Bar segmentation rear end heat compensation device

By installing a high-frequency or medium-frequency electromagnetic induction coil and a pyrometer on the baling machine, the end of the steel is heated to 400°C-700°C in a short time, which solves the problem of cracking caused by stress concentration during sawing and shearing of medium and high carbon alloy steel. Stress relief annealing is achieved, improving production efficiency and product quality.

CN118726709APending Publication Date: 2024-10-01NANJING IRON & STEEL CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410775362.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-17
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

During the sawing and shearing process of medium and high carbon alloy steel, the stress concentration caused by low hot shearing temperature causes end cracking, which is difficult to effectively solve with existing technology.

Method used

After the baler hits the baffle, a high-frequency or medium-frequency electromagnetic induction coil and a pyrometer are installed to heat it to 400°C-700°C in a short period of time and automatically control and monitor it to eliminate cracks caused by concentration of shear stress.

Benefits of technology

It effectively eliminates shear stress, prevents cracking, simplifies offline placement requirements, and improves production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118726709A_ABST
    Figure CN118726709A_ABST
Patent Text Reader

Abstract

The invention discloses a bar segmentation rear end heat compensation device which is characterized in that an electromagnetic induction coil and a pyrometer are additionally arranged after a packer collides with a baffle in order, heating is carried out within a short time to reach the needed temperature, automatic control and monitoring are achieved, and shearing stress caused by shearing is eliminated on line. According to the method, cracks caused by stress concentration generated by shearing are eliminated by increasing the temperature of the end of the steel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of metallurgy, and in particular to a heat supplement device for the rear end of a bar segment. Background Art

[0002] Bearing steel is used to make balls, rollers and bearing rings. Bearing steel has high and uniform hardness and wear resistance, as well as high elastic limit. The uniformity of the chemical composition of bearing steel, the content and distribution of non-metallic inclusions, and the distribution of carbides are very strict. It is one of the most stringent steel grades in all steel production.

[0003] Spring steel refers to special alloy steel used to manufacture various springs and other elastic components. According to performance requirements and usage conditions, it can be divided into ordinary alloy spring steel and special alloy spring steel. Spring steel has excellent comprehensive performance, excellent metallurgical quality (high purity and uniformity), good surface quality (strictly control surface defects and decarburization), precise shape and size.

[0004] When medium and high carbon alloy steels such as bearing steel and spring steel are cut by sawing and then sheared, there is a problem of low hot shearing temperature causing stress concentration at the ends and resulting in cracking.

[0005] Therefore, it is necessary to develop a targeted heating device for the rear end of the bar segment to prevent cracking caused by low temperature. Summary of the invention

[0006] Purpose of the invention: In view of the shortcomings and defects of the prior art, the present invention provides a heating device for the rear end of a bar segment, which eliminates cracks caused by stress concentration due to shearing by increasing the temperature of the steel end.

[0007] Technical solution: The present invention is a device for supplementing heat at the rear end of a segmented bar, which is characterized by installing an electromagnetic induction coil and a pyrometer after the baler hits the baffle, heating to the required temperature in a short time to achieve automatic control and monitoring, and online elimination of shear stress caused by shearing.

[0008] Wherein, the electromagnetic induction coil is a high-frequency or medium-frequency electromagnetic induction coil.

[0009] Wherein, the temperature is heated and maintained at 400°C-700°C by the electromagnetic induction coil and the pyrometer.

[0010] Wherein, the electromagnetic induction coil is arranged on the roller table, and the pyrometer is arranged on the side of the roller table.

[0011] Wherein, the electromagnetic induction coil wraps the roller.

[0012] Beneficial effects: Compared with the prior art, the present invention has the following significant advantages: the present invention uses high-frequency / medium-frequency induction heating and a pyrometer installed after the baler hits the baffle plate, heats to the required temperature in a short time to achieve automatic control and monitoring, eliminates the shear stress caused by shearing online, and the subsequent offline placement requirements are relatively simple. It will not cause cracking and other phenomena. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 It is a structural schematic diagram of the present invention;

[0014] In the figure, 1 is a roller, 2 is an electromagnetic induction coil, and 3 is a pyrometer. DETAILED DESCRIPTION

[0015] The technical solution of the present invention is further described below in conjunction with the accompanying drawings and specific implementation methods.

[0016] The bar segment rear end supplementary heating device of the present invention utilizes an electromagnetic induction coil and a pyrometer installed after the baler hits the baffle plate to heat to the required temperature in a short time to achieve automatic control and monitoring, and eliminate the shear stress caused by shearing online. The electromagnetic induction coil is a high-frequency or medium-frequency electromagnetic induction coil. The electromagnetic induction coil and the pyrometer heat and maintain the temperature at 400°C-700°C. The electromagnetic induction coil is arranged on the roller, and the pyrometer is arranged on the side of the roller. The electromagnetic induction coil wraps the roller.

[0017] The invention is aimed at shearing tests of different temperatures on GCr15 bearing steel saws of Nanjing Iron and Steel Medium Rod Plant. When the shearing temperature is greater than 460°C, the temperature entering the slow cooling pit is greater than 400°C and there is no cracking after exiting the pit. When the shearing temperature is lower than 460°C, the temperature entering the slow cooling pit is lower than 400°C and there is cracking at the end after exiting the pit.

[0018] When the shear temperature is lower than 460℃, the crack control method is: use the electromagnetic induction coil and the pyrometer set after the baling machine is finished to heat to above 400℃. When stress relief annealing is performed, the metal relaxes the residual stress under a certain temperature through internal local plastic deformation (when the stress exceeds the yield strength of the material at this temperature) or local relaxation process (when the stress is less than the yield strength of the material at this temperature) to achieve the purpose of eliminating the residual stress.

[0019] Control method for entering the slow cooling pit when the steel is offline: After both ends of the steel are electromagnetically heated to the appropriate temperature and then put into the pit, choose a low-level sheltered place and cover both ends with a blanket made of insulation material (industrial refractory aluminum silicate insulation cotton). After keeping it for a period of time, slowly cool it to prevent the generation of new residual stress.

[0020] The principle of the present invention is that when stress relief annealing is performed, the metal relaxes the residual stress through internal local plastic deformation or local relaxation process under a certain temperature to achieve the purpose of eliminating shear cracks caused by stress concentration.

[0021] The present invention controls the compensation temperature of the round steel end to ensure that the medium-high carbon alloy steel enters the slow cooling pit at a low temperature after shearing, and cracks caused by stress concentration due to shearing cannot be eliminated. In addition, the saw blade consumption is reduced by changing from sawing to shearing, and the production efficiency is improved.

Claims

1. A device for heating the rear end of a bar segment, characterized in that: By installing an electromagnetic induction coil (2) and a pyrometer (3) after the baler collides with the baffle plate, heating to the required temperature is performed in a short time to realize automatic control and monitoring, and the shear stress caused by shearing is eliminated online.

2. The device for supplementary heating of the rear end of the bar segment according to claim 1 is characterized in that: The electromagnetic induction coil (2) is a high-frequency or medium-frequency electromagnetic induction coil.

3. The device for supplementary heating of the rear end of the bar segment according to claim 1, characterized in that: The temperature is heated and maintained at 400° C.-700° C. by means of the electromagnetic induction coil (2) and the pyrometer (3).

4. The device for supplementary heating of the rear end of the bar segment according to claim 1, characterized in that: The electromagnetic induction coil (2) is arranged on the roller (1), and the pyrometer (3) is arranged on the side of the roller (1).

5. The device for supplementary heating of the rear end of the bar segment according to claim 1, characterized in that: The electromagnetic induction coil (2) wraps the roller (1).

Citation Information

Patent Citations

  • Method for online eliminating shearing cracks at end part of spring flat steel

    CN117265236A

  • Online steel end heating device

    CN219851391U

  • Laser beam side trimmer device

    JP1990052187A

  • Method for cutting thick steel plate

    JP2007245261A

  • Multifunctional high-strength steel sheet or strip heat treatment production system and method