Hydrogen production electrolytic cell mastoid pole plate capable of rapidly replacing alkali liquor in high-temperature area

By designing multiple and spaced convex structures on the electrolytic water hydrogen production mastoid plate, a temperature control area at the outlet of the alkali solution is formed, which solves the local high temperature problem caused by the heat accumulation of the alkali solution, improves the electrolysis efficiency and safety, and achieves The flow rate of alkali solution is significantly improved.

CN118756181APending Publication Date: 2024-10-11QI DIAN DI TAN ZHI NENG ZHUANG BEI (ZHE JIANG) YOU XIAN GONG SI
View PDF 0 Cites 3 Cited by

Patent Information

Application Number
CN202411228861.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

In the existing electrolysis water hydrogen production technology, the heat accumulation of the alkali solution at the top of the electrolysis chamber leads to excessive local temperature, causing damage to the plates, diaphragms and electrodes, and may cause safety issues such as gas explosions.

Method used

Design a mastoid plate that forms alkali solution diffusion area and alkali solution outlet temperature control area by arranging multiple and spaced first protrusions and second protrusion structures at the alkali solution outlet. The third convex structure narrows the flow channel, promotes the rapid outflow of alkali liquid, and reduces local high temperatures.

Benefits of technology

It effectively reduces the backflow and backflow of alkali solution, improves the uniformity of temperature distribution, reduces the risk of damage to the plates and separators, improves electrolysis efficiency and safety, and the flow rate of alkali solution is 2-10 times that of the existing technology.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118756181A_ABST
    Figure CN118756181A_ABST
Patent Text Reader

Abstract

The invention discloses a hydrogen production electrolytic cell mastoid pole plate capable of rapidly replacing alkali liquor in a high-temperature area, which is applied to an electrolytic cell and comprises a mastoid pole plate (1), the mastoid pole plate (1) is provided with a surface A and a surface B which are oppositely arranged, the mastoid pole plate (1) is provided with an alkali liquor diffusion area (6) and an alkali liquor outlet temperature control area (7), and the mastoid pole plate is divided into a surface A2 and a surface B2 by the alkali liquor diffusion area; the surface of B2 is concaved inwards to form first protrusions (8) on the surface of A2, the surface of A2 is concaved inwards to form second protrusions (9) on the surface of B2, and a plurality of first protrusions (8) and a plurality of second protrusions (9) are arranged at intervals; the mastoid pole plate is divided into an A1 surface and a B1 surface by the alkali liquor outlet temperature control area (7), and third bulges (10) are symmetrically and densely arranged on the A1 surface and the B1 surface. According to the invention, the third bulge narrows the alkali liquor flow channel, accelerates the flow speed, quickly discharges the alkali liquor which is easy to form a high-temperature accumulation area originally, and reduces the structural damage and safety problems caused by local high temperature.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of hydrogen production by electrolysis of water, and in particular to a mastoid plate of a hydrogen production electrolyzer for rapidly replacing alkaline solution in a high temperature zone. Background Art

[0002] Hydrogen energy has the advantages of being environmentally friendly, storable, and renewable. Electrolysis of water to produce hydrogen is an important way to achieve large-scale and cheap production of hydrogen. Currently, industrial water electrolysis to produce hydrogen mostly uses bipolar filter press electrolyzers. The space between the two main plates forms an electrolyzer chamber, and hundreds of electrolyzer chambers with the same structure make up the electrolyzer.

[0003] like Figure 1 As shown, it is a schematic diagram of the explosion structure of a bipolar filter press type electrolytic cell in the prior art. The bipolar filter press type electrolytic cell mainly includes two pole plates 01, two electrodes 02 symmetrically arranged between the two pole plates 01, which are respectively the positive pole and the negative pole of the power supply, and a diaphragm 03 arranged between the positive pole and the negative pole. The diaphragm 03 can prevent the gases from penetrating each other. Gaskets 04 are arranged at both ends of the diaphragm 03, and pole frames 05 are arranged at both ends of the electrode 01. The space between the two pole plates 01 constitutes an electrolytic cell chamber.

[0004] The working principle of hydrogen production by water electrolysis is that when the alkali solution enters the electrolysis chamber from the bottom and flows upward, the two plates 01 are connected to the positive and negative electrodes of the DC power supply respectively. Under the action of the two electrodes 01, water is electrolyzed into hydrogen and oxygen. The overall reaction formula for hydrogen production by water electrolysis is: 2H2O=2H2↑+O2↑+exothermic. The water electrolysis efficiency of the alkali solution electrolyzer is about 60% to 80% of the input power, and the rest is lost in the form of heat release. Most of this heat enters the alkali solution, which increases the temperature of the alkali solution flowing through the electrolysis chamber.

[0005] The surface characteristics of the main plate will affect the flow characteristics of the electrolytic chamber, the flow characteristics of the electrolytic chamber will affect the flow of the electrolyte, the flow characteristics of the electrolyte will affect the temperature distribution of the electrolytic chamber, the temperature distribution of the electrolytic chamber will affect the voltage of the electrolytic chamber, and thus affect the energy consumption. If the local temperature of the electrolytic chamber is too high, it will also damage the performance of the diaphragm, and further have an adverse effect on the safe operation of the entire electrolytic cell. Therefore, the surface characteristics of the plate are crucial to the performance of the electrolytic cell.

[0006] In the related art, in order to form a contact point with the electrolysis and provide a diffusion channel for the alkali solution, a concave-convex nipple structure spaced apart on the surface of the electrode plate is designed as a support between the electrode plate and the electrode, and an electrolyte transmission channel is formed between the nipple structure. In this way, the nipple-shaped concave-convex structure can play a turbulent role in the electrolyte. However, when the alkali solution flows from bottom to top, the heat generated by the electrolysis gradually accumulates, and when it reaches the top of the electrolysis chamber, it is blocked by the electrode frame. The alkali solution cannot flow out of the electrolysis chamber quickly, and even forms local reflux and flow dead corners. This will cause local excessive temperature and cause varying degrees of damage to the diaphragm, gasket, electrode and plate. Summary of the invention

[0007] In order to solve the problem caused by heat accumulation at the top of the electrolysis chamber, the present application provides a hydrogen production electrolytic cell mastoid plate for quickly replacing alkaline solution in the high temperature zone.

[0008] The present application adopts the following technical scheme: a mastoid plate for a hydrogen production electrolyzer for rapidly replacing alkali solution in a high temperature zone is provided, which is applied to an electrolyzer, including a mastoid plate, the mastoid plate having an A surface and a B surface arranged opposite to each other, a first alkali solution inlet and a second alkali solution inlet are arranged at one end of the mastoid plate, and an outlet for hydrogen and alkali solution and an outlet for oxygen and alkali solution are arranged at the other end, the first alkali solution inlet and the outlet for oxygen and alkali solution are designed to be on the same surface; the second alkali solution inlet and the outlet for hydrogen and alkali solution are arranged on the mastoid plate. The other side of the electrode plate; the mastoid electrode plate has an alkali solution diffusion zone and an alkali solution outlet temperature control zone, the alkali solution diffusion zone divides the mastoid electrode plate into an A2 surface and a B2 surface, the B2 surface is concave on the A2 surface to form a first protrusion, the A2 surface is concave on the B2 surface to form a second protrusion, and the first protrusion and the second protrusion are arranged in multiples and spaced apart; the alkali solution outlet temperature control zone divides the mastoid electrode plate into an A1 surface and a B1 surface, and the A1 surface and the B1 surface both have a third protrusion that is symmetrically and densely arranged.

[0009] Preferably, the third protrusions on the A1 surface and the B1 surface are arranged in multiple groups, with multiple protrusions in each group, and the third protrusions in the entire alkali liquid outlet temperature control zone are distributed in a herringbone shape on the A1 surface and the B1 surface.

[0010] Preferably, the third protrusion is hemispherical, and of course, according to requirements, the third protrusion can also be spherical, teardrop-shaped, pear-shaped, or ellipsoidal.

[0011] Preferably, the distance between the hemispherical centers of two adjacent third protrusions on the A1 surface and the B1 surface is 2R+2mm-5mm, where R is the radius of the third protrusion.

[0012] Preferably, the distance between the hemispherical centers of two adjacent third protrusions on the A1 surface and the B1 surface is 2R+2 mm, and the density of the protrusions on the A1 surface and the B1 surface is adjusted by controlling the distance between the centers of two adjacent third protrusions.

[0013] Preferably, the third protrusion radius R ranges from 2.5 mm to 8 mm.

[0014] Preferably, the first protrusion and the second protrusion are ellipsoidal.

[0015] Preferably, the protrusion heights of the first protrusion, the second protrusion and the third protrusion on the same mastoid electrode are consistent.

[0016] Beneficial effects of this application: The present application divides the mastoid electrode into an alkali solution diffusion zone and an alkali solution outlet temperature control zone, and arranges a first protrusion and a second protrusion on the A2 surface and the B2 surface of the alkali solution diffusion zone. Through the structural shapes of the first protrusions and the second protrusions arranged at intervals, the backflow and reflux area of ​​the electrolyte flowing through the alkali solution diffusion zone is reduced, the temperature distribution is more uniform, and the normal flow rate and flow requirements of the electrolyte are guaranteed.

[0017] 2. The present application symmetrically and densely arranges the third protrusions at the alkali solution outlet of the mastoid plate to form an alkali solution outlet temperature control zone. In the electrolysis chamber formed when the two mastoid plates are working, when the alkali solution enters the alkali solution outlet temperature control zone, the structural shape of the third protrusion makes the flow channel narrower, and the flow rate of the alkali solution is accelerated, and the alkali solution that is originally prone to form a high-temperature gathering area is quickly sent to the outside of the electrolysis chamber, thereby reducing the current local high temperature at the outlet of the mastoid plate and the plate damage caused by high temperature, diaphragm damage, and gas explosion caused by the mutual crosstalk between hydrogen and oxygen caused by diaphragm damage and other safety issues.

[0018] 3. The third protrusion of the present application is distributed in a herringbone shape. The herringbone structure enhances the effect of the alkali solution gathering toward the center. Combined with the narrowing of the flow channel, the flow rate of the alkali solution is further increased, prompting the alkali solution to quickly flow out of the electrolysis chamber at the outlet, avoiding local high temperature at the outlet, making the temperature distribution of the alkali solution more uniform, the energy consumption is stable, and the electrolysis efficiency and safety of the electrolytic cell are improved.

[0019] 4. The design of the third protrusion of the present application can make the alkali solution flow rate in the alkali solution outlet temperature control zone (A1 / B1 zone) be Figure 1 The flow rate is 2-10 times that of the existing bipolar filter press electrolytic cells. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a schematic diagram of the explosion structure of a bipolar filter-press electrolytic cell in the prior art; Figure 2 This is a schematic diagram of the main structure of the mastoid electrode of the present application; Figure 3 yes Figure 2 A side view schematic diagram of the structure; Figure 4 It is a schematic diagram of the working principle of the electrolysis chamber formed by the mastoid electrode of the present application.

[0021] Reference numerals: 01-plate, 02-electrode, 03-diaphragm, 04-gasket, 05-polar frame; 1- mastoid plate, 2- first alkali solution inlet, 3- second alkali solution inlet, 4- hydrogen and alkali solution outlet, 5- oxygen and alkali solution outlet, 6- alkali solution diffusion zone, 7- alkali solution outlet temperature control zone, 8- first protrusion, 9- second protrusion, 10- third protrusion. DETAILED DESCRIPTION

[0022] The specific implementation methods of the present application are described below in conjunction with the accompanying drawings so that those skilled in the art can better understand the present application.

[0023] like Figure 1 As shown, it is a bipolar filter press electrolytic cell described in the background technology, including two pole plates 01, two electrodes 02 symmetrically arranged between the two pole plates 01, which are respectively the positive pole and the negative pole of the power supply, and a diaphragm 03 arranged between the positive pole and the negative pole. The diaphragm 03 can prevent the gases from penetrating each other. Gaskets 04 are arranged at both ends of the diaphragm 03, and pole frames 05 are arranged at both ends of the electrode 01. The space between the two pole plates 01 constitutes an electrolytic cell chamber. Figure 1 In this bipolar filter-press electrolyzer, when the alkali solution flows from bottom to top, the heat released by water electrolysis to produce hydrogen will be gradually accumulated at the outlet of the alkali solution, causing the temperature at the outlet of the alkali solution to be too high, causing varying degrees of damage to the diaphragm, gasket, electrode and plate. Figure 1 The alkali solution outlet flow channel space is wide, and the alkali solution flow rate is slow, which easily forms backflow and flow dead corners, exacerbating the formation of high temperature at the alkali solution outlet.

[0024] To solve Figure 1 The same or similar technical problems existing in similar plate structures, such as Figure 2 and Figure 3 As shown, the present application provides a mastoid plate for a hydrogen production electrolyzer for rapidly replacing alkali solution in a high temperature zone, comprising a mastoid plate 1, wherein the mastoid plate 1 has an A surface and a B surface that are arranged opposite to each other (see Figure 2, the right side is marked as surface A, and the left side is marked as surface B), a first alkali solution inlet 2 and a second alkali solution inlet 3 are arranged at the lower end of the mastoid pole plate 1, a hydrogen and alkali solution outlet 4 and an oxygen and alkali solution outlet 5 are arranged at the upper end of the mastoid pole plate 1, and the first alkali solution inlet 2 and the oxygen and alkali solution outlet 5 are arranged on the same surface, the second alkali solution inlet 3 and the hydrogen and alkali solution outlet 4 are arranged on the other side of the mastoid pole plate 1, and the alkali solution flows from bottom to top, and the mastoid pole plate 1 has an alkali solution diffusion area 6 and an alkali solution outlet The temperature control area 7 and the alkali solution diffusion area 6 divide the mastoid electrode 1 into an A2 surface and a B2 surface. The B2 surface is concave on the A2 surface to form a first protrusion 8, and the A2 surface is concave on the B2 surface to form a second protrusion 9. The first protrusion 8 and the second protrusion 9 are arranged in multiples and spaced apart. The spaced arrangement here means that whether viewed in the horizontal or vertical direction, a second protrusion 9 is arranged between two adjacent first protrusions 8, and a first protrusion 8 is arranged between two adjacent second protrusions 9 (see Figure 1 ), the first protrusion 8 and the second protrusion 9 are ellipsoidal; the alkali liquid outlet temperature control zone 7 is close to the hydrogen and alkali liquid outlet 4 and the oxygen and alkali liquid outlet 5, dividing the mastoid pole plate 1 into an A1 surface and a B1 surface, the A1 surface and the A2 surface constitute the A surface of the mastoid pole plate, the B1 surface and the B2 surface constitute the B surface of the mastoid pole plate, and the A1 surface and the B1 surface both have a third protrusion 10 symmetrically and densely arranged.

[0025] like Figure 2 As shown, the third protrusion 10 of the entire alkali liquid outlet temperature control zone 7 protrudes outward on the A1 surface and the B1 surface, without a concave structure shape, and the third protrusion 10 is distributed in multiple groups of herringbone shapes on the A1 surface and the B1 surface, and each group is provided with multiple hemispherical shapes, and the hemispherical center distance between two adjacent third protrusions 10 is 2R+2mm, where R is the radius of the third protrusion 10, and generally R has a value range of 2.5mm-8mm, forming dense protrusions on the A1 surface and the B1 surface. When the mastoid electrode is manufactured, the protrusion heights of the first protrusion 8, the second protrusion 9 and the third protrusion 10 remain consistent.

[0026] The working principle of this application is: Figure 3 As shown, two mastoid plates of the present application form an electrolysis chamber with positive and negative electrodes, and the alkali solution flows from bottom to top and first enters the alkali solution diffusion zone 6 ( Figure 3In the A2 / B2 section), the first protrusion 8 and the second protrusion 9 in the alkali solution diffusion zone 6 form a flow channel with a wider space. The alkali solution is electrolyzed in this area. The electrolysis reaction formula is: 2H2O=2H2↑+O2↑+exothermic. The H2 formed by electrolysis is discharged through the hydrogen and alkali solution outlet channel 4, and the O2 formed by electrolysis is discharged through the oxygen and alkali solution outlet channel 5. The heat generated in the process enters the alkali solution. Under the action of the first protrusion 8 and the second protrusion 9, the temperature distribution of the alkali solution can be made more uniform, and the retention and reflux of the alkali solution can also be reduced. When the alkali solution enters the alkali solution outlet temperature control zone 7 ( Figure 3 In the middle A1 / B1 section), the alkali solution flow channel formed by the third protrusion 10 of the present application becomes narrower, and the third protrusion 10 is distributed in a herringbone shape, the alkali solution will gather from both sides to the middle, the alkali solution flow rate will be accelerated, so that the alkali solution can flow out quickly, avoiding the alkali solution on both sides in the electrolysis chamber The large fluid resistance forms a dead corner where it stays for a long time, and avoiding the alkali solution Due to the accumulation of electrolysis heat, the local temperature of the alkali solution outlet is too high, The damage to the structures such as the mastoid plates and the diaphragm arranged between the mastoid plates, and the safety hazard of gas explosion caused by the mutual crosstalk between hydrogen and oxygen due to the damage to the diaphragm.

[0027] In order to further intuitively experience the degree of acceleration of the flow rate of the alkali solution outlet temperature control zone 7 of the present application, the following description is made: Figure 1 The flow channel of the existing electrode plate in the area corresponding to the A1 / B1 area of ​​the present application is composed of concave and convex shapes (see Figure 1 ). The flow rate comparison is calculated as follows: For a fixed alkali solution volume flow rate Q, the relationship between its flow rate through the electrode plate and the total volume passing through the regional flow channel is: Q=V*S Formula 1 Where: Q is the flow rate; V is the flow channel volume; S is the alkali solution flow rate.

[0028] Assumptions: Figure 1 The volume corresponding to the A1 / B1 area of ​​the conventional concave-convex plate in this application is V1, and the flow through Figure 1 The alkali solution flow rate is S1, then Q1=V1*S1.

[0029] In contrast, the mastoid plate described in the present application has only the third protrusion 10 in the A1 / B1 region, and is densely arranged. The flow channel volume between the two mastoid plates A1 / B1 regions is recorded as V2, the alkali solution flow rate flowing through the A1 / B1 region of the present application is recorded as S2, and the flow rate is recorded as Q2. Then V2 is equal to V1 minus the total volume V3 of the third protrusion, that is: V2=V1-V3 Formula 2 =V1-(4 / 3)πR³* N =V1-(4 / 3)πR³N Where: N is the number of hemispherical shapes of a single mastoid pole plate; (4 / 3)πR³ is Figure 4 When the two mastoid electrodes are working, the volume formed by the two hemispheres in the A1 / B1 region is equal to the volume of a spherical shape with a radius of R.

[0030] When N takes different values, V1 / V2=2~10. Combined with formula 1, when the flow rate Q1=Q2 is the same, the ratio of the flow channel volume V is inversely proportional to the ratio of the iodine solution flow rate S. Therefore, when V1 / V2=2~10, S2 / S1=2~10, that is, the flow rate of the alkali solution outlet temperature control zone 7 of the present application is Figure 1 2 to 10 times the size of the electrode structure.

[0031] The above description is only a preferred feasible implementation example of the present application, and does not limit the scope of rights of the present application. All equivalent structural changes made using the contents of this application and the drawings are included in the scope of rights of the present application.

Claims

1. A mastoid plate for a hydrogen production electrolyzer for rapidly replacing alkali solution in a high temperature zone, applied to the electrolyzer, comprising a mastoid plate (1), the mastoid plate (1) having an A surface and a B surface arranged opposite to each other, a first alkali solution inlet (2) and a second alkali solution inlet (3) being arranged at one end of the mastoid plate (1), and an outlet (4) for hydrogen and alkali solution and an outlet (5) for oxygen and alkali solution being arranged at the other end, the first alkali solution inlet (2) and the outlet (5) for oxygen and alkali solution being arranged on one side of the mastoid plate (1), and the second alkali solution inlet (3) and the outlet (4) for hydrogen and alkali solution being arranged on the other side of the mastoid plate (1), characterized in that: The mastoid electrode (1) comprises an alkali solution diffusion zone (6) and an alkali solution outlet temperature control zone (7); the alkali solution diffusion zone (6) divides the mastoid electrode (1) into an A2 surface and a B2 surface; the B2 surface is concave on the A2 surface to form a first protrusion (8); the A2 surface is concave on the B2 surface to form a second protrusion (9); a plurality of first protrusions (8) and second protrusions (9) are provided and are arranged at intervals; the alkali solution outlet temperature control zone (7) divides the mastoid electrode (1) into an A1 surface and a B1 surface; the A1 surface and the B1 surface both have third protrusions (10) arranged symmetrically and densely.

2. The hydrogen production electrolyzer mastoid plate for rapid replacement of alkali solution in high temperature zone according to claim 1, characterized in that: The third protrusions (10) on the A1 surface and the B1 surface are arranged in a plurality of groups, with a plurality of protrusions in each group, and the third protrusions (10) of the entire alkali liquid outlet temperature control zone (7) are distributed in a herringbone shape on both the A1 surface and the B1 surface.

3. The hydrogen production electrolyzer mastoid plate for rapid replacement of alkali solution in high temperature zone according to claim 1, characterized in that: The third protrusion (10) is hemispherical.

4. The mastoid plate for a hydrogen production electrolyzer for rapidly replacing alkali solution in a high temperature zone according to claim 3, characterized in that: The distance between the hemispherical centers of two adjacent third protrusions (10) on the A1 surface and the B1 surface is 2R+2mm-5mm, where R is the radius of the third protrusion (10).

5. The mastoid plate for a hydrogen production electrolyzer for rapidly replacing alkali solution in a high temperature zone according to claim 4, characterized in that: The distance between the hemispherical centers of two adjacent third protrusions (10) on the A1 surface and the B1 surface is 2R+2 mm.

6. A hydrogen production electrolyzer mastoid plate for rapid replacement of alkali solution in high temperature zone according to claim 4 or 5, characterized in that: The radius R of the third protrusion (10) ranges from 2.5 mm to 8 mm.

7. The mastoid plate for a hydrogen production electrolyzer for rapidly replacing alkali solution in a high temperature zone according to claim 1, characterized in that: The first protrusion (8) and the second protrusion (9) are elliptical cone-shaped.

8. A hydrogen production electrolyzer mastoid plate for rapid replacement of alkali solution in a high temperature zone according to claim 1, characterized in that: The protrusion heights of the first protrusion (8), the second protrusion (9) and the third protrusion (10) on the same mastoid electrode are consistent.

Citation Information

Cited By

  • Bipolar plate for producing hydrogen by electrolyzing water and pressure control method

    CN121006564A

  • A bipolar plate for hydrogen production via water electrolysis and a pressure control method

    CN121006564B

  • Composite polar plate and corresponding electrolytic bath and hydrogen production device

    CN223723239U