Display panel and display device

By covering at least two light panel units with each optical film on the display panel and performing deaeration treatment, the defect problem at the splicing gap is solved, the use and splicing of optical films is reduced, and the display effect and structure are improved. stability and reduced costs.

CN118781925APending Publication Date: 2024-10-15JIANGXI MTC VISUAL DISPLAY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410998159.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-10-15

Smart Images

  • Figure CN118781925A_ABST
    Figure CN118781925A_ABST
Patent Text Reader

Abstract

The invention discloses a display panel and a display device, and the display panel comprises a lamp panel which is provided with a light emitting side and comprises a plurality of lamp panel units which are spliced with one another; the at least one optical film covers the whole light emitting side; and each optical film covers at least two lamp panel units. Each optical film covers at least two lamp panel units, so that the display effect at the splicing gaps of the lamp panel units can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular, to a display panel and a display device. Background Art

[0002] Currently, some spliced ​​display panels, such as the display screens of televisions or all-in-one conference machines, are often spliced ​​together using multiple light board units.

[0003] In the related art, an independent film is provided on the light-emitting surface of each light panel unit. The light panel units are often spliced ​​after independent lamination, which requires high splicing accuracy. If the splicing gap and flatness of the light panel units do not meet the requirements, the film of the adjacent light panel units is prone to defects at the splicing gap, affecting the display effect. Summary of the invention

[0004] Some embodiments of the present application provide a display panel and a display device to improve the problem that defects are easily generated at the joint gaps of the membranes of adjacent light panel units.

[0005] As a first aspect of the present application, some embodiments of the present application provide a display panel, including:

[0006] A light board having a light emitting side and comprising a plurality of light board units spliced ​​to each other;

[0007] At least one optical film, covering the entire light-emitting side;

[0008] Wherein, each of the optical films covers at least two of the light panel units.

[0009] Optionally, in some embodiments of the present application, each of the light board units has a light emitting surface, and the light emitting surface of each of the light board units is flush with the light emitting surface of an adjacent light board unit.

[0010] Optionally, in some embodiments of the present application, each of the light board units further has a plurality of side surfaces connected to the light emitting surface and connected end to end along the circumference of the light board unit. For any two adjacent light board units, two oppositely arranged side surfaces of the two units abut against each other.

[0011] Optionally, in some embodiments of the present application, the thickness of the optical film ranges from 80 microns to 150 microns.

[0012] Optionally, in some embodiments of the present application, the number of the light panel units covered by each of the optical films ranges from 2 to 300.

[0013] Optionally, in some embodiments of the present application, the aspect ratio of the optical film ranges from 1.1 to 2.5.

[0014] Optionally, in some embodiments of the present application, the number of the optical film is one, and the format size of the optical film is the same as the format size of the light board.

[0015] Optionally, in some embodiments of the present application, the display panel includes a plurality of optical films, the plurality of optical films are spliced ​​together, and the format size of the plurality of optical films after splicing is the same as the format size of the light board.

[0016] Optionally, in some embodiments of the present application, at least some of the plurality of optical films have different sizes, and the size of the optical film located in the middle of the light board is larger than the size of the optical film located around the light board.

[0017] Optionally, in some embodiments of the present application, the optical film includes: an AG layer, a base layer and a back adhesive layer;

[0018] Wherein, the adhesive layer is bonded to the light-emitting side surface of the light board, and the base layer is sandwiched between the AG layer and the adhesive layer;

[0019] The thickness of the AG layer ranges from 5 microns to 10 microns; the thickness of the base layer ranges from 20 microns to 100 microns; and the thickness of the back adhesive layer ranges from 30 microns to 120 microns.

[0020] As a second aspect of the present application, some embodiments of the present application provide a display device, including the aforementioned display panel.

[0021] As a third aspect of the present application, some embodiments of the present application provide a method for manufacturing a display device, comprising the following steps:

[0022] Provide multiple light panel units;

[0023] A plurality of the light board units are spliced ​​into a light board, wherein the light board has a light emitting side;

[0024] Providing at least one optical film;

[0025] The optical film is attached to the light emitting side of the lamp panel so that each of the optical films covers at least two of the lamp panel units.

[0026] Optionally, in some embodiments of the present application, the following step is also included: installing the light panel to the box.

[0027] Optionally, in some embodiments of the present application, attaching the optical film to the light board so that each of the optical films covers at least two of the light board units includes:

[0028] A degassing process is performed between the optical film and the lamp panel unit at a preset pressure and a preset temperature.

[0029] Optionally, in some embodiments of the present application, the preset pressure and / or the preset temperature is proportional to the thickness of the optical film.

[0030] The beneficial effect of the present application is that by making each optical film cover at least two light board units, compared with the prior art, when the display panel size is constant, the number of optical films used can be reduced, thereby reducing the seams between the optical films to improve the display effect; at the same time, for multiple light board units covered by the same optical film, since there is no overlapping effect of the seams of the light board units and the seams of the optical films, it also helps to improve the display effect at the seams of the light board units. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] In the attached picture:

[0032] Figure 1 is a three-dimensional diagram of a display panel according to an embodiment of the present application;

[0033] Figure 2 is an exploded view of a display panel according to an embodiment of the present application;

[0034] Figure 3 is a partial exploded view of a light board in a display panel according to an embodiment of the present application;

[0035] Figure 4 is a cross-sectional view of a spliced ​​display panel in the prior art;

[0036] Figure 5 is a cross-sectional view of a display panel according to a first embodiment of the present application;

[0037] Figure 6 is a cross-sectional view of a display panel according to a second embodiment of the present application;

[0038] Figure 7 is a cross-sectional view of a display panel according to a third embodiment of the present application;

[0039] Figure 8 is a cross-sectional view of a display panel according to a fourth embodiment of the present application;

[0040] Fig. 9 is a cross-sectional view of a display panel according to a fifth embodiment of the present application;

[0041] Fig.10 yes Fig. 9 A magnified view of a portion of the image.

[0042] Fig.11is a stereoscopic diagram of a display device at a first viewing angle according to an embodiment of the present application;

[0043] Fig.12 is a stereoscopic diagram of a display device at a second viewing angle according to an embodiment of the present application;

[0044] Fig.13 is an exploded view of a display device according to an embodiment of the present application.

[0045] Description of reference numerals:

[0046] 100. Display panel;

[0047] 110, lamp board; 110a, light emitting side; 111, lamp board unit; 111a, side surface; 112, colloid;

[0048] 120, optical film; 121, AG layer; 122, base layer; 122a, place-occupying protrusion; 123, adhesive layer; 123a, groove; 123b, embedded part;

[0049] Da, the distance between the two sides;

[0050] D0, thickness of optical film;

[0051] D1, thickness of AG layer;

[0052] D2, thickness of the base layer;

[0053] D3, thickness of adhesive layer;

[0054] 10. Display device; 200. Cabinet. DETAILED DESCRIPTION

[0055] Embodiments of the present application will be described in more detail below with reference to the accompanying drawings. Although certain embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be construed as being limited to the embodiments set forth herein. On the contrary, these embodiments are provided to provide a more thorough and complete understanding of the present application. It should be understood that the drawings and embodiments of the present application are only for exemplary purposes and are not intended to limit the scope of protection of the present application.

[0056] It should also be noted that, for ease of description, only the parts related to the invention are shown in the drawings. In the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other.

[0057] It should be noted that the concepts such as "first" and "second" mentioned in this application are only used to distinguish different devices, modules or units, and are not used to limit the order or interdependence of the functions performed by these devices, modules or units.

[0058] It should be noted that the modifications of "one" and "plurality" mentioned in the present application are illustrative rather than restrictive, and those skilled in the art should understand that unless otherwise clearly indicated in the context, it should be understood as "one or more".

[0059] The names of the messages or information exchanged between multiple devices in the embodiments of the present application are only used for illustrative purposes and are not used to limit the scope of these messages or information.

[0060] The present application will be described in detail below with reference to the accompanying drawings and in combination with embodiments.

[0061] Reference Figures 1 to 3 As shown, the present application provides a display panel 100 , which includes: a light board 110 and an optical film 120 .

[0062] The lamp board 110 has a light emitting side 110a, and includes a plurality of lamp board units 111 spliced ​​to each other; it can be understood that adjacent lamp board units 111 are spliced ​​in a direct contact manner so that the splicing gap is controlled within a smaller range.

[0063] At least one optical film 120 is provided to cover the entire light-emitting side 110a; each optical film 120 covers at least two light board units 111. It can be understood that the optical film 120 can at least cover the gap between the two light board units 111, or at least cover the surfaces of the two light board units 111 and the gap between two adjacent light board units 111.

[0064] By adopting the above scheme, by making each optical film cover at least two light board units, compared with the prior art, when the size of the display panel is constant, the number of optical films used can be reduced, thereby reducing the joints between the optical films to improve the display effect; at the same time, for multiple light board units covered by the same optical film, since there is no superposition effect of the joints of the light board units and the joints of the optical films, it also helps to improve the display effect at the joints of the light board units.

[0065] Moreover, by making each optical film 120 cover at least two light board units 111, the height difference and gap caused by the splicing of the light board units 111 can be effectively eliminated, and black lines can be avoided during color correction due to height differences and gaps on the spliced ​​light boards, thereby affecting the viewing experience. It can also reduce the impact on the smoothness of writing with a stylus or finger, and even avoid the outward peeling of the optical film caused by scratches from a stylus or finger.

[0066] At the same time, since multiple light panel units 111 are formed as a whole through the optical film 120, during the assembly process with the box 200, the whole formed by the light panel 110 and the optical film 120 is directly assembled with the box 200, and there is no need to splice the light panel units 111 piece by piece on the box 200. This can effectively reduce the clamping components and magnetic components used for positioning and fixing on the light panel units 111, thereby saving costs to a great extent.

[0067] In some embodiments, the plurality of light panel units 111 may be spliced ​​and fixed by bonding.

[0068] As an optional bonding method, refer to Figure 5 As shown, a colloid 112 is provided at the joints on the back of the plurality of light board units 111 , and the plurality of light board units 111 are assembled into a whole by the colloid 112 to maintain the flatness of the light emitting side 110 a of the light board 110 .

[0069] The colloids 112 located at the seams may be independent of each other, or a plurality of colloids 112 located at the seams may be connected to each other.

[0070] As another optional bonding method, a support body is provided on the back of the light board unit 111, and the support body is bonded to at least two light board units 111 through the colloid 112 at the same time. While realizing the splicing and fixation of multiple light board units 111, it can support the light board units 111 and improve the structural stability of the display panel 100.

[0071] In some embodiments, each light board unit 111 has a light emitting surface, and the light emitting surface of each light board unit 111 is flush with the light emitting surface of an adjacent light board unit 111 .

[0072] By adopting such a solution, there is no height difference between the multiple lamp board units 111 , thereby improving the flatness of the light emitting side 110 a of the lamp board 110 formed by the multiple lamp board units 111 , so that it can better fit with the optical film 120 .

[0073] In some embodiments, reference Figure 3 As shown, each lamp board unit 111 also has a plurality of side surfaces 111a connected to the light emitting surface and connected end to end along the circumference of the lamp board unit 111. For any two adjacent lamp board units 111, the two side surfaces 111a disposed opposite to each other abut against each other.

[0074] Since two adjacent lamp panel units 111 abut against each other through two oppositely arranged side surfaces 111 a , the splicing gap can be better controlled, which is beneficial to reducing the size of the splicing gap.

[0075] It is understandable that due to factors such as installation accuracy or the structure itself, there may be a certain gap between the two side surfaces 111a of two adjacent light board units 111. Figure 5 As shown, the distance Da between two oppositely disposed side surfaces 111 a of two adjacent lamp board units 111 is less than or equal to 5 micrometers.

[0076] By limiting the distance Da between two oppositely disposed side surfaces 111 a of the light board unit 111 , the colloid 112 is prevented from penetrating into the gap between adjacent light board units 111 during the splicing process of the light board units 111 , thereby improving the splicing effect.

[0077] In some embodiments, reference Figure 5 As shown, the thickness D0 of the optical film 120 ranges from 80 micrometers to 150 micrometers.

[0078] By adopting such thickness parameters, good display effects can be achieved while meeting the requirements of operational performance and cost control.

[0079] During the design and manufacturing process of the display panel 100 , the optimal film thickness can be adjusted to balance these factors according to the characteristics of the light board unit 111 and usage requirements, so as to achieve the best display effect, user experience and cost control.

[0080] In some embodiments, the number of light panel units 111 covered by each optical film 120 ranges from 2 to 300.

[0081] As a preferred solution, the number of light board units 111 covered by each optical film 120 ranges from 8 to 200.

[0082] In some embodiments, the aspect ratio of the optical film 120 ranges from 1.1 to 2.5.

[0083] In some embodiments, there is one optical film 120, and the format size of the optical film 120 is the same as the format size of the light board 110. With such an optical film 120 covering scheme, all light board units 111 can be covered in one laminating operation, and the laminating efficiency is high.

[0084] In some embodiments, the maximum size L of the optical film 120 satisfies the following formula:

[0085] L=K×D0+A

[0086] Wherein, L is the maximum size of the optical film 120, in micrometers, D0 is the thickness of the optical film 120, in micrometers, K is the product coefficient, and A is the correction constant. The value range of K is 16000 to 25000, and the value range of A is 80 to 115, in micrometers.

[0087] When laminating the optical film 120, the general idea is to set the thickness of the optical film 120 according to the requirements of the display panel 100, which is determined by the design of the display panel 100 and the display effect. According to the principle of integrated lamination, the thicker the optical film 120 is, the more it can compensate for the uneven defects caused by the splicing of the light board unit 111.

[0088] Although it is a preferred solution to use the same optical film 120 for the entire light board 110, the larger the size of the optical film 120, the more likely it is that internal wrinkles or uneven trimming defects will cause thickness changes. As the length of the optical film 120 increases, some parts will be more severely uneven than the light board unit 111. Therefore, as an optional solution, it is necessary to balance and limit the size of a single optical film 120. It cannot be too small to achieve the technical effect of integrated coating, nor too large to cause defects due to the accumulation of length. Based on the above considerations, the above empirical formula can be used to balance the size design.

[0089] In some embodiments, the display panel 100 includes a plurality of optical films 120 , which are spliced ​​together, and the size of the spliced ​​optical films 120 is the same as the size of the light board 110 .

[0090] The light board 110 is covered by splicing a plurality of optical films 120 , so that the same optical film 120 can cover a plurality of light board units 111 , while reducing the requirement on the size of the optical film 120 .

[0091] As an optional solution, multiple optical films 120 have the same size and are regularly arranged on the light-emitting side 110a of the lamp board 110. Using multiple optical films 120 with the same size and regularly arranged on the light-emitting side 110a of the lamp board 110 reduces the size requirements for the optical films 120 and reduces the difficulty of the lamination process.

[0092] When the user watches the image displayed by the display panel 100, the user mainly focuses on the middle area of ​​the light board 110. As another optional solution, at least some of the multiple optical films 120 have different formats, and the format size of the optical film 120 located in the middle of the light board 110 is larger than the format size of the optical film 120 located around the light board 110. By using optical films 120 of different formats for lamination, and using an optical film 120 of a larger format size in the middle of the light board 110, the size requirement of the optical film 120 is reduced while ensuring the display effect and improving the user experience, thereby balancing the display effect and manufacturing difficulty.

[0093] In some embodiments, reference Figure 5 As shown, the optical film 120 includes an AG layer 121 , a base layer 122 and a back adhesive layer 123 .

[0094] Specifically, the adhesive layer 123 is bonded to the light-emitting side 110a surface of the lamp board 110 to fix the optical film 120 to the lamp board 110; the base layer 122 is sandwiched between the AG layer 121 and the adhesive layer 123 to support the AG layer 121 and the adhesive layer 123 to improve the structural stability of the optical film 120. The thickness D1 of the AG layer 121 ranges from 5 microns to 10 microns; the thickness D2 of the base layer 122 ranges from 20 microns to 100 microns; the thickness D3 of the adhesive layer 123 ranges from 30 microns to 120 microns.

[0095] Since the optical film 120 adopts the above composite film layer structure, it is possible to balance the optical and tensile forces of the optical film 120, effectively solve the attachment process and ensure the display effect.

[0096] In some embodiments, the base layer 122 is a PET layer. The adhesive layer 123 is an OCA layer. The surface of the AG layer 121 is a plane. The display panel 100 is a Micro-LED display panel 100.

[0097] Reference Figure 4 As shown, when each lamp panel unit 111 is coated independently, Figure 4 The gap defects between the optical films 120 shown in the figure, and due to the inconsistent shrinkage between the optical film 120 and the light board 110, the gap size Da between adjacent light board units 111 and the gap size Db between adjacent optical films 120 will be inconsistent, further aggravating the gap size and unevenness defects.

[0098] Reference Figure 5As shown, by adopting the coating solution of the present application, it can be seen that the optical film 120 will cover the gaps between the light board units 111 to avoid defects. However, due to the above-mentioned problem of the length of the optical film 120 and the different shrinkage rates of the optical film 120 and the light board units 111, uneven defects will still occur at the gaps between the light board units 111.

[0099] Reference Figure 6 As shown, as a preferred solution, a placeholder protrusion 122a is formed on the base layer 122 of the optical film 120 at the gap between the light board units 111, and is embedded in the back glue layer 123 to form a groove 123aa in the back glue layer 123, so that when the back glue layer 123 is attached, an embedded portion 123b is generated which is embedded in the gap between the light board units 111 due to the existence of the placeholder protrusion 122a. This embedded portion 123b helps to eliminate the uneven defects caused by the gap, and at the same time, it will relatively limit the optical film 120 when the light board units 111 and the optical film 120 shrink inconsistently, so that it will not produce large wrinkles. Figure 6 The placeholder protrusion 122 a of the solution shown is rectangular, which is easier to process, but the adhesive layer 123 will generate stress concentration.

[0100] Reference Figure 7 As shown, as an improvement solution, a trapezoidal interface can be used to relatively improve the stress concentration situation.

[0101] Reference Figure 8 As shown, as a further improvement, a semicircular cross-section can be used, which not only ensures uniform force in all directions but also has a better space-occupying effect.

[0102] Reference Fig. 9 and Fig.10 As shown, as a further improvement, a circular arc and two tangent lines tangent thereto may be used to form a cross-sectional shape to form the space-occupying protrusion 122a, which can achieve the space-occupying effect as much as possible and relatively eliminate the problem of stress concentration.

[0103] Reference Fig.11 and Fig.13 As shown, the present application also provides a display device 10, comprising the aforementioned display panel 100 and a box 200. The box 200 is used to fix the display panel 100 and make the multiple light board units 111 in the display panel 100 form a whole.

[0104] Since the multiple light panel units 111 are formed into a whole, during the assembly process with the box body 200, the whole can be directly assembled with the box body 200, and there is no need to splice the light panel units 111 piece by piece on the box body 200. This can effectively reduce the clamping components and magnetic components used for positioning and fixing on the box body 200, thereby saving costs to a great extent.

[0105] The present application also provides a method for manufacturing a display device 10, the method comprising the following steps:

[0106] S110: providing a plurality of light board units 111;

[0107] S120: splicing a plurality of light board units 111 into a light board 110, wherein the light board 110 has a light emitting side 110a;

[0108] S130: providing at least one optical film 120;

[0109] S140 : attaching the optical film 120 to the light emitting side 110 a of the light board 110 , so that each optical film 120 covers at least two light board units 111 .

[0110] By adopting the above solution, a plurality of light board units 111 are covered by an integral optical film 120 , which can effectively eliminate the height difference and gap caused by splicing the light board units 111 , thereby improving the display effect.

[0111] In some embodiments, the manufacturing method of the display device 10 further includes the following steps:

[0112] The light board 110 is mounted to the box 200 .

[0113] In some embodiments, step 120 includes:

[0114] S121: Laying the plurality of light panel units on a splicing platform with their light emitting surfaces facing each other, and positioning the adjacent light panel units so that their side surfaces are in abutment with each other;

[0115] S122: Glue is applied to the joint gaps on the back of the light panel units;

[0116] S123: solidifying the glued colloid to fix each lamp panel unit into a lamp panel.

[0117] Among them, in step S121, the splicing platform has a reference plane, and a vacuum adsorption device is used on the splicing platform, so that the light-emitting surfaces of all light board units are laid on the reference plane with the reference plane as the positioning reference, ensuring that the light-emitting surfaces of each light board unit are flush.

[0118] In step S121, the splicing platform is further provided with a horizontal pushing device, which provides a thrust parallel to the reference plane on the outer side of the whole formed by the multiple light board units, so that the side surfaces of adjacent light board units abut against each other.

[0119] In step S122, glue is dispensed at the joint gap using glue dispensing equipment. The glue at the joint gap may be independent of each other, or a plurality of glues at the joint gap may be connected to each other.

[0120] In step S123, the colloid may be cured by UV light irradiation or thermal curing, and the curing method and curing time are selected according to the specific process.

[0121] As a specific implementation, taking a 135-inch display panel as an example, the length of the light board is about 3000 mm (that is, 20 light board units are set in the horizontal direction), and the width is about 1687.5 mm (that is, 10 light board units are set in the vertical direction). In this way, the light board is composed of 200 light board units.

[0122] The width of the optical film used for the integrated lamination is about 1690 mm, so that one side is about 1.25 mm wider than the light board, and the length of the optical film is a continuous roll.

[0123] The light board moves over the optical film and rolls together with the optical film below (for example, using a plastic sealing process) until the entire light board covers the optical film, and then cuts it in the length direction. The cut optical film is usually about 1 mm longer than the light board. Finally, cut off the extra optical film on the four sides of the entire light board, keeping the edge of the optical film flush with the edge of the light board.

[0124] It can be understood that the integrally coated optical film is larger than the light emitting side of the covered lamp board by a certain size, and then cut to be flush with the side of the lamp board.

[0125] In some embodiments, step S140 includes:

[0126] A degassing process is performed between the optical film 120 and the lamp board unit 111 at a preset pressure and a preset temperature.

[0127] By adopting the degassing treatment, the bubbles between the optical film 120 and the light board unit 111 are discharged, thereby ensuring that the optical film 120 and the light board unit 111 are fully covered and bonded.

[0128] In some embodiments, the preset pressure and / or the preset temperature is proportional to the thickness of the optical film 120 .

[0129] In some embodiments, the preset pressure P, the preset temperature T, the maximum size L of the optical film 120, the thickness D0 of the optical film 120, and the degassing rate V satisfy the following formula:

[0130] V=Q×(P×T) / (D0×L)

[0131] Wherein, Q is an empirical constant; Q can be selected according to the specific process.

[0132] The above description is only some preferred embodiments of the present application and an explanation of the technical principles used. Those skilled in the art should understand that the scope of the invention involved in the embodiments of the present application is not limited to the technical solutions formed by the specific combination of the above technical features, but should also cover other technical solutions formed by any combination of the above technical features or their equivalent features without departing from the above invention concept. For example, the above features are replaced with (but not limited to) the technical features with similar functions disclosed in the embodiments of the present application to form a technical solution.

Claims

1. A display panel, characterized in that: include: A light board having a light emitting side and comprising a plurality of light board units spliced ​​to each other; At least one optical film, covering the entire light-emitting side; Wherein, each of the optical films covers at least two of the light panel units.

2. The display panel according to claim 1, characterized in that: Each of the light board units has a light emitting surface, and the light emitting surface of each of the light board units is flush with the light emitting surface of the adjacent light board units.

3. The display panel according to claim 2, characterized in that: Each of the light board units also has a plurality of side surfaces connected to the light emitting surface and connected end to end along the circumferential direction of the light board unit. For any two adjacent light board units, two side surfaces that are arranged opposite to each other abut against each other.

4. The display panel according to any one of claims 1 to 3, characterized in that: The thickness of the optical film is in a range of 80 micrometers to 150 micrometers.

5. The display panel according to claim 4, characterized in that: The number of the light panel units covered by each optical film ranges from 2 to 300.

6. The display panel according to claim 4, characterized in that: The aspect ratio of the optical film ranges from 1.1 to 2.

5.

7. The display panel according to claim 6, characterized in that: The number of the optical film is one, and the format size of the optical film is the same as the format size of the light board.

8. The display panel according to claim 6, characterized in that: The display panel includes a plurality of optical films, which are spliced ​​together, and the format size of the spliced ​​optical films is the same as the format size of the light board.

9. The display panel according to claim 8, characterized in that: At least some of the plurality of optical films have different sizes, and the size of the optical film located in the middle of the light board is larger than the size of the optical film located around the light board.

10. The display panel according to claim 4, characterized in that: The optical film comprises: an AG layer, a base layer and a back adhesive layer; Wherein, the adhesive layer is bonded to the light-emitting side surface of the light board, and the base layer is sandwiched between the AG layer and the adhesive layer; The thickness of the AG layer ranges from 5 microns to 10 microns; the thickness of the base layer ranges from 20 microns to 100 microns; and the thickness of the back adhesive layer ranges from 30 microns to 120 microns.

11. A display device, characterized in that: A display panel comprising the claim according to any one of claims 1 to 10.