Application of platinum-carbon catalyst-loaded electrode in benzyl carbon-hydrogen bond oxidation reaction of aryl compound
The problem of low reaction efficiency and selectivity in the prior art is solved by supporting platinum carbon-hydrogen bond oxidation reaction of aryl compound benzyl carbon catalyst, and efficient catalysis is achieved at room temperature, and the electrode can be reused to reduce the Catalyst preparation cost and step complexity.
Patent Information
- Application Number
- CN202410931639.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-07-12
AI Technical Summary
The existing aryl compounds have low efficiency and selectivity in benzyl carbon-hydrogen bond oxidation reactions, high cost of catalyst preparation, cumbersome steps, and difficult to achieve the recovery and use of catalysts.
In the aryl compound benzyl carbon catalyst-hydrogen bond oxidation reaction, the aryl compound, electrolyte and solvent are mixed under a protective atmosphere, and the electrode supported by the platinum carbon catalyst is used as the cathode and the carbon rod is an anode. , an oxidation reaction was carried out to obtain an oxidation product, and the platinum carbon catalyst was mixed with the Nafion solution and coated on the electrode to prepare a supported platinum carbon catalyst electrode.
The reaction at room temperature and air atmosphere has excellent catalytic effect. It shows high conversion and selectivity for benzyl carbon-hydrogen bond oxidation of various aryl compounds, and the electrode can be reused, reducing the cost of catalyst preparation and step complexity.
Smart Images

Figure CN118895515A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of electrode preparation and synthesis application, and in particular to application of an electrode loaded with a platinum-carbon catalyst in a benzylic carbon-hydrogen bond oxidation reaction of an aromatic compound. Background Art
[0002] The benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds has been developed for decades and is a challenging and significant project. Aromatic side chain compounds such as benzylic aldehydes and ketones are widely used in the fields of pharmacy and fine chemicals, so the synthesis of such compounds has always been a promising research project.
[0003] In recent years, the method for selective oxidation of benzylic carbon-hydrogen bonds is still mainly catalytic oxidation. Although a series of major advances have been made in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds in homogeneous catalytic systems such as transition metal catalytic systems (halogen salts, carboxylates, acetylacetonates of transition metals such as Co, Fe, and Mn) and some metal-free systems, the preparation steps of some photocatalysts are cumbersome and recyclability is difficult to achieve.
[0004] In heterogeneous systems, the use of oxidants is generally required, such as TBHP, NHPI, etc., and the benzylic carbon-hydrogen bond oxidation reaction is only limited to the reaction substrate adaptability range under visible light irradiation and oxygen atmosphere.
[0005] In the electrochemical system, it is generally necessary to add precious metal complexes such as ruthenium complexes, and non-precious metal complexes such as nickel diphosphine complexes, cobalt triphosphine complexes, bionic iron complexes, etc. for electrocatalytic selective oxidation, and use oxygen or water as the oxygen source. The direct utilization efficiency of oxygen in the air is low.
[0006] It can be seen that the existing oxidative activation of the benzylic CH bond of aromatic compounds usually requires the use of transition metal catalysis or the addition of stoichiometric oxidants and relatively harsh reaction conditions, such as high temperature, high oxygen pressure, strong oxidants, etc.
[0007] Therefore, improving the reaction efficiency and selectivity of the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, while reducing the preparation cost of catalysts for the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, simplifying the preparation process, and improving recyclability are technical problems that need to be urgently solved. Summary of the invention
[0008] The purpose of the present invention is to provide an electrode loaded with platinum-carbon catalyst for use in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, so as to solve the problems of low efficiency and selectivity of the prior art benzylic carbon-hydrogen bond oxidation and high preparation cost of the catalyst for the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, complicated preparation steps and inability to be recycled.
[0009] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:
[0010] The invention provides application of an electrode loaded with a platinum-carbon catalyst in a benzylic carbon-hydrogen bond oxidation reaction of an aromatic compound.
[0011] Preferably, in the application of the above-mentioned electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, the application method comprises the following steps:
[0012] Under a protective atmosphere, an aromatic compound, an electrolyte and a solvent are mixed, and an electrode loaded with a platinum-carbon catalyst is used as a cathode and a carbon rod is used as an anode to carry out an oxidation reaction to obtain an oxidation product.
[0013] Preferably, in the application of the above-mentioned electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, the aromatic compound is a chain alkylbenzene with -CH2- at the benzylic position, 1,2,3,4-tetrahydronaphthalene, 1,2,3,4-tetrahydronaphthalene substitutes, indane, indane substitutes, fluorene, fluorene substitutes, 9,10-dihydroanthracene, 9,10-dihydroanthracene substitutes, xanthene or xanthene substitutes;
[0014] The structure of the chain alkylbenzene with -CH2- at the benzyl position is shown in Formula 1:
[0015]
[0016] Among them, R 1 is selected from hydrogen, methyl, ethyl, propyl or butyl; R 2 , R 3 , R 5 , R 6 R is independently selected from hydrogen or ethyl; 4 is selected from hydrogen, methyl, ethyl, a halogen atom or benzyl;
[0017] The 1,2,3,4-tetralin substituent is 5-methyl-1,2,3,4-tetralin, 5-amino-1,2,3,4-tetralin or 5-chloro-1,2,3,4-tetralin;
[0018] The indane substituent is 5-chloro-2,3-dihydro-1H-indene;
[0019] The fluorene substituent is 2-chlorofluorene or 2,7-dichlorofluorene;
[0020] The 9,10-dihydroanthracene substitute is 2-chloro-9,10-dihydroanthracene or 2,6-dimethyl-9,10-dihydroanthracene;
[0021] The xanthene substitute is 2-methylxanthene or 2,4-dimethylxanthene.
[0022] Preferably, in the application of the above-mentioned electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, the preparation method of the electrode loaded with platinum-carbon catalyst comprises the following steps:
[0023] The platinum-carbon catalyst is mixed with a Nafion solution to obtain a suspension, and the suspension is coated on an electrode to obtain an electrode loaded with the platinum-carbon catalyst.
[0024] Preferably, in the application of the above-mentioned electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, the content of platinum in the platinum-carbon catalyst is 10 to 60 wt %;
[0025] The concentration of the Nafion solution is 0.02-0.1 wt %.
[0026] Preferably, in the application of the above-mentioned electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, the dosage ratio of the platinum-carbon catalyst to the Nafion solution is 0.1-10 mg: 500-2000 μL.
[0027] Preferably, in the application of the above-mentioned electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, drying is further included after the coating is completed.
[0028] Preferably, in the application of the above-mentioned electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, the loading amount of platinum-carbon catalyst in the electrode loaded with platinum-carbon catalyst is 0.1-10 mg / 0.1 cm 3 .
[0029] Preferably, in the application of the above-mentioned electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, the protective atmosphere is air or oxygen;
[0030] The electrolyte is tetrabutylammonium tetrafluoroborate;
[0031] The solvent is acetonitrile, dichloromethane, dichloroethane, acetone, methanol or ethanol;
[0032] The usage ratio of the aromatic compound, the electrolyte and the solvent is 0.1-2 mmol: 0.1-2 mmol: 3-10 mL.
[0033] It can be seen from the above technical solution that compared with the prior art, the present invention has the following beneficial effects:
[0034] (1) The electrode loaded with platinum-carbon catalyst provided by the present invention is used as the cathode of the electrochemical reaction. The prepared electrode can directly reduce and activate oxygen, so that the benzylic carbon-hydrogen bond oxidation reaction of the aromatic compound is carried out under mild conditions such as room temperature and air atmosphere. The electrode loaded with platinum-carbon catalyst is used for the benzylic carbon-hydrogen bond oxidation reaction of chain alkylbenzene, and has excellent catalytic effect on the catalytic oxidation of benzylic aromatic compounds having electron-donating substituents or electron-withdrawing substituents on the aromatic ring; it also has excellent catalytic effect on the benzylic oxidation reaction of cyclic aromatic compounds such as 1,2,3,4-tetrahydronaphthalene, indane, and fluorene. It has good substrate adaptability, high oxygen utilization rate, excellent reaction conversion rate and selectivity, and the electrode can be reused. After multiple uses, the yield is still very high.
[0035] (2) Currently, platinum-carbon catalyst materials are generally only used in the field of fuel cells and are rarely used in organic reactions. The present invention provides an application method of a loaded platinum-carbon catalyst electrode in electrochemical organic synthesis. The loaded platinum-carbon catalyst can directly utilize the cathode to activate oxygen in the air, thereby oxidizing the benzylic carbon-hydrogen bond of the aromatic compound.
[0036] (3) The preparation process of the electrode loaded with platinum-carbon catalyst in the present invention is simple and safe. Meanwhile, the raw materials for preparing the electrode loaded with platinum-carbon catalyst are easily available, the equipment for preparing the electrode is simple, and the operation is simple. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required to be used in the description of the embodiments or the prior art are briefly introduced below.
[0038] Figure 1 The scanning electron microscope characterization of the electrode loaded with platinum-carbon catalyst in Example 1;
[0039] Figure 2 This is an electron paramagnetic resonance spectrum of the superoxide radical anion generated by the reaction on the electrode of the platinum-carbon catalyst in Example 1. DETAILED DESCRIPTION
[0040] The invention provides application of an electrode loaded with a platinum-carbon catalyst in a benzylic carbon-hydrogen bond oxidation reaction of an aromatic compound.
[0041] In the present invention, the application method comprises the following steps:
[0042] Under a protective atmosphere, an aromatic compound, an electrolyte and a solvent are mixed, and an electrode loaded with a platinum-carbon catalyst is used as a cathode and a carbon rod is used as an anode to carry out an oxidation reaction to obtain an oxidation product.
[0043] In the present invention, the aromatic compound is preferably a chain alkylbenzene with -CH2- at the benzyl position, 1,2,3,4-tetralin, 1,2,3,4-tetralin substitution, indane, indane substitution, fluorene, fluorene substitution, 9,10-dihydroanthracene, 9,10-dihydroanthracene substitution, xanthene or xanthene substitution;
[0044] The structure of the chain alkylbenzene with -CH2- at the benzyl position is shown in Formula 1:
[0045]
[0046] Among them, R 1 is selected from hydrogen, methyl, ethyl, propyl or butyl; R 2 , R 3 , R 5 , R 6 R is independently selected from hydrogen or ethyl; 4 is selected from hydrogen, methyl, ethyl, a halogen atom or benzyl;
[0047] The 1,2,3,4-tetralin substituent is preferably 5-methyl-1,2,3,4-tetralin, 5-amino-1,2,3,4-tetralin or 5-chloro-1,2,3,4-tetralin;
[0048] The indane substituent is preferably 5-chloro-2,3-dihydro-1H-indene;
[0049] The fluorene substituent is preferably 2-chlorofluorene or 2,7-dichlorofluorene;
[0050] The 9,10-dihydroanthracene substitute is preferably 2-chloro-9,10-dihydroanthracene or 2,6-dimethyl-9,10-dihydroanthracene;
[0051] The xanthene substitute is preferably 2-methylxanthene or 2,4-dimethylxanthene.
[0052] In the present invention, the method for preparing the electrode loaded with platinum-carbon catalyst comprises the following steps:
[0053] The platinum-carbon catalyst is mixed with a Nafion solution to obtain a suspension, and the suspension is coated on an electrode to obtain an electrode loaded with the platinum-carbon catalyst.
[0054] In the present invention, the content of platinum in the platinum-carbon catalyst is preferably 10 to 60 wt %, more preferably 20 to 50 wt %, and more preferably 40 wt %.
[0055] In the present invention, the platinum-carbon catalyst is a commercially available platinum-carbon catalyst.
[0056] In the present invention, the concentration of the Nafion solution is preferably 0.02 to 0.1 wt %, more preferably 0.04 to 0.08%, and even more preferably 0.05%.
[0057] In the present invention, the usage ratio of the platinum-carbon catalyst to the Nafion solution is preferably 0.1-10 mg: 500-2000 μL, more preferably 0.5-5 mg: 800-1500 μL, and more preferably 1 mg: 1000 μL.
[0058] In the present invention, the mixing temperature is 20-25°C, more preferably 21-24°C, and more preferably 22-23°C; the mixing time is preferably 20-40 min, more preferably 25-35 min, and more preferably 30 min.
[0059] In the present invention, the mixing method is preferably ultrasonic mixing.
[0060] In the present invention, the coating process further includes drying; the drying temperature is 50 to 65°C, more preferably 52 to 63°C, and more preferably 55 to 60°C.
[0061] In the present invention, the electrode is preferably a graphite felt electrode.
[0062] In the present invention, the thickness of the graphite felt electrode is preferably 1 mm, and the size of the graphite felt electrode is preferably 1 cm×1 cm.
[0063] In the present invention, the loading amount of the platinum-carbon catalyst in the electrode loaded with the platinum-carbon catalyst is preferably 0.1 to 10 mg / 0.1 cm 3 , more preferably 2 to 8 mg / 0.1 cm 3 , more preferably 5 to 6 mg / 0.1 cm 3 .
[0064] In the present invention, the protective atmosphere is preferably air or oxygen, more preferably oxygen.
[0065] In the present invention, the electrolyte is preferably tetrabutylammonium tetrafluoroborate.
[0066] In the present invention, the solvent is preferably acetonitrile, dichloromethane, dichloroethane, acetone, methanol or ethanol.
[0067] In the present invention, the usage ratio of the aromatic compound, electrolyte and solvent is preferably 0.1-2 mmol: 0.1-2 mmol: 3-10 mL, more preferably 0.5-1 mmol: 0.5-1 mmol: 4-7 mL, and more preferably 0.5 mmol: 0.5 mmol: 5 mL.
[0068] In the present invention, the conditions of the oxidation reaction are: the temperature is preferably 20-25°C, more preferably 21-24°C, more preferably 22-23°C; the time is preferably 1-6h, more preferably 2-4h, more preferably 3h; the constant current is preferably 3-20mA, more preferably 6-14mA, more preferably 10mA.
[0069] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0070] In the following examples, the platinum-carbon catalyst was purchased from Suzhou Shengernuo Technology Co., Ltd., model number PremetekSPT40;
[0071] The Nafion solution was purchased from Beijing Inokai Technology Co., Ltd., model A40008.
[0072] Example 1
[0073] 1 mg of platinum carbon catalyst with a platinum content of 40 wt% was ultrasonically mixed with 1000 μL of Nafion solution with a concentration of 0.05 wt% at 25°C for 30 min to obtain a suspension, which was coated on a graphite felt electrode with a size of 1 cm×1 cm and a thickness of 1 mm, and dried at 60°C to obtain a platinum carbon catalyst with a loading of 1 mg / 0.1 cm 3 Electrode loaded with platinum-carbon catalyst.
[0074] Figure 1 The scanning electron microscopy characterization of the electrode loaded with platinum-carbon catalyst prepared in Example 1. Figure 1 It can be seen that the electrode loaded with platinum-carbon catalyst is a nanocluster structure.
[0075] Figure 2 This is the electron paramagnetic resonance spectrum of the superoxide radical anion generated by the electrode reaction of the captured supported platinum carbon catalyst in Example 1. Figure 2 It can be seen that the electrode loaded with platinum-carbon catalyst as a cathode can effectively reduce oxygen in the air to superoxide radical anions, thereby activating oxygen.
[0076] The electrode loaded with platinum-carbon catalyst prepared in Example 1 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The reaction process was as follows:
[0077]
[0078] The method of application comprises the following steps:
[0079] In an air atmosphere, 0.5 mmol 1,2,3,4-tetrahydronaphthalene, 0.5 mmol tetrabutylammonium tetrafluoroborate (n-Bu4NBF4) as electrolyte, carbon rod as anode, the electrode loaded with platinum carbon catalyst prepared in Example 1 as cathode, 5 mL acetonitrile as solvent were placed in an open position; the reaction was stirred at a constant current of 10 mA and 25°C for 3 h, and the obtained mixture was analyzed by high performance liquid chromatography after the reaction was completed. The conditions of high performance liquid chromatography analysis were: wavelength of 210 nm, and mobile phase selected as V (acetonitrile): V (deionized water) = 50:50. After testing, the reaction conversion rate was 95%, the selectivity was 95%, and the yield was 90%.
[0080] Example 2
[0081] 1 mg of platinum carbon catalyst with a platinum content of 10 wt% was ultrasonically mixed with 1000 μL of Nafion solution with a concentration of 0.05 wt% at 25 ° C for 30 min to obtain a suspension, which was coated on a graphite felt electrode with a size of 1 cm × 1 cm and a thickness of 1 mm, and dried at 60 ° C to obtain a platinum carbon catalyst with a loading of 1 mg / 0.1 cm 3 Electrode loaded with platinum-carbon catalyst.
[0082] The electrode loaded with platinum-carbon catalyst prepared in Example 2 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The reaction process was as follows:
[0083]
[0084] The method of application comprises the following steps:
[0085] In an air atmosphere, 0.5 mmol 1,2,3,4-tetrahydronaphthalene, 0.5 mmol tetrabutylammonium tetrafluoroborate (n-Bu4NBF4) as electrolyte, carbon rod as anode, the electrode loaded with platinum carbon catalyst prepared in Example 2 as cathode, 5 mL acetonitrile as solvent, and placed in an open position; the reaction was stirred at a constant current of 10 mA and 25°C for 3 hours, and the obtained mixture was analyzed by high performance liquid chromatography after the reaction was completed. The conditions of high performance liquid chromatography analysis were: wavelength of 210 nm, and mobile phase selected as V (acetonitrile): V (deionized water) = 50:50. After testing, the reaction conversion rate was 85%, the selectivity was 90%, and the yield was 77%.
[0086] Example 3
[0087] 1 mg of platinum carbon catalyst with a platinum content of 20 wt% was ultrasonically mixed with 1000 μL of Nafion solution with a concentration of 0.05 wt% at 25°C for 30 min to obtain a suspension, which was coated on a graphite felt electrode with a size of 1 cm×1 cm and a thickness of 1 mm, and dried at 60°C to obtain a platinum carbon catalyst with a loading of 1 mg / 0.1 cm 3 Electrode loaded with platinum-carbon catalyst.
[0088] The electrode loaded with platinum-carbon catalyst prepared in Example 3 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The reaction process was as follows:
[0089]
[0090] The method of application comprises the following steps:
[0091] Under air atmosphere, 0.5mmol 1,2,3,4-tetrahydronaphthalene, 0.5mmol tetrabutylammonium tetrafluoroborate (n-Bu4NBF4) as electrolyte, carbon rod as anode, the electrode loaded with platinum carbon catalyst prepared in Example 3 as cathode, 5mL acetonitrile as solvent were placed in an open position in a 25mL three-mouth reactor; the reaction was stirred at a constant current of 10mA and 25°C for 3h, and the obtained mixture was analyzed by high performance liquid chromatography after the reaction was completed. The conditions of high performance liquid chromatography analysis were: wavelength of 210nm, mobile phase selected as V (acetonitrile): V (deionized water) = 50:50. After testing, the reaction conversion rate was 87%, the selectivity was 92%, and the yield was 80%.
[0092] Example 4
[0093] 1 mg of platinum carbon catalyst with a platinum content of 60 wt% was ultrasonically mixed with 1000 μL of Nafion solution with a concentration of 0.05 wt% at 25°C for 30 min to obtain a suspension, which was coated on a graphite felt electrode with a size of 1 cm×1 cm and a thickness of 1 mm, and dried at 60°C to obtain a platinum carbon catalyst with a loading of 1 mg / 0.1 cm 3 Electrode loaded with platinum-carbon catalyst.
[0094] The electrode loaded with platinum-carbon catalyst prepared in Example 4 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The reaction process was as follows:
[0095]
[0096] The method of application comprises the following steps:
[0097] In an air atmosphere, 0.5 mmol 1,2,3,4-tetrahydronaphthalene, 0.5 mmol tetrabutylammonium tetrafluoroborate (n-Bu4NBF4) as electrolyte, carbon rod as anode, the electrode loaded with platinum carbon catalyst prepared in Example 4 as cathode, 5 mL acetonitrile as solvent were placed in an open position; the reaction was stirred at a constant current of 10 mA and 25°C for 3 h, and the obtained mixture was analyzed by high performance liquid chromatography after the reaction was completed. The conditions of high performance liquid chromatography analysis were: wavelength of 210 nm, and mobile phase selected as V (acetonitrile): V (deionized water) = 50:50. After testing, the reaction conversion rate was 96%, the selectivity was 95%, and the yield was 91%.
[0098] Example 5
[0099] The electrode loaded with platinum-carbon catalyst prepared in Example 1 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The application method was the same as that in Example 1, except that tetrabutylammonium hexafluorophosphate (n-Bu4NPF6), tetrabutylammonium acetate (n-Bu4N(OAc)2), tetrabutylammonium perchlorate (n-Bu4NClO4), LiBr, and LiClO4 were used as electrolytes, respectively. The reaction results are shown in Table 1.
[0100] Table 1 Reaction results in Example 5
[0101] Electrolytes Selectivity (%) Conversion rate (%) Yield (%) <![CDATA[n-Bu4NPF6]]> 93 83 77 <![CDATA[n-Bu4N(OAc)2]]> 87 75 65 <![CDATA[n-Bu4NClO4]]> 91 77 70 LiBr 91 33 30 <![CDATA[LiClO4]]> 93 68 63
[0102] Example 6
[0103] The electrode loaded with platinum-carbon catalyst prepared in Example 1 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The reaction process was as follows:
[0104]
[0105] The method used is the same as that in Example 1, except that dichloromethane (DCM), dichloroethane (DCE), acetone (Acetone), methanol (MeOH), and ethanol (EtOH) are used as solvents, respectively. The reaction results are shown in Table 2.
[0106] Table 2 Reaction results in Example 6
[0107] Electrolytes Selectivity (%) Conversion rate (%) Yield (%) DCM 93 31 29 DCE 94 24 23 Acetone 93 61 57 MeOH 95 38 36 EtOH 97 80 78
[0108] Example 7
[0109] Different electrodes were applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The application method was consistent with that in Example 1, except that: a carbon rod was used as an anode and platinum was used as a cathode (C(+)|Pt(-)); a carbon rod was used as an anode and a carbon rod was used as a cathode (C(+)|C(-)); a carbon rod was used as an anode and a nickel was used as a cathode (C(+)|Ni(-)); platinum was used as an anode and the electrode loaded with a platinum-carbon catalyst prepared in Example 1 was used as a cathode (Pt(+)|Pt / C(-)); platinum was used as an anode and a platinum was used as a cathode (Pt(+)|Pt(-)); the reaction results are shown in Table 3.
[0110] Table 3 Reaction results in Example 7
[0111] electrode Selectivity (%) Conversion rate (%) Yield (%) C(+)|Pt(-) 98 28 27 C(+)|C(-) 86 43 37 C(+)|Ni(-) 90 56 50 Pt(+)|Pt / C(-) 82 75 62 Pt(+)|Pt(-) 79 21 17
[0112] Example 8
[0113] The electrode loaded with platinum-carbon catalyst prepared in Example 1 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The application method was consistent with that in Example 1, except that N2 and O2 were used as protective atmospheres, respectively. The reaction results are shown in Table 4.
[0114] Table 4 Reaction results in Example 8
[0115] Protective atmosphere Selectivity (%) Conversion rate (%) Yield (%) <![CDATA[N2]]> 0 0 0 <![CDATA[O2]]> 95 96 91
[0116] Example 9
[0117] The electrode loaded with platinum-carbon catalyst prepared in Example 1 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The application method was the same as that in Example 1, except that the constant current was changed to 5 mA and 20 mA. The reaction results are shown in Table 5.
[0118] Table 5 Reaction results in Example 9
[0119] Constant current Selectivity (%) Conversion rate (%) Yield (%) 5mA 93 27 25 20mA 83 60 50
[0120] Example 10
[0121] The electrode loaded with platinum-carbon catalyst prepared in Example 1 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The application method was the same as that in Example 1, except that the reaction time was changed to 1.5 h, 6 h, and 12 h. The reaction results are shown in Table 6.
[0122] Table 6 Reaction results in Example 10
[0123] Reaction time Selectivity (%) Conversion rate (%) Yield (%) 1.5h 93 58 54 6h 88 75 66 12h 75 70 53
[0124] Embodiment 11
[0125] The electrode loaded with platinum-carbon catalyst prepared in Example 1 was applied to the benzylic carbon-hydrogen bond oxidation reaction of 1,2,3,4-tetralin. The application method was the same as that in Example 1, except that the reaction was repeated 5 times using the electrode loaded with platinum-carbon catalyst prepared in Example 1. The reaction results are shown in Table 7.
[0126] Table 7 Reaction results in Example 11
[0127]
[0128]
[0129] Example 12
[0130] The electrode loaded with platinum-carbon catalyst prepared in Example 1 was applied to the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds. The application method was the same as that in Example 1, except that the aromatic compound was changed.
[0131] The yields of different aromatic compounds are as follows:
[0132] The aromatic compound is ethylbenzene and the product is The yield is 90%;
[0133] The aromatic compound is 4-ethyltoluene and the product is The yield is 69%;
[0134] The aromatic compound is 1,4-diethylbenzene and the product is The yield is 82%;
[0135] The aromatic compound is 1-bromo-4-ethylbenzene and the product is The yield is 74%;
[0136] The aromatic compound is 1-chloro-4-ethylbenzene and the product is The yield is 82%;
[0137] The aromatic compound is propylbenzene, and the product is The yield is 81%;
[0138] The aromatic compound is n-butylbenzene and the product is The yield is 77%;
[0139] The aromatic compound is pentylbenzene and the product is The yield is 67%;
[0140] The aromatic compound is 1,2-diethylbenzene and the product is The yield is 75%;
[0141] The aromatic compound is 1,3,5-triethylbenzene and the product is The yield is 65%;
[0142] The aryl compound is diphenylmethane and the product is The yield is 77%;
[0143] The aromatic compound is 5-methyl-1,2,3,4-tetrahydronaphthalene, and the product is The yield is 70%; the aromatic compound is 5-amino-1,2,3,4-tetrahydronaphthalene, and the product is The yield is 69%; the aromatic compound is 5-chloro-1,2,3,4-tetrahydronaphthalene, and the product is The yield is 75%; the aromatic compound is indane, and the product is The yield is 89%;
[0144] The aryl compound is 5-chloro-2,3-dihydro-1H-indene, and the product is The yield is 80%; the aromatic compound is fluorene, and the product is The yield is 81%;
[0145] The aromatic compound is 2-chlorofluorene, and the product is The yield is 75%;
[0146] The aromatic compound is 2,7-dichlorofluorene and the product is The yield is 75%;
[0147] The aromatic compound is 9,10-dihydroanthracene, and the product is The yield is 80%;
[0148] The aromatic compound is 2-chloro-9,10-dihydroanthracene, and the product is The yield is 78%;
[0149] The aromatic compound is 2,6-dimethyl-9,10-dihydroanthracene, and the product is The yield is 75%;
[0150] The aromatic compound is xanthene, and the product is The yield is 77%;
[0151] The aromatic compound is 2-methylxanthene and the product is The yield is 72%;
[0152] The aromatic compound is 2,4-dimethylxanthene and the product is The yield is 73%;
[0153] The aromatic compound is 4-ethylbiphenyl and the product is The yield is 45%;
[0154] The aromatic compound is 4-n-propylbiphenyl, and the product is The yield is 41%;
[0155] The aromatic compound is 4-bromo-4'-ethylbiphenyl, and the product is The yield is 44%;
[0156] The aryl compound is 2-ethylnaphthalene and the product is The yield is 50%;
[0157] The aromatic compound is toluene and the product is The yield is 89%;
[0158] The aromatic compound is 1,4-dimethylbenzene and the product is The yield is 84%;
[0159] The aromatic compound is mesitylene, and the product is The yield was 81%.
[0160] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. Application of an electrode loaded with platinum-carbon catalyst in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds.
2. The use of the electrode loaded with platinum-carbon catalyst according to claim 1 in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, characterized in that: The application method comprises the following steps: Under a protective atmosphere, an aromatic compound, an electrolyte and a solvent are mixed, and an electrode loaded with a platinum-carbon catalyst is used as a cathode and a carbon rod is used as an anode to carry out an oxidation reaction to obtain an oxidation product.
3. The use of the electrode loaded with platinum-carbon catalyst according to claim 2 in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, characterized in that: The aromatic compound is a chain alkylbenzene with -CH2- at the benzyl position, 1,2,3,4-tetralin, 1,2,3,4-tetralin substitution, indane, indane substitution, fluorene, fluorene substitution, 9,10-dihydroanthracene, 9,10-dihydroanthracene substitution, xanthene or xanthene substitution; the structure of the chain alkylbenzene with -CH2- at the benzyl position is as shown in Formula 1: Among them, R 1 is selected from hydrogen, methyl, ethyl, propyl or butyl; R 2 , R 3 , R 5 , R 6 R is independently selected from hydrogen or ethyl; 4 is selected from hydrogen, methyl, ethyl, a halogen atom or benzyl; The 1,2,3,4-tetralin substituent is 5-methyl-1,2,3,4-tetralin, 5-amino-1,2,3,4-tetralin or 5-chloro-1,2,3,4-tetralin; The indane substituent is 5-chloro-2,3-dihydro-1H-indene; The fluorene substituent is 2-chlorofluorene or 2,7-dichlorofluorene; The 9,10-dihydroanthracene substitute is 2-chloro-9,10-dihydroanthracene or 2,6-dimethyl-9,10-dihydroanthracene; The xanthene substitute is 2-methylxanthene or 2,4-dimethylxanthene.
4. The use of the electrode loaded with platinum-carbon catalyst according to claim 2 in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, characterized in that: The method for preparing the electrode loaded with platinum-carbon catalyst comprises the following steps: The platinum-carbon catalyst is mixed with a Nafion solution to obtain a suspension, and the suspension is coated on an electrode to obtain an electrode loaded with the platinum-carbon catalyst.
5. The use of the platinum-carbon catalyst-supported electrode according to claim 4 in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, characterized in that: The platinum content in the platinum-carbon catalyst is 10 to 60 wt %; The concentration of the Nafion solution is 0.02-0.1 wt %.
6. Use of the electrode loaded with platinum-carbon catalyst according to claim 4 in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, characterized in that: The usage ratio of the platinum-carbon catalyst to the Nafion solution is 0.1-10 mg: 500-2000 μL.
7. Use of the electrode loaded with platinum-carbon catalyst according to claim 5 in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, characterized in that: The coating process further includes drying.
8. Use of the electrode loaded with platinum-carbon catalyst according to claim 5 or 6 in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, characterized in that: The loading amount of the platinum-carbon catalyst in the electrode loaded with the platinum-carbon catalyst is 0.1 to 10 mg / 0.1 cm 3 .
9. Use of the electrode loaded with platinum-carbon catalyst according to claim 8 in the benzylic carbon-hydrogen bond oxidation reaction of aromatic compounds, characterized in that: The protective atmosphere is air or oxygen; The electrolyte is tetrabutylammonium tetrafluoroborate; The solvent is acetonitrile, dichloromethane, dichloroethane, acetone, methanol or ethanol; The usage ratio of the aromatic compound, the electrolyte and the solvent is 0.1-2 mmol: 0.1-2 mmol: 3-10 mL.
Citation Information
Patent Citations
Synthesis method of 9-aryl-9H-oxo / thioxanthene compound
CN113322479A
Method for preparing aromatic aldehyde ketone compound based on electro-catalysis
CN114351172A
Supported heterostructure nano electro-catalytic material AB (at) (ABOx)-(A / B-)-L-C and preparation
CN115418661A
Method for synthesizing aromatic-substituted alicyclic ketone compound
JP2009155299A
Rotor and turbo-machine comprising the same
KR102284507B1
Cited By
Electrochemical oxidation method for selective benzyl carbon-hydrogen bonds
CN119082750A
Method for constructing planar chiral [2, 2] paracyclophane through cobalt-catalyzed asymmetric carbon-hydrogen bond activation-kinetic resolution
CN119530825A
A method for constructing facially chiral [2,2]paracyclophanes by cobalt-catalyzed asymmetric carbon-hydrogen bond activation-kinetic resolution
CN119530825B
Method for preparing indan compound under electrochemical condition
CN120041846A