Anti-corrosion coating material for marine steel structure, and preparation process and equipment of anti-corrosion coating material
By using a combination of lignosulfonate embedded healing agent and polyurea prepolymer in the marine steel structure coating, combined with the heating tube and fin structure of the thermal insulation mixer, the problem of uneven temperature of the coating material is solved. It achieves self-healing and corrosion resistance, extending the service life of the steel structure.
Patent Information
- Application Number
- CN202410994358.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-01-31
- Filing Date
- 2024-07-24
- Publication Date
- 2024-10-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
During the preparation process of anti-corrosion coating materials for marine steel structures, there is uneven material temperature, which affects the mixing effect of the materials.
Microcapsules embedded with lignin sulfonate healing agent are combined with polyurea prepolymer, and the heating tube and fin structure in the thermal mixer are used to achieve uniform heating of the raw material temperature, thus overcoming the problem of temperature unevenness.
The self-healing performance of the anti-corrosion coating material of the marine steel structure is realized, the service life of the steel structure is extended, and the corrosion resistance and aging resistance of the coating are improved.
Smart Images

Figure CN118725706A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of anti-corrosion coatings, and in particular to an anti-corrosion coating material for marine steel structures, and a preparation process and equipment thereof. Background Art
[0002] Marine steel structures include offshore wind turbines, cross-sea bridges, offshore oil platforms and port terminals. These steel structures are exposed to the marine atmosphere or immersed in seawater for a long time, creating conditions for the occurrence and development of corrosion.
[0003] In the prior art, the hardness and color of polyurea, an anti-corrosion coating for marine steel structures, can be freely adjusted according to demand. In addition, polyurea has its own strength that is not dependent on the substrate, that is, polyurea can be used as a coating as well as a lining. However, when affected by external forces such as squeezing and friction of marine organisms and marine garbage, cracks will appear in the polyurea coating, and then seawater will penetrate and corrode the steel structure. At present, in the market, microcapsules encapsulating the healing agent are added to the polyurea coating, which has obvious corrosion resistance compared to the polyurea coating without adding microcapsules, and significantly extends the service life of the steel sheet. On the basis of the characteristics of good flexibility, high strength, corrosion resistance and aging resistance of the polyurea coating itself, the polyurea coating is endowed with self-healing properties, which better plays the advantages of the polyurea coating. However, during the preparation process of the above-mentioned materials, the raw materials need to be heated and stirred. During the stirring process, the raw material temperature near the heating tube on the inner wall of the container is higher than that in the middle of the container, that is, there is an uneven raw material temperature, which will affect the mixing effect of the raw materials.
[0004] Therefore, we need an anti-corrosion coating material for marine steel structures, its preparation process and equipment, which can be used to solve the problem of uneven material temperature in the preparation process of the existing anti-corrosion coating material for marine steel structures. The anti-corrosion coating material for marine steel structures can be prepared and the temperature of the raw materials inside the container can be uniform during the mixing process. Summary of the invention
[0005] The purpose of the present invention is to provide an anti-corrosion coating material for marine steel structures, its preparation process and equipment, so as to solve the problem of uneven material temperature during the preparation process of the existing anti-corrosion coating material for marine steel structures mentioned in the above background technology, and to achieve uniform temperature of raw materials inside the container during the process of mixing materials in the preparation of the anti-corrosion coating material for marine steel structures.
[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solution: an anti-corrosion coating material for marine steel structures, the anti-corrosion coating material comprising the following components by weight: 1 to 10 parts of lignin sulfonate-embedded microcapsules of a healing agent; 10 to 90 parts of a polyurea prepolymer; and 20 to 100 parts of a mixture of an amino-terminated polyether and a hindered amine chain extender.
[0007] A process for preparing an anti-corrosion coating material for marine steel structures, the preparation process comprising the following steps:
[0008] Mixing 10 to 100 parts by weight of a lignin sulfonate aqueous solution with 1 to 50 parts by weight of a microcapsule healing agent formed of an aromatic isocyanate and an aliphatic isocyanate, emulsifying, and drying at room temperature to obtain microcapsules of the lignin sulfonate-embedded healing agent;
[0009] The amino-terminated polyether and aliphatic isocyanate are mixed in a molar ratio of 0.5:1 to 2:1, the temperature is raised to 20°C to 100°C, and the mixture is stirred in a heat-insulating mixer for 10 minutes to 24 hours to obtain a polyurea prepolymer;
[0010] A mixture of lignin sulfonate-embedded healing agent microcapsules, amino-terminated polyether and hindered amine chain extender is added to a polyurea prepolymer and reacted at room temperature for 10 minutes to 4 hours to obtain a lignin sulfonate-dispersed self-healing polyurea coating.
[0011] A device for preparing anti-corrosion coating materials for marine steel structures, the thermal insulation mixer comprising a cover plate, a motor assembly is mounted on the surface of the cover plate, a sleeve is fixed to the bottom end of the shaft of the motor assembly, an assembling block is plugged into the bottom end of the sleeve, a slot is provided on the surface of the assembling block, a limit block is plugged into the inside of the slot, the limit block passes through the sleeve, a central paddle board is fixed to the bottom end of the assembling block, a battery is mounted inside the central paddle board, blades are fixed on both sides of the central paddle board, the top surface and the bottom surface of the blade are slidably connected with a traction arm, a heating tube is mounted inside the traction arm, a fin is mounted on the top surface of the traction arm, an auxiliary paddle board is fixed to the surface of the central paddle board, and a knife plate is fixed to the surface of the auxiliary paddle board.
[0012] A through hole is provided in the center of the top surface of the cover plate, a bearing is fixed inside the through hole, the bearing sleeve is arranged on the shaft body of the motor assembly, the sleeve is a cylindrical structure, the inner ring groove of the sleeve is a square groove structure, the assembling block is a square block, the missing groove is an annular groove, the center paddle board is a square plate structure, the assembling block is centered on the top surface of the center paddle board, a reserved groove is provided on the outer ring surface of the sleeve, a socket is provided on the surface of the reserved groove, two sockets are provided, the two sockets are symmetrically distributed about the sleeve, and the limit plug is movably inserted in the socket.
[0013] Preferably, a notch is provided at one end of the limit block extending into the sleeve slot, an elastic band is fixed on the surface of the notch, and the two ends of the elastic band are respectively fixed on two parallel side walls of the socket. When one end of the limit block is inserted into the slot, the elastic band is in a stretched deformation state, and the other end of the limit block is provided with an inclined surface, the inclined surface faces upward, the length of the limit block is greater than the depth of the socket, a retaining ring is provided inside the reserved groove, a rubber ring is fixed on the inner ring surface of the retaining ring, the rubber ring is clamped between the retaining ring and the reserved groove, and a pick-out groove is provided on the outer ring surface of the retaining ring, the pick-out groove is an annular groove with a right-angled trapezoidal cross-section, and the inclined surface of the right-angled trapezoid is at the bottom.
[0014] Preferably, a battery slot is provided on the bottom surface of the central paddle board, a rubber pad is fixed on the top surface of the battery slot, the rubber pad is in the form of an annular plate, the battery is inserted into the battery slot, a sealing plate is plugged into the bottom end of the battery slot, the sealing plate is in the form of a "convex" shape, the bottom surface size of the sealing plate is equal to the bottom surface size of the central paddle board, the bottom plate of the sealing plate is fixed to the bottom surface of the central paddle board by screws, and the rubber pad is squeezed by the battery slot to produce elastic deformation.
[0015] Preferably, the top surface of the battery slot is provided with an air supply hole, the air supply hole passes through the sleeve, the assembly block and the shaft of the motor assembly, the top side wall of the air supply hole is provided with a plurality of air dispersion holes, the perforated side wall is provided with a plurality of exhaust holes, the exhaust holes are "L"-shaped holes, the exhaust holes pass through the top surface of the cover plate, the top surface of the cover plate is fixed with a limit frame, the limit frame is a "T"-shaped circular ring plate, a mesh ring and a dust cover are fixed between the bottom surface of the top plate of the limit frame and the top surface of the cover plate, and the mesh ring is sleeved on the outside of the dust cover.
[0016] Preferably, the top surface and the bottom surface of the blade are both provided with a storage groove, the long side length of the storage groove is smaller than the long side length of the blade, the surface of the storage groove close to the center paddle plate is provided with an embedding groove, an electric push rod is fixed inside the embedding groove, the piston rod of the electric push rod is fixed to the surface of the traction arm, an installation groove is provided at one end of the traction arm away from the electric push rod, the heating tube is movably inserted in the installation groove, an assembling block is fixed at one end of the traction arm, the assembling block is movably inserted in the assembling groove, the assembling groove is provided on the surface of the side sealing plate, the assembling block is fixed in the assembling groove by screw two, one end of the heating tube is inserted in the buckle groove, and the buckle groove is provided on the surface of the side sealing plate.
[0017] Preferably, a pad strip is fixed to the bottom surface of the mounting groove, the heating tube is overlapped on the pad strip, a plurality of sockets are provided on the top surface of the traction arm, the sockets are connected to the mounting groove, a block is plugged into the inside of the socket, the bottom surface of the block is an arc surface, the arc surface is overlapped on the heating tube, a notch is provided on the surface of the block, the fin is fixed to the top surface of the block, blades are provided on both sides of the fin, a pressure relief tube is plugged into the top surface of the bottom end of the notch, the pressure relief tube passes through the block and the fin, and the pressure relief tube is an inverted "U" shaped tube.
[0018] Preferably, an extension plate is fixed on the surface of the side sealing plate, the extension plate is slidably connected in the side groove, the side groove is opened on the surface of the blade, two extension plates are provided, and the two extension plates are symmetrically distributed about the blade.
[0019] Preferably, the heating tube and the electric push rod are both connected to the battery via wires.
[0020] Compared with the prior art, the present invention has the following beneficial effects:
[0021] The present invention proposes an anti-corrosion coating material for marine steel structures, a preparation process and equipment thereof. A self-healing polyurea coating is obtained by adding microcapsules of lignin sulfonate-embedded healing agents into a polyurea coating. The preparation of the self-healing polyurea coating expands the application of lignin in polymer materials and overcomes the problem that the polyurea coating is difficult to repair after stress damage. The coating can be better applied to the anti-corrosion of steel structures and the field of material surface protection. It has a good prospect for application as a marine steel structure material. A slidable traction arm is installed on the blades, and a heating tube is installed inside the traction arm. That is, during the process of the blades stirring the raw materials, the raw materials are heated and insulated by the heating tube, and the heating tube moves with the traction arm, thereby increasing the heating range of the heating tube. The fins on the top of the traction arm not only increase the contact area between the raw materials and the heating structure, but also the fins can break up the agglomerated materials. The problem of uneven material temperature in the preparation process of the existing anti-corrosion coating materials for marine steel structures is further solved. The anti-corrosion coating materials for marine steel structures can be prepared and the temperature of the raw materials inside the container can be uniform during the mixing of materials. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the structure of the present invention;
[0023] Figure 2 It is a schematic diagram of the bottom structure of the present invention;
[0024] Figure 3 for Figure 2 A schematic diagram of the structure enlargement in the middle;
[0025] Figure 4 It is a top view of the structure of the present invention;
[0026] Figure 5 for Figure 4 Structural cross-section at AA in the middle;
[0027] Figure 6 for Figure 5 A magnified schematic diagram of the structure at B in the middle;
[0028] Figure 7 for Figure 5 A magnified schematic diagram of the structure at C in the middle;
[0029] Figure 8 for Figure 6 A magnified schematic diagram of the structure at D in the middle;
[0030] Fig. 9 This is a schematic diagram of the limit plug structure of the present invention;
[0031] Fig.10 This is a schematic diagram of the central paddle board structure of the present invention;
[0032] Fig.11 This is a schematic diagram of the structure of the extension plate after extension of the present invention;
[0033] Fig.12 It is a schematic diagram of the connection structure of the traction arm and the side sealing plate of the present invention;
[0034] Fig.13 for Fig.12 Top view of the structure;
[0035] Fig.14 for Fig.13 Structural cross-section at the middle BB;
[0036] Fig.15 for Fig.14 The enlarged schematic diagram of the structure at E in the middle;
[0037] Fig.16 It is a schematic diagram of the connection structure of the stopper and the fin of the present invention;
[0038] Fig.17 It is a schematic diagram of the connection structure of the extension plate and the side sealing plate of the present invention;
[0039] Fig.18 for Fig.17 A magnified schematic diagram of the structure at F in the middle;
[0040] Fig.19 This is a schematic diagram of the blade structure of the present invention;
[0041] Fig. 20 for Fig.19 Enlarged schematic diagram of the structure at G in the middle.
[0042] In the figure: cover plate 1, perforation 2, motor assembly 3, bearing 4, sleeve 5, assembly block 6, center paddle 7, reserved slot 8, socket 9, limit plug 10, missing slot 11, elastic band 12, card slot 13, inclined surface 14, retaining ring 15, rubber clamp 16, pick-up slot 17, battery slot 18, rubber pad 19, sealing plate 20, screw 1 21, air delivery hole 22, air diffusion hole 23, exhaust hole 24, limit frame 25, Mesh collar 26, dust cover 27, battery 28, blade 29, storage slot 30, embedding slot 31, electric push rod 32, traction arm 33, installation slot 34, heating tube 35, cushion strip 36, assembly block 37, assembly slot 38, side sealing plate 39, screw 40, jack 41, block 42, fin 43, pressure relief capillary 44, extension plate 45, side slot 46, auxiliary paddle plate 47, knife plate 48, buckle slot 49. DETAILED DESCRIPTION
[0043] In order to make the purpose and technical solution of the present invention clearly and completely described, and the advantages more clearly understood, the embodiments of the present invention are further described in detail with reference to the accompanying drawings. It should be understood that the specific embodiments described herein are part of the embodiments of the present invention, rather than all of the embodiments, and are only used to explain the embodiments of the present invention, and are not used to limit the embodiments of the present invention. All other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0044] Embodiment 1
[0045] The invention provides a technical solution: an anti-corrosion coating material for marine steel structures, wherein the anti-corrosion coating material comprises the following components obtained by reacting in parts by mass: 1 to 10 parts of microcapsules of lignin sulfonate-embedded healing agents; 10 to 90 parts of polyurea prepolymers; and 20 to 100 parts of a mixed solution of amino-terminated polyethers and hindered amine chain extenders; a self-healing polyurea coating is obtained by adding microcapsules of lignin sulfonate-embedded healing agents into the polyurea coating. The preparation of the self-healing polyurea coating expands the application of lignin in polymer materials and overcomes the problem that the polyurea coating is difficult to repair after stress damage, and can be better applied to the anti-corrosion of steel structures and can be applied to the field of material surface protection. The application of the self-healing polyurea coating as a marine steel structure material has a good prospect.
[0046] Embodiment 2
[0047] Refer to the attached Figures 1 to 4 Based on Example 1, a preparation process of an anti-corrosion coating material for marine steel structures is proposed, and the preparation process comprises the following steps:
[0048] Mixing 10 to 100 parts by weight of a lignin sulfonate aqueous solution with 1 to 50 parts by weight of a microcapsule healing agent formed of an aromatic isocyanate and an aliphatic isocyanate, emulsifying, and drying at room temperature to obtain microcapsules of the lignin sulfonate-embedded healing agent;
[0049] The amino-terminated polyether and aliphatic isocyanate are mixed in a molar ratio of 0.5:1 to 2:1, the temperature is raised to 20°C to 100°C, and the mixture is stirred in a heat-insulating mixer for 10 minutes to 24 hours to obtain a polyurea prepolymer;
[0050] A mixture of lignin sulfonate-embedded healing agent microcapsules, amino-terminated polyether and hindered amine chain extender is added to a polyurea prepolymer and reacted at room temperature for 10 minutes to 4 hours to obtain a lignin sulfonate-dispersed self-healing polyurea coating.
[0051] The heat preservation mixer comprises a cover plate 1, a motor assembly 3 is mounted on the surface of the cover plate 1, a sleeve 5 is fixed at the bottom end of the shaft of the motor assembly 3, an assembling block 6 is inserted at the bottom end of the sleeve 5, a slot 13 is provided on the surface of the assembling block 6, a limit block 10 is inserted inside the slot 13, the limit block 10 passes through the sleeve 5, a central paddle board 7 is fixed at the bottom end of the assembling block 6, a battery 28 is mounted inside the central paddle board 7, blades 29 are fixed on both sides of the central paddle board 7, the top surface of the blade 29 and the bottom surface of the blade 29 are slidably connected with a traction arm 33, a heating tube 35 is mounted inside the traction arm 33, a fin 43 is mounted on the top surface of the traction arm 33, and an auxiliary paddle board 47 is fixed on the surface of the central paddle board 7, the auxiliary paddle board 47 A knife plate 48 is fixed on the surface; a slidable traction arm 33 is installed on the blade 29, and a heating tube 35 is installed inside the traction arm 33, that is, when the blade 29 stirs the raw material, the raw material is heated and kept warm by the heating tube 35, and the heating tube 35 moves with the traction arm 33, thereby increasing the heating range of the heating tube 35, and the fin 43 on the top of the traction arm 33 not only increases the contact area between the raw material and the heating structure, but also the fin 43 can break the agglomerated material; it further solves the problem of uneven material temperature in the preparation process of the existing anti-corrosion coating material for marine steel structure, and can prepare the anti-corrosion coating material for marine steel structure. In the process of mixing materials, the temperature of the raw materials inside the container is uniform.
[0052] Embodiment 3
[0053] Refer to the attached Figure 5 and Figure 6On the basis of the second embodiment, in order to fix the central paddle plate 7 on the sleeve 5, a through hole 2 is opened in the center of the top surface of the cover plate 1, and a bearing 4 is fixed inside the through hole 2. The bearing 4 is sleeved on the shaft body of the motor assembly 3. The sleeve 5 has a cylindrical structure, and the inner ring groove of the sleeve 5 has a square groove structure. The assembling block 6 is a square block, and the notch 11 is an annular groove. The central paddle plate 7 has a square plate-shaped structure, and the assembling block 6 is centered on the top surface of the central paddle plate 7. A reserved groove 8 is opened on the outer ring surface of the sleeve 5, and a socket 9 is opened on the surface of the reserved groove 8. There are two sockets 9, and the two sockets 9 are symmetrically distributed about the sleeve 5. The limiting plug 10 is movably plugged into the socket 9; a notch 11 is opened at one end of the limiting plug 10 extending into the notch of the sleeve 5, and a notch 11 is fixed on the surface of the notch 11. An elastic band 12, the two ends of the elastic band 12 are respectively fixed on two parallel side walls of the socket 9. When one end of the limit plug 10 is inserted into the slot 13, the elastic band 12 is in a stretched deformation state. The other end of the limit plug 10 is provided with a slope 14, and the slope 14 faces upward. The length of the limit plug 10 is greater than the depth of the socket 9. A retaining ring 15 is provided inside the reserved groove 8. A rubber ring is fixed on the inner ring surface of the retaining ring 15. The rubber ring is clamped between the retaining ring 15 and the reserved groove 8. A pick-up groove 17 is provided on the outer ring surface of the retaining ring 15. The pick-up groove 17 is an annular groove with a right-angled trapezoidal cross-section. The slope of the right-angled trapezoid is at the bottom. A rubber clamp 16 is fixed between the top surface of the retaining ring 15 and the top surface of the reserved groove 8. The rubber clamp 16 is an annular plate structure.
[0054] When the central paddle board 7 is suspended under the sleeve 5 by the assembling block 6, the retaining ring 15 pushes the limiting plug-in block 10 to be inserted into the card slot 13. At this time, the assembling block 6 will not detach from the slot body of the sleeve 5. The reason why the assembling block 6 and the slot body of the sleeve 5 are both set to be square is to enable the motor assembly 3 to drive the sleeve 5 to drive the central paddle board 7 to rotate synchronously. Since the central paddle board 7 is a square plate, when the central paddle board 7 is driven to rotate, it also stirs the raw materials in the container, and during the stirring process of the raw materials by the auxiliary paddle board 47, the knife plate 48 cuts the agglomerated raw materials close to the central paddle board 7 into pieces; the central paddle board 7 is a detachable structure under the sleeve 5. When the central paddle board 7 needs to be removed, the fingers are pinched into the picking groove 17, and the retaining ring 15 is pushed upward to move along the reserved groove 8 Slide until the retaining ring 15 and the limiting plug block 10 are misaligned. At this time, the tensioned elastic band 12 rebounds, driving the limiting plug block 10 to move toward the reserved groove 8, and one end of the limiting plug block 10 is pulled out of the slot 13. There is no longer any limit between the assembling block 6 and the sleeve 5, and the central paddle board 7 is pulled out to remove the assembling block 6 from the sleeve 5; the rubber ring at the inner ring mouth of the retaining ring 15 increases the friction between the retaining ring 15 and the reserved groove 8 to ensure that when the retaining ring 15 squeezes the limiting plug block 10, the retaining ring 15 is prevented from bumping; it further solves the problem of uneven material temperature in the preparation process of the existing anti-corrosion coating material for marine steel structure, and can prepare the anti-corrosion coating material for marine steel structure and achieve uniform raw material temperature inside the container during the mixing process.
[0055] Embodiment 4
[0056] Refer to the attached Figure 8 On the basis of the third embodiment, in order to realize the heat dissipation generated by the battery 28, a battery slot 18 is provided on the bottom surface of the central paddle board 7, and a rubber pad 19 is fixed on the top surface of the battery slot 18. The rubber pad 19 is an annular plate. The battery 28 is inserted into the battery slot 18. A sealing plate 20 is plugged into the bottom end of the battery slot 18. The sealing plate 20 is a "convex" shaped plate. The bottom surface size of the sealing plate 20 is equal to the bottom surface size of the central paddle board 7. The bottom plate of the sealing plate 20 is fixed to the bottom surface of the central paddle board 7 by a screw 21. The rubber pad 19 is squeezed by the battery slot 18 to produce elastic deformation; The top surface of the battery slot 18 is provided with an air supply hole 22, which passes through the sleeve 5, the assembly block 6 and the shaft of the motor assembly 3. The top side wall of the air supply hole 22 is provided with a plurality of air diffusion holes 23. The side wall of the perforation 2 is provided with a plurality of exhaust holes 24, and the exhaust holes 24 are "L"-shaped holes. The exhaust holes 24 pass through the top surface of the cover plate 1. A limiting frame 25 is fixed on the top surface of the cover plate 1. The limiting frame 25 is a "T"-shaped circular ring plate. A mesh ring 26 and a dust cover 27 are fixed between the bottom surface of the top plate of the limiting frame 25 and the top surface of the cover plate 1, and the mesh ring 26 is sleeved on the outside of the dust cover 27.
[0057] The heat generated by the battery 28 working for a long time rises through the air transmission hole 22 and is dissipated only through the air dissipation hole 23, and the dissipated hot air is discharged through the exhaust hole 24 to avoid heat accumulation inside the battery slot 18, and the limit frame 25, the mesh ring 26 and the dust cover 27 are protected above the exhaust hole 24 to prevent foreign objects and debris from entering the container below the cover plate 1 through the exhaust hole 24; the mesh ring 26 is sleeved on the outside of the dust cover 27 because the hot air will support the dust cover 27 when it is dissipated to the outside. After the mesh ring 26 is sleeved on the outside of the dust cover 27, the dust cover 27 will not have the problem of expansion and tearing; it further solves the problem of uneven material temperature in the preparation process of the existing anti-corrosion coating material for marine steel structure, and can prepare the anti-corrosion coating material for marine steel structure and achieve uniform raw material temperature inside the container during the mixing process.
[0058] Embodiment 5
[0059] On the basis of the fourth embodiment, in order to adjust the heating laying area of the heating tube 35, a storage groove 30 is provided on the top surface and the bottom surface of the blade 29. The long side length of the storage groove 30 is less than the long side length of the blade 29. The surface of the storage groove 30 close to the center paddle plate 7 is provided with an embedding groove 31. An electric push rod 32 is fixed inside the embedding groove 31. The piston rod of the electric push rod 32 is fixed to the surface of the traction arm 33. The traction arm 33 has an installation groove 34 at one end away from the electric push rod 32. The heating tube 35 is movably inserted in the installation groove 34. An assembling block 37 is fixed at one end of the traction arm 33. The assembling block 37 is movably inserted in the assembling groove 38. The assembling groove 38 is provided on the surface of the side sealing plate 39. The assembling block 37 is fixed in the assembling groove 38 by screws 40. One end of the heating tube 35 is inserted in the buckle groove 49. The buckle groove 49 is provided on the surface of the side sealing plate 39. Installation A pad strip 36 is fixed to the bottom surface of the groove 34, and the heating tube 35 is overlapped on the pad strip 36. A plurality of plug holes 41 are provided on the top surface of the traction arm 33, and the plug holes 41 are connected to the installation groove 34. A stopper 42 is inserted into the inside of the plug hole 41. The bottom surface of the stopper 42 is an arc surface, and the arc surface overlaps the heating tube 35. A notch is provided on the surface of the stopper 42. The fin 43 is fixed to the top surface of the stopper 42. Both sides of the fin 43 are provided with a blade, and the top surface of the bottom end of the notch is A pressure relief capillary 44 is inserted, and the pressure relief capillary 44 passes through the block 42 and the fin 43, and the pressure relief capillary 44 is an inverted "U"-shaped tube; an extension plate 45 is fixed to the surface of the side sealing plate 39, and the extension plate 45 is slidably connected in the side groove 46, and the side groove 46 is opened on the surface of the blade 29. There are two extension plates 45, and the two extension plates 45 are symmetrically distributed about the blade 29; the heating tube 35 and the electric push rod 32 are connected to the battery 28 through wires.
[0060] When the central paddle plate 7 is driven by the motor assembly 3 to stir the raw materials, the switch of the heating tube 35 is triggered. After the heating tube 35 is heated, it heats and keeps the raw materials on the upper and lower sides of the blade 29 warm. Since the radiation area of the blade 29 is circular after the rotation of the central paddle plate 7, the range of the raw materials heated by the heating tube 35 becomes larger; when the switch of the electric push rod 32 is triggered, the piston rod of the preset electric push rod 32 reciprocates and retracts. During this process, the traction arm 33 is pulled by the electric push rod 32 to slide back and forth along the storage groove 30, and the radiation area of the heating tube 35 is expanded in the horizontal direction. The hot air inside the installation groove 34 is dissipated through the pressure relief capillary 44, and the hot air heats the fins 43. The fins 43 are inserted into the raw materials, which increases the contact area between the heat generated by the heating tube 35 and the raw materials, and the dissipated hot air also heats and keeps the raw materials warm, and the blades on both sides of the fins 43 can achieve the effect of chopping the agglomerated raw materials, so that the fins 43 can not only achieve The mounting groove 34 relieves pressure and increases the heating contact area between the heating tube 35 and the raw material. The fins 43 can also break up the agglomerated materials. The fins 43 have multiple uses. When the heating tube 35 is damaged, the heating tube 35 can be replaced separately. After loosening the screw 40 and disengaging it from the assembly groove 38, the side sealing plate 39 is pulled out from the end of the storage groove 30. At this time, one end of the heating tube 35 is exposed, and the heating tube 35 can be pulled out from the mounting groove 34. It should be noted that the wire between the heating tube 35 and the battery 28 is reserved with sufficient length in the mounting groove 34, that is, when the heating tube 35 is pulled out from the mounting groove 34, the connector at the end of the wire can be manually unplugged from the interface of the heating tube 35. This further solves the problem of uneven material temperature in the preparation process of the existing anti-corrosion coating material for marine steel structures. The anti-corrosion coating material for marine steel structures can be prepared and the temperature of the raw materials inside the container can be uniform during the mixing process of the materials.
[0061] During actual use, when the central paddle board 7 is suspended under the sleeve 5 through the assembling block 6, the retaining ring 15 pushes the limiting plug block 10 to be inserted into the card slot 13. At this time, the assembling block 6 will not detach from the slot body of the sleeve 5. The reason why the assembling block 6 and the slot body of the sleeve 5 are both set to be square is to enable the motor assembly 3 to drive the sleeve 5 to drive the central paddle board 7 to rotate synchronously. Since the central paddle board 7 is a square plate, when the central paddle board 7 is driven to rotate, it also stirs the raw materials in the container, and during the stirring process of the auxiliary paddle board 47 on the raw materials, the knife plate 48 will chop the agglomerated raw materials close to the central paddle board 7; the central paddle board 7 is a detachable structure under the sleeve 5. When the central paddle board 7 needs to be removed, the fingers are pinched in the picking groove 17, and the retaining ring 15 is pushed upward along the The retaining ring 15 slides up along the reserved groove 8 until the retaining ring 15 and the limiting plug 10 are misaligned. At this time, the tensioned elastic band 12 rebounds, driving the limiting plug 10 to move toward the reserved groove 8, and one end of the limiting plug 10 is pulled out of the card slot 13. There is no limit between the assembly block 6 and the sleeve 5, and the central paddle plate 7 is pulled out to remove the assembly block 6 from the sleeve 5; the rubber ring at the inner ring mouth of the retaining ring 15 increases the friction between the retaining ring 15 and the reserved groove 8 to ensure that when the retaining ring 15 squeezes the limiting plug 10, the retaining ring 15 is prevented from bumping; the heat generated by the battery 28 working for a long time rises through the air transmission hole 22 and only dissipates through the air dissipation hole 23, and the dissipated hot air is discharged through the exhaust hole 24 to avoid the internal temperature accumulation of the battery slot 18, and the limit frame 25 and the mesh ring 26 The dust cover 27 is protected above the exhaust hole 24 to prevent foreign objects and debris from entering the container below the cover plate 1 through the exhaust hole 24; the mesh ring 26 is sleeved on the outside of the dust cover 27 because the hot air will support the dust cover 27 when it dissipates to the outside. After the mesh ring 26 is sleeved on the outside of the dust cover 27, the dust cover 27 will not have the problem of expansion and tearing; during the process of the central paddle plate 7 being driven by the motor assembly 3 to stir the raw materials, the switch of the heating tube 35 is triggered. After the heating tube 35 is heated, the raw materials on the upper and lower sides of the blade 29 are heated and kept warm. Since the radiation area of the blade 29 is circular after rotating with the central paddle plate 7, the range of raw materials heated by the heating tube 35 becomes larger; when the switch of the electric push rod 32 is triggered, the preset electric The piston rod of the push rod 32 reciprocates and retracts. During this process, the traction arm 33 is pulled by the electric push rod 32 to slide reciprocatingly along the storage groove 30. The radiation area of the heating tube 35 is expanded in the horizontal direction, and the hot air inside the installation groove 34 is dissipated through the pressure relief capillary 44. The hot air heats the fins 43. The fins 43 are inserted into the raw materials, which increases the contact area between the heat generated by the heating tube 35 and the raw materials. The dissipated hot air also heats and keeps the raw materials warm. The blades on both sides of the fins 43 can cut the agglomerated raw materials. In this way, the fins 43 not only relieve the pressure on the installation groove 34, but also increase the contact area between the heating tube 35 and the raw materials. The fins 43 can also break the agglomerated materials. The fins 43 have multiple uses.When the heating tube 35 is damaged, the heating tube 35 can be replaced separately. After loosening the screw 240 and disengaging it from the assembly groove 38, the side sealing plate 39 is pulled out from the end of the storage groove 30. At this time, one end of the heating tube 35 is exposed, and the heating tube 35 can be pulled out from the installation groove 34. It should be noted that the wire between the heating tube 35 and the battery 28 is reserved with sufficient length in the installation groove 34, that is, when the heating tube 35 is pulled out from the installation groove 34, the connector at the end of the wire can be manually unplugged from the interface of the heating tube 35. ;
[0062] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. An anti-corrosion coating material for marine steel structures, characterized in that: The anti-corrosion coating material is obtained by reacting the following components by mass: 1 to 10 parts of lignin sulfonate microcapsules embedding a healing agent; 10 to 90 parts of polyurea prepolymers; and 20 to 100 parts of a mixed solution of amino-terminated polyether and a sterically hindered amine chain extender.
2. A process for preparing the anti-corrosion coating material for marine steel structures according to claim 1, characterized in that: The preparation process comprises the following steps: Mixing 10 to 100 parts by weight of a lignin sulfonate aqueous solution with 1 to 50 parts by weight of a microcapsule healing agent formed of an aromatic isocyanate and an aliphatic isocyanate, emulsifying, and drying at room temperature to obtain microcapsules of the lignin sulfonate-embedded healing agent; The amino-terminated polyether and aliphatic isocyanate are mixed in a molar ratio of 0.5:1 to 2:1, the temperature is raised to 20°C to 100°C, and the mixture is stirred in a heat-insulating mixer for 10 minutes to 24 hours to obtain a polyurea prepolymer; A mixture of lignin sulfonate-embedded healing agent microcapsules, amino-terminated polyether and hindered amine chain extender is added to a polyurea prepolymer and reacted at room temperature for 10 minutes to 4 hours to obtain a lignin sulfonate-dispersed self-healing polyurea coating.
3. The preparation equipment of the anti-corrosion coating material for marine steel structure according to claim 2, characterized in that: The heat preservation mixer comprises a cover plate (1), a motor assembly (3) is mounted on the surface of the cover plate (1), a sleeve (5) is fixed to the bottom end of the shaft of the motor assembly (3), an assembly block (6) is plugged into the bottom end of the sleeve (5), a slot (13) is provided on the surface of the assembly block (6), a limit block (10) is plugged into the interior of the slot (13), the limit block (10) passes through the sleeve (5), a central paddle board (7) is fixed to the bottom end of the assembly block (6), and the central paddle board A storage battery (28) is installed inside (7), blades (29) are fixed on both sides of the central paddle board (7), the top surface of the blade (29) and the bottom surface of the blade (29) are slidably connected with a traction arm (33), a heating tube (35) is installed inside the traction arm (33), a fin (43) is installed on the top surface of the traction arm (33), and an auxiliary paddle board (47) is fixed on the surface of the central paddle board (7), and a knife plate (48) is fixed on the surface of the auxiliary paddle board (47); A through hole (2) is provided in the center of the top surface of the cover plate (1), a bearing (4) is fixed inside the through hole (2), the bearing (4) is sleeved on the shaft of the motor assembly (3), the sleeve (5) is in a cylindrical structure, the inner ring groove of the sleeve (5) is in a square groove structure, the assembly block (6) is in a square block, the notch (11) is in an annular groove, the center paddle plate (7) is in a square plate structure, the assembly block (6) is centered on the top surface of the center paddle plate (7), the outer ring surface of the sleeve (5) is provided with a reserved groove (8), the surface of the reserved groove (8) is provided with a socket (9), two sockets (9) are provided, the two sockets (9) are symmetrically distributed about the sleeve (5), and the limit plug (10) is movably plugged into the socket (9).
4. The preparation device of the anti-corrosion coating material for marine steel structure according to claim 3, characterized in that: One end of the limiting plug (10) extending into the notch of the sleeve (5) is provided with a notch (11), an elastic band (12) is fixed on the surface of the notch (11), and the two ends of the elastic band (12) are respectively fixed on two parallel side walls of the socket (9). When one end of the limiting plug (10) is inserted into the slot (13), the elastic band (12) is in a stretched deformation state, and the other end of the limiting plug (10) is provided with an inclined surface (14). The inclined surface (14) faces upwards, the length of the limiting plug (10) is greater than the depth of the socket (9), a retaining ring (15) is sleeved inside the reserved groove (8), a rubber ring is fixed on the inner ring surface of the retaining ring (15), and the rubber ring is clamped between the retaining ring (15) and the reserved groove (8), and a picking groove (17) is opened on the outer ring surface of the retaining ring (15), and the picking groove (17) is an annular groove with a right-angled trapezoidal cross-section, and the inclined surface of the right-angled trapezoid is located at the bottom.
5. The preparation equipment of the anti-corrosion coating material for marine steel structure according to claim 3, characterized in that: The bottom surface of the central paddle board (7) is provided with a battery slot (18), the top surface of the battery slot (18) is fixed with a rubber pad (19), the rubber pad (19) is an annular plate, the storage battery (28) is inserted into the battery slot (18), the bottom end of the battery slot (18) is plugged with a sealing plate (20), the sealing plate (20) is a "convex" shaped plate, the bottom surface size of the sealing plate (20) is equal to the bottom surface size of the central paddle board (7), the bottom plate of the sealing plate (20) is fixed to the bottom surface of the central paddle board (7) by a screw (21), and the rubber pad (19) is squeezed by the battery slot (18) to produce elastic deformation.
6. The preparation equipment of the anti-corrosion coating material for marine steel structure according to claim 5, characterized in that: The top surface of the battery slot (18) is provided with an air delivery hole (22), the air delivery hole (22) penetrates the sleeve (5), the assembly block (6) and the shaft of the motor assembly (3), the top side wall of the air delivery hole (22) is provided with a plurality of air diffusion holes (23), the side wall of the perforation (2) is provided with a plurality of exhaust holes (24), the exhaust holes (24) are "L"-shaped holes, and the exhaust holes (24) penetrate the top surface of the cover plate (1), the top surface of the cover plate (1) is fixed with a limiting frame (25), the limiting frame (25) is a "T"-shaped circular ring plate, a mesh ring (26) and a dust cover (27) are fixed between the bottom surface of the top plate of the limiting frame (25) and the top surface of the cover plate (1), and the mesh ring (26) is sleeved on the outside of the dust cover (27).
7. The preparation equipment of the anti-corrosion coating material for marine steel structure according to claim 3, characterized in that: The top surface of the blade (29) and the bottom surface of the blade (29) are both provided with a receiving groove (30), the long side length of the receiving groove (30) is shorter than the long side length of the blade (29), the surface of the receiving groove (30) close to the central paddle plate (7) is provided with an embedding groove (31), an electric push rod (32) is fixed inside the embedding groove (31), the piston rod of the electric push rod (32) is fixed on the surface of the traction arm (33), and the traction arm (33) is provided with a piston rod at one end away from the electric push rod (32). The heating tube (35) is movably inserted in the installation groove (34), one end of the traction arm (33) is fixed with an assembly block (37), the assembly block (37) is movably inserted in the assembly groove (38), the assembly groove (38) is arranged on the surface of the side sealing plate (39), the assembly block (37) is fixed in the assembly groove (38) by screws (40), one end of the heating tube (35) is inserted in the buckle groove (49), and the buckle groove (49) is arranged on the surface of the side sealing plate (39).
8. The preparation equipment of the anti-corrosion coating material for marine steel structure according to claim 3, characterized in that: A pad strip (36) is fixed to the bottom surface of the installation groove (34), and the heating tube (35) is overlapped on the pad strip (36). A plurality of plug holes (41) are provided on the top surface of the traction arm (33), and the plug holes (41) are connected to the installation groove (34). A stopper (42) is inserted inside the plug hole (41). The bottom surface of the stopper (42) is an arc surface, and the arc surface overlaps the heating tube (35). A notch is provided on the surface of the stopper (42). The fin (43) is fixed to the top surface of the stopper (42), and blades are provided on both sides of the fin (43). A pressure relief tube (44) is inserted on the top surface of the bottom end of the notch. The pressure relief tube (44) passes through the stopper (42) and the fin (43), and the pressure relief tube (44) is an inverted "U"-shaped tube.
9. The preparation equipment of the anti-corrosion coating material for marine steel structure according to claim 3, characterized in that: An extension plate (45) is fixed on the surface of the side sealing plate (39). The extension plate (45) is slidably connected in a side groove (46). The side groove (46) is opened on the surface of the blade (29). Two extension plates (45) are provided, and the two extension plates (45) are symmetrically distributed about the blade (29).
10. The preparation equipment of the anti-corrosion coating material for marine steel structure according to claim 7, characterized in that: The heating tube (35) and the electric push rod (32) are both connected to the battery (28) via wires.
Citation Information
Patent Citations
Heating-humidifying integral transfusion rack
CN106902417A
Soybean meal fermentation device and method for extracting soybean protein
CN114134014A
Automatic control by temperature change calcium carbonate thick liquids surface modification device
CN207596486U
Petroleum asphalt production solvent mixing device
CN210045128U
Novel powder storage equipment for concrete mixing plant
CN212448958U