Method for replacing periodic maintenance with plasma-assisted process

The plasma-assisted process method forms a staggered stack of insulating and conductive films on the carrier plate, which solves the problem of increased thickness of the insulating film on the carrier plate, extends the maintenance cycle, improves equipment efficiency, and avoids high costs and pollution.

CN118841302APending Publication Date: 2024-10-25SKYTECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310443240.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-24
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

During the atomic layer deposition process, the increase in the thickness of the insulating film on the carrier plate will cause the loss of conductive properties, affecting the observation of process parameters and the uniformity of the film. In addition, existing cleaning methods are costly and can easily lead to contamination, affecting equipment efficiency.

Method used

The plasma-assisted process method is used to form a staggered stack of insulating films and conductive films on the carrier plate to determine and control the thickness of the insulating film, avoid opening the cavity for cleaning, and extend the maintenance cycle of the carrier plate.

Benefits of technology

It effectively extends the cleaning and maintenance cycle of the carrier plate, improves equipment usage efficiency, reduces cleaning costs and contamination risks, and maintains the observability of process parameters and the uniformity of the film.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118841302A_ABST
    Figure CN118841302A_ABST
Patent Text Reader

Abstract

The invention relates to a method for replacing periodic maintenance with a plasma-assisted process, which mainly comprises the following steps of: performing first atomic layer deposition on a substrate on a bearing disc to form a thin film on the substrate, and judging that the thickness of an insulating thin film deposited on the surface of the bearing disc is greater than a preset value; and performing second atomic layer deposition on the bearing disc without the substrate, and forming a conductive film on the insulating film of the bearing disc, so that the bearing disc has a conductive characteristic. The substrate may then be placed on a carrier, and first atomic layer deposition is performed on the substrate on the carrier. By means of the method, the period of cleaning and maintaining the bearing disc can be greatly prolonged, and the use efficiency of equipment can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for replacing periodic maintenance with a plasma-assisted process, which can significantly extend the cycle of cleaning and maintaining a carrier plate and is beneficial to improving the efficiency of equipment use. Background Art

[0002] With the continuous advancement of integrated circuit technology, electronic products are currently developing towards being thin, light, short, high-performance, highly reliable and intelligent. The miniaturization of transistors in electronic products is crucial. As the size of transistors decreases, the current transmission time and energy consumption can be reduced to achieve the purpose of fast computing and energy saving. In today's miniaturized transistors, some key thin films are only a few atoms thick, and the atomic layer deposition process is one of the main technologies for developing these micro structures.

[0003] The atomic layer deposition process is a technology that deposits materials layer by layer on the surface of a wafer in the form of single atoms. The main reactants of atomic layer deposition are two chemical substances, usually called precursors, and the two precursors are delivered to the reaction space in sequence.

[0004] In actual application, the first precursor is first delivered to the reaction space so that the first precursor is guided to the surface of the wafer. An inert gas is delivered to the reaction space, and the gas in the reaction space is extracted to remove the residual first precursor in the reaction space. The second precursor is injected into the reaction space so that the second precursor reacts with the first precursor on the surface of the wafer to form a thin film. Then, an inert gas is injected into the reaction space to remove the residual second precursor in the reaction space. The above steps are repeated to form a thin film on the wafer. Summary of the invention

[0005] The present invention proposes a novel method of replacing periodic maintenance with a plasma-assisted process, which mainly performs a first atomic layer deposition on a substrate on a carrier plate to form a thin film on the substrate and determines whether the thickness of an insulating film deposited on the surface of the carrier plate is greater than a preset value.

[0006] If the thickness of the insulating film deposited on the surface of the carrier disc is greater than a preset value, the substrate on the carrier disc is removed, and a second atomic layer deposition is performed on the surface of the carrier disc without the substrate, so as to form a conductive film on the insulating film of the carrier disc. Then, the substrate can be placed on the carrier disc, and the first atomic layer deposition is performed on the substrate on the carrier disc. The method of the present invention can greatly extend the cycle of cleaning and maintaining the carrier disc, and is conducive to improving the efficiency of equipment use.

[0007] In order to achieve the above-mentioned purpose, the present invention proposes a method of replacing periodic maintenance with a plasma-assisted process, including: performing a first atomic layer deposition on a substrate on a carrier plate to form a thin film on the substrate, wherein an insulating film is formed on the carrier plate when the first atomic layer deposition is performed; determining that the thickness of the insulating film of the carrier plate is greater than a preset value; and performing a second atomic layer deposition on the carrier plate to form a conductive film on the insulating film of the carrier plate.

[0008] In at least one embodiment of the present invention, the method includes: determining that the number of times the second atomic layer deposition is performed is greater than a threshold value; and cleaning the carrier plate to remove the insulating film and the conductive film on the carrier plate.

[0009] In at least one embodiment of the present invention, the carrier plate is located in a containing space of a chamber, comprising: sequentially transporting a first precursor and a second precursor to the containing space of the chamber, and performing the first atomic layer deposition on the substrate on the carrier plate.

[0010] In at least one embodiment of the present invention, the method includes: sequentially delivering a third precursor and the second precursor to the accommodating space of the chamber, and performing the second atomic layer deposition on the carrier in the accommodating space.

[0011] In at least one embodiment of the present invention, the thickness of the insulating film is greater than that of the conductive film.

[0012] In at least one embodiment of the present invention, the method includes: taking the substrate on which the first atomic layer deposition has been completed from the carrier plate, and then performing the second atomic layer deposition on the carrier plate.

[0013] In at least one embodiment of the present invention, the method includes: after completing the second atomic layer deposition, placing the substrate on the carrier plate and performing the first atomic layer deposition.

[0014] In at least one embodiment of the present invention, the preset value is 1000 angstroms.

[0015] In at least one embodiment of the present invention, the thickness of the conductive film is greater than 300 angstroms.

[0016] In at least one embodiment of the present invention, a precursor used in the first atomic layer deposition is different from a precursor used in the second atomic layer deposition.

[0017] The beneficial effect of the present invention is that a novel method of replacing periodic maintenance with a plasma-assisted process is proposed, which can significantly extend the cycle of cleaning and maintaining the carrier plate and is beneficial to improving the efficiency of equipment use. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1A flowchart of an embodiment of the method of replacing periodic maintenance with a plasma-assisted process according to the present invention

[0019] Figure 2 The cross-sectional view of an embodiment of a deposition apparatus suitable for the method of replacing periodic maintenance with a plasma-assisted process described in the present invention is shown.

[0020] Figure 3 A cross-sectional view of an embodiment of a carrier plate formed by a plasma-assisted process instead of a periodic maintenance method according to the present invention.

[0021] Explanation of the reference numerals: 20 - deposition equipment; 21 - chamber; 22 - accommodating space; 23 - spray head; 231 - hole; 24 - substrate; 25 - carrier plate; 261 - insulating film; 2611 - first insulating film; 2613 - second insulating film; 263 - conductive film; 2631 - first conductive film; 2633 - second conductive film; 27 - transmission pipeline; 271 - radio frequency coil. DETAILED DESCRIPTION

[0022] Figure 1 FIG. 1 is a flow chart of the steps of an embodiment of a method for replacing periodic maintenance with a plasma-assisted process according to the present invention. Figure 2 The cross-sectional view of an embodiment of a deposition device applicable to the method of replacing periodic maintenance with a plasma-assisted process described in the present invention is shown. The deposition device 20 includes a chamber 21, a spray head 23 and a carrier plate 25, wherein the spray head 23 is connected to the chamber 21 and faces a receiving space 22 of the chamber 21, and the carrier plate 25 is located in the receiving space 22 of the chamber 21.

[0023] The spray head 23 is connected to a delivery pipeline 27, wherein the delivery pipeline 27 is used to deliver one or more precursors to the spray head 23. The spray head 23 includes a plurality of holes 231, and the precursors are delivered to the accommodating space 22 of the chamber 21 through the holes 231 of the spray head 23.

[0024] In one embodiment of the present invention, the delivery line 27 may include a radio frequency coil 271, for example, the radio frequency coil 271 may be wound around the outside of the delivery line 27. The precursor in the delivery line 27 is subjected to the magnetic field generated by the radio frequency coil 271 to form plasma, so that the deposition apparatus 20 becomes a plasma-assisted atomic layer deposition apparatus. In addition, the radio frequency coil 271 may be disposed around the chamber 21. In different embodiments, the deposition apparatus 20 may not include the radio frequency coil 271, and a remote plasma source may be connected to the delivery line 27.

[0025] The carrier plate 25 is used to carry one or more substrates 24 and to heat the substrates 24 placed on the carrier plate 25 . The spray head 23 is located above the carrier plate 25 , wherein the holes 231 of the spray head 23 face the upper surfaces of the carrier plate 25 and the substrates 24 .

[0026] During the deposition process, the precursor is transported to the spray head 23 via the delivery pipeline 27 and transported to the carrier plate 25 and the substrate 24 disposed on the surface of the carrier plate 25 through the holes 231 on the spray head 23, so that the precursor contacts the carrier plate 25 and the substrate 24 to form a thin film on the surface of the substrate 24.

[0027] In practical applications, the first precursor can be transported to the containing space 22 of the chamber 21 through the holes 231 on the spray head 23, wherein the first precursor is deposited on the substrate 24. Then, an inert gas is injected into the containing space 22 of the chamber 21 through the holes 231 of the spray head 23 to remove the unreacted first precursor and byproducts in the containing space 22.

[0028] The second precursor is then transported to the containing space 22 of the chamber 21 through the holes 231 on the spray head 23, where the second precursor reacts with the first precursor on the surface of the substrate 24 to form a thin film. Then, an inert gas is injected into the containing space 22 of the chamber 21 through the holes 231 of the spray head 23 again to remove the unreacted second precursor and byproducts in the containing space 22.

[0029] By repeatedly performing the above-mentioned cycle, a thin film can be formed on the surface of the substrate 24, and the thickness of the thin film can be controlled by the number of cycles.

[0030] Generally speaking, the first precursor may be a volatile metal compound, and the second precursor may be a non-metal compound such as H2O, NH3 or O3. For example, the first precursor may be trimethylaluminum (TMA), and the second precursor may be NH3, and an aluminum nitride (AlN) film may be formed on the surface of the substrate 24.

[0031] like Figure 3 As shown, during the process of depositing a thin film on the surface of the substrate 24, a thin film will also be formed on the surface of the carrier plate 25. For example, the carrier plate 25 can be a titanium plate and has conductive properties. After the first atomic layer deposition is performed on multiple batches of substrates 24, the thickness of the film deposited on the carrier plate 25 will increase, and an insulating film 261, such as an aluminum nitride film, will be formed on the surface of the carrier plate 25, so that the carrier plate 25 gradually loses its conductive properties.

[0032] As a result, some important process parameters such as DC bias cannot be observed during PEALD. In addition, the insulating film 261 on the carrier 25 will also reduce the uniformity (U%) of the film deposited on the surface of the substrate 24.

[0033] Generally speaking, when the thickness of the insulating film 261 on the surface of the carrier plate 25 is too thick, the cavity 21 needs to be opened and the carrier plate 25 in the cavity 21 needs to be taken out for cleaning to remove the insulating film 261 deposited on the surface of the carrier plate 25. After the cleaning of the carrier plate 25 is completed, the carrier plate 25 can be put back into the accommodating space 22 of the cavity 21, and the thin film deposition can continue through the deposition device 20.

[0034] Through the above-mentioned step of cleaning the carrier plate 25, the insulating film 261 deposited on the surface of the carrier plate 25 can be effectively removed to avoid the inability to observe some process parameters and the reduction of the uniformity of the film on the surface of the substrate 24. However, removing the carrier plate 25 from the chamber 21 and cleaning it will undoubtedly increase the cost and delay the subsequent process. In addition, in the process of opening the chamber 21, external contaminants may also enter the accommodating space 22 of the chamber 21, thereby affecting the subsequent process.

[0035] Therefore, the present invention proposes a method of replacing periodic maintenance with a plasma-assisted process, which can effectively extend the maintenance period of the carrier plate 25. Figure 1 As shown, at least one substrate 24 is placed on a carrier plate 25, a first atomic layer deposition is performed on the substrate 24 on the carrier plate 25, and a thin film is formed on the surface of the substrate 24, as shown in step 11. The first atomic layer deposition is generally a deposition step performed on the surface of the substrate 24, for example, the thin film formed on the surface of the substrate 24 can be aluminum nitride.

[0036] During the first atomic layer deposition process on the substrate 24 , the precursor will also contact the surface of the carrier plate 25 and form an insulating film 261 on the carrier plate 25 .

[0037] It is determined whether the thickness of the insulating film 261 deposited on the carrier plate 25 is greater than a preset value, as shown in step 13. In actual application, the thickness of the insulating film 261 can be calculated by the magnitude of the induced voltage between the RF coil 271 and the carrier plate 25, and it is determined whether the thickness of the insulating film 261 is greater than the preset value. The setting of the preset value can be adjusted based on the experience of actually operating the deposition device 20 or the accumulated data, for example, the preset value can be 1000 angstroms.

[0038] In different embodiments, whether the thickness of the insulating film 261 deposited on the carrier plate 25 is greater than a preset value may also be determined according to the number of cycles of performing the first atomic layer deposition.

[0039] When the thickness of the insulating film 261 on the surface of the carrier plate 25 is greater than a preset value, a second atomic layer deposition may be performed on the carrier plate 25 to form a conductive film 263 on the surface of the insulating film 261 of the carrier plate 25 , as shown in step 15 .

[0040] The insulating film 261 formed by the first atomic layer deposition and the conductive film 263 formed by the second atomic layer deposition are made of different materials, and the precursor used in the first atomic layer deposition is also different from the precursor used in the second atomic layer deposition.

[0041] During the first atomic layer deposition, the first precursor and the second precursor may be sequentially delivered to the containing space 22 of the chamber 21 through the showerhead 23. During the second atomic layer deposition, the third precursor and the second precursor may be sequentially delivered to the containing space 22 of the chamber 21 through the showerhead 23.

[0042] In one embodiment of the present invention, the insulating film 261 may be aluminum nitride, and the conductive film 263 may be titanium nitride. In addition, the first precursor used in the first atomic layer deposition may be trimethylaluminum, and the second precursor may be ammonia, and the third precursor used in the second atomic layer deposition may be tetrakis(dimethylamino)titanium (TDMAT) or tetrakis(diethylamino)titanium (TDEAT), and the second precursor may be ammonia.

[0043] In practical applications, after the first atomic layer deposition is completed on the substrate 24 on the carrier plate 25, the substrate 24 on which the first atomic layer deposition is completed is removed from the carrier plate 25. Then, different precursors are transported to the accommodating space 22 of the chamber 21 through the hole 231 of the spray head 23, and the second atomic layer deposition is performed on the carrier plate 25 to form a conductive film 263 on the surface of the insulating film 261 of the carrier plate 25.

[0044] After the second atomic layer deposition is completed, the conductive film 263 deposited on the carrier plate 25 reaches a certain thickness, for example, the thickness of the conductive film 263 can be greater than 300 angstroms, which will make the carrier plate 25 conductive. Then, the substrate 24 can be placed on the carrier plate 25, and the first atomic layer deposition is continued on the substrate 24.

[0045] When performing the above method, there is no need to open the cavity 21 or remove the carrier plate 25 from the cavity 21 , which can greatly reduce the time and cost of cleaning the carrier plate 25 and avoid possible contamination during the process of opening the cavity 21 .

[0046] In one embodiment of the present invention, Figure 3As shown, the thickness of the insulating film 261 formed on the carrier plate 25 may be greater than the thickness of the conductive film 263. For example, the insulating film 261 may be aluminum nitride with a thickness of 1000 angstroms, while the conductive film 263 may be titanium nitride with a thickness of 300 angstroms.

[0047] By using the method described in the present invention, steps 11 to 15 can be repeated, and an insulating film 261 and a conductive film 263 that are stacked in an alternating manner can be formed on the surface of the carrier plate 25. For example, a first insulating film 2611 is formed on the surface of the carrier plate 25, and a first conductive film 2631 is formed on the surface of the first insulating film 2611, a second insulating film 2613 is formed on the surface of the first conductive film 2631, and then a second conductive film 2633 is formed on the surface of the second insulating film 2613.

[0048] In addition, when the number of times steps 11 to 15 are repeated or the number of times the second atomic layer deposition is performed is greater than a threshold value, for example, between ten and twenty times, it may be necessary to open the chamber 21, remove the carrier plate 25 from the chamber 21 for cleaning, and remove the insulating film 261 and the conductive film 263 on the surface of the carrier plate 25.

[0049] Advantages of the present invention:

[0050] A novel method of replacing periodic maintenance with a plasma-assisted process is proposed, which can significantly extend the cleaning and maintenance cycle of the carrier plate and is beneficial to improving the efficiency of equipment use.

[0051] The above is only a preferred embodiment of the present invention and is not intended to limit the scope of the present invention. That is, all equivalent changes and modifications to the shape, structure, characteristics and spirit described in the patent application scope of the present invention should be included in the patent application scope of the present invention.

Claims

1. A method of replacing periodic maintenance with a plasma-assisted process, characterized in that: include: Performing a first atomic layer deposition on a substrate on a carrier to form a thin film on the substrate, wherein an insulating thin film is formed on the carrier during the first atomic layer deposition; Determining that the thickness of the insulating film of the carrier plate is greater than a preset value; and A second atomic layer deposition is performed on the carrier disk, and a conductive film is formed on the insulating film of the carrier disk.

2. The method of claim 1, wherein: include: determining that the number of times the second atomic layer deposition is performed is greater than a threshold value; and The carrier plate is cleaned to remove the insulating film and the conductive film on the carrier plate.

3. The method of claim 1, wherein: The carrier plate is located in a containing space of a cavity, and includes: sequentially transporting a first precursor and a second precursor to the containing space of the cavity, and performing the first atomic layer deposition on the substrate on the carrier plate.

4. The method of claim 3, wherein: include: A third precursor and the second precursor are sequentially transported to the accommodating space of the chamber, and the second atomic layer deposition is performed on the carrier in the accommodating space.

5. The method of claim 1, wherein: The thickness of the insulating film is greater than that of the conductive film.

6. The method of claim 1, wherein: include: The substrate on which the first atomic layer deposition is completed is taken out from the carrier plate, and then the second atomic layer deposition is performed on the carrier plate.

7. The method of claim 6, wherein: include: After the second atomic layer deposition is completed, the substrate is placed on the carrier plate and the first atomic layer deposition is performed.

8. The method of claim 1, wherein: The preset value is 1000 angstroms.

9. The method of claim 1, wherein: The thickness of the conductive film is greater than 300 angstroms.

10. The method of claim 1, wherein: A precursor used in the first atomic layer deposition is different from a precursor used in the second atomic layer deposition.