Corrosion-resistant filter material
Through the combination of composite materials and corrosion-resistant coatings, the problem of insufficient corrosion resistance of the filter material is solved, the overall strength and corrosion resistance of the filter material are improved, and the stable operation of the filtration system is ensured.
Patent Information
- Application Number
- CN202411035092.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-10-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing filter materials have poor corrosion resistance in specific environments, resulting in shortened service life, and it is difficult for a single coating to ensure the durability of corrosion resistance.
The pre-filter layer, main filter layer and depth filter layer are made of composite materials. Through a combination of hot-pressed connection and corrosion-resistant coating, the overall strength and corrosion resistance are increased, using polytetrafluoroethylene fiber, carbon fiber, microcapsules and Zirconium oxide powder and other materials are used to form crisscross reinforcement strips to enhance the corrosion resistance of the filter material.
It improves the overall strength and corrosion resistance of the filter material, can better withstand the pressure and airflow impact during the filtration process, reduces damage and loss, and ensures the stable operation of the filtration system.
Smart Images

Figure CN118767543A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of environmentally friendly dust removal filter materials, in particular to a corrosion-resistant filter material. Background Art
[0002] Currently, most of the filter materials on the market are made of a single material, such as polyester fiber or glass fiber. These materials have poor corrosion resistance in certain environments, resulting in a shortened service life. Therefore, the development of a new type of corrosion-resistant filter material has important market value.
[0003] A Chinese patent with publication number CN116459589B discloses a method for producing a high-precision, high-temperature-resistant filter material impregnated with PTFE emulsion. By using polyester fiber or PTFE fiber or a mixture of the two fibers, the polyester fiber and PTFE fiber are light in weight and have a strong high-temperature resistance effect. When used on the filter material, the base fabric layer of the filter material forms a strong high-temperature resistance effect. In addition, in this patent, the preparation of the base fabric layer requires first dipping the fiber felt in an impregnation tank filled with PTFE emulsion, which greatly improves the corrosion resistance of the fiber felt. Then, the formed base fabric layer has the best high-temperature and corrosion resistance.
[0004] Although this patent solves the problem of insufficient high temperature resistance of filter media in the background technology to a certain extent, in this application, the main measures to improve the high filtration accuracy and high temperature resistance of the filter media are impregnation and coating. However, if the corrosion resistance is improved only by the coating, the bonding strength between the coating and the filter media will directly affect its corrosion resistance, and it is difficult to ensure the corrosion resistance of the filter media after the coating falls off. Summary of the invention
[0005] The purpose of the present invention is to provide a corrosion-resistant filter material, which is made of a composite material, each layer of which has a certain corrosion resistance. At the same time, the overall strength of the entire filter material is increased due to the setting of reinforcement strips. The high-strength filter material can better withstand the pressure, water flow and air flow impact during the filtration process, reduce the damage and loss of the filter material, thereby ensuring the stable operation of the filtration system, and solving the problems raised in the above-mentioned background technology.
[0006] To achieve the above-mentioned purpose, the present invention provides the following technical scheme: a corrosion-resistant filter material, comprising a pre-filter layer, a main filter layer and a depth filter layer arranged along the filtering direction of the filter medium, the pre-filter layer, the main filter layer and the depth filter layer are hot-pressed and connected, and the pre-filter layer, the main filter layer and the depth filter layer after hot-pressing are coated with a corrosion-resistant coating, the main filter layer is formed by overlapping the edges of a plurality of filter fiber meshes, and the filter fiber mesh is a composite material made of polytetrafluoroethylene fiber, carbon fiber and microcapsules.
[0007] Preferably, the filter fiber mesh is a square structure, and overlapping edges are provided on two adjacent sides of the filter fiber mesh.
[0008] Preferably, the pre-filtration layer is provided with criss-cross reinforcing strips at the overlapped positions of the edges of the filter fiber web, and the reinforcing strips are automatically formed under the ejection effect of the overlapped edges during hot pressing, and the reinforcing strips cover the overlapped edges.
[0009] Preferably, the pre-filtration layer is a uniform composite fiber web formed by a carding machine using hydrophobic polypropylene fibers, glass fibers and microcapsules.
[0010] Preferably, the core material of the microcapsules used to prepare the filter fiber web is activated carbon powder, and the core material of the microcapsules used to prepare the pre-filtration layer is a mixture of volcanic rock powder and alumina powder.
[0011] Preferably, the preparation method of the microcapsules is as follows: the core material is dispersed in deionized water to form a core material dispersion, the wall material is dissolved in a solvent to form a wall material solution, the core material dispersion is slowly dripped into the wall material solution by an interfacial polymerization method, and an appropriate catalyst is added at the same time, and the dripping acceleration and stirring speed are controlled to form uniform microcapsules, the mass ratio of the core material to the wall material is 2:1, the microcapsules are cured at room temperature for at least 24 hours, and the microcapsules are washed with distilled water for multiple times until the washing liquid is clear to form microcapsules.
[0012] Preferably, the depth filtration layer is a uniform composite fiber web formed by a carding machine using high temperature resistant aramid fiber, nano silicon dioxide and zirconium oxide powder.
[0013] Preferably, the preparation method of the depth filtration layer is as follows: the zirconium oxide powder is surface treated with a coupling agent, and the treated zirconium oxide powder, high temperature resistant aramid fiber, and nano-silica are put into a carding machine, and the mass ratio of high temperature resistant aramid fiber, nano-silica and zirconium oxide powder is 8:1:1.
[0014] Preferably, the corrosion-resistant coating is formed by drying a corrosion-resistant polymer solution, and the preparation method of the corrosion polymer solution is as follows: weigh the polymer powder polyvinylidene fluoride, dissolve the polyvinylidene fluoride in N-methylpyrrolidone, and heat it with a magnetic stirrer until it is completely dissolved to form a solution with a concentration of 5%.
[0015] Preferably, the main body thicknesses of the pre-filtration layer and the main filtration layer are 1 mm and 2 mm respectively, and the thickness of the depth filtration layer is 1 mm.
[0016] Compared with the prior art, the present invention has the following beneficial effects:
[0017] The corrosion-resistant filter material proposed by the present invention, the pre-filter layer, the main filter layer and the deep filter layer are all made of composite materials. The pre-filter layer is enhanced by adding microcapsules with aluminum oxide powder and volcanic rock powder as core materials to enhance the adhesion between the aluminum oxide powder and the pre-filter layer, and enhance the corrosion resistance of the pre-filter layer. The main filter layer is made of polytetrafluoroethylene fiber as the main material, which has strong corrosion resistance itself, and the zirconium oxide powder added in the deep filter layer improves the corrosion resistance of the layer. After the pre-filter layer, the main filter layer and the deep filter layer are connected, due to the setting of the overlapping edges, criss-cross reinforcement strips are formed on the surface of the filter material. When the corrosion-resistant polymer solution is coated, the filter material separated by the reinforcement strips is distributed in blocks, which is conducive to the uniform distribution of the corrosion-resistant coating. At the same time, the overall strength of the entire filter material is increased due to the setting of the reinforcement strips. The high-strength filter material can better withstand the impact of pressure, water flow and air flow during the filtration process, reduce the damage and loss of the filter material, and thus ensure the stable operation of the filtration system. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a schematic diagram of the overall structure of the corrosion-resistant filter material of the present invention;
[0019] Figure 2 It is a schematic cross-sectional view of the corrosion-resistant filter material of the present invention;
[0020] Figure 3 It is a schematic diagram of the structure of the filter fiber net of the present invention.
[0021] In the figure: 1, pre-filtration layer; 11, reinforcement strip; 2, main filtration layer; 21, filter fiber mesh; 211, overlapping edge; 3, deep filtration layer. DETAILED DESCRIPTION
[0022] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0023] In order to solve the problem that the existing filter media only improves its corrosion resistance through coating, the bonding strength between the coating and the filter media directly affects its corrosion resistance, and it is difficult to ensure the corrosion resistance of the filter media after the coating falls off. Figure 1-Figure 3 , this embodiment provides the following technical solutions:
[0024] A corrosion-resistant filter material comprises a pre-filter layer 1, a main filter layer 2 and a deep filter layer 3 arranged along the filtering direction of the filter medium, wherein the pre-filter layer 1, the main filter layer 2 and the deep filter layer 3 are connected by hot pressing, and the pre-filter layer 1, the main filter layer 2 and the deep filter layer 3 connected by hot pressing are coated with a corrosion-resistant coating. The pre-filter layer 1 is made of a composite material of hydrophobic polypropylene fiber and glass fiber, is located at the outermost layer, directly contacts the medium to be filtered, intercepts larger particles, reduces the burden of the subsequent filter layer, and provides a certain waterproof performance to prevent moisture from entering the internal filter layer. The main filter layer 2 is between the pre-filter layer 1 and the deep filter layer 3, provides efficient filtering performance, and has excellent chemical stability and high temperature resistance, and is the core part of the entire filter material. The polytetrafluoroethylene fiber has an extremely low friction coefficient, excellent corrosion resistance, and is suitable for a wide range of pH values. The deep filter layer 3 is made of a composite material of high-temperature resistant aramid fiber and nano-silicon dioxide, which further improves the filtering accuracy, especially for the filtering of tiny particles, and also provides additional high temperature resistance, and can withstand continuous operation under high temperature conditions.
[0025] In this embodiment, the main filter layer 2 is formed by overlapping the edges of several filter fiber meshes 21. The filter fiber mesh 21 is a composite material made of polytetrafluoroethylene fiber, carbon fiber and microcapsules. Through microencapsulation, the active substance can be protected from the influence of the external environment and its release can be controlled. The activated carbon can effectively adsorb organic matter in the fluid, such as solvents, dyes, etc., remove odors, adsorb substances that cause odors, and adsorb VOCs in the air to improve air quality.
[0026] In this embodiment, the filter fiber mesh 21 is a square structure, and overlapping edges 211 are provided on both adjacent sides of the filter fiber mesh 21. The adjacent ends of the overlapping edges 211 do not touch each other. When the main filter layer 2 is spliced, the overlapping edges 211 cover the adjacent filter fiber meshes 21, and a protrusion is formed on the edge of the filter fiber mesh 21. The protrusion enhances the structural strength of the main filter layer 2, and at the same time, the protrusion divides the main filter layer 2 into a plurality of squares.
[0027] In this embodiment, the pre-filter layer 1 is located at the overlapping position of the edge of the filter fiber mesh 21 and has criss-crossed reinforcing strips 11 formed thereon. The reinforcing strips 11 are automatically formed under the ejection action of the overlapping edges 211 during hot pressing. The reinforcing strips 11 cover the overlapping edges 211. After the pre-filter layer 1 is bonded to the main filter layer 2, the reinforcing strips 11 divide the pre-filter layer 1 into a number of squares. When the corrosion-resistant layer is coated, the reinforcing strips 11 can assist in the convergence of the solution, thereby strengthening the bonding strength between the corrosion-resistant layer and the surface of the filter material.
[0028] In this embodiment, the pre-filtration layer 1 is a uniform composite fiber web formed by a carding machine using hydrophobic polypropylene fibers, glass fibers and microcapsules.
[0029] In this embodiment, the core material of the microcapsules used to prepare the filter fiber mesh 21 is activated carbon powder, and the core material of the microcapsules used to prepare the pre-filter layer 1 is a mixture of volcanic rock powder and alumina powder. Volcanic rock has a porous structure and can absorb heavy metal ions in water, such as lead and mercury. The micropores on the surface of volcanic rock can become a good carrier for the growth of microorganisms and help the biodegradation process. Alumina is a hard ceramic material with very good corrosion resistance and wear resistance.
[0030] In this embodiment, the preparation method of microcapsules is as follows: the core material is dispersed in deionized water to form a core material dispersion, the wall material is dissolved in a solvent to form a wall material solution, the core material dispersion is slowly dripped into the wall material solution by interfacial polymerization, and a suitable catalyst is added at the same time, and the dripping acceleration and stirring speed are controlled to form uniform microcapsules, the mass ratio of the core material to the wall material is 2:1, the microcapsules are cured at room temperature for at least 24 hours, and the microcapsules are washed with distilled water for multiple times until the washing liquid is clear to form microcapsules.
[0031] Preparation method of microcapsules with activated carbon powder as the core material: 20g of activated carbon powder is dispersed in 50mL of water to form a dispersion with a concentration of about 40g / L, 10g of polylactic acid is dissolved in 100mL of ethyl acetate to form a solution with a concentration of about 10%, and the core material dispersion is slowly dripped into the wall material solution by interfacial polymerization. At the same time, isocyanate is added as a catalyst, and the dripping acceleration and stirring speed are controlled to form uniform microcapsules. The mass ratio of activated carbon powder to polylactic acid is 2:1. The microcapsules are cured at room temperature for 26 hours, and the microcapsules are washed with distilled water for many times until the washing liquid is clear to make microcapsules with activated carbon powder as the core material.
[0032] The preparation method of the microcapsules used in the pre-filtration layer 1 is as follows: alumina powder and volcanic rock powder are dispersed in 50 mL of water, the mass ratio of alumina powder to volcanic rock powder is 1:2, and a magnetic stirrer is used to stir until completely dispersed to form a uniform suspension with a concentration of about 40 g / L, 10 g of polylactic acid is dissolved in 100 mL of ethyl acetate, and heated by a magnetic stirrer until completely dissolved to form a solution with a concentration of about 10%, the core material dispersion is slowly dripped into the wall material solution, and a catalyst is added at the same time. The stirring speed can be set to 500-1000 rpm, and the dripping speed is about 1-2 mL per minute. The microcapsules are cured at room temperature for 24 hours, and the washing liquid is removed by centrifugation. This process is repeated at least three times, and the washed microcapsules are placed in an oven and dried at a temperature of 60°C for at least 12 hours to remove residual moisture and solvent.
[0033] In this embodiment, the depth filtration layer 3 is a uniform composite fiber web made of high temperature resistant aramid fiber, nano silicon dioxide and zirconium oxide powder through a carding machine, and the nano silicon dioxide and zirconium oxide powder are used to improve the high temperature resistance and corrosion resistance.
[0034] In this embodiment, the preparation method of the deep filtration layer 3 is as follows: the zirconium oxide powder is surface treated with a coupling agent, and the treated zirconium oxide powder, high temperature resistant aramid fiber, and nano-silica are put into a carding machine. The mass ratio of high temperature resistant aramid fiber, nano-silica and zirconium oxide powder is 8:1:1.
[0035] Weigh 1 g of 3-aminopropyltriethoxysilane and dissolve it in 100 mL of anhydrous ethanol. Stir it with a magnetic stirrer until it is completely dissolved. Add 5 g of zirconium oxide powder to the coupling agent solution and stir it evenly with a magnetic stirrer to ensure that the powder is completely dispersed. Continue to stir the mixture for 1-2 hours to ensure that the coupling agent is evenly covered on the surface of the zirconium oxide powder. Wash the treated zirconium oxide powder with deionized water several times to remove unreacted coupling agent and by-products. Place the washed zirconium oxide powder in an oven and dry it at 80°C for at least 12 hours to remove residual moisture and solvent to obtain surface-treated zirconium oxide powder.
[0036] In this embodiment, the corrosion-resistant coating is formed by drying a corrosion-resistant polymer solution. The preparation method of the corrosion polymer solution is as follows: weigh the polymer powder polyvinylidene fluoride, dissolve the polyvinylidene fluoride in N-methylpyrrolidone, and heat it with a magnetic stirrer until it is completely dissolved to form a solution with a concentration of 5%.
[0037] In this embodiment, the main body thicknesses of the pre-filtration layer 1 and the main filtration layer 2 are 1 mm and 2 mm respectively, the thickness of the main filtration layer 2 at the overlap edge 211 is 4 mm, and the thickness of the depth filtration layer 3 is 1 mm.
[0038] Processing method: hydrophobic polypropylene fiber, glass fiber and microcapsule are made into a uniform composite fiber web through a carding machine, and a pre-filter layer 1 is cut out; polytetrafluoroethylene fiber, carbon fiber and microcapsule are made into a uniform composite fiber web through a carding machine, and the composite fiber web is cut to make a filter fiber web 21 embryo; the filter fiber web 21 embryo is further cut to process an overlap edge 211 to make a filter fiber web 21; high temperature resistant aramid fiber, nano silicon dioxide and zirconium oxide powder are made into a uniform composite fiber web through a carding machine, and a depth filter layer 3 is cut out; the filter fiber web 21 is spliced on the surface of the depth filter layer 3 into a main filter layer 2, and the overlap edge 211 covers the adjacent filter fiber web 21 edge, and then on the main filter layer 2 The pre-filter layer 1 is covered on the filter material and laminated tightly together by hot pressing process. A corrosive polymer solution is prepared. The filter material is cleaned with deionized water and a mild detergent to remove impurities and grease on the surface. The filter material can be cleaned more thoroughly by using an ultrasonic cleaner. It is rinsed with deionized water and then blown dry with compressed air. The surface of the filter material is activated by plasma treatment or ultraviolet light irradiation to improve the adhesion between the coating and the filter material. The pre-treated filter material is immersed in the polymer solution and kept for a period of time to ensure full absorption. The filter material is slowly removed to allow excess solution to drip off. The dipping process is repeated to obtain a thicker coating. The coated filter material is placed in an oven for heating and curing. The curing time is usually 1-2 hours.
[0039] In summary, the present invention proposes a corrosion-resistant filter material, wherein the pre-filter layer 1, the main filter layer 2 and the deep filter layer 3 are all made of composite materials. The pre-filter layer 1 is made of microcapsules with aluminum oxide powder and volcanic rock powder as core materials to enhance the adhesion between the aluminum oxide powder and the pre-filter layer 1, and enhance the corrosion resistance of the pre-filter layer 1. The main material of the main filter layer 2 is polytetrafluoroethylene fiber, which has strong corrosion resistance itself, and the zirconium oxide powder added in the deep filter layer 3 improves the corrosion resistance of the layer. After the pre-filter layer 1, the main filter layer 2 and the deep filter layer 3 are connected, due to the setting of the overlapping edge 211, criss-cross reinforcement strips 11 are formed on the surface of the filter material. When the corrosion-resistant polymer solution is coated, the filter material separated by the reinforcement strips 11 is distributed in blocks, which is conducive to the uniform distribution of the corrosion-resistant coating. At the same time, the overall strength of the entire filter material is increased due to the setting of the reinforcement strips 11. The high-strength filter material can better withstand the impact of pressure, water flow and air flow during the filtration process, reduce the damage and loss of the filter material, and thus ensure the stable operation of the filtration system.
[0040] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0041] While the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that many changes, modifications, substitutions and variations can be made to the embodiments without departing from the principles and spirit of the invention.
Claims
1. A corrosion-resistant filter material, comprising a pre-filter layer (1), a main filter layer (2) and a depth filter layer (3) arranged along the filtering direction of the filter medium, Features: The pre-filter layer (1), the main filter layer (2) and the depth filter layer (3) are connected by hot pressing, and a corrosion-resistant coating is applied to the pre-filter layer (1), the main filter layer (2) and the depth filter layer (3) after the hot pressing. The main filter layer (2) is formed by overlapping the edges of a plurality of filter fiber meshes (21), and the filter fiber mesh (21) is a composite material made of polytetrafluoroethylene fibers, carbon fibers and microcapsules.
2. The corrosion-resistant filter material according to claim 1, Features: The filter fiber net (21) is of a square structure, and overlapping edges (211) are provided on two adjacent sides of the filter fiber net (21).
3. The corrosion-resistant filter material according to claim 2, Features: The pre-filter layer (1) is provided with crisscross reinforcing strips (11) at the overlapped positions of the edges of the filter fiber web (21); the reinforcing strips (11) are automatically formed under the ejection action of the overlapped edges (211) during hot pressing, and the reinforcing strips (11) cover the overlapped edges (211).
4. The corrosion-resistant filter material according to claim 1, Features: The pre-filtration layer (1) is a uniform composite fiber web formed by a carding machine using hydrophobic polypropylene fibers, glass fibers and microcapsules.
5. The corrosion-resistant filter material according to claim 4, Features: The core material of the microcapsules used to prepare the filter fiber net (21) is activated carbon powder, and the core material of the microcapsules used to prepare the pre-filtration layer (1) is a mixture of volcanic rock powder and alumina powder.
6. The corrosion-resistant filter material according to claim 5, Features: The preparation method of the microcapsules is as follows: dispersing the core material in deionized water to form a core material dispersion, dissolving the wall material in a solvent to form a wall material solution, slowly dripping the core material dispersion into the wall material solution by an interfacial polymerization method, adding a proper catalyst, controlling the dripping speed and stirring speed to form uniform microcapsules, wherein the mass ratio of the core material to the wall material is 2:1, curing the microcapsules at room temperature for at least 24 hours, and washing the microcapsules with distilled water for multiple times until the washing liquid is clear, thereby preparing the microcapsules.
7. The corrosion-resistant filter material according to claim 1, Features: The depth filtration layer (3) is a uniform composite fiber web made of high temperature resistant aramid fibers, nano silicon dioxide and zirconium oxide powder through a carding machine.
8. The corrosion-resistant filter material according to claim 7, Features: The preparation method of the depth filtration layer (3) is as follows: a coupling agent is used to perform surface treatment on zirconium oxide powder, and the treated zirconium oxide powder, together with high temperature resistant aramid fiber and nano-silicon dioxide, is put into a carding machine, wherein the mass ratio of the high temperature resistant aramid fiber, nano-silicon dioxide and zirconium oxide powder is 8:1:
1.
9. The corrosion-resistant filter material according to claim 8, Features: The corrosion-resistant coating is formed by drying a corrosion-resistant polymer solution. The preparation method of the corrosion polymer solution is as follows: weigh polymer powder polyvinylidene fluoride, dissolve the polyvinylidene fluoride in N-methylpyrrolidone, and heat it with a magnetic stirrer until it is completely dissolved to form a solution with a concentration of 5%.
10. The corrosion-resistant filter material according to claim 1, Features: The main body thicknesses of the pre-filtration layer (1) and the main filtration layer (2) are 1 mm and 2 mm respectively, and the thickness of the depth filtration layer (3) is 1 mm.
Citation Information
Cited By
Low-temperature-resistant high-efficiency air filtering material and preparation method thereof
CN119971627A