Manufacturing method for improving structural compactness of composite material
By forming a wet buffer protective layer on the surface of composite parts and using vacuum curing technology, the problem of insufficient density of composite sandwich structures is solved, achieving efficient density improvement and cost reduction, and is suitable for large curvature or tubular structures. of composite materials manufacturing.
Patent Information
- Application Number
- CN202410994987.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-10-11
AI Technical Summary
The composite sandwich structure is prone to shrinkage in high-temperature environments, and the curing pressure is low, resulting in insufficient density. Existing methods increase the number of curing times or improve the properties of the core material, which will increase the cost and weight, and the lamination of large curvature or tubular structures It is susceptible to uneven pressure and difficult to manufacture.
Use a wet buffer protective layer, including a peelable protective layer, non-porous isolation film, dry glass cloth and epoxy resin, to form a liquid buffer layer in a vacuum environment to evenly disperse the curing pressure and avoid local pressure concentration. Use a vacuum bag for curing , simplify the process and reduce costs.
It improves the density and surface quality of composite parts, avoids pores and wrinkles, reduces the weight and manufacturing cost of the parts, and maintains the overall performance and load-bearing efficiency of the parts.
Smart Images

Figure CN118752803A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of composite material parts (assemblies) manufacturing, in particular to a manufacturing method for improving the structural density of a composite material. Background Art
[0002] Strong designability is a prominent feature of composite materials. Sandwich structures, large curvature or tubular structures and other parts (assemblies) that reflect the advantages of composite materials have been widely used in the fields of aviation and aerospace.
[0003] The composite sandwich structure is to set low-density or porous materials such as honeycomb core or foam core in the whole or part of the parts (assemblies) to increase structural rigidity, reduce product weight and improve load-bearing efficiency.
[0004] Porous materials such as honeycomb cores tend to shrink in high temperature environments and have poor pressure resistance. Therefore, the curing pressure of composite sandwich structures is significantly lower than that of laminated structures, generally less than 0.3Mpa. After curing, the density inside the parts is low, and defects such as pores and delamination are prone to occur. ("Manufacturing Process of Advanced Composite Materials", FC Campbell, first edition, Shanghai Jiaotong University Press, P212) Complex structures can improve the load-bearing efficiency of composite parts (assemblies) and have been widely used in aviation, aerospace and other fields.
[0005] In order to improve the density of composite sandwich structures, commonly used methods include multiple curing and improving the pressure bearing capacity of the core material. Multiple curing means that the core lower layer is first cured by co-bonding or secondary bonding, and then bonded to the honeycomb core (foam core) and the core upper layer, or the core lower and core upper layers are cured separately, and then bonded to the honeycomb core (foam core). When the core lower (core upper) layer is cured separately, the porosity content can be reduced by increasing the curing pressure. However, this method increases the number of curing times, prolongs the cumulative time of the parts (assemblies) in a high temperature environment, and may affect the overall performance of the parts. Improving the pressure bearing capacity means increasing the density of the core material, and then the curing pressure of the parts (assemblies) can be appropriately increased to reduce the porosity content. However, this method increases the weight of the parts (assemblies) and reduces the structural load-bearing efficiency.
[0006] Enhancing the density of composite material structures is an important part of improving the utilization rate of composite materials. In the prior art, the density is mainly improved by increasing the number of curing times or improving the performance of the core material. Increasing the number of curing times, such as "Composite Curing Process for Aircraft Tail Leading Edge" (CN115923198A), adopts a co-bonding process to first cure the lower core layer under high pressure, and then glue the core material and the upper core layer. Improving the performance of the core material means improving the compressive strength of the core material. Increasing the number of curing times will greatly increase the manufacturing cost, and the cumulative time of the raw materials in a high temperature environment will be extended, which may affect the overall performance. Increasing the compressive strength of the core material will increase the density of the material, increase the weight of the product, and decrease the load-bearing efficiency.
[0007] Large curvature or tubular conforming material structure, complex profile, uneven layer pressure, and wrinkles. The existing method is mainly to make a pressure pad to evenly disperse the curing pressure, such as "A flexible pressure pad for hot pressing parts with complex profiles" (CN105479778A). The pressure pad fits the profile of one side of the part (assembly), has many reinforcement layers, complex cross-sectional changes, and is difficult to manufacture. Pressure pads made of metal materials require CNC machining of the profile. Pressure pads made of non-metallic materials need to be manufactured using special molds, which are costly and time-consuming. Summary of the invention
[0008] In order to overcome the deficiencies of the prior art, the purpose of the present application is to provide a manufacturing method for improving the density of composite material structures, so as to improve the density of composite material parts (components), reduce internal porosity, and improve surface quality.
[0009] A manufacturing method for improving the density of a composite material structure, characterized by comprising the following contents: 1) laying a part blank on a tooling surface according to the composite material structure and vacuuming and compacting it; 2) laying a wet buffer protective layer comprising a peelable protective layer, a non-porous isolation film, dry glass cloth and epoxy resin on the surface of the part blank and vacuuming and compacting it; 3) making a vacuum bag, pressurizing the part blank and the wet buffer protective layer at a pressure of more than 0.35 MPa in a vacuum environment to cure; 4) separating the buffer protective layer from the part after curing.
[0010] The manufacturing method for improving the structural density of composite materials is characterized in that in the step 2), a peelable protective layer is laid on the surface of the part blank in sequence, vacuumed and compacted, a non-porous isolation film is laid, vacuumed and compacted, and then 1 to 3 layers of dry glass cloth are laid, and then epoxy resin is brushed on the dry glass cloth to fully infiltrate the dry glass cloth with the epoxy resin, forming a wet buffer protective layer on the wet surface of the part blank.
[0011] The manufacturing method for improving the structural density of the composite material is characterized in that in the step 2), when laying the dry glass cloth, the dry glass cloth can be spliced or cut, and a layer of dry glass cloth patch is partially covered above the splicing seam or cut, and the length and width of the patch exceed the splicing seam or cut by at least 10 mm on one side.
[0012] The manufacturing method for improving the structural density of composite materials is characterized in that after a wet buffer protective layer is formed on the wet surface of the part blank, it should be left to stand for at least 10 minutes, and then vacuumed and compacted until the epoxy resin surface is dry.
[0013] The manufacturing method for improving the density of composite material structure of the present invention adopts "wet molding" and "direct matching" strategies, using epoxy resin and dry glass cloth to form a liquid buffer layer on the surface of parts (components). Under vacuum pressure, the liquid buffer layer is closely attached to the surface of the parts (components) and gradually solidifies and molds. During solidification, the buffer layer bears pressure as a whole and evenly disperses the pressure to avoid local pressure concentration or pressure loss. For sandwich structures, the buffer layer can also limit the position as a whole to avoid the core material from shrinking or collapsing under pressure. The sandwich structure can be solidified under higher pressure to improve the internal density. The liquid buffer layer can evenly distribute the solidification pressure of large curvature or tubular structure, avoid wrinkles, and make the surface flat and smooth. Its advantages are as follows: 1) Simple. The buffer protective layer only uses a peelable protective layer, a non-porous isolation film, epoxy resin and dry glass cloth, does not rely on complex molds, and has low cost; 2) Does not affect performance. There is no increase in the number of tank fillings or material changes, and there is no effect on the comprehensive performance and load-bearing efficiency of parts (components). 3) Reliable. Under the action of vacuum, the buffer protection layer is wet-fitted with the parts (assemblies) to avoid secondary transfer of molds or fake parts, and achieve better matching.
[0014] The present application is further described in detail below in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 Schematic diagram of honeycomb sandwich structure
[0016] Figure 2 Schematic diagram of tubular beam structure
[0017] Explanation of numbers in the figure: 1-core lower layer, 2-honeycomb core, 3-core upper layer, 4-part blank, 5-peelable protective layer, 6-porous isolation film, 7-dry glass cloth, 8-tubular beam blank, 9-dry glass cloth patch, 10-tooling, 11 buffer protective layer. DETAILED DESCRIPTION
[0018] This method adopts the strategy of "direct matching" and "wet shaping" to directly make a wet buffer protection layer on the surface of the composite material component (assembly) blank, which improves the matching of the buffer protection layer and the component (assembly), and plays a role in uniformly conducting pressure and limiting position. The component (assembly) can be cured under high pressure environment, which improves the internal density.
[0019] Example 1, a method for improving the density of honeycomb sandwich panels.
[0020] This application takes honeycomb sandwich wall panels as an example to illustrate a method for improving the density of composite materials, including a tooling body, a peelable protective layer, a non-porous isolation film, dry glass cloth and epoxy resin, the peelable protective layer is laid on the surface of the part blank, the non-porous isolation film is placed on the peelable protective layer, the dry glass cloth is placed on the non-porous isolation film, and the epoxy resin is brushed on the dry glass cloth. The specific steps are as follows: 1) Laying a part blank 4 of a sandwich structure on the surface of the tooling 10, the part blank 4 includes a core lower layer 1, a honeycomb core 2 and a core upper layer 3 , after the part blank 4 is laid, it is vacuumed and compacted; 2) a peelable protective layer 5 is laid on the surface of the blank, and it is vacuumed and compacted; a non-porous isolation film 6 is placed on the peelable protective layer, and it is vacuumed and compacted; two layers of dry glass cloth 7 are laid on the non-porous isolation film; the prepared epoxy resin is brushed on the dry glass cloth 7, and it is allowed to stand for 30 minutes to form a wet buffer protective layer 11; 3) a vacuum bag is made outside the buffer protective layer 11, and it is vacuumed and compacted for 24 hours; 4) It is cured using a vacuum bag, and the curing pressure is 0.5Mpa.
[0021] Embodiment 2, a method for improving the density of tubular beam parts.
[0022] This application takes a tubular beam as an example to illustrate a method for improving the density of a composite material, including a main tooling 1, a peelable protective layer 5, a non-porous isolation film 6, a dry glass cloth 7 and an epoxy resin, wherein the peelable protective layer 5 is spread on the surface of a part blank 4, the non-porous isolation film 6 is placed on the peelable protective layer, the dry glass cloth 7 is placed on the non-porous isolation film, and the epoxy resin is brushed on the dry glass cloth 7. The specific steps are as follows: 1) laying the part blank 4 of the tubular beam on the surface of the tooling 10, and vacuuming and compacting it; 2) laying the peelable protective layer 5 on the surface of the blank, and vacuuming and compacting it; placing a non-porous isolation film on the peelable protective layer 6. Vacuum and compact; lay a whole layer of dry glass cloth 7 on the non-porous isolation film, splice the dry glass cloth in the R corner area, and locally lay a layer of dry glass cloth patch 9 above each joint. The length of the dry glass cloth patch 9 is 10mm larger than the single side of the joint below, and the width of the patch is 20mm larger than the single side of the joint below; brush the prepared epoxy resin on the dry glass cloth 7, let it stand for 20 minutes, and form a wet buffer protection layer 11; 3) Make a vacuum bag outside the buffer protection layer 11, vacuum and compact for 10 hours; 4) Use the vacuum bag to cure, and the curing pressure is 0.7Mpa.
Claims
1. A method for improving the structural density of a composite material, characterized in that The following contents are included: 1) Laying the part blank on the surface of the tooling according to the composite material structure and vacuuming and compacting it; 2) Laying a wet buffer protective layer consisting of a peelable protective layer, a non-porous isolation film, dry glass cloth and epoxy resin on the surface of the part blank and vacuuming and compacting it; 3) Making a vacuum bag, pressurizing the part blank and the wet buffer protective layer to more than 0.35Mpa in a vacuum environment to cure; 4) Separating the buffer protective layer from the part after curing.
2. The manufacturing method for improving the structural density of a composite material according to claim 1, characterized in that: In the step 2), a peelable protective layer is sequentially laid on the surface of the part blank, vacuumed and compacted, a non-porous isolation film is laid, vacuumed and compacted, and then 1 to 3 layers of dry glass cloth are laid, and then epoxy resin is brushed on the dry glass cloth to fully infiltrate the dry glass cloth, forming a wet buffer protective layer on the wet surface of the part blank.
3. The manufacturing method for improving the structural density of a composite material according to claim 1, characterized in that: In the step 2), when laying the dry glass cloth, the dry glass cloth can be spliced or cut, and a dry glass cloth patch is partially covered above the splicing seam or cut, and the length and width of the patch exceed the splicing seam or cut by at least 10 mm on one side.
4. The manufacturing method for improving the structural density of a composite material according to claim 2 or 3, characterized in that: After a wet buffer protective layer is formed on the wet surface of the part blank, it should be left to stand for at least 10 minutes before vacuuming and compacting until the epoxy resin surface is dry.
Citation Information
Patent Citations
Forming method capable of improving flatness of non-fitted forming surface of composite material part
CN108068357A
Manufacturing method of normal temperature cured high-temperature-resistant auxiliary tool material system suitable for autoclave molding process
CN108749028A