Forging forming method for high-rib branch type die forgings
Through the matching design of the pre-forging die and the final forging die, the height-to-width ratio of the high-strength branch die forging blanks is gradually adjusted, which solves the problems of forging difficulty and low material utilization caused by the height-to-width ratio, and realizes the high-strength branch Y High qualification rate and high production efficiency of die forgings.
Patent Information
- Application Number
- CN202410899534.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-10-08
AI Technical Summary
During the forging process, high-strength branch die forgings are difficult to produce due to their high-to-width ratio, and the material utilization rate is low. They are prone to uneven structures and folding, resulting in low qualification rates and low production efficiency.
The matching design of the pre-forging mold and the final forging mold is adopted, and the aspect ratio of the blank is gradually adjusted through the pre-forging and final forging processes to ensure that the blank can be completely placed into the cavity, reducing the manufacturing difficulty and improving material utilization. Specific steps include forming a blank on a free forging hammer, placing it in a heating furnace for heating, then transferring it to a pre-forging die for pre-forging, and then transferring it to a final forging die for final forging, using water-based graphite emulsion lubrication and slow pressing technology.
It effectively reduces the difficulty of making blanks, improves the qualification rate and production efficiency of forgings, avoids uneven tissue and folding phenomena, and improves material utilization and product quality.
Smart Images

Figure CN118744218A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of structural part forging, and in particular relates to a forging method for high-rib branch-type die forgings. Background Art
[0002] The fuselage structural parts of my country's aviation aircraft usually include frames, beams, ribs, slide rails, etc., and often have structural features such as high ribs, webs, ribs, and branches. This type of die forgings has a complex structure, complex production steps, great difficulty in operation, difficult die forging, and a low pass rate.
[0003] In actual die forging production, for high-rib branch-type forgings with a height-to-width ratio ≥ 3, since the ribs of the forgings are narrow and high, it is difficult to fill the top of the ribs. In the process of making the rough forgings of this type, if the rough rib width is less than the rib width of the forging, in order to ensure that the forging rib blank is sufficient to meet the die forging forming, the rough rib height must be greater than the rib height, resulting in the rough rib height-to-width ratio being far greater than 3. In order to ensure the rough size, it is necessary to repeatedly stretch. Since stretching is performed by successively feeding and repeatedly rotating the blank for compression deformation, it is a forging process that consumes the most man-hours in forging production. Especially in the later stage of drawing, as the width of the blank decreases, the temperature drop rate increases, the deformation resistance increases, and the plasticity decreases, forging cracks are very likely to occur, and it is necessary to reheat and continue to draw. Aviation structural parts are mostly titanium alloy forgings. Titanium alloys are sensitive to forging temperatures. Repeated heating and drawing can easily cause overheating of the center of the blank, resulting in uneven organization, etc., and in the actual die forging process, excessive aspect ratio may cause concave in the middle of the rib, billet deviation, etc. Further forging will cause folding, increase the workload of subsequent grinding, and in severe cases, lead to scrapping of the forging.
[0004] If the blank rib width is greater than the forging rib width, the blank rib height is less than the forging rib height, and the blank rib aspect ratio is less than 3, the blank width is too wide during die forging, resulting in the blank not being able to be completely placed in the die cavity. The blank part that exceeds the cavity is placed at the die bridge. During die forging, the blank at the bridge is split off, forming burrs, and cannot be used to fill the forging. This solution requires the blank volume to be much larger than the forging volume, and the material utilization rate is low. In addition, the blank that exceeds the cavity width is very likely to fold during die forging, which poses a great threat to the quality of the forging. Summary of the invention
[0005] Purpose of the invention: To provide a forging method for high-rib branch-like die forgings, so as to improve the qualified rate and production efficiency of high-rib branch-like die forgings.
[0006] Technical solution:
[0007] A forging method for a high-rib branch-type die forging, comprising:
[0008] Step 1: Forging a blank on a free forging hammer or a free forging press, wherein the cross section of the blank at the branch is rectangular;
[0009] Step 2: placing the blank into a heating furnace for heating and heat preservation for a certain period of time, and quickly transferring the blank to a pre-forging die after it is taken out of the furnace, and forging the blank into the cavity along the die tapping slope of the pre-forging die to obtain a pre-forged part, wherein the cross-section of the branches of the pre-forging die is a trapezoid, wherein the cross-sectional area s2 of the blank at the high ribs is equal to 1.1 to 1.5 times the cross-sectional area s1 of the pre-forging die at the high ribs, the height h2 of the cross-sectional area at the high ribs of the blank is less than the height h1 of the cross-sectional area at the high ribs of the pre-forging die, the width b2 of the cross-sectional area at the high ribs of the blank is less than the width b2 of the cross-sectional area at the high ribs of the pre-forging die, h2 / b2 is less than 3, and in the height direction, at least 1 / 3 of the blank height h2 can be placed in the pre-forging cavity;
[0010] Step three: Place the pre-forging in a heating furnace and heat it for a certain period of time. After it is taken out of the furnace, quickly transfer it to the final forging die, and forge it to finally obtain the final forging, wherein the cross-sectional area s1 at the high ribs of the pre-forging die is equal to 1.1 to 1.5 times the cross-sectional area s at the high ribs of the final forging die, the height h1 of the cross-sectional area at the high ribs of the pre-forging die is less than the height h of the cross-sectional area at the high ribs of the final forging die, the width b1 of the cross-sectional area at the high ribs of the pre-forging die is greater than the width b of the cross-sectional area at the high ribs of the final forging die, the draft angle of the final forging die is less than the draft angle of the pre-forging die, and in the height direction, at least 1 / 3 of the height h1 of the pre-forging can be placed in the final forging cavity.
[0011] Furthermore, in step one, the preheating temperature of the hammer anvil and the tool fixture is 200-300°C.
[0012] Furthermore, the draft angle of the final forging die is θ=1-3°, and the draft angle of the pre-forging die is θ1=5-10°.
[0013] Furthermore, the draft angle of the final forging die is θ=3-5°, and the draft angle of the pre-forging die is θ1=10-15°.
[0014] Furthermore, the draft angle of the final forging die is θ=5-7°, and the draft angle of the pre-forging die is θ1=15-20°.
[0015] Furthermore, the preheating temperature of the pre-forging die and the final forging is 250-350° C., and the die is lubricated with water-based graphite emulsion.
[0016] Furthermore, when using the counter-hammer forging, the equipment wind pressure is less than 0.6MPa.
[0017] Furthermore, when forging using a press machine, the pressing speed is less than 10 mm / s.
[0018] Beneficial effects:
[0019] By designing the pre-forging die and blank, the aspect ratio of the blank is effectively reduced, the difficulty of blank production is reduced, and it is ensured that the pre-forging can be completely placed in the final forging die cavity. The pre-forging die and the final forging die are well matched, which solves the problems of low material utilization, difficulty in blank production, uneven structure, forging folding, etc., and improves the forging qualification rate and production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 This is a schematic diagram of the cross section of the high rib of the final forging die;
[0021] Figure 2 It is a schematic diagram of the cross section of the high rib of the pre-forging die;
[0022] Figure 3 This is a schematic diagram of the cross section of the wild type high rib;
[0023] Figure 4 It is a schematic diagram of a wing joint forging of a certain type of aircraft in the embodiment. DETAILED DESCRIPTION
[0024] The present invention is a forging method for high-rib branch-like die forgings, which is mainly used for high-rib and branch-like difficult-to-form die forgings with an aspect ratio of ≥ 3. The method is targeted at high-rib branch-like forgings with an aspect ratio of ≥ 3, reduces the difficulty of making blanks by free forging under the existing technology, and effectively solves various quality problems generated during the die forging process, thereby improving the product qualification rate and production efficiency.
[0025] For high-ribbed branch-like forgings with an aspect ratio of ≥3, the corresponding final forging die is designed according to the die forging drawings provided by the customer, and then a pre-forging die is designed and its size is determined according to the size of the final forging die, and then the required blank size is finally determined according to the size requirements of the pre-forging die. The method can effectively reduce the aspect ratio of the blank and reduce the difficulty of blank production, wherein the height and width of the blank are determined according to the height and width of the pre-forging die. For high-ribbed branch-like forgings with an aspect ratio of ≥3, the above method is used for forging, which effectively avoids the central overheating and uneven structure caused by repeated forging of the blank, further avoids the occurrence of folding during the actual die forging process, reduces the workload of grinding, reduces the difficulty of forging, and improves production efficiency and product quality.
[0026] For a high-rib branch-type die forging with an aspect ratio greater than 3, a pre-forging die cavity is designed according to the cross-sectional structure of the die forging, including: a proportional relationship between a cross-sectional area s1 at the high ribs of the pre-forging die and a cross-sectional area s at the high ribs of the final forging die; a proportional relationship between a height h1 and a width b1 of a cross-sectional area at the high ribs of the pre-forging die and a height h and a width b of a cross-sectional area at the high ribs of the final forging die; and a matching relationship between a draft angle θ1 of the pre-forging die and a draft angle θ of the final forging die.
[0027] like Figure 1 and Figure 2 The cavity size of the pre-forging die is calculated and determined based on the cavity size of the final forging die, where the cross-sectional area at the high ribs of the pre-forging die s1 = the cross-sectional area at the high ribs of the final forging die s×(1.1-1.5); the height h1 of the cross section at the high ribs of the pre-forging die < the height h of the cross section at the high ribs of the final forging die; the width b1 of the cross section at the high ribs of the pre-forging die > the width b of the cross section at the high ribs of the final forging die.
[0028] The draft angle of the final forging die is θ=1-3°, and the draft angle of the pre-forging die is θ1=5-10°;
[0029] The draft angle of the final forging die is θ=3-5°, and the draft angle of the pre-forging die is θ1=10-15°;
[0030] The draft angle of the final forging die is θ=5-7°, and the draft angle of the pre-forging die is θ1=15-20°;
[0031] In the height direction, at least 1 / 3 of the pre-forging height h1 can be placed in the final forging cavity.
[0032] The blank is placed in a heating furnace for heating and heat preservation for a certain period of time. After it comes out of the furnace, it is quickly transferred to the pre-forging die. The die forging hammer or press is slowly pressed down to slowly press the blank into the cavity along the die slope of the pre-forging die. The subsequent light tapping and slow pressing can effectively ensure that the blank flows into the cavity instead of forming a large amount of flash, and finally a pre-forged part is obtained. After cleaning the burrs and surface of the pre-forged part, final forging is carried out.
[0033] The pre-forgings are placed in a heating furnace and heated for a certain period of time. After being taken out of the furnace, they are quickly transferred to the final forging die. The die forging hammer or press is slowly pressed down to slowly press the pre-forgings into the cavity along the die slope of the final forging die. Subsequent light tapping and slow pressing can effectively ensure that the pre-forgings flow into the cavity instead of forming a large amount of flash, and finally obtain the final forgings.
[0034] According to the designed pre-forging die, a blank with a height-to-width ratio of less than 3 is designed: the proportional relationship between the cross-sectional area s2 at the high ribs of the blank and the cross-sectional area s1 at the high ribs of the pre-forging die; the matching relationship between the height h2 and width b2 of the cross-sectional area at the high ribs of the blank and the height h2 and width b2 of the cross-sectional area at the high ribs of the pre-forging die; the blank has no demoulding slope.
[0035] like Figure 2 and Figure 3 The size of the blank is calculated and determined based on the size of the pre-forging die: the cross-sectional area of the blank at the high ribs s2 = the cross-sectional area of the pre-forging die at the high ribs s1 × (1.1-1.5); the height h2 of the section at the high ribs of the blank < the height h1 of the cross-sectional area at the high ribs of the pre-forging die; the width b2 < the width b2 of the cross-sectional area at the high ribs of the pre-forging die, where h2 / b2 < 3; in the height direction, at least 1 / 3 of the blank height h2 can be placed in the pre-forging cavity.
[0036] Determine the appropriate blank and forge it on a free forging hammer or free forging press. The preheating temperature of the hammer anvil and tool fixture is 200-300℃. The preheating temperature of the pre-forging die and final forging is 250-350℃, and the die is lubricated with water-based graphite emulsion.
[0037] The materials of the pre-forging die and final forging die used above are both 5CrNiMo.
[0038] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution of the present invention will be further described below in conjunction with the accompanying drawings in the embodiments of the present invention.
[0039] The wing joint forging of a certain type of aircraft is made of Ti-6AL-4V and has a cross-shaped high-ribbed branch-like forging. See the schematic diagram of the forging for Figure 4 The length of the wings on both sides of the forging is L = 240mm, the width of the high rib cross-section of the final forging die is b = 18mm, the height is h = 65mm, the die draft angle is θ = 5°, the aspect ratio is 3.6, and the cross-sectional area is s = 1560㎡.
[0040] Step 1: Forge the blank on a 3T free forging hammer, heat it to 35℃ below the phase change point, and quickly transfer it to the hammer anvil after it comes out of the furnace. Forge the bar to the blank shape required by the process, where the cross-sectional width of the blank at the high rib of the wings is b2=38mm, the height is h2=60mm, the aspect ratio is 1.6, and the cross-sectional area is s2=2280㎡. Get a suitable blank, where the preheating temperature of the hammer anvil and tool fixture is 200-300℃.
[0041] Step 2: Pre-forging is performed on a 400KJ hammer, and glass lubricant is evenly sprayed on the surface of the blank before heating. The heating temperature is kept at 35°C below the phase change point. After being taken out of the furnace, it is quickly transferred to the pre-forging die. The first hammer is slowly pressed down to make the blank slowly fill the cavity along the die draft of the pre-forging die. Subsequently, 3-5 light hammers are struck, which can effectively ensure that the blank flows into the cavity instead of forming flash, so as to ensure that the pre-forging is completely filled. The cross-sectional width of the high rib of the pre-forging die is b1=18mm, the height is h1=58mm, the aspect ratio is 3.2, the cross-sectional area is s1=1915㎜2, and the die draft is θ1=15°; the preheating temperature of the pre-forging die is 250-350°C, and the die lubrication is water-based graphite emulsion.
[0042] Step 3: Final forging is performed on a 400KJ hammer. Glass lubricant is evenly sprayed on the surface of the pre-forged part before heating. The heating temperature is kept at 35°C below the phase change point. After being taken out of the furnace, it is quickly transferred to the final forging die. The first hammer is slowly pressed down to allow the pre-forged part to slowly fill the cavity along the die draft of the final forging die. Subsequently, 4-6 hammers are lightly struck to effectively ensure that the pre-forged part flows into the cavity instead of forming flash, thereby ensuring that the final forging part is completely filled. The cross-sectional width of the high rib of the final forging die is b=18mm, the height is h=65mm, the aspect ratio is 3.6, the cross-sectional area is s=1540㎜2, and the die draft θ=5°; the preheating temperature of the final forging die is 250-350°C, and the die lubrication is water-based graphite emulsion.
[0043] The mold materials used above are all 5CrNiMo.
Claims
1. A forging method for high-rib branch-type die forgings, characterized in that: include: Step 1: Forging a blank on a free forging hammer or a free forging press, wherein the cross section of the blank at the branch is rectangular; Step 2: placing the blank into a heating furnace for heating and heat preservation for a certain period of time, and quickly transferring the blank to a pre-forging die after it is taken out of the furnace, and forging the blank into the cavity along the die tapping slope of the pre-forging die to obtain a pre-forged part, wherein the cross-section of the branches of the pre-forging die is a trapezoid, wherein the cross-sectional area s2 of the blank at the high ribs is equal to 1.1 to 1.5 times the cross-sectional area s1 of the pre-forging die at the high ribs, the height h2 of the cross-sectional area at the high ribs of the blank is less than the height h1 of the cross-sectional area at the high ribs of the pre-forging die, the width b2 of the cross-sectional area at the high ribs of the blank is less than the width b2 of the cross-sectional area at the high ribs of the pre-forging die, h2 / b2 is less than 3, and in the height direction, at least 1 / 3 of the blank height h2 can be placed in the pre-forging cavity; Step three: Place the pre-forging in a heating furnace and heat it for a certain period of time. After it is taken out of the furnace, quickly transfer it to the final forging die, and forge it to finally obtain the final forging, wherein the cross-sectional area s1 at the high ribs of the pre-forging die is equal to 1.1 to 1.5 times the cross-sectional area s at the high ribs of the final forging die, the height h1 of the cross-sectional area at the high ribs of the pre-forging die is less than the height h of the cross-sectional area at the high ribs of the final forging die, the width b1 of the cross-sectional area at the high ribs of the pre-forging die is greater than the width b of the cross-sectional area at the high ribs of the final forging die, the draft angle of the final forging die is less than the draft angle of the pre-forging die, and in the height direction, at least 1 / 3 of the height h1 of the pre-forging can be placed in the final forging cavity.
2. The method according to claim 1, characterized in that: In step 1, the preheating temperature of the hammer, anvil and tool fixture is 200-300℃.
3. The method according to claim 1, characterized in that The draft angle of the final forging die is θ=1-3°, and the draft angle of the pre-forging die is θ1=5-10°.
4. The method according to claim 1, characterized in that: The draft angle of the final forging die is θ=3-5°, and the draft angle of the pre-forging die is θ1=10-15°.
5. The method according to claim 4, characterized in that The draft angle of the final forging die is θ=5-7°, and the draft angle of the pre-forging die is θ1=15-20°.
6. The method according to claim 1, characterized in that The preheating temperature of the pre-forging die and final forging is 250-350℃, and the die is lubricated with water-based graphite emulsion.
7. The method according to claim 1, characterized in that When using counter-hammer forging, the equipment wind pressure is less than 0.6MPa.
8. The method according to claim 1, characterized in that When using a press for forging, the pressing speed is less than 10mm / s.
Citation Information
Patent Citations
Forging method for crossed-shaped die forging
CN107159831A
Die forging method for high-temperature alloy finish-forged blades
CN109365731A
Forging method of high-boss TC18 titanium alloy die forging
CN114160732A
Forming method of special-shaped titanium alloy die forging with shape distributed in vertical plane
CN115846555A
Aircraft landing gear die forging manufacturing method