Solar cell metallization method and solar cell

By combining screen printing with light-induced and electric field-induced plating methods, the problems of high silver consumption and process complexity in solar cells are solved, and silver consumption is reduced and solar cell performance is improved.

CN118738159APending Publication Date: 2024-10-01TRINA SOLAR CO LTD

Patent Information

Application Number
CN202411106035.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The existing solar cell metallization technology consumes a lot of silver, which leads to increased costs, and the traditional process is highly complex, making it difficult to effectively control the aspect ratio and line resistance of the silver grid lines.

Method used

Screen printing is used to prepare silver grating lines, and a preset metal layer is electroplated on the surface of the silver grating lines by combining light-induced electroplating and electric field-induced plating methods, avoiding laser grooves and mask exposure steps, reducing silver consumption and process complexity, and being flexible Control the aspect ratio of the gate line to improve the ability to derive carriers.

Benefits of technology

It achieves reduced silver consumption, lowers production costs, improves the photoelectric conversion efficiency and performance of solar cells, simplifies the process flow, and reduces open voltage losses.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738159A_ABST
    Figure CN118738159A_ABST
Patent Text Reader

Abstract

The invention relates to a solar cell metallization method and a solar cell. First silver grid lines are prepared on the first surface of a cell piece through silk-screen printing, and second silver grid lines are prepared on the second surface of the cell piece through silk-screen printing; electroplating a first preset metal layer on the surface of the first silver grid line through a light-induced electroplating method; and electroplating a second preset metal layer on the surface of the second silver grid line through an electric field induced electroplating method. According to the method, the traditional steps of laser grooving, mask exposure, back etching and the like can be avoided, so that the production cost and the process complexity are greatly reduced, and the opening pressure loss is reduced; in addition, a first preset metal layer and a second preset metal layer are respectively electroplated on the surfaces of the first silver grid line and the second silver grid line by using a light-induced electroplating method and an electric field-induced electroplating method in a mixed way, so that the height-width ratio of the grid lines can be changed and flexibly controlled according to requirements, and a metal grid line structure with a composite structure with a good height-width ratio can be prepared; light incoming is improved, overall line resistance is reduced, good carrier export capability is achieved, and silver consumption is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of solar cells, and in particular to a solar cell metallization method and a solar cell. Background Art

[0002] The photovoltaic industry is developing rapidly. Currently, TOPCON cells and heterojunction cells are gradually replacing PERC cells and becoming the mainstream of the market due to their excellent conversion efficiency. However, with the increase in battery production, the consumption of silver paste also increases. According to incomplete statistics, the silver consumption of the photovoltaic industry accounts for about 10% of the global annual silver production. Due to the high price of silver, the cost of the battery remains high. Therefore, reducing silver consumption is crucial to saving costs. However, the existing metallization technology has a high silver consumption, which is not conducive to cost control. Summary of the invention

[0003] Based on this, it is necessary to provide a solar cell metallization method and a solar cell that can reduce silver consumption in order to solve the above technical problems.

[0004] In a first aspect, the present application provides a solar cell metallization method, the method comprising:

[0005] Prepare a first silver grid line on the first surface of the battery cell and prepare a second silver grid line on the second surface by screen printing; the first surface and the second surface are two opposite sides of the battery cell;

[0006] Electroplating a first preset metal layer on the surface of the first silver grid line by light-induced electroplating; Electroplating a first preset metal layer on the surface of the first silver grid line;

[0007] A second preset metal layer is electroplated on the surface of the second silver grid line by electric field induced electroplating.

[0008] In one embodiment, electroplating the first preset metal layer on the surface of the first silver grid line by light-induced electroplating includes:

[0009] Providing a first auxiliary electrode; the first auxiliary electrode is made of a preset metal;

[0010] Electrically connecting the first auxiliary electrode and the first silver grid line disposed in a preset electrolyte;

[0011] Applying a preset bias voltage to the cell through the first auxiliary electrode and the first silver grid line;

[0012] Preset lighting conditions are provided to photo-induce the cell sheet so as to electroplate the first preset metal layer on the surface of the first silver grid line.

[0013] In one embodiment, providing a preset light condition to photo-induce the cell to electroplate the first preset metal layer on the surface of the first silver grid line includes:

[0014] Provide a dark space;

[0015] A preset lighting condition is provided in the light-proof space to photo-induce the cell sheet so as to electroplate the first preset metal layer on the surface of the first silver grid line.

[0016] In one embodiment, the preset illumination conditions include: the illumination wavelength λ satisfies the condition: 400nm≤λ≤800nm; the light intensity I satisfies the condition: 25mW / cm 2 ≤I≤60mW / cm 2 ; The lighting time t1 meets the conditions: 4min≤t1≤8min.

[0017] In one embodiment, electroplating the second preset metal layer on the surface of the second silver grid line by electric field induced electroplating includes:

[0018] Providing a second auxiliary electrode; the second auxiliary electrode is made of a preset metal;

[0019] Placing the second silver grid line and the second auxiliary electrode in a preset electrolyte;

[0020] Under a preset power supply condition, a voltage is applied to the first silver grid line and the second auxiliary electrode to electroplate the second preset metal layer on the surface of the second silver grid line.

[0021] In one embodiment, the preset power supply conditions include: the target constant current i satisfies the condition: 0.1A≤i≤0.5A; the first power supply time t2 satisfies the condition: 1min≤t2≤30min; the first ambient temperature T1 satisfies the condition: 20℃≤T1≤50℃.

[0022] In one embodiment, the preset power supply conditions include: the target constant voltage v satisfies the condition: 0.4V≤v≤2V; the second power supply time t3 satisfies the condition: 1min≤t3≤30min; the second ambient temperature T2 satisfies the condition: 25℃≤T2≤60℃.

[0023] In one embodiment, the preset metal includes one of copper, aluminum, and nickel.

[0024] In one embodiment, the thickness of the first preset metal layer and the second preset metal layer are both 4um~6μm.

[0025] In one embodiment, the first silver grid lines are prepared on the first surface of the cell and the second silver grid lines are prepared on the second surface by screen printing, including:

[0026] Preparing a first silver main grid line and a first silver fine grid line on the first surface of the battery cell by screen printing;

[0027] Prepare a second silver main grid line and a second silver fine grid line on the second surface of the battery cell by screen printing;

[0028] The first silver main grid line, the first silver thin grid line, the second silver main grid line and the second silver thin grid line are sintered.

[0029] In one embodiment, the width of the first silver fine grid line is 15um-25um.

[0030] In one embodiment, the aspect ratio of the second silver fine grid line is 5% to 20%.

[0031] In one embodiment, the height of the second silver fine grid line is 5um~5um, and the width of the second silver fine grid line is 3um~7um.

[0032] In a second aspect, the present application further provides a solar cell, comprising:

[0033] A second silver fine grid line is provided on the second surface of the battery cell; the height-to-width ratio of the second silver fine grid line is 5% to 20%;

[0034] The second preset metal layer is disposed on a side of the second silver fine grid line facing away from the second surface.

[0035] In one embodiment, it also includes:

[0036] A first silver fine grid line is provided on a first surface of the battery cell; the first surface is opposite to the second surface;

[0037] The first preset metal layer is disposed on a side of the first silver fine grid line facing away from the first surface.

[0038] In one embodiment, the width of the first silver fine grid line is 15um-25um.

[0039] In one embodiment, the thickness of the first preset metal layer and the second preset metal layer are both 4um~6μm.

[0040] In one embodiment, the height of the second silver fine grid line is 5um~5um, and the width of the second silver fine grid line is 3um~7um.

[0041] The above-mentioned solar cell metallization method and solar cell respectively prepare the first silver grid line on the first surface of the cell sheet and the second silver grid line on the second surface by screen printing; electroplate the first preset metal layer on the surface of the first silver grid line by light-induced electroplating; and electroplate the second preset metal layer on the surface of the second silver grid line by electric field-induced electroplating. That is, the present application prepares the first silver grid line and the second silver grid line by screen printing, avoiding the use of traditional laser grooving, mask exposure, back-engraving and other steps, greatly reducing the production cost and process complexity, and reducing the opening voltage loss. In addition, the light-induced electroplating method and the electric field-induced electroplating method are mixed to electroplate the first preset metal layer and the second preset metal layer on the surface of the first silver grid line and the second silver grid line, respectively, so that the preset metal plated on the surface of the first silver grid line and the second silver grid line is more uniform, and the aspect ratio of the grid line can be flexibly controlled according to the needs, so that a metal grid line structure with a composite structure having a good aspect ratio can be prepared, which improves light intake and reduces the overall line resistance, achieves a good carrier extraction capability, and reduces silver consumption. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] In order to more clearly illustrate the technical solutions in the embodiments of the present application or related technologies, the drawings required for use in the embodiments of the present application or related technical descriptions will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.

[0043] Figure 1 is a schematic flow chart of a solar cell metallization method in one embodiment;

[0044] Figure 2 It is a schematic diagram of a process of electroplating a first preset metal layer on the surface of a first silver grid line by light-induced electroplating in one embodiment;

[0045] Figure 3 It is a schematic diagram of a process of electroplating a second preset metal layer on the surface of a second silver grid line by electric field induced electroplating in one embodiment;

[0046] Figure 4 It is a schematic diagram of a process of preparing a first silver grid line on a first surface of a battery cell and preparing a second silver grid line on a second surface by screen printing in one embodiment;

[0047] Figure 5 A solar cell prepared by a TOPCon cell metallization method in one embodiment;

[0048] Figure 6 A solar cell prepared by the electroplating method in the first comparative example;

[0049] Figure 7This is a solar cell manufactured using the screen printing process in the second comparative example. DETAILED DESCRIPTION

[0050] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0051] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0052] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of this application, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0053] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0054] In this field, mature metallization solutions all complete the metallization process by screen printing silver paste, and the aspect ratio of the metal grid line is difficult to control, and the line resistance of the metal silver grid line is relatively large.

[0055] In order to reduce the cost of silicon solar cells and improve the efficiency of cells, electroplating copper grid line technology has been introduced in this field to replace the screen printing silver paste technology. The electroplating process mainly involves four steps: 1. First, the seed layer is deposited on the surface of the silicon solar cell by PVD method (to improve the adhesion of the electroplated copper grid line); 2. The passivation reflective layer (SiNx) on the surface is opened by laser grooving and other technologies to expose the n-Si substrate, and the nickel seed layer is deposited by PVD method; 3. Then the copper grid line is electroplated; 4. The seed layer outside the patterned area is removed by etching, cleaning and other steps to complete the copper metallization process. However, since expensive physical vapor deposition (PVD) and other equipment are required in this process, and the preparation of the seed layer increases the process complexity and cost, it is difficult to achieve the effect of reducing costs. In addition, laser grooving will damage the c-Si substrate and cause voltage loss. The subsequent etching and cleaning steps increase the process and cost.

[0056] In one embodiment, the present application also provides a solar cell metallization method, see the attached Figure 1 , attached Figure 1 The schematic flow chart of the solar cell metallization method in this embodiment is shown. The solar cell metallization method in this embodiment includes the following steps S101 to S103.

[0057] Step S101 , preparing a first silver grid line on a first surface of a cell and preparing a second silver grid line on a second surface by screen printing; the first surface and the second surface are two opposite sides of the cell.

[0058] Among them, the cell refers to the blue film cell, that is, the cell that is not metallized after coating. The first surface and the second surface of the cell refer to the front side facing the sunlight and the back side opposite to the front side, respectively. In this application, the first surface is the back side of the cell and the second surface is the front side of the cell for explanation.

[0059] In step S101, a relatively low metal silver grid line is first printed through a conventional screen printing process, which reduces silver consumption and serves as an adaptive seed layer for a subsequent electroplating process, thereby enhancing the adhesion of the first preset metal layer, the second preset metal layer and the silver metal grid line, and improving the reliability of the solar cell. In addition, it avoids the use of traditional laser grooving, mask exposure, back engraving and other steps, greatly reducing production costs and process complexity, and reducing opening voltage losses.

[0060] Step S102: electroplating a first preset metal layer on the surface of the first silver grid line by light-induced electroplating.

[0061] Photoinduced electroplating is a technology that uses light energy to initiate or control the deposition of metal ions on a specific surface. When the cell absorbs light energy, a photovoltaic reaction is performed. When an external light source shines on the pn junction of the cell, holes are generated in the p region and electrons are generated in the n region. These electrons then reduce the metal ions in the solution, thereby forming a deposited layer of a preset metal on the surface of the first silver grid line, thereby achieving the electroplating of the first preset metal layer on the surface of the first silver grid line.

[0062] Step S103, electroplating a second preset metal layer on the surface of the second silver grid line by electric field induced plating method.

[0063] The second preset metal layer and the first preset metal layer have the same preset metal type, and the preset metal can be a metal with similar conductivity to silver, such as copper, aluminum, nickel, etc., but not limited thereto. A relatively low-cost metal can be preferred.

[0064] Electric field induced electroplating is a technology that uses the action of an electric field to achieve metal ion deposition on a specific surface. During the electric field induced electroplating process, the external electric field will guide the metal ions in the plating solution to migrate and deposit to a specific area. By controlling the direction and intensity of the electric field, the position and shape of the metal deposition preset in this embodiment can be accurately controlled. In addition, the magnitude of the current directly affects the reduction rate of the metal ions, thereby affecting the deposition rate and the quality of the deposited layer. Therefore, in this embodiment, the preset metal is plated on the surface of the first silver grid line and the second silver grid line respectively through light induced electroplating and electric field induced electroplating, and the aspect ratio of the grid line can be flexibly controlled according to demand. A metal grid line structure with a composite structure having a good aspect ratio can be prepared, which improves light intake and reduces overall line resistance, achieves good carrier extraction capability, and reduces silver consumption.

[0065] In one embodiment, see the attached Figure 2 , attached Figure 2 A schematic diagram of the process of electroplating a first preset metal layer on the surface of a first silver grid line by light-induced electroplating is shown. In this embodiment, electroplating a first preset metal layer on the surface of a first silver grid line by light-induced electroplating includes the following steps S201 to S204.

[0066] Step S201, providing a first auxiliary electrode; the first auxiliary electrode is made of a preset metal.

[0067] According to different types of preset metals, the first auxiliary electrode may also correspond to different metal rods, for example, a copper rod, a nickel rod, etc., but is not limited thereto.

[0068] Step S202, electrically connecting a first auxiliary electrode and a first silver grid line disposed in a preset electrolyte.

[0069] The preset electrolyte may include an electrolyte including copper ions. For example, the components of the preset electrolyte include a mixture of copper sulfate, sulfuric acid, copper chloride, ammonium phosphate, deionized water, etc. The specific concentration can be freely matched according to the requirements of the aspect ratio of the metal gate line structure. In addition, the pH value of the preset electrolyte in this embodiment is 3.0-4.2, for example, 3.0, 3.1, 3.2, 3.3, 3.4, 3.5, 3.6, 3.7, 3.8, 3.9, 4.0, 4.1, 4.2, etc., but not limited to this.

[0070] Step S203: applying a preset bias voltage to the cell through the first auxiliary electrode and the first silver grid line.

[0071] A preset bias voltage is applied to the cell through the first auxiliary electrode and the first silver grid line, so that electrons inside the cell flow from the p-type semiconductor to the n-type semiconductor, thereby enabling the solar cell to generate electricity and copper ions in the electrolyte to be deposited on the surface of the first silver grid line.

[0072] Step S204 , providing a preset light condition to perform light induction on the cell to electroplate a first preset metal layer on the surface of the first silver grid line.

[0073] The preset lighting conditions include lighting time, lighting intensity, light source wavelength, etc., which can be flexibly set according to actual needs. In addition, in order to avoid the unstable light source in the surrounding environment affecting the stability of electroplating, step S204 can also be performed in a closed environment to perform electroplating using the self-provided light source as the only light source. Among them, the preset lighting conditions can be provided by a specific light source device, for example, the light source device includes a light-shielding space and an LED light source arranged in the light-shielding space, and the LED light source can be flexibly controlled by a specific control circuit to meet the above-mentioned preset lighting conditions.

[0074] In this embodiment, a light-induced electroplating method is used to electroplate a first preset metal layer on the surface of the first silver grid line. On the one hand, it can form a precise pattern and metal deposition on the surface of the first silver grid line, optimize the design and distribution of the battery surface electrodes, and effectively improve the photoelectric conversion efficiency of the solar cell; on the other hand, it can reduce the silver consumption during screen printing and reduce the preparation cost.

[0075] In one embodiment, providing preset lighting conditions to photo-induce the cell to electroplate a first preset metal layer on the surface of the first silver grid line includes: providing a light-proof space; providing preset lighting conditions in the light-proof space to photo-induce the cell to electroplate the first preset metal layer on the surface of the first silver grid line.

[0076] In this embodiment, a light-proof space is further provided to prevent unstable light sources in the surrounding environment from affecting the stability of the electroplating, thereby improving the stability of the electroplating.

[0077] In one embodiment, the preset illumination conditions include: the illumination wavelength λ satisfies the condition: 400nm≤λ≤800nm; the light intensity I satisfies the condition: 25mW / cm 2 ≤I≤60mW / cm 2 ; The lighting time t1 meets the conditions: 4min≤t1≤8min.

[0078] For example, the illumination wavelength λ may be 400 nm, 450 nm, 500 nm, 550 nm, 600 nm, 650 nm, 700 nm, 750 nm, 800 nm, but is not limited thereto. The light intensity I may be 25 mW / cm 2 、30mW / cm 2 、35mW / cm 2 , 40mW / cm 2 , 45mW / cm 2 、50mW / cm 2 、60mW / cm 2 The illumination time t1 may be 4 min, 5 min, 6 min, 7 min, 8 min, but is not limited thereto.

[0079] In this embodiment, the preset illumination conditions are set to the illumination wavelength λ satisfying the condition: 400nm≤λ≤800nm; the light intensity I satisfying the condition: 25mW / cm 2 ≤I≤60mW / cm 2 ; The illumination time t1 satisfies the condition: 4min≤t1≤8min, which can ensure that the light-induced electroplating proceeds stably.

[0080] In one embodiment, see the attached Figure 3 , attached Figure 3 A schematic diagram of the process of electroplating a second preset metal layer on the surface of the second silver grid line by electric field induced electroplating is shown. In this embodiment, electroplating a second preset metal layer on the surface of the second silver grid line by electric field induced electroplating includes the following steps S301 to S303.

[0081] Step S301, providing a second auxiliary electrode; the second auxiliary electrode is made of a preset metal.

[0082] Similar to the first auxiliary electrode, the second auxiliary electrode may be a copper rod, a nickel rod, etc. according to different preset metals.

[0083] Step S302: placing the second silver grid line and the second auxiliary electrode in a preset electrolyte.

[0084] The preset electrolyte is the same as the electrolyte used when the preset metal is electroplated on the surface of the first silver grid line, and any electrolyte can be used as long as it includes ions corresponding to the preset metal. Exemplarily, the components of the preset electrolyte may include a mixture of copper sulfate, sulfuric acid, copper chloride, ammonium phosphate, deionized water, etc., and the specific concentration can be freely proportioned according to the requirements of the aspect ratio of the metal grid line structure. In addition, the pH value of the preset electrolyte in this embodiment is 3.0 to 4.2, such as 3.0, 3.1, 3.2, 3.3, 3.4, 3.5, 3.6, 3.7, 3.8, 3.9, 4.0, 4.1, 4.2, etc., but is not limited thereto.

[0085] Step S303 , applying a voltage to the first silver grid line and the second auxiliary electrode under a preset power supply condition to electroplate a second preset metal layer on the surface of the second silver grid line.

[0086] Specifically, the first silver grid line is used as a cathode, the second auxiliary electrode is used as an anode, and the second surface of the battery cell (such as the P-type surface of the TOPcon battery) contacts the electrolyte, so that electroplating is performed under preset power supply conditions.

[0087] Among them, the preset power supply conditions are different according to different electroplating methods. For example, if the electroplating method is constant potential power supply, the corresponding preset power supply conditions include constant voltage, power supply time and power supply temperature. If the electroplating method is constant current power supply, the corresponding preset power supply conditions include constant current, power supply time and power supply temperature.

[0088] In the present embodiment, a second preset metal layer is plated on the surface of the second silver grid line by electric field induced electroplating to form a preset metal deposition with a precise pattern on the surface of the second silver grid line without using shielding or covering technology. On the one hand, it can improve the photoelectric conversion efficiency of the solar cell, and on the other hand, it can reduce the silver consumption generated during screen printing and reduce costs.

[0089] In one embodiment, the preset power supply conditions include: the target constant current i satisfies the condition: 0.1A≤i≤0.5A; the first power supply time t2 satisfies the condition: 1min≤t2≤30min; the first ambient temperature T1 satisfies the condition: 20℃≤T1≤50℃.

[0090] Exemplarily, the target constant current i may be 0.1A, 0.2A, 0.3A, 0.4A, 0.5A, etc., but not limited thereto. The first power supply time t2 may be 1min, 5min, 10min, 15min, 20min, 25min, 30min, etc., but not limited thereto. The first ambient temperature T1 may be 20°C, 25°C, 30°C, 35°C, 40°C, 45°C, 50°C, etc., but not limited thereto.

[0091] In this embodiment, the preset conditions are that the target constant current i satisfies the condition: 0.1A≤i≤0.5A; the first power supply time t2 satisfies the condition: 1min≤t2≤30min; the first ambient temperature T1 satisfies the condition: 20℃≤T1≤50℃, and the second preset metal layer is electroplated on the surface of the second silver grid line, that is, the second preset metal layer is electroplated on the surface of the second silver grid line by constant current electroplating, and there is no need to introduce a reference electrode, the operation is simple, it is not affected by the solution resistance and capacitance effects, and it can instantly reach a higher value, and electroplating is efficiently achieved. In one embodiment, the preset power supply conditions include: the target constant voltage v satisfies the condition: 0.4V≤v≤1.2V; the second power supply time t3 satisfies the condition: 1min≤t3≤30min; the second ambient temperature T2 satisfies the condition: 25℃≤T2≤60℃.

[0092] Exemplarily, the target constant voltage v may be 0.4V, 0.5V, 0.6V, 0.7V, 0.8V, 0.9V, 1.0V, 1.1V, 1.2V, etc., but not limited thereto. The second power supply time t3 may be 1min, 5min, 10min, 15min, 20min, 25min, 30min, etc., but not limited thereto. The second ambient temperature T2 may be 25°C, 30°C, 35°C, 40°C, 45°C, 50°C, 55°C, 60°C, etc., but not limited thereto.

[0093] In this embodiment, the preset conditions are that the target constant voltage v satisfies the condition: 0.4V≤v≤1.2V; the second power supply time t3 satisfies the condition: 1min≤t3≤30min; the second ambient temperature T2 satisfies the condition: 25℃≤T2≤60℃, and the second preset metal layer is electroplated on the surface of the second silver grid line. That is, the second preset metal layer is electroplated on the surface of the second silver grid line by constant potential electroplating, which can well control the current efficiency and the alloy composition of the preset metal in silver, and there is no need to adjust the current due to the increase or decrease of the plated parts.

[0094] In one embodiment, the preset metal in the first preset metal layer and the second preset metal layer includes one of copper, aluminum, and nickel. In this embodiment, the first preset metal layer is formed by electroplating on the surface of the first silver grid line, and the second preset metal layer is formed by electroplating on the surface of the second silver grid line, wherein the preset metal can be one of copper, aluminum, and nickel, which can reduce silver consumption and thus reduce costs.

[0095] In one embodiment, the thickness of the first preset metal layer and the second preset metal layer are both 4um-6um, illustratively, 4um, 4.5um, 5um, 5.5um, 6um, etc., but not limited thereto.

[0096] In the present embodiment, the thickness of the preset metal of the electroplating and the thickness of the silver grid line will affect the photoelectric conversion efficiency and performance of the solar cell. The width and thickness of the grid line determine the light receiving area it occupies. The thicker the grid line is, the larger its cross-sectional area is, and more light receiving area is occupied, thereby increasing the light shielding loss. The height and thickness of the grid line determine its resistance and contact resistance. Although theoretically the increase of the thickness of the grid line will reduce its resistance, in practice, the overly thick grid line will increase the contact resistance because the effective contact area between the thick grid line and the silicon wafer is reduced. At the same time, the thick grid line is also prone to uneven contact during the sintering process, further increasing the series resistance, reducing the fill factor and output power. During the sintering process, the overly thick grid line requires more heat to sinter the grains, which will increase the thermal stress of the silicon wafer. This thermal stress may cause micro-cracks or warping of the silicon wafer, affecting the mechanical stability and long-term performance of the battery. In order to reduce silver consumption in the present application, shorter first and second silver grid lines are printed when printing the silver grid lines. The thickness of the first preset metal layer and the second preset metal layer can be controlled to be between 4um and 6μm through light-induced electroplating and electric field-induced electroplating, thereby ensuring that the silver consumption is reduced while ensuring the photoelectric conversion efficiency and performance of the solar cell.

[0097] In one embodiment, see the attached Figure 4 , attached Figure 4 A schematic diagram of the process of preparing a first silver grid line on the first surface of a battery cell and preparing a second silver grid line on the second surface by screen printing is shown. In this embodiment, the first silver grid line is prepared on the first surface of the battery cell and the second silver grid line is prepared on the second surface by screen printing, including the following steps S401 to S403.

[0098] Step S401 , preparing a first silver main grid line and a first silver fine grid line on a first surface of a solar cell by screen printing.

[0099] The height of the first silver main grid line and the first silver thin grid line can be 2.5um~3μm, such as 2.5um, 2.6um, 2.7um, 2.8um, 2.9um, 3um, etc., but not limited thereto. The width of the first silver thin grid line can be 15um~25μm, such as 15um, 16um, 17um, 18um, 19um, 20um, 21um, 22um, 23um, 24um, 25um, etc., but not limited thereto.

[0100] Step S402 , preparing a second silver main grid line and a second silver fine grid line on the second surface of the solar cell by screen printing.

[0101] The height of the second silver main grid line can be 2.5um~3μm, such as 2.5um, 2.6um, 2.7um, 2.8um, 2.9um, 3um, etc., but not limited thereto. The height of the second silver fine grid line can be 3um~7μm, such as 3um, 3.5um, 4um, 4.5um, 5um, 5.5um, 6um, 6.5um, 7um, etc., but not limited thereto. The width of the second silver fine grid line can be 1.5um~5μm, such as 1.5um, 2um, 2.5um, 3um, 3.5um, 4um, 4.5um, 5um, etc., but not limited thereto.

[0102] Step S403, sintering the first silver main grid line, the first silver thin grid line, the second silver main grid line and the second silver thin grid line.

[0103] Specifically, the sintering method can be sintering or LECO (Laser-enhanced Contact Optimization). Sintering is a traditional heat-driven process that burns the metal slurry and forms a conductive path by heating, while LECO (Laser Enhanced Contact Optimization) uses laser technology to precisely control the contact between the metal and the silicon wafer to reduce contact resistance and improve battery efficiency. In addition, it can also be double-sided electroplating or single-sided electroplating. In the actual preparation process, the battery cell can also be cleaned after sintering.

[0104] In this embodiment, a relatively short metal silver grid line is first printed through a conventional screen printing process, which reduces silver consumption and acts as an adaptive seed layer for a subsequent electroplating process, thereby enhancing the adhesion of the first preset metal layer, the second preset metal layer and the silver metal grid line, thereby improving the reliability of the solar cell. In addition, it avoids the use of traditional laser grooving, mask exposure, back engraving and other steps, thereby greatly reducing production costs and process complexity, and reducing opening voltage losses.

[0105] In one embodiment, the aspect ratio of the second silver thin grid line is 5% to 20%. Exemplarily, it can be 5%, 6%, 7%, 8%, 9%, 10%, 11%, 12%, 13%, 14%, 15%, 16%, 17%, 18%, 19%, 20%, etc., but not limited thereto. The second silver thin grid line in this embodiment is located on the second surface of the battery sheet. If the second surface is the side facing the light source, the aspect ratio of the second silver thin grid line can be controlled to 5% to 20% through the solar cell metallization method in this embodiment, which can effectively improve the photoelectric conversion efficiency and performance of the solar cell.

[0106] In one embodiment, the height of the second silver fine grid line is 1.5um~5um, and the width of the second silver fine grid line is 3um~7um. Exemplarily, the height of the second silver fine grid line can be 3um~7μm, such as 3um, 3.5um, 4um, 4.5um, 5um, 5.5um, 6um, 6.5um, 7um, etc., but not limited thereto. The width of the second silver fine grid line can be 1.5um~5μm, such as 1.5um, 2um, 2.5um, 3um, 3.5um, 4um, 4.5um, 5um, etc., but not limited thereto.

[0107] In one embodiment, a TOPCon battery metallization method is provided for preparing Figure 5 The solar cell shown, TOPCon cell metallization method includes the following steps:

[0108] (1) Select TOPCon battery blue film as the base material (i.e. battery cell).

[0109] (2) First step of metallization: by screen printing, sintering and LECO, the back main grid, back fine grid, front main grid and front fine grid are printed on the front side (i.e. the second surface in any of the above embodiments) and the back side (i.e. the first surface in any of the above embodiments) of the solar cell, respectively. The height of the front and front and back main grids is 2.5 μm to 3 μm, the width of the back fine grid is 15 μm to 25 μm and the height is 3 μm, the width of the front fine grid is 12 μm to 16 μm and the height is 2 μm to 4 μm, and then sintering and LECO are performed to complete the first step of metallization.

[0110] (3) The second step is metallization: a layer of metal copper with a thickness of 4 μm to 6 μm is plated on the main grid and fine grid printed metal silver grid lines on the front and back sides of the battery cell by electroplating to obtain the TOPCon battery with the mixed metallization structure; wherein the electroplating method can be double-sided electroplating at the same time or single-sided electroplating, and cleaning is performed after electroplating.

[0111] Specifically, the back copper plating includes placing the screen-printed battery cell on a carrier as a working electrode, taking a metal copper rod as an auxiliary electrode, placing the auxiliary electrode and the main and fine grid lines on the back of the battery cell in an electrolyte, connecting the auxiliary electrode to the main and fine grid lines on the back of the battery cell through a wire, applying an auxiliary power supply and light source above the battery cell, and performing light-induced electroplating in a light-proof space.

[0112] The light source parameters applied are: light wavelength of 400nm to 800nm, light intensity of 25 to 60mW / cm 2The processing time is 4min to 8min, wherein the electrolyte includes: the electroplating solution used in the copper electroplating process includes a mixture of copper sulfate, sulfuric acid, copper chloride, ammonium phosphate, deionized water, etc. The concentration can be freely proportioned according to demand, and the pH value of the electrolyte is 3.0 to 4.2.

[0113] Front electroplating: The main and fine grid lines on the back of the cell after light-induced electroplating are used as the cathode, the p-type surface of the cell contacts the electrolyte, and the metal copper rod is used as the anode and placed in the electrolyte for electroplating. The metal copper grid line is deposited on the screen-printed grid line surface on the front of the solar cell. The electrolytic process is: constant current electroplating: the current is set to 0.1A~0.5A, the time is 1min~30min, and the temperature is 20℃~50℃.

[0114] In a specific embodiment, the deposition method of the copper conductive layer includes light-induced electroplating, electric field-induced electroplating, etc. The electroplating method can be constant current electroplating, constant potential electroplating, and the electroplating parameters are: constant current electroplating: the current is set to 0.1A~0.5A, the time is 1min~30min, and the temperature is 20℃~50℃; constant potential electroplating: the voltage is set to 0.4V~1.2V, the time is 1min~30min, and the temperature is 25℃~60℃. The electroplating solution used in the copper electroplating process contains a mixed solution composed of copper sulfate, sulfuric acid, copper chloride, ammonium phosphate, deionized water, etc., and the concentration can be freely proportioned according to demand. Finally, a mixed metallized TOPCON solar cell is obtained.

[0115] In order to more clearly illustrate the beneficial effects of the solar cell metallization method in this embodiment, a first comparative example is also provided in this embodiment: a solar cell metallization method is used to prepare a solar cell metallization method. Figure 6 The solar cell shown comprises the following steps:

[0116] (1) Select TOPCon battery blue film as the base material.

[0117] (2) A laser is used to groove the fine grid and main grid positions on the front and back surfaces of the substrate material to complete the graphic processing, wherein the laser wavelength range is 805nm~1100nm and the spot size is 10μm~50μm.

[0118] (4) A layer of metal copper with a thickness of 4um to 6μm is plated on the main grid and fine grid printed metal silver grid lines on the front and back sides of the battery cell by electroplating to obtain the TOPCon battery with the mixed metallization structure, so that the bus height of the combined structure of the front silver fine grid and copper reaches 8.9um, the bus width reaches 18um, and the overall aspect ratio reaches 49.44%; wherein the electroplating method can be double-sided simultaneous electroplating or single-sided electroplating, and cleaning is performed after electroplating.

[0119] In a specific embodiment, the deposition method of the copper conductive layer includes light-induced electroplating, electric field-induced electroplating, etc. The electroplating method can be constant current electroplating, constant potential electroplating, and the electroplating parameters are: constant current electroplating: the current is set to 0.1-0.5 A, the time is 1-30min, 20-50°C; constant potential electroplating: the voltage is set to 0.4-1.2 V, the time is 1-30min, and the temperature is 25-60°C. The electroplating solution used in the copper electroplating process contains a mixed solution composed of copper sulfate, sulfuric acid, copper chloride, ammonium phosphate, deionized water, etc., and the concentration can be freely proportioned according to demand. Finally, a plated TOPCON solar cell is obtained.

[0120] (3) A nickel seed layer with a thickness of 0.4 μm is plated on the surface of the cell by PVD (Physical Vapor Deposition);

[0121] A second comparative example is also provided - the same Figure 7 The solar cell shown comprises the following steps:

[0122] (1) Select TOPCon battery blue film as the base material.

[0123] (2) Metallization: The back main grid, back fine grid, front main grid and front fine grid are printed in sequence by screen printing, sintering and LECO. The height of the front and front main grids is 5 μm~8 μm, the width of the back fine grid is 30 μm~45 μm and the height is 5 μm~7 μm, the width of the front fine grid is 17 μm~21 μm and the height is 8 μm~10 μm. The metallization step is then completed by sintering and LECO to finally obtain a TOPCON solar cell.

[0124] Based on the above comparison, we can get Table 1:

[0125] Table 1 Comparison of parameters of solar cells prepared in the first comparative example, the second comparative example and this embodiment

[0126]

[0127] Wherein ρc refers to conversion efficiency, and Rline refers to line resistance. Based on the above table, it can be seen that the solar cell preparation method in this embodiment can prepare a metal grid line structure with a composite structure with a good aspect ratio, improve light input and reduce the overall line resistance, achieve good carrier extraction ability, and higher grid line tension, and reduce silver consumption, thereby reducing the preparation cost of solar cells on the basis of improving the photoelectric conversion efficiency and performance of solar cells.

[0128] It should be understood that, although the various steps in the flowcharts involved in the above-mentioned embodiments are displayed in sequence according to the indication of the arrows, these steps are not necessarily executed in sequence according to the order indicated by the arrows. Unless there is a clear explanation in this article, the execution of these steps does not have a strict order restriction, and these steps can be executed in other orders. Moreover, at least a part of the steps in the flowcharts involved in the above-mentioned embodiments can include multiple steps or multiple stages, and these steps or stages are not necessarily executed at the same time, but can be executed at different times, and the execution order of these steps or stages is not necessarily carried out in sequence, but can be executed in turn or alternately with other steps or at least a part of the steps or stages in other steps.

[0129] In one embodiment, a solar cell is also provided. The solar cell in this embodiment includes a second silver fine grid line and a second preset metal layer. The second silver fine grid line is arranged on the second surface of the battery cell; the aspect ratio of the second silver fine grid line is 5%~20%; the second preset metal layer is arranged on the side of the second silver grid line away from the second surface.

[0130] The solar cell in this embodiment can be prepared by the solar cell metallization method in any of the above embodiments. The solar cell in this embodiment includes a combined grid line structure formed by a second silver fine grid line and a second preset metal layer, which has a stronger bonding force and a larger welding tensile force. In addition, the aspect ratio of the second silver fine grid line is 5% to 20%, which can effectively improve the photoelectric conversion efficiency and performance of the solar cell.

[0131] In one embodiment, the solar cell in this embodiment also includes a first silver fine grid line and a first preset metal layer, the first silver fine grid line is arranged on the first surface of the battery cell; the first surface is opposite to the second surface; the first preset metal layer is arranged on the side of the first silver grid line away from the first surface.

[0132] In one embodiment, the width of the first silver fine grid line in this embodiment is 15um-25um.

[0133] The first silver thin grid line can be a thin grid line on the side of the solar cell facing away from the sunlight, and its width will affect the secondary reflection of sunlight on the back side. In this embodiment, the width of the first silver thin grid line is 15um~25um, which can ensure the photon utilization rate of the solar cell.

[0134] In one embodiment, the thickness of the first preset metal layer and the second preset metal layer in this embodiment are both 4 um to 6 μm.

[0135] In this embodiment, the thickness of the first preset metal layer and the second preset metal layer are both 4um~6μm, which can enhance the bonding strength and welding tension of the combined grid line structure composed of the first preset metal layer and the first silver fine grid line and the combined grid line structure composed of the second preset metal layer and the second silver fine grid line, thereby improving the reliability of the solar cell.

[0136] In one embodiment, the height of the second silver thin grid line in this embodiment is 1.5um-5um, and the width of the second silver thin grid line is 3um-7um.

[0137] In this embodiment, the height of the second silver fine grid line is 1.5um~5um, and the width of the second silver fine grid line is 3um~7um, which can ensure that the aspect ratio of the second silver fine grid line is in a larger range, thereby reducing the shading and overall line resistance of the solar cell and improving the photoelectric conversion efficiency.

[0138] It should be noted that the solar cell in this embodiment can be prepared by the solar cell metallization method in any of the above embodiments. When the solar cell metallization method in any of the above embodiments has further technical effects, the corresponding method also has further technical effects.

[0139] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this application.

[0140] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the present application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the attached claims.

Claims

1. A solar cell metallization method, It is characterized in that The method comprises: Prepare a first silver grid line on the first surface of the battery cell and prepare a second silver grid line on the second surface by screen printing; the first surface and the second surface are two opposite sides of the battery cell; Electroplating a first preset metal layer on the surface of the first silver grid line by light-induced electroplating; Electroplating a first preset metal layer on the surface of the first silver grid line; A second preset metal layer is electroplated on the surface of the second silver grid line by electric field induced electroplating.

2. The solar cell metallization method according to claim 1, It is characterized in that Electroplating the first preset metal layer on the surface of the first silver grid line by light-induced electroplating includes: Providing a first auxiliary electrode; the first auxiliary electrode is made of a preset metal; Electrically connecting the first auxiliary electrode and the first silver grid line disposed in a preset electrolyte; Applying a preset bias voltage to the cell through the first auxiliary electrode and the first silver grid line; Preset lighting conditions are provided to photo-induce the cell sheet so as to electroplate the first preset metal layer on the surface of the first silver grid line.

3. The solar cell metallization method according to claim 2, It is characterized in that Providing a preset light condition to photo-induce the cell to electroplate the first preset metal layer on the surface of the first silver grid line, comprising: Provide a dark space; A preset lighting condition is provided in the light-proof space to photo-induce the cell sheet so as to electroplate the first preset metal layer on the surface of the first silver grid line.

4. The solar cell metallization method according to claim 2, It is characterized in that The preset illumination conditions include: the illumination wavelength λ satisfies the condition: 400nm≤λ≤800nm; the light intensity I satisfies the condition: 25mW / cm 2 ≤I≤60mW / cm 2 ; Lighting time t 1 Satisfy the conditions: 4min≤t 1 ≤8min.

5. The solar cell metallization method according to claim 1, It is characterized in that Electroplating the second preset metal layer on the surface of the second silver grid line by electric field induction electroplating includes: Providing a second auxiliary electrode; the second auxiliary electrode is made of a preset metal; Placing the second silver grid line and the second auxiliary electrode in a preset electrolyte; Under a preset power supply condition, a voltage is applied to the first silver grid line and the second auxiliary electrode to electroplate the second preset metal layer on the surface of the second silver grid line.

6. The solar cell metallization method according to claim 5, It is characterized in that The preset power supply conditions include: the target constant current i satisfies the condition: 0.1A≤i≤0.5A; the first power supply time t 2 Satisfy the conditions: 1min≤t 2 ≤30min; first ambient temperature T 1 Satisfy the conditions: 20℃≤T 1 ≤50℃.

7. The solar cell metallization method according to claim 5, It is characterized in that The preset power supply conditions include: the target constant voltage v satisfies the condition: 0.4V≤v≤1.2V; the second power supply time t 3 Satisfy the conditions: 1min≤t 3 ≤30min; Second ambient temperature T 2 Satisfy the conditions: 25℃≤T 2 ≤60℃.

8. The solar cell metallization method according to any one of claims 1 to 7, It is characterized in that The preset metal includes one of copper, aluminum and nickel.

9. The solar cell metallization method according to any one of claims 1 to 7, It is characterized in that The thickness of the first preset metal layer and the second preset metal layer are both 4um-6μm.

10. The solar cell metallization method according to claim 1, It is characterized in that The method comprises: preparing the first silver grid lines on the first surface of the battery cell and preparing the second silver grid lines on the second surface by screen printing, comprising: Preparing a first silver main grid line and a first silver fine grid line on the first surface of the battery cell by screen printing; Prepare a second silver main grid line and a second silver fine grid line on the second surface of the battery cell by screen printing; The first silver main grid line, the first silver thin grid line, the second silver main grid line and the second silver thin grid line are sintered.

11. The solar cell metallization method according to claim 10, It is characterized in that The width of the first silver fine grid line is 15um-25um.

12. The solar cell metallization method according to claim 10, It is characterized in that The aspect ratio of the second silver fine grid line is 5% to 20%.

13. The solar cell metallization method according to claim 10 or 12, It is characterized in that The height of the second silver thin grid line is 1.5um-5um, and the width of the second silver thin grid line is 3um-7um.

14. A solar cell, It is characterized in that include: A second silver fine grid line is provided on the second surface of the battery cell; the height-to-width ratio of the second silver fine grid line is 5% to 20%; The second preset metal layer is disposed on a side of the second silver fine grid line facing away from the second surface.

15. The solar cell according to claim 14, It is characterized in that Also includes: A first silver fine grid line is provided on a first surface of the battery cell; the first surface is opposite to the second surface; The first preset metal layer is disposed on a side of the first silver fine grid line facing away from the first surface.

16. The solar cell according to claim 15, It is characterized in that The width of the first silver fine grid line is 15um-25um.

17. The solar cell according to claim 15, It is characterized in that The thickness of the first preset metal layer and the second preset metal layer are both 4um-6μm.

18. The solar cell according to claim 14, It is characterized in that The height of the second silver thin grid line is 1.5um-5um, and the width of the second silver thin grid line is 3um-7um.

Citation Information

Patent Citations

  • Method for manufacturing solar cell positive electrode grid line

    CN103996752A

  • Production method of front grid line electrode of crystalline silicon solar cell

    CN104362216A

  • Solar cell photoinductive electroplating method

    CN105633195A

  • Method for forming grid line electrode of photovoltaic device and photovoltaic device

    CN114695599A

  • Solar cell electroplating method

    CN115896888A

Cited By

  • Copper plating electroplating solution as well as preparation method and application thereof

    CN119593028A

  • A copper plating solution, its preparation method and application

    CN119593028B