Hyperbranched polyamide ethyl acrylate demulsifier as well as preparation method and application thereof
Through the preparation of hyperbranched polyamide ethyl acrylate demulsifier, the problem of non-flowing emulsions produced in formation pore throats during the oil and gas collection process is solved, oil-water separation and emulsion pollution cleaning are achieved, improving oil and gas development efficiency and reducing costs. cost.
Patent Information
- Application Number
- CN202310353353.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-04
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-04-04
AI Technical Summary
During the process of oil and gas collection and reservoir development, a large amount of non-flowing emulsion is produced in the formation pore throats, resulting in reservoir water lock and reduction of well production, increasing production costs.
Hyperbranched polyamide ethyl acrylate demulsifier is used and prepared through specific synthesis routes and process steps, including the use of raw materials such as diglycolamine, maleic anhydride and triethylamine for amidation and esterification reactions to form a Highly surface active and adaptable hyperbranched polyamide ethyl acrylate demulsifier.
The demulsifier can effectively separate oil and water, reduce the non-fluidity of emulsion, extend equipment life, increase oil and gas well production, reduce development costs, and is cheap, low-toxic, and highly adaptable.
Smart Images

Figure BDA0004162510400000011 
Figure BDA0004162510400000031 
Figure BDA0004162510400000032
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of demulsifier preparation, in particular to a hyperbranched polyamide ethyl acrylate demulsifier and a preparation method and application thereof. Background Art
[0002] With the gradual acceleration of oil development and the development of tertiary oil recovery technology, the water content of oil and gas produced fluids continues to increase, and the amount of O / W emulsions to be processed has increased dramatically. At the same time, the tertiary oil recovery process, the oil transportation process, microbial action, dirty oil and ground crude oil will cause the aged oil to produce viscous W / O emulsions, shortening the service life of equipment materials and making them difficult to handle. In the process of oil and gas field reservoir development, such as enhanced recovery, fracturing, drilling, etc., due to the immiscibility of the water-based phase and the oil phase, a large amount of non-flowing emulsions are produced in the pores near the wellbore, and the water lock and jamin damage of the reservoir are aggravated, resulting in reduced oil and gas well production or increased production (lifting) costs.
[0003] Therefore, it is urgent to design a hyperbranched polyamide ethyl acrylate demulsifier to achieve oil-water separation in the near-wellbore area and on the ground emulsion, so as to achieve the purpose of cleaning the near-wellbore formation and inhibiting emulsion pollution, thereby improving the efficiency of oil and gas development and reducing the cost of oil and gas development. It has high strategic significance for stable oil and gas production and environmental protection technology. Summary of the invention
[0004] The invention provides a hyperbranched polyamide ethyl acrylate demulsifier, a preparation method and an application thereof, which overcome the deficiencies of the above-mentioned prior art and can effectively solve the problems of a large amount of non-flowing emulsions generated in the pore throats of the formations during oil production, fracturing and reservoir development, aggravated damage of reservoir water lock and Jamin effect, thereby causing a reduction in the production of oil and gas wells or an increase in production (lifting) costs.
[0005] One of the technical solutions of the present invention is achieved by the following measures: a hyperbranched polyamide ethyl acrylate demulsifier, the structural formula is:
[0006]
[0007] The following is a further optimization and / or improvement of one of the above-mentioned technical solutions:
[0008] The above-mentioned preparation is carried out according to the following steps: the first step is to add the required amount of diethylene glycol amine, maleic anhydride and excess triethylamine into a reaction container, mix them, and react at a constant temperature to obtain a crude product of diethylene glycol difumaric acid amide; the second step is to wash the crude product of diethylene glycol difumaric acid amide with dilute hydrochloric acid and rotary evaporate it, collect the liquid phase, and purify it by column chromatography to obtain purified diethylene glycol difumaric acid amide; the third step is to add a solvent to the required amount of diethylene glycol difumaric acid amide after purification and stir it until it is completely mutually soluble, then add a required amount of catalyst, react under negative pressure, and after the reactant is cooled, remove the solvent and catalyst to obtain a reaction product; the fourth step is to add excess diethylene glycol amine and triethylamine to the reaction product, and then react at a constant temperature, and after the reaction is cooled and concentrated, a light yellow viscous liquid is obtained, namely, a hyperbranched polyamide ethyl acrylate demulsifier.
[0009] In the first step, the molar ratio of diglycolamine to maleic anhydride is 1:2.1.
[0010] In the first step above, the isothermal reaction temperature is room temperature and the reaction time is 5 h.
[0011] In the third step, the solvent is N,N-dimethylformamide, and 50 mL of N,N-dimethylformamide is added to every 0.05 mol of purified diethylene glycol difumaric acid amide.
[0012] In the third step, the catalyst is p-toluenesulfonic acid, and 0.02 mol of p-toluenesulfonic acid is added to every 0.05 mol of purified diethylene glycol difumaric acid amide.
[0013] In the third step, the reaction temperature is 130°C and the reaction time is 10 h.
[0014] In the fourth step, the isothermal reaction temperature is 50°C and the reaction time is 5.5h.
[0015] The second technical solution of the present invention is achieved by the following measures: a preparation method of a hyperbranched polyamide ethyl acrylate demulsifier, which is carried out according to the following steps: the first step is to add a required amount of diglycolamine, maleic anhydride and excess triethylamine into a reaction container, mix them, and react at a constant temperature to obtain a crude product of diethylene glycol difumaric acid amide; the second step is to wash the crude product diethylene glycol difumaric acid amide with dilute hydrochloric acid and rotary evaporate it, collect the liquid phase, and purify it by column chromatography to obtain purified diethylene glycol difumaric acid amide; the third step is to add a solvent to the purified required amount of diethylene glycol difumaric acid amide and stir it until it is completely mutually soluble, then add a required amount of catalyst, react under negative pressure, and after the reactant is cooled, remove the solvent and catalyst to obtain a reaction product; the fourth step is to add an excess of diglycolamine and triethylamine to the reaction product, and then react at a constant temperature, and after the reaction is cooled and concentrated, a light yellow viscous liquid is obtained, namely, the hyperbranched polyamide ethyl acrylate demulsifier.
[0016] The third technical solution of the present invention is achieved through the following measures: application of a hyperbranched polyamide ethyl acrylate demulsifier in the elimination of emulsification damage near the wellbore area of oil and gas reservoirs and oil-water separation of produced fluid.
[0017] The synthetic raw materials of the present invention are cheap and low in toxicity, and have strong adaptability to the temperature, water content and viscosity of crude oil emulsion. The preparation process is simple, the cost is low and the demulsification effect is good. It is a new technical approach to solve the pollution of formation emulsion. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Attached Figure 1 It is the infrared spectrum of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention.
[0019] Attached Figure 2 The figure is a relationship diagram between the surface tension and concentration of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention.
[0020] Attached Figure 3 This is a graph showing the effect of demulsifier content on emulsion dehydration rate in a static demulsification experiment of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention.
[0021] Attached Figure 4 This is a graph showing the effect of temperature on the dehydration rate of the emulsion in a static demulsification experiment of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention.
[0022] Attached Figure 5 This is a graph showing the effect of the water content of the emulsion on the dehydration rate of the emulsion in a static demulsification experiment of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention.
[0023] Attached Figure 6 This is a graph showing the effect of crude oil viscosity on the dehydration rate of the emulsion in a static demulsification experiment of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention.
[0024] Attached Figure 7 This is a graph showing the dehydration rate of emulsions with different demulsifiers in a static demulsification experiment of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention. DETAILED DESCRIPTION
[0025] The present invention is not limited by the following embodiments, and the specific implementation method can be determined according to the technical scheme of the present invention and the actual situation. Unless otherwise specified, the various chemical reagents and chemicals mentioned in the present invention are all chemical reagents and chemicals known and used in the prior art. Normal temperature and room temperature in the present invention generally refer to a temperature of 15°C to 25°C, and are generally defined as 25°C.
[0026] The present invention will be further described below in conjunction with embodiments:
[0027] Example 1: The hyperbranched polyamide ethyl acrylate demulsifier has the structural formula:
[0028]
[0029] The synthetic route of hyperbranched polyacetamide ethyl acrylate (P-DAEA) in the present invention is as follows:
[0030]
[0031] Wherein, DGA is diglycolamine, TEA is triethylamine, TsOH is p-toluenesulfonic acid, and P-DAEA is the target product hyperbranched poly(acetamide ethyl acrylate).
[0032] Embodiment 2: As the optimization of the above embodiment, it is prepared according to the following steps: the first step is to add the required amount of diethylene glycol amine, maleic anhydride and excess triethylamine into a reaction vessel, mix them, and react at a constant temperature to obtain a crude product of diethylene glycol difumaramide; the second step is to wash the crude product diethylene glycol difumaramide with dilute hydrochloric acid and rotary evaporate it, collect the liquid phase, and purify it by column chromatography to obtain purified diethylene glycol difumaramide; the third step is to add a solvent to the required amount of diethylene glycol difumaramide after purification and stir until it is completely miscible, then add a required amount of catalyst, react under negative pressure, and after the reactant is cooled, remove the solvent and catalyst to obtain a reaction product; the fourth step is to add an excess of diethylene glycol amine and triethylamine to the reaction product, and then react at a constant temperature. After the reaction is cooled and concentrated, a light yellow viscous liquid is obtained, i.e., a hyperbranched polyamide ethyl acrylate demulsifier.
[0033] In the present invention, diglycolamine is selected because it not only has certain surface activity, but also can provide amino groups and hydroxyl groups at the same time, and can undergo amidation and esterification reactions; and it has low cost, good water solubility, good wettability, strong reaction activity, and is a good polymerization raw material.
[0034] Maleic anhydride can be used for amidation reaction with primary amines, with strong reactivity and low boiling point. Its synthesis and processing costs are low, and it is very suitable as a raw material for oil and gas field chemicals. Maleic anhydride and diglycolamine are amidated to provide the carboxyl group required for esterification reaction for the hyperbranched structure.
[0035] In the first step of the preparation process of the hyperbranched polyamide ethyl acrylate demulsifier, triethylamine is selected as an acid-binding agent and catalyst because of its low cost, high catalytic efficiency, and ability to bind to carboxyl groups to avoid the inability of the reaction to proceed due to the protonation of amines by carboxylic acids; excess triethylamine can be washed with dilute hydrochloric acid to become weakly acidic, is insoluble in water, and can be easily removed after rotary evaporation.
[0036] Example 3: As an optimization of the above example, in the first step, the molar ratio of diglycolamine to maleic anhydride is 1:2.1.
[0037] Example 4: As an optimization of the above example, in the first step, the isothermal reaction temperature is room temperature and the reaction time is 5 hours.
[0038] In the present invention, in the first step of the preparation process of the hyperbranched polyamide ethyl acrylate demulsifier, the temperature of the isothermal reaction is controlled at room temperature, so that maleic anhydride can react with the primary amine under mild conditions for amidation, and the reaction time is controlled at 5 hours to ensure that the reactants react fully. If the reaction time is less than 5 hours, the reaction is insufficient and the conversion rate is low. If the reaction time is greater than 5 hours, the conversion rate does not change significantly. Considering the conversion rate, time cost and energy consumption issues comprehensively, the reaction time at room temperature is selected to be 5 hours.
[0039] Example 5: As an optimization of the above example, in the third step, the solvent is N,N-dimethylformamide (DMF), and 50 mL of N,N-dimethylformamide is added to every 0.05 mol of purified diethylene glycol difumaric acid amide.
[0040] Example 6: As an optimization of the above example, in the third step, the catalyst is p-toluenesulfonic acid, and 0.02 mol of p-toluenesulfonic acid is added to every 0.05 mol of purified diethylene glycol difumaramide.
[0041] Example 7: As an optimization of the above example, in the third step, the reaction temperature is 130°C and the reaction time is 10 h.
[0042] In the present invention, in the third step of the preparation process of the hyperbranched polyamide ethyl acrylate demulsifier, p-toluenesulfonic acid is selected as a catalyst for the hyperbranching (esterification) reaction because it has low cost and high catalytic efficiency; the constant temperature of 130° C. under negative pressure conditions is because the esterification reaction needs to be carried out at high temperature, and the negative pressure reduces the corresponding reaction activation energy at the reaction temperature, and the conversion rate does not change significantly above 130° C. and is prone to produce by-products, and the esterification reaction cannot be carried out below the temperature; the reaction time is less than 10 hours, the reaction is insufficient and the conversion rate is low, and the reaction time is greater than 10 hours, and the conversion rate does not change significantly. Considering the conversion rate, time cost and energy consumption issues comprehensively, the reaction time at room temperature is selected to be 10 hours.
[0043] Example 8: As an optimization of the above example, in the fourth step, the isothermal reaction temperature is 50°C and the reaction time is 5.5h.
[0044] In the present invention, in the fourth step of the preparation process of the hyperbranched polyamide ethyl acrylate demulsifier, the optimal reaction temperature of 50° C. and the optimal reaction time of 5.5 h are selected, which can reduce the by-products and reduce the raw material and reaction costs.
[0045] Embodiment 9: The preparation method of the hyperbranched polyamide ethyl acrylate demulsifier is carried out according to the following steps: the first step is to add the required amount of diglycolamine, maleic anhydride and excess triethylamine into a reaction container, mix them, and react at a constant temperature to obtain a crude product of diethylene glycol difumaramide; the second step is to wash the crude product diethylene glycol difumaramide with dilute hydrochloric acid and rotary evaporate it, collect the liquid phase, and purify it by column chromatography to obtain purified diethylene glycol difumaramide; the third step is to add a solvent to the required amount of diethylene glycol difumaramide after purification and stir until it is completely mutually soluble, then add a required amount of catalyst, react under negative pressure, and after the reactant is cooled, remove the solvent and catalyst to obtain a reaction product; the fourth step is to add excess diglycolamine and triethylamine to the reaction product, and then react at a constant temperature, and after the reaction is cooled and concentrated, a light yellow viscous liquid is obtained, i.e., a hyperbranched polyamide ethyl acrylate demulsifier.
[0046] Example 10: Application of the hyperbranched polyamide ethyl acrylate demulsifier in eliminating emulsification damage near the wellbore area of oil and gas reservoirs and in oil-water separation of produced fluid.
[0047] Example 11: The hyperbranched polyamide ethyl acrylate demulsifier is prepared according to the following steps: the first step is to mix 2.10g of diglycolamine, 4.20g of maleic anhydride and excess triethylamine in a three-necked glass flask, and carry out constant temperature reaction for 5h under stirring at room temperature. The reaction is carried out under a nitrogen atmosphere throughout the process to ensure the anaerobic condition of the reaction, and obtain a light yellow liquid, i.e., a crude product of diethylene glycol difumaric acid amide; the second step is to wash the crude product of diethylene glycol difumaric acid amide with dilute hydrochloric acid for 2 to 3 times, and then use a rotary evaporator to evaporate at a negative pressure of 40°C, collect the liquid phase, and use a silica gel column for chromatographic separation (the eluent is chloroform and methanol in a ratio of 10:1), and then evaporate again after elution to obtain a purified product. The purified diethylene glycol difumaric acid amide was added with 50 mL of DMF solvent into 11.35 g of diethylene glycol difumaric acid amide, placed in a flask and stirred until completely dissolved, and then 0.02 mol of p-toluenesulfonic acid was added, and the reaction was carried out at 130° C. under negative pressure for 10 hours. After the reactant was cooled, the solvent DMF and the catalyst p-toluenesulfonic acid were removed by rotary evaporation to obtain a reaction product. The fourth step was to add excess diglycolamine and triethylamine to 11.2 g of the reaction product, and the reaction was carried out at a constant temperature of 50° C. for 5.5 hours. After the reaction was cooled, it was washed with dilute hydrochloric acid twice and rotary evaporated to obtain a light yellow viscous liquid, i.e., a hyperbranched polyamide ethyl acrylate demulsifier.
[0048] The diethylene glycol difumaric acid amide and the hyperbranched polyamide ethyl acrylate demulsifier (P-DAEA for short) obtained in Example 11 were tested as follows:
[0049] 1. Infrared characterization
[0050] Take a small amount of dried KBr and press it into tablets using an infrared tablet press; smear the P-DAEA prepared in Example 11 on the KBr thin slice and dry it; use a WQF-520 infrared spectrometer to perform infrared spectrum scanning and collect instrument background. The infrared spectrum of the multifunctional cleaning agent is as follows: Figure 1 shown.
[0051] from Figure 1 It can be seen that at 3500cm -1 The absorption peak near is the stretching vibration peak of -OH; at 2900cm -1 Up to 3200cm -1 The absorption peak near is the stretching vibration peak of amide; at 1680cm -1 Up to 1630cm -1 It is the amide I band; at 1570cm -1 Up to 1510cm -1 and 1335cm -1 Up to 1200cm -1 The absorption peaks nearby are the amide II band and amide III band caused by the coupling between NH and CN; at 1150cm -1 The nearby absorption peak is the stretching vibration peak of -O-, and the characteristic absorption peaks of each monomer are all presented in the spectrum, proving that the target product has been synthesized.
[0052] 2. Determination of surface tension and critical micelle concentration (cmc) of P-DAEA
[0053] P-DAEA aqueous solutions with concentration gradients of 0.01 mg / L, 0.1 mg / L, 1 mg / L, 100 mg / L, 300 mg / L, 500 mg / L, 550 mg / L, 600 mg / L, 650 mg / L, 700 mg / L, 750 mg / L, 800 mg / L, 1000 mg / L and 10000 mg / L were prepared respectively, and the surface tension was measured using the German KRUSSDSA30S interface parameter integrated measurement system. The scatter plot of the experimental results is shown in Figure 2, and the curve is fitted to determine the critical micelle concentration. Figure 5 shown.
[0054] Figure 5 for The inflection point coordinates are (650,32.5), which is the function point corresponding to the critical micelle, and the corresponding surface tension is 32.5mN / m. When the P-DAEA concentration is higher than 650mg / L, the surface tension remains almost unchanged, so the critical micelle concentration is 32.5mN / m. A lower critical micelle concentration corresponds to a lower dosage, higher surface activity, and a stronger ability to reduce the interfacial tension of the oil-water surface in the emulsion and destroy the oil-water interface.
[0055] 3. Determination of turbidity point, HLB value (hydrophile-lipophile balance) and RSN (correlated activity coefficient) of P-DAEA
[0056] The solubility of non-ionic surfactants in aqueous solution decreases with increasing temperature. When the temperature reaches a certain value, turbidity appears. After standing or centrifugation, two liquid phases can be obtained. This temperature is called the turbidity point of the surfactant. Weigh 0.5g of P-DAEA (accurate to 0.01g), add 100mL of deionized water, and stir until completely dissolved. Measure 15mL of the above P-DAEA solution, place it in a test tube, insert a thermometer, place the test tube in a water bath and heat it. Use a thermometer to gently stir until the solution is completely turbid (the solution temperature does not exceed 10°C of the turbidity temperature), stop heating, and the test tube is still in the beaker. Slowly cool down under the stirring of the thermometer, and record the temperature at which the turbidity completely disappears. Repeat the test twice, and the difference between the parallel results is no more than 0.5°C. The arithmetic mean is the turbidity point of P-DAEA. And compare it with the commonly used block polyether demulsifier.
[0057] The HLB value is called the hydrophilic-hydrophobic balance value, also known as the water-oil ratio. HLB is equal to the hydrophilicity of the hydrophilic group / the lipophilicity of the lipophilic group. The larger the HLB value, the stronger the hydrophilicity, and the smaller the HLB value, the stronger the lipophilicity. Its size is related to the basic properties of the surfactant, such as the surface (interface) tension, adsorption on the interface, emulsification and emulsion stability, dispersibility, solubility, and detergency. The HLB value is generally between 1 and 40, and the hydrophilic-lipophilic turning point HLB is 10. Less than 10 is lipophilic, and greater than 10 is hydrophilic. And compared with the commonly used block polyether demulsifier. The HLB calculation formula based on non-ionic surfactants is as follows:
[0058] HLB=7+4.02log(1 / cmc)
[0059] RSN value is also used to evaluate the lipophilicity and hydrophilicity of surfactants. The larger the value, the stronger the hydrophilicity of P-DAEA, and the smaller the value, the stronger the lipophilicity of P-DAEA. Prepare a certain amount of toluene (volume fraction is 2.6 vol%) ethylene glycol dimethyl ether solution as the RSN value determination solution. Dissolve 1g of sample in 30mL of RSN determination solution. The volume of deionized water consumed is the RSN value of P-DAEA. Take the average value of three measurements. And compare with commonly used block polyether demulsifiers.
[0060] The cloud points, HLB values and RSN values of P-DAEA and block polyether are shown in Table 1 below.
[0061] As can be seen from Table 1, P-DAEA exhibits a relatively high HLB value, indicating that it is a hydrophilic surfactant that can effectively adsorb water molecules in W / O, destroy the water molecule layer of O / W, and have good dehydration performance for the emulsion; the turbidity point of P-DAEA indicates that its hyperbranched molecules have more hydrophilic groups that can adsorb water molecules by hydrogen bonding force, and have good dehydration performance; the higher the RSN value, the stronger the hydrophilicity of P-DAEA, and the stronger its dehydration and demulsification ability for the emulsion.
[0062] 4. Static demulsification experiment of hyperbranched polyamide ethyl acrylate demulsifier
[0063] According to the petroleum and natural gas industry standard SY / T5281-2000 of the People's Republic of China "Test Method for Performance of Crude Oil Demulsifier (Bottle Test Method)", a static demulsification experiment of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention is designed, and the specific implementation scheme is as follows.
[0064] Preparation method of crude oil emulsion: accurately weigh 500g crude oil and 500g water and place them in a beaker, and preheat them at a constant temperature of 40°C for 30 minutes. Put the preheated crude oil and water mixed solution into the HT-2 high-speed mixer at once, and stir at 3000rpm for 30 minutes to complete the preparation of uniform water-containing crude oil emulsion (water content 50%). The crude oil emulsion used in the experiment is used as soon as it is prepared, ensuring that fresh crude oil emulsion is used in each experiment to prevent the emulsion from aging due to long preparation time.
[0065] Preparation method of the test solution of hyperbranched polyamide ethyl acrylate demulsifier: Accurately weigh a quantitative P-DAEA sample in a beaker, transfer it to a volumetric flask, dilute it to the scale with deionized water, and shake it well to make the mass concentration of the P-DAEA aqueous solution 1g / 100mL (i.e. 10000mg / L).
[0066] (1) Effect of P-DAEA content on demulsification rate of crude oil emulsion
[0067] The above 70mL crude oil emulsion (water content 50%) was placed in a 100mL stoppered graduated test tube, preheated in a constant temperature water bath (40°C) for 30min, and a quantitative amount of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention was added to ensure that the P-DAEA concentration was 10mg / L, 20mg / L, 40mg / L, 60mg / L, 80mg / L, 100mg / L, 200mg / L, 500mg / L, 1000mg / L, and 10000mg / L, respectively. The tube was shaken 200 times (100 times with the left and right hands respectively), with an amplitude greater than 20cm, and then placed in a constant temperature water bath, and the volume of water removed at different times was recorded, and the crude oil dehydration rate was calculated from the volume of water removed. The experimental results are as follows: Figure 3 shown.
[0068] Figure 3 It can be seen that when the P-DAEA content of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention is higher than 40 mg / L, the dehydration rate of the crude oil emulsion is significantly improved, and the dehydration rate is greater than 50% within 20 minutes; when the P-DAEA content is greater than 80 mg / L, the dehydration rate of the crude oil emulsion is as high as 65% within 20 minutes, and the dehydration rate is greater than 90% within 100 minutes. As the P-DAEA content increases, the greater the adsorption amount on the oil-water interface of the emulsion, the stronger the interface molecule displacement effect, the greater the ability to destroy the oil-water interface, and the higher the dehydration rate. Therefore, when the hyperbranched polyamide ethyl acrylate demulsifier of the present invention has an effective content of 80 mg / L, it can meet the demulsification demand of crude oil emulsion at the oil and gas field development site.
[0069] (2) Effect of temperature on the demulsification rate of crude oil emulsion
[0070] The above 70 mL crude oil emulsion (water content 50%) was placed into a 100 mL stoppered graduated test tube, and placed in different constant temperature water baths for preheating for 30 min, at temperatures of 30°C, 40°C, 50°C, 60°C, 70°C, 80°C, and 90°C, respectively. A quantitative amount of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention was added to ensure that the P-DAEA concentration was 80 mg / L, and the mixture was shaken 200 times (100 times for each hand), with an amplitude greater than 20 cm, and then placed in a constant temperature water bath (temperature the same as above), and the volume of water removed at different times was recorded, and the crude oil dehydration rate was calculated from the volume of water removed. The experimental results are as follows: Figure 4 shown.
[0071] Figure 4 It can be seen that the hyperbranched polyamide ethyl acrylate demulsifier of the present invention exhibits a good dehydration rate of crude oil emulsion at 30°C to 80°C, and the dehydration rate can finally reach more than 94% within 120 minutes. When the temperature is higher than 70°C, the dehydration rate increases significantly, because the molecular motion is intense at high temperature, which accelerates the interaction between P-DAEA molecules and the oil-water interface. Increasing the temperature is more conducive to the dehydration rate of the hyperbranched polyamide ethyl acrylate demulsifier on crude oil emulsion.
[0072] (3) Effect of emulsion water content on emulsion dehydration rate
[0073] 70 mL of freshly prepared crude oil emulsion (water content of 30%, 40%, 50%, 60%, 70%) were placed in 100 mL stoppered graduated test tubes, and placed in a constant temperature water bath (40°C) for preheating for 30 min. A quantitative amount of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention was added to ensure that the P-DAEA concentration was 80 mg / L, and the mixture was shaken 200 times (100 times for each hand), with an amplitude greater than 20 cm, and then placed in a constant temperature water bath (temperature as above), and the volume of water removed at different times was recorded, and the crude oil dehydration rate was calculated from the volume of water removed. The experimental results are as follows: Figure 5 shown.
[0074] Figure 5 It can be seen that the higher the water content of the crude oil emulsion, the higher the dehydration rate of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention. When the water content of the crude oil emulsion is higher than 50%, the emulsion is of O / W type, the P-DAEA molecule is a hydrophilic molecule, has a strong ability to act at the oil-water interface, and has a strong ability to replace the outer water molecules of the oil droplets, which can effectively destroy the oil-water interface and achieve the purpose of demulsification. At the same time, for low-water-content crude oil emulsions, i.e. W / O emulsions, the hyperbranched polyamide ethyl acrylate demulsifier of the present invention can still achieve a dehydration rate of 90% within 100 minutes. In summary, the hyperbranched polyamide ethyl acrylate demulsifier of the present invention has strong adaptability to the type of crude oil emulsion and can meet the needs of eliminating damage to crude oil emulsification at the oil and gas field site.
[0075] (4) Effect of crude oil viscosity on emulsion dehydration rate
[0076] According to the viscosity of ground crude oil, it can be divided into low-viscosity crude oil when μOS < 10mPa·s, medium-viscosity crude oil when μOS = 10mPa·s to 100mPa·s, and high-viscosity crude oil when μOS > 100mPa·s. The low-, medium-, and high-viscosity test crude oils in the present invention are crude oils from different layers in the Mahu area of Xinjiang, my country.
[0077] 70 mL of freshly prepared crude oil emulsion (the viscosity of crude oil is 8.6 mPa·s, 54.5 mPa·s, 189.5 mPa·s, 307.8 mPa·s) were placed in 100 mL stoppered graduated test tubes, and placed in a constant temperature water bath (40°C) for preheating for 30 min. A quantitative amount of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention was added to ensure that the P-DAEA concentration was 80 mg / L, and the mixture was shaken 200 times (100 times for each hand), with an amplitude greater than 20 cm, and then placed in a constant temperature water bath (temperature as above), and the volume of water removed at different times was recorded, and the crude oil dehydration rate was calculated from the volume of water removed. The experimental results are as follows: Figure 6 shown.
[0078] Figure 6It can be seen that the lower the viscosity of crude oil, the higher the dehydration rate of the hyperbranched polyamide ethyl acrylate demulsifier of the present invention on the emulsion. This is because the lower the viscosity of crude oil, the lower the relative molecular weight of its organic hydrocarbons, the weaker the oil-water interface force formed, and the easier it is to be destroyed. At the same time, for heavy oil, the present invention still has a dehydration rate of more than 85% within 120 minutes, which can meet the demulsification of emulsions produced by most oil reservoirs.
[0079] (5) Dehydration rate of emulsions by different demulsifiers
[0080] Several demulsifiers commonly used in the market and oil and gas fields in my country were selected, including ionic demulsifiers and non-ionic demulsifiers, and compared with the hyperbranched polyamide ethyl acrylate demulsifier of the present invention under uniform test conditions. The basic information of the selected demulsifiers is shown in Table 2.
[0081] 70 mL of freshly prepared crude oil emulsion was placed in 100 mL stoppered graduated test tubes, and placed in a constant temperature water bath (40°C) for preheating for 30 min. A quantitative quaternary ammonium salt demulsifier, a carboxylate demulsifier, a chain block polyether demulsifier, a branched two-stage polyether demulsifier and the hyperbranched polyamide ethyl acrylate demulsifier of the present invention were added respectively to ensure that the concentration of the effective ingredient was 80 mg / L, and shaken 200 times (100 times for each hand), with an amplitude greater than 20 cm, and then placed in a constant temperature water bath (temperature as above), and the volume of water removed at different times was recorded, and the crude oil dehydration rate was calculated from the volume of water removed. The experimental results are as follows: Figure 7 shown.
[0082] Figure 7 It can be seen that the hyperbranched polyamide ethyl acrylate demulsifier of the present invention has the highest dehydration rate for crude oil emulsion compared with other types of products, and the dehydration rate increases faster over time than other types of products. This is because the hyperbranched molecular structure of the active ingredient P-DAEA in the hyperbranched polyamide ethyl acrylate demulsifier of the present invention has multiple hydrophilic groups, a large available area, and a more significant effect of breaking the oil-water interface. Anionic and cationic types may have electrostatic effects due to problems such as compatibility with crude oil, which reduces the effect of the active ingredient. Therefore, the hyperbranched polyamide ethyl acrylate demulsifier of the present invention has a fast dehydration rate for crude oil emulsion within 180 minutes, and has a significant dehydration effect, which can meet the requirements of the oil and gas field development site.
[0083] 5. Dynamic demulsification experiment of hyperbranched polyamide ethyl acrylate demulsifier
[0084] (1) Preparation of experimental fluid (base fluid)
[0085] Preparation method of hyperbranched polyamide ethyl acrylate demulsifier: accurately weigh 0.08 g of P-DAEA and dissolve it in deionized water, and make up to volume with a 1000 mL volumetric flask;
[0086] Preparation method of crude oil emulsion: accurately weigh 500g crude oil and 500g water and place them in a beaker, and preheat them at a constant temperature of 40°C for 30 minutes. Put the preheated crude oil and water mixed solution into the HT-2 high-speed mixer at once, and stir at 3000rpm for 30 minutes to complete the preparation of uniform water-containing crude oil emulsion (water content 50%). The crude oil emulsion used in the experiment is used as soon as it is prepared, ensuring that fresh crude oil emulsion is used in each experiment to prevent the emulsion from aging due to long preparation time.
[0087] (2) Core preparation
[0088] ①The core is taken from artificial core of sandstone and the processing is carried out according to the core analysis method of SY / T5336-2006.
[0089] ① Cut the core into a cylinder with a diameter of about 25 mm and a length of 1 to 1.5 times the diameter. Grind both end surfaces flat and make them perpendicular to the smooth cylindrical surface. Classify and retain the cut rock cuttings, write labels and store them properly.
[0090] ②Put the cut core in an oven at about 100℃ for drying. Weigh the core at regular intervals to confirm that it is completely dried if the weight does not change.
[0091] ③Evacuate the core and saturate it with 1.5% KCl brine.
[0092] (3) Core emulsification damage repair experiment:
[0093] A multifunctional core displacement experimental device was used to positively displace the sample at a temperature of 60°C with a displacement rate of 0.5 mL min -1 , measure the basic water phase permeability K1; then use crude oil emulsion (water content 50%) to displace 1.5PV to the core forward, record the pressure change; then use the repair fluid to displace 2PV to the core reversely, maintain the temperature, and let it stand for 0.5h; then the core is displaced forward with clean water again, and the oil phase permeability is measured. The experimental results are shown in Tables 3 and 4.
[0094] It can be seen from Tables 3 and 4 that the core permeability is reduced from 19.75 mD to 10.21 mD after the core is injected with crude oil emulsion. After the hyperbranched polyamide ethyl acrylate demulsifier of the present invention is injected, the permeability recovery rate is as high as 85.92%, thus indicating that the hyperbranched polyamide ethyl acrylate demulsifier of the present invention has good dynamic demulsification performance.
[0095] In summary, the synthetic raw materials of the present invention are cheap and low in toxicity, and have strong adaptability to the temperature, water content and viscosity of crude oil emulsions. The preparation process is simple, the cost is low and the demulsification effect is good. It is a new technical approach to solve the pollution of formation emulsions.
[0096] The above technical features constitute the embodiments of the present invention, which have strong adaptability and implementation effect. Non-essential technical features can be added or reduced according to actual needs to meet the requirements of different situations.
[0097] Table 1
[0098] name Cloud point(℃) HLB value RSN value P-DAEA 39.5 26.9 12.8 Block polyether 36.0 13.2 9.8
[0099] Table 2
[0100]
[0101] Table 3
[0102] Core number Dry weight / kg Pore volume / cm3 Permeability / mD Water injection pressure / MPa L-2357 0.103 16.4 19.75 0.129
[0103] Table 4
[0104]
Claims
1. A hyperbranched polyamide ethyl acrylate demulsifier, characterized in that The structural formula is:
2. The hyperbranched polyamide ethyl acrylate demulsifier according to claim 1, characterized in that The preparation is carried out according to the following steps: first, adding the required amount of diethylene glycol amine, maleic anhydride and excess triethylamine into a reaction container, mixing, and reacting at a constant temperature to obtain a crude product of diethylene glycol difumaric acid amide; second, washing the crude product of diethylene glycol difumaric acid amide with dilute hydrochloric acid and rotary evaporating, collecting the liquid phase, and purifying it by column chromatography to obtain purified diethylene glycol difumaric acid amide; The third step is to add a solvent to the purified required amount of diethylene glycol difumaric acid amide and stir until they are completely mutually dissolved, then add a required amount of catalyst, react under negative pressure, and after the reactant is cooled, remove the solvent and catalyst to obtain a reaction product; The fourth step is to add excess diglycolamine and triethylamine to the reaction product, and then carry out a constant temperature reaction. After the reaction is cooled and concentrated, a light yellow viscous liquid is obtained, namely, a hyperbranched polyamide ethyl acrylate demulsifier.
3. The hyperbranched polyamide ethyl acrylate demulsifier according to claim 2, characterized in that In the first step, the molar ratio of diglycolamine to maleic anhydride is 1:2.
1.
4. The hyperbranched polyamide ethyl acrylate demulsifier according to claim 2 or 3, characterized in that In the first step, the isothermal reaction temperature is room temperature and the reaction time is 5 h.
5. The hyperbranched polyamide ethyl acrylate demulsifier according to claim 2, 3 or 4, characterized in that In the third step, the solvent is N,N-dimethylformamide, and 50 mL of N,N-dimethylformamide is added to every 0.05 mol of purified diethylene glycol difumaric acid amide.
6. The hyperbranched polyamide ethyl acrylate demulsifier according to claim 2, 3, 4 or 5, characterized in that In the third step, the catalyst is p-toluenesulfonic acid, and 0.02 mol of p-toluenesulfonic acid is added to every 0.05 mol of purified diethylene glycol difumaramide.
7. The hyperbranched polyamide ethyl acrylate demulsifier according to claim 2 or 3 or 4 or 5 or 6, characterized in that In the third step, the reaction temperature was 130°C and the reaction time was 10 h.
8. The hyperbranched polyamide ethyl acrylate demulsifier according to claim 2 or 3 or 4 or 5 or 6 or 7, characterized in that In the fourth step, the isothermal reaction temperature was 50°C and the reaction time was 5.5 h.
9. A method for preparing a hyperbranched polyamide ethyl acrylate demulsifier according to claim 1 or 3 or 4 or 5 or 6 or 7 or 8, characterized in that The following steps are followed: first, adding the required amount of diethylene glycol amine, maleic anhydride and excess triethylamine into a reaction container, mixing, and reacting at a constant temperature to obtain a crude product of diethylene glycol difumaric acid amide; second, washing the crude product of diethylene glycol difumaric acid amide with dilute hydrochloric acid and rotary evaporating, collecting the liquid phase, and purifying it by column chromatography to obtain purified diethylene glycol difumaric acid amide; The third step is to add a solvent to the purified required amount of diethylene glycol difumaric acid amide and stir until they are completely mutually dissolved, then add a required amount of catalyst, react under negative pressure, and after the reactant is cooled, remove the solvent and catalyst to obtain a reaction product; The fourth step is to add excess diglycolamine and triethylamine to the reaction product, and then carry out a constant temperature reaction. After the reaction is cooled and concentrated, a light yellow viscous liquid is obtained, namely, a hyperbranched polyamide ethyl acrylate demulsifier.
10. Use of the hyperbranched polyamide ethyl acrylate demulsifier according to any one of claims 1 to 8 in eliminating emulsification damage near the wellbore area of oil and gas reservoirs and separating oil and water in produced fluid.
Citation Information
Patent Citations
Application of polyamidoamine hyperbranched polymer as demulsifying agent
CN105601941A
Hyper-branched macromolecular flocculation demulsifying agent for treating oil-containing high-salt industrial waste water, and preparation method and use method thereof
CN106279554A
Method for demulsification of oil-in-water type emulsion
CN109364530A
Method of using amphiphilic hyperbranched polyamides to demulsify oil-in-water emulsions
CN109575280A
Modified hyperbranched polyamidoamine polymer and preparation method thereof
CN111019127A