Preparation method of amino acid strontium

By optimizing the chelating conditions of amino acid strontium, using compound amino acid powder and strontium chloride to perform a chelation reaction, and concentrating through rotary evaporation or heating, the problems of high chelation temperature and long time in the existing technology are solved, and the cost is reduced and Improved chelation rate and stability of amino acid strontium.

CN118772000APending Publication Date: 2024-10-15FRUIT TREE INST OF CHINESE ACAD OF AGRI SCI +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410851650.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing research on amino acid metal chelates has problems such as high chelation temperatures and long chelation times, resulting in high overall chelation costs.

Method used

Compound amino acid powder and strontium chloride are used for chelation reaction. By adjusting the temperature, pH value and reaction time, combined with rotary evaporation or heating concentration, absolute ethanol is used as the leaching agent to optimize the chelation conditions of amino acid strontium.

Benefits of technology

The cost of raw materials is reduced, the chelating rate and stability of amino acid strontium are improved, and the obtained amino acid strontium chelate has a high chelating rate and is relatively stable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004916969870000031
    Figure BDA0004916969870000031
  • Figure BDA0004916969870000041
    Figure BDA0004916969870000041
  • Figure BDA0004916969870000051
    Figure BDA0004916969870000051
Patent Text Reader

Abstract

The invention relates to the technical field of preparation of amino acid strontium, in particular to a preparation method of amino acid strontium. The preparation method is prepared by carrying out chelation reaction on compound amino acid and strontium chloride, and specifically comprises the following steps: S1, preparing a 0.2 mol / L amino acid solution, and heating to a designed temperature of 40 DEG C or 55 DEG C; s2, after the designed temperature of the amino acid solution is stable, adjusting the pH value of the amino acid solution to 6-7; s3, slowly adding a pre-prepared strontium chloride solution into the amino acid solution, mixing, and carrying out chelation reaction to obtain an amino acid strontium solution; the reaction time of the chelation reaction is 60 minutes; s4, concentrating the amino acid strontium solution obtained in the step S3 in a rotary evaporation or heating manner; and S5, extracting the amino acid strontium by using an extracting agent. Good chelating conditions of the amino acid strontium are determined, the compound amino acid powder is selected as the raw material, the cost of the raw material is greatly reduced, and the obtained amino acid strontium is high in chelating rate and relatively stable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of strontium amino acid preparation, and in particular to a method for preparing strontium amino acid. Background Art

[0002] Strontium exists mainly in a chemical state in nature. It is widely distributed in the earth's crust but its content is very low. In 1972, it was clearly stated that strontium is an essential trace element for the human body. Strontium plays a very important role in promoting human bone health, preventing dental caries and osteoporosis, cardiovascular diseases, relieving depression, and promoting reproductive health. Amino acids, as chelating agents, have a moderate stability constant and are a good carrier that can prevent metal ions from being fixed or difficult to absorb during the absorption and utilization of soil and plants. And while plants absorb trace elements, they can be directly absorbed by crops.

[0003] At present, the research on amino acid metal chelates is mostly focused on elements such as copper, iron, zinc, and calcium. The amino acid raw materials required for chelation are mostly a single amino acid. At the same time, there are problems such as high chelation temperature and long chelation time, and the overall chelation cost is very high. Summary of the invention

[0004] In view of the problems existing in the prior art such as high chelation temperature and long chelation time, and high overall chelation cost, the present invention provides a method for preparing strontium amino acid, which can overcome certain or some defects of the prior art.

[0005] A method for preparing strontium amino acid according to the present invention comprises the following steps:

[0006] A method for preparing strontium amino acid, which is prepared by chelating composite amino acid powder and strontium chloride, specifically comprising:

[0007] Step S1, prepare 0.2 mol / L amino acid solution and heat to the designed temperature of 40°C or 55°C;

[0008] Step S2, after the amino acid solution is stabilized at the designed temperature, adjusting the pH value of the amino acid solution to 6-7;

[0009] Step S3, slowly adding the pre-prepared strontium chloride solution into the amino acid solution and mixing them to carry out a chelation reaction to obtain an amino acid strontium solution; the concentration of the strontium chloride solution is 3 / 5 mol / L; and the reaction time of the chelation reaction is 60 min.

[0010] Step S4, concentrating the amino acid strontium solution obtained in step S3 to 1 / 8-1 / 10 of the original volume by rotary evaporation or heating.

[0011] Step S5: extracting the strontium amino acid using an extractant, wherein the extractant is anhydrous ethanol.

[0012] Preferably, the coordination ratio of the amino acid to the strontium ion is ≥3:1.

[0013] Preferably, the coordination ratio is 4:1, 5:1 or 6:1.

[0014] Preferably, the reaction temperature of the chelating reaction is ≤70°C.

[0015] Preferably, the reaction time of the chelating reaction is 60 min.

[0016] Preferably, the substances for adjusting pH in step S2 are sodium hydroxide and hydrochloric acid;

[0017] Compared with the prior art, the present invention has the following beneficial effects:

[0018] The invention determines the optimal chelating conditions of amino acid strontium, selects composite amino acid powder as raw material, greatly reduces the cost of raw materials, and obtains amino acid strontium with high chelating rate and is relatively stable. DETAILED DESCRIPTION

[0019] Example 1

[0020] Purchase amino acid raw materials on the market: composite amino acid 80 powder (total amino acid content ≥ 80%), strontium chloride hexahydrate (purity ≥ 98%); hydrochloric acid, sodium hydroxide, anhydrous ethanol, anhydrous methanol and purified water are analytical grade.

[0021] This example determines the conditions that have the greatest impact on the chelation rate of amino acid metal compounds: coordination ratio, reaction temperature, pH value and reaction time. A 4-factor 3-level orthogonal experimental L9 (34) design is adopted, with a total of 9 treatments. The experimental orthogonal table is shown in Table 1.

[0022] The first batch of test plan: prepare 0.1mol / L amino acid solution, heat it to the design temperature in a water bath, adjust it to the required pH value, add an appropriate amount of strontium chloride solution, heat it to the design temperature in a water bath, maintain the above temperature for the required reaction time, cool it to room temperature, and rotary evaporate the amino acid strontium solution to 1 / 10 of the original volume. Transfer 0.5ml of the above concentrate to a centrifuge tube, add 8ml of anhydrous ethanol, shake for 10min, and centrifuge at 9000r / min for 10min. After separating the supernatant, add 8ml of anhydrous ethanol to the precipitate, centrifuge at 9000r / min for 10min, discard the supernatant, and precipitate the strontium content to be measured.

[0023] Table 1 Orthogonal test table L9 (34) - Batch 1

[0024]

[0025] Note: The amino acid solution is 0.1 mol / L.

[0026] The data were collated and statistically analyzed using SAS, EXCEL and other software.

[0027] Example 2

[0028] The difference between this embodiment and embodiment 1 is that the orthogonal experimental design is optimized based on the analysis results of embodiment 1: the second batch of experimental scheme: increase the coordination ratio of amino acids and metal ions, reduce the reaction temperature, widen the reaction time range, and redesign the 4-factor 3-level orthogonal experiment L9 (34). The experimental orthogonal table is shown in Table 2.

[0029] A 0.2 mol / L amino acid solution was prepared, and the remaining test steps were the same as those in Example 1.

[0030] Table 2 Orthogonal test table L9 (34) - Batch 2

[0031]

[0032] Note: The second batch of test amino acid solutions are 0.1 mol / L and 0.2 mol / L.

[0033] The data were collated and statistically analyzed using SAS, EXCEL and other software.

[0034] Example 3

[0035] The present embodiment is the same as Example 2. The difference between this embodiment and Example 2 is that the reaction conditions are adjusted according to the results of Example 2, and the experiment is redesigned: the third batch of test plan: the coordination ratios of amino acid to metal ion are selected as 4:1, 5:1 and 6:1; the pH values ​​are 6 and 7; the reaction temperatures are 40°C, 55°C and 70°C; the reaction time is 30min and 60min; when concentrating the strontium amino acid solution, rotary evaporation and heating are selected to screen the concentration method of the strontium amino acid solution, and the optimal chelating conditions of the strontium amino acid obtained by the screening are verified again.

[0036] Table 3 Amino acid strontium chelation test design - Batch 3

[0037]

[0038] Note: The amino acid solution in the third batch of tests was 0.2 mol / L.

[0039] The data were collated and statistically analyzed using SAS, EXCEL and other software.

[0040] Example 4

[0041] This example is used to determine the effect of different leaching agents on the leaching effect of strontium amino acids.

[0042] Pipette 0.5 ml of amino acid strontium concentrate into a centrifuge tube, add 8 ml of anhydrous ethanol and anhydrous methanol respectively, shake for 10 minutes, and centrifuge at 9000 r / min for 10 minutes. After separating the supernatant, add 8 ml of anhydrous ethanol and anhydrous methanol to the precipitate, centrifuge at 9000 r / min for 10 minutes, discard the supernatant, and precipitate the strontium content to be measured.

[0043] The prior art indicates that amino acid metal ion chelates are almost insoluble in organic solvents. In this embodiment, methanol and ethanol are selected as leaching agents to screen suitable organic solvents so that the solubility of amino acid strontium in the organic solvent is minimized. As can be seen from Table 4, the amino acid strontium product has the lowest solubility in anhydrous ethanol and the best leaching effect.

[0044] Table 4 Effect of different extractants on the chelation rate of strontium amino acid

[0045]

[0046] Example 5

[0047] This example is used to study the effect of different concentrations of amino acid solutions on the chelation rate of amino acid strontium

[0048] In the amino acid chelate metal ion test, the concentration of the amino acid solution in the prior art is generally 0.1mol / L, and the specific concentration is related to the solubility of the amino acid powder used. In this test, amino acid solutions with concentrations of 0.1mol / L and 0.2mol / L are set respectively to screen the appropriate amino acid solution concentration. As can be seen from Table 6, when the amino acid solution is 0.2mol / L, the overall amino acid strontium chelation rate is higher than that of 0.1mol / L, and the cost is also lower. (In the first batch of tests, a concentration of 0.3mol / L amino acid was tried, and it was found that the amino acid solution was turbid and unclear at this concentration).

[0049] Table 5 Effect of different amino acid solution concentrations on amino acid strontium chelation rate

[0050]

[0051] As can be seen from Table 6, the influence ranking and F value of the first two tests in Example 1 show that the coordination ratio of amino acid to metal ion has the greatest influence on the chelation rate, and the theoretical optimal level is 3 levels, which indicates that the optimal coordination ratio is ≥3:1, and the subsequent coordination ratio needs to be increased. The theoretical optimal reaction temperature is 70°C at level 1, which indicates that the optimal chelation temperature is ≤70°C, and this condition can be lowered in subsequent tests. The remaining two optimal conditions were not screened out in the first batch of two tests, which is related to the low coordination ratio of the first batch of experimental design and the excessive influence of the coordination ratio factor on the chelation rate.

[0052] Table 6 Theoretical optimal conditions and influence ranking of chelation reaction

[0053]

[0054] As shown in Table 7, the SAS analysis results of the amino acid strontium chelation rate in Example 2;

[0055] From the F values ​​of the second batch of two tests in Example 2, it can be seen that the influence of each condition is relatively close, which is conducive to screening out the best conditions. The best conditions after screening are: coordination ratio 5:1 or 4:1, pH value 6-7, reaction temperature 55°C, reaction time 60min. According to the results of this test, the third batch of tests was reset to verify the best chelating conditions of amino acid strontium obtained by screening.

[0056] Table 7 Theoretical optimal conditions and influence ranking of chelation reaction

[0057]

[0058] As shown in Table 8, the SAS analysis results of the amino acid strontium chelation rate in Example 3;

[0059] In Example 3, the third batch of two tests selected two concentration methods: rotary evaporation and heating concentration. As can be seen from the table below, the two concentration methods are not much different, but heating concentration is the most commonly used concentration method in factory production, and no additional equipment is required. In addition, it can be seen that the amino acid strontium chelation rate of treatment 3, treatment 4 and treatment 8 is high and relatively stable. The optimal chelation conditions for amino acid strontium are coordination ratios of 4:1, 5:1 or 6:1; pH value between 6 and 7; reaction temperature 40°C, 55°C; reaction time 60min. The specific implementation conditions can be selected within the optimal range according to cost and equipment characteristics.

[0060] Table 8 Theoretical optimal conditions and influence ranking of chelation reaction

[0061]

[0062] It is easy to understand that those skilled in the art can combine, split, reorganize, etc. the embodiments of the present application to obtain other embodiments based on one or several embodiments provided in the present application, and these embodiments do not exceed the protection scope of the present application.

[0063] The present invention and its implementation methods are described schematically above, and the description is not restrictive. The embodiments shown in the embodiments are only part of the implementation methods of the present invention, and the actual structure is not limited thereto. Therefore, if a person skilled in the art is inspired by the embodiments and designs a structure and an implementation method similar to the technical solution without creativity without departing from the purpose of the invention, they should all fall within the protection scope of the present invention.

Claims

1. A method for preparing strontium amino acid, It is characterized in that It is prepared by chelating a composite amino acid and strontium chloride, specifically comprising: Step S1, prepare 0.2 mol / L amino acid solution and heat to the designed temperature of 40°C or 55°C; Step S2, after the amino acid solution is stabilized at the designed temperature, adjusting the pH value of the amino acid solution to 6-7; Step S3, slowly adding the pre-prepared strontium chloride solution into the amino acid solution and mixing them to perform a chelation reaction to obtain an amino acid strontium solution; the concentration of the strontium chloride solution is 3 / 5 mol / L; and the reaction time of the chelation reaction is 60 min; Step S4, concentrating the amino acid strontium solution obtained in step S3 to 1 / 8-1 / 10 of the original volume by rotary evaporation or heating; Step S5: extracting the strontium amino acid using an extractant, wherein the extractant is anhydrous ethanol.

2. A method for preparing strontium amino acid according to claim 1, It is characterized in that The coordination ratio of the amino acid to the strontium ion is ≥3:

1.

3. A method for preparing strontium amino acid according to claim 2, It is characterized in that The coordination ratio is 4:1, 5:1 or 6:

1.

4. A method for preparing strontium amino acid according to claim 1, It is characterized in that The reaction temperature of the chelating reaction is ≤70°C.

5. A method for preparing strontium amino acid according to claim 1, It is characterized in that The substances for adjusting pH in step S2 are sodium hydroxide and hydrochloric acid.

Citation Information

Patent Citations

  • Amino acid chelated trace element fertilizer and preparation method thereof

    CN114292146A

  • Feed additive amino acid chelated strontium as well as preparation method and application thereof

    CN117586137A