Method for producing electrode body for nonaqueous secondary battery

By using an adhesive layer solution of a highly soluble second solvent to fill the interface gap between the positive electrode layer and the adhesive layer in a non-aqueous secondary battery, and using heating and compression technology, the problem of insufficient bonding strength between the positive electrode layer and the solid electrolyte layer is solved. Improved battery capacity and durability.

CN118738288APending Publication Date: 2024-10-01HONDA MOTOR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410207834.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-28
Filing Date
2024-02-26
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The bonding strength between the positive electrode layer and the solid electrolyte layer in existing non-aqueous secondary batteries is insufficient, resulting in low interface strain strength and affecting the stability of the electrode layer and the electrolyte layer.

Method used

A manufacturing method is adopted in which a positive electrode layer solution containing a positive electrode active material and a binder and an adhesive layer solution containing a solid electrolyte are prepared, and the adhesive layer solution with a higher solubility of the binder in a second solvent is used in the lamination process. Interface voids and improved bonding through heating and compression.

Benefits of technology

The bonding between the positive electrode layer and the adhesive layer is improved, the interface connection between the positive electrode layer and the solid electrolyte layer is enhanced, the resistance is reduced, and the battery capacity and durability are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738288A_ABST
    Figure CN118738288A_ABST
Patent Text Reader

Abstract

The problem to be solved by the present invention is to provide a method for manufacturing an electrode body for a nonaqueous secondary battery, which enables the connection between a positive electrode layer and a solid electrolyte layer to be more continuous or firmer. In order to solve the problem, the present invention provides a method for producing an electrode body for a non-aqueous secondary battery, the method comprising: a positive electrode layer solution preparation step for preparing a positive electrode layer solution containing a positive electrode active material, a binder, and a first solvent; a positive electrode layer molding step for molding a positive electrode layer using the positive electrode layer solution; an electrolyte layer molding step for molding an electrolyte layer containing a solid electrolyte; an adhesive layer solution preparation step for preparing an adhesive layer solution containing a solid electrolyte and a second solvent; an adhesive layer forming step for forming an adhesive layer using the adhesive layer solution; and a lamination step in which the positive electrode layer, the adhesive layer, and the electrolyte layer are laminated in this order. The second solvent has a greater solubility with respect to the binder than the first solvent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for producing an electrode body for a non-aqueous secondary battery. Background Art

[0002] In recent years, research and development related to secondary batteries that contribute to energy efficiency have been conducted in order to ensure that more people have access to affordable, reliable, sustainable and advanced energy.

[0003] As such a secondary battery, it is known that there are non-aqueous secondary batteries such as lithium ion secondary batteries in which an electrolyte layer is configured between the positive electrode layer and the negative electrode layer. In a non-aqueous secondary battery, the interface between the electrode layer and the electrolyte layer is in solid contact, and the formation of an ion path is an important issue. However, since the mechanical bonding strength of the interface is low and it is a bonding of different materials, it is necessary to improve the strength of the interface strain that may potentially occur. As a technology for maintaining the stability of the interface between the electrode layer and the electrolyte layer, it is known that a technology for cross-linking the binder of the electrode layer by a cross-linking agent is used (for example, with reference to patent document 1).

[0004] In addition to the above, as a technology that can form a good interface between solid particles, there is known a technology involving an all-solid secondary battery, which has an intermediate layer containing compounds such as Li2Ti2O5 between the solid electrolyte layer and the negative electrode active material layer (for example, refer to patent document 2).

[0005] [Prior Technical Literature]

[0006] (Patent Document)

[0007] Patent Document 1: Japanese Patent Application Publication No. 2014-116164

[0008] Patent Document 2: Japanese Patent Application Publication No. 2016-212991 Summary of the invention

[0009] [Problems to be solved by the invention]

[0010] In the technology disclosed in Patent Document 1, the positive electrode and the negative electrode contain a non-polar binder, and the binder is cross-linked by a cross-linking agent. In addition, the positive electrode and the negative electrode are bonded to the electrolyte layer by a non-polar binder. The technology disclosed in Patent Document 2 is a technology for configuring an intermediate layer between the solid electrolyte layer and the negative electrode active material layer to obtain a good interface formation between the negative electrode active material layer and the solid electrolyte layer. On the other hand, it is desired to make the bonding between the positive electrode layer and the solid electrolyte layer more continuous or firm.

[0011] The present invention has been made in view of the above, and an object of the present invention is to provide a method for producing an electrode body for a non-aqueous secondary battery, which can make the connection between the positive electrode layer and the solid electrolyte layer more continuous or strong.

[0012] [Technical means to solve the problem]

[0013] (1) It relates to a method for manufacturing an electrode body for a non-aqueous secondary battery, which comprises: a positive electrode layer solution preparation step, preparing a positive electrode layer solution comprising a positive electrode active material, a binder and a first solvent; a positive electrode layer forming step, using the aforementioned positive electrode layer solution to form a positive electrode layer; an electrolyte layer forming step, forming an electrolyte layer comprising a solid electrolyte; an adhesive layer solution preparation step, preparing an adhesive layer solution comprising a solid electrolyte and a second solvent; an adhesive layer forming step, using the aforementioned adhesive layer solution to form an adhesive layer; and a stacking step, stacking the aforementioned positive electrode layer, the aforementioned adhesive layer and the aforementioned electrolyte layer in sequence; the aforementioned second solvent has a greater solubility in the aforementioned binder than the aforementioned first solvent.

[0014] According to the invention of (1), the amount of binder eluted at the interface between the positive electrode layer and the adhesive layer can be increased, thereby providing a method for producing an electrode body for a non-aqueous secondary battery, which can make the connection between the positive electrode layer and the solid electrolyte layer more continuous or strong.

[0015] (2) The method for producing an electrode body for a nonaqueous secondary battery according to (1), wherein the second solvent has a boiling point lower than that of the first solvent.

[0016] According to the invention of (2), after the gap at the interface between the positive electrode layer and the adhesive layer is filled with the adhesive, the second solvent evaporates smoothly, so that the interface is easily filled with the adhesive and gaps are not easily generated on the interface. Therefore, the bonding property between the positive electrode layer and the adhesive layer can be further improved.

[0017] (3) The method for producing an electrode body for a nonaqueous secondary battery according to (1) or (2), wherein in the lamination step, when laminating the positive electrode layer and the adhesive layer, the second solvent is present at least in the adhesive layer.

[0018] According to the invention of (3), the fixing effect of the binder contained in the positive electrode layer can be exerted, and the bonding property between the positive electrode layer and the adhesive layer can be further improved.

[0019] (4) The method for producing an electrode body for a nonaqueous secondary battery according to any one of (1) to (3), wherein the adhesive layer solution does not contain a binder.

[0020] According to the invention of (4), the dissolution of the binder contained in the positive electrode layer by the second solvent and its infiltration into the adhesive layer are further promoted, so that the bonding property between the positive electrode layer and the adhesive layer can be further improved.

[0021] (5) The method for producing an electrode body for a nonaqueous secondary battery according to any one of (1) to (3), wherein the adhesive layer solution contains a binder of the same type as the binder contained in the positive electrode layer solution.

[0022] According to the invention of (5), the compatibility between the binder contained in the positive electrode layer and the binder contained in the adhesive layer is improved, so that the positive electrode layer and the adhesive layer can be made more continuous or stronger. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a diagram showing a state in which the positive electrode layer and the adhesive layer are stacked according to this embodiment.

[0024] Figure 2 It is a diagram showing a bonding state between a positive electrode layer and an adhesive layer according to this embodiment. DETAILED DESCRIPTION

[0025] The manufacturing method of the electrode body for non-aqueous secondary batteries of the present embodiment is a method for manufacturing an electrode body for non-aqueous secondary batteries, wherein the electrode body for non-aqueous secondary batteries at least includes a positive electrode layer, an electrolyte layer, and an adhesive layer stacked between these layers constituting the non-aqueous secondary battery. In addition to the above-mentioned layers, the non-aqueous secondary battery also includes at least a negative electrode layer. The negative electrode layer is stacked in a manner that is in contact with the above-mentioned electrolyte layer.

[0026] [Non-aqueous secondary battery]

[0027] The non-aqueous secondary battery of the present embodiment can be listed as: a semi-solid lithium ion battery with a gel electrolyte, an all-solid lithium ion battery with a solid electrolyte, etc. As a non-aqueous secondary battery, a semi-solid lithium metal battery or an all-solid lithium metal battery using lithium metal for the negative electrode is particularly preferred. This is because the expansion and contraction caused by charging and discharging of these solid batteries is relatively large, and it is expected that the bonding strength between the positive electrode layer and the solid electrolyte layer is stronger, and according to the manufacturing method of the electrode body for a non-aqueous secondary battery of the present embodiment, the bonding between the positive electrode layer and the solid electrolyte layer can be made more continuous or firm.

[0028] (Positive electrode layer)

[0029] The positive electrode layer includes a positive electrode active material layer and a positive electrode current collector. In this embodiment, the positive electrode active material layers are stacked on both sides of the positive electrode current collector, and the adhesive layer is stacked on the outer surface of each positive electrode active material layer.

[0030] The positive electrode active material layer is a layer that must contain a positive electrode active material. The positive electrode active material is not particularly limited, and known materials as the positive electrode active material of a non-aqueous secondary battery can be used. As the positive electrode active material, for example, ternary system positive electrode materials such as LiCoO2, LiNiO2, NCM (Li(NixCoyMnz)O2, (0 < x < 1, 0 < y < 1, 0 < z < 1, x + y + z = 1)), layered positive electrode active material particles such as LiVO2, LiCrO2, spinel type positive electrode active materials such as LiMn2O4, Li(Ni 0.25 Mn 0.75 )2O4, LiCoMnO4, Li2NiMn3O8, olivine type positive electrode active materials such as LiCoPO4, LiMnPO4, LiFePO4, etc.

[0031] In addition to the positive electrode active material, the positive electrode active material layer contains a binder. Additionally, a solid electrolyte, a conductive additive, etc. may also be contained. The solid electrolyte, the conductive additive, the binder, etc. are not particularly limited, and known materials as the electrode materials of a non-aqueous secondary battery can be applied.

[0032] The binder is not particularly limited, and preferably a particulate or fibrous binder that does not hinder the bulk contact between particles. As the types of binders, for example, polyvinylidene fluoride (PVdF), polymethyl methacrylate (PMMA), polyisobutylene (PIB), styrene butadiene rubber (SBR), polyethylene-vinyl acetate copolymer (PEVA), nitrile butadiene rubber (NBR), hydrogenated nitrile butadiene rubber (HNBR), etc. can be cited. These can be used alone or in combination of two or more.

[0033] The positive electrode current collector is not particularly limited, and known materials as the positive electrode current collector of a non-aqueous secondary battery can be used. As the positive electrode current collector, for example, metal foils such as stainless steel (SUS) foil and aluminum (Al) foil can be cited.

[0034] (Adhesive layer)

[0035] The bonding layer is a layer stacked between the positive electrode layer and the electrolyte layer. The bonding layer can make the bonding between the positive electrode layer and the electrolyte layer more continuous or firm. The bonding layer is a layer that must contain a solid electrolyte. By including a solid electrolyte in the bonding layer, the ion conductivity between the positive electrode layer and the electrolyte layer can be improved. The solid electrolyte contained in the bonding layer is not particularly limited, and a substance known as an electrode material for a non-aqueous secondary battery can be applied.

[0036] The adhesive layer may include an adhesive. When the adhesive layer includes an adhesive, the type of the adhesive is preferably the same as the type of adhesive contained in the positive electrode layer. As the source of the adhesive contained in the adhesive layer, sometimes the adhesive contained in the adhesive layer solution described later is contained in the adhesive layer, and sometimes the adhesive contained in the positive electrode layer moves, and the result is contained in the adhesive layer.

[0037] (Negative electrode layer)

[0038] The negative electrode layer includes a negative electrode active material layer and a negative electrode current collector. In this embodiment, the negative electrode active material layer is stacked so as to be in contact with the electrolyte layer, and the negative electrode current collector is stacked on the outermost layer of the stack.

[0039] The negative electrode active material layer is a layer that must contain a negative electrode active material. The negative electrode active material is not particularly limited, and a material known as a negative electrode active material for a non-aqueous secondary battery can be used. Examples of the negative electrode active material include lithium titanate (Li4Ti5O 12 ) and other lithium transition metal oxides, TiO2, Nb2O3 and WO3 and other transition metal oxides; metal sulfides; metal nitrides; carbon materials such as graphite, soft carbon and hard carbon; silicon materials such as silicon element, silicon alloys, silicon compounds; and lithium metal, lithium alloys and metal indium.

[0040] The negative electrode active material layer may contain, in addition to the negative electrode active material, a solid electrolyte, a conductive aid, a binder, etc. The solid electrolyte, conductive aid, binder, etc. are not particularly limited, and any known electrode material for a nonaqueous secondary battery may be used.

[0041] The negative electrode current collector is not particularly limited, and any known negative electrode current collector for non-aqueous secondary batteries can be used. Examples of the negative electrode current collector include metal foils such as copper (Cu) foil, stainless steel (SUS) foil, and aluminum (Al) foil.

[0042] (Electrolyte layer)

[0043] The electrolyte layer is a layer that necessarily contains a solid electrolyte. In addition to the above, the electrolyte layer may also contain a binder and the like. In this embodiment, the electrolyte layer is stacked between the positive electrode layer and the adhesive layer and the negative electrode layer.

[0044] The solid electrolyte is not particularly limited, and examples thereof include sulfide-based solid electrolytes, oxide-based solid electrolytes, nitride-based solid electrolytes, and halide-based solid electrolytes.

[0045] <Method for producing electrode body for non-aqueous secondary battery>

[0046] The method for producing an electrode body for a non-aqueous secondary battery comprises a positive electrode layer solution preparation step, a positive electrode layer forming step, an electrolyte layer forming step, an adhesive layer solution preparation step, an adhesive layer forming step and a lamination step.

[0047] As a limitation on the order of performing the above-mentioned processes, there is no limitation on the order except that the forming process of each layer is performed after the solution preparation process of each layer, and the lamination process is performed after the forming process of each layer. For example, each layer may be formed separately and then the lamination process may be performed, or after forming a certain layer, other layers may be formed on the layer.

[0048] In the positive electrode layer solution preparation step, each component contained in the positive electrode active material layer is dissolved and / or dispersed in a first solvent to prepare a positive electrode layer solution. The first solvent is a solvent in which the solubility of the binder contained in the positive electrode layer is lower than that of the second solvent described below.

[0049] In the adhesive layer solution preparation step, an adhesive layer solution is prepared by dissolving and / or dispersing the components contained in the adhesive layer in a second solvent. The second solvent is a solvent in which the solubility of the binder contained in the positive electrode layer is higher than that of the first solvent.

[0050] As the first solvent and the second solvent, as long as it is a solvent with affinity to the material contained in the positive electrode layer solution and the bonding layer solution, it is not particularly limited, and can include, for example, aliphatic hydrocarbons, aromatic hydrocarbons, esters, ethers, ketones, nitriles, etc. The first solvent and the second solvent can be selected respectively according to the difference in solubility for the preselected binder.

[0051] The adhesive layer solution may also not contain an adhesive. Thus, the amount of adhesive in the positive electrode layer dissolved into the adhesive layer solution increases, and therefore, the bonding property of the positive electrode layer and the adhesive layer can be further improved. On the other hand, the adhesive layer solution may also include an adhesive of the same type as the adhesive contained in the positive electrode layer solution. Thus, the compatibility of the adhesive contained in the adhesive layer and the adhesive contained in the positive electrode layer is improved, and therefore, the positive electrode layer and the adhesive layer can be more continuously and firmly bonded. In addition, by including an adhesive in the adhesive layer solution, the coating property of the adhesive layer solution can be improved.

[0052] The solubility of the binder contained in the positive electrode layer solution of the second solvent is higher than that of the first solvent. Thus, the bonding between the positive electrode layer and the adhesive layer can be made more continuous or firm. The above effects are described below with reference to the drawings.

[0053] Figure 1 This is a cross-sectional view conceptually showing a state in which a positive electrode layer and an adhesive layer according to this embodiment are stacked. Figure 1 and Figure 2 The symbols in 1 are as follows: 10: positive electrode layer (positive electrode layer solution), 11: positive electrode active material, 20: adhesive layer (adhesive layer solution), 21: solid electrolyte, V: binder, S: second solvent.

[0054] exist Figure 1 In the embodiment, a second solvent S having a higher solubility of the binder V than the first solvent exists inside the adhesive layer 20. Therefore, when the first solvent exists inside the positive electrode layer 10, the binder V is miscible with the second solvent, and the movement of the binder V from the inside of the positive electrode layer 10 to the adhesive layer 20 is promoted. Even when the first solvent does not exist inside the positive electrode layer 10, the binder V inside the positive electrode layer 10 is dissolved by the second solvent and moves to the adhesive layer 20.

[0055] Figure 2 It is a conceptual depiction of the Figure 1 The positive electrode layer 10 and the adhesive layer 20 are bonded (laminated) in a cross-sectional view. Figure 2 As shown, at the interface L between the positive electrode layer 10 and the adhesive layer 20, there is an adhesive V that moves from the positive electrode layer 10 to the adhesive layer 20. This adhesive V is drawn out to the vicinity of the interface L by the second solvent, and is combined with the solid electrolyte 21 or the adhesive originally present in the adhesive layer 20 to be fused, thereby exerting a fixing effect. As a result, the gaps at the interface L are filled, so that the bonding between the positive electrode layer and the adhesive layer can be made more continuous or firm.

[0056] The second solvent preferably has a lower boiling point than the first solvent. By means of the above, after the gap at the interface of the positive electrode layer and the bonding layer is filled with the adhesive, the second solvent will volatilize smoothly, so it is easy to fill the interface with the adhesive and it is not easy to generate gaps on the interface. Thus, the bonding property of the positive electrode layer and the bonding layer can be further improved.

[0057] The positive electrode layer forming process is a process for forming the positive electrode layer, including a process for applying a positive electrode layer solution. The object to which the positive electrode layer solution is applied may be an adhesive layer. In addition to the above, the positive electrode layer forming process may also be a process for separately forming a sheet-shaped positive electrode layer by applying a positive electrode layer solution on any object such as a positive electrode collector and drying it. As a method for applying the positive electrode layer solution, a coating method using an applicator such as a doctor blade method, spraying, screen printing, etc. may be cited.

[0058] The adhesive layer forming process is a process for forming the adhesive layer, including a process for applying an adhesive layer solution. The object to which the adhesive layer solution is applied may be the positive electrode layer. In addition to the above, the adhesive layer forming process may also be a process for separately forming a sheet-shaped adhesive layer by applying an adhesive layer solution on an arbitrary object and drying it. However, it is necessary that a second solvent remains in the adhesive layer formed by the adhesive layer forming process. The method for applying the adhesive layer solution may be the same method as the method for applying the positive electrode layer solution.

[0059] The electrolyte layer forming step is a step of forming the electrolyte layer, including a step of applying an electrolyte solution, wherein the electrolyte solution contains the components contained in the above-mentioned electrolyte layer. The object to which the electrolyte solution is applied may be an adhesive layer. In addition to the above, the electrolyte layer forming step may also be a step of applying the electrolyte solution on any object and drying it to form a sheet-like electrolyte layer separately. The method of applying the electrolyte solution may be the same as the method of applying the positive electrode layer solution.

[0060] The step of forming each layer may include a compression step of compressing each formed layer to increase its density. The compression method in the compression step is not particularly limited, and examples thereof include flat pressing and roll pressing.

[0061] The lamination process is a process of sequentially laminating the positive electrode layer, the adhesive layer and the electrolyte layer formed by the forming process of the above-mentioned layers. The lamination process may be a process of laminating the layers formed separately. Alternatively, the lamination process may be a process of forming other layers on a certain layer formed separately. In this case, the forming process of the above-mentioned layers also serves as the lamination process. The lamination process may also be a combination of a process of laminating the layers formed separately and a process of forming other layers on a certain layer formed separately.

[0062] Preferably, in the lamination process, when laminating the positive electrode layer and the adhesive layer, the second solvent is present at least in the adhesive layer. Thus, as described above, the following effect can be obtained: the binder present in the positive electrode layer moves to the adhesive layer by the second solvent, so that the bonding between the positive electrode layer and the adhesive layer is more continuous or firm. More preferably, in addition to the above, when laminating the positive electrode layer and the adhesive layer, the first solvent is present at least in the positive electrode layer.

[0063] The forming process or lamination process of each layer may also include a heating and compressing process for heating and compressing each layer or the laminate of each layer. By means of the heating and compressing process, the density of each layer can be increased, and each layer is closely attached, and the adhesive is fused to each other to improve the bonding property of each layer. Among them, it is preferred that, as described above, when the positive electrode layer and the adhesive layer are stacked, the second solvent is at least present in the adhesive layer. Therefore, it is preferred that the laminate after at least the positive electrode layer and the adhesive layer are stacked is subjected to a heating and compressing process.

[0064] The heating and compressing method in the heating and compressing step is not particularly limited, and examples thereof include hot flat pressing and hot roll pressing.

[0065] The following describes an application example of a method for manufacturing an electrode body for a non-aqueous secondary battery. First, in the positive electrode layer solution preparation process, a positive electrode layer solution containing a positive electrode active material, SBR as a binder, and butyl butyrate (boiling point 165 degrees) as a first solvent is prepared. Next, in the positive electrode layer forming process, a thin film is formed on an arbitrary object by a doctor blade method, and is compressed by a roller press under a Hertzian surface pressure of 200MPa to 1,000MPa to make it high-density.

[0066] Next, in the electrolyte layer forming step, an electrolyte solution containing a solid electrolyte and a binder is used to form a film with an applicator, and the film is compressed by a roll press under a Hertzian surface pressure of 200 MPa to 1,000 MPa to increase the density.

[0067] Next, in the adhesive layer solution preparation process, an adhesive layer solution is prepared that includes a solid electrolyte, toluene (boiling point 110 degrees) as a second solvent, a solid electrolyte, and an adhesive such as SBR as needed. Next, in the adhesive layer forming process that also serves as a lamination process, the prepared adhesive layer solution is applied to the above-formed positive electrode layer with a thickness of 1 μm to 5 μm. Next, in the lamination process, the above-formed electrolyte layer is transferred to the above-formed adhesive layer, and rolling and bonding are performed using a roller press or the like.

[0068] In the above application example, butyl butyrate is used as the first solvent and toluene is used as the second solvent. However, for example, toluene may be used as the first solvent and xylene may be used as the second solvent.

[0069] According to the method for manufacturing an electrode body for a non-aqueous secondary battery of this embodiment, the bonding between the positive electrode layer and the solid electrolyte layer can be made more continuous or firm. Therefore, the interface between the positive electrode layer and the solid electrolyte layer can be made low-resistance, thereby increasing the battery capacity and improving the durability.

[0070] As mentioned above, although the preferred embodiment of the present invention has been described, the present invention is not limited to the above-mentioned embodiment, and modifications and improvements within the scope that can achieve the object of the present invention are included in the present invention.

[0071] Reference numerals

[0072] 10 positive electrode layer

[0073] 11Positive electrode active material

[0074] 20 Adhesive layer

[0075] 21 Solid Electrolyte

[0076] V Adhesive

[0077] S Secondary Solvent

Claims

1. A method for producing an electrode body for a non-aqueous secondary battery, comprising: A positive electrode layer solution preparation step, preparing a positive electrode layer solution comprising a positive electrode active material, a binder and a first solvent; a positive electrode layer forming step, using the positive electrode layer solution to form a positive electrode layer; An electrolyte layer forming step of forming an electrolyte layer including a solid electrolyte; An adhesive layer solution preparation step, preparing an adhesive layer solution including a solid electrolyte and a second solvent; an adhesive layer forming step, using the adhesive layer solution to form an adhesive layer; and A lamination step of laminating the positive electrode layer, the adhesive layer and the electrolyte layer in sequence; The solubility of the second solvent in the binder is greater than that of the first solvent.

2. The method for producing an electrode body for a non-aqueous secondary battery according to claim 1, wherein: The second solvent has a lower boiling point than the first solvent.

3. The method for producing an electrode body for a non-aqueous secondary battery according to claim 1 or 2, wherein: In the lamination step, when the positive electrode layer and the adhesive layer are laminated, the second solvent is present at least in the adhesive layer.

4. The method for producing an electrode body for a non-aqueous secondary battery according to claim 3, wherein: The aforementioned adhesive layer solution does not contain an adhesive.

5. The method for producing an electrode body for a non-aqueous secondary battery according to claim 1 or 2, wherein: The adhesive layer solution contains the same type of binder as the binder contained in the positive electrode layer solution.