Ceramic wine container preparation method for reducing fusel oil content in wine and firing device
By designing a multi-angle controlled firing device, the problem of instability of temperature and oxidizing atmosphere during the firing of ceramic wine vessels has been solved, and the ceramic wine vessels have been able to effectively reduce the fusel oil content in wine and stabilize product quality. properties to avoid poor sintering and deformation.
Patent Information
- Application Number
- CN202410783925.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-18
- Publication Date
- 2024-10-18
AI Technical Summary
The existing ceramic wine vessel preparation method and firing device cannot provide a constant temperature and oxidizing atmosphere environment, resulting in the ceramic wine vessel's functionality to reduce the fusel oil content in wine being unstable, and there are problems with poor sintering and deformation of the product.
A firing device including a lower support rod, an upper adjustment table, a lateral communication pipe, a valve and a heating pipe is designed. Through the control of multiple angles and temperatures, combined with the operation of the display screen and knobs, the ceramic blanks can be easily processed. Precise temperature and oxidation atmosphere adjustments are made to ensure the uniformity and stability of the firing process.
It achieves efficient firing of ceramic wine vessels, ensures the stability and consistency of product quality, reduces the fusel oil content in wine, and optimizes energy utilization efficiency and environmental protection performance.
Smart Images

Figure CN118794249A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of ceramic wine vessel preparation, in particular to a ceramic wine vessel preparation method and a firing device for reducing fusel oil content in wine. Background Art
[0002] Fusel oil is a monohydric higher alcohol with carbon number greater than or equal to 3 formed by the decomposition of proteins, amino acids, sugars, etc. in the raw materials during the grain wine brewing process. It mainly includes isopentanol, isobutanol and n-propanol. The production of fusel oil is closely related to the wine brewing process. The type of raw materials, the type and amount of koji yeast, the culture temperature and time, the fermentation temperature and time, and the distillation process will affect the content of fusel oil in the wine. The content of fusel oil in the wine can be reduced by optimizing the fermentation process, but traditional methods generally have the problem of complex processes. Moreover, changing the mature brewing process will bring high costs, product quality stability problems, and bring risks to enterprises.
[0003] The current ceramic wine vessel preparation method and firing device may have some defects, depending on the actual design and use. The body material formula of the ceramic wine glass is: Al2O3, SiO2, K2O, Na2O, Fe2O3, MgO. The formula of basic glaze A is: potassium feldspar, sodium feldspar, calcite, talc, kaolin, zinc oxide, quartz, barium carbonate and aluminum oxide. The formula of functional glaze B is: clay, far-infrared ceramic material, Bian stone, shale and limestone. When the above materials are used to prepare ceramic wine vessels, due to the particularity of the formula, the firing temperature of each part of the ceramic wine vessel must be uniform to ensure that the quality of the ceramic wine vessel is not deformed, and the concentration of the oxidizing atmosphere in the furnace body is required to be within a certain range, otherwise it will affect the function of the ceramic wine vessel to reduce the content of fusel oil in the wine. The current firing device has certain defects and cannot provide a constant temperature and ensure the sintering atmosphere environment conditions, resulting in the instability of the ceramic wine vessel's functionality to reduce the content of fusel oil in the wine, as well as the problems of poor sintering and deformation of the product. Summary of the invention
[0004] 1. Technical issues to be resolved
[0005] In view of the deficiencies in the prior art, the present invention provides a method for preparing a ceramic wine vessel and a firing device for reducing the fusel oil content in wine, thereby solving the problem that machine firing of ceramics with special formulas affects product performance.
[0006] (II) Technical solution
[0007] To achieve the above purpose, the present invention is implemented by the following technical scheme: a ceramic wine vessel firing device for reducing the content of fusel oil in wine, comprising:
[0008] A lower support rod, the upper surface of which is fixedly connected to a box, the upper surface of which is fixedly connected to an upper adjustment platform, the side surface of which is fixedly connected to a lateral connecting pipe, the end of which away from the box is fixedly connected to a valve, the inner surface of which is fixedly connected to a fixing plate, the inner surface of which is fixedly connected to a heating pipe;
[0009] The side surface of the lower support rod is fixedly connected with a lower fixing plate, the upper surface of the lower fixing plate is fixedly connected with a telescopic rod, the output end of the telescopic rod is fixedly connected with a lower horizontal plate, the upper surface of the lower horizontal plate is fixedly connected with an intermediate fixing rod, the side surface of the intermediate fixing rod is provided with a through hole, the outer surface of the intermediate fixing rod is provided with a horizontal separation plate, and the interior of the box is fixedly connected with a thermal insulation layer;
[0010] The inner surface of the box body is slidably connected to a limit plate, the front surface of the limit plate is fixedly connected to a limit rod, the outer surface of the limit rod is slidably connected to a sleeve, and the lower surface of the lower horizontal separation plate is fixedly connected to a limit sliding rod.
[0011] Preferably, a display screen is provided on the front surface of the upper adjustment platform, and a knob is provided on the front surface of the upper adjustment platform.
[0012] Preferably, one end of the valve away from the lateral connecting pipe is fixedly connected with a flange, and the number of the lateral connecting pipes is two and they are distributed on the left and right.
[0013] Preferably, one end of the lateral connecting pipe away from the valve is fixedly connected to a separation pipe, a vent hole is provided on the side surface of the separation pipe, and a lower roller is provided on the lower surface of the lower support rod.
[0014] Preferably, a limiting round rod is provided on the outer surface of the horizontal separation plate, and the limiting round rod extends to the inside of the through hole.
[0015] Preferably, a cavity is formed inside the thermal insulation layer, and the heating tube is electrically connected to an external power source.
[0016] Preferably, the side surface of the collar is fixedly connected to the lower horizontal plate, the front limit plate is fixedly connected to the inner surface of the insulation layer, the upper limit plate is fixedly connected to the limit sliding rod, the front surface of the box body is rotatably connected to the box door, the front surface of the box door is fixedly connected to a handle, the front surface of the box door is threadedly connected to a fixed wheel, the side surface of the box body is fixedly connected to a fixed block, and the fixed block is threadedly connected to the fixed wheel.
[0017] A method for preparing a ceramic wine vessel for reducing the content of fusel oil in wine comprises the following steps:
[0018] S1. Mix the ceramic wine vessel blank material with the formula of Al2O3, SiO2, K2O, Na2O, Fe2O3, and MgO in the mass ratio of 18:72:4.7:1.11:0.7:3.49, add water and ball-mill to 200 mesh, take out and age for 7 days, and then press or grout to make a blank of the required shape; dry the obtained ceramic wine vessel blank;
[0019] S2, the dried green body is placed in the device for biscuit firing, and then naturally cooled to room temperature. The firing system is specifically divided into five stages: 25-80°C, 20 minutes, 80-140°C, 60 minutes, 140-300°C, 40 minutes, 300-850°C, 120 minutes, 850°C, constant temperature for 20 minutes. During the firing process, the telescopic rod moves up and down to facilitate the control of a more uniform temperature.
[0020] S3. At room temperature, take out the bisque-fired body from the kiln, blow and clean it to remove dust on the surface of the body and then set it aside for use;
[0021] S4, prepare the raw material of basic glaze A, then ball-mill it to 250 mesh, prepare the raw material of functional glaze B, then ball-mill it to 200 mesh, mix the basic glaze A and functional glaze B evenly according to the proportion, and then adjust them into glaze slurry with water, wherein the mass ratio of glaze to water is 1:1.5, and glaze the body by dipping, and set it aside after drying, the dipping time is 4 to 10 seconds, and there is no need to take out the whole device during the glazing process, slide out the lower horizontal plate for easy operation, and slide between the ring and the limit rod;
[0022] S5. The glazed body is placed in the electric kiln for oxidizing flame firing. The lateral connecting pipe can adjust the amount of oxidizing gas entering. It is then naturally cooled to room temperature to obtain a ceramic wine vessel. The firing system is specifically divided into seven stages: 25-150°C, 120 min, 150-350°C, 70 min, 350-650°C, 80 min, 650°C, constant temperature for 10 min, 650-1100°C, 110 min, 1100-1200°C, 60 min, 1200°C, constant temperature for 30 min.
[0023] (III) Beneficial effects
[0024] The present invention provides a method for preparing a ceramic wine vessel and a firing device for reducing the content of fusel oil in wine. The invention has the following beneficial effects:
[0025] The device includes multiple components such as the lower support rod, the upper adjustment platform, the lateral connecting pipe, the valve, the heating pipe and other components. These designs can realize the control and adjustment of the firing process of the ceramic wine vessel at multiple angles and different temperatures. Through the cooperation of the heating system and the control system, the temperature in the furnace body can be accurately controlled to ensure that the ceramic blank reaches the ideal temperature curve during the firing process, which is beneficial to the stability and consistency of product quality. The design of the device takes into account the convenience of operation. For example, a display screen and a knob are set on the upper adjustment platform. The arrangement of the lateral connecting pipe and the valve makes it more convenient to adjust the gas, and the gas in the furnace body can be accurately adjusted to ensure that the ceramic glaze reaches the ideal oxidizing atmosphere during the firing process. Ensure that the ceramic wine vessel can reduce the content of fusel oil in the wine. The setting of the telescopic rod and the roller facilitates the movement and adjustment of the furnace body. The insulation layer design in the device can effectively reduce energy loss. The heating pipe is electrically connected to the external power supply to optimize the energy utilization efficiency. At the same time, the design of the emission system helps to reduce exhaust gas emissions and meets environmental protection requirements. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a schematic diagram of the internal structure of the present invention;
[0027] Figure 2 for Figure 1 A schematic diagram of the structure enlargement in the middle;
[0028] Figure 3 for Figure 1 A magnified schematic diagram of the structure at B in the middle;
[0029] Figure 4 It is a partial structural schematic diagram of the present invention;
[0030] Figure 5 It is a schematic diagram of the overall structure of the present invention.
[0031] Among them, 1. lower support rod; 2. lower roller; 3. lower fixed plate; 4. box body; 5. box door; 6. handle; 7. fixed wheel; 8. fixed block; 9. lateral connecting pipe; 10. valve; 11. upper adjustment table; 12. display screen; 13. knob; 14. cavity; 15. lower horizontal plate; 16. limit plate; 17. ring; 18. limit rod; 19. middle fixed rod; 20. horizontal separation plate; 21. heating tube; 22. flange; 23. separation tube; 24. vent; 25. fixed plate; 26. telescopic rod; 27. insulation layer; 28. limit sliding rod. DETAILED DESCRIPTION
[0032] The technical solutions in the embodiments of the present invention are described clearly and completely. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0033] like Figure 1-5 As shown, the embodiment of the present invention provides a method for preparing a ceramic wine vessel for reducing the content of fusel oil in wine and a firing device, comprising a lower support rod 1, the upper surface of the lower support rod 1 is fixedly connected to a box body 4, the upper surface of the box body 4 is fixedly connected to an upper adjustment platform 11, the front surface of the upper adjustment platform 11 is provided with a display screen 12, the front surface of the upper adjustment platform 11 is provided with a knob 13, the side surface of the box body 4 is fixedly connected to a lateral connecting pipe 9, the end of the lateral connecting pipe 9 away from the box body 4 is fixedly connected to a valve 10, the end of the valve 10 away from the lateral connecting pipe 9 is fixedly connected to a flange 22, the number of the lateral connecting pipes 9 is two and they are distributed on the left and right, the end of the lateral connecting pipe 9 away from the valve 10 is fixedly connected to a separation pipe 23, the side surface of the separation pipe 23 is provided with a vent hole 24, the lower surface of the lower support rod 1 is provided with a lower roller 2, the inner surface of the box body 4 is fixedly connected to a fixing plate 25, and the inner surface of the fixing plate 25 is fixedly connected to a heating pipe 21.
[0034] The side surface of the lower support rod 1 is fixedly connected with the lower fixing plate 3, the upper surface of the lower fixing plate 3 is fixedly connected with the telescopic rod 26, the output end of the telescopic rod 26 is fixedly connected with the lower horizontal plate 15, the upper surface of the lower horizontal plate 15 is fixedly connected with the middle fixing rod 19, the side surface of the middle fixing rod 19 is provided with a through hole, the outer surface of the middle fixing rod 19 is provided with a horizontal separation plate 20, the outer surface of the horizontal separation plate 20 is provided with a limiting round rod, the limiting round rod extends to the inside of the through hole, the inside of the box body 4 is fixedly connected with the thermal insulation layer 27, the inside of the thermal insulation layer 27 forms a cavity 14, and the heating tube 21 is electrically connected to the external power supply.
[0035] The inner surface of the box body 4 is slidably connected to the limit plate 16, the front surface of the limit plate 16 is fixedly connected to the limit rod 18, the outer surface of the limit rod 18 is slidably connected to the ring 17, the side surface of the ring 17 is fixedly connected to the lower horizontal plate 15, the front limit plate 16 is fixedly connected to the inner surface of the insulation layer 27, the upper limit plate 16 is fixedly connected to the limit sliding rod 28, the front surface of the box body 4 is rotatably connected to the box door 5, the front surface of the box door 5 is fixedly connected to the handle 6, the front surface of the box door 5 is threadedly connected to the fixed wheel 7, the side surface of the box body 4 is fixedly connected to the fixed block 8, the fixed block 8 is threadedly connected to the fixed wheel 7, and the lower surface of the lower horizontal separation plate 20 is fixedly connected to the limit sliding rod 28.
[0036] A method for preparing a ceramic wine vessel for reducing the content of fusel oil in wine comprises the following steps:
[0037] S1. Mix the ceramic wine vessel blank materials with the formula of Al2O3, SiO2, K2O, Na2O, Fe2O3, and MgO in the mass ratio of 18:72:4.7:1.11:0.7:3.49, add water and ball-mill to 200 mesh, take out and age for 7 days, and then press or grout to make a blank of the desired shape; the obtained ceramic wine vessel blank is dried.
[0038] S2. The dried green body is placed in the device for bisque firing, and then naturally cooled to room temperature. The firing system is specifically divided into five stages: 25-80°C, 20 minutes, 80-140°C, 60 minutes, 140-300°C, 40 minutes, 300-850°C, 120 minutes, 850°C, constant temperature for 20 minutes. During the firing process, the telescopic rod 26 moves up and down to facilitate the control of a more uniform temperature.
[0039] S3. At room temperature, take the bisque-fired body out of the kiln, blow it clean to remove dust on the surface of the body and then set it aside for use.
[0040] S4. Functional glaze raw materials are prepared, and then ball-milled to 250 meshes, and then adjusted to glaze slurry with water, wherein the mass ratio of glaze to water is 1:1.5. The green body is coated with glaze slurry by dipping glaze, and then dried for standby use. The dipping time is 4 to 10 seconds. During the glazing process, there is no need to take out the entire device. The lower horizontal plate 15 is slid out for easy operation, and the sleeve ring 17 slides between the limit rod 18.
[0041] S5. The glazed body is placed in the electric kiln for reducing flame firing. The lateral connecting pipe 9 can adjust the amount of oxidizing gas entering. It is then naturally cooled to room temperature to obtain a ceramic wine vessel. The firing system is specifically divided into seven stages: 25-150°C, 120 min, 150-350°C, 70 min, 350-650°C, 80 min, 650°C, constant temperature for 10 min, 650-1100°C, 110 min, 1100-1200°C, 60 min, 1200°C, constant temperature for 30 min.
[0042] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A ceramic wine vessel firing device for reducing the fusel oil content in wine, characterized in that: include: A lower support rod (1), the upper surface of the lower support rod (1) is fixedly connected to a box body (4), the upper surface of the box body (4) is fixedly connected to an upper adjustment platform (11), the side surface of the box body (4) is fixedly connected to a lateral connecting pipe (9), the end of the lateral connecting pipe (9) away from the box body (4) is fixedly connected to a valve (10), the inner surface of the box body (4) is fixedly connected to a fixing plate (25), and the inner surface of the fixing plate (25) is fixedly connected to a heating pipe (21); The side surface of the lower support rod (1) is fixedly connected to a lower fixing plate (3), the upper surface of the lower fixing plate (3) is fixedly connected to a telescopic rod (26), the output end of the telescopic rod (26) is fixedly connected to a lower horizontal plate (15), the upper surface of the lower horizontal plate (15) is fixedly connected to an intermediate fixing rod (19), the side surface of the intermediate fixing rod (19) is provided with a through hole, the outer surface of the intermediate fixing rod (19) is provided with a horizontal separation plate (20), and the interior of the box body (4) is fixedly connected to a heat-insulating layer (27); The inner surface of the box body (4) is slidably connected to a limit plate (16), the front surface of the limit plate (16) is fixedly connected to a limit rod (18), the outer surface of the limit rod (18) is slidably connected to a collar (17), and the lower surface of the lower horizontal separation plate (20) is fixedly connected to a limit sliding rod (28).
2. The ceramic wine vessel firing device for reducing fusel oil content in wine according to claim 1, characterized in that: A display screen (12) is provided on the front surface of the upper adjustment platform (11), and a knob (13) is provided on the front surface of the upper adjustment platform (11).
3. The ceramic wine vessel firing device for reducing fusel oil content in wine according to claim 1, characterized in that: One end of the valve (10) away from the lateral connecting pipe (9) is fixedly connected with a flange (22), and the number of the lateral connecting pipes (9) is two and they are distributed on the left and right.
4. The ceramic wine vessel firing device for reducing fusel oil content in wine according to claim 1, characterized in that: The end of the lateral connecting pipe (9) away from the valve (10) is fixedly connected to a separation pipe (23), the side surface of the separation pipe (23) is provided with a vent hole (24), and the lower surface of the lower support rod (1) is provided with a lower roller (2).
5. The ceramic wine vessel firing device for reducing fusel oil content in wine according to claim 1, characterized in that: The outer surface of the horizontal separation plate (20) is provided with a limiting round rod, and the limiting round rod extends to the inside of the through hole.
6. The ceramic wine vessel firing device for reducing fusel oil content in wine according to claim 1, characterized in that: A cavity (14) is formed inside the thermal insulation layer (27), and the heating tube (21) is electrically connected to an external power source.
7. The ceramic wine vessel firing device for reducing fusel oil content in wine according to claim 1, characterized in that: The side surface of the collar (17) is fixedly connected to the lower horizontal plate (15), the front limiting plate (16) is fixedly connected to the inner surface of the insulation layer (27), the upper limiting plate (16) is fixedly connected to the limiting sliding rod (28), the front surface of the box body (4) is rotatably connected to the box door (5), the front surface of the box door (5) is fixedly connected to the handle (6), the front surface of the box door (5) is threadedly connected to the fixed wheel (7), the side surface of the box body (4) is fixedly connected to the fixed block (8), and the fixed block (8) is threadedly connected to the fixed wheel (7).
8. A method for preparing a ceramic wine vessel for reducing the content of fusel oil in wine, characterized in that: The following steps are involved: S1. Mix the ceramic wine vessel blank material with the formula of Al2O3, SiO2, K2O, Na2O, Fe2O3, and MgO in the mass ratio of 18:72:4.7:1.11:0.7:3.49, add water and ball-mill to 200 mesh, take out and age for 7 days, and then press or grout to make a blank of the required shape; dry the obtained ceramic wine vessel blank; S2, placing the dried green body in the device for biscuit firing, and then naturally cooling to room temperature, the firing system is specifically divided into five stages: 25-80°C, 20 minutes, 80-140°C, 60 minutes, 140-300°C, 40 minutes, 300-850°C, 120 minutes, 850°C, constant temperature for 20 minutes, during the firing process, the telescopic rod (26) moves up and down to facilitate the control of temperature more uniformly; S3. At room temperature, take out the bisque-fired body from the kiln, blow and clean it to remove dust on the surface of the body and then set it aside for use; S4, prepare the raw material of basic glaze A, then ball-mill it to 250 mesh, prepare the raw material of functional glaze B, then ball-mill it to 200 mesh, mix the basic glaze A and functional glaze B evenly according to the proportion, and then adjust them into glaze slurry with water, wherein the mass ratio of glaze to water is 1:1.5, and apply glaze slurry to the body by dipping glaze, and then dry it for standby use, the dipping time is 4 to 10 seconds, and the whole device does not need to be taken out during the glazing process, and the lower horizontal plate (15) is slid out for easy operation, and the sleeve ring (17) and the limit rod (18) are slid between them; S5. The glazed body is placed in the electric kiln for oxidizing flame firing. The lateral connecting pipe (9) can adjust the amount of oxidizing gas entering. It is then naturally cooled to room temperature to obtain a ceramic wine vessel. The firing system is specifically divided into seven stages: 25-150°C, 120 min, 150-350°C, 70 min, 350-650°C, 80 min, 650°C, constant temperature for 10 min, 650-1100°C, 110 min, 1100-1200°C, 60 min, 1200°C, constant temperature for 30 min.