Production process of bonded neodymium iron boron assembly
By subjecting the NdFeB magnetic ring and the ring-shaped iron parts to constant-temperature heating and hot assembly, they are then immersed in the adhesive and subjected to vacuum treatment, which solves the problem of low bonding efficiency and low bonding efficiency between NdFeB magnets and ring-shaped iron parts in the existing technology. The problem of high cost is achieved, and a more efficient and stronger bonded connection and a simpler production process are achieved.
Patent Information
- Application Number
- CN202410858564.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-10-08
AI Technical Summary
The existing bonding process between NdFeB magnets and ring-shaped iron parts has low efficiency and high cost. Conventional methods have problems such as uneven glue application, glue overflow, and low coordination efficiency among multiple people.
The NdFeB magnetic ring and the ring-shaped iron parts are heated at a constant temperature, hot assembled, and the assembled components are completely immersed in the adhesive, vacuumed and constant pressure treated, followed by cleaning and drying, and finally Sampling inspection of dimensions and pressure-off force enables bonded connections without manual glue application.
It improves work efficiency, enhances bonding strength and adequacy, reduces cleaning difficulty and production costs, simplifies the assembly process, and improves production efficiency.
Smart Images

Figure CN118748121A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a production process of a bonded NdFeB component, belonging to the technical field of NdFeB magnet production. Background Art
[0002] In the prior art, an annular iron piece usually needs to be fixed on the outer ring of the annular NdFeB magnet to protect and isolate the magnet, and to facilitate the installation of the NdFeB magnet. As market demand and output increase, conventional production requires the NdFeB magnet and the annular iron piece to be bonded together with glue, which requires processes such as gluing, assembling, and wiping. Three people work on the assembly line, and the product gluing efficiency is slow, the work efficiency is low, and the gluing cost is high, which makes it uncompetitive in the market.
[0003] There are two conventional solutions: 1. Use a clearance fit, brush glue on the iron sleeve or magnet, and bake to cure; 2. Use an interference fit, brush glue on the magnet, heat-install and press it in, and then bake to cure. The first solution has the following problems: It is difficult to evaluate how much to brush when brushing glue. Sometimes, when the brush is not full or the gap between the magnet and the iron sleeve is large, the adhesion and release force cannot meet the requirements. If too much glue is brushed, it will overflow outside, causing waste and is difficult to clean. The second solution has the following problems: Due to the small interference fit clearance, a large amount of glue will overflow during the press-in process between the magnet and the iron sleeve. If the assembly is not correct, there will be glue on one side and no glue on the other side. Moreover, it requires multiple people to complete, which is very inefficient. Summary of the invention
[0004] The present invention aims to provide a production process for bonded NdFeB components, which solves the problems of low production efficiency and high production cost in the prior art.
[0005] The above technical purpose of the present invention is mainly solved by the following technical solution: A production process of a bonded NdFeB component, including a NdFeB magnetic ring and an annular iron piece sleeved on the outer wall of the NdFeB magnetic ring, comprising the following steps: S1. Heating the NdFeB magnetic ring at a constant temperature and maintaining it for a certain period of time; S2, hot-fitting and assembling the NdFeB magnetic ring and the annular iron piece to form a NdFeB assembly; S3, completely immersing the NdFeB assembly assembled in step S2 into the binder; S4, evacuate the NdFeB component immersed in the binder and maintain constant pressure; S5, taking out the NdFeB component impregnated in step S4 and cleaning it with a cleaning solution; S6, heating and drying the NdFeB component cleaned in step S5; S7, performing random inspection on the size standard and the compression-release force of the NdFeB components dried in step S6; The above method is used to bond and fix the NdFeB magnetic ring and the annular iron part, without the need for manual glue application, thus reducing manpower requirements and improving work efficiency. The glue is more sufficient and has higher strength, which reduces the difficulty of cleaning and makes assembly easier, thus reducing production costs and improving production efficiency.
[0006] Preferably, the inner wall of the annular iron piece abuts against the outer wall of the NdFeB magnetic ring, and the axial width of the annular iron piece is greater than or equal to the axial width of the NdFeB magnetic ring; the inner wall of the annular iron piece abuts against the outer wall of the NdFeB magnetic ring, so that the annular iron piece and the NdFeB magnetic ring are more tightly connected, and the axial width of the annular iron piece is greater than or equal to the axial width of the NdFeB magnetic ring, so that after the annular iron piece and the NdFeB magnetic ring are assembled, the NdFeB magnetic ring can be protected by the annular iron piece, and the external magnetic field can be isolated by the annular iron piece to avoid affecting the NdFeB magnetic ring, and the subsequent installation of the NdFeB magnetic ring is more convenient through the annular iron piece.
[0007] Preferably, the heating temperature of the NdFeB magnetic ring in step S1 is 200±50°C; the heating temperature of the above-mentioned NdFeB magnetic ring is 200±50°C, so that the NdFeB magnetic ring can be better thermally matched with the annular iron part within this temperature range, while avoiding the influence of temperatures outside the range on the magnetic field of the NdFeB magnetic ring.
[0008] Preferably, the heating time of the NdFeB magnetic ring in step S1 is 15-30mi; the heating time of the above-mentioned NdFeB magnetic ring is 15-30mi, so that the NdFeB magnetic ring can be heated to and maintained in a specified temperature range, ensuring that the NdFeB magnetic ring is heated in place and the quality of thermal matching is guaranteed.
[0009] Preferably, in step S4, the environment in which the NdFeB component immersed in the adhesive is located is maintained at a constant pressure of -0.5~0MPa; the environment in which the NdFeB component is located is maintained at a constant pressure of -0.5~0MPa, so that the adhesive can penetrate more quickly and fully between the NdFeB magnetic ring and the annular iron part, thereby improving the bonding strength and bonding efficiency.
[0010] Preferably, in step S4, the environment in which the NdFeB components immersed in the adhesive are located is maintained at a constant pressure for 3-15 minutes; the environment in which the NdFeB components are located is maintained at a constant pressure for 3-15 minutes, so that the NdFeB components can be more fully and completely impregnated with adhesive, thereby ensuring the bonding strength between the NdFeB components.
[0011] Preferably, the cleaning liquid in step S5 is soapy water; the cleaning liquid being soapy water can ensure that the residual adhesive on the surface of the NdFeB component is cleaned, thereby improving the cleaning effect and reducing the cleaning cost.
[0012] Preferably, the inner side of the annular iron piece in contact with the outer wall of the NdFeB component is a rough surface; the rough surface on the inner side of the annular iron piece can increase the friction force when bonding with the NdFeB component, thereby improving the bonding strength.
[0013] Therefore, the present invention has the characteristics of no need for manual glue application, reducing manpower requirements, improving work efficiency, more sufficient glue, higher bonding strength and efficiency, reduced cleaning difficulty, improved production efficiency, easier assembly, and protection and magnetic isolation of NdFeB magnetic rings. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a process flow chart of the present invention.
[0015] Figure 2 It is a schematic structural diagram of the NdFeB magnetic ring and the annular iron piece after being assembled. DETAILED DESCRIPTION
[0016] The technical solution of the present invention is further specifically described below through embodiments and in conjunction with the accompanying drawings.
[0017] like Figure 1-2 As shown, a production process of a bonded NdFeB component includes a NdFeB magnetic ring 1 and an annular iron piece 2 sleeved on the outer wall of the NdFeB magnetic ring 1, including the following steps: S1. Heating the NdFeB magnetic ring at a constant temperature and maintaining it for a certain period of time; S2, hot-fitting and assembling the NdFeB magnetic ring and the annular iron piece to form a NdFeB assembly; S3, completely immersing the NdFeB assembly assembled in step S2 into the binder; S4, evacuate the NdFeB component immersed in the binder and maintain constant pressure; S5, taking out the NdFeB component impregnated in step S4 and cleaning it with a cleaning solution; S6, heating and drying the NdFeB component cleaned in step S5; S7, performing random inspections on the size standard and the compression-release force of the NdFeB components dried in step S6.
[0018] According to the size of NdFeB magnet ring and annular iron part, suitable shrink fit tooling is designed. Because the impregnation process is adopted, it is necessary to ensure that the size of the component is qualified before impregnation with adhesive. Interference fit needs to be selected. The NdFeB magnet ring is heated before fitting. Then the NdFeB component is soaked in the adhesive (glue solution), and the container where the adhesive and NdFeB component are located is evacuated and maintained for a certain period of time. The roughness such as scratches is made on the inner wall of the annular iron part. Under the same impregnation conditions, the higher the roughness of the annular iron part, the higher the pressure-release strength of the NdFeB component, but When the roughness is too high, it is easy to cause the NdFeB magnetic ring to crack and bend during the assembly process. After the NdFeB component is impregnated with glue, the adhesive remaining on the surface of the NdFeB component is cleaned with soapy water, and then the NdFeB component is dried. It can be heated and dried by air drying or resistance heat drying. Finally, the dried NdFeB components are sampled to detect the size standard and press-off force of the NdFeB components. The press-off force is the axial pressure applied to the NdFeB magnetic ring or the annular iron part to loosen the NdFeB magnetic ring and the annular iron part.
[0019] like Figure 1-2 As shown, the inner wall of the annular iron piece 2 abuts against the outer wall of the NdFeB magnetic ring 1, the axial width of the annular iron piece 2 is greater than or equal to the axial width of the NdFeB magnetic ring 1, the heating temperature of the NdFeB magnetic ring in step S1 is 200°C, the heating time of the NdFeB magnetic ring in step S1 is 20min, the environment of the NdFeB component immersed in the binder is maintained at a constant pressure of -0.1MPa in step S4, the environment of the NdFeB component immersed in the binder is maintained at a constant pressure of 5min in step S4, the cleaning liquid in step S5 is soapy water, and the inner side of the annular iron piece 2 in contact with the outer wall of the NdFeB component 1 is a rough surface.
[0020] The concentration and specification of the above-mentioned glue are selected according to customer needs, and different glue solutions are used to carry out compression strength and life tests, from which glue with high life and high compression strength is selected. The cleaning solution uses soapy water with low cost but good cleaning effect. The specific concentration of soapy water is adopted according to needs. The rough surface of the above-mentioned annular iron piece can be formed by using a processing tool to scratch the inner wall of the annular iron piece or to create other uneven surfaces to form a rough surface.
Claims
1. A process for producing a bonded NdFeB component, comprising a NdFeB magnetic ring (1) and an annular iron piece (2) sleeved on the outer wall of the NdFeB magnetic ring (1), characterized in that: The following steps are involved: S1. Heating the NdFeB magnetic ring at a constant temperature and maintaining it for a certain period of time; S2, hot-fitting and assembling the NdFeB magnetic ring and the annular iron piece to form a NdFeB assembly; S3, completely immersing the NdFeB assembly assembled in step S2 into the binder; S4, evacuate the NdFeB component immersed in the binder and maintain constant pressure; S5, taking out the NdFeB component impregnated in step S4 and cleaning it with a cleaning solution; S6, heating and drying the NdFeB component cleaned in step S5; S7, performing random inspections on the size standard and the compression-release force of the NdFeB components dried in step S6.
2. The process for producing bonded NdFeB components according to claim 1, characterized in that: The inner wall of the annular iron piece (2) abuts against the outer wall of the NdFeB magnetic ring (1); the axial width of the annular iron piece (2) is greater than or equal to the axial width of the NdFeB magnetic ring (1).
3. The process for producing bonded NdFeB components according to claim 1, characterized in that: The heating temperature of the NdFeB magnetic ring in step S1 is 200±50°C.
4. The process for producing bonded NdFeB components according to claim 1, characterized in that: The heating time of the NdFeB magnetic ring in step S1 is 15-30 minutes.
5. The process for producing bonded NdFeB components according to claim 1, characterized in that: In the step S4, the environment where the NdFeB component immersed in the binder is located is maintained at a constant pressure of -0.5~0MPa.
6. The process for producing bonded NdFeB components according to claim 1, characterized in that: In the step S4, the environment of the NdFeB component immersed in the binder is kept at a constant pressure for 3-15 minutes.
7. The process for producing bonded NdFeB components according to claim 1, characterized in that: The cleaning liquid in step S5 is soapy water.
8. The process for producing bonded NdFeB components according to claim 1, characterized in that: The inner side of the annular iron piece (2) which contacts the outer wall of the NdFeB component (1) is a rough surface.