A packaging method and packaging structure of an automotive-grade chip
Through the automotive-grade chip packaging method, the problems of high-temperature tape residue, thin dielectric layer thickness and insufficient heat dissipation are solved, and higher product reliability and heat dissipation effect are achieved.
Patent Information
- Application Number
- CN202411203764.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-30
AI Technical Summary
In the existing chip packaging process, high-temperature tape is easily separated during the melting semi-cured sheet, resulting in residual tape on the surface, affecting product reliability; thin dielectric layer thickness leads to high-voltage breakdown and conductive cation migration defects; the heat dissipation area is limited, and the heat dissipation effect is Difference.
Using automotive-grade chip packaging methods, including surface treatment to form a multi-layer structure, using composite adhesive film to fill gaps, perform pressure transfer and curing, supplementing browning, increasing heat dissipation area, optimizing blind and through-hole designs, and filling copper columns and resin.
Effectively prevent explosive plate layering caused by residual tape, increase the thickness of the dielectric layer, enhance the bonding force on the back of the copper base, and significantly improve the reliability and heat dissipation effect of the product.
Smart Images

Figure CN118763009B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of chip packaging technology, and in particular to a packaging method and packaging structure of an automotive-grade chip. Background Art
[0002] With the advancement of technologies such as artificial intelligence and the Internet of Things, the performance of electronic products has become increasingly intelligent, and this trend has led to a growing demand for advanced packaging processes. The original chip packaging process mainly includes installing power chips on a heat-dissipating copper substrate, temporarily fixing the power module in the through-slot of a double-sided copper-clad laminate using high-temperature tape, bonding conductive copper foil with a prepreg, removing the high-temperature tape, processing blind holes and through holes to form semi-finished products, and performing solder mask silk screen printing, exposure, development, post-curing and other processes to form the final product.
[0003] However, when the inventors packaged the chips according to the original manufacturing process, they found the following problems: During the intermediate manufacturing process, when the semi-cured sheet was melted at high temperature, the high-temperature tape attached to the semi-finished chip was also affected by the high temperature and high pressure. The adhesive layer and the film layer of the high-temperature tape were easily separated. When the high-temperature tape was subsequently removed, adhesive marks of the tape remained on the surface, which required manual cleaning with alcohol, which was labor-intensive. If the cleaning was not thorough, the residual adhesive remaining in the board could easily cause the product to explode and delaminate, affecting product reliability. The flow glue generated by the melting of the semi-cured sheet was used to fill the gap between the power module and the core board slot. This will cause the thickness of the L2 / 3 dielectric layer near the power module to be seriously lower than the specified thickness. During the use of subsequent products, high-voltage breakdown and conductive cation migration defects are likely to occur at the thin position of the dielectric layer. When the power module is browned on the horizontal browning line, the bottom of the fixture is a non-hollow structure, resulting in the copper base back side not being completely browned. Due to structural factors, the back side cannot be supplemented with browning, resulting in poor bonding between the copper base back side of the final product and the L4 / 5 semi-cured sheet resin. When the chip formed by the original process is working, it is limited by the heat dissipation area and the overall heat dissipation effect is poor. Summary of the invention
[0004] To this end, the embodiments of the present application provide a packaging method and packaging structure for an automotive-grade chip, thereby improving the quality and yield rate of the product.
[0005] In a first aspect, the present application provides a packaging method for an automotive-grade chip.
[0006] This application is achieved through the following technical solutions:
[0007] A packaging method for an automotive-grade chip, comprising:
[0008] S1, performing surface treatment on the upper surface of the core board to form an L3 layer, performing surface treatment on the lower surface of the core board to form an L4 layer, processing grooves on the surface treated core board and performing browning treatment;
[0009] S2, sticking adhesive tape on the surface of the L4 layer, mounting the power module into the through groove, punching the composite adhesive film into adhesive film rectangular blocks of a preset size, and then mounting and fixing the adhesive film rectangular blocks to the area of the L3 layer corresponding to the embedded power module;
[0010] S3, performing a pressure transfer treatment on the core plate treated in step S2, so that the rectangular block of the adhesive film is heated and melted and fills the gap between the power module and the core plate, and then solidifies;
[0011] S4, removing the tape on the surface of the L4 layer, and performing additional browning treatment on the surface of the heat dissipation copper base of the power module close to the L4 layer;
[0012] S5, plasma treatment is performed on the L3 layer and the L4 layer, and multiple layers of semi-cured resin sheets and a layer of copper foil are sequentially stacked on the surface of the L3 layer and pressed to form the L2 layer, and multiple layers of semi-cured resin sheets and a layer of copper foil are sequentially stacked on the surface of the L4 layer and pressed to form the L5 layer;
[0013] S6, processing blind holes between the L2 layer and the L3 layer and between the L5 layer and the L4 layer, filling the blind holes with copper pillars, processing through holes through the L2 layer to the L5 layer, and metalizing the inner walls of the through holes;
[0014] S7, performing surface treatment on the L2 layer of the core board, performing surface treatment on the L5 layer, and performing browning treatment on the surface treated L2 layer and L5 layer;
[0015] S8, using a vacuum plug resin stencil, filling the metallized through-holes and the surface gap of the L5 layer with resin to obtain an L2 / 5 semi-finished board, and performing two-stage baking on the L2 / 5 semi-finished board;
[0016] S9, plasma treatment is performed on the L2 layer and the L5 layer, a plurality of semi-cured resin sheets and a copper foil are stacked on the surface of the L2 layer, and pressed to form the L1 layer, and a sheet of RCC material is arranged on the surface of the L5 layer, and pressed to form the L6 layer;
[0017] S10, processing blind holes between the L1 layer and the L2 layer, filling the blind holes by electroplating to form copper pillars, performing surface treatment on the L1 layer and the L6 layer to form an L1 / 6 semi-finished board, and performing processing based on the L1 / 6 semi-finished board to form a final product.
[0018] In a preferred example of the present application, it can be further configured that the RCC material in step S9 includes a layer of adhesive film with a thickness of 135μm~150μm and a layer of copper foil with a thickness of 35μm, the components of the adhesive film include 5% epoxy resin and 95% filler particles, and the filler particles include aluminum oxide and boron nitride.
[0019] In a preferred example of the present application, it can be further configured that the thermal conductivity of the adhesive film is 10 W / mK.
[0020] In a preferred example of the present application, it can be further configured that the L6 layer does not process any through holes and / or blind holes, so that the L6 layer forms a complete metal surface layer.
[0021] In a preferred example of the present application, it can be further configured that the semi-cured resin sheet is composed of glass fiber cloth and epoxy resin.
[0022] In a preferred example of the present application, it can be further configured that in step S2, the composite adhesive film is punched into adhesive film rectangular blocks of a preset size, including:
[0023] Take a roll of adhesive film material, the adhesive film material includes three layers, namely, 38 μm PET film, 60 μm adhesive film, and 10 μm OPP film;
[0024] Take a roll of micro-mucosa, which includes three layers, namely, a 30 μm PVC film, a 10 μm acrylic film, and a 75 μm PI film;
[0025] Tear off the OPP film of the adhesive film material and the PVC film of the micro-adhesive film, and stick the adhesive film of the adhesive film material on the acrylic film of the micro-adhesive film to form a composite adhesive film;
[0026] The combined adhesive film is mounted on the product shaft of the automatic cutting mechanism, the adhesive film portion of the combined adhesive film is punched into adhesive film rectangular blocks, and the adhesive film rectangular blocks are removed from the micro-adhesive film, wherein the side length of the adhesive film rectangular block is 6 mm longer than the side length of the power module.
[0027] In a preferred example of the present application, it can be further configured that in step S2, the rectangular block of adhesive film is mounted and fixed to the area of the L3 layer corresponding to the embedded power module, including:
[0028] Heat the suction head and carrier of the automatic film laminating machine to 100°C, use the suction head to suck up the rectangular block of adhesive film, and stick it to the area on the L3 layer corresponding to the embedded power module, maintaining a pressure of 0.3 MPa for 1.0 second.
[0029] In a preferred example of the present application, it can be further configured that before the core plate processed in step S2 is subjected to pressure transfer processing, the method further includes:
[0030] A release film is attached to the surface of the rectangular block of adhesive film, and the size of the release film is the same as that of the L3 layer.
[0031] In a preferred example of the present application, it can be further configured that after step S7 performs browning treatment on the surface treated L2 layer and L5 layer, the method further includes:
[0032] Make the core board pass the grinding line, and only open the nylon brush section on the grinding line. Use the nylon brush to grind off the brown film on the top surface of the line, and keep the brown film on the side wall of the line.
[0033] In a preferred example of the present application, it can be further configured that step S8 performs two-stage baking on the L2 / 5 semi-finished board, including:
[0034] The first stage is baked at 110°C for 60 minutes; the second stage is baked at 150°C for 30 minutes.
[0035] In a preferred example of the present application, it can be further configured that, in step S6, the aperture of the blind hole is 0.2 mm, and the aperture of the through hole is 0.4 mm.
[0036] In a preferred example of the present application, it can be further configured that the diameter of the blind hole in step S10 is 0.15 mm.
[0037] In a second aspect, the present application provides a packaging structure for an automotive-grade chip.
[0038] This application is achieved through the following technical solutions:
[0039] A packaging structure of an automotive-grade chip, wherein the packaging structure is prepared by the method described in the first aspect, comprising:
[0040] A core plate, wherein a through groove penetrating the upper and lower surfaces is formed on the core plate; a power module is fixed to the through groove, and a gap between the power module and the core plate is connected after being filled with an adhesive film by hot-melt and solidified; the upper surface of the core plate is a L3 layer formed by surface treatment, and the lower surface of the core plate is a L4 layer formed by surface treatment;
[0041] The surface of the L3 layer is connected to the copper foil through a dielectric layer to form the L2 layer, and the surface of the L4 layer is connected to the copper foil through a dielectric layer to form the L5 layer; wherein blind holes are opened between the L2 layer and the L3 layer and between the L5 layer and the L4 layer, and the blind holes are filled with copper pillars; and through holes are opened through the L2 layer to the L5 layer;
[0042] The surface of the L2 layer is connected to the copper foil through a dielectric layer to form the L1 layer, and the surface of the L5 layer is connected to the RCC material to form the L6 layer; wherein a blind hole is opened between the L1 layer and the L2 layer.
[0043] In a preferred example of the present application, it can be further configured that the core board is a double-sided copper-clad board, the total thickness of the double-sided copper-clad board is 1.292 mm, and the thickness of the copper board on the upper surface and the copper board on the lower surface are both 42 μm.
[0044] In a preferred example of the present application, it can be further configured that the surface spacing and through holes of the L5 layer are filled with resin through a vacuum plug resin mesh.
[0045] The present application solves the problem of severe high-temperature tape adhesive residue on the surface of the L4 layer in the multi-layer chip by optimizing the process steps, which can effectively prevent the problem of board delamination at the residual adhesive position due to heat generated during operation of the final product, and significantly improves the reliability of the product; solves the problem of severe thinness of the dielectric layer thickness of the L2 and L3 layers near the embedded power module, which can effectively prevent high-voltage breakdown or conductive cation migration defects at the thin dielectric layer position during operation of the final product; by supplementing the browning of the back side of the heat dissipation copper base, the bonding strength between the back side of the copper base and the semi-cured resin sheet is ensured, thereby improving the reliability of the product; and by optimizing the heat dissipation channel and increasing the heat dissipation area of the L6 layer, the heat dissipation effect is improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figure 1 A schematic diagram of a process for packaging a vehicle-grade chip provided in one embodiment of the present application;
[0047] Figure 2 A schematic diagram of the structure of a core board used for an automotive-grade chip provided in an embodiment of the present application;
[0048] Figure 3 A schematic diagram of the structure after the core plate is grooved according to another embodiment of the present application;
[0049] Figure 4 A schematic diagram of the structure of a mounted power module provided in another embodiment of the present application;
[0050] Figure 5 A schematic diagram of a structure for filling the gap between a power module and a core plate provided in yet another embodiment of the present application;
[0051] Figure 6 A schematic structural diagram of an L2 / 5 semi-finished plate provided in yet another embodiment of the present application;
[0052] Figure 7 A schematic diagram of a structure for opening a hole in an L2 / 5 semi-finished plate provided in another embodiment of the present application;
[0053] Figure 8 A schematic structural diagram of an L1 / 6 semi-finished plate provided in another embodiment of the present application;
[0054] Fig. 9A schematic diagram of the packaging structure of an automotive-grade chip provided in another embodiment of the present application;
[0055] Description of reference numerals:
[0056] Core board-1, through slot-101, power module-2, L3 layer-30, L4 layer-40, L2 layer-20, L2 dielectric layer-20b, L2 copper foil-20a, L5 layer-50, L5 dielectric layer-50b, L5 copper foil-50a, blind hole-7, L1 layer-10, L1 dielectric layer-10b, L1 copper foil-10a, L6 layer-60, L6 dielectric layer-60a, L6 copper foil-60b, blind hole-8, through hole-9. DETAILED DESCRIPTION
[0057] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.
[0058] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0059] In addition, the term "and / or" in this application is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this application, unless otherwise specified, generally indicates that the associated objects before and after are in an "or" relationship.
[0060] In this application, the terms "first", "second", etc. are used to distinguish identical or similar items with basically the same effects and functions. It should be understood that there is no logical or temporal dependency between "first", "second", and "nth", nor is there any limitation on quantity and execution order.
[0061] The following is a further detailed description of the embodiments of the present application in conjunction with the drawings in the specification. The packaging method proposed in this application is suitable for the packaging of automotive-grade chips. Automotive-grade chips are mainly used in automotive electronic systems, such as engine control, braking systems, safety systems, etc. Automotive-grade chips have extremely high requirements for reliability and stability, and need to meet the requirements for stable operation of automobiles under extreme temperature, high vibration, high voltage, electromagnetic interference and other working conditions. Figure 1As shown, the packaging method proposed in this application includes:
[0062] S1, performing surface treatment on the upper surface of the core board to form an L3 layer, performing surface treatment on the lower surface of the core board to form an L4 layer, processing grooves on the surface treated core board and performing browning treatment.
[0063] Specifically, a double-sided copper-clad laminate is used as the core board, the total thickness of the core board is 1.292 mm, the thickness of the copper board on the upper surface is 41 μm, and the thickness of the copper board on the lower surface is 41 μm. Figure 2 As shown, first clean the upper and lower surfaces of the core board to ensure that the board surface is clean and dry. The inner layer pattern is transferred on the copper plate on the upper surface of the core board to form a circuit layout pattern as the L3 layer; the inner layer pattern is transferred on the copper plate on the lower surface of the core board to form a circuit layout pattern as the L4 layer. At this time, the core board is recorded as an L3 / 4 semi-finished board. It should be noted that the circuit layout pattern on the upper surface and the circuit layout pattern on the lower surface can be the same circuit pattern or different circuit images. The surface treatment process of the upper surface and the surface treatment process of the lower surface can be carried out simultaneously, or the upper surface can be treated first and then the lower surface, or the lower surface can be treated first and then the upper surface.
[0064] like Figure 3 As shown, a through groove is processed on the L3 / 4 semi-finished board after surface treatment using an automatic optical alignment milling machine. The through groove is used to place the power module. The power module is composed of a chip and a copper base with a groove. The chip is fixed to the groove part of the copper base by sintering silver. The single-side size of the through groove is 100μm larger than the side of the copper base, that is, the gap between the copper base and the through groove needs to be controlled at 100μm, taking into account possible manufacturing tolerances and assembly gaps to ensure that the power module can be accurately placed in. After processing the through groove, the L3 / 4 semi-finished board needs to be browned to improve the roughness and adhesion of the copper surface so that it can be better combined with subsequent materials.
[0065] S2, sticking tape on the surface of L4 layer, mounting the power module into the through groove, punching the composite adhesive film into adhesive film rectangular blocks of preset size, and then mounting and fixing the adhesive film rectangular blocks to the area on L3 layer corresponding to the embedded power module.
[0066] like Figure 4As shown, after the browning treatment, a high-temperature resistant tape is pasted on the surface of the L4 layer. The power module is mounted into the through slot using a high-precision placement machine. The high-temperature resistant tape pasted on the L4 layer can fix the power module to prevent movement. In the actual operation process, take a roll of adhesive film material, which includes three layers, namely 38μm PET film (polyester film), 60μm adhesive film (semi-cured adhesive sheet), and 10μm OPP film (oriented polypropylene film). The width of the adhesive film material is 550μm, and it needs to be cut into a width of 127mm before use.
[0067] Take a roll of micro-mucosal film with a width of 127mm, which includes three layers, namely 30μm PVC film (polyvinyl chloride film), 10μm acrylic film, and 75μm PI film (polyimide film); tear off the OPP film of the adhesive film material and the PVC film of the micro-mucosal film, and stick the adhesive film of the adhesive film material on the acrylic film of the micro-mucosal film to form a composite adhesive film; install the combined adhesive film on the product shaft of the automatic cutting mechanism, and cut the size of the 140mm The 70mm small die is fixed on the table of the automatic punching machine, with the blade of the small die facing upwards. The equipment is started to punch and cut the adhesive film part of the combined adhesive film into 42mm The 33mm adhesive film rectangular block is removed from the micro-mucosal film; wherein the side length of the adhesive film rectangular block is 6mm longer than the side length of the power module. Because the micro-mucosal film layer is thick and is not broken, the adhesive film rectangular block is finally removed from the micro-mucosal film.
[0068] The suction head and carrier of the automatic film laminating machine are heated to 100℃, and the adhesive film rectangular block is sucked by the suction head and attached to the area corresponding to the embedded power module on the L3 layer, and maintained at a pressure of 0.3MPa for 1.0s. A rectangular block of 33um adhesive film is attached to the embedded power module area on the L3 layer of the core board, and a pressure of 0.3MPa is maintained for 1s, so that the adhesive film is heated and melted and attached to the L3 layer of the core board. The glass transition temperature of the adhesive film is 210℃, which is higher than the maximum heating temperature of the chip when it is working, and meets the product's requirements for heat resistance of the material. This means that the adhesive film can still maintain stable performance in a high temperature environment and will not deform or fail due to temperature changes, thereby ensuring the long-term stability and reliability of the chip package.
[0069] S3, performing pressure transfer treatment on the core plate processed in step S2, so that the rectangular block of adhesive film is heated and melted and fills the gap between the power module and the core plate, and then solidifies.
[0070] Specifically, the pressure transmission condition is 40N / cm at a temperature of 130°C.2 Pressing. Figure 5 As shown, the adhesive film is heated and melted during the high-temperature pressure transfer process, and the resin and filler particles contained in the adhesive film flow into and fill the gap between the power module and the L3 layer and the L4 layer. Then the resin solidifies and firmly embeds the power module inside the core board.
[0071] In some embodiments, before the pressure transfer treatment is performed, a release film is attached to the surface of the rectangular block of the adhesive film, and the size of the release film is the same as the size of the L3 layer. The release film can be a polyethylene protective film. After the pressure transfer treatment is completed, the release film is torn off for subsequent treatment.
[0072] S4, remove the tape on the surface of the L4 layer, and perform additional browning treatment on the surface of the heat dissipation copper base of the power module close to the L4 layer.
[0073] Remove the high temperature resistant tape on the surface of the L4 layer, pass the L3 / 4 semi-finished board through the browning line again, and perform additional browning on the back of the heat dissipation copper base, that is, the surface close to the L4 layer. Through the additional browning treatment, it can be ensured that all copper surfaces that need to be browned are fully processed, thereby improving the overall quality and reliability of the finished product.
[0074] S5, plasma treatment is performed on the L3 layer and the L4 layer, and multiple layers of semi-cured resin sheets and a layer of copper foil are sequentially stacked on the surface of the L3 layer and pressed to form the L2 layer, and multiple layers of semi-cured resin sheets and a layer of copper foil are sequentially stacked on the surface of the L4 layer and pressed to form the L5 layer.
[0075] Plasma treatment is performed on the L3 layer and L4 layer of the L3 / 4 semi-finished board to roughen the surface of the adhesive film into a honeycomb shape, and hydrophilic hydroxyl and carboxyl groups are generated on the surface of the adhesive film to enhance the bonding strength between the adhesive film and the semi-cured sheet resin to be subsequently pressed. Specifically, the semi-cured resin sheet is a RC74 type PP sheet composed of glass fiber cloth and epoxy resin, wherein the weight proportion of the epoxy resin is 74%. In some embodiments, Figure 6 As shown, two layers of semi-cured resin sheets and a layer of copper foil are sequentially stacked on the surface of the L3 layer and pressed together to form the L2 layer, and two layers of semi-cured resin sheets and a layer of copper foil are sequentially stacked on the surface of the L4 layer and pressed together to form the L5 layer. Each layer is firmly combined together to form an integral multi-layer circuit board structure.
[0076] S6, processing blind holes between the L2 layer and the L3 layer and between the L5 layer and the L4 layer, filling copper pillars in the blind holes, processing through holes through the L2 layer to the L5 layer, and metalizing the inner walls of the through holes.
[0077] In the actual implementation process, after pre-treating the surface of the L2 layer and the surface of the L5 layer, a laser drill is used to process blind holes at the location of the copper base and the chip, that is, at the location of the power module. The blind holes are located between the L2 layer and the L3 layer and between the L5 layer and the L4 layer. The drilling smudge on the blind hole is removed, and the blind hole is filled with electroplating to form a ∅0.2mm copper column. A ∅0.4mm mechanical hole is drilled through the L2 layer to the L5 layer, that is, through the L2 layer, the L3 layer, the core board, the L4 layer and the L5 layer, that is, a through hole, and then the drilling smudge of the through hole is removed, and the inner wall of the through hole is metalized by electroplating until the electroplated hole copper is ≥25um.
[0078] The diameter of the blind hole is ∅0.2mm, and the diameter of the through hole is ∅0.4mm. Blind holes are mainly used to achieve electrical connections in specific areas within the same layer or between different layers, while through holes are used to penetrate the entire circuit board and connect copper foil lines between different layers to ensure that signals and power can be transmitted smoothly between layers.
[0079] S7, performing surface treatment on the L2 layer of the core board, performing surface treatment on the L5 layer, and performing browning treatment on the surface treated L2 layer and L5 layer.
[0080] An image transfer is performed on the copper plate surface of the L2 layer to form a circuit layout pattern, and an image transfer is performed on the copper plate surface of the L5 layer to form a circuit layout pattern. The surface-treated L2 layer and L5 layer are subjected to browning treatment, so that a layer of browning film is formed on the line surface of the L2 layer and L5 layer, including the top surface of the line and the side wall of the line. The browning film is a metal copper organic complex with a thickness at the molecular level. It has the characteristics of large specific surface area, high surface tension, and is a polar film. It can significantly increase the bonding force between the buried hole and the line surface and the plugging / filling resin, and improve product reliability. It should be noted that the circuit layout pattern on the surface of the L2 layer and the circuit layout pattern on the surface of the L5 layer can be the same image, and can be set to different patterns according to actual needs. At the same time, the surface treatment process of the L2 layer and the surface treatment process of the L5 layer can be processed simultaneously, or they can be processed one after another.
[0081] In some embodiments, after the browning treatment in step S7, the step further includes: passing the core board through a grinding line, where only a nylon brush section is opened, and the browning film on the top surface of the circuit is ground off with a nylon brush, and the browning film on the side wall of the circuit is retained. The purpose of this operation is to remove the browning film on the surface of the circuit, prevent the plugging / gap filling resin from diffusing to the top surface of the circuit along the micro texture of the browning film, and ensure that the buried hole and the circuit spacing are tightly filled with resin.
[0082] S8, using a vacuum plug resin stencil, filling the metallized through-holes and the surface spacing of the L5 layer with resin to obtain an L2 / 5 semi-finished board, and performing two-stage baking on the L2 / 5 semi-finished board.
[0083] In the actual implementation process, a vacuum plug resin film is first made, and then the vacuum plug resin stencil is made with the film. The opening of the buried hole position on the vacuum plug resin stencil is 0.5mm larger than the actual buried hole diameter, and the opening of the spacing position on the stencil is 0.5mm larger than the actual spacing, so as to ensure that the resin can be fully filled into the buried hole and the line spacing on the L5 layer surface.
[0084] The baking process is divided into two stages: the first stage is 110°C for 60 minutes; the second stage is 150°C for 30 minutes. After baking, the resin is solidified, but the resin monomer has not yet completely cross-linked and polymerized, ensuring that the resin monomer of the ink can further cross-link and polymerize with the resin monomer of the high heat dissipation material during the subsequent high-temperature pressing process, which helps to improve product reliability.
[0085] S9, plasma treatment is performed on the L2 layer and the L5 layer, a plurality of semi-cured resin sheets and a copper foil are stacked on the surface of the L2 layer, and pressed together to form the L1 layer, and a sheet of RCC material is arranged on the surface of the L5 layer, and pressed together to form the L6 layer.
[0086] After step S8, the drilling smears on the L2 layer and the L5 layer need to be removed. After the drilling smears are removed, the L2 layer and the L5 layer are subjected to plasma treatment to roughen the surface of the resin ink into a honeycomb shape and generate hydrophilic hydroxyl and carboxyl groups on the surface of the resin ink to enhance its bonding strength with the subsequent prepreg resin to be laminated.
[0087] Specifically, a layer of RCC material is arranged on the surface of the L5 layer; the RCC material includes a layer of adhesive film with a thickness of 135μm~150μm and a layer of copper foil with a thickness of 35μm, wherein the adhesive film is an adhesive sheet with high heat dissipation performance, and the components of the adhesive film include 5% epoxy resin and 95% filler particles, and the filler particles include aluminum oxide and boron nitride. The adhesive film of the RCC material is connected to the surface of the L5 layer to form a dielectric layer. It should be noted that the thermal conductivity of the adhesive film part is 10W / mK. The reason why the L5 layer line spacing needs to be filled with resin is that the thickness of the L2 layer copper plate and the L5 layer copper plate is as high as 115um, and the demand for glue filling is large, while the resin content of the adhesive sheet with high heat dissipation performance is low. Even if high temperature and high pressure are applied for pressure transmission, the L5 layer line spacing cannot be filled. After the pressure transmission, there will be serious glue filling voids, which affects the reliability of the product. The glass transition temperature of the plugging / filling resin is 170°C, which is higher than the maximum heating temperature (165°C) of the buried vias and L5 layer line spacing when the substrate is working. It meets the product's requirements for material heat resistance and can effectively improve the thermal stability of the final product.
[0088] S10, processing blind holes between the L1 layer and the L2 layer, filling the blind holes by electroplating to form copper pillars, performing surface treatment on the L1 layer and the L6 layer to form an L1 / 6 semi-finished board, and performing processing based on the L1 / 6 semi-finished board to form a final product.
[0089] The diameter of the blind hole between the L1 layer and the L2 layer is 0.15 mm. The surface treatment of the L1 layer and the L6 layer refers to transferring the outer layer image of the L1 layer to form a circuit layout pattern, and transferring the outer layer image of the L6 layer to form a circuit layout pattern.
[0090] like Figure 8 As shown in the figure, the L6 layer formed by lamination does not process any through holes and / or blind holes, so that the L6 layer forms a complete metal surface layer, which is insulated from any other layers. The large gold surface of the L6 surface can be used to weld a whole large water-cooled radiator for heat dissipation. It effectively increases the heat dissipation area of the product and improves the heat dissipation effect, so as to prevent the problem of large heat accumulation in the power chip inside the package and excessively high junction temperature of the product. At the same time, only one water-cooled radiator needs to be welded, which effectively simplifies the workload of the back-end process.
[0091] In the actual implementation process, the L1 / 6 semi-finished board is semi-finished for solder mask screen printing, solder mask exposure, solder mask development, and post-curing to form a solder mask pattern, deposit nickel palladium gold, and the product gong board forms a Set unit to form the final product.
[0092] The packaging method proposed in this application solves the problem of serious residual adhesive traces of the high-temperature resistant tape on the L4 layer by optimizing the packaging process, which can effectively prevent the heat generated during the operation of the product from causing the board to explode and delaminate at the residual adhesive position, significantly improving the product reliability; solves the problem of the serious thinness of the dielectric layer thickness of the L2 and L3 layers near the embedded power module, which can effectively prevent high-voltage breakdown or conductive cation migration defects at this position during the operation of the product; realizes the browning of the back of the heat dissipation copper base, ensures the bonding strength between the back of the copper base and the semi-cured sheet resin, significantly improving the product reliability; the heat dissipation channel design is optimized, the area is increased, and the heat dissipation effect is significantly enhanced. When the new chip is working, the heat is transferred to the water-cooled radiator welded to the large gold surface of the L6 layer through the path of "power chip → sintered silver layer → heat dissipation copper base → copper pillars from L4 to L5 layers → copper layer L5 → high heat dissipation adhesive sheet → large gold surface of L6". The heat dissipation area is equivalent to the area of the large gold surface, which is 2520mm 2 , which is much larger than the heat dissipation area of the original product; all power modules on the same product share a water-cooled radiator, which significantly reduces the assembly workload of the rear-end water-cooled radiator.
[0093] Another embodiment of the present application further provides a packaging structure of an automotive-grade chip, which is prepared by the packaging method of the automotive-grade chip described above. Fig. 9 As shown, the packaging structure includes:
[0094] A core board 1, on which a through groove 101 is provided that passes through the upper and lower surfaces; a power module 2 is fixed to the through groove 101, and a gap between the power module 2 and the core board 1 is connected after being filled with an adhesive film by hot-melt and solidified; the upper surface of the core board 1 is a L3 layer 30 formed by surface treatment, and the lower surface of the core board is a L4 layer 40 formed by surface treatment;
[0095] The upper surface of the L3 layer 30 is connected to the L2 copper foil 20a through the L2 dielectric layer 20b to form the L2 layer 20, and the lower surface of the L4 layer is connected to the L5 copper foil 50a through the L5 dielectric layer 50b to form the L5 layer 50; wherein blind holes 7 are opened between the L2 layer 20 and the L3 layer 30 and between the L5 layer 50 and the L4 layer 40, and the blind holes 7 are filled with copper pillars;
[0096] The upper surface of the L2 layer 20 is connected to the L1 copper foil 10a through the L1 dielectric layer 10b to form the L1 layer 10, and the lower surface of the L5 layer is connected to the RCC material to form the L6 layer 60, and the L6 layer 60 includes the L6 dielectric layer 60b and the L1 copper foil 60a; wherein a blind hole 8 is opened between the L1 layer and the L2 layer.
[0097] A through hole 9 is provided through the L2 layer 20 to the L5 layer 50 .
[0098] In some embodiments, the core board 1 is a double-sided copper clad laminate, the total thickness of the double-sided copper clad laminate is 1.292 mm, the thickness of the copper plate on each surface is 42 μm, and the thickness of the copper plate on the upper surface and the copper plate on the lower surface are both 42 μm.
[0099] In some embodiments, the surface spacing of the L5 layer 50, ie, the line spacing and the through-hole 9, is filled with resin through a vacuum plug resin stencil.
[0100] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0101] Those skilled in the art can clearly understand that for the convenience and simplicity of description, only the division of the above-mentioned functional units and modules is used as an example. In actual applications, the above-mentioned functions can be distributed and completed by different functional units and modules as needed, that is, the internal structure of the system described in the present application is divided into different functional units or modules to complete all or part of the functions described above.
Claims
1. A packaging method for an automotive-grade chip, characterized in that: include: S1, performing surface treatment on the upper surface of the core board to form an L3 layer, performing surface treatment on the lower surface of the core board to form an L4 layer, processing grooves on the surface treated core board and performing browning treatment; S2, sticking adhesive tape on the surface of the L4 layer, mounting the power module into the through groove, punching the composite adhesive film into adhesive film rectangular blocks of a preset size, and then mounting and fixing the adhesive film rectangular blocks to the area of the L3 layer corresponding to the embedded power module; S3, performing a pressure transfer treatment on the core plate treated in step S2, so that the rectangular block of the adhesive film is heated and melted and fills the gap between the power module and the core plate, and then solidifies; S4, removing the tape on the surface of the L4 layer, and performing additional browning treatment on the surface of the heat dissipation copper base of the power module close to the L4 layer; S5, plasma treatment is performed on the L3 layer and the L4 layer, and multiple layers of semi-cured resin sheets and a layer of copper foil are sequentially stacked on the surface of the L3 layer and pressed to form the L2 layer, and multiple layers of semi-cured resin sheets and a layer of copper foil are sequentially stacked on the surface of the L4 layer and pressed to form the L5 layer; S6, processing blind holes between the L2 layer and the L3 layer and between the L5 layer and the L4 layer, filling the blind holes with copper pillars, processing through holes through the L2 layer to the L5 layer, and metalizing the inner walls of the through holes; S7, performing surface treatment on the L2 layer of the core board, performing surface treatment on the L5 layer, and performing browning treatment on the surface treated L2 layer and L5 layer; S8, using a vacuum plug resin stencil, filling the metallized through-holes and the surface gap of the L5 layer with resin to obtain an L2 / 5 semi-finished board, and performing two-stage baking on the L2 / 5 semi-finished board; S9, plasma treatment is performed on the L2 layer and the L5 layer, a plurality of semi-cured resin sheets and a copper foil are stacked on the surface of the L2 layer, and pressed to form the L1 layer, and a sheet of RCC material is arranged on the surface of the L5 layer, and pressed to form the L6 layer; S10, processing blind holes between the L1 layer and the L2 layer, filling the blind holes with electroplating to form copper pillars, performing surface treatment on the L1 layer and the L6 layer to form an L1 / 6 semi-finished board, and performing processing on the basis of the L1 / 6 semi-finished board to form a final product; Step S2 is to punch the composite adhesive film into rectangular adhesive film blocks of a preset size, including: Take a roll of adhesive film material, the adhesive film material includes three layers, namely, 38 μm PET film, 60 μm adhesive film, and 10 μm OPP film; Take a roll of micro-mucosa, which includes three layers, namely, a 30 μm PVC film, a 10 μm acrylic film, and a 75 μm PI film; Tear off the OPP film of the adhesive film material and the PVC film of the micro-adhesive film, and stick the adhesive film of the adhesive film material on the acrylic film of the micro-adhesive film to form a composite adhesive film; The composite adhesive film is mounted on the product shaft of the automatic cutting mechanism, the adhesive film part of the composite adhesive film is punched into adhesive film rectangular blocks, and the adhesive film rectangular blocks are removed from the micro-adhesive film, wherein the side length of the adhesive film rectangular block is 6 mm longer than the side length of the power module.
2. The packaging method of the automotive-grade chip according to claim 1, characterized in that: In step S9, the RCC material includes: a layer of adhesive film with a thickness of 135 μm-150 μm and a layer of copper foil with a thickness of 35 μm, wherein the components of the adhesive film include 5% epoxy resin and 95% filler particles, and the filler particles include aluminum oxide and boron nitride.
3. The packaging method of the automotive-grade chip according to claim 2, characterized in that: The thermal conductivity of the adhesive film is 10 W / mK.
4. The packaging method of the automotive-grade chip according to claim 1, characterized in that: No through holes and / or blind holes are processed in the L6 layer, so that the L6 layer forms a complete metal surface layer.
5. The packaging method of the automotive-grade chip according to claim 1, characterized in that: The semi-cured resin sheet is composed of glass fiber cloth and epoxy resin.
6. The packaging method of the automotive-grade chip according to claim 1, characterized in that: Step S2 includes mounting and fixing the rectangular block of adhesive film to the area corresponding to the embedded power module on the L3 layer, including: Heat the suction head and carrier of the automatic film laminating machine to 100°C, use the suction head to suck up the rectangular block of adhesive film, and stick it to the area on the L3 layer corresponding to the embedded power module, maintaining a pressure of 0.3 MPa for 1.0 second.
7. The packaging method of the automotive-grade chip according to claim 1, characterized in that: Before the core plate processed in step S2 is subjected to pressure transfer processing, the method further includes: A release film is attached to the surface of the rectangular block of adhesive film, and the size of the release film is the same as that of the L3 layer.
8. The packaging method of the automotive-grade chip according to claim 1, characterized in that: After the surface treated L2 layer and L5 layer are subjected to browning treatment in step S7, the following steps are further included: Make the core board pass the grinding line, and only open the nylon brush section on the grinding line. Use the nylon brush to grind off the brown film on the top surface of the line, and keep the brown film on the side wall of the line.
9. The packaging method of the automotive-grade chip according to claim 1, characterized in that: Step S8 performs two-stage baking on the L2 / 5 semi-finished board, including: The first stage is baked at 110°C for 60 minutes; the second stage is baked at 150°C for 30 minutes.
10. The method for packaging an automotive-grade chip according to claim 1, characterized in that: In step S6, the diameter of the blind hole is 0.2 mm, and the diameter of the through hole is 0.4 mm.
11. The packaging method of the automotive-grade chip according to claim 1, characterized in that: In step S10 , the diameter of the blind hole is 0.15 mm.
12. A packaging structure of an automotive-grade chip, prepared by the method according to any one of claims 1 to 11, characterized in that: include: A core plate, wherein a through groove penetrating the upper and lower surfaces is formed on the core plate; a power module is fixed to the through groove, and a gap between the power module and the core plate is connected after being filled with an adhesive film by hot-melt and solidified; the upper surface of the core plate is a L3 layer formed by surface treatment, and the lower surface of the core plate is a L4 layer formed by surface treatment; The surface of the L3 layer is connected to the copper foil through a dielectric layer to form the L2 layer, and the surface of the L4 layer is connected to the copper foil through a dielectric layer to form the L5 layer; wherein blind holes are opened between the L2 layer and the L3 layer and between the L5 layer and the L4 layer, and the blind holes are filled with copper pillars; and through holes are opened through the L2 layer to the L5 layer; The surface of the L2 layer is connected to the copper foil through a dielectric layer to form the L1 layer, and the surface of the L5 layer is connected to the RCC material to form the L6 layer; wherein a blind hole is opened between the L1 layer and the L2 layer.
13. The packaging structure of the automotive-grade chip according to claim 12, characterized in that: The core board is a double-sided copper-clad board, the total thickness of the double-sided copper-clad board is 1.292 mm, and the thickness of the copper board on the upper surface and the copper board on the lower surface are both 42 μm.
14. The packaging structure of the automotive-grade chip according to claim 12, characterized in that: The surface spacing and through holes of the L5 layer are filled with resin through a vacuum plug resin stencil.