Non-sticky composite current collector and preparation method thereof
By forming the first coating and the second coating with different particle microstructures on the support layer of the composite current collector, the adhesion problem of the composite current collector is solved, and the battery performance and finished product qualification rate are improved.
Patent Information
- Application Number
- CN202410808669.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-21
- Publication Date
- 2024-10-01
AI Technical Summary
Composite current collectors are prone to adhesion problems during rolling, storage and transportation, resulting in inability to open or surface damage, affecting battery performance.
A first coating layer and a second coating layer with different particle microstructures are formed on the two surfaces of the support layer of the composite current collector. Vertical columnar and inclined columnar particle structures are formed through vacuum evaporation to ensure that the particles do not penetrate and adhere to each other. .
This effectively prevents the composite current collector from adhering to each other during rolling, storage and transportation, and improves the finished product qualification rate and battery performance.
Smart Images

Figure CN118738402A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of lithium batteries, and in particular to a non-adhesive composite current collector and a preparation method thereof. Background Art
[0002] The composite current collector is a new type of current collector material composed of polymer materials and metals. It is used to gather current in batteries. Its structure is a "sandwich" structure with a plastic film layer in the middle and two surfaces in the thickness direction of the plastic film layer. There are metal layers on the two surfaces. Compared with traditional pure metal current collectors, composite current collectors have advantages in safety and potential cost-effectiveness.
[0003] However, the composite current collectors currently produced by manufacturers are usually rolled up for storage and transportation. During the rolling up, storage and transportation process, the parts of the composite current collectors that are in contact with each other are prone to stick to each other, resulting in the composite current collector being unable to be opened or being forced open, causing damage to its surface, thereby affecting battery performance. Summary of the invention
[0004] In view of the above-mentioned deficiencies in the prior art, the object of the present invention is to provide a non-sticky composite current collector and a preparation method thereof, aiming to solve the problem that the composite current collector is prone to sticking when winding, and to improve the finished product qualification rate of the composite current collector.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions:
[0006] The present invention provides a non-stick composite current collector, which includes a support layer, wherein the support layer has a first coating and a second coating in the thickness direction, the first coating is arranged on one surface of the support layer, and the second coating is arranged on the other surface of the support layer, and the particle microstructure of the first coating is different from the particle microstructure of the second coating.
[0007] In one embodiment, the materials of the first coating and the second coating are independently selected from one or more of aluminum metal, nickel metal, titanium metal, copper metal, nickel alloy, copper alloy, aluminum alloy, and titanium alloy.
[0008] In one embodiment, the particles of the first coating layer are vertical columnar particles, and at least part of the particles of the second coating layer are inclined columnar particles.
[0009] In one embodiment, the particles of the first coating layer are flat particles, and the particles of the second coating layer are columnar particles.
[0010] In one embodiment, the angle between the inclined columnar particles and the support layer is greater than 45° and less than 90°.
[0011] In one embodiment, the content of the inclined columnar particles in the second coating layer is 80%-90%.
[0012] In one embodiment, an oxide layer of the first coating layer or an oxide layer of the second coating layer is correspondingly disposed on the first coating layer or the second coating layer.
[0013] In one embodiment, the roughness of the first coating layer is different from the roughness of the second coating layer.
[0014] In one embodiment, the density of the support layer is greater than the density of the first coating layer and the second coating layer.
[0015] The present invention also provides a method for preparing a non-stick composite current collector, which comprises the following steps:
[0016] Providing a support layer, and placing the support layer in a vacuum chamber;
[0017] forming a first coating layer on one surface of the support layer and forming a second coating layer on the other surface of the support layer by vacuum evaporation to obtain a metal-coated support layer, wherein the particle microstructure of the first coating layer is different from the particle microstructure of the second coating layer;
[0018] The metal-coated support layer is cooled to obtain the non-stick composite current collector.
[0019] Compared with the prior art, the present invention provides a non-stick composite current collector and a preparation method thereof, wherein the non-stick composite current collector comprises a support layer, wherein the support layer has a first coating layer and a second coating layer in the thickness direction, wherein the first coating layer is disposed on one surface of the support layer, and the second coating layer is disposed on another surface of the support layer, and the particle microstructure of the first coating layer is different from the particle microstructure of the second coating layer. The non-stick composite current collector of the present invention forms a first coating layer and a second coating layer with different particle microstructures on two surfaces of the support layer, respectively, so that when the first coating layer and the second coating layer contact each other, the particles will not penetrate each other and bond together, so that the parts of the composite current collector that contact each other during the winding, storage and transportation process will not be unable to be opened or the surface will be damaged due to mutual adhesion, effectively improving the finished product qualification rate of the composite current collector, which is beneficial to improving battery performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the prior art descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those of ordinary skill in the art, other drawings can be obtained according to the structures shown in these drawings without creative work. In the drawings:
[0021] Figure 1 Schematic diagram of the structure of the non-stick composite current collector in an embodiment of the present invention;
[0022] Figure 2 An electron microscope image of the second coating layer of the non-stick composite current collector in an embodiment of the present invention;
[0023] Figure 3 Another electron microscope image of the second coating layer of the non-stick composite current collector in an embodiment of the present invention;
[0024] Figure 4 Flow chart of the method for preparing the non-stick composite current collector in an embodiment of the present invention. DETAILED DESCRIPTION
[0025] In order to make the technical problems, technical solutions and beneficial effects to be solved by the embodiments of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0026] It should be noted that when a component is referred to as being "fixed to" or "disposed on" another component, it can be directly on the other component or indirectly on the other component. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element. In addition, connection can be used for fixing or for circuit connection.
[0027] It should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the embodiments of the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0028] In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the embodiments of the present invention, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined. In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the ability of ordinary technicians in the field to implement. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0029] The present invention provides a non-stick composite current collector, such as Figure 1 As shown, the non-stick composite current collector includes a support layer 100, wherein the support layer 100 has a first coating layer 201 and a second coating layer 202 in a thickness direction, wherein the first coating layer 201 is disposed on one surface of the support layer 100, and the second coating layer 202 is disposed on another surface of the support layer 100, for example Figure 1 The first coating 201 is arranged on the upper surface of the support layer 100, and the second coating 202 is arranged on the lower surface of the support layer 100. Of course, the first coating 201 can also be arranged on the lower surface of the support layer 100, and the second coating 202 can be arranged on the upper surface of the support layer 100, which is not limited in this embodiment. Among them, the particle microstructure of the first coating 201 is different from the particle microstructure of the second coating 202. Since the first coating 201 and the second coating 202 respectively arranged on the two surfaces will contact each other during the winding, storage and transportation of the composite current collector, the present invention forms the first coating 201 and the second coating 202 with different particle microstructures on the two surfaces of the support layer 100, respectively, so that when the first coating 201 and the second coating 202 contact each other, the particles will not penetrate each other and stick together, so that the parts of the composite current collector that contact each other during the winding, storage and transportation will not be unable to open or the surface will be damaged due to mutual adhesion, which effectively improves the qualified rate of the finished composite current collector and is conducive to improving the battery performance.
[0030] Specifically, the support layer 100 is a film made of at least one material selected from polyamide, polyterephthalate, polyimide, polyethylene, polypropylene, polystyrene, polyvinyl chloride, acrylonitrile-butadiene-styrene copolymer, polybutylene terephthalate, poly(p-phenylene terephthalamide), polypropylene, polyoxymethylene, epoxy resin, phenolic resin, polytetrafluoroethylene, polyvinylidene fluoride, silicone rubber, and polycarbonate. Using a film made of a polymer material as the support layer 100 is beneficial to improving the safety and lightness of the current collector and improving the energy density of the battery.
[0031] In the present invention, PP film is preferably used as the support layer 100, because it is more acid- and alkali-resistant and can greatly improve the service life of the composite current collector of the present invention. The PP film is preferably 3um-8um, which can reduce the mass of the current collector of the present invention and improve the energy density of the battery.
[0032] Preferably, the thickness of the first coating layer 201 and the second coating layer 202 is 1 um, which can provide good conductivity while maintaining the light weight of the composite current collector. The thicker the thickness, the worse the density, which will affect the conductive effect. By using the first coating layer 201 and the second coating layer 202 with different particle microstructures of appropriate thickness, the light weight characteristics of the composite current collector can be improved while avoiding adhesion of the composite current collector.
[0033] Specifically, the materials of the first coating 201 and the second coating 202 are independently selected from one or more of aluminum metal, nickel metal, titanium metal, copper metal, nickel alloy, copper alloy, aluminum alloy, and titanium alloy. The materials of the first coating 201 and the second coating 202 can be the same, for example, the materials of the first coating 201 and the second coating 202 are both copper metal; or the materials of the first coating 201 and the second coating 202 can be different, for example: the material of the first coating 201 is copper metal, and the material of the second coating 202 is nickel alloy, which can be flexibly selected according to actual needs.
[0034] Preferably, in the non-stick composite current collector of the present invention, the particles of the first coating 201 are vertical columnar particles, and at least part of the particles of the second coating 202 are inclined columnar particles. That is, the first coating 201 and the second coating 202 in this embodiment are similar in that the microscopic particles of both are columnar particles, preferably formed in one step and grown on the two surfaces of the support layer 100 to improve the binding force of the metal particles; the difference is that the particles of the first coating 201 are vertical columnar particles that are perpendicular to the support layer 100, while the particles of the second coating 202 include at least part of the inclined columnar particles that are not perpendicular to the support layer 100, such as Figure 2As shown, it is a microstructure diagram of the second coating 202. The particles of the second coating 202 are columnar particles, which grow on the support layer 100 in a one-time molding, and the columnar particles are not formed vertically on the support layer 100. At least part of the columnar particles are inclined columnar particles that form a certain angle with the support layer 100. In this way, not only the particle microstructures of the first coating 201 and the second coating 202 are different, and the non-adhesion effect is achieved, but also compared with the particles being vertically arranged on the support layer 100, when used in a battery, the electrolyte will not easily contact the support layer 100 through the gaps between the particles, thereby improving the life of the composite current collector of the present invention. Specifically, the particles of the second coating 202 can all be inclined columnar particles, or part of them can be inclined columnar particles and the remaining part can be vertical columnar particles. The content of the inclined columnar particles can be flexibly adjusted according to demand, and this embodiment does not limit this.
[0035] Preferably, in the non-stick composite current collector of the present invention, the particles of the first coating layer 201 are flat particles, and the particles of the second coating layer 202 are columnar particles. That is, in this embodiment, by making the microstructure of the particles of the first coating layer 201 a flat structure, such as a circular or elliptical structure or other polygonal structure, and the microstructure of the particles of the second coating layer 202 a columnar structure, such as all vertical columnar particles, or all inclined columnar particles, or both vertical columnar particles and inclined columnar particles, the purpose of making the microscopic particle structures of the coatings on the two surfaces of the support layer 100 different can be achieved, thereby preventing the coatings from sticking to each other.
[0036] Further, in the non-stick composite current collector of the present invention, when there are inclined columnar particles in the second coating 202, the angle between the inclined columnar particles and the support layer 100 is greater than 45° and less than 90°. When the second coating 202 having inclined columnar particles is formed on the support layer 100, taking the vacuum evaporation method as an example, the inclination angle of the inclined columnar particles can be achieved by controlling the speed of the support layer 100 in the vacuum chamber and the number of evaporation boats arranged in the vacuum chamber. For example, in production, the speed of the support layer 100 in the vacuum chamber is controlled to be 5-7m / min. In the vacuum chamber, two evaporation areas are provided, and the number of evaporation boats in each evaporation area is 10-16 in total, divided into two rows, 5-8 in one row, and arranged alternately on the left and right. During the vacuum evaporation process, the metal melts into liquid in the evaporation boat, forming metal vapor that begins to volatilize. The atoms in the vapor are rapidly transmitted to the upper support layer 100 in a linear motion with basically no collision. The gaseous particles reaching the surface of the support layer 100 adhere to the surface of the support layer 100 to deposit and grow. The deposition position and angle of the metal particles on the support layer 100 are related to the starting position of the metal particles (i.e., the arrangement position and number of the evaporation boats in the vacuum chamber), and are also related to the moving speed of the support layer 100 itself (i.e., the moving speed of the support layer 100 in the vacuum chamber). By controlling the moving speed of the support layer 100 in the vacuum chamber and the number and distribution of the evaporation boats during production, columnar particles with an inclination angle of 45°-90° to the support layer 100 can be obtained, thereby improving the life of the composite current collector. This method is specifically implemented in a vacuum evaporation device of suspended plating. Suspended plating means that the support layer 100 passes through the upper part of the evaporation boat and then the support layer 100 is cooled, rather than being cooled when passing through the upper part of the evaporation boat. Suspended plating can make the coating more uniform, the cooling effect better, and the coating quality higher.
[0037] Furthermore, in the non-stick composite current collector of the present invention, when there are inclined columnar particles in the second coating 202, the content of the inclined columnar particles in the second coating 202 is 80%-90%, and the remaining columnar particles can be vertical particles perpendicular to the support layer 100. The second coating 202 has both inclined columnar particles and vertical particles. The presence of vertical particles can release the stress formed by the second coating 202 of inclined columnar particles. The stresses offset each other, which can greatly reduce the curling and warping of the plated film, affecting the adhesion of the current collector and the subsequent processing performance of the current collector coating process. Specifically, the content of inclined columnar particles and vertical particles can be adjusted by multiple coatings in a vacuum chamber. For example, in a vacuum chamber of suspension plating, a small amount or a large number of inclined columnar particles are first formed on the support layer 100 by a fast travel speed and a small number of evaporation boats, and then a slow travel speed, a large number of evaporation boats or a small number of evaporation boats are used to form vertical particles. For example, when forming 80%-90% columnar inclined columnar particles, a film speed of 2-3m / min can be used first, with 2-3 evaporation boats in a row, 2 rows in total, cross-arranged, and 4-6 in total; then use suspended vacuum evaporation, and then use a travel speed of 5-7m / min, with 4-6 evaporation boats in a row, 2 rows in total, and relatively arranged evaporation boats for coating, so as to form a second coating 202 with both inclined columnar particles and vertical particles on the support layer 100, thereby improving the performance of the composite current collector.
[0038] Furthermore, in the non-stick composite current collector of the present invention, the diameter of the inclined columnar particles with a certain angle is greater than 50nm and less than or equal to 150nm. The composite current collector with such metal coating particles can be formed more quickly, reduces the overall cost of the composite current collector, and is not easy to fall off.
[0039] Furthermore, in the non-stick composite current collector of the present invention, the average gap between the metal coating particles is greater than 0 nm and less than or equal to 10 nm, so that the coating of the composite current collector can have better density. Figure 2 As shown, when used in a battery, it is difficult for the electrolyte to penetrate into and react with the support layer, thereby increasing the service life of the battery.
[0040] Preferably, in the non-stick composite current collector of the present invention, the first coating layer 201 or the second coating layer 202 is also provided with an oxide layer of the first coating layer 201 or the oxide layer of the second coating layer 202. On the basis that the particle microstructures of the first coating layer 201 and the second coating layer 202 are different, an oxide layer of the first coating layer 201 or the second coating layer 202 is formed on the first coating layer 201 or the second coating layer 202, so that the first coating layer 201 or the second coating layer 202 has a different structure from the oxide layer, which can prevent the first coating layer 201 and the second coating layer 202 from adhering to each other, thereby improving the anti-sticking effect.
[0041] Preferably, the thickness of the oxide layer is 10 nm-50 nm, which can reduce the damage to the conductive performance of the first coating 201 or the second coating 202 and also prevent the first coating 201 and the second coating 202 from being bonded.
[0042] Preferably, in the non-stick composite current collector of the present invention, the roughness of the first coating 201 is different from the roughness of the second coating 202. By performing roughness treatment on the first coating 201 or the second coating 202, for example, by changing the roughness of the first coating 201 or the second coating 202 through roughness treatment methods such as plasma treatment, corona treatment or manual polishing, the roughness between the first coating 201 and the second coating 202 is different, so that the first coating 201 and the second coating 202 cannot adhere to each other, thereby improving the anti-adhesion effect. After unlimited tests by the inventor, when the difference between the roughness of the first coating 201 and the roughness of the second coating 202 is in the range of 0.02ra-0.1ra, the effect is best. If it is too high, the surface stress of the first coating 201 and the second coating 202 will be damaged, resulting in curling.
[0043] Preferably, in the non-stick composite current collector of the present invention, the density of the support layer 100 is greater than the density of the first coating layer 201 and the second coating layer 202. This can prevent the first coating layer 201 and the second coating layer 202 from burning the support layer 100 into holes when the first coating layer 201 and the second coating layer 202 are formed on the support layer 100, thereby improving the qualified rate of finished products.
[0044] Preferably, in the non-stick composite current collector of the present invention, the upper and lower surfaces of the support layer 100 have a structure of low sites and high sites, wherein the low sites are areas below the plane where the support layer 100 is located, and the high sites are areas above the plane where the support layer 100 is located, and the particles of the first coating 201 and the second coating 202 are located in the low sites and the high sites, and multiple high sites surround the low sites. Figure 3As shown at the bottom, the surface of the support layer 100 in the composite current collector of the present invention is not smooth. Before preparing the first coating 201 and the second coating 202 on the upper and lower surfaces of the support layer 100, a physical method, such as corona or plasma treatment, or a chemical etching method is used to treat the surface of the support layer 100, so that the structure with low sites and high sites is formed on the upper and lower surfaces of the support layer 100, so that the first coating 201 and the second coating 202 of the composite current collector after coating also form a high-low structure, and then the coating on the surface of the composite current collector forms a structure similar to a hole, which helps to release stress and prevent curling, etc. On the other hand, when the active material is coated on the composite current collector, the hole can be more closely combined with the active material to prevent the active material from falling off. More active materials can also be coated to increase the energy density of the battery. Preferably, the number of high sites on the support layer 100 is 2-5 times the number of low sites, so that better effects can be achieved.
[0045] Preferably, in the non-sticky composite current collector of the present invention, a lithium-philic layer is further provided on the first coating layer 201 and the second coating layer 202, and the thickness of the lithium-philic layer is 10nmn-50nm. At this time, since the first coating layer 201 and the second coating layer 202 on the surface of the composite current collector are affected by the high and low positions of the support layer 100 to form holes, the lithium-philic layer covers both the holes and other positions. By providing the lithium-philic coating, on the one hand, the lithium source can be supplemented for the battery, and on the other hand, the metal coating can be protected from oxidation, thereby improving the battery performance.
[0046] Preferably, in the non-stick composite current collector of the present invention, an anti-corrosion layer is also provided between the first coating layer 201 and the second coating layer 202 and the support layer 100. When the first coating layer 201 and the second coating layer 202 are prepared by vacuum evaporation, the anti-corrosion layer is also formed in the evaporation cavity, that is, the anti-corrosion layer is first formed on the two surfaces of the support layer 100, and then the first coating layer 201 and the second coating layer 202 are respectively formed on the anti-corrosion layers on the two surfaces. The one-step coating method improves the coating efficiency and also avoids the coating from being oxidized. The particle microstructure of the anti-corrosion layer is circular or elliptical or other polygonal structure. The main function of the anti-corrosion layer is to prevent the electrolyte from corroding the support layer 100, and it can also enhance the bonding force between the first coating layer 201 and the second coating layer 202 and the support layer 100. From the microscopic structure, the morphological characteristics of the anti-corrosion layer are circular or elliptical or other polygonal structures, which are different from the morphology of the first coating layer 201 and the second coating layer 202. Preferably, the structure is multi-deformed, and the particles of the radiation protection layer are in close contact with each other, which can prevent the electrolyte from corroding the support layer 100 and improve the service life. The material of the anti-corrosion layer can be aluminum oxide, silicon oxide, etc.
[0047] The present invention also provides a method for preparing a non-stick composite current collector. Figure 4As shown, it includes the following steps:
[0048] S100, providing a support layer, and placing the support layer in a vacuum chamber;
[0049] S200, forming a first coating on one surface of the support layer by vacuum evaporation, and forming a second coating on the other surface of the support layer to obtain a metal-coated support layer, wherein the particle microstructure of the first coating is different from the particle microstructure of the second coating;
[0050] S300, cooling the metal-coated support layer to obtain the non-stick composite current collector.
[0051] The preparation method of the non-stick composite current collector of the present invention is a one-step molding method, firstly, a support layer is taken, and then the support layer is placed in a vacuum cavity, vacuumized, and then a metal coating with a thickness of 1um is formed on the upper and lower surfaces of the support layer in the vacuum cavity by vacuum evaporation for multiple times, wherein the metal coating includes a first coating and a second coating with different particle microstructures, and vacuum evaporation refers to: melting the metal into a liquid state, forming metal vapor to begin to volatilize, and then condensing the atoms in the vapor to deposit and grow on the surface of the polymer material, and the deposition speed of vacuum evaporation is 3-4 times that of magnetron sputtering, and the thickness of the metal coating can be quickly supplemented, and its advantages are: 1) heating and melting, fast film forming rate and high efficiency; 2) evaporation and attachment do not require a high voltage electric field, and the equipment is relatively simple and easy to operate; 3) the momentum of vacuum heating evaporation atoms is low, and the film thickness is uniform. The one-shot molding method completes the coating in one vacuum chamber without frequently opening and closing the vacuum chamber, which saves energy and is more efficient. At the same time, because there is no need to open and close the vacuum chamber, there is no process of transferring to the next workspace after production in multiple molding, so the coating can be prevented from being oxidized and the yield rate can be improved.
[0052] The present invention forms a first coating layer and a second coating layer with different particle microstructures on two surfaces of a support layer in one step by vacuum evaporation, so that when the first coating layer and the second coating layer contact each other, the particles will not penetrate each other and stick together, so that the parts of the composite current collector that contact each other during the winding, storage and transportation process will not be unable to be opened or the surface will be damaged due to mutual adhesion, which effectively improves the qualified rate of the finished product of the composite current collector and is beneficial to improving the battery performance.
[0053] Preferably, before the step of forming a first coating on one surface of the support layer and forming a second coating on another surface of the support layer by vacuum evaporation to obtain the metal-coated support layer, the method further comprises:
[0054] The support layer is surface treated to obtain a structure with low sites and high sites on the upper and lower surfaces of the support layer.
[0055] The present invention performs surface treatment on the support layer before forming the metal coating, so that the surface of the support layer of the subsequent coating is not smooth. Physical methods, such as corona or plasma treatment, or chemical etching methods can be used to treat the support layer, so as to form a structure with low sites and high sites on the upper and lower surfaces of the support layer, wherein the low site is a region below the plane where the support layer is located, and the high site is a region above the plane where the support layer is located. Multiple high sites surround the low site, and the particles of the metal coating after evaporation of the metal coating are located in the low site and the high site. The upper and lower surfaces of the support layer are formed by surface treatment to form such a structure with low sites and high sites, so that the metal coating of the composite current collector after coating also forms a high-low structure, and then the metal coating on the surface of the composite current collector forms a structure similar to a hole, which helps to release stress and prevent curling, etc. on the one hand, and on the other hand, when the active material is coated on the composite current collector, the hole can be more closely combined with the active material to prevent the active material from falling off. More active materials can also be coated to improve the energy density of the battery. Preferably, the number of high sites on the support layer is 2-5 times the number of low sites, so that better effects can be achieved.
[0056] Preferably, after the step of forming a first coating on one surface of the support layer and a second coating on another surface of the support layer by vacuum evaporation to obtain a metal-coated support layer, the method further comprises:
[0057] The first coating layer or the second coating layer is subjected to roughness treatment so that the roughness of the first coating layer is different from the roughness of the second coating layer.
[0058] After forming the first coating and the second coating on the two surfaces of the support layer, the present invention further changes the roughness of the first coating or the second coating by roughness treatment methods such as plasma treatment, corona treatment or manual polishing, so that the roughness of the first coating and the second coating is different, thereby preventing the first coating and the second coating from adhering to each other, thereby improving the anti-adhesion effect. After unlimited tests by the inventor, when the difference between the roughness of the first coating and the roughness of the second coating is in the range of 0.02ra-0.1ra, the effect is best. If it is too high, the surface stress of the first coating and the second coating will be damaged, resulting in curling.
[0059] Preferably, an optical density tester can be added to the vacuum evaporation. The optical density tester directly senses the light transmittance or optical density of the film through optical contact, and uses a certain proportional relationship between optical density and coating thickness to detect the uniformity of coating thickness. By adding an optical density tester to the vacuum evaporation, the thickness of the coating formed on the support layer can be detected online at any time. In this way, there is no need to open the cavity and then use a square resistance tester to detect the coating thickness, so that the coating thickness is accurately controllable, which effectively improves the preparation efficiency and performance reliability of the non-stick composite current collector.
[0060] In summary, the present invention provides a non-stick composite current collector and a preparation method thereof, wherein the non-stick composite current collector comprises a support layer, wherein the support layer has a first coating layer and a second coating layer in a thickness direction, wherein the first coating layer is disposed on one surface of the support layer, and the second coating layer is disposed on another surface of the support layer, and the particle microstructure of the first coating layer is different from the particle microstructure of the second coating layer. The non-stick composite current collector of the present invention forms a first coating layer and a second coating layer with different particle microstructures on two surfaces of the support layer, respectively, so that when the first coating layer and the second coating layer contact each other, the particles will not penetrate each other and bond together, so that the parts of the composite current collector that contact each other during the winding, storage and transportation process will not be unable to be opened or the surface will be damaged due to mutual adhesion, effectively improving the finished product qualification rate of the composite current collector, which is beneficial to improving battery performance.
[0061] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For those skilled in the art of the present invention, several equivalent substitutions or obvious variations can be made without departing from the concept of the present invention, and the performance or use is the same, which should be regarded as belonging to the protection scope of the present invention.
Claims
1. A non-stick composite current collector, characterized in that: The invention comprises a supporting layer, wherein the supporting layer has a first coating and a second coating in a thickness direction, wherein the first coating is arranged on one surface of the supporting layer, and the second coating is arranged on another surface of the supporting layer, and the particle microstructure of the first coating is different from the particle microstructure of the second coating.
2. The non-stick composite current collector according to claim 1, characterized in that: The materials of the first coating layer and the second coating layer are independently selected from one or more of aluminum metal, nickel metal, titanium metal, copper metal, nickel alloy, copper alloy, aluminum alloy, and titanium alloy.
3. The non-stick composite current collector according to claim 1, characterized in that: The particles of the first coating layer are vertical columnar particles, and at least part of the particles of the second coating layer are inclined columnar particles.
4. The non-stick composite current collector according to claim 1, characterized in that: The particles of the first coating layer are flat particles, and the particles of the second coating layer are columnar particles.
5. The non-stick composite current collector according to claim 3, characterized in that: The angle between the inclined columnar particles and the support layer is greater than 45° and less than 90°.
6. The non-stick composite current collector according to claim 3, characterized in that: The content of the inclined columnar particles in the second coating layer is 80%-90%.
7. The non-stick composite current collector according to claim 1, characterized in that: The first coating layer or the second coating layer is also provided with an oxide layer of the first coating layer or an oxide layer of the second coating layer correspondingly.
8. The non-stick composite current collector according to claim 1, characterized in that: The roughness of the first coating layer is different from the roughness of the second coating layer.
9. The non-stick composite current collector according to claim 1, characterized in that: The density of the support layer is greater than the density of the first coating layer and the second coating layer.
10. A method for preparing a non-stick composite current collector, characterized in that: The steps include: Providing a support layer, and placing the support layer in a vacuum chamber; forming a first coating layer on one surface of the support layer and forming a second coating layer on the other surface of the support layer by vacuum evaporation to obtain a metal-coated support layer, wherein the particle microstructure of the first coating layer is different from the particle microstructure of the second coating layer; The metal-coated support layer is cooled to obtain the non-stick composite current collector.