Semiconductor device and method for manufacturing semiconductor device
By designing a conductive type drift layer, well region and impurity region in the semiconductor device, and using a field insulating film to cover the upper corner of the terminal trench, the problem of insulating film damage in the trench gate structure is solved and the electric field control is achieved. The relaxation and protection of the insulating film improve the reliability and manufacturing efficiency of the device.
Patent Information
- Application Number
- CN202280092813.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-03
- Publication Date
- 2024-10-15
AI Technical Summary
In a semiconductor device with a trench gate structure, the insulating film in the gate lead-out portion is easily damaged due to electric field concentration, resulting in thinning of the thickness of the insulating film and concentration of electric field in the conductive state, thereby causing damage to the insulating film.
A semiconductor device is designed, which includes a conductive type drift layer, a well region and an impurity region. The gate trench is connected to the terminal trench, the gate insulating film is grounded on both sides, and the field insulating film covers the upper end of the terminal trench. The corner portion is thicker than the gate insulating film. The second gate electrode is in contact with the field insulating film and carries the field insulating film to relax the electric field.
This effectively prevents the insulation film from being damaged at the upper end corner of the terminal trench of the gate lead-out portion, improves the reliability and life of the semiconductor device, and reduces the manufacturing cost.
Smart Images

Figure CN118786531A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a trench gate semiconductor device and a method for manufacturing the same, and in particular to a structure of a gate electrode on the outer periphery of a semiconductor device. Background Art
[0002] Semiconductor devices such as insulated gate bipolar transistors (IGBT) and metal oxide semiconductor field effect transistors (MOSFET) having a trench gate structure are used for power control applications in automotive equipment, industrial equipment, and the like.
[0003] In a semiconductor device having a trench gate structure, a gate electrode lead portion is provided in a trench extending toward a terminal region outside the active region to form a gate trench of the active region through which a main current flows. Patent document 1 discloses that an insulating film is formed on the gate electrode lead portion, the insulating film on the trench is opened with high precision to connect the gate electrode to the gate pad, and the electric field concentration of the insulating film at the corner of the upper end of the trench far from the active region is relaxed.
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Publication No. 2006-520091 ( Figure 7 C reference) Summary of the invention
[0007] However, when the insulating film on the trench of the gate lead portion shown in Patent Document 1 is opened, the thickness of the insulating film at the upper corner of the trench of the gate lead portion far from the active region may become thinner due to the position of the opening being offset or not being opened vertically, etc. In this case, in the on-state of the semiconductor device with a voltage above the threshold applied to the gate electrode, the electric field may be concentrated on the insulating film formed at the upper corner of the trench of the gate lead portion far from the active region, causing the insulating film to be destroyed.
[0008] The present disclosure has been made to solve the above-mentioned problems, and an object of the present disclosure is to provide a semiconductor device that prevents the destruction of an insulating film formed at an upper corner of a trench far from an active region in a gate lead-out portion.
[0009] The semiconductor device disclosed in the present invention comprises: a drift layer of the first conductivity type; a well region of the second conductivity type, which is arranged on the surface of the drift layer; an impurity region of the first conductivity type, which is arranged on the surface of the well region; a gate trench, which penetrates the well region from the surface of the impurity region and reaches the drift layer; a terminal trench, which is connected to the gate trench when viewed from above, and the width of the gate trench in the extension direction is wider than the width of the gate trench; a gate insulating film, which is formed in contact with the gate trench and the inner surface of the terminal trench; a first gate electrode, which is formed on the inner wall and bottom surface of the gate trench and the terminal trench through the gate insulating film; a field insulating film, which is in contact with the first gate electrode formed in the terminal trench, is formed from the inner side to the outer side of the terminal trench so as to cover the upper end corner of the terminal trench on the side farther from the gate trench in the extension direction, and has a thickness thicker than the gate insulating film; and a second gate electrode, which is in contact with the field insulating film and the first gate electrode formed in the terminal trench, and is supported by the field insulating film from the inner side to the outer side of the terminal trench in the extension direction.
[0010] In addition, the manufacturing method of the semiconductor device disclosed in the present invention comprises: a step of forming a drift layer of the first conductivity type; a step of providing a well region of the second conductivity type on the surface layer of the drift layer; a step of providing an impurity region of the first conductivity type on the surface layer of the well region; a step of providing a gate trench that penetrates the well region from the surface of the impurity region and reaches the drift layer; a step of providing a terminal trench that is connected to the gate trench in a plan view and has a width in an extension direction of the gate trench that is wider than the width of the gate trench; a step of forming a gate insulating film that is in contact with the inner side of the gate trench and the terminal trench; a step of providing a gate insulating film that is in contact with the inner side of the gate trench and the terminal trench; a step of providing a gate trench that is connected to the gate trench and the terminal trench; a step of providing a gate insulating film that is connected to the inner side of the gate trench and the terminal trench; a step of providing a gate trench that is connected to ... gate trench and the terminal trench; a step of providing a gate trench that is connected to the gate trench and the terminal trench; a step of providing a gate trench that is connected to the gate trench and the terminal trench; a step of providing a gate trench that is connected to the gate trench and the terminal trench; a step of providing a gate trench that is connected to the A process of forming a first gate electrode on the inner side of the groove through a gate insulating film; a process of forming a field insulating film, which is connected to the first gate electrode formed in the terminal trench and covers the upper end corner of the terminal trench on the side far from the gate trench in the extension direction from the inside to the outside of the terminal trench, and the thickness of the field insulating film is set to be greater than the thickness of the gate insulating film; and a process of forming a second gate electrode, which is connected to the field insulating film and the first gate electrode formed in the terminal trench, and is supported by the field insulating film from the inside to the outside of the terminal trench in the extension direction.
[0011] According to the present disclosure, it is possible to obtain a semiconductor device that prevents the insulation film formed at the upper corner of the termination trench on the side farther from the active region in the gate lead-out portion from being destroyed. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 It is a schematic plan view showing a schematic structure of a semiconductor device in Embodiment 1.
[0013] Figure 2 This is a schematic diagram showing a schematic structure of a semiconductor device in Embodiment 1.
[0014] Figure 3 It is a schematic cross-sectional view showing a schematic structure of a semiconductor device in Embodiment 1.
[0015] Figure 4 This is an explanatory diagram of the method for manufacturing the semiconductor device in the first embodiment.
[0016] Figure 5 This is an explanatory diagram of the method for manufacturing the semiconductor device in the first embodiment.
[0017] Figure 6 This is an explanatory diagram of the method for manufacturing the semiconductor device in the first embodiment.
[0018] Figure 7 This is an explanatory diagram of the method for manufacturing the semiconductor device in the first embodiment.
[0019] Figure 8 This is an explanatory diagram of the method for manufacturing the semiconductor device in the first embodiment.
[0020] Fig. 9 It is a schematic plan view showing a schematic structure of a modified example of the semiconductor device in the first embodiment.
[0021] Fig.10 This is a schematic diagram showing a schematic structure of a semiconductor device in the second embodiment.
[0022] Fig.11 This is a schematic diagram showing a schematic structure of a semiconductor device in the second embodiment.
[0023] Fig.12 It is a schematic plan view showing a schematic structure of a semiconductor device in a third embodiment.
[0024] Fig.13 This is a schematic diagram showing a schematic structure of a semiconductor device in a third embodiment.
[0025] (Explanation of symbols)
[0026] 1: semiconductor substrate; 2: drift layer; 3: well region; 4: impurity region; 5: contact region; 6: gate trench; 6a: upper corner of gate trench; 7: terminal trench; 7a: upper corner of terminal trench; 8: gate insulating film; 9: first gate electrode; 10: field insulating film; 11: first electric field relaxation region; 12: second electric field relaxation region; 13: second gate electrode; 13a: second gate electrode lead-out portion; 13b: second gate electrode periphery; 14: interlayer insulating film; 15: gate contact hole; 16: gate pad; 17: source contact hole; 18: surface ohmic electrode; 19: back ohmic electrode; 20: surface electrode; 21: back electrode; 22: etching mask; 23: channel blocking region; 24: peripheral electric field relaxation region; 40: active region; 50: terminal region; 60: partial region; 70: gate lead-out portion. DETAILED DESCRIPTION
[0027] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. The accompanying drawings are schematically shown, and the sizes and positions of the drawings shown in different drawings may be appropriately changed. In addition, for the sake of simplicity, the details of the semiconductor layer and the electrode are sometimes omitted in the accompanying drawings. In addition, terms such as top, bottom, side, bottom, surface or back that mean specific positions and directions are used for the convenience of description and have nothing to do with the direction during implementation.
[0028] In addition, in the embodiments of the present disclosure, the first conductivity type of the semiconductor is described as n-type and the second conductivity type is p-type, but the first conductivity type may be p-type and the second conductivity type may be n-type. In addition, the semiconductor device is described as a MOSFET, but it may be an IGBT. In addition, the material of the semiconductor substrate and the drift layer is described as silicon carbide (SiC), but it may be silicon or a material with a larger band gap than silicon, such as gallium nitride or diamond, or a combination thereof. Implementation method 1.
[0029] First, the structure of the semiconductor device in this embodiment is described. Figure 1 1 is a schematic top view showing the schematic structure of the semiconductor device in this embodiment. Figure 1 As shown, the semiconductor device includes an active region 40 as a region through which a main current flows when the semiconductor device is in operation, and a termination region 50 as a region outside the active region 40. Here, for simplicity of description, the field insulating film 10 and the surface electrode 20 are omitted.
[0030] The active region 40 is provided with a stripe-shaped gate trench 6 and a first gate electrode 9. The terminal region 50 is provided with a terminal trench 7 connected to the gate trench 6 and the first gate electrode 9, and further provided with a second gate electrode 13 connected to the first gate electrode 9 in a direction perpendicular to the paper surface. In addition, the terminal region 50 is provided with a gate pad 16 connected to the second gate electrode 13. Here, the boundary between the active region 40 and the terminal region 50 is the position where the gate trench 6 and the terminal trench 7 are connected and the position where the gate pad 16 is arranged when viewed from above.
[0031] Figure 2 is a schematic diagram showing a schematic structure of a semiconductor device in this embodiment, which is a perspective view Figure 1 FIG. 6 is a diagram of a cross section and a top surface of a partial area 60. In addition, Figure 3 is a schematic cross-sectional view showing a schematic structure of a semiconductor device in Embodiment 1, and is a schematic view showing Figure 1 A diagram of the cross section under line A1-A2.
[0032] like Figure 2 As shown in FIG. 1 , in the semiconductor device, a drift layer 2, a well region 3, an impurity region 4, a contact region 5, a gate trench 6, a gate insulating film 8, and a first gate electrode 9 are provided on the surface side of a semiconductor substrate 1, and further, a termination trench 7, a field insulating film 10, a first electric field relaxation region 11, a second electric field relaxation region 12, and a second gate electrode 13 are provided. In addition, as Figure 2 As shown, in the semiconductor device, a back ohmic electrode 19 and a back electrode 21 are provided on the back side of the semiconductor substrate 1 .
[0033] Here, in the gate lead-out portion 70 forming the second gate electrode 13, the upper corner portion 7a of the terminal trench on the side far from the gate trench 6 is covered with a field insulating film 10 thicker than the gate insulating film 8, and the second gate electrode 13 supported by the field insulating film 10 from above the first gate electrode 9 is formed.
[0034] The drift layer 2 is provided on the semiconductor substrate 1 composed of n-type silicon carbide and is composed of n-type silicon carbide. The n-type impurity of the drift layer 2 may be nitrogen or phosphorus, and the impurity concentration of the drift layer 2 is 1×10 14 cm -3 Above and 1×10 17 cm -3 The thickness of the drift layer 2 may be set to be approximately 5 μm or more and 200 μm or less.
[0035] The well region 3 is a p-type region provided on the surface of the drift layer 2 and is composed of silicon carbide. The p-type impurity of the well region 3 may be aluminum, boron or gallium, and the impurity concentration of the well region 3 is 1×10 15 cm-3 Above and 1×10 20 cm -3 Here, the impurity concentration of the well region 3 may be constant in the depth direction or may not be constant. The thickness of the well region 3 may be set to be about 0.3 μm or more and 3 μm or less.
[0036] The impurity region 4 is an n-type region provided in the surface layer of the well region 3 and is composed of silicon carbide. In other words, the impurity region 4 is a source region. The n-type impurity of the impurity region 4 may be nitrogen or phosphorus, and the impurity concentration of the impurity region 4 may be 1×10 18 cm -3 Above and 1×10 21 cm -3 The thickness of the impurity region 4 may be less than or equal to the thickness of the well region 3 .
[0037] The contact region 5 is a p-type region provided on the surface layer of the well region 3 and is composed of silicon carbide. The contact region 5 is connected to the impurity region 4 and the surface ohmic electrode 18 described later. When the contact region 5 is formed, a path is formed from the impurity region 4 to the surface ohmic electrode 18 via the contact region 5, and the electrical connection becomes good in the path from the impurity region 4 to the surface ohmic electrode 18.
[0038] The p-type impurity of the contact region 5 can be set to aluminum, boron or gallium, and the impurity concentration of the contact region 5 is set to 1×10 18 cm -3 Above and 1×10 22 cm -3 The thickness of the contact region 5 may be less than or equal to the thickness of the well region 3. Here, an example in which the contact region 5 is provided in the semiconductor device is shown, but it is not necessarily provided.
[0039] The gate trench 6 is a groove that penetrates the well region 3 from the surface of the impurity region 4 and reaches the drift layer 2. Figure 1 As shown, the gate trench 6 is provided in a stripe shape, that is, in parallel, in the active region 40. When the gate trench 6 is provided in a stripe shape, when the semiconductor device in this embodiment is made into a trench gate type MOSFET using silicon carbide in the semiconductor substrate 1 and the drift layer 2, a surface such as a (1-100) surface with high channel mobility can be used as a channel, and the characteristics of the semiconductor device can be improved. In addition, the gate trench 6 extends in the direction from the active region 40 toward the terminal region 50. Hereinafter, the direction of this extension is sometimes set as the extension direction of the gate trench 6.
[0040] The width of the gate trench 6 is Figure 2The width of the cross section on the front side of the gate trench 6 in the left-right direction may be set to be greater than 1 μm and less than 10 μm. When the shape of the gate trench 6 is a tapered shape when viewed in cross section, the width of the gate trench 6 refers to the width of the widest part of the tapered shape. The depth of the gate trench 6 may be set to be greater than 1 μm and less than 6 μm.
[0041] The terminal trench 7 is connected to the gate trench 6 when viewed from above, and is a trench whose width in the extension direction of the gate trench 6 is wider than the width of the gate trench 6. The terminal trench 7 can be provided extending in the gate trench 6 when viewed from above. The depth of the terminal trench 7 can be the same as or different from the depth of the gate trench 6. The width of the terminal trench 7 in the extension direction of the gate trench 6 can be set to be less than 3 times the width of the gate trench 6, for example, it can be set to more than 1 μm and less than 30 μm.
[0042] When the width of the terminal groove 7 is selected in this way, the upper part of the terminal groove upper end corner 7a on the side far from the gate groove 6 can be easily covered with the field insulating film 10 described later, and the gate lead portion 70 can be easily formed. That is, it is not necessary to use a process for opening the field insulating film 10 with high precision, and the first gate electrode 9 and the second gate electrode 13 formed in the terminal groove 7 described later can be connected. In addition, it is possible to prevent the first gate electrode 9 from disappearing and disconnecting in the etching back process of the first gate electrode 9 described later. Here, the upper end corner 7a of the terminal groove is as shown in FIG. Figure 2 or Figure 3 As shown, the boundary between the inner and outer sides of the terminal trench 7 includes a point at the corner of the terminal trench 7 and a region near the corner where the gate insulating film 8 can be formed. That is, the upper corner 7a of the terminal trench includes a part of the inner side and a part of the outer side of the terminal trench 7, in other words, includes the vicinity of the upper corner 7a of the terminal trench.
[0043] The gate insulating film 8 is formed in contact with the inner surface of the gate trench 6 and the terminal trench 7 and is made of silicon dioxide. Figure 2 As shown in FIG. 1 , the gate insulating film 8 may be formed to the position of the gate trench upper corner 6a and the terminal trench upper corner 7a or a position lower than the position, respectively, on the inner side of the gate trench 6 and the terminal trench 7. The thickness of the gate insulating film 8 may be set to be greater than 10 nm and less than 100 nm. In addition, the gate insulating film 8 may also be formed as Figure 2 or Figure 3 As shown, it is formed outside the gate trench 6 or the termination trench 7, for example, on the well region 3 of the termination region 50 or on the impurity region 4. When the gate insulating film 8 is formed on the well region 3 of the termination region 50, the gate insulating film 8 covers the upper corner 7a of the termination trench.
[0044] The first gate electrode 9 is formed inside the gate trench 6 and the terminal trench 7 via a gate insulating film 8 and is made of a conductive material such as polysilicon. Figure 2 As shown, the inner sides of the gate trench 6 and the terminal trench 7 are formed to the positions of the gate trench upper end corners 6a and the terminal trench upper end corners 7a or to a position lower than the positions, that is, below.
[0045] When the first gate electrode 9 is formed in such a manner that the upper end is located below the gate trench upper corner 6a and the terminal trench upper corner 7a, the electric field applied to the gate insulating film 8 formed near the gate trench upper corner 6a and the terminal trench upper corner 7a in the operating state of the semiconductor device can be mitigated, thereby preventing the gate insulating film 8 from being damaged.
[0046] The field insulating film 10 is in contact with the first gate electrode 9 formed in the terminal trench 7, and is formed from the inside to the outside of the terminal trench 7 so as to cover the upper corner 7a of the terminal trench on the side farther from the gate trench 6 in the extension direction of the gate trench 6. That is, the field insulating film 10 is continuously formed from the upper surface of the first gate electrode 9 to the surface on the outer peripheral side of the terminal trench 7, covering the upper corner 7a of the terminal trench. Figure 3 , an example is shown in which the field insulating film 10 is formed on the first gate electrode 9 of the termination region 50 and on the gate insulating film 8 overlapping the termination trench upper corner 7a and the well region 3. The thickness of the field insulating film 10 may be thicker than the thickness of the gate insulating film 8, and may be set to, for example, 0.1 μm or more and 5.0 μm or less.
[0047] When the field insulating film 10 thicker than the gate insulating film 8 covers the upper corner 7a of the terminal trench far from the gate trench 6, the electric field applied to the gate insulating film 8 formed near the upper corner 7a of the terminal trench can be relaxed, and the gate insulating film 8 can be suppressed from being damaged, compared with the structure in which only the gate insulating film 8 covers the upper corner 7a of the terminal trench. Here, when the thickness of the field insulating film 10 is set to be twice or more of the thickness of the gate insulating film 8, the gate insulating film 8 can be further suppressed from being damaged. The field insulating film 10 can be made of an insulating material such as silicon dioxide.
[0048] The first electric field relaxation region 11 is a p-type region provided below the bottom surface of the gate trench 6 and is composed of silicon carbide. The first electric field relaxation region 11 has a conductivity type opposite to that of the drift layer 2, and can relax the electric field applied to the gate insulating film 8 formed on the bottom surface of the gate trench 6 in the operating state of the semiconductor device, thereby preventing the gate insulating film 8 from being damaged. The depth of the first electric field relaxation region 11 can be set to be greater than 0.1 μm and less than 2.0 μm from the bottom surface of the gate trench 6. Here, the first electric field relaxation region 11 can also be in contact with the bottom surface of the gate trench 6. The p-type impurity of the first electric field relaxation region 11 can be set to aluminum, boron or gallium, and the impurity concentration of the first electric field relaxation region 11 is set to 1×10 15 cm -3 Above and 1×10 19 cm -3 The following level will suffice.
[0049] The second electric field relaxation region 12 is a p-type region provided below the bottom surface of the terminal trench 7 and is composed of silicon carbide. The second electric field relaxation region 12 has a conductivity type opposite to that of the drift layer 2, and can relax the electric field applied to the gate insulating film 8 formed on the bottom surface of the terminal trench 7 when the semiconductor device is in operation, thereby preventing the gate insulating film 8 from being damaged. The depth of the second electric field relaxation region 12 can be set to a depth of 0.1 μm or more and 2.0 μm or less from the bottom surface of the terminal trench 7 downward. Here, the second electric field relaxation region 12 can also be in contact with the bottom surface of the terminal trench 7. The p-type impurity of the second electric field relaxation region 12 can be set to aluminum, boron or gallium, and the impurity concentration of the first electric field relaxation region 11 can be set to 1×10 15 cm -3 Above and 1×10 19 cm -3 The following level will suffice.
[0050] The second gate electrode 13 is in contact with the field insulating film 10 and the first gate electrode 9 formed in the terminal trench 7, and is supported by the field insulating film 10 from the inside to the outside of the terminal trench 7 in the extending direction of the gate trench 6. That is, the second gate electrode 13 is continuously formed from the step on the upper surface of the first gate electrode 9 that exceeds the end of the field insulating film 10 to the upper surface of the field insulating film 10, covering the end of the field insulating film 10 on the terminal trench 7. The second gate electrode 13 can be made of the same material as the first gate electrode 9, such as polysilicon, or a material different from the first gate electrode 9, such as a metal material such as aluminum. When the second gate electrode 13 is made of a material different from the first gate electrode 9, the second gate electrode 13 can be easily manufactured.
[0051] The second gate electrode 13 is as follows Figure 3As shown, the wiring for connecting the first gate electrode 9 formed in the terminal groove 7 to the gate pad 16. The gate pad 16 is formed on the second gate electrode 13 outside the terminal groove 7, and is connected to the second gate electrode 13 via a gate contact hole 15 provided in an interlayer insulating film 14 composed of silicon dioxide. The gate pad 16 is also formed on the interlayer insulating film 14. When the structure is set to connect the second gate electrode 13 and the gate pad 16 outside the terminal groove 7, the likelihood of selecting the arrangement position and size of the gate contact hole 15 can be improved.
[0052] In addition, if Figure 3 As shown, the surface electrode 20 is separated from the gate pad 16 and formed on the interlayer insulating film 14. The surface electrode 20 is made of a metal material such as aluminum.
[0053] The back ohmic electrode 19 is formed on the back side of the semiconductor substrate 1 and is composed of a reaction product, such as nickel silicide, of a metal film mainly composed of nickel and the semiconductor substrate 1. The back electrode 21 is formed in contact with the back ohmic electrode 19 and is composed of titanium, nickel, silver, gold, aluminum, etc.
[0054] The semiconductor device in this embodiment is configured as described above.
[0055] Next, use Figures 4 to 8 A method for manufacturing a semiconductor device in this embodiment is described. Figures 4 to 8 is an illustration of the various manufacturing stages of a semiconductor device. Figure 1 First, without using the drawings, the following description will be given until the Figure 4 A method for manufacturing a semiconductor device in a state.
[0056] A semiconductor substrate 1 composed of n-type silicon carbide having a polytype of 4H is prepared, and an n-type drift layer 2 is epitaxially grown on the surface side of the semiconductor substrate 1 by chemical vapor deposition (CVD) or the like. Next, aluminum, boron or gallium may be ion-implanted using a resist mask formed on the drift layer 2 by photolithography to provide a p-type well region 3 on the surface of the drift layer 2. Here, the well region 3 may also be provided by epitaxial growth.
[0057] Next, nitrogen or phosphorus is ion-implanted using a resist mask formed on the well region 3 by photolithography, and an n-type impurity region 4, in other words, a source region, is provided on the surface layer of the well region 3. Furthermore, aluminum, boron or gallium is ion-implanted using a resist mask formed on the well region 3 and the impurity region 4, and a p-type contact region 5 is provided on the surface layer of the well region 3. Here, the heating temperature of the semiconductor substrate 1 during the ion implantation may be set to 150° C. or higher. When the heating temperature is set to 150° C. or higher, the resistance of the contact region 5 can be reduced, and the resistance loss in the operating state of the semiconductor device can be reduced.
[0058] Next, a silicon dioxide film with a thickness of about 1 μm to 2 μm is formed on the well region 3, the impurity region 4, and the contact region 5, and an etching mask 22 with openings corresponding to the gate trench 6 and the terminal trench 7 is formed by reactive ion etching (RIE). Then, the gate trench 6 and the terminal trench 7 are formed by RIE. Figure 4 status.
[0059] Figure 5 The state shown is that the first electric field relaxation region 11 and the second electric field relaxation region 12 are provided below the gate trench 6 and the terminal trench 7 , respectively, and the gate insulating film 8 and the first gate electrode 9 are formed inside the gate trench 6 and the terminal trench 7 .
[0060] exist Figure 4 In the state of , aluminum, boron or gallium are ion-implanted, and the first electric field relaxation region 11 and the second electric field relaxation region 12 are respectively set below the gate trench 6 and the terminal trench 7. Next, after removing the etching mask 22, annealing is performed to activate the ion-implanted impurities. The annealing is performed in an inert gas atmosphere such as argon or in a vacuum at a temperature of 1500°C to 1900°C for a time of 30 seconds to 1 hour. Here, in order to prevent the degradation of silicon carbide due to high-temperature heating, that is, surface roughening, a carbon film can also be formed on the silicon carbide before the annealing.
[0061] Then, a gate insulating film 8 is formed on the surface of the drift layer 2 including the inner side of the gate trench 6 and the terminal trench 7 and the surface of the well region 3 of the terminal region 50 by thermal oxidation or CVD, and then polysilicon to be the first gate electrode 9 is formed by CVD. Furthermore, the polysilicon is etched back by an etch-back process, and the first gate electrode 9 is formed below the positions of the gate trench upper end corner 6a and the terminal trench upper end corner 7a, respectively, inside the gate trench 6 and the terminal trench 7. In this way, Figure 5 status.
[0062] Figure 6The state where the upper part of the termination trench upper end corner portion 7 a on the side far from the gate trench 6 is covered with the field insulating film 10 is shown.
[0063] exist Figure 5 In the state of being formed, an insulating film such as silicon dioxide is formed by CVD method or the like to become the field insulating film 10, and a resist mask is formed on the insulating film by photolithography. Then, the insulating film is etched and opened to form the field insulating film 10, and the resist mask is removed. In this way, Figure 6 status.
[0064] Here, the field insulating film 10 can be formed by patterning the insulating film by RIE, or can be formed by patterning by wet etching such as hydrofluoric acid, or can be formed by combining them. When the field insulating film 10 is formed by RIE or wet etching, compared with the case where the insulating film is opened with high precision by dry etching to form the field insulating film 10, the manufacturing can be facilitated or the field insulating film 10 can be formed with high precision in a manner that protects the upper corner 7a of the terminal trench. In addition, compared with the case where the field insulating film 10 is formed by selective oxidation (LOCOS: Local Oxidation of Silicon), the formation time can be shortened and the manufacturing cost can be reduced.
[0065] Figure 7 The state where the second gate electrode 13 is formed on the first gate electrode 9 and the field insulating film 10 covering the upper corner portion 7 a of the termination trench upper end is shown.
[0066] exist Figure 6 In the state of , a conductive material such as polysilicon that becomes the second gate electrode 13 is formed by CVD method, etc., and a resist mask is formed on the polysilicon by photolithography. Next, the polysilicon is etched to form the second gate electrode 13, and the resist mask is removed. In this way, Figure 7 status.
[0067] Figure 8 The interlayer insulating film 14 having the gate contact hole 15 and the backside ohmic electrode 19 formed thereon are shown.
[0068] exist Figure 7In the state, an interlayer insulating film 14 is formed on the first gate electrode 9 and the second gate electrode 13 by a reduced pressure CVD method or the like, and a resist mask is formed on the interlayer insulating film 14 by photolithography. Next, the interlayer insulating film 14 is etched in the active region 40 not shown to provide a source contact hole 17 to be described later, a metal film is formed in contact with the impurity region 4 and the contact region 5, and annealing is performed to form a surface ohmic electrode 18 to be described later. Furthermore, the metal film on the interlayer insulating film 14 is removed by etching, and the resist mask is removed. In addition, a metal film is formed on the back side of the semiconductor substrate 1, and annealing is performed to form a back side ohmic electrode 19. Here, the heating temperature of each annealing treatment can be set to a level of not less than 600°C and not more than 1100°C.
[0069] Furthermore, a resist mask is formed on the interlayer insulating film 14 by photolithography. Next, the interlayer insulating film 14 located outside the termination trench 7 is etched to form a gate contact hole 15 reaching the second gate electrode 13, and the resist mask is removed. Figure 8 status.
[0070] Then, a metal film such as aluminum is formed on the interlayer insulating film 14 and inside the gate contact hole 15 by sputtering or evaporation, and a resist mask is formed on the metal film by photolithography. Next, the metal film is removed by etching to form the gate pad 16 and the surface electrode 20, and the resist mask is removed. Finally, a back electrode 21 is formed on the back ohmic electrode 19 by sputtering or evaporation.
[0071] As mentioned above, manufacturing Figure 3 semiconductor device.
[0072] Next, the operation of the semiconductor device according to this embodiment will be described.
[0073] When a voltage above the threshold is applied between the gate pad 16 and the surface electrode 20, a channel is formed in the well region 3 opposite to the first gate electrode 9, and electrons flow from the impurity region 4 into the drift layer 2. When a voltage is applied between the surface electrode 20 and the back electrode 21 to generate an electric field, electrons reach the back electrode 21 via the drift layer 2 and the semiconductor substrate 1, that is, a current is generated from the back electrode 21 toward the surface electrode 20, and the semiconductor device becomes conductive.
[0074] Here, an electric field is generated in the gate insulating film 8 near the gate trench upper corner 6a and the terminal trench upper corner 7a. However, the first gate electrode 9 is formed to the position of the gate trench upper corner 6a and the terminal trench upper corner 7a or a position lower than the position, and the field insulating film 10 is formed to cover the upper end of the terminal trench upper corner 7a on the side far from the gate trench 6, so that the electric field generated in the gate insulating film 8 near the gate trench upper corner 6a and the terminal trench upper corner 7a is suppressed, and the gate insulating film 8 is prevented from being destroyed. In particular, the second gate electrode 13 is formed above the terminal trench upper corner 7a on the side far from the gate trench 6 through the field insulating film 10 which is thicker than the gate insulating film 8, so that the electric field to the gate insulating film 8 in the gate lead-out portion 70 is suppressed, and the gate insulating film 8 is prevented from being destroyed.
[0075] On the other hand, when a voltage lower than the threshold is applied between the gate pad 16 and the surface electrode 20, a channel is not formed in the well region 3 opposite to the first gate electrode 9, and no current is generated from the back electrode 21 toward the surface electrode 20, and the semiconductor device is in the off state. In the off state of the semiconductor device, a voltage higher than the voltage in the on state is applied between the surface electrode 20 and the back electrode 21, and the depletion layer expands from the well region 3 to the drift layer 2.
[0076] Here, the depletion layer also extends from the first electric field relaxation region 11 and the second electric field relaxation region 12 to the bottom, that is, the drift layer 2. Furthermore, the gate insulating film 8 at the bottom surface or bottom surface corner of the gate trench 6 and the terminal trench 7 is suppressed from being damaged by the electric field generated by the high voltage applied between the surface electrode 20 and the back electrode 21.
[0077] Furthermore, when the semiconductor device switches from the off state to the on state, the voltage applied between the front electrode 20 and the back electrode 21 decreases, and the depletion layer extending into the drift layer 2 shrinks.
[0078] As described above, the semiconductor device in this embodiment operates by alternately repeating the on state and the off state.
[0079] By configuring the semiconductor device in this way, it is possible to obtain a semiconductor device that prevents the gate insulating film 8 formed at the upper corner 7a of the terminal trench on the side far from the gate trench 6 in the gate lead-out portion 70 from being damaged. In addition, compared with the case where the insulating film is opened with high precision by dry etching to form the field insulating film 10, it is possible to facilitate manufacturing or form the field insulating film 10 with high precision in a manner that protects the upper corner 7a of the terminal trench. In addition, compared with the case where the field insulating film 10 is formed by selective oxidation (LOCOS: Local Oxidation of Silicon), the formation time can be shortened and the manufacturing cost can be reduced. In addition, the field insulating film 10 can be formed by wet etching composition, so that over-etching of the first gate electrode 9 is suppressed when the field insulating film 10 is etched.
[0080] In addition, if Figure 1 As shown, the second gate electrode 13 may be formed so as to surround the gate trench 6 in a plan view. In addition, the termination trench 7 or the field insulating film 10 may be formed so as to completely surround the gate trench 6 in a plan view, or may be formed so as to surround the gate trench 6 with an intermittent portion.
[0081] In addition, if Figure 1 As shown in FIG. 1 , the terminal groove 7 is formed on the side of the gate pad 16 in a plan view, but it may not be formed on the side. Fig. 9 As shown, in Figure 1 The terminal trench 7 does not cut off the gate trench 6, but continuously surrounds the gate trench 6 in a plan view. Here, the gate pad 16 is connected to the second gate electrode 13 via a gate contact hole 15 provided in an interlayer insulating film 14 (not shown) on the second gate electrode 13 outside the terminal trench 7. Fig. 9 A gate wiring is formed on the inner side of the gate contact hole 15 provided in the interlayer insulating film 14 (not shown) and on the interlayer insulating film 14 in at least a portion of the terminal region 50 of the partial region 60, and the gate wiring is extended along the second gate electrode 13 or the interlayer insulating film 14 in a plan view to be connected to the gate pad 16. In this case, the gate wiring can be easily formed by forming a metal film and etching at the same time as the gate pad 16 is formed.
[0082] In addition, you can also Figure 1 As shown in FIG. 1 , a channel stop region 23 is provided in the terminal region 50 to suppress the extension of the depletion layer to the end of the semiconductor device. The channel stop region 23 is an n-type region provided on the outer peripheral side of the terminal trench 7 and is composed of silicon carbide. The n-type impurity of the channel stop region 23 can be nitrogen or phosphorus, and the impurity concentration of the channel stop region 23 is 1×10 18 cm -3 Above and 1×10 21 cm-3 The thickness of the channel stop region 23 may be the same as or different from the thickness of the impurity region 4. The channel stop region 23 may be provided by ion implantation, or may be formed simultaneously with the impurity region 4 using a resist mask for providing the impurity region 4, or may be formed before or after the impurity region 4 is formed.
[0083] In addition, you can also Figure 1 As shown, the terminal region 50 surrounds the active region 40 and continuously or intermittently sets a peripheral electric field mitigation region 24 such as an FLR (Field Limiting Ring). For example, ion implantation of aluminum, boron, etc. from the surface of the drift layer 2 to a depth of 0.2 to 3 μm not exceeding the drift layer 2, and a p-type peripheral electric field mitigation region 24 is continuously set to surround the active region 40. The p-type impurity concentration of the peripheral electric field mitigation region 24 is set to exceed the impurity concentration of the drift layer 2, and is set to 1×10 15 cm -3 Above and 1×10 19 cm -3 The following will do.
[0084] In addition, the order of the process of forming the well region 3 and the process of forming the impurity region 4 may be exchanged. The method of forming the well region 3 and the impurity region 4 may also be a method of forming the well region 3 by ion implanting n-type impurities on the surface of the well region 3 to set the impurity region 4, forming a resist mask thereon by photolithography, and ion implanting p-type impurities at positions other than the impurity region 4 to form the well region 3.
[0085] In addition, the thickness of the etching mask 22 and the RIE process are adjusted in such a way that the etching mask 22 is left after the gate trench 6 and the terminal trench 7 are formed, but the etching mask 22 can also be removed without being left, and ion implantation using a resist mask formed by photolithography can be used to form the first electric field relaxation region 11 and the second electric field relaxation region 12.
[0086] In addition, the first electric field relaxation region 11 may be formed simultaneously with the second electric field relaxation region 12, or may be formed before or after the first electric field relaxation region 11 is formed. Furthermore, p-type impurities may be ion-implanted into the opening of the gate trench 6 from an oblique direction to form a p-type semiconductor layer in the drift layer 2 in contact with the side surface of the gate trench 6, and the first electric field relaxation region 11 and the well region 3 may be electrically connected via the semiconductor layer. When the first electric field relaxation region 11 and the well region 3 are electrically connected, the frequency characteristics of the semiconductor device are improved compared to the state in which the first electric field relaxation region 11 is in a floating state.
[0087] Furthermore, although an example of a MOSFET is shown as the semiconductor device, in the case of an IGBT, the conductivity type of the semiconductor substrate 1 may be set to a p-type, and the semiconductor substrate 1 may be polished to be thinner. Implementation method 2.
[0088] In the first embodiment, an example in which the second gate electrode 13 is not branched at the connection portion between the first gate electrode 9 and the second gate electrode 13 is shown, but in the present embodiment, an example in which the second gate electrode 13 has a plurality of branched, i.e., mutually separated, lead portions is described. The other structures are the same as those in the first embodiment.
[0089] Fig.10 is a schematic diagram showing a schematic structure of a semiconductor device in this embodiment, and Figure 1 The figure corresponds to the cross section and top surface of the partial area 60. Fig.10 As shown, the second gate electrode 13 includes a second gate electrode lead portion 13 a and a second gate electrode outer peripheral portion 13 b , and the second gate electrode lead portion 13 a branched from the second gate electrode outer peripheral portion 13 b is connected to the first gate electrode 9 .
[0090] A plurality of second gate electrode lead portions 13a are formed apart from each other, are in contact with the field insulating film 10 and the first gate electrode 9 formed in the terminal trench 7, and are supported by the field insulating film 10 from the inside to the outside of the terminal trench 7 in the extending direction of the gate trench 6. That is, the second gate electrode lead portion 13a is continuously formed from a step above the upper surface of the first gate electrode 9 that exceeds the end of the field insulating film 10 to the upper surface of the field insulating film 10, covering the end of the field insulating film 10 above the terminal trench 7. In addition, as Fig.10 As shown, the end portion of the field insulating film 10 is exposed in the separated regions of the plurality of second gate electrode lead-out portions 13 a.
[0091] The second gate electrode peripheral portion 13b is formed on the field insulating film 10 and is in contact with the second gate electrode lead portion 13a. The second gate electrode peripheral portion 13b is a wiring that connects the first gate electrode 9 formed in the terminal trench 7 to the gate pad 16 via the second gate electrode lead portion 13a. The second gate electrode peripheral portion 13b is connected to the gate pad 16 via the gate contact hole 15 of the second gate electrode 13 that reaches the interlayer insulating film 14 provided outside the terminal trench 7. The gate pad 16 is also formed on the interlayer insulating film 14. Here, the gate contact hole 15 may also be provided in the interlayer insulating film on the second gate electrode lead portion 13a.
[0092] The semiconductor device thus constructed can also obtain the same effects as those of the first embodiment. In addition, when a plurality of second gate electrode lead-out portions 13a are formed to be spaced apart from each other, as shown in the perspective view, Figure 1 The cross-section and top surface of the partial area 60 of the accompanying drawings correspond to Fig.11 As shown, the terminal trench 7 can be divided and formed. That is, the terminal trench 7 can be intermittently provided to surround the active region 40 in which the gate trench 6 is formed. Thus, when the first gate electrode 9 is formed inside the terminal trench 7 by etching back, the etching back can be advanced in the same manner as the gate trench 6 connected to the divided terminal trench 7, and the disappearance of the first gate electrode 9 due to etching back can be suppressed. Implementation method 3.
[0093] In the first embodiment, an example in which gate trenches 6 are provided in stripes in plan view is described, but in this embodiment, an example in which gate trenches 6 are provided in a lattice in plan view is described. The other structures are the same as those in the first embodiment.
[0094] Fig.12 1 is a schematic top view showing the schematic structure of the semiconductor device in this embodiment. Fig.12 As shown, gate trenches 6 are arranged in a grid pattern in the active region 40, and first gate electrodes 9 are formed inside the gate trenches 6. Here, a plurality of gate trenches 6 are arranged in an orthogonal grid pattern throughout the active region 40, but they may also be arranged in a staggered pattern with non-orthogonal portions.
[0095] Fig.13 is a schematic diagram showing a schematic structure of a semiconductor device in this embodiment, Fig.12 Even in the case where the gate trenches 6 are arranged in a grid pattern, as shown in FIG. Fig.13 As shown, the depth of the gate trench 6 is preferably the same as the depth of the terminal trench 7 or is formed to the same extent. Fig.13 , an example is shown in which a source contact hole 17 is provided in the interlayer insulating film 14 in the active region 40, and a contact region 5 and a surface ohmic electrode 18 in contact with the contact region 5 are formed, but the contact region 5 and the surface ohmic electrode 18 may not be formed. Here, the surface ohmic electrode 18 is composed of a reaction product of a metal film mainly composed of nickel and the semiconductor substrate 1, such as nickel silicide.
[0096] The semiconductor device thus constructed can also achieve the same effects as those of Embodiment 1. In addition, when the gate trenches 6 are arranged in a grid pattern, compared with a structure in which the gate trenches 6 are arranged in a stripe pattern, power loss due to the resistance of the first gate electrode 9 during switching operation of the semiconductor device can be suppressed.
[0097] In each embodiment of the present disclosure, the material, size, shape, relative arrangement relationship, implementation conditions, etc. of each component may be described, but these are examples and are not limited to the description of each embodiment.
[0098] In addition, numerous modifications not shown in the examples are contemplated within the scope of each embodiment. For example, this includes the case where any constituent element is deformed, any constituent element is added, or any constituent element is omitted. Furthermore, this also includes the case where constituent elements in each embodiment are extracted and combined.
[0099] In addition, as long as no contradiction occurs, each embodiment may include one or more constituent elements of the invention. Furthermore, constituent elements of the invention are conceptual units, and there are examples where the constituent elements are composed of a plurality of structures or correspond to a part of a structure.
Claims
1. A semiconductor device comprising: A drift layer of a first conductivity type; A well region of the second conductivity type is provided on the surface layer of the drift layer; An impurity region of the first conductivity type is disposed in a surface layer of the well region; A gate trench extending from a surface of the impurity region through the well region and reaching the drift layer; a terminal trench connected to the gate trench in a plan view, wherein the width of the terminal trench in the extension direction of the gate trench is wider than the width of the gate trench; A gate insulating film is formed in contact with the inner surfaces of the gate trench and the terminal trench; a first gate electrode formed on the inner wall and bottom surface of the gate trench and the terminal trench via the gate insulating film; a field insulating film, which is in contact with the first gate electrode formed in the terminal trench, is formed from the inside to the outside of the terminal trench so as to cover the upper corner of the terminal trench on the side farther from the gate trench in the extension direction, and has a thickness thicker than that of the gate insulating film; as well as The second gate electrode is in contact with the field insulating film and the first gate electrode formed in the termination trench, and is supported on the field insulating film from the inside to the outside of the termination trench in the extending direction.
2. The semiconductor device according to claim 1, It is characterized in that The second gate electrode has: A plurality of second gate electrode lead-out portions are formed apart from each other, are in contact with the field insulating film and the first gate electrode formed in the terminal trench, and are supported by the field insulating film from the inside to the outside of the terminal trench in the extending direction; as well as The second gate electrode outer peripheral portion is formed on the field insulating film and is in contact with the second gate electrode lead portion.
3. The semiconductor device according to claim 1 or 2, It is characterized in that Also available: A gate pad connected to the second gate electrode via a gate contact hole reaching the second gate electrode in an interlayer insulating film provided outside the termination trench.
4. The semiconductor device according to any one of claims 1 to 3, It is characterized in that The second gate electrode surrounds the gate trench in a plan view.
5. The semiconductor device according to any one of claims 1 to 4, It is characterized in that The width of the terminal trench in the extending direction is less than or equal to three times the width of the gate trench.
6. The semiconductor device according to any one of claims 1 to 5, It is characterized in that The thickness of the field insulating film is at least twice the thickness of the gate insulating film.
7. The semiconductor device according to any one of claims 1 to 6, It is characterized in that An upper end of the first gate electrode formed in the termination trench is located below an upper end of the termination trench in a cross-sectional view.
8. The semiconductor device according to any one of claims 1 to 7, It is characterized in that The first gate electrode and the second gate electrode are made of different materials.
9. The semiconductor device according to any one of claims 1 to 8, It is characterized in that The gate trenches are arranged in a stripe shape or a lattice shape.
10. The semiconductor device according to any one of claims 1 to 9, It is characterized in that An electric field relaxation region of the second conductivity type is provided below at least one of the bottom surface of the gate trench and below the bottom surface of the termination trench.
11. A method for manufacturing a semiconductor device, comprising: A step of forming a drift layer of a first conductivity type; A step of providing a well region of a second conductivity type in a surface layer of the drift layer; A step of providing an impurity region of a first conductivity type in a surface layer of the well region; A step of providing a gate trench penetrating from the surface of the impurity region through the well region and reaching the drift layer; A step of providing a terminal trench connected to the gate trench in a plan view and having a width in an extending direction of the gate trench wider than a width of the gate trench; forming a gate insulating film in contact with the inner wall and bottom surface of the gate trench and the terminal trench; forming a first gate electrode inside the gate trench and the terminal trench via the gate insulating film; A step of forming a field insulating film, the field insulating film being in contact with the first gate electrode formed in the terminal trench, covering the upper corner of the terminal trench on the side farther from the gate trench in the extending direction from the inside to the outside of the terminal trench, and setting the thickness of the field insulating film to be greater than the thickness of the gate insulating film; as well as A step of forming a second gate electrode, the second gate electrode being in contact with the field insulating film and the first gate electrode formed in the termination trench, and being supported by the field insulating film from the inside to the outside of the termination trench in the extending direction.
12. The method for manufacturing a semiconductor device according to claim 11, It is characterized in that The field insulating film is formed by patterning through reactive ion etching or wet etching.
13. The method for manufacturing a semiconductor device according to claim 11 or 12, It is characterized in that The field insulating film is formed by a CVD method.
14. The method for manufacturing a semiconductor device according to any one of claims 11 to 13, It is characterized in that The first gate electrode is formed by etching back so as to be located below the upper end of the termination trench in a cross-sectional view.
15. The method for manufacturing a semiconductor device according to any one of claims 11 to 14, It is characterized in that Also available: forming an interlayer insulating film on the second gate electrode and on the first gate electrode formed in the termination trench; A step of providing a gate contact hole reaching the second gate electrode in the interlayer insulating film outside the termination trench; and A step of forming a gate pad on the second gate electrode via the gate contact hole.