Failure analysis sample preparation positioning method

By forming the bonding points and leads on the conductors on the sample chip and grinding them layer by layer, it solves the problems of high failure analysis cost and difficult positioning in the existing technology, and achieves efficient and accurate failure point positioning and grinding.

CN118730658APending Publication Date: 2024-10-01青岛旭芯互联科技研发有限公司 +2
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410852342.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In the existing technology, the cost of failure analysis is high, it is impossible to conduct failure analysis on a large number of samples in a short time, and it is impossible to accurately locate the failure point, resulting in a high grinding failure rate.

Method used

By forming front and back bonding points on the conductors on the sample chip, bonding wires from these points, and vertically grinding layer by layer until the wires break, ensuring precise location and exposure of the failure point.

Benefits of technology

It achieves precise positioning of failure points and efficient grinding, reduces costs, improves the success rate of grinding, and can complete the analysis of a large number of samples in a short period of time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118730658A_ABST
    Figure CN118730658A_ABST
Patent Text Reader

Abstract

The invention provides a failure analysis sample preparation positioning method which comprises the following steps: S1, confirming a failure point location of a sample chip to obtain a failure point location position; s2, determining a conductor beside the failure point location based on the position of the failure point location; s3, forming a front bonding point in front of the failure point on the conductor, and bonding a front bonding lead wire from the front bonding point to obtain a processed sample chip; s4, performing glue pouring on the sample chip subjected to embedding treatment, and enabling the front bonding lead to be exposed out of a preset length to obtain a sealed sample chip; and S5, carrying out layer-by-layer vertical grinding on the sealed sample chip, stopping grinding until the front bonding lead is broken and the front bonding point is completely ground off, and exposing the failure point. The failure analysis sample preparation positioning method disclosed by the invention is easy to implement and low in cost, the problem of shielding of epoxy resin during overlooking observation and judgment can be avoided, the grinding accuracy is high, and an operator can complete failure point location analysis on a large number of samples within a relatively short time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of semiconductor technology, and in particular to a method for positioning a sample for failure analysis. Background Art

[0002] Failure analysis is a developing new discipline, which has been popularized from military industry to ordinary enterprises in recent years. It is generally based on the failure mode and phenomenon, through analysis and verification, simulation and reproduction of failure phenomenon, find out the cause of failure, and dig out the failure mechanism. It has great practical significance in improving product quality, technology development, improvement, product repair and arbitration failure accidents.

[0003] As semiconductor and integrated circuit devices become smaller and smaller, the difficulty of failure analysis has greatly increased, especially in destructive testing, slicing is the most difficult problem to solve. Slice analysis can obtain rich information about the microstructure of the IC (integrated circuit) quality, providing a good basis for the next step of quality improvement. The main slicing analysis methods in the existing technology include traditional inlay-grinding and FIB (focused ion beam) micro-nano processing.

[0004] Patent application with publication number CN116577628A discloses the use of FIB to cut samples. Although FIB has high processing accuracy, does not require sample inlay processing and is conducive to observation and positioning, the FIB equipment is expensive and the purchase cost is high. In addition, the processing time of FIB cutting samples is long, so it cannot meet the demand for completing failure point analysis of a large number of samples in a relatively short time.

[0005] For the traditional inlay-grinding scheme, when the sample chip is ground vertically layer by layer, each layer of the grinding surface after cross-section grinding is very flat and has no ups and downs (such as Fig.12As shown in the figure, and there is almost no difference between each layer of the grinding surface. The observation surface during grinding is a rectangle, and the failure point can only be judged and located on which grinding surface layer the failure point is located by relying on the color difference of the failure point. For example, when the failure point is large and the failure point is a hole and the sample chip is made of silicon, when grinding to the failure point, the grinding surface will show that the failure point is black and the grinding surface outside the failure point is grayish white. At this time, it is easy to locate the failure point. However, the specific size, color, shape (for example, the layer is linear and the hole is round), morphology, etc. of the failure point are unpredictable. Sometimes the color of the failure point is similar to the color of the sample chip, sometimes impurities are mixed in the sample chip, and sometimes the failure point is at the micron level. In these cases, during the grinding process, it cannot be ensured that the failure point can be easily located every time by relying on the color difference of the failure point as described above. In most cases, it is difficult to distinguish the failure point. Therefore, during the grinding process, the failure point dislocation is easily ground off as grinding debris, the grinding accuracy is low, and the grinding failure rate will be greatly increased. As a destructive test, test failure will lead to damage to the sample, which is unacceptable for failure analysis tests.

[0006] In order to solve the above problems, the prior art uses an optical microscope to observe and search for a characteristic position with a special structure near the failure point on the surface of the sample chip. For example, the surface where the characteristic position is located has a special pattern, so the special pattern near the failure point can be used as a characteristic point, so that when grinding, it can be judged whether the failure point has been ground according to the relative position of the characteristic point before and after the failure point. However, in the traditional inlay-grinding scheme, the sample chip needs to be filled with epoxy resin to form a sealed sample chip. Due to the presence of bubbles in the epoxy resin layer or the deterioration of transparency or incomplete transparency and refraction, it is difficult to clearly see the characteristic point and failure point of the sealed sample chip when observing under an optical microscope. Especially in the case of micrometer-level failure points, even a tiny impurity in the epoxy resin layer is larger than the failure point, which seriously interferes with the positioning of the failure point.

[0007] Therefore, there is still much room for improvement in the existing methods of sample preparation and positioning for failure analysis. Summary of the invention

[0008] The present invention provides a method for positioning a sample for failure analysis, so as to solve the technical problems in the prior art of high failure analysis cost, inability to perform failure analysis of a large number of samples in a short period of time, and high grinding failure rate caused by inability to accurately locate failure points.

[0009] In order to solve the above technical problems, the present disclosure provides a method for positioning a sample for failure analysis, comprising the following steps: S1. Confirm the failure point of the sample chip and obtain the failure point position; S2, determining the conductor next to the failure point based on the location of the failure point; S3, forming a front bonding point located in front of the failure point on the conductor, and bonding a front bonding wire from the front bonding point to obtain a processed sample chip; S4, filling and embedding the processed sample chip with glue, and making the front bonding wire leak out a predetermined length to obtain a sealed sample chip; S5. Grind the sealed sample chip vertically layer by layer until the front bonding wire is broken and the front bonding point is completely ground away, and then stop grinding. At this time, the failure point is exposed.

[0010] In some embodiments, In step S5, the sealed sample chip is vertically ground layer by layer starting from the side of the sealed sample chip in a direction perpendicular to the failure point, and the front bonding point is set in front of the failure point in the direction in which the grinding surface is ground away layer by layer, and the front bonding wire extends along the direction in which the grinding surface is ground away layer by layer, and, The plane where the end of the front bonding point is located is adjacent to the plane where the starting end of the failure point is located, and the plane where the end of the front bonding point is located and the plane where the starting end of the failure point is located are parallel to the vertical grinding direction respectively.

[0011] In some embodiments, In step S3, the following steps are also included: forming a rear bonding point on the conductor and bonding a rear bonding wire from the rear bonding point, wherein the rear bonding point is arranged behind the failure point in the direction in which the grinding surface is ground away layer by layer, and the rear bonding wire extends along the direction in which the grinding surface is ground away layer by layer; and In step S4, the step of causing the post-bonding wire to leak out by a predetermined length is also included.

[0012] In some embodiments, the lead portions of the front bonding wire and the back bonding wire that are leaked out of a predetermined length are respectively connected to an external ammeter or a semiconductor tracer through conductive tapes to form an electrical loop.

[0013] In some embodiments, in step S1, a micro-light microscope, an optical microscope or an electrical measurement method is used to confirm the failure point of the sample chip.

[0014] In some embodiments, in step S3, a manual bonding machine is used to bond the front bonding wire and the rear bonding wire, the front bonding point, the rear bonding point, the front bonding wire and the rear bonding wire are made of copper or gold, the front bonding point and the rear bonding point are cylindrical respectively, and the minimum diameter of the front bonding wire and the rear bonding wire is 15μm.

[0015] In some embodiments, In step S4, epoxy resin is used to embed the processed sample chip, and the embedding amount of the epoxy resin is 1g / cm 3 , thickness is 5mm; In step S5, 1200-grit sandpaper is used to vertically grind the epoxy resin layer layer by layer until the sample chip is exposed, and 2400-grit sandpaper is used to vertically grind the sample chip layer by layer.

[0016] In some embodiments, If the sample chip has been packaged, the step of unpacking the sample chip is also included before step S1; and After step S5, the method further includes the step of polishing the exposed failure points with a 4800-mesh polishing cloth.

[0017] The present disclosure also provides a method for positioning a sample for failure analysis, comprising the following steps: S1. Confirm the failure point of the sample chip; S2, forming a bonding point located in front of the failure point on the sample chip to obtain a processed sample chip; S3, the sample chip after the glue-filling and inlaying process is obtained to obtain a sealed sample chip; S4. Grind the sealed sample chip vertically layer by layer until the bonding point is completely ground away, and then stop grinding. At this time, the failure point is exposed.

[0018] In some embodiments, In step S4, the sealed sample chip is vertically ground layer by layer starting from the side of the sealed sample chip in a direction perpendicular to the failure point, and the bonding point is set in front of the failure point in the direction of the grinding surface being ground away layer by layer, and, The plane where the end of the bonding point is located is adjacent to the plane where the starting end of the failure point is located, and the plane where the end of the bonding point is located and the plane where the starting end of the failure point is located are parallel to the vertical grinding direction respectively.

[0019] Compared with the prior art, the beneficial technical effects of the present disclosure are: In the case where there is a conductor next to the failure point of the sample chip, the present disclosure achieves accurate grinding and positioning of the failure point by accurately determining the size of the front bonding point, the positional relationship of the front bonding point and the rear bonding point relative to the failure point, and the extension direction of the front bonding line relative to the front bonding point. In the case where there is no conductor next to the failure point of the sample chip, the present disclosure achieves accurate grinding and positioning of the failure point by accurately determining the size of the bonding point and the positional relationship of the bonding point relative to the failure point. The failure analysis sample preparation and positioning method disclosed in the present disclosure is simple to operate, easy to implement, and low in cost. It can avoid the obstruction of epoxy resin when observing and judging from a bird's-eye view, can accurately locate the failure point, has high grinding accuracy, high grinding success rate, and the operator can complete the failure point analysis of a large number of samples in a relatively short time. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0021] Figure 1 A schematic flow chart of a method for positioning a sample for failure analysis disclosed in an embodiment of the present disclosure is shown; Figure 2 A schematic side view of a sample chip disclosed in an embodiment of the present disclosure is shown, wherein a front bonding wire and a rear bonding wire are bonded to a conductor next to a failure point; Figure 3 Shows Figure 2 A schematic top view of a sample chip; Figure 4 Shows the Figure 2 A schematic three-dimensional diagram of a sealed sample chip obtained after the sample chip is filled with glue and embedded; Figure 5 Shows Figure 4 A schematic cross-sectional view of a sealed sample chip, wherein the grinding direction of the sealed sample chip is shown, and the front bonding wire and the rear bonding line are not shown; Figure 6 Shows Figure 4 A schematic cross-sectional view of a sealed sample chip after grinding, wherein the epoxy resin layer is not shown; Figure 7 Shows Figure 2 A partial schematic side view of a sample chip is shown, showing the positional relationship of the front bonding wire relative to the front bonding point; Figure 8A schematic flow chart of another failure analysis sample preparation and positioning method disclosed in an embodiment of the present disclosure is shown; Fig. 9 A schematic top view of another sample chip disclosed in an embodiment of the present disclosure is shown, wherein there is no conductor next to the failure point; Fig.10 Shows the Fig. 9 A schematic cross-sectional view of a sealed sample chip obtained after the sample chip is glue-filled and embedded, showing the direction in which the sealed sample chip is ground; Fig.11 Shows Fig.10 A schematic cross-sectional view of a sealed sample chip after grinding, wherein the epoxy resin layer is not shown; Fig.12 A schematic cross-sectional view showing a polished surface of a sample chip disclosed in an embodiment of the present disclosure during polishing is shown, wherein no bonding points are formed on the sample chip; Fig.13 A schematic cross-sectional view of a polished surface of a sample chip during polishing according to an embodiment of the present disclosure is shown, wherein bonding points on the sample chip are shown.

[0022] Description of Reference Numerals 1. Sample chip; 2. Failure point; 3. Conductor; 4. Front bonding point; 5. Front bonding lead; 6. Sealed sample chip; 7. Back bonding point; 8. Back bonding lead; 9. Lead portion leaking out of a predetermined length; 10. Epoxy resin layer; 11. Conductive tape; 20. Sample chip; 21. Failure point; 21', Failure point; 22. Bonding point; A. Arrow, indicating the direction of vertical grinding; B. Arrow, indicating the direction in which the grinding surface is worn away layer by layer; O. The end of the bonding point; P. The starting end of the failure point. DETAILED DESCRIPTION

[0023] The following is a further detailed description of the embodiments of the present disclosure in conjunction with the accompanying drawings and examples. The detailed description of the following embodiments and the accompanying drawings are used to exemplarily illustrate the principles of the present disclosure, but cannot be used to limit the scope of the present disclosure. The present disclosure can be implemented in many different forms and is not limited to the specific embodiments disclosed herein, but includes all technical solutions that fall within the scope of the claims.

[0024] The present disclosure provides these embodiments to make the present disclosure thorough and complete, and to fully express the scope of the present disclosure to those skilled in the art. It should be noted that unless otherwise specifically stated, the relative arrangement of the parts and steps, the composition of the materials, the numerical expressions and the numerical values ​​set forth in these embodiments should be interpreted as being merely exemplary, and not as limiting.

[0025] It should be noted that, in the description of the present disclosure, unless otherwise specified, the meaning of "multiple" is greater than or equal to two; the terms "upper", "lower", "left", "right", "inner", "outer", etc., indicating the orientation or positional relationship, are only for the convenience of describing the present disclosure and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present disclosure. When the absolute position of the object being described changes, the relative positional relationship may also change accordingly.

[0026] In addition, the words "first", "second" and similar words used in the present disclosure do not indicate any order, quantity or importance, but are only used to distinguish different parts. "Vertical" does not mean vertical in the strict sense, but is within the tolerance range. "Parallel" does not mean parallel in the strict sense, but is within the tolerance range. "Include" or "comprising" and similar words mean that the elements before the word include the elements listed after the word, and do not exclude the possibility of including other elements.

[0027] It should also be noted that in the description of the present disclosure, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present disclosure can be understood according to the specific circumstances. When a specific device is described as being located between a first device and a second device, there may or may not be an intermediate device between the specific device and the first device or the second device.

[0028] All terms used in the present disclosure have the same meanings as those understood by those of ordinary skill in the art to which the present disclosure belongs, unless otherwise specifically defined. It should also be understood that terms defined in general dictionaries, for example, should be interpreted as having meanings consistent with their meanings in the context of the relevant technology, and should not be interpreted in an idealized or extremely formal sense, unless explicitly defined as such herein.

[0029] Technologies, methods, and equipment known to ordinary technicians in the relevant art may not be discussed in detail, but where appropriate, the technologies, methods, and equipment should be considered part of the specification.

[0030] Example 1 In one embodiment of the present disclosure, Figure 1 As shown, the present disclosure provides a method for positioning a sample for failure analysis, comprising the following steps: S1. Confirm the failure point 2 of the sample chip 1 and obtain the failure point position.

[0031] In a preferred embodiment, in step S1 , conventional technical means in the art such as micro-light microscope (Emmi), optical microscope (metallographic microscope) or electrical measurement method can be used to confirm the failure point 2 of the sample chip 1 .

[0032] S2, based on the position of the failure point, determine the conductor 3 next to the failure point 2 (such as Figure 2 and Figure 3 as shown).

[0033] S3, forming a front bonding point 4 located in front of the failure point 2 on the conductor 3, and bonding a front bonding wire 5 from the front bonding point 4 to obtain a processed sample chip (such as Figure 2 as shown).

[0034] S4, the sample chip after the glue filling and embedding treatment is made, and the front bonding wire 5 is leaked out by a predetermined length to obtain a sealed sample chip 6 (such as Figure 4 as shown).

[0035] In a preferred embodiment, in step S4, epoxy resin is used to embed the processed sample chip, and the embedding amount of the epoxy resin is 1 g / cm 3 , with a thickness of 5 mm. Since the sample chip is very small, it is impossible to grind it while clamping it, so the processed sample chip needs to be embedded with glue, so that the overall size of the sample chip after embedding with glue is larger than the size of the original sample chip, so as to facilitate the operation of clamping and grinding.

[0036] S5, grinding the sealed sample chip 6 layer by layer vertically until the front bonding wire 5 is broken and the front bonding point 4 is completely ground off, then the grinding is stopped, and the failure point 4 is exposed (such as Figure 5 and Figure 6 as shown).

[0037] In order to solve the technical problems mentioned in the background art regarding the inlay-grinding scheme, step S2 of the above-mentioned embodiment 1 of the present disclosure is designed to form a front bonding point 4 located in front of the failure point 2 on the conductor 3 next to the failure point 2, so as to assist in locating the failure point 2. Those skilled in the art should understand that it is easy to determine the precise position (high dot-marking accuracy) and size (the front bonding point 4 can be very small as required) of the front bonding point 4 on the conductor 3 of the sample chip 1, and the shape (for example, designed as a cylinder) and color (for example, the material of the front bonding point 4 is copper or gold, so the color is yellow) of the front bonding point 4 are fixed, and appear on the grinding surface as a yellow protrusion (such as a certain height (rectangular) and very clear) Fig.13As shown in the figure, the front bonding point 4 can be easily observed, and then the failure point 2 can be located. The design of the front bonding point 4 solves the problem of being unable to observe clearly due to the obstruction of the epoxy resin layer 10 when observing from above. In other words, the operator can accurately bond the front bonding point 4 with the help of a microscope, and can accurately determine the size of the front bonding point 4 and the positional relationship of the front bonding point 4 relative to the failure point 2, so as to achieve the purpose of accurately grinding to the failure point 2 with the front bonding point 4 as a reference.

[0038] In a preferred embodiment, if Figure 5 As shown, the sealed sample chip 6 is vertically ground layer by layer starting from the side of the sealed sample chip 6 in a direction perpendicular to the failure point 2 (the direction indicated by the arrow A). In addition, in the direction in which the grinding surface is ground away layer by layer (the direction indicated by the arrow B), the front bonding point 4 is arranged in front of the failure point 2 and the front bonding wire 5 extends along the direction in which the grinding surface is ground away layer by layer (as shown in FIG. Figure 7 ), to ensure that the front bonding wire 5 and the front bonding point 4 can be ground off at the same time, and the front bonding wire 5 will not be ground off first and then the front bonding point 4 will not be ground off. In addition, the plane where the end M of the front bonding point 4 is located is adjacent to the plane where the starting end N of the failure point 2 is located, and the plane where the end M of the front bonding point 4 is located and the plane where the starting end N of the failure point 2 is located are parallel to the vertical grinding direction (the direction indicated by the arrow A).

[0039] like Figure 5 As shown, facing Figure 5 , starting from the left side of the sealed sample chip 6, a virtual plane parallel to the direction indicated by arrow A is used to vertically grind the sealed sample chip 6 layer by layer (along the direction indicated by arrow A). As time goes by, the grinding surface changes from Figure 5 The left side to the right side of the front bonding point 4 is ground off in sequence. When the front bonding point 4 is ground off from the left side of the starting end to the right side of the end M of the front bonding point 4 until the end M of the front bonding point 4 is ground off, the starting end N on the left side of the failure point 2 is precisely reached, thereby achieving precise grinding to the failure point 2 and exposing the failure point 2 (such as Figure 6 As shown in the figure), it is convenient for the subsequent microstructure analysis of the failure point 2.

[0040] In a preferred embodiment, if Figures 2 to 4As shown, in step S3, the following steps are also included: forming a rear bonding point 7 on the conductor 3 and bonding a rear bonding lead 8 from the rear bonding point 7. In step S4, the following steps are also included: making the rear bonding lead 8 leak out by a predetermined length. In the direction of travel (the direction indicated by arrow B) in which the grinding surface is worn away layer by layer, the rear bonding point 7 is set behind the failure point 2, and the rear bonding lead 8 extends along the direction of travel in which the grinding surface is worn away layer by layer. The lead portions 9 of the front bonding lead 5 and the rear bonding lead 8 that leak out by a predetermined length can be pasted with a conductive tape 11, and the lead portions 9 of the front bonding lead 5 and the rear bonding lead 8 that leak out by a predetermined length are respectively connected to an external ammeter or a semiconductor tracer through the conductive tape 11 to form an electrical circuit.

[0041] In one embodiment, the lengths of the front bonding lead 5 and the rear bonding lead 8 are 1 cm respectively, and the thickness of the epoxy resin layer 10 is about 5 mm. Since the front bonding lead 5 and the rear bonding lead 8 do not leak out of the epoxy resin layer 10 straight up and down, the length of the lead portion 9 of the front bonding lead 5 and the rear bonding lead 8 leaking out of the predetermined length is about 3-4 mm.

[0042] like Figure 7 As shown, facing Figure 7 , the front bonding lead 5 extends along the direction of the grinding surface being ground off layer by layer (the direction indicated by the arrow B). This arrangement makes a certain part of the front bonding lead 5 and the end M of the front bonding point 4 in the same plane, and the same plane is parallel to the vertical grinding direction (the direction indicated by the arrow A). Therefore, when the end M of the front bonding point 4 is ground off vertically using an imaginary plane, the certain part of the front bonding lead 5 is also ground off at the same time. At this time, the electrical circuit formed by the front bonding lead 5, the conductor 3, the rear bonding lead 8 and the external ammeter or semiconductor tracer is disconnected, so that by measuring the resistance of the electrical circuit, it can also be determined that the grinding has reached the failure point 2.

[0043] In a preferred embodiment, in step S3, a manual bonding machine is used to bond the front bonding wire 5 and the rear bonding wire 8. In a preferred embodiment, in step S3, the front bonding point 4, the rear bonding point 7, the front bonding wire 5 and the rear bonding wire 8 are made of copper or gold, the front bonding point 4 and the rear bonding point 7 are cylindrical, and the minimum diameter of the front bonding wire 5 and the rear bonding wire 8 is 15 μm. In a preferred embodiment, in step S5, 1200-grit sandpaper is used to vertically grind the epoxy resin layer 10 layer by layer until the sample chip 1 is exposed, and 2400-grit sandpaper is used to vertically grind the sample chip 1 layer by layer.

[0044] In a preferred embodiment, if the sample chip 1 has been packaged, the step of unpacking the sample chip 1 is included before step S1. In a preferred embodiment, after step S5, the step of polishing the exposed failure point 2 with a 4800-mesh polishing cloth is included to facilitate subsequent observation and analysis.

[0045] Example 2 In another embodiment of the present disclosure, Figure 8 As shown, the present disclosure provides a method for positioning a sample for failure analysis, comprising the following steps: S1 . Confirm the failure point 21 of the sample chip 20 .

[0046] S2. Form a bonding point 22 located in front of the failure point 21 on the sample chip 20 to obtain a processed sample chip.

[0047] S3, the sample chip 20 after the glue-filling and embedding process is obtained to obtain the sealed sample chip 6.

[0048] S4, vertically grinding the sealed sample chip 6 layer by layer until the bonding point 22 is completely ground away and then the grinding is stopped. At this time, the failure point 21 is exposed.

[0049] The above-mentioned embodiment 2 of the present disclosure uses the bonding point 22 formed on the sample chip 20 and located in front of the failure point 21 to help improve the grinding accuracy of the grinding positioning failure point 20, thereby achieving the purpose of grinding to the failure point 20.

[0050] In a preferred embodiment, if Fig.10 As shown, the sealed sample chip 6 is vertically ground layer by layer starting from the side of the sealed sample chip 6 in a direction perpendicular to the failure point 21 (the direction indicated by arrow A), and in the direction of travel (the direction indicated by arrow B) in which the grinding surface is ground away layer by layer, the bonding point 22 is set in front of the failure point 21. In addition, the plane where the end O of the bonding point is located is adjacent to the plane where the starting end P of the failure point is located, and the plane where the end O of the bonding point is located and the plane where the starting end P of the failure point is located are parallel to the direction of vertical grinding respectively.

[0051] like Fig. 9 As shown, in the above embodiment, there is no conductor next to the failure point 21 of the sample chip 20, so only a bonding point 22 is formed on the sample chip 20 to assist in locating the failure point 21. Fig.10 As shown, facing Fig.10 , starting from the left side of the sealed sample chip 6, a virtual plane parallel to the direction indicated by arrow A is used to vertically grind the sealed sample chip 6 layer by layer (along the direction indicated by arrow A). As time goes by, the grinding surface changes from Fig.10The left side to the right side of the bonding point 22 is ground off in sequence. When the bonding point 22 is ground off from the left side of the starting end to the right side of the bonding point 22 until the end O of the bonding point is ground off, the starting end P on the left side of the failure point 21 is precisely reached, thereby achieving precise grinding to the failure point 21 and exposing the failure point 21 (such as Fig.11 As shown), the subsequent microstructure analysis of the failure point 21 is facilitated. It should be understood by those skilled in the art that the failure point (2, 21) disclosed herein may be located inside the sample chip (1, 20) or on the surface of the sample chip (1, 20). For example, the failure point 21' is located on the surface of the sample chip 20 ( Fig.10 ).

[0052] There is no conductor next to the failure point 21 in the embodiment 2 of the present disclosure, so a bonding point 22 located in front of the failure point 21 is formed on the sample chip 20. The concept of the embodiment 2 is similar to that of the embodiment 1 and will not be described again.

[0053] In the case where there is a conductor next to the failure point of the sample chip, the present disclosure achieves accurate grinding and positioning of the failure point by accurately determining the size of the front bonding point, the positional relationship of the front bonding point and the rear bonding point relative to the failure point, and the extension direction of the front bonding line relative to the front bonding point. In the case where there is no conductor next to the failure point of the sample chip, the present disclosure achieves accurate grinding and positioning of the failure point by accurately determining the size of the bonding point and the positional relationship of the bonding point relative to the failure point. The failure analysis sample preparation and positioning method disclosed in the present disclosure is simple to operate, easy to implement, and low in cost. It can avoid the obstruction of epoxy resin when observing and judging from a bird's-eye view, can accurately locate the failure point, has high grinding accuracy, high grinding success rate, and the operator can complete the failure point analysis of a large number of samples in a relatively short time.

[0054] Those skilled in the art should understand that the scope of application of the failure analysis sample preparation and positioning method disclosed herein may include situations where the failure point is located in a deep layer and cannot be observed using a metallographic microscope, but can be observed using observation means such as a low-light microscope, an XR microscope, an ultrasonic microscope, etc.

[0055] So far, various embodiments of the present disclosure have been described in detail. In order to avoid obscuring the concept of the present disclosure, some details known in the art are not described. Based on the above description, those skilled in the art can fully understand how to implement the technical solution disclosed here.

[0056] Although some specific embodiments of the present disclosure have been described in detail by way of examples, it should be understood by those skilled in the art that the above examples are for illustration only and are not intended to limit the scope of the present disclosure. It should be understood by those skilled in the art that the above embodiments may be modified or some technical features may be replaced by equivalents without departing from the scope and spirit of the present disclosure. In particular, the various technical features mentioned in the various embodiments may be combined in any manner as long as there is no structural conflict.

Claims

1. A method for sample preparation and positioning for failure analysis, characterized in that: The following steps are involved: S1, confirming the failure point (2) of the sample chip (1) and obtaining the position of the failure point; S2, determining the conductor (3) next to the failure point (2) based on the position of the failure point; S3, forming a front bonding point (4) located in front of the failure point (2) on the conductor (3), and bonding a front bonding wire (5) from the front bonding point (4) to obtain a processed sample chip; S4, embedding the processed sample chip with glue, and making the front bonding wire (5) leak out by a predetermined length, so as to obtain a sealed sample chip (6); S5, grinding the sealed sample chip (6) vertically layer by layer until the front bonding wire (5) is broken and the front bonding point (4) is completely ground away, then stopping the grinding, at which time the failure point (4) is exposed.

2. The method for sample preparation and positioning for failure analysis according to claim 1, characterized in that: In step S5, the sealed sample chip (6) is vertically ground layer by layer starting from the side surface of the sealed sample chip (6) in a direction perpendicular to the failure point (2), and in the direction in which the ground surface is ground away layer by layer, the front bonding point (4) is arranged in front of the failure point (2), and the front bonding wire (5) extends along the direction in which the ground surface is ground away layer by layer, and, The plane where the end (M) of the front bonding point (4) is located is adjacent to the plane where the starting end (N) of the failure point (2) is located, and the plane where the end (M) of the front bonding point (4) is located and the plane where the starting end (N) of the failure point (2) is located are respectively parallel to the direction of vertical grinding.

3. The method for preparing and positioning a failure analysis sample according to claim 2, characterized in that: In step S3, the following steps are also included: forming a rear bonding point (7) on the conductor (3) and bonding a rear bonding wire (8) from the rear bonding point (7), wherein in the direction in which the grinding surface is ground away layer by layer, the rear bonding point (7) is arranged behind the failure point (2), and the rear bonding wire (8) extends along the direction in which the grinding surface is ground away layer by layer; and In step S4, the following step is also included: making the post-bonding wire (8) leak out by a predetermined length.

4. The method for preparing and positioning a failure analysis sample according to claim 3, characterized in that: The lead portions (9) of the front bonding lead (5) and the rear bonding lead (8) that leak out of a predetermined length are respectively connected to an external ammeter or a semiconductor tracer through a conductive tape (11) to form an electrical circuit.

5. The method for preparing and positioning a failure analysis sample according to claim 1, characterized in that: In step S1, a micro-light microscope, an optical microscope or an electrical measurement method is used to confirm the failure point (2) of the sample chip (1).

6. The method for preparing and positioning a failure analysis sample according to claim 3, characterized in that: In step S3, a manual bonding machine is used to bond the front bonding lead (5) and the rear bonding lead (8); the front bonding point (4), the rear bonding point (7), the front bonding lead (5) and the rear bonding lead (8) are made of copper or gold; the front bonding point (4) and the rear bonding point (7) are cylindrical respectively; and the minimum diameter of the front bonding lead (5) and the rear bonding lead (8) is 15 μm.

7. The method for preparing and positioning a failure analysis sample according to claim 1, characterized in that: In step S4, the processed sample chip is embedded with epoxy resin, and the embedding amount of the epoxy resin is 1g / cm 3 , thickness is 5mm; In step S5, 1200-grit sandpaper is used to vertically grind the epoxy resin layer (10) layer by layer until the sample chip (1) is exposed, and 2400-grit sandpaper is used to vertically grind the sample chip (1) layer by layer.

8. The method for preparing and positioning a failure analysis sample according to claim 1, characterized in that: If the sample chip (1) has been packaged, the method further includes the step of unpacking the sample chip (1) before step S1; and After step S5, the method further includes the step of polishing the exposed failure point (2) using a 4800 mesh polishing cloth.

9. A method for positioning a sample for failure analysis, characterized in that: The following steps are involved: S1, confirming the failure point (21) of the sample chip (20); S2, forming a bonding point (22) located in front of the failure point (21) on the sample chip (20) to obtain a processed sample chip; S3, injecting glue to embed the processed sample chip (20) to obtain a sealed sample chip (6); S4, vertically grinding the sealed sample chip (6) layer by layer until the bonding point (22) is completely ground away and then stopping the grinding, at which time the failure point (21) is exposed.

10. The method for preparing and positioning a failure analysis sample according to claim 9, characterized in that: In step S4, the sealed sample chip (6) is vertically ground layer by layer starting from the side surface of the sealed sample chip (6) in a direction perpendicular to the failure point (21), and in the direction of travel in which the grinding surface is ground away layer by layer, the bonding point (22) is arranged in front of the failure point (21), and, The plane where the end (O) of the bonding point (22) is located is adjacent to the plane where the starting end (P) of the failure point (21) is located, and the plane where the end (O) of the bonding point (22) is located and the plane where the starting end (P) of the failure point (21) is located are respectively parallel to the direction of vertical grinding.

Citation Information

Patent Citations

  • Failure point positioning method for semiconductor power device