Preparation method of release material with air guide groove

The air guide groove is formed through pre-curing and secondary curing of the UV cured layer, and the release layer is coated after complete curing, which solves the delamination and curling problems caused by different polarities and high-temperature curing in the existing technology, and achieves The stable shaping of the air guide groove and the product quality improvement of the release profile.

CN118745262APending Publication Date: 2024-10-08KANGWATER NEW MATERIALS (SUZHOU) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410766642.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-14
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

The existing textured exhaust release profile process has delamination problems caused by different polarities and shrinkage of the PE coating caused by high-temperature curing, which makes it difficult to release the internal stress of the release material and cause curling problems.

Method used

The air guide groove is formed by pre-curing and secondary curing of the UV cured layer, and a release layer is applied after complete curing, and the air guide groove is formed by a pressure roller to ensure rapid molding of the air guide groove and reduce deformation.

Benefits of technology

It effectively prevents delamination and curling of the release profile, improves product quality, and achieves stable shaping of the air guide groove.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118745262A_ABST
    Figure CN118745262A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of a release material with an air guide groove, and the preparation method of the release material comprises the following steps: pre-curing a UV curing layer, forming the air guide groove on the UV curing layer, and then completely curing the UV curing layer and coating the release layer, so that the rapid molding of the air guide groove on the UV curing layer can be ensured by adopting the mode; and the UV curing layer is pre-cured firstly, so that the deformation amount of the UV curing layer is small, the situation that the release material is layered or curled can be effectively prevented, and the product quality of the release material can be effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of release materials, and in particular to a method for preparing a release material with air guide grooves. Background Art

[0002] Electronic tape is a special-purpose tape, mainly used for packaging, fixing and insulation of electronic components. It plays an important role in the electronics industry and is often used in the manufacturing, maintenance and assembly of electronic equipment. Electronic tape is a tape specially designed for the electronics field, with a variety of special properties to meet the special needs of electronic components in the manufacturing, assembly and maintenance process. Electronic tape usually has the characteristics of insulation, high temperature resistance, chemical resistance, stickiness, easy tearing, anti-static properties, etc. As an electronic tape, it is mainly composed of substrate, adhesive, and release material. As an important component of the tape, the release material plays the role of isolation, protection, and shaping on the surface of the adhesive layer of the tape. The surface of the release material has a smooth surface, a textured exhaust surface, and a concave and convex rough surface due to different uses. The textured exhaust profile can form various concave and convex shapes on the surface of the functional tape adhesive layer, and has conductive air grooves. When the functional tape is attached to the object, the air between the adhesive layer and the object can be quickly exhausted through the air guide grooves, so that the adhesive layer and the object are closely attached, thereby achieving a better bonding and fixing effect.

[0003] Conventional textured exhaust release profiles on the market are generally made by pouring PE onto the surface of release base paper or PET film through melt casting, and then transferring the pattern through a steel rod engraved with patterns by hot pressing to form a permanent texture on the PE coating surface, and then coating the textured surface with silicon to form a textured release profile. This method has a simple process and is easy to achieve the texture, but there are unstable factors. For example, due to the different polarities, stratification problems are prone to occur between the PE coating and the base paper or PET film; since the curing temperature of silicone oil is generally 150~180℃, and the conventional PE temperature resistance is 80℃, when silicone is applied, the high temperature PE coating shrinks, making it difficult to release the internal stress of the release material, resulting in curling problems. Summary of the invention

[0004] The technical problem to be solved by the present invention is to provide a method for preparing a release profile which is simple in implementation, easy to realize air guide grooves in the release profile, and can effectively ensure the quality of the release layer product.

[0005] In order to solve the above-mentioned technical problems, the present invention adopts the following technical scheme: a method for preparing a release material with an air guide groove, characterized in that it comprises the following steps: 1) providing a substrate layer, coating a UV curing layer on the substrate layer, and pre-curing the UV curing layer, with a curing rate of 20-80%; 2) rolling the surface of the pre-cured UV curing layer with a pressure roller to form air guide grooves on the surface of the UV curing layer; 3) further curing the UV curing layer to cure the UV curing layer into shape; 4) coating a release layer on the cured UV curing layer.

[0006] Preferably, the curing rate of the UV curing layer pre-curing in step 1) is 40-60%.

[0007] Preferably, the UV curing layer is composed of UV curing resin A, UV curing resin B, fumed silica, a photoinitiator, an inhibitor, and a leveling agent.

[0008] Preferably, the UV curable resin A comprises 50-90 parts by weight of UV curable resin, 5-15 parts by weight of 1,4-butanediol acrylate, and 5-10 parts by weight of isobornyl acrylate; and the UV curable resin B is a UV curable epoxy acrylate resin.

[0009] Preferably, the photoinitiator is 1-hydroxycyclohexyl phenyl ketone, 2-hydroxy-methylphenylpropane-1-one, 2,4,6-trimethylbenzoyldiphenylphosphine oxide, ethyl 4-(N,N-dimethylamino)benzoate, benzophenone, 2-methyl-1-(4-methylthiophenyl)-2-morpholinyl-1-propanone, preferably one or more of 1-hydroxycyclohexyl phenyl ketone and 2,4,6-trimethylbenzoyldiphenylphosphine oxide.

[0010] Preferably, the substrate layer is paper, PET film, PC film or PI film.

[0011] Preferably, the thickness of the substrate layer is 12 μm to 500 μm.

[0012] Preferably, the UV curing layer is applied by blade coating, roller coating, gravure coating, micro-concave coating, slot extrusion coating, spray coating or die coating.

[0013] Preferably, the air guide groove is a brushed air guide groove or a concave-convex air guide groove.

[0014] Preferably, the release layer is a mixture of organic silicone oil and organic silicone adhesive.

[0015] The above technical scheme has the following beneficial effects: the method for preparing the release profile first pre-cures the UV-curing layer and forms air guide grooves on the UV-curing layer, and then completely cures the UV-curing layer and coats the release layer. This method can ensure the rapid molding of the air guide grooves on the UV-curing layer, and because the UV-curing layer is pre-cured first, the deformation of the UV-curing layer is small, which can effectively prevent the release profile from being delaminated or curled, and can effectively improve the product quality of the release profile. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 is a flow chart of an embodiment of the present invention.

[0017] Figure 2 It is a schematic structural diagram of the first embodiment of the release profile of the present invention.

[0018] Figure 3 It is a schematic structural diagram of a second embodiment of a release profile of the present invention.

[0019] Original part number description: 1. Base material layer; 2. UV curing layer; 3. Release layer. DETAILED DESCRIPTION

[0020] The following is an explanation of the disclosed embodiments of the present invention through specific embodiments. Those skilled in the art can understand the advantages and effects of the present invention from the contents disclosed in this specification. The present invention can be implemented or applied through other different specific embodiments, and the details in this specification can also be modified and changed in various ways based on different viewpoints and applications without departing from the concept of the present invention. In addition, the drawings of the present invention are only simple schematic illustrations and are not depicted according to actual dimensions. It is stated in advance. The following embodiments will further explain the relevant technical contents of the present invention in detail, but the disclosed contents are not intended to limit the scope of protection of the present invention.

[0021] like Figure 1 , 2 As shown, the present invention discloses a method for preparing a release profile with an air guide groove, which comprises the following steps: 1) Provide a substrate layer 1, coat a UV curing layer 2 on the substrate layer 1, and pre-cure the UV curing layer 2. The curing rate of the pre-cure is usually 20-80%. As a preferred method, the curing rate can be set to 40-60%. Too high or too low a curing rate may result in poor shaping effect of the air guide groove; 2) The surface of the pre-cured UV curing layer 2 is rolled with a pressure roller to form air guide grooves on the surface of the UV curing layer.

[0022] 3) The UV curing layer is then cured for a secondary cure, so that the UV curing layer is cured and formed, and a permanent air guide groove is formed in the UV curing layer. The air guide groove may be a wire drawing air guide groove or a concave-convex air guide groove; 4) A release layer 3 is coated on the cured UV-cured layer. Different release agent models and formulations can be selected according to the actual release force and silicon transfer requirements. The release layer is coated on the surface of the UV-cured layer by coating, and then cured by a heat curing oven or UV curing.

[0023] As a preferred embodiment of the present invention, the UV curing layer is composed of UV curing resin A, UV curing resin B, fumed silica, photoinitiator, inhibitor, and leveling agent. The UV curing resin A includes 50-90 parts by mass of UV curing resin, 5-15 parts by mass of 1,4-butanediol acrylate, and 5-10 parts by mass of isobornyl acrylate; the UV curing resin B is a UV curing epoxy acrylic resin. The photoinitiator is 1-hydroxycyclohexyl phenyl ketone, 2-hydroxy-methylphenylpropane-1-one, 2,4,6-trimethylbenzoyldiphenylphosphine oxide, 4-(N,N-dimethylamino) ethyl benzoate, benzophenone, 2-methyl-1-(4-methylthiophenyl)-2-morpholinyl-1-propanone, preferably one or more of 1-hydroxycyclohexyl phenyl ketone and 2,4,6-trimethylbenzoyldiphenylphosphine oxide.

[0024] The substrate layer 1 may be paper, PET film, PC film or PI film, and the thickness of the substrate layer 1 is 12 μm to 500 μm. The UV curing layer may be coated on the substrate layer 1 by blade coating, roller coating, gravure coating, micro-concave coating, slot extrusion coating, spray coating or die coating.

[0025] The pre-curing and secondary curing in the preparation method can adopt various curing forms such as thermal curing, UV curing, and radiation curing. The two curings can adopt the same curing process or different curing processes. The formation process of the air guide groove in the preparation method can adopt a single shape of air guide groove or a composite air guide groove of various forms according to different air guide groove design schemes to meet different application requirements. For example, the air guide groove can use a secondary shaping roller to form a regular concave and convex shape of the brushed air guide groove on the surface of the UV curing layer 2; or use a roller engraved with various concave or convex shapes and roll it on the UV curing layer 2 to make the UV curing layer 2 have corresponding convex or concave air guide grooves.

[0026] The release layer 3 is mainly a mixture of silicone oil and silicone adhesive, in which silicone oil is the main component, which plays an internal support role in the release layer to prevent collapse and deformation after coating. The silicone adhesive plays an auxiliary role, increasing the structural elasticity and strength of the release layer, and preventing the problem of cracks and powdering due to insufficient internal elasticity of the release layer caused by the increase in the thickness of the release material. Release layer formula: silicone oil, curing agent, anchoring agent, catalyst, etc., mainly provided by Dow Corning, Wacker, Shin-Etsu, etc. According to the different requirements of release force and silicon transfer rate, different raw material models and components are selected for adjustment to meet specific needs.

[0027] like Figure 3 As shown, another embodiment of the release material of the present invention is shown. In this embodiment, a UV curing layer 2 and a release layer 3 can be respectively provided on both sides of the substrate layer 1. The preparation method thereof is the same as that of the above-mentioned single-sided profile.

[0028] The method for preparing a release profile first pre-cures the UV curing layer and forms air guide grooves on the UV curing layer, and then completely cures the UV curing layer and coats the release layer. This method can ensure the rapid molding of the air guide grooves on the UV curing layer, and because the UV curing layer is pre-cured first, the deformation of the UV curing layer is small, which can effectively prevent the release profile from being delaminated or curled, and can effectively improve the product quality of the release profile.

[0029] The contents disclosed above are only preferred feasible embodiments of the present invention, and are not intended to limit the scope of the present invention. Therefore, all equivalent technical changes made using the contents of the present invention's specification and drawings are included in the scope of the present invention.

Claims

1. A method for preparing a release profile with air guide grooves, characterized in that: It includes the following steps: Providing a substrate layer, coating a UV curing layer on the substrate layer, and pre-curing the UV curing layer with a curing rate of 20-80%; The surface of the pre-cured UV curing layer is rolled by a pressure roller to form air guide grooves on the surface of the UV curing layer; The UV curing layer is then cured for a secondary cure to cure the UV curing layer into a shape; A release layer is applied on the cured UV-cured layer.

2. The method for preparing a release profile with air guide grooves according to claim 1, characterized in that: The curing rate of the UV curing layer pre-curing in step 1) is 40-60%.

3. The method for preparing a release profile with air guide grooves according to claim 1, characterized in that: The UV curing layer consists of UV curing resin A, UV curing resin B, gas phase silica, photoinitiator, inhibitor and leveling agent.

4. The method for preparing a release profile with air guide grooves according to claim 3, characterized in that: The UV curable resin A comprises 50-90 parts by weight of UV curable resin, 5-15 parts by weight of 1,4-butanediol acrylate, and 5-10 parts by weight of isobornyl acrylate; the UV curable resin B is a UV curable epoxy acrylate resin.

5. The method for preparing a release profile with air guide grooves according to claim 3, characterized in that: The photoinitiator is 1-hydroxycyclohexyl phenyl ketone, 2-hydroxy-methylphenyl propane-1-one, 2,4,6-trimethylbenzoyl diphenyl phosphine oxide, ethyl 4-(N,N-dimethylamino)benzoate, benzophenone, 2-methyl-1-(4-methylthiophenyl)-2-morpholinyl-1-propanone, preferably one or more of 1-hydroxycyclohexyl phenyl ketone and 2,4,6-trimethylbenzoyl diphenyl phosphine oxide.

6. The method for preparing a release profile with air guide grooves according to claim 1, characterized in that: The substrate layer is paper, PET film, PC film or PI film.

7. The method for preparing a release profile with air guide grooves according to claim 6, characterized in that: The thickness of the substrate layer is 12 μm to 500 μm.

8. The method for preparing a release profile with air guide grooves according to claim 1, characterized in that: The UV curing layer is coated by blade coating, roller coating, gravure coating, micro-concave coating, slit extrusion coating, spray coating or die coating.

9. The method for preparing a release profile with air guide grooves according to claim 1, characterized in that: The air guide groove is a wire drawing air guide groove or a concave-convex air guide groove.

10. The method for preparing a release profile with air guide grooves according to claim 1, characterized in that: The release layer is a mixture of organic silicone oil and organic silicone adhesive.