Color developing structure and preparation method thereof
By arranging texture grooves and covering the color layer on the surface of the substrate of the structural color material, the particle size of the color particles is adjusted, which solves the problem of single specular reflection in the existing technology and achieves richer color expression and application scenario expansion.
Patent Information
- Application Number
- CN202310470958.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-21
- Publication Date
- 2024-10-22
AI Technical Summary
Due to the single specular reflection effect of existing structural color materials, their use scenarios are limited and they cannot effectively weaken the problem of specular reflection.
By setting texture grooves on the surface of the substrate and covering the color layer, the color layer includes a photonic crystal structure layer or a metal film layer, and the average particle size of the color particles does not exceed 35 microns, or by adding a photonic crystal structure layer or a metal film layer The colored particles are obtained by crushing, and a colored layer is formed on the substrate. The difference in roughness and smoothness of the colored layer or the size of the particles are adjusted to weaken the specular reflection and enhance the scattering performance.
It achieves weakening the mirror effect of the color layer, enhances the scattering performance, provides richer color expression and matte metallic or milky white appearance, and expands the application range of structural colors.
Smart Images

Figure CN118818641A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of biological structural color materials, and in particular to a color development structure and a preparation method thereof. Background Art
[0002] Color is an important carrier of visual information in nature. Traditional chemical pigments produce color through light absorption or luminescence, but they inevitably pollute the environment. In order to overcome these shortcomings, people have proposed the concept of structural color. Its principle is based on the interference of nano-periodic structures on light. By adjusting the physical size of the nanostructure and the optical properties of the constituent materials, different colors can be achieved. Compared with traditional chemical dyes and pigments, it is more environmentally friendly. Since the structure that produces structural color is at the nanometer level and is very small, the structural color usually presents a mirror reflection effect. This feature results in a relatively simple appearance of structural color, the lack of some color effects, and the use scenarios are limited to a certain extent. Summary of the invention
[0003] The main technical problem solved by the present invention is to provide a color display structure and a preparation method thereof, so as to solve the problem that the mirror reflection cannot be weakened in the prior art.
[0004] In order to solve the above technical problems, the first technical solution adopted by the present invention is: to provide a color development structure, the color development structure comprising:
[0005] A substrate having a first surface and a second surface disposed opposite to each other;
[0006] A color development layer covering the first surface of the substrate;
[0007] The roughness of the first surface is greater than the roughness of the second surface, or the average particle size of the color-developing particles forming the color-developing layer does not exceed 35 micrometers.
[0008] The color development layer includes a photonic crystal structure layer or a metal film layer, and the photonic crystal structure layer includes at least two alternately stacked layers of materials with different refractive indices.
[0009] When the roughness of the first surface is greater than that of the second surface, a groove is formed on the first surface, the color developing layer at least covers the inner wall surface of the groove, and the width of the groove is less than 15 microns.
[0010] When the roughness of the first surface is greater than that of the second surface, a groove is formed on the first surface, the color developing layer at least covers the inner wall surface of the groove, and the width of the groove is greater than 15 microns.
[0011] The color-developing particles are obtained by crushing a photonic crystal structure layer or a metal film layer; or, by growing seed particles; and the size of the seed particles is smaller than the size of the color-developing particles.
[0012] Wherein, the average particle size of the color-developing particles does not exceed 15 microns.
[0013] The average particle size of the color-developing particles is 10 microns.
[0014] The color display structure further includes a refractive index matching layer, and the refractive index matching layer is arranged on a surface of the photonic crystal structure layer which is away from the substrate.
[0015] The difference between the refractive index of the refractive index matching layer and the refractive index of the substrate does not exceed 0.2.
[0016] The substrate is a silicon wafer, a glass wafer or a quartz wafer.
[0017] In order to solve the above technical problems, the second technical solution adopted by the present invention is: to provide a method for preparing a color-developing structure, the method for preparing a color-developing structure comprising:
[0018] Obtaining a substrate; the substrate having a first surface and a second surface;
[0019] performing a roughening process on the first surface of the substrate;
[0020] A color development layer is disposed on the roughened first surface.
[0021] In order to solve the above technical problems, the third technical solution adopted by the present invention is: to provide a method for preparing a color-developing structure, the method for preparing a color-developing structure comprising:
[0022] obtaining a substrate;
[0023] A coating layer containing color-developing particles is coated on the surface of the substrate to form a color-developing layer; wherein the average particle size of the color-developing particles does not exceed 35 micrometers.
[0024] The method for obtaining the color-developing particles includes:
[0025] Obtaining a substrate;
[0026] Forming a prefabricated film on the surface of the substrate; the prefabricated film includes a photonic crystal structure layer or a metal film layer;
[0027] The prefabricated film is separated from the substrate, and the prefabricated film is crushed to obtain color-developing particles.
[0028] The method for obtaining the color-developing particles includes: obtaining seed particles; the size of the seed particles is smaller than the size of the color-developing particles; and obtaining the color-developing particles by growing the seed particles.
[0029] The beneficial effects of the present invention are as follows: different from the prior art, a color development structure and a preparation method thereof are provided, wherein the color development structure comprises a substrate and a color development layer, wherein the substrate has a first surface and a second surface disposed opposite to each other; the color development layer covers the first surface of the substrate; wherein the roughness of the first surface is greater than the roughness of the second surface, or the average particle size of the color development particles forming the color development layer does not exceed 35 microns. In the present application, by disposing the color development layer on the surface of the substrate with a greater roughness, or by using color development particles with an average particle size of no more than 35 microns to form the color development layer, the reflective performance of the color development layer is weakened, thereby weakening the mirror effect of the color development layer, thereby improving the scattering performance of the color development layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0031] Figure 1 It is a structural schematic diagram of an embodiment of a color development structure provided by the present invention;
[0032] Figure 2 It is a structural schematic diagram of a specific embodiment of a photonic crystal structure layer in a color development structure provided by the present invention;
[0033] Figure 3 It is a structural schematic diagram of a specific embodiment of the color development structure provided by the present invention;
[0034] Figure 4 is a structural schematic diagram of another embodiment of the color development structure provided by the present invention;
[0035] Figure 5 It is a schematic flow chart of an embodiment of a method for preparing a color development structure provided by the present invention;
[0036] Figure 6 It is a schematic flow chart of another embodiment of the method for preparing the color development structure provided by the present invention.
[0037] In the figure: color development structure 100; substrate 10; first surface 11; groove 111; second surface 12; color development layer 20; photonic crystal structure layer 21; refractive index matching layer 30. DETAILED DESCRIPTION
[0038] The scheme of the embodiment of the present application is described in detail below in conjunction with the drawings of the specification.
[0039] In the following description, for the purpose of explanation rather than limitation, specific details such as specific system structures, interfaces, and technologies are provided to facilitate a thorough understanding of the present application.
[0040] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0041] The terms "first", "second", "third" in this application are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. Thus, the features defined as "first", "second", "third" can expressly or implicitly include at least one of the features. In the description of this application, the meaning of "multiple" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined. In the embodiments of this application, all directional indications (such as up, down, left, right, front, back...) are only used to explain the relative position relationship, movement, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication also changes accordingly. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions. For example, a process, method, system, product or device comprising a series of steps or units is not limited to the steps or units listed, but optionally also includes steps or units that are not listed, or optionally also includes other steps or units inherent to these processes, methods, products or devices.
[0042] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0043] In order to enable those skilled in the art to better understand the technical solution of the present invention, a color development structure and a preparation method thereof provided by the present invention are further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0044] See also Figure 1 , Figure 1 It is a structural schematic diagram of an embodiment of a color development structure provided by the present invention.
[0045] In this embodiment, a color development structure 100 is provided, and the color development structure 100 includes a substrate 10 and a color development layer 20. The substrate 10 has a first surface 11 and a second surface 12 disposed opposite to each other. The color development layer 20 covers the first surface 11 of the substrate 10.
[0046] In this embodiment, the substrate 10 may also be a light-transmitting plate. The substrate 10 may be glass or a resin such as polyethylene, acrylic acid, polycarbonate, and polyethylene terephthalate. The substrate 10 may be other light-transmitting materials that can transmit visible light with a wavelength of 380-780 nm. Specifically, the substrate 10 is a glass sheet or a quartz sheet. The refractive index nd of the substrate 10 may be 1.5. In another embodiment, the substrate 10 may also be a non-light-transmitting plate. The substrate 10 may be a silicon sheet or a ceramic sheet; in addition, the substrate 10 may also be paper or fabric, etc. The substrate 10 may be formed into various forms including concave / convex surfaces and curved surfaces, such as thin films and plates.
[0047] In one embodiment, the roughness of the first surface 11 is greater than the roughness of the second surface 12. In this embodiment, the second surface 12 is a smooth surface.
[0048] Specifically, the first surface 11 is provided with a groove 111, and the color development layer 20 covers at least the inner wall surface of the groove 111. The width of the groove 111 may be greater than 15 microns. Furthermore, the width of the groove 111 may be greater than 20 microns. Among them, the pattern of the groove 111 is a wave pattern, a horizontal pattern and / or a vertical pattern. The color development layer 20 is covered on the first surface 11 of the substrate 10 having the groove 111. The groove 111 in the first surface 11 of the substrate 10 improves the color development effect of the color development layer 20 due to the local mirror reflection of the texture. Compared with directly covering the color development layer 20 on a smooth surface, the color development structure 100 in this embodiment presents a weakened mirror effect and presents a non-mirror metal appearance effect. Specifically, the incident light is irradiated from the first surface 11 of the substrate 10 to the direction of the second surface 12, and the color development structure 100 presents a matte metal appearance effect.
[0049] The thickness of the color layer 20 can be set to between 3 nanometers and 5 micrometers. Specifically, the thickness of the color layer 20 can be set to between 3 nanometers and 50 nanometers. Specifically, the thickness of the color layer 20 can be set to between 60 nanometers and 150 nanometers. Specifically, the thickness of the color layer 20 can be set to between 1 micrometer and 5 micrometers.
[0050] Specifically, the first surface 11 is provided with a groove 111, and the color development layer 20 at least covers the inner wall surface of the groove 111, and the width of the groove 111 is less than 15 microns. Furthermore, the width of the groove 111 is less than 10 microns. The color development layer 20 is covered on the first surface 11 of the substrate 10 having the groove 111. The groove 111 in the first surface 11 of the substrate 10 improves the color development effect of the color development layer 20 due to the mirror reflection effect of the dense texture. Compared with directly covering the color development layer 20 on a smooth surface, the color development structure 100 in this embodiment presents a milky white appearance effect, which expands the color development range of the structural color. Furthermore, the width of the groove 111 can also be less than 5 microns.
[0051] In other embodiments, the width and depth of the texture groove 111 may also be adjusted according to the actual color rendering effect required.
[0052] See also Figure 2 , Figure 2 It is a structural schematic diagram of a specific embodiment of the photonic crystal structure layer in the color display structure provided by the present invention.
[0053] In one embodiment, the color development layer 20 is a photonic crystal structure layer 21, and the photonic crystal structure layer 21 includes at least two alternating layers of materials with different refractive indices. In this embodiment, the photonic crystal structure layer 21 is formed by alternating high refractive index materials and low refractive index materials. The high refractive index material includes at least one of titanium oxide, zinc oxide, zirconium oxide, niobium oxide, molybdenum oxide, iron oxide, tantalum oxide, hafnium oxide, cerium oxide, zinc sulfide, lanthanum titanate, etc., and the low refractive index material includes at least one of silicon dioxide, aluminum oxide, magnesium fluoride, calcium fluoride, lithium fluoride, cerium fluoride, organic resin, etc.
[0054] The structure of the stack is ever-changing. Using inorganic materials and polymer materials as the film material of photonic crystals makes photonic crystals have a variety of different properties. It is easy to form and process, the production process is simple, the cost is low, and it is conducive to large-scale production. In addition, there are many types of inorganic materials and polymer materials, and the refractive index and density can be adjusted, which provides a large selection space for the production of photonic crystals.
[0055] The number of layers of the stack is in the range of [11, 21]. The visible light band of the color development layer 20 is adjusted by regulating the film thickness of each stack. The thickness of the photonic crystal structure layer 21 can be set to between 10 nanometers and 5 micrometers. Specifically, the thickness of the photonic crystal structure layer 21 can be set to between 30 nanometers and 50 nanometers. Specifically, the thickness of the photonic crystal structure layer 21 can be set to between 60 nanometers and 150 nanometers. Specifically, the thickness of the photonic crystal structure layer 21 can be set to between 1 micrometer and 5 micrometers. The thickness of the photonic crystal structure layer 21 can be set to between 300 nanometers and 500 nanometers.
[0056] In the present embodiment, light in a wavelength range of 360 nm to 780 nm is used as light in the visible region, and light in a wavelength range of 780 nm to 2526 nm is used as light in the near-infrared region.
[0057] See also Figure 3 , Figure 3 It is a structural schematic diagram of a specific embodiment of the color development structure provided by the present invention.
[0058] The color display structure 100 further includes a refractive index matching layer 30, which is disposed on a surface of the photonic crystal structure layer 21 away from the substrate 10. In this embodiment, the substrate 10 is made of a light-transmitting material that can transmit visible light with a wavelength of 380-780 nm. The material of the refractive index matching layer 30 includes, but is not limited to, organic materials such as resins, such as PMMA (Polymethylmethacrylate), PS (Polystyrene), PDMS (Polydimethylsiloxane), epoxy resin, and the like.
[0059] Specifically, the photonic crystal structure disposed on the first surface 11 of the substrate 10 is highly reflective in the visible light band and highly transparent in the near infrared band. By disposing a refractive index matching layer 30 on the surface of the photonic crystal structure away from the substrate 10, the refractive index matching layer 30 is transparent in the visible light band and the near infrared band, thereby forming a refractive index matching layer 30 that shields or stealths visible light and has high near infrared transmittance on the substrate 10. Furthermore, the band range of high transmittance, stealth, and shielding of the refractive index matching layer 30 can be controlled by controlling the material forming the refractive index matching layer 30. The difference between the refractive index of the refractive index matching layer 30 and the refractive index of the substrate 10 does not exceed 0.2. In a preferred embodiment, the difference between the refractive index of the refractive index matching layer 30 and the refractive index of the substrate 10 does not exceed 0.1.
[0060] In other embodiments, the material and thickness of the refractive index matching layer 30 may also be adjusted according to the actual color rendering effect required.
[0061] In a specific embodiment, the color development layer 20 is a metal film layer. The metal material forming the metal film layer includes but is not limited to iron, copper, manganese, steel, tin alloy, aluminum alloy, magnesium alloy, copper alloy, aluminum alloy and zinc alloy. By arranging the metal film layer on the first surface 11 of the substrate 10 having the grain groove 111, the metal film layer at least covers the inner wall surface of the grain groove 111.
[0062] The thickness of the metal film layer can be set to be between 3 nanometers and 600 nanometers. Specifically, the thickness of the metal film layer can be set to be between 10 nanometers and 300 nanometers. The thickness of the metal film layer can be set to be between 250 nanometers and 450 nanometers.
[0063] See also Figure 4 , Figure 4 It is a structural schematic diagram of another embodiment of the color development structure provided by the present invention.
[0064] In another embodiment, the average particle size of the color particles forming the color layer 20 does not exceed 35 microns. The color particles are obtained by crushing the photonic crystal structure layer 21 or the metal film layer formed on a smooth surface. In another embodiment, the color particles are obtained by growing seed particles; the size of the seed particles is smaller than the size of the color particles. When the color layer 20 formed by the color particles with an average particle size of no more than 35 microns presents a metallic reflective appearance on the substrate 10, the mirror effect presented by the color structure 100 is weakened.
[0065] In a preferred embodiment, the average particle size of the color-developing particles does not exceed 15 microns.
[0066] In a specific embodiment, the average particle size of the coloring particles is 10 microns. When the coloring layer 20 formed by the coloring particles with an average particle size of 10 microns presents a milky white appearance on the substrate 10, the mirror effect and metal reflection effect of the coloring structure 100 are weakened.
[0067] In other embodiments, the size of the color-developing particles may also be adjusted according to the color-developing effect actually required.
[0068] In this embodiment, by changing the microscopic size of the substrate 10 where the color-developing layer 20 is located or the physical size of the color-developing particles forming the color-developing layer 20, the color presented by the color-developing structure 100 is changed, and a color effect that cannot be achieved by the traditional structural color scheme is achieved. The color-developing structure provided in this embodiment includes a substrate and a color-developing layer, the substrate having a first surface and a second surface arranged opposite to each other; the color-developing layer covers the first surface of the substrate; wherein the roughness of the first surface is greater than the roughness of the second surface, or the average particle size of the color-developing particles forming the color-developing layer does not exceed 35 microns. In this application, by setting the color-developing layer on the surface of the substrate with a greater roughness, or by making the color-developing layer with color-developing particles having an average particle size of no more than 35 microns, the reflective performance of the color-developing layer is weakened, thereby weakening the mirror effect of the color-developing layer, and thereby improving the scattering performance of the color-developing layer.
[0069] See also Figure 5 , Figure 51 is a flow chart of an embodiment of a method for preparing a color-developing structure provided by the present invention. In this embodiment, a method for preparing a color-developing structure is provided, and the method for preparing a color-developing structure comprises the following steps.
[0070] S11: Obtain a substrate.
[0071] Specifically, the substrate has a first surface and a second surface opposite to each other. In this embodiment, the first surface and the second surface are both smooth planes.
[0072] In this embodiment, the substrate may also be a light-transmitting plate. The substrate may be glass or a resin such as polyethylene, acrylic acid, polycarbonate, and polyethylene terephthalate. The substrate may be other light-transmitting materials that can transmit visible light with a wavelength of 380-780 nm. Specifically, the substrate is a glass sheet or a quartz sheet. The refractive index nd of the substrate may be 1.5. In another embodiment, the substrate may also be a non-light-transmitting plate. The substrate may be a silicon sheet or a ceramic sheet; in addition, the substrate may also be paper or fabric, etc. The substrate may be formed into various forms including concave / convex surfaces and curved surfaces, such as film and plate.
[0073] S12: performing a roughening process on the first surface of the substrate.
[0074] Specifically, the first surface of the substrate may be roughened by mechanical processing or chemical etching to form a groove on the first surface of the substrate. The pattern of the groove may be a wave pattern, a horizontal pattern and / or a vertical pattern. The width of the groove may be set to be greater than 15 microns. The width of the groove may be set to be greater than 20 microns. The width of the groove may be set to be less than 15 microns. The width of the groove may be set to be less than 10 microns.
[0075] S13: forming a color development layer on the roughened first surface.
[0076] Specifically, a stack can be formed on the roughened first surface by spraying, printing, etc. Specifically, a first stack is formed on the roughened first surface based on a material of a first refractive index; and a second stack is formed on the side of the first stack away from the substrate based on a material of a second refractive index, and the material based on the first refractive index and the material of the second refractive index overlap in sequence to form a photonic crystal structure layer. In this embodiment, the stacking range of the photonic crystal structure layer is [11, 21]. Among them, the refractive index of the material of the first refractive index is greater than that of the material of the second refractive index. The material of the first refractive index includes at least one of titanium oxide, zinc oxide, zirconium oxide, niobium oxide, molybdenum oxide, iron oxide, tantalum oxide, hafnium oxide, cerium oxide, zinc sulfide, lanthanum titanate, etc., and the material of the second refractive index includes at least one of silicon dioxide, aluminum oxide, magnesium fluoride, calcium fluoride, lithium fluoride, cerium fluoride, organic resin, etc. The photonic crystal structure layer at least covers the inner wall surface of the grain groove. It is also possible to form a stack based on the material of the first refractive index and the material of the second refractive index on the roughened first surface by deposition, thereby forming a photonic crystal structure layer. Specifically, the deposition methods include physical vapor deposition, chemical vapor deposition, chemical water bath deposition, chemical solution method, electroplating and the like.
[0077] In another embodiment, a color developing layer can be formed on the roughened first surface based on a metal material. The color developing layer is a metal film layer. The metal material forming the metal film layer includes but is not limited to iron, copper, manganese, steel, tin alloy, aluminum alloy, magnesium alloy, copper alloy, aluminum alloy and zinc alloy. The metal film layer at least covers the inner wall surface of the grain groove.
[0078] In another embodiment, when the color development layer is a photonic crystal structure layer, a refractive index matching layer can be set on the side of the photonic crystal structure layer away from the substrate. The material of the refractive index matching layer includes but is not limited to organic materials such as resin, such as PMMA, PS, PDMS, epoxy resin, etc.
[0079] Specifically, the photonic crystal structure disposed on the first surface of the substrate is highly reflective in the visible light band and highly transparent in the near-infrared band. By disposing a refractive index matching layer on the surface of the photonic crystal structure on the side away from the substrate, the refractive index matching layer is transparent in the visible light band and the near-infrared band, thereby forming a special coating on the substrate that shields or stealths visible light and has high transmittance in the near-infrared band. Furthermore, by controlling the material forming the refractive index matching layer, the band range of high transmittance, stealth, and shielding of the refractive index matching layer can be controlled. The difference between the refractive index of the refractive index matching layer and the refractive index of the substrate does not exceed 0.2. In a preferred embodiment, the difference between the refractive index of the refractive index matching layer and the refractive index of the substrate does not exceed 0.1.
[0080] The method for preparing the color development structure provided in this embodiment comprises obtaining a substrate; the substrate having a first surface and a second surface; roughening the first surface of the substrate; and arranging a color development layer on the roughened first surface. The color development layer is arranged on a surface of the substrate with a greater roughness to reduce the reflective performance of the color development layer, thereby reducing the mirror effect of the color development layer, and thereby improving the scattering performance of the color development layer.
[0081] See also Figure 6 , Figure 6 1 is a flow chart of another embodiment of the method for preparing a color-developing structure provided by the present invention. In this embodiment, a method for preparing a color-developing structure is provided, and the method for preparing a color-developing structure comprises the following steps.
[0082] S21: Obtain a substrate.
[0083] Specifically, the substrate has a first surface and a second surface opposite to each other.
[0084] In this embodiment, both the first surface and the second surface are smooth planes.
[0085] In this embodiment, the substrate may also be a light-transmitting plate. The substrate may be glass or a resin such as polyethylene, acrylic acid, polycarbonate, and polyethylene terephthalate. The substrate may be other light-transmitting materials that can transmit visible light with a wavelength of 380-780 nm. Specifically, the substrate is a glass sheet or a quartz sheet. The refractive index nd of the substrate may be 1.5. In another embodiment, the substrate may also be a non-light-transmitting plate. The substrate may be a silicon sheet or a ceramic sheet; in addition, the substrate may also be paper or fabric, etc. The substrate may be formed into various forms including concave / convex surfaces and curved surfaces, such as film and plate.
[0086] S22: coating a coating layer containing color-developing particles on the surface of the substrate to form a color-developing layer; wherein the average particle size of the color-developing particles does not exceed 35 micrometers.
[0087] Specifically, a substrate is obtained and a prefabricated film is formed on the surface of the substrate. The prefabricated film includes a photonic crystal structure layer or a metal film layer. The prefabricated film is separated from the substrate, and the prefabricated film is crushed, ground or mechanically rolled to obtain color-developing particles. The material of the substrate can be the same as or different from that of the substrate, and is selected according to actual conditions. In order to facilitate the peeling of the prefabricated film, the surface of the prefabricated film is smooth. The color-developing layer is formed by applying a coating containing color-developing particles to the surface of the substrate.
[0088] In other embodiments, seed particles may also be obtained; the size of the seed particles is smaller than the size of the color-developing particles; and the color-developing particles are obtained by growing the seed particles.
[0089] The method for preparing the color development structure provided in this embodiment comprises obtaining a substrate; coating a coating containing color development particles on the surface of the substrate to form a color development layer; wherein the average particle size of the color development particles is no more than 35 microns. The color development layer is made of color development particles having an average particle size of no more than 35 microns to reduce the reflective performance of the color development layer, thereby reducing the mirror effect of the color development layer, thereby improving the scattering performance of the color development layer.
[0090] The above are only implementation modes of the present invention, and are not intended to limit the patent protection scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A color development structure, characterized in that: The color development structure comprises: A substrate having a first surface and a second surface disposed opposite to each other; A color development layer, covering the first surface of the substrate; Wherein, the roughness of the first surface is greater than the roughness of the second surface, or the average particle size of the color-developing particles forming the color-developing layer does not exceed 35 micrometers.
2. The color development structure according to claim 1, characterized in that: The color development layer includes a photonic crystal structure layer or a metal film layer, and the photonic crystal structure layer includes at least two alternately stacked layers of materials with different refractive indices.
3. The color development structure according to claim 1, characterized in that: When the roughness of the first surface is greater than that of the second surface, a grain groove is provided on the first surface, the color development layer at least covers the inner wall surface of the grain groove, and the width of the grain groove is less than 15 micrometers.
4. The color development structure according to claim 1, characterized in that: When the roughness of the first surface is greater than that of the second surface, a grain groove is provided on the first surface, the color development layer at least covers the inner wall surface of the grain groove, and the width of the grain groove is greater than 15 micrometers.
5. The color development structure according to claim 1, characterized in that: The color-developing particles are obtained by crushing a photonic crystal structure layer or a metal film layer, or by growing seed particles; the size of the seed particles is smaller than the size of the color-developing particles.
6. The color development structure according to claim 1 or 5, characterized in that: The average particle size of the color-developing particles is no more than 15 microns.
7. The color development structure according to claim 1 or 5, characterized in that: The average particle size of the color-developing particles is 10 microns.
8. The color development structure according to claim 2, characterized in that: The color development structure further includes a refractive index matching layer, and the refractive index matching layer is arranged on a surface of the photonic crystal structure layer on a side away from the substrate.
9. The color development structure according to claim 8, characterized in that: The difference between the refractive index of the index matching layer and the refractive index of the substrate does not exceed 0.
2.
10. The color development structure according to claim 1, characterized in that: The substrate is one of a silicon wafer, a glass wafer or a quartz wafer.
11. A method for preparing a color development structure, characterized in that: The manufacturing method comprises: Obtaining a substrate; the substrate having a first surface and a second surface; Performing a roughening process on the first surface of the substrate; A color development layer is formed on the roughened first surface.
12. A method for preparing a color development structure, characterized in that: The manufacturing method comprises: obtaining a substrate; A coating layer containing color-developing particles is coated on the surface of the substrate to form a color-developing layer; wherein the average particle size of the color-developing particles does not exceed 35 micrometers.
13. The method for preparing a color development structure according to claim 12, characterized in that: The method for obtaining the color-developing particles comprises: Obtaining a substrate; Forming a prefabricated film on the surface of the substrate; the prefabricated film includes a photonic crystal structure layer or a metal film layer; The prefabricated film is separated from the substrate, and the prefabricated film is crushed to obtain the color-developing particles.
14. The method for preparing a color development structure according to claim 12, characterized in that: The method for obtaining the color-developing particles comprises: Obtaining seed particles; the size of the seed particles is smaller than the size of the color-developing particles; The color-developing particles are obtained by growing the seed particles.