Method for ornamental planting by using waste foamed bricks
By mixing waste foam bricks with sludge and nutrient soil, and using them for ornamental planting after treatment, the problems of soil compaction and resource waste are solved, soil aeration and water permeability are improved, plant growth is promoted, and environmental pollution is reduced pollute.
Patent Information
- Application Number
- CN202311421045.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-31
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-10-31
AI Technical Summary
The existing ornamental nutrient soil is easy to compact and has poor water permeability, which is not conducive to the growth of vegetation. In addition, the recycling cost of waste foam bricks is high, resulting in serious waste of resources and contamination of the soil and groundwater environment after landfill.
The waste foam bricks are broken into 1~10mm particles and mixed with sludge and nutrient soil. The soil structure is improved through heating and foaming agent treatment, increasing aeration and water permeability, and forming soil suitable for ornamental planting.
It improves soil porosity, increases resource utilization, reduces environmental pollution, reduces land occupation and production costs, and promotes the normal growth of plants.
Smart Images

Figure FT_1 
Figure SMS_1 
Figure SMS_2
Abstract
Description
Technical Field
[0001] The invention relates to the field of resource application of waste foam bricks, and in particular to a method for using waste foam bricks for ornamental planting. Background Art
[0002] Most of the existing raw materials for ornamental nutrient soil are a mixture of garden soil, river sand, peat soil, mountain mud, sawdust, wood ash, humus, crop straw and fungus cultivation waste. They are not properly formulated and sterilized, are easily compacted, have poor water permeability, and are not conducive to the normal growth and development of vegetation. For example, a Chinese patent with publication number CN 109232072 A discloses a nutrient soil for potted pomegranates, which comprises the following raw materials by weight: 35-40 parts of garden soil, 0.2-0.5 parts of decomposed chicken manure, 0.8-1.2 parts of fish bone meal, 0.6-0.8 parts of plant ash, 0.2-0.4 parts of bentonite, 5-8 parts of mountain mud, 50-70 parts of coniferous soil, 10-20 parts of chitosan, 5-10 parts of plant ash, 5-10 parts of pine bark, 0.2-0.3 parts of decomposed bean cake, 1-1.5 parts of peat soil, 0.4-0.6 parts of bentonite, 1.2-1.5 parts of decomposed cottonseed hulls, 0.6-0.8 parts of ash, 0.2-0.4 parts of bentonite, 0.6-0.4 parts of ash ... .6 parts, 1-3 parts of old lime, 10-20 parts of earthworm castings, 5-10 parts of river sand, 2-5 parts of active microorganisms, and the rest is humus soil. This patent is made by mixing garden soil, humus, crop straw and fungus cultivation waste materials, and has not undergone reasonable ingredient preparation and disinfection and sterilization. It is easy to become compacted and has poor water permeability, which is not conducive to the normal growth and development of vegetation.
[0003] In recent years, foam bricks have been widely used as a building insulation material. There are two types of foam bricks in terms of raw materials, one is foam cement bricks and the other is autoclaved foam concrete bricks. Foam cement bricks are made by mixing small foam particles with cement and condensing them. They have the excellent properties of light weight, heat preservation, sound insulation and fire resistance. Autoclaved foam concrete bricks are mainly made of cement, slag powder and river sand as raw materials. After mixing, they are foamed by pressurized air, and air is forced into the mixed slurry to form a micro-bubble structure of concrete casting molds, and are made through processes such as autoclaving reaction.
[0004] At present, a large amount of waste foam bricks will inevitably be generated during the house demolition process. At present, the resource utilization direction of waste foam bricks and other waste building materials is mainly to recycle them as raw materials and then make foam bricks again. In the process of remaking foam bricks from waste building materials such as waste foam bricks, since it is necessary to crush and chemically react the waste building materials such as waste foam bricks for multiple times, the preparation process is complicated and the production cost is high. Since the demolition of houses is dispersed and small-scale, the cost of recycling waste foam bricks is increased, resulting in that the waste foam bricks cannot be fully recycled, causing a certain waste of resources. For example, the Chinese patent with the authorization announcement number CN101412634B discloses a method for making foam bricks from waste building materials, which includes mixing, foaming, mixing and injection molding. The patent requires crushing and chemically reacting the waste building materials such as waste foam bricks for multiple times, the preparation process is complicated and the production cost is high. Since a large number of waste foam bricks are required in the production process, the foam bricks are collected and transported from the dispersed and small-scale disassembly, which increases the cost of recycling waste foam bricks, resulting in that the waste foam bricks cannot be fully recycled, causing a certain waste of resources. At present, the treatment of waste foam bricks is mainly based on landfilling, which increases the pressure of landfilling of construction waste and also pollutes the soil and groundwater environment to a certain extent.
[0005] Therefore, a method for using waste foam bricks for ornamental planting is proposed to solve the above problems. Summary of the invention
[0006] The purpose of the present invention is to provide a method for using waste foam bricks for ornamental planting. The waste foam bricks used are derived from waste materials generated after the removal of thermal insulation materials in the conventional construction industry, and contain cement, slag powder, river sand, etc., which are crushed to prepare particles with a particle size of 1 to 10 mm. Cement is a powdery hydraulic inorganic cementitious material. After adding water and stirring, it becomes a slurry, which can harden in the air or in water, and can firmly cement materials such as sand and stone together. Slag powder is the abbreviation of granulated blast furnace slag powder, which is a high-quality concrete admixture. The slag powder contains more than 95% of vitreous and minerals such as dicalcium silicate, calcium feldspar, and wollastonite. River sand is produced by natural stone in a natural state, which is repeatedly impacted and rubbed by water for a long time. Its composition is relatively complex, the surface has a certain smoothness, and the impurity content is high. River sand can be used as a building material and a soil type with certain quality requirements; mixing waste foam bricks and sludge with nutrient soil is conducive to improving the compaction of nutrient soil and keeping the soil loose. This method uses a variety of waste materials in the ingredients, which not only turns waste into treasure and improves resource utilization, but also occupies less land and reduces pollution to the environment. The object of the present invention is achieved in that: A method for using waste foamed bricks for ornamental planting comprises the following steps: Step 1: preparing a sludge foaming agent solution: taking dehydrated sludge and adding water to prepare a sludge-water mixture of a certain proportion, placing the mixture on a magnetic stirrer, stirring, adding an alkaline agent and a commercially available foaming agent, heating, and preparing a sludge foaming agent solution; the commercially available foaming agent is a surfactant, and its main function is to produce stable foam in an aqueous solution. Adding a foaming agent to the sludge can improve the carbon-nitrogen ratio (C / N) of the sludge, provide a skeleton structure, and is beneficial to the stabilization of the sludge. This step can obtain a foaming solution with good foaming performance; Step 2: Prepare waste foam brick particles: crush the waste foam bricks into particles of a certain size. The moderate particle size has a uniform texture, has good ventilation and drainage capabilities, and can retain water and fertilizer, which is very beneficial to plant growth. If the particle size is too large, it has a large porosity and a low specific surface area, so it usually has better air permeability and water permeability, and poor water infiltration and retention effects, resulting in excessive loss of water and salt; if the particle size is too small, although it can better retain water and nutrients, it will have poor air permeability, which will affect plant growth; Step 3: Prepare the molding raw materials: take the conventional commercially available ornamental planting nutrient soil and place it in a plastic container, take the waste foam brick particles prepared in step 2 and pour them into the plastic container, mix the commercially available ornamental planting nutrient soil and the waste foam brick particles evenly and place them; the waste foam brick particles are porous inside, have low density, high porosity, and strong adsorption and interception capacity, and can be used to loosen soil and hydrophobic materials, while the commercially available ornamental planting nutrient soil is rich in organic matter and nutrients. After the two are evenly mixed, the waste foam brick particles can be used to improve the soil structure, increase the air permeability and water permeability of the soil, and the nutrient soil can also be used to provide rich nutrients to promote plant growth; Step 4: preparing the sludge foaming agent: pouring the sludge foaming agent solution prepared in step 1 into a commercially available foaming machine for foaming, and the foamed foam is stored in a 25kg plastic bucket; this step can produce foam with uniform particle size and stable and unbreakable foam; Step 5: preparing the molding raw material: injecting the foam prepared in step 4 into the mixed molding raw material of the commercially available ornamental planting nutrient soil and the waste foamed brick particles prepared in step 3, slowly mixing evenly, so that the foam is evenly mixed in the commercially available ornamental planting nutrient soil and the waste foamed brick particles, which can improve the physical properties of the soil and improve its air permeability and water permeability; Step 6: Molding: Inject the molding raw materials prepared in step 5 into the planting box to a height of 3 to 12 cm, and place a water tray at the bottom of the planting box; Step 7: Maintenance and cultivation: Sprinkle the prepared ornamental plant seeds into the planting box prepared in step 6, place it in a place with visible sunlight at room temperature, water it 1 to 2 times a day, 0.5 to 1.5L each time, and observe the germination time and growth of the plants.
[0007] The specific operation of step 1 is as follows: 0.5-2 kg of dehydrated sludge discharged from the centrifugal dehydration room of a domestic sewage treatment plant in Zhengzhou is taken in a 10 kg plastic bucket, placed in a 5L high temperature resistant polypropylene container or other container, and water is added to the container to form a mud-water mixture with a solid content of 5%-10%; the container is placed on a magnetic stirrer, stirred, 10-50 g of calcium hydroxide or sodium hydroxide solid is added while stirring, and 1-5 mL of a commercially available foaming agent is added dropwise, mixed evenly, and then placed in a heating rod for heating, stirred while heating, and the temperature is measured. When the temperature rises to 60-90 ° C, the heating is stopped for 5 minutes to obtain a sludge foaming agent solution. This step is placed in a ventilation device for operation, and the upper end of the container is sealed with plastic wrap during the heating of the mud-water mixture, and a thermometer is suspended through a central drilling hole for temperature measurement.
[0008] The specific operation of step 2 is as follows: take 2-8 kg of waste foam bricks, first crush them into large blocks using a crushing tool, and then place them in a crusher for 2-10 minutes to crush them into waste foam brick particle size, and the amount of waste foam brick particles with a diameter of 1-10 mm in the waste foam brick particles is greater than 80% of the total amount of waste foam brick particles.
[0009] The waste foam bricks used in step 2 come from waste materials generated after the removal of thermal insulation materials in the conventional construction industry.
[0010] In the step 3, 2.5-10 kg of commercially available ornamental planting nutrient soil is placed in a plastic container and evenly mixed with 2-8 kg of the prepared waste foam brick particles.
[0011] The dimensions of the planting box are 60 cm in length, 30 cm in width and 14 cm in depth, and the prepared mixed raw materials are poured into a height of 3 to 12 cm.
[0012] The beneficial effect of the present invention is that the waste foamed bricks and sludge are mixed with nutrient soil, which is beneficial to improving the compaction of the nutrient soil and keeping the soil loose. The method uses a variety of waste materials in the ingredients, which not only turns waste into treasure and improves the resource utilization rate, but also can occupy less land and reduce pollution to the environment. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 It is a flow chart of the steps of the present invention. DETAILED DESCRIPTION
[0013] The present invention is further described below in conjunction with the accompanying drawings and embodiments. Example
[0014] A method for using waste foam bricks for ornamental planting, comprising the following steps: Step 1: Use a 10kg plastic bucket to take 1kg of dehydrated sludge discharged from the centrifugal dehydration room of a domestic sewage treatment plant in Zhengzhou City into a 5L high-temperature resistant polypropylene container or other container, and add water to the container to prepare a mud-water mixture with a solid content of 10%. Place the container on a magnetic stirrer, start stirring, add 20g of calcium hydroxide solid while stirring, and drop 2mL of a commercially available foaming agent at the same time. After mixing evenly, put a heating rod in for heating, stir while heating, measure the temperature, and stop heating for 5 minutes when the temperature rises to about 80°C to obtain a sludge foaming agent solution. This step is placed in a ventilation device for operation, and during the heating of the mud-water mixture, the upper end of the container is sealed with plastic wrap, and a thermometer is hung through a central drilled hole for temperature measurement.
[0015] Step 2: Take 3 kg of waste foam bricks generated by conventional house demolition, first break them into large blocks with a hammer, and then place them in a crusher for 4 minutes until the particle size of the waste foam bricks is more than 80% within the range of 1 to 10 mm.
[0016] Step 3: Take 7 kg of conventional commercially available ornamental planting nutrient soil and place it in a 20 L plastic container. Take 3 kg of the prepared waste foam brick particles and pour them into the plastic container. Mix well and then place aside.
[0017] Step 4: Pour the prepared sludge foaming agent solution into a commercially available foaming machine for foaming, and put the foamed solution into a 25kg plastic barrel.
[0018] Step 5: Inject the foam into the prepared mixed molding raw material of commercially available ornamental planting nutrient soil and waste foam brick particles, and slowly mix evenly to make the foam evenly mixed in the commercially available ornamental planting nutrient soil and waste foam brick particles.
[0019] Step 6: Inject the prepared molding raw materials into a planting box with a length of 60 cm, a width of 30 cm, and a depth of 14 cm to a height of 5 cm, and place a water receiving tray at the bottom of the planting box.
[0020] Step 7, sprinkle 20 prepared ornamental plant seeds into the prepared planting box, put them in the visible sunlight at room temperature, water them 2 times a day, 1L of water each time, observe that 6 seeds have sprouted on the 10th day, 15 seeds sprouted on the 20th day, the average height of the plants is about 10cm, and they are growing well, the average height of the plants is about 15cm at 30 days, and they are growing well, the average height of the plants is about 23cm at 40 days, and they are growing well, the average height of the plants is about 30cm at 50 days, and they are growing well, and the average height of the plants is about 35cm at 60 days, and they are growing well. By monitoring the plant culture raw materials at different periods, the following data are obtained, as shown in Table 1.
[0021] Table 1 List of monitoring data of plant culture raw materials
[0022] A method for using waste foam bricks for ornamental planting, comprising the following steps: Step 1: Use a 10kg plastic bucket to take 1kg of dehydrated sludge discharged from the centrifugal dehydration room of a domestic sewage treatment plant in Zhengzhou City into a 5L high-temperature resistant polypropylene container or other container, and add water to the container to prepare a mud-water mixture with a solid content of 10%. Place the container on a magnetic stirrer, start stirring, add 20g of calcium hydroxide solid while stirring, and drop 2mL of a commercially available foaming agent at the same time. After mixing evenly, put a heating rod in for heating, stir while heating, measure the temperature, and stop heating for 5 minutes when the temperature rises to about 80°C to obtain a sludge foaming agent solution. This step is placed in a ventilation device for operation, and during the heating of the mud-water mixture, the upper end of the container is sealed with plastic wrap, and a thermometer is hung through a central drilled hole for temperature measurement.
[0023] Step 2: Take 10 kg of regular commercially available ornamental planting nutrient soil and place it in a 20 L plastic container.
[0024] Step 3: Pour the prepared sludge foaming agent solution into a commercially available foaming machine for foaming, and put the foamed solution into a 25kg plastic barrel.
[0025] Step 4: Inject the foam into the prepared raw material of commercially available ornamental planting nutrient soil, and slowly mix evenly to make the foam evenly mixed in the commercially available ornamental planting nutrient soil.
[0026] Step 5: Inject the prepared molding raw materials into a planting box with a length of 60 cm, a width of 30 cm, and a depth of 14 cm to a height of 5 cm, and place a water receiving tray at the bottom of the planting box.
[0027] Step 6, sprinkle 20 prepared ornamental plant seeds into the prepared planting box, put them in the visible sunlight at room temperature, water them 2 times a day, 1L of water each time, observe that 7 seeds have sprouted on the 10th day, 17 seeds sprouted on the 20th day, the average height of the plant is 12cm, the plant grows well, the average height of the plant is about 20cm at 30 days, and the growth is good, the average height of the plant is about 26cm at 40 days, and the growth is slow, the average height of the plant is about 28cm at 50 days, and the growth is slow, and the average height of the plant is about 31cm at 60 days, and the growth is slow, and the phenomenon of leaf withering occurs. By monitoring the plant nutrition soil at different periods, the following data are obtained, as shown in Table 2.
[0028] Table 2 List of plant nutrient soil monitoring data
[0029] In summary, the present invention mixes waste foamed bricks and sludge with nutrient soil, which is beneficial to improving the compaction of the nutrient soil, keeping the soil loose, and allowing green plants to grow well.
Claims
1. A method for using waste foamed bricks for ornamental planting, characterized in that: The following steps are involved: Step 1: preparing a sludge foaming agent solution: taking dehydrated sludge and adding water to prepare a sludge-water mixture of a certain proportion, placing the mixture on a magnetic stirrer, stirring, adding an alkaline agent and a commercially available foaming agent, heating, and preparing a sludge foaming agent solution; the commercially available foaming agent is a surfactant, and its function is to produce stable foam in an aqueous solution. Adding a foaming agent to the sludge can improve the carbon-nitrogen ratio of the sludge, provide a skeleton structure, and is conducive to the stabilization of the sludge. This step can obtain a foaming solution with good foaming performance; Step 2: Prepare waste foam brick particles: crush the waste foam bricks into particles of a certain size, moderate particle size, uniform texture, good ventilation and drainage capacity, and can retain water and fertilizer, which is conducive to plant growth; Step 3: Prepare the molding raw materials: take the conventional commercially available ornamental planting nutrient soil and place it in a plastic container, take the waste foam brick particles prepared in step 2 and pour them into the plastic container, mix the commercially available ornamental planting nutrient soil and the waste foam brick particles evenly and place them; the waste foam brick particles are porous inside, have low density, high porosity, and strong adsorption and interception capacity, and can be used to loosen soil and hydrophobic materials, while the commercially available ornamental planting nutrient soil is rich in organic matter and nutrients. After the two are evenly mixed, the waste foam brick particles can be used to improve the soil structure, increase the air permeability and water permeability of the soil, and the nutrient soil can also be used to provide rich nutrients to promote plant growth; Step 4: preparing a sludge foaming agent: pouring the sludge foaming agent solution prepared in step 1 into a commercially available foaming machine for foaming, and the foamed foam is stored in a 25kg plastic bucket. This step can produce foam with uniform particle size and stable and unbreakable foam; Step 5: preparing the molding raw material: injecting the foam prepared in step 4 into the mixed molding raw material of the commercially available ornamental planting nutrient soil and the waste foamed brick particles prepared in step 3, slowly mixing evenly, so that the foam is evenly mixed in the commercially available ornamental planting nutrient soil and the waste foamed brick particles, which can improve the physical properties of the soil and improve its air permeability and water permeability; Step 6: Molding: Inject the molding raw materials prepared in step 5 into the planting box to a height of 3-12 cm, and place a water tray at the bottom of the planting box; Step 7: Maintenance and cultivation: Sprinkle the prepared ornamental plant seeds into the planting box prepared in step 6, place it in a place with visible sunlight at room temperature, water it 1 to 2 times a day, 0.5 to 1.5L each time, and observe the germination time and growth of the plants.
2. The method for using waste foamed bricks for ornamental planting according to claim 1, characterized in that: The specific operation of step 1 is as follows: 0.5-2 kg of dehydrated sludge discharged from the centrifugal dehydration room of a domestic sewage treatment plant in Zhengzhou is taken in a 10 kg plastic bucket, placed in a 5L high temperature resistant polypropylene container or other container, and water is added to the container to form a mud-water mixture with a solid content of 5%-10%; the container is placed on a magnetic stirrer, stirred, 10-50 g of calcium hydroxide or sodium hydroxide solid is added while stirring, and 1-5 mL of a commercially available foaming agent is added dropwise, mixed evenly, and then placed in a heating rod for heating, stirred while heating, and the temperature is measured. When the temperature rises to 60-90 ° C, the heating is stopped for 5 minutes to obtain a sludge foaming agent solution. This step is placed in a ventilation device for operation, and the upper end of the container is sealed with plastic wrap during the heating of the mud-water mixture, and a thermometer is suspended through a central drilling hole for temperature measurement.
3. The method for using waste foamed bricks for ornamental planting according to claim 1, characterized in that: The specific operation of step 2 is as follows: take 2-8 kg of waste foam bricks, first crush them into large blocks using a crushing tool, and then place them in a crusher for 2-10 minutes to crush them into waste foam brick particle size, and the amount of waste foam brick particles with a diameter of 1-10 mm in the waste foam brick particles is greater than 80% of the total amount of waste foam brick particles.
4. The method for using waste foamed bricks for ornamental planting according to claim 1, characterized in that: The waste foam bricks used in step 2 come from waste materials generated after the removal of thermal insulation materials in the conventional construction industry.
5. The method for using waste foamed bricks for ornamental planting according to claim 1, characterized in that: In the step 3, 2.5-10 kg of commercially available ornamental planting nutrient soil is placed in a plastic container and evenly mixed with 2-8 kg of the prepared waste foam brick particles.
6. The method for using waste foamed bricks for ornamental planting according to claim 1, characterized in that: The dimensions of the planting box are 60 cm in length, 30 cm in width and 14 cm in depth, and the prepared mixed raw materials are poured into a height of 3 to 12 cm.
Citation Information
Patent Citations
Method for manufacturing foaming brick from waste construction material
CN101412634A
Regenerated green planting soil and production method thereof
CN102173916A
Production method of sludge compressed nutrient soil
CN104119184A
Method for preparing haycite and nutrient solution for soilless culture by utilizing sludge
CN106927790A
Municipal sludge-based artificial planting soil and preparation method thereof
CN113336498A