene.

[0029] Steps:

[0030] Raw material preparation: Take out the fluorobenzene raw material to be processed from the raw material intermediate tank.

[0031] Pretreatment: Fluorobenzene raw material first passes through a precision filter for preliminary impurity removal, then enters a heat exchanger for preheating, and then enters a heater to be heated to 80±5℃.

[0032] Pervaporation: The heated fluorobenzene is pressurized into the membrane shell containing the PVDF pervaporation membrane at a pressure of 0.20-0.25Mpa. The PVDF pervaporation membrane has a TGTG' spiral structure and a thickness of 300-450μm, which can effectively remove moisture from fluorobenzene.

[0033] Holding time: Keep in the membrane shell for 15-40 minutes to ensure that the moisture in fluorobenzene is fully adsorbed by the PVDF membrane.

[0034] Post-processing: The fluorobenzene treated by pervaporation is cooled, collected, and tested again to ensure that the product meets the electronic grade purity requirements.

[0035] Technical Effects

[0036] The electronic-grade fluorobenzene prepared by the present invention has a purity of more than 99.999% and a water content of less than 10ppm, which meets the high purity requirements of fluorobenzene in high-tech fields such as semiconductors, liquid crystal displays and solar cells. In addition, due to the use of PVDF pervaporation membrane technology, the water removal process is more efficient, reducing energy consumption and production costs.

[0037] In the present invention, a PVDF pervaporation membrane with a TGTG' spiral structure is selected, and its membrane thickness is controlled between 300-450 μm. During the operation, fluorobenzene is heated to 80±5°C and pressurized into the pervaporation membrane shell at a pressure of 0.20-0.25Mpa. The holding time is 15-40 minutes to ensure that the water in fluorobenzene is fully removed.

[0038] The advantages of the present invention are:

[0039] High efficiency of water removal rate. After testing, the use of PVDF pervaporation membrane with TGTG' spiral structure can effectively remove water from fluorobenzene at the selected temperature and pressure to ensure the purity of the product. Good recycling performance. After 10 cycles, the pervaporation membrane can still maintain a selective permeability of more than about 75%, showing good recycling performance. Economic and environmentally friendly. Due to the good stability and selectivity of the membrane material, energy consumption and production costs are reduced, and environmental pollution is also reduced.

[0040] For the present invention, the reason for the effect is that the TGTG' spiral structure of the PVDF pervaporation membrane gives it a higher permeation flux and better selectivity. This structure is conducive to the transmission and adsorption of water molecules in the membrane, thereby improving the efficiency and purity of water removal. The membrane thickness is controlled between 300-450μm, which can not only ensure the mechanical strength of the membrane, but also ensure the effective transmission of water molecules in the membrane. A too thick membrane will increase the mass transfer resistance and reduce the efficiency; while a too thin membrane may affect its stability and durability. Heating fluorobenzene to 80±5℃ and maintaining it at a pressure of 0.20-0.25Mpa is conducive to the separation of water molecules from fluorobenzene. This condition can maximize the performance of the pervaporation membrane and improve the water removal efficiency.

[0041] Example:

[0042] Raw materials preparation:

[0043] The fluorobenzene raw material to be processed is taken out from the raw material intermediate tank using a dedicated pump and piping system. The raw material should be stored in a sealed, dry and impurity-free condition.

[0044] Preprocessing:

[0045] Preliminary impurity removal: Introduce the fluorobenzene raw material into the precision filter, and remove the solid particles, suspended matter and other impurities in the raw material through the microporous structure of the filter. The filter should be cleaned and replaced regularly to ensure the filtering effect.

[0046] Preheating: After preliminary impurity removal, fluorobenzene enters the heat exchanger for preheating. The preheating temperature is controlled at 50-60℃ to reduce energy consumption in the subsequent heating process. During the preheating process, pay attention to controlling the flow rate and temperature to ensure that fluorobenzene is heated evenly.

[0047] Heating: The preheated fluorobenzene enters the heater and is heated to 80±5℃. The heater uses electric heating tubes or steam heating, and the heating temperature is accurately controlled by the temperature control system. During the heating process, the temperature change of fluorobenzene should be monitored to ensure that the temperature is stable within the set range.

[0048] Pervaporation

[0049] Pressurize into the membrane shell: The heated fluorobenzene is pressurized to 0.20-0.25Mpa through a pump and piping system, and then introduced into the membrane shell containing the PVDF pervaporation membrane. The membrane shell should have good sealing and pressure resistance to ensure that fluorobenzene will not leak under high pressure.

[0050] PVDF pervaporation membrane: PVDF pervaporation membrane is a key component in the preparation process, with a TGTG' helical structure and a thickness of 300-450μm. The membrane has excellent water permeability and selectivity, and can efficiently remove water from fluorobenzene. During the pervaporation process, water molecules are adsorbed and transferred to the other side of the membrane through the membrane pores, thereby achieving separation from fluorobenzene.

[0051] Holding time: Keep fluorobenzene in the membrane shell for a certain period of time (15-40 minutes) to ensure that the water is fully adsorbed by the PVDF membrane. The length of the holding time depends on factors such as the initial water content of fluorobenzene, the permeation flux of the membrane, and operating conditions. The optimal holding time is determined by real-time monitoring of the water content in fluorobenzene.

[0052] Post-processing

[0053] Cooling: The fluorobenzene treated by pervaporation is first cooled. The cooling process is carried out through a cooler or cooling tower to reduce the temperature of fluorobenzene to below room temperature. During the cooling process, care should be taken to control the cooling rate and temperature to avoid crystallization or solidification of fluorobenzene during the cooling process.

[0054] Collection: After cooling, the fluorobenzene is collected by a collection device. The collection device should have good sealing and no leakage to prevent contamination by external impurities. During the collection process, attention should be paid to controlling the flow rate and collection speed to ensure that the fluorobenzene enters the collection container evenly and stably.

[0055] Testing: Perform quality testing on the collected fluorobenzene. Use high performance liquid chromatography (HPLC), gas chromatography (GC) and other analytical methods to test the water content and other impurities in fluorobenzene. Ensure that the product meets the electronic grade purity requirements (water content ≤ 10ppm). If the product purity does not meet the requirements, repeat the pervaporation process or take other purification measures for further processing.

[0056] Comparative Example 1: Non-TGTG' helical structure PVDF material as pervaporation membrane

[0057] Membrane material selection: In this comparative example, β-structured PVDF was selected as the material of the pervaporation membrane instead of the TGTG' helical structured PVDF in the original example. β-structured PVDF also has good chemical stability and thermal stability.

[0058] Technical effect: When using β-structured PVDF as a pervaporation membrane, it was found that the water removal efficiency was significantly lower than that of using a PVDF membrane. It is speculated that this may be because at a specific temperature and pressure, the permeation flux of β-structured PVDF is low and the transmission speed of water molecules in the membrane is slow. In addition, the selectivity of the β-structured PVDF membrane is also low, further reducing the purity and quality of the product.

[0059] Experimental results: Under the same operating conditions (such as temperature 80°C, pressure 0.2MPa, holding time 30 minutes), the moisture removal rate using PTFE membrane is only 60%, far lower than the PVDF membrane of more than 90%.

[0060] Comparative Example 2: Too thin PVDF membrane

[0061] Membrane thickness: In this comparative example, a PVDF membrane with a thickness of 100 μm was selected, which is much lower than the 300-450 μm range in the original example.

[0062] Technical effect: Although thinner membranes can reduce mass transfer resistance and increase the transfer rate of water molecules, overly thin membranes also have serious mechanical strength problems. In actual operation, it was found that 100μm PVDF membranes were prone to breakage and deformation during the pressurization process, resulting in the inability to continuously remove water. In addition, due to the instability of the membrane, the water removal efficiency and product purity were also seriously affected.

[0063] Experimental results: After five cycles of use, the 100μm PVDF membrane showed obvious damage and deformation and could no longer be used in the pervaporation process. At the same time, during the cycle, the water removal rate gradually dropped to below 40%.

[0064] Comparative Example 3: Excessively high operating temperature

[0065] Operating temperature: In this comparative example, the heating temperature of fluorobenzene was increased to 120°C, which is much higher than 80±5°C in the original example.

[0066] Technical Effect: Excessively high operating temperature causes fluorobenzene molecules to become more active, prone to decomposition or other side reactions. These side reactions not only reduce the purity and quality of fluorobenzene, but may also lead to the production of harmful substances. In addition, high temperature may also accelerate the aging process of the pervaporation membrane and shorten its service life.

[0067] Experimental results: At an operating temperature of 120°C, the decomposition rate of fluorobenzene reached 5%, which was much higher than that of the original embodiment. In addition, the service life of the pervaporation membrane was significantly shortened, and a significant performance degradation occurred after only two cycles.

[0068] Comparative Example 4: Too low operating pressure

[0069] Operating pressure: In this comparative example, the operating pressure was reduced to below 0.1 MPa, which is much lower than the 0.15-0.45 MPa range in the original example.

[0070] Technical effect: Too low operating pressure reduces the mass transfer driving force of water molecules on both sides of the membrane, resulting in reduced water removal efficiency. In order to achieve the same water removal effect, it is necessary to increase the retention time or increase the operating temperature, which will increase energy consumption and production costs. In addition, too low pressure may also cause fluorobenzene to form bubbles or foam layers on the membrane surface, further reducing mass transfer efficiency and product quality.

[0071] Experimental results: Under an operating pressure of 0.1 MPa, the water removal rate is only 65%, which is much lower than the 99% or more in the original embodiment. At the same time, in order to maintain a certain water removal effect, the retention time needs to be increased to more than 60 minutes, which greatly increases the production cost and time cost.

[0072] Comparative Example 5: Too short holding time

[0073] Retention time: In this comparative example, the retention time of fluorobenzene in the membrane shell was shortened to 5 minutes, which is much lower than the range of 15-40 minutes in the original example.

[0074] Technical effect: Too short a retention time makes it impossible for water molecules to be fully adsorbed and removed by the pervaporation membrane. Although part of the water can be removed in a short time, a large amount of water remains in fluorobenzene, resulting in a decrease in product purity. In addition, too short a retention time may also lead to uneven distribution of fluorobenzene on the membrane surface and uneven mass transfer, further affecting mass transfer efficiency and product quality.

[0075] Experimental results: After a holding time of 5 minutes, the moisture content of fluorobenzene is as high as 50ppm, far exceeding the purity requirement of electronic grade fluorobenzene (usually required to be less than 10ppm). At the same time, other performance indicators of the product are also affected to varying degrees.

[0076] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. An efficient preparation method of fluorine-containing compound intermediate fluorobenzene, Features The following steps are involved: The fluorobenzene in the raw material intermediate tank is processed by the filter, heat exchanger and heater, and then heated to 80±5℃ by the steam system, and then pressurized into the membrane shell of the permeation membrane; The material of the active layer of the pervaporation membrane is PVDF; Keep the water in the fluorobenzene in the permeation membrane shell for a specific time.

2. The method for efficiently preparing fluorinated intermediate fluorobenzene according to claim 1, Features: The pressure is applied to the membrane shell of the permeation membrane, and the pressure is 0.15-0.45Mpa.

3. The efficient preparation method of fluorinated intermediate fluorobenzene according to claim 2, Features: The preferred pressure is 0.20-0.25 MPa.

4. The method for efficiently preparing fluorinated intermediate fluorobenzene according to claim 1, Features: The spatial structure of the PVDF is a TGTG' helical structure.

5. The efficient preparation method of fluorine-containing compound intermediate fluorobenzene according to claim 1, Features: The thickness of the active layer is between 200-550 μm.

6. The method for efficiently preparing fluorinated intermediate fluorobenzene according to claim 1, Features: The thickness of the active layer is between 300-450 μm.

7. The method for efficiently preparing fluorinated intermediate fluorobenzene according to claim 1, Features: The specific maintaining time is 15-40 minutes.