Preparation method of flexible double-layer polymer optical waveguide

By preparing a soft base layer and a spin-coated polymer layer on a hard board substrate, and using identification marks to align and press them, the preparation of a flexible double-layer polymer optical waveguide is simplified, and the problems of complex processes and high costs in the existing technology are solved. , achieving efficient optical waveguide plate production and high-density interconnection.

CN118732167APending Publication Date: 2024-10-01SHANGHAI UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410944214.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The existing flexible double-layer polymer optical waveguide preparation method is complex, requires precision equipment and high technical level, increases preparation cost and time, and is difficult to meet the needs of mass production and high-density interconnection.

Method used

Prepare a soft base layer on a hard board substrate, spin-coat the polymer cladding and core layers, perform UV exposure and development, use identification marks to align and press and fix, and finally peel off the hard board substrate to prepare a flexible double-layer polymer optical waveguide .

Benefits of technology

It simplifies the preparation process, improves flexibility and preparation efficiency, is suitable for mass production, and enhances the application of high-density optical waveguide plate interconnection technology.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118732167A_ABST
    Figure CN118732167A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of optical communication and microelectronics, and discloses a preparation method of a flexible double-layer polymer optical waveguide. The preparation method of the flexible double-layer polymer optical waveguide comprises the following steps: S1, preparing a soft substrate layer on a hard board substrate by using a soft waveguide substrate adhesive or a soft waveguide substrate film; s2, polymer cladding glue is spin-coated, and a lower cladding is prepared on the substrate layer; s3, spin-coating polymer core layer glue, performing ultraviolet exposure and development, and preparing a waveguide core layer on the lower cladding to obtain a waveguide core and an identification mark; s4, covering the core layer with an upper cladding to obtain a layer of waveguide; and S5, repeating the steps S1 to S4 to prepare two same waveguides, and stripping the hard board substrate of one sample. The optical waveguide prepared by the preparation method of the flexible double-layer polymer optical waveguide provided by the invention is not influenced by roughness generated by processes such as photoetching, developing and pressing, and has the advantages of simple and flexible operation and high preparation efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the fields of optical communication technology and microelectronic technology, and in particular to a method for preparing a flexible double-layer polymer optical waveguide. Background Art

[0002] Compared with traditional electrical interconnection, optical interconnection has obvious advantages in supporting high-speed, large-capacity, low-latency information transmission and resisting electromagnetic interference. Polymer optical waveguides have attracted much attention due to their flexible wiring and compatibility with printed circuit board processes. Compared with conventional waveguides prepared based on hard boards, flexible polymer optical waveguides break through the mechanical constraints of rigid waveguide devices and can achieve flexible bending and movement in any direction and angle in three-dimensional space. They are suitable for high-speed connection application scenarios with small pitch, bending, folding and movable parts. In application areas such as high-density interconnection, flexible double-layer polymer optical waveguides can better achieve high-density, arbitrary-direction interconnection and integration.

[0003] At present, the preparation methods of flexible double-layer polymer optical waveguides mainly use mosquito method, ultraviolet photolithography and hot mold embossing method. Although these methods can achieve certain accuracy and effects, their process flow is relatively complicated, involving multiple steps and requiring precision equipment. For example, the mosquito method requires precise control of the volume and position of the droplets, the ultraviolet photolithography method requires a high-precision lithography process, and the hot mold embossing method involves high temperature and high pressure operations. These complex processes not only increase the preparation cost and time, but also put higher requirements on the technical level of the operator. It is particularly important to find a simpler and more efficient method for preparing flexible double-layer polymer optical waveguides.

[0004] Therefore, it is necessary to provide a method for preparing a flexible double-layer polymer optical waveguide to solve the above technical problems. Summary of the invention

[0005] In order to solve the above technical problems, the present invention provides a method for preparing a flexible double-layer polymer optical waveguide.

[0006] To achieve the above object, the present invention adopts the following technical solution:

[0007] The method for preparing a flexible double-layer polymer optical waveguide provided by the present invention comprises the following steps:

[0008] S1. preparing a soft substrate layer on a hard board substrate by using a soft waveguide substrate glue or a soft waveguide substrate film;

[0009] S2, spin coating a polymer cladding glue to prepare a lower cladding layer on the base layer;

[0010] S3, spin coating a polymer core layer glue, and performing ultraviolet exposure and development to prepare a waveguide core layer on the lower cladding layer to obtain a waveguide core and an identification mark;

[0011] S4, covering the core layer with a cladding layer to obtain a waveguide layer;

[0012] S5, repeat S1-S4 to prepare two identical waveguides, and peel off the hard board substrate of one of the samples;

[0013] S6, placing the waveguide sample substrate containing the hard board substrate downward, placing the waveguide sample substrate containing only the soft waveguide substrate upward, aligning the positions using identification marks, and pressing and fixing;

[0014] S7. Peel off the remaining hard board substrate, and finally prepare a flexible double-layer polymer optical waveguide aligned up and down.

[0015] Preferably, in step S1, the hard board substrate is a PCB board, an SOI substrate, a SiO2 substrate or a glass substrate, and is plasma cleaned and roughened before use to increase the adhesion between the hard board substrate and the soft substrate; the soft substrate is a polyimide film, a PMMA film or other transparent and flexible polymer film, and the prepared soft substrate is prepared by direct spin coating of a soft substrate glue, or the soft substrate film can be directly pressed with the hard board substrate.

[0016] Preferably, in step S2, the polymer coating glue is prepared by spin coating.

[0017] Preferably, in step S3, the optical waveguide and the identification mark can be prepared by using a positive mask in combination with a positive photoresist, or by using a negative mask in combination with a negative photoresist. The identification marks are located on both sides of the waveguide, and the number of the identification marks is 2, 4, 6 or more. In order to improve the recognition accuracy, a metal film can be prepared on the identification mark.

[0018] Preferably, in step S4, the thickness of the upper cladding layer is greater than the thickness of the waveguide core layer.

[0019] Preferably, in step S5, the thickness of the intermediate thin cladding is smaller than the thickness of the cladding in step S3.

[0020] Preferably, in step S6, the waveguide sample whose hard board substrate has not been peeled off is placed with its substrate facing downward, and the waveguide sample whose hard board substrate has been peeled off is placed with its soft substrate facing upward, and the positions of the two waveguide samples are aligned using identification marks, and they are pressed and fixed using embossing technology, or they are directly pasted using quick-drying glue or UV-curing glue.

[0021] Preferably, in step S7, the flexible double-layer polymer optical waveguide is aligned vertically.

[0022] Compared with the related art, the method for preparing the flexible double-layer polymer optical waveguide provided by the present invention has the following beneficial effects:

[0023] The method for preparing a flexible double-layer polymer optical waveguide provided by the present invention is relatively simple to prepare and can be directly prepared by combining the preparation process of a single-layer waveguide with the printing technology. It has high flexibility and high waveguide transmission performance. The method of the present invention is suitable for the requirements of large-scale industrial production of optical waveguide plates and promotes the application of high-density optical waveguide plate interconnection technology. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a schematic flow chart of a method for preparing the flexible double-layer waveguide optical waveguide of the present invention;

[0025] Figure 2 It is a schematic diagram of preparing a soft substrate on a hard board substrate;

[0026] Figure 3 is a schematic diagram of preparing the lower cladding;

[0027] Figure 4 It is a schematic diagram of a positive mask;

[0028] Figure 5 It is a schematic diagram of a negative mask;

[0029] Figure 6 is a schematic diagram of preparing the core layer;

[0030] Figure 7 is a schematic diagram of preparing the upper cladding layer;

[0031] Figure 8 This is a schematic diagram of the soft waveguide after the hard board substrate is peeled off;

[0032] Fig. 9 is a schematic diagram of a flexible double-layer polymer optical waveguide with a rigid substrate;

[0033] Fig.10 Schematic diagram of a flexible double-layer polymer optical waveguide after peeling off the rigid substrate.

[0034] Numbers in the figure: 1. hard board substrate; 2. soft substrate; 3. lower cladding; 4. positive mask light leakage area; 5. positive mask waveguide area; 6. positive mask identification mark area; 7. negative mask light shielding area; 8. negative mask waveguide area; 9. negative mask identification mark area; 10. core layer; 11. upper cladding. DETAILED DESCRIPTION

[0035] The present invention will be further described below in conjunction with the accompanying drawings and implementation modes.

[0036] Embodiment 1:

[0037] A method for preparing a flexible double-layer polymer optical waveguide based on a spin coating process, the process comprising the following steps:

[0038] S1. preparing a soft base layer on a hard board base using a soft waveguide base glue;

[0039] S2, spin coating a polymer cladding glue to prepare a lower cladding layer on the base layer;

[0040] S3, spin coating a polymer core layer glue, and performing ultraviolet exposure and development, preparing a waveguide core layer on the lower cladding layer, obtaining a waveguide core and an identification mark, and performing a metal film covering treatment on the identification mark;

[0041] S4, covering the core layer with a cladding layer to obtain a waveguide layer;

[0042] S5, repeat S1-S4 to prepare two identical waveguides, and peel off the hard board substrate of one of the samples;

[0043] S6, placing the waveguide sample substrate containing the hard board substrate downward, placing the waveguide sample substrate containing only the soft waveguide substrate upward, aligning the positions using identification marks, and pressing and fixing;

[0044] S7. Peel off the remaining hard board substrate, and finally prepare a flexible double-layer polymer optical waveguide aligned up and down.

[0045] The substrate in S1 is a PCB board, an SOI substrate, a SiO2 substrate or a glass substrate. The cleaning process of the PCB board includes ultrasonic cleaning with acetone, alcohol and deionized water. The cleaning process of the SOI substrate, the SiO2 substrate and the glass substrate includes ultrasonic cleaning with acetone, methanol, isopropanol and deionized water, followed by drying with nitrogen and bombarding the surface with plasma to increase the adhesion between the substrate and the cladding glue. The soft base glue in S1 uses polyimide glue, which is spin-coated and cured to reach the soft base layer.

[0046] The lower cladding layer in S2 is obtained by spin coating and curing.

[0047] The mask pattern in the mask plate in S3 is a rectangular waveguide and an identification mark, wherein the waveguide width and length can be designed according to actual needs, the spin coating thickness determines the waveguide height, the mask plate design width and the ultraviolet exposure time determine the waveguide width, the number of rectangular waveguides in each group is N, N is equal to 12 or 4 or 8 or 24 or 48, and the overlay mark is in the form of a cross or a grid, and is located on both sides of the waveguide.

[0048] If the mask in S3 is a positive plate, it is used in combination with a positive cladding adhesive, and if the mask is a negative plate, it is used in combination with a negative cladding adhesive to obtain a waveguide and identification mark structure.

[0049] In the above S4, the thickness of the upper cladding layer is much greater than the thickness of the core layer. If the cladding layer is a negative resist, the entire sample is exposed. If the cladding layer is a positive resist, no exposure is performed.

[0050] In S5, the peeling of the hard board substrate is achieved by blade cutting or liquid immersion.

[0051] In the S6, the identification is performed by observation and alignment using a microscope, and the imprinting is performed by a hot embossing method.

[0052] In S7, the flexible double-layer polymer optical waveguide is aligned up and down.

[0053] Embodiment 2:

[0054] In this example, the soft substrate in step S1 is processed by directly laminating a polyimide film with a FR4 substrate.

[0055] Step S3, using magnetron sputtering to prepare a metal film on the identification mark area to increase the recognition degree of the identification mark.

[0056] In step P6, the upper and lower waveguides are fixed by gluing with quick-drying glue.

[0057] The method for preparing a flexible double-layer polymer optical waveguide provided by the present invention has the following beneficial effects:

[0058] The optical waveguide of the present invention is not affected by the roughness generated by processes such as photolithography, development, and lamination, and is simple and flexible to operate with high preparation efficiency. It can be directly prepared by combining the preparation process of a single-layer waveguide with the imprinting technology, which has high flexibility and high waveguide transmission performance. The method of the present invention is suitable for the requirements of large-scale industrial production of optical waveguide plates, and promotes the application of high-density optical waveguide plate interconnection technology.

[0059] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. A method for preparing a flexible double-layer polymer optical waveguide, characterized in that: Includes steps: S1, preparing a soft substrate layer (2) on a hard board substrate (1); S2, preparing a lower cladding layer (3) on the base layer (2); S3, preparing a waveguide core layer (10) on the lower cladding layer (3); S4, covering the core layer (4) with a cladding layer (11) to obtain a waveguide layer; S5, repeating steps S1-S4 to prepare two waveguides in total, and peeling off the hard board substrate (1) from one of them; S6. Place the two waveguide substrates facing outwards and align and press them together; S7. Peel off the remaining hard board substrate (1) to finally prepare a flexible double-layer polymer optical waveguide.

2. The method for preparing a flexible double-layer polymer optical waveguide according to claim 1, characterized in that: In the S1, the hard board substrate (1) is made of a printed circuit board substrate, a silicon substrate or a glass substrate material, and the soft substrate (2) is made of a polyimide film or a PMMA transparent polymer film with flexibility. The soft substrate (2) is prepared by hot stamping, spin coating or scraper method.

3. The method for preparing a flexible double-layer polymer optical waveguide according to claim 1, characterized in that: In S2, the lower cladding layer (3) is prepared by spin coating, and the refractive index of the lower cladding layer (3) is smaller than the refractive index of the core layer (10).

4. The method for preparing a flexible double-layer polymer optical waveguide according to claim 1, characterized in that: In S3, if the mask is a positive plate, it is used in combination with a positive core layer adhesive, and if the mask is a negative plate, it is used in combination with a negative core layer adhesive to obtain a waveguide core layer and identification marks. The identification marks are located on both sides of the waveguide, and the number of identification marks is 2, 4, 6 or more. The identification marks can be used to prepare a metal film according to the alignment recognition requirements.

5. The method for preparing a flexible double-layer polymer optical waveguide according to claim 1, characterized in that: In the above S4, the thickness of the upper cladding layer (11) is much greater than the thickness of the core layer. If the cladding layer is a negative resist, the entire sample is exposed. If the cladding layer is a positive resist, no exposure is performed.

6. The method for preparing a flexible double-layer polymer optical waveguide according to claim 1, characterized in that: In the above S5, the mask patterns, photolithography, development time, and spin coating thickness process parameters of the two waveguides are kept consistent, and the stripping of the hard board substrate (1) is achieved by blade cutting and liquid immersion process.

7. The method for preparing a flexible double-layer polymer optical waveguide according to claim 1, characterized in that: In S6, the hard board substrate (1) of the waveguide sample from which the hard board substrate has not been peeled off is placed downward, and the soft board substrate (2) of the waveguide sample from which the hard board substrate has been peeled off is placed upward. The positions of the two waveguide samples are aligned using identification marks, and they are pressed together using embossing technology. Quick-drying glue or ultraviolet curing glue can also be used to fix the upper and lower parts.

8. The method for preparing a flexible double-layer polymer optical waveguide according to claim 1, characterized in that: In the above S7, the flexible double-layer polymer optical waveguide is vertically aligned up and down, and the misalignment error is controlled within 2 μm.