A solid waste-based modular artificial wetland filler

By using core-shell slag particles and sludge in artificial wetland fillers and forming polymer coatings through polymer solutions, the problems of filler blockage and stability are solved, and pollutant adsorption capacity and wetland system treatment efficiency are improved.

CN118743985BActive Publication Date: 2024-11-12皖创环保股份有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411233650.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-12
Estimated Expiration
2044-09-04

AI Technical Summary

Technical Problem

Existing artificial wetland fillers are prone to pore blockage due to the accumulation of moisture and organic matter during long-term use, which affects the sewage treatment effect, and microbial metabolites may lead to changes in the filler structure and performance, affecting the stability and purification ability of the wetland system.

Method used

Core-shell slag particles and sludge are used as filler raw materials, and a stable polymer coating is formed under ultrasonic treatment through polymer solution to enhance the adsorption and mechanical strength of the filler, and a tight core-shell structure is formed to improve the adsorption capacity of pollutants. and selectively reduce the risk of blockage.

Benefits of technology

It improves the adsorption capacity and selectivity of the filler, extends the service life, prevents expansion and blockage caused by excessive water absorption, maintains the smoothness of the pore structure, and thus improves the treatment efficiency of pollutants in the wetland system.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to the technical field of artificial wetland fillers, and in particular to a solid waste-based modular artificial wetland filler, which includes the following raw materials by weight: 30-60 parts of core-shell slag particles, 10-20 parts of sludge, and 1-8 parts of binder; wherein, the core-shell slag particles are prepared by the following steps: S1, collecting slag, first washing it with water, removing iron, then pickling it, neutralizing it to a pH value of 6-7, crushing it, and obtaining pre-treated slag; S2, immersing the pre-treated slag in a polymer solution, ultrasonically treating it for 10-30min, filtering and washing it, and heat treating it for 2-4h to obtain core-shell slag particles. The present invention utilizes the resource attribute characteristics of high compressive strength, high specific surface area and porosity of biomass power plant slag, and prepares artificial wetland fillers by modifying the slag, effectively reducing the cost of the filler while improving the operating efficiency of the artificial wetland.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of artificial wetland fillers, and in particular to a solid waste-based modular artificial wetland filler. Background Art

[0002] As an efficient, low-cost and environmentally friendly sewage treatment technology, artificial wetlands have been widely used in the deep treatment of tailwater from sewage treatment plants in recent years. Its core advantage is that it produces almost no sludge and can significantly remove pollutants that are difficult to treat with traditional processes, such as pesticides, hormones, surfactants, etc. At the same time, artificial wetlands play a positive role in maintaining biodiversity and providing ecological services, and are of great significance for water resource conservation and recycling. The action mechanism of fillers in artificial wetlands is complex, involving multiple reactions such as physical filtration, adsorption precipitation, ion exchange and chemical chelation. It not only directly removes pollutants, but also provides a medium for the attachment and growth of wetland plants and microorganisms. In the selection of filler raw materials, low cost and stable supply are key considerations. As a waste, biomass power plant slag has the advantages of high strength, high specific surface area, adjustable particle size and low cost, and is an ideal raw material for preparing artificial wetland fillers.

[0003] With the increasing use of biomass energy, the amount of slag produced by biomass power plants is also increasing. my country is rich in biomass resources. The theoretical annual production of straw resources in my country is about 829 million tons, and the collectible resources are about 694 million tons. Based on the average ash production of 6.8% of dry biomass, the annual production of ash is about 47 million tons. However, the stacking of ash not only occupies land resources, but also may bring risks to the surrounding environment.

[0004] In the prior art, the invention patent with the patent publication number CN111499000A discloses an artificial wetland filler and a preparation method thereof, including activated sludge, blast furnace slag, carbon slag, bentonite, nitrogen adsorbent and phosphorus adsorbent, which has the advantages of low raw material price, easy availability, strong adsorption of phosphorus and nitrogen, etc. However, in practical applications, only relying on slag, carbon slag, etc. as adsorption media, the adsorption capacity is small, a large amount of water, organic matter and difficult-to-degrade organic matter will gradually accumulate in the wetland, and easily adsorb on the surface of the filler, causing the pores of the filler to be blocked. On the other hand, the microorganisms in the wetland will multiply in large numbers in the process of decomposing organic pollutants, and the metabolites produced may also cause the clogging of the filler. Once the blockage occurs, the water receiving capacity of the wetland will be significantly reduced, thereby affecting the sewage treatment effect of the entire wetland system. In addition, fillers such as sludge and carbon slag will be chemically eroded, and the ion exchange capacity is limited, resulting in changes in their structure and performance, thereby affecting the stability and purification capacity of the wetland system. Summary of the invention

[0005] In order to solve the problems mentioned in the above background technology, the present invention provides a solid waste-based modular artificial wetland filler.

[0006] In order to achieve the above object, the present invention adopts the following technical solutions:

[0007] A solid waste-based modular artificial wetland filler, comprising the following raw materials by weight: 30-60 parts of core-shell slag particles, 10-20 parts of sludge, and 1-8 parts of a binder;

[0008] The core-shell slag particles are prepared by the following steps:

[0009] S1. Collect slag particles from a biomass power plant, wash them with water to remove dust and impurities on the surface, remove iron with a magnetic separator, and then pickle them with dilute hydrochloric acid to remove alkaline oxides and other soluble impurities. After pickling, neutralize them with a 0.1 mol / L sodium hydroxide solution, adjust the pH value to 6-7, crush the slag, and pass it through a 200-mesh sieve to obtain pretreated slag;

[0010] S2. Immerse the pretreated slag in a polymer solution. Under ultrasonic treatment, allow the polymer solution to fully penetrate into the pores of the slag particles and interact with the slag surface. The ultrasonic treatment time is 10-30 minutes. After the treatment is completed, filter and wash, and heat treat for 2-4 hours to allow the polymer coating to form a stable core-shell structure on the slag surface.

[0011] Furthermore, the binder includes one or more of silicate cement, gypsum or water glass.

[0012] Furthermore, in step S2, the power of the ultrasonic treatment is 100-200 W, and the frequency of the ultrasonic treatment is 40-50 KHz.

[0013] Furthermore, the temperature of the heat treatment in step S2 is 50-60°C.

[0014] Furthermore, the polymer solution in step S2 is prepared by the following steps:

[0015] A1. Add amino acid methyl ester and methyl 2-fluoroacrylate to N,N-dimethylformamide, add 4-dimethylaminopyridine and tetrabutyl titanate under a nitrogen atmosphere, control the reaction temperature, and continue stirring the reaction to obtain a prepolymer solution;

[0016] A2. Pour the prepolymer solution into methanol, add dicyclohexylcarbodiimide, heat up and stir rapidly to react. After the reaction is completed, let it stand and precipitate. After filtering and washing, put it into a vacuum oven and dry it at 60-70°C to constant weight. Then use N,N-dimethylformamide as solvent to prepare a 20-30% polymer solution.

[0017] Furthermore, in step A1, the mass ratio of amino acid methyl ester, 2-fluoroacrylate methyl ester, N,N-dimethylformamide, 4-dimethylaminopyridine and tetrabutyl titanate is (10-15): (9-17): 20: (0.02-0.03): (0.5-0.7), and the amino acid methyl ester includes one of L-serine methyl ester hydrochloride, L-alanine methyl ester hydrochloride and L-methionine methyl ester hydrochloride.

[0018] Furthermore, in step A1, the reaction temperature is 40-45° C., the stirring speed is 100-200 rpm, and the reaction time is 1-3 h.

[0019] Furthermore, in step A2, the mass ratio of the prepolymer solution, methanol and dicyclohexylcarbodiimide is (10-12):20:(0.2-0.6).

[0020] Furthermore, in step A2, the reaction temperature is 60-70° C., the stirring speed is 300-400 rpm, and the reaction time is 20-40 min.

[0021] Furthermore, the artificial wetland filler is prepared by the following steps: weighing core-shell slag particles, sludge and binder by weight, putting them into a mixer after washing, mixing 5-20wt% water into a slurry, drying to constant weight, and granulating or cutting according to the particle size and shape.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] 1. In this technical solution, amino acid methyl ester and methyl 2-fluoroacrylate react in N,N-dimethylformamide solvent, 4-dimethylaminopyridine is used as a catalyst, and tetrabutyl titanate is used as a promoter to undergo a condensation reaction to generate a prepolymer having ester bonds and amide bonds, and the prepolymer molecular chain has amino, carboxyl and other functional groups. Dicyclohexylcarbodiimide is used as a cross-linking agent, and the carbodiimide group in its molecular structure can react with the carboxyl group on the polymer chain to generate a stable urea group, thereby achieving cross-linking between polymer chains and forming a more stable polymer three-dimensional network structure. The pores and channels in the polymer network structure are conducive to the adsorption and diffusion of pollutants, increase the adsorption capacity and selectivity of pollutants, reduce the occurrence of seasoning blockage, increase the service life, and avoid expansion and blockage caused by excessive water absorption.

[0024] 2. The flexible chains in the polymer solution prepared by the present technical solution are matched to the tiny bumps and pores on the surface of the slag particles by bending, twisting and stretching, penetrating into the pores of the slag particles to form a uniform shell layer and maximizing the contact area with the slag surface. After heat treatment, a tight core-shell structure is formed between the coating and the slag particles, in which the slag particles serve as the core and the polymer coating serves as the shell, forming a uniform composite material, which enhances the mechanical strength of the slag particles and provides more adsorption sites. The functional groups and pore structures on the surface of the polymer coating can adsorb and fix pollutants, resist damage from the external environment such as water erosion and microbial degradation, prevent deformation or collapse during use, maintain the patency of the pore structure, and thus improve the wetland system's treatment efficiency for pollutants. DETAILED DESCRIPTION

[0025] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0026] Unless otherwise specified, the raw materials used in the present invention are all from conventional products purchased on the market, the slag particles are from the biomass power plant in northern Anhui, and the sludge is from the secondary sedimentation tank of the urban domestic sewage treatment plant.

[0027] Preparation Example 1

[0028] The polymer solution is prepared by the following steps:

[0029] A1. Add 10 kg of L-serine methyl ester hydrochloride and 9 kg of methyl 2-fluoroacrylate to 2 kg of N,N-dimethylformamide, add 0.02 kg of 4-dimethylaminopyridine and 0.5 kg of tetrabutyl titanate under a nitrogen atmosphere, control the reaction temperature to 40°C, and continue stirring at a speed of 100 rpm for 1 hour to obtain a prepolymer solution;

[0030] A2. Pour 10kg of prepolymer solution into 20kg of methanol, add 0.2kg of dicyclohexylcarbodiimide, heat to 60°C, stir rapidly at 300rpm for 20min, let stand and precipitate after the reaction, filter and wash, put into a vacuum oven, dry to constant weight at 60°C, take 5kg of product and use 20kg of N,N-dimethylformamide as solvent to prepare a 20% polymer solution.

[0031] Preparation Example 2

[0032] The polymer solution is prepared by the following steps:

[0033] A1. Add 12.5 kg of L-alanine methyl ester hydrochloride and 13 kg of methyl 2-fluoroacrylate to 2 kg of N,N-dimethylformamide, add 0.025 kg of 4-dimethylaminopyridine and 0.6 kg of tetrabutyl titanate under a nitrogen atmosphere, control the reaction temperature to 42° C., and continue stirring at a speed of 150 rpm for 2 hours to obtain a prepolymer solution;

[0034] A2. Pour 11kg of prepolymer solution into 20kg of methanol, add 0.4kg of dicyclohexylcarbodiimide, heat to 65°C, stir rapidly at 350rpm for 30min, let stand to precipitate after the reaction, filter and wash, put into a vacuum oven, dry at 65°C to constant weight, take 5kg of product and use 15kg of N,N-dimethylformamide as solvent to prepare a 25% polymer solution.

[0035] Preparation Example 3

[0036] The polymer solution is prepared by the following steps:

[0037] A1. Add 15 kg of L-methionine methyl ester hydrochloride and 17 kg of methyl 2-fluoroacrylate to 2 kg of N,N-dimethylformamide, add 0.03 kg of 4-dimethylaminopyridine and 0.7 kg of tetrabutyl titanate under a nitrogen atmosphere, control the reaction temperature to 45°C, and continue stirring at a speed of 200 rpm for 3 hours to obtain a prepolymer solution;

[0038] A2. Pour 12kg of prepolymer solution into 20kg of methanol, add 0.6kg of dicyclohexylcarbodiimide, heat to 70°C, stir rapidly at 400rpm for 40min, let stand and precipitate after the reaction, filter and wash, put into a vacuum oven, dry to constant weight at 70°C, take 5kg of product and use 11.67kg of N,N-dimethylformamide as solvent to prepare a 30% polymer solution. Example 1

[0039] The solid waste-based modular artificial wetland filler is prepared by the following steps:

[0040] S1. Collect slag particles from a biomass power plant, wash them with water, remove iron with a magnetic separator, and then pickle them with dilute hydrochloric acid. After pickling, neutralize them with a 0.1 mol / L sodium hydroxide solution, adjust the pH value to 6, crush the slag, and pass it through a 200-mesh sieve to obtain pretreated slag;

[0041] S2, immerse 10 kg of pretreated slag in 10 L of polymer solution prepared in Preparation Example 1, and ultrasonically treat for 10 min, the power of ultrasonic treatment is 100 W, the frequency is 40 KHz, after the treatment is completed, filter and wash, and heat treat at 50 ° C for 2 h;

[0042] S3. Weigh 30 parts of core-shell slag particles, 10 parts of sludge and 1 part of Portland cement by weight, wash and put them into a mixer, add 5wt% water to make a slurry, and dry to constant weight. Example 2

[0043] The solid waste-based modular artificial wetland filler is prepared by the following steps:

[0044] S1. Collect slag particles from a biomass power plant, wash them with water, remove iron with a magnetic separator, and then pickle them with dilute hydrochloric acid. After pickling, neutralize them with a 0.1 mol / L sodium hydroxide solution, adjust the pH value to 7, crush the slag, and pass it through a 200-mesh sieve to obtain pretreated slag;

[0045] S2, immerse 10kg of pretreated slag in 10L of polymer solution prepared in Preparation Example 2, and ultrasonically treat for 20min, the power of ultrasonic treatment is 150W, the frequency is 45KHz, after the treatment, filter and wash, and heat treat at 55°C for 3h;

[0046] S3. Weigh 45 parts of core-shell slag particles, 15 parts of sludge and 4 parts of gypsum by weight, wash and put them into a mixer, add 10wt% water to a slurry state, and dry to constant weight to obtain the product. Example 3

[0047] The solid waste-based modular artificial wetland filler is prepared by the following steps:

[0048] S1. Collect slag particles from a biomass power plant, wash them with water, remove iron with a magnetic separator, and then pickle them with dilute hydrochloric acid. After pickling, neutralize them with a 0.1 mol / L sodium hydroxide solution, adjust the pH value to 7, crush the slag, and pass it through a 200-mesh sieve to obtain pretreated slag;

[0049] S2, immerse 10kg of pretreated slag in 10L of polymer solution prepared in Preparation Example 3, and ultrasonically treat for 30min, the power of ultrasonic treatment is 200W, the frequency is 50KHz, after the treatment is completed, filter and wash, and heat treat at 60°C for 4h;

[0050] S3. Weigh 60 parts of core-shell slag particles, 20 parts of sludge and 8 parts of water glass by weight, wash and put them into a mixer, add 5-20wt% water to a slurry state, and dry to constant weight to obtain the product.

[0051] Comparative Example 1

[0052] L-serine methyl ester hydrochloride was added to the solvent N,N-dimethylformamide to prepare a 0.1 mol / L solution.

[0053] Comparative Example 2

[0054] L-alanine methyl ester hydrochloride was added to the solvent N,N-dimethylformamide to prepare a 0.2 mol / L solution.

[0055] Comparative Example 3

[0056] L-methionine methyl ester hydrochloride was added to the solvent N,N-dimethylformamide to prepare a 0.3 mol / L solution.

[0057] Comparative Example 4

[0058] Methyl 2-fluoroacrylate was added to N,N-dimethylformamide to prepare a 0.1 mol / L solution.

[0059] Comparative Example 5

[0060] The difference between this comparative example and Example 1 is that in step S2, the sample is immersed in the solution prepared in Comparative Example 1, and the remaining steps are the same as those in Example 1.

[0061] Comparative Example 6

[0062] The difference between this comparative example and Example 2 is that in step S2, the sample is immersed in the solution prepared in Comparative Example 2, and the remaining steps are the same as those in Example 2.

[0063] Comparative Example 7

[0064] The difference between this comparative example and Example 3 is that in step S2, the sample is immersed in the solution prepared in Comparative Example 3, and the remaining steps are the same as those in Example 3.

[0065] Comparative Example 8

[0066] The difference between this comparative example and Example 1 is that in step S2, the sample is immersed in the solution prepared in Comparative Example 4, and the remaining steps are the same as those in Example 1.

[0067] Comparative Example 9

[0068] The difference between this comparative example and Example 2 is that in step S2, the mixture is immersed in N,N-dimethylformamide, and the remaining steps are the same as those in Example 2.

[0069] Comparative Example 10

[0070] The difference between this comparative example and Example 3 is that the substrate is immersed in deionized water in step S2, and the remaining steps are the same as those in Example 3.

[0071] The artificial wetland fillers prepared in Examples 1-3 and Comparative Examples 5-10 were subjected to treatment performance tests.

[0072] (Ⅰ)Experimental setup:

[0073] Water inlet system: An adjustable flow water inlet system, including a 100L water storage tank and an adjustable flow meter;

[0074] Wetland beds: multiple wetland beds and drainage outlets of the same size, the bed size is 1m long × 0.5m wide × 0.6m high, the number of beds is 9, and the drainage outlet diameter is 5cm;

[0075] Outlet system: an outlet collection system, including an outlet and a sampling port. The outlet diameter is 5 cm. The sampling port is located 10 cm above the outlet. The sampling frequency is once a week.

[0076] (II) Filling:

[0077] The fillers prepared in Examples 1-3 and Comparative Examples 5-10 were cut into 10 cm×10 cm×20 cm modules, loaded into the wetland bed in a staggered arrangement with a gap of 2 cm between each layer, and filled with soil to construct a small vertical subsurface flow artificial wetland.

[0078] (III) Planting:

[0079] 70% of reeds and 30% of cattails were planted in each wetland bed, and the number of plants planted in each wetland bed was the same.

[0080] (IV) Water quality monitoring:

[0081] The wastewater produced by a chemical plant was divided into 9 batches and introduced into each wetland bed respectively, with a flow rate of 10 mL / min and a retention time of 24 h. The influent water quality is shown in Table 1:

[0082] Table 1. Influent water quality (unit: mg / L)

[0083] name content <![CDATA[BOD5]]> 68.5 <![CDATA[COD Cr ]]> 139.3 SS 21.4 <![CDATA[NH3-N]]> 12.7 TP 2.4

[0084] Referring to HJ 2005-2010 "Technical Specifications for Constructed Wetland Wastewater Treatment Engineering", the pollutant removal efficiency of each wetland bed is shown in Table 2:

[0085] Table 2. Pollutant removal efficiency of each wetland bed (unit: %)

[0086] serial number <![CDATA[BOD5]]> <![CDATA[COD Cr ]]> SS <![CDATA[NH3-N]]> TP Example 1 83.85 79.36 65.24 72.25 91.77 Example 2 86.24 80.35 66.92 73.32 92.18 Example 3 87.21 83.42 65.87 77.01 92.21 Comparative Example 5 61.70 68.32 62.72 62.24 72.21 Comparative Example 6 62.14 67.96 63.32 63.41 76.54 Comparative Example 7 58.36 67.87 66.17 63.59 73.44 Comparative Example 8 9.85 10.58 60.21 44.32 22.94 Comparative Example 9 18.35 14.25 59.05 33.27 13.58 Comparative Example 10 10.43 12.32 58.23 31.24 14.22

[0087] As shown in Table 2, the artificial wetland fillers prepared in Examples 1-3 have a high BOD5 and COD Cr , SS, NH3-N and TP removal efficiencies all showed high performance, without the need for additional nitrogen adsorbents or phosphorus adsorbents, indicating that Examples 1-3 may have produced artificial wetland filler composite materials with high-efficiency adsorption and catalytic degradation capabilities.

[0088] Comparative Examples 5-7 respectively used solutions prepared from single polymer solution components (L-serine methyl ester hydrochloride, L-alanine methyl ester hydrochloride, and L-methionine methyl ester hydrochloride) to treat slag. Compared with the examples, the removal efficiency was lower, indicating that the single-component solution may not provide sufficient adsorption and catalytic degradation capabilities, thereby affecting the treatment performance of the filler.

[0089] Comparative Example 8 used a polymer solution containing only 2-fluoroacrylate methyl ester for slag treatment, which showed that 2-fluoroacrylate methyl ester may not have the ability of adsorption and catalytic degradation when used alone, compared with Comparative Example 9. Comparative Examples 9-10 used N,N-dimethylformamide and deionized water for slag treatment, respectively, as a control, indicating that without the participation of the polymer solution, the treatment performance of the slag would be significantly reduced.

[0090] The adsorption capacity test was then conducted on the artificial wetland fillers prepared in Examples 1-3 and Comparative Examples 5-7.

[0091] Prepare 100 mg / L Pb 2+ The solution was used as a simulated pollutant solution. The fillers prepared in Examples 1-3 and Comparative Examples 5-7 of the same mass (10 g) were taken and placed in a series of beakers, respectively. An equal amount (100 mL) of the simulated pollutant solution was added to each beaker to ensure that the fillers were completely immersed. The beakers were shaken at a speed of 150 rpm at 25°C for 24 hours. The supernatant was taken to measure the residual pollutant concentration and the adsorption capacity was calculated. The adsorption capacity (Q) = (C0-C) × V / m, where C0 is the initial pollutant concentration (mg / L), C is the residual pollutant concentration (mg / L), V is the solution volume (L), and m is the filler mass (g). The results are shown in Table 3:

[0092] Table 3. Adsorption capacity of Examples 1-3 and Comparative Examples 5-7 (unit: mg / g)

[0093] serial number Adsorption capacity Q Example 1 8.98 Example 2 9.13 Example 3 9.22 Comparative Example 5 6.43 Comparative Example 6 6.58 Comparative Example 7 6.32

[0094] As shown in Table 3, the artificial wetland fillers prepared in Examples 1-3 have a significant effect on Pb 2+ The comparative examples 5-7 have good adsorption capacity. Due to the different polymer solutions immersed in them, the adsorption performance of the final fillers is different from that of the examples 1-3.

[0095] In summary, the artificial wetland fillers prepared in Examples 1-3 exhibited higher treatment performance and higher adsorption capacity, which may be because the complex composition of the polymer solution and the addition of pretreated slag together provided efficient adsorption and catalytic degradation capabilities.

[0096] In the description of the specification, the description with reference to the terms "preparation example", "embodiment", "various embodiments" and the like means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or preparation example are included in at least one embodiment or preparation example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or preparation example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or preparation examples in a suitable manner.

[0097] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A solid waste-based modular artificial wetland filler, characterized in that: The raw materials include the following by weight: 30-60 parts of core-shell slag particles, 10-20 parts of sludge, and 1-8 parts of binder; The core-shell slag particles are prepared by the following steps: S1, collecting slag, washing it with water, removing iron, then acid washing it, neutralizing it to a pH value of 6-7, and crushing it to obtain pre-treated slag; S2, immersing the pretreated slag in a polymer solution, ultrasonically treating for 10-30 min, filtering and washing, and heat treating for 2-4 h to obtain core-shell slag particles; Wherein, the polymer solution in step S2 is prepared by the following steps: A1. Add amino acid methyl ester and methyl 2-fluoroacrylate to N,N-dimethylformamide, add 4-dimethylaminopyridine and tetrabutyl titanate under a nitrogen atmosphere, control the reaction temperature, and continue stirring the reaction to obtain a prepolymer solution; A2. Pour the prepolymer solution into methanol, add dicyclohexylcarbodiimide, heat up and stir rapidly to react, let stand and precipitate after the reaction, filter and wash, put into a vacuum oven, dry at 60-70°C to constant weight, and then use N,N-dimethylformamide as solvent to prepare a 20-30% polymer solution; The binder includes one or more of silicate cement, gypsum or water glass; In step A1, the mass ratio of amino acid methyl ester, methyl 2-fluoroacrylate, N,N-dimethylformamide, 4-dimethylaminopyridine and tetrabutyl titanate is (10-15): (9-17): 20: (0.02-0.03): (0.5-0.7), and the amino acid methyl ester includes one of L-serine methyl ester hydrochloride, L-alanine methyl ester hydrochloride and L-methionine methyl ester hydrochloride; In step A2, the mass ratio of the prepolymer solution, methanol and dicyclohexylcarbodiimide is (10-12):20:(0.2-0.6).

2. The solid waste-based modular artificial wetland filler according to claim 1, characterized in that: The power of the ultrasonic treatment in step S2 is 100-200 W, and the frequency of the ultrasonic treatment is 40-50 KHz.

3. The solid waste-based modular artificial wetland filler according to claim 1, characterized in that: The temperature of the heat treatment in step S2 is 50-60°C.

4. The solid waste-based modular constructed wetland filler according to claim 1, characterized in that: In step A1, the reaction temperature is 40-45° C., the stirring speed is 100-200 rpm, and the reaction time is 1-3 h.

5. The solid waste-based modular artificial wetland filler according to claim 1, characterized in that: In step A2, the reaction temperature is 60-70° C., the stirring speed is 300-400 rpm, and the reaction time is 20-40 min.