Method for preparing oxalic acid diester compound by using gold-based catalyst
The supported gold catalyst is used to convert nitrite ester and CO into oxalic acid diester in the CO coupling reaction, which solves the problems of environmental pollution and explosion risk in the existing technology, achieves mild reaction conditions and high product yield, and is suitable for Industrial production.
Patent Information
- Application Number
- CN202410945486.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2024-10-01
AI Technical Summary
The existing dimethyl oxalate preparation technology has problems of environmental pollution, explosion risks and insufficient catalyst selectivity. In particular, the reaction of homogeneous Pd catalysts in CO/O2 atmosphere has explosion risks, and there is a lack of development of non-Pd-based catalytic systems. .
Using a supported gold catalyst, nitrite compounds and CO are converted into oxalate diester compounds through a CO coupling reaction at room temperature ~ 200°C and 0.1 ~ 2MPa. ZnO is used as a carrier and co-precipitated through precipitation. The gold catalyst is prepared by the method, liquid phase reduction method or gas phase reduction method, which avoids the risk of explosion and improves the reaction selectivity.
Mild reaction conditions, reusable catalysts and high product yields are achieved, which is suitable for industrial production, expands application prospects, and avoids environmental pollution and explosion risks.
Smart Images

Figure CN118724716A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for preparing dimethyl oxalate compounds by using a gold-based catalyst, in particular to a method for preparing dimethyl oxalate by CO-CO coupling under the catalysis of an Au-based catalyst using methyl nitrite and CO as raw materials, and belongs to the technical field of industrial catalysis. Background Art
[0002] As a type of high value-added chemicals, dimethyl oxalate has a wide range of uses: for example, it can be further hydrogenated to ethylene glycol or glycolic acid, as an important monomer for polyethylene glycol and polyglycolic acid; dimethyl oxalate is exchanged with high-carbon alcohols to form oxalate esters with higher added value; dimethyl oxalate is exchanged with ammonia to form oxalamide, which can be used as a high-efficiency slow-release nitrogen fertilizer; it is also a key raw material for the synthesis of N-ethyl-2,3-dioxypiperazine. As an important pharmaceutical chemical intermediate, N-ethyl-2,3-dioxypiperazine is a key intermediate for the preparation of piperacillin (domestic market sales reached 8.1 billion yuan in 2019), cefoperazone (domestic market sales reached 7 billion yuan in 2019), cefoperazone and other types of compounds.
[0003] There are three main technical routes for preparing dimethyl oxalate (Applied Chemical Industry, 2023, 52, 1248-1252): The first route is to use methanol and oxalic acid, with strong acids such as sulfuric acid as catalysts, to produce it through esterification reaction. This technology has problems such as large discharge of three wastes and serious environmental pollution; The second route is to use methanol, carbon monoxide, and oxygen (air) as raw materials, using a homogeneous Pd catalyst, and produce dimethyl oxalate through oxidative carbonylation reaction (J. Org. Chem. 1974, 39, 5, 701–704), but this method requires CO / O 2 Reaction under atmosphere, CO / O 2 The atmosphere has the risk of explosion, which limits the further application of the reaction. The third route is to use methyl nitrite and CO as raw materials, use supported palladium as a catalyst, and generate dimethyl oxalate and NO. NO is recycled to generate methyl nitrite, which is further involved in the reaction as a raw material. This process avoids the reaction in CO / O 2The reaction takes place under the atmosphere, thus avoiding the risk of explosion. In the third technical solution, it mainly relies on regulating the valence state, crystal surface and addition of auxiliary agents of the palladium catalyst, thereby regulating the selectivity of the monocarbonylation or dicarbonylation (CO coupling) of the product to prepare dimethyl carbonate and dimethyl oxalate. For example, the literature (ACS Catal. 2013, 3, 118−122) reports that by regulating the catalyst, more Pd (111) surfaces are exposed to make it have a higher CO coupling selectivity. Chinese patent CN115228502A improves the CO coupling selectivity of the palladium catalyst by regulating the auxiliary agent. As a useful catalytic conversion process, the development of other non-Pd-based catalytic systems is also of great significance. Therefore, the present invention provides a gold-based catalyst and a method for preparing dimethyl oxalate compounds using a gold-based catalyst. Summary of the invention
[0004] The present invention aims to provide a method for preparing oxalic acid diester compounds using a gold-based catalyst, so as to provide different catalytic synthesis schemes and realize the diversification of technical routes for preparing dimethyl oxalate.
[0005] The present invention provides a method for preparing oxalic acid diester compounds using a gold-based catalyst, characterized in that: under the action of a supported gold catalyst, a nitrite compound and CO are reacted by CO coupling reaction for 1 to 24 hours at room temperature to 200° C. and a pressure of 0.1 to 2 MPa to obtain an oxalic acid diester compound. Calculated by gold content, the molar amount of the supported gold catalyst is 0.01 to 5% of the molar amount of the nitrite compound. The reaction is carried out in a kettle reactor or a fixed bed reactor.
[0006] The reaction process is as follows:
[0007] The nitrite compound is at least one of methyl nitrite, ethyl nitrite, propyl nitrite, butyl nitrite or isoamyl nitrite The carrier used in the supported gold catalyst is ZnO or a composite containing ZnO, preferably ZnO; the loading amount of the active component gold is 0.1% to 10%, preferably 1%.
[0008] The molar ratio of CO to nitrite ester compound is 1:1 to 100:1.
[0009] The CO coupling reaction can be carried out in the absence of a solvent or in a reaction solvent, wherein the reaction solvent includes one or more of methanol, ethanol, propanol, butanol, tetrahydrofuran, acetonitrile, dioxane, ethyl acetate, toluene, xylene, and cyclohexane.
[0010] The supported gold catalyst is prepared by precipitation method, coprecipitation method, liquid phase reduction method or gas phase reduction method, and precipitation method and coprecipitation method are preferred.
[0011] The precipitation method and the co-precipitation method are to add the gold source and the ZnO carrier into deionized water, and add a precipitant, and stand the reaction at room temperature for 10-15 hours, wash and dry to obtain a precursor, and then roast the precursor at 200-700°C for 1-5 hours; the precipitant used is at least one of sodium carbonate, ammonium carbonate, sodium hydroxide, potassium hydroxide, and ammonia water, and the co-precipitation method also uses at least one of zinc nitrate, zinc chloride, zinc sulfate, zinc acetate, zinc bromide, and zinc phosphate as a co-precipitant; The liquid phase reduction method is to add the gold source and the ZnO carrier into deionized water, then add the reducing agent, let it stand for reaction at room temperature for 10 to 15 hours, and then wash and dry to obtain; the reducing agent includes at least one of sodium borohydride, potassium borohydride, and hydrazine hydrate; The gas phase reduction method is to add the gold source and ZnO carrier into deionized water, then add sodium carbonate, let it stand for 10-15 hours at room temperature, wash and dry, and then introduce H into the tube furnace. 2 and N 2 The mixed gas is reduced at 100 ~ 500 ℃ for 2 ~ 3h; The gold source includes at least one of chloroauric acid, potassium chloroaurate, and triphenylphosphine gold chloride.
[0012] In summary, the method for catalytically preparing oxalic acid diester compounds provided by the present invention uses CO and nitrite as raw materials, uses a supported gold catalyst, and synthesizes oxalic acid diester compounds through CO coupling. The present invention has the advantages of mild reaction conditions, reusability, high product yield, etc., is suitable for industrial production, and has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 This is a transmission electron microscopy image of the 0.5% Au / ZnO catalyst prepared in Example 1 of the present invention. DETAILED DESCRIPTION
[0014] The present invention is further explained below with reference to specific embodiments.
[0015] Example 1 Preparation of Au / ZnO Catalyst by Precipitation Method Weigh 0.1 g of chloroauric acid (HAuCl 4 ·3H 2O) was added to a 250 mL three-necked flask, and 100 ml of deionized water was added. Then, it was stirred and dissolved at room temperature. Then, 10 g of ZnO carrier was slowly added. After the addition was completed, it was fully stirred. A certain amount of sodium carbonate solution was added. After adjusting the pH to 8, it was stirred for 3 hours and then aged at room temperature for 12 hours. Then, the filter cake was washed with deionized water until neutral, and dried in a 60℃ oven for 12 hours. After drying, it was calcined at 300℃ in a muffle furnace for 3 hours to obtain 0.5% Au / ZnO-300 catalyst (catalyst 1). The same method was used to prepare catalysts with different loading amounts of 1% Au / ZnO-300 (catalyst 2), 2% Au / ZnO-300 (catalyst 3) and 5% Au / ZnO-300 (catalyst 4) and catalysts with different calcination temperatures of 0.5% Au / ZnO-400 (catalyst 5) and 0.5% Au / ZnO-500 (catalyst 6).
[0016] The transmission electron microscopy image of 0.5% Au / ZnO-300 catalyst is shown in Figure 1 , it can be seen that the gold nanoparticles are evenly dispersed on the carrier.
[0017] Example 2 Preparation of Au / ZnO Catalyst by Coprecipitation Method Weigh 0.1 g of chloroauric acid (HAuCl 4 ·3H 2 O) and 36.4 g zinc nitrate (Zn(NO 3 ) 3 6H 2 O) was added to a 500 mL three-necked flask, and 200 ml of deionized water was added. After stirring and dissolving at room temperature, 10 g of ZnO carrier was slowly added and stirred thoroughly. A certain amount of sodium carbonate solution was added, and the pH was adjusted to 8 and stirred for 3 hours. After aging and standing for 12 hours, the filter cake was washed with deionized water until neutral, and then placed in a 60°C oven for 12 hours. After drying, it was calcined at 400°C in a muffle furnace for 3 hours to obtain 0.5% Au / ZnO-400 catalyst (catalyst 7). The same method was used to prepare catalysts with different loading amounts of 1% Au / ZnO-400 (catalyst 8) and 2% Au / ZnO-400 (catalyst 9) and catalysts with different calcination temperatures of 0.5% Au / ZnO-500 (catalyst 10) and 0.5% Au / ZnO-600 (catalyst 11).
[0018] Example 3 Preparation of Au / ZnO Catalyst by Liquid Phase Reduction Weigh 0.1 g of chloroauric acid into a 250 mL three-necked flask, add 100 ml of deionized water, and then stir to dissolve at room temperature. Then slowly add 10 g of ZnO carrier, stir well after adding, and add a certain amount of NaBH 4 After the gold was reduced to gold nanoparticles, the mixture was stirred for 3 hours and then aged for 12 hours. The filter cake was then washed with deionized water until neutral and dried in a 60°C oven for 12 hours to obtain a 0.5% Au / ZnO catalyst (catalyst 12). The same method was used to prepare catalysts with different loading amounts of 1% Au / ZnO (catalyst 13) and 2% Au / ZnO (catalyst 14).
[0019] Example 4 Preparation of Au / ZnO Catalyst by Gas Phase Reduction Weigh 0.1 g of chloroauric acid and add it to a 250 mL three-necked flask, add 100 ml of deionized water, and then stir and dissolve at room temperature. Then slowly add 10 g of ZnO carrier, stir thoroughly after the addition is completed, add a certain amount of sodium carbonate solution, adjust the pH to 8, continue stirring for 3 hours, and age and stand for 12 hours; then wash the filter cake with deionized water until it is neutral, put it in a 60 ° C oven and dry it for 12 hours. After drying, pass H into the tube furnace. 2 and N 2 Mixed gas (H 2 The 0.5% Au / ZnO catalyst (catalyst 15) was obtained by reduction at 300 °C for 3 h.
[0020] Application Example 1 3 mL of methanol was added to a 50 mL autoclave, and the catalysts prepared in Examples 1-4 were added respectively (the catalyst was 0.5% mol of nitrite, calculated as gold). After about 3 mmol of methyl nitrite was added, 2 MPa of CO was added, and the reaction was carried out at 60°C for 12 h. After the reaction was completed, the reaction liquid was centrifuged and the product dimethyl oxalate was quantitatively analyzed by gas chromatography. The results are shown in Table 1 below.
[0021] Table 1 Comparison of conversion and selectivity of Example 1-4 catalyzing methyl nitrite to synthesize dimethyl oxalate
[0022] It can be seen that the conversion rate and selectivity of the catalyst prepared by the present invention in synthesizing dimethyl oxalate from methyl nitrite are both at a relatively high level.
[0023] Application Example 2 3 mL of ethanol was added to a 50 mL autoclave, and the Au / ZnO catalysts prepared in Examples 1-4 were added respectively (the catalyst was 0.5% mol of nitrite, calculated as gold). After about 3 mmol of ethyl nitrite was added, 2 MPa of CO was continuously added, and the reaction was carried out at 60 °C for 12 h. After the reaction was completed, the reaction liquid was centrifuged, and the product dimethyl oxalate was quantitatively analyzed by gas chromatography, and qualitatively analyzed by GC-MS. The conversion rate of ethyl nitrite was 96%, and the selectivity of diethyl oxalate was 98%.
[0024] .
[0025] Application Example 3 3 mL of propanol was added to a 50 mL autoclave, and the Au / ZnO catalysts prepared in Examples 1-4 were added (the catalyst was 0.5% mol of nitrite, calculated as gold). About 3 mmol of propyl nitrite was added, 2 MPa of CO was charged, and the reaction was carried out at 60°C for 12 h. After the reaction was completed, the reaction liquid was centrifuged, and the product dimethyl oxalate was quantitatively analyzed by gas chromatography and qualitatively analyzed by GC-MS. The conversion rate of propyl nitrite was 95%, and the selectivity of dipropyl oxalate was 93%.
[0026] .
[0027] Application Example 4 3 mL of butanol was added to a 50 mL autoclave, and the Au / ZnO catalysts prepared in Examples 1-4 were added (the catalyst was 0.5% mol of nitrite, calculated as gold). About 3 mmol of butyl nitrite was added, 2 MPa of CO was charged, and the reaction was carried out at 60°C for 12 h. After the reaction was completed, the reaction solution was centrifuged, and the product dimethyl oxalate was quantitatively analyzed by gas chromatography and qualitatively analyzed by GC-MS. The conversion rate of butyl nitrite was 92%, and the selectivity of dibutyl oxalate was 85%.
[0028] .
[0029] Comparative application example 1 3 mL of methanol was added to a 50 mL autoclave, and 100 mg of the prepared catalyst 1 was added. 2 MPaCO was charged and the reaction was carried out at 60°C for 12 h. After the reaction was completed, the gas chromatography analysis did not detect the formation of the target product dimethyl oxalate. This indicates that the product in the application example was generated through (methyl) nitrite, not methanol.
[0030] In summary, the method for catalytically preparing oxalic acid diester compounds provided by the present invention uses CO and nitrite as raw materials, uses a supported gold catalyst, and synthesizes oxalic acid diester compounds through CO coupling. The present invention has the advantages of mild reaction conditions, reusability, high product yield, etc., is suitable for industrial production, and has broad application prospects.
[0031] It should be understood that the above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable people familiar with the technology to understand the content of the present invention and implement it accordingly, and they cannot be used to limit the protection scope of the present invention. Any equivalent changes or modifications made according to the spirit of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for preparing oxalic acid diester compounds using a gold-based catalyst, characterized in that: Under the action of a supported gold catalyst, nitrite compounds react with CO at room temperature to 60°C and a pressure of 0.1 to 2 MPa for 1 to 24 h to obtain oxalic acid diester compounds.
2. A method for preparing oxalic acid diester compounds using a gold-based catalyst as claimed in claim 1, characterized in that: The nitrite ester compound is at least one of methyl nitrite, ethyl nitrite, propyl nitrite, or butyl nitrite, and the corresponding oxalate diester compounds are dimethyl oxalate, diethyl oxalate, dipropyl oxalate, or dibutyl oxalate.
3. A method for preparing oxalic acid diester compounds using a gold-based catalyst as claimed in claim 1, characterized in that: The molar ratio of CO to nitrite ester compound is 1:1~100:
1.
4. A method for preparing oxalic acid diester compounds using a gold-based catalyst as claimed in claim 1, characterized in that: The CO coupling reaction can be carried out in the absence of a solvent or in the presence of a solvent, wherein the solvent is one or more of methanol, ethanol, propanol, butanol, tetrahydrofuran, acetonitrile, dioxane, ethyl acetate, toluene, xylene, and cyclohexane.
5. A method for preparing oxalic acid diester compounds using a gold-based catalyst as claimed in claim 1, characterized in that: Calculated based on the gold content, the molar amount of the supported gold catalyst is 0.01% to 5% of the molar amount of the nitrite compound.
6. A method for preparing oxalic acid diester compounds using a gold-based catalyst as claimed in claim 1, characterized in that: The supported gold catalyst is prepared by a precipitation method, a coprecipitation method, a liquid phase reduction method or a gas phase reduction method. Precipitation method: Add the gold source and ZnO carrier into deionized water, add a precipitant, and let it stand for 10-15 hours at room temperature to react. Wash and dry to obtain a precursor, and then calcine the precursor at 200-700°C for 1-5 hours. The precipitant used is at least one of sodium carbonate, ammonium carbonate, sodium hydroxide, potassium hydroxide, and ammonia water. Co-precipitation method: add the gold source and ZnO carrier into deionized water, add the precipitant and co-precipitant, let it stand for reaction at room temperature for 10-15 hours, wash and dry to obtain a precursor, and then roast the precursor at 200-700°C for 1-5 hours; the precipitant is at least one of sodium carbonate, ammonium carbonate, sodium hydroxide, potassium hydroxide, and ammonia water; the co-precipitant is at least one of zinc nitrate, zinc chloride, zinc sulfate, zinc acetate, zinc bromide, and zinc phosphate; Liquid phase reduction method: add the gold source and ZnO carrier into deionized water, then add the reducing agent, let it stand for reaction at room temperature for 10-15 hours, wash and dry to obtain; the reducing agent is at least one of sodium borohydride, potassium borohydride and hydrazine hydrate; Gas phase reduction method: Add the gold source and ZnO carrier into deionized water, then add sodium carbonate, let it stand at room temperature for 10-15 hours, wash and dry, then introduce a mixed gas of H2 and N2 into a tubular furnace and reduce it at 100-500℃ for 2-3 hours.
7. A method for preparing oxalic acid diester compounds using a gold-based catalyst as claimed in claim 6, characterized in that: The gold source is at least one of chloroauric acid, potassium chloroaurate, and triphenylphosphine gold chloride.
8. A method for preparing oxalic acid diester compounds using a gold-based catalyst as claimed in claim 6, characterized in that: The loading amount of active component gold in the supported gold catalyst is 0.1% to 10%.
9. A method for preparing oxalic acid diester compounds using a gold-based catalyst as claimed in claim 1, characterized in that: The reaction is carried out in a tank reactor or a fixed bed reactor.