Arsenic molybdate-based rare earth derivative and preparation method thereof, modified compound of arsenic molybdate-based rare earth derivative and preparation method thereof, modified electrode and application thereof

Through in-situ self-assembly and composite technology, the problem of difficulty in the synthesis of heteropolymolybdate-based rare earth derivatives has been solved, and the synthesis of arsenic molybdate-based rare earth derivatives and their composite with carboxylated multi-walled carbon nanotubes have been achieved. Used to modify electrodes to achieve highly sensitive electrochemical detection of nitrite.

CN118852017APending Publication Date: 2024-10-29CHANGCHUN UNIV OF CHINESE MEDICINE
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410873587.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-01
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

The difficulty in synthesizing heteropolymolybdates among existing polyacid-based rare earth derivatives is mainly due to its instability in solution and the rapid combination of rare earth ions and vacuous heteropolymolybdates, resulting in heteropolymolybdate-based rare earths. Derivatives have limited applications.

Method used

A mixed solution of NaAsO2 and (NH4)6Mo7O24 is used for in-situ self-assembly with praseodymium chloride and imidazole. The pH value is adjusted to form arsenic molybdate-based rare earth derivatives, which are then combined with carboxylated multi-walled carbon nanotubes to modify the electrode for sub-surface use. Electrochemical detection of nitrate.

Benefits of technology

The successful synthesis of arsenic molybdate-based rare earth derivatives shows excellent electrocatalytic activity, enables sensitive electrochemical detection of nitrite, and expands the application scope of polyacid-based rare earth derivatives.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118852017A_ABST
    Figure CN118852017A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of electrochemical analysis, and particularly relates to an arsenic molybdate-based rare earth derivative and a preparation method thereof, a modified compound of the arsenic molybdate-based rare earth derivative and a preparation method thereof, and a modified electrode and application thereof. Sodium arsenite, ammonium molybdate, praseodymium chloride and imidazole are used as starting raw materials, and the novel arsenic molybdate rare earth derivative with the chemical formula as shown in the formula 1 is synthesized by adopting an in-situ self-assembly method. The arsenic molybdate-based rare earth derivative has excellent electrocatalytic activity on nitrite; the arsenic molybdate-based rare earth derivative / COOH-MCNTs composite material prepared by compounding the COOH-MCNTs and carboxylated multi-walled carbon nanotubes realizes sensitive electrochemical detection of nitrite under the synergistic signal amplification effect of the two. In the formula 1, H4 (NH4) 2 (C3N2H5) 16 [Na (C3N2H4)] 2 [Pr0. 5Na0. 5 (H2O) 3] 2 [AsMo10O35] 4. 32H2O.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of electrochemical analysis, and specifically relates to an arsenomolybdate-based rare earth derivative and a preparation method thereof, a modified composite of an arsenomolybdate-based rare earth derivative and a preparation method thereof, a modified electrode and applications thereof. Background Art

[0002] Polyoxometalates (abbreviated as polyoxometalates) are a class of nanoscale metal oxygen clusters with adjustable size and charge. Due to their diverse structures, high electronegativity and multiple active coordination sites, they can be assembled with rare earth ions in various modes to construct polyoxometalates-based rare earth derivatives with rich structures. Because rare earth ions have unique 4f electronic configurations, they exhibit excellent magnetic, optical, and electrical properties. Therefore, polyoxometalates-based rare earth derivatives have the advantages of both polyoxometalates and rare earths, and show potential application prospects in the fields of magnetism, optics, and electrochemistry. The existing polyoxometalates-based rare earth derivatives are mainly heteropolytungstate-based rare earth derivatives, while the synthesis of heteropolymolybdate-based rare earth derivatives is rarely studied. This is mainly because the stability of vacant heteropolymolybdates in solution is poor and they are easily decomposed or converted into stable saturated structures. At the same time, rare earth ions not only undergo hydrolysis, but also easily combine with vacant heteropolymolybdates to quickly form amorphous precipitates; this brings great difficulties to the synthesis of heteropolymolybdate-based rare earth derivatives. The synthesis of arsenomolybdate-based rare earth derivatives will increase the types of polyoxometalates-based rare earth derivatives and thus expand their application range. Summary of the invention

[0003] In view of this, the present invention provides an arsenomolybdate-based rare earth derivative and a preparation method thereof, a modified composite of an arsenomolybdate-based rare earth derivative and a preparation method thereof, a modified electrode and an application thereof. The present invention provides a novel arsenomolybdate-based rare earth derivative, which shows excellent electrocatalytic activity to nitrite after modification, and the electrode modified with the arsenomolybdate-based rare earth derivative can realize sensitive electrochemical detection of nitrite.

[0004] In order to solve the above technical problems, the present invention provides an arsenomolybdate-based rare earth derivative having a chemical formula shown in Formula 1:

[0005] H4(NH4)2(C3N2H5) 16 [Na(C3N2H4)]2[Pr 0.5 Na 0.5 (H2O)3]2[AsMo 10 O 35 ]4·32H2O Formula 1;

[0006] The arsenomolybdate-based rare earth derivatives are composed of 4 [AsMo 10 O 35 ] 7- Anion, 4 [H+ ], 16 [C3N2H5] + cation, 2 [Pr 0.5 Na 0.5 (H2O)3] 2+ unit and 2 [Na(C3N2H4)2] + The unit is composed of 32 crystal water molecules;

[0007] The [AsMo 10 O 35 ] 7- The Mo-O bond length in the anion is The [AsMo 10 O 35 ] 7- The As-O bond length in the anion is

[0008] 4 [AsMo 10 O 35 ] 7- The anion is formed by the interaction with two [Pr 0.5 Na 0.5 (H2O)3] 2+ unit and 2 [Na(C3N2H4)2] + The units are connected by coordination to form a ring structure;

[0009] [C3N2H5] + Cations and crystal water molecules fill the spaces between adjacent ring structures;

[0010] [Na(C3N2H4)2] + Na in unit + With two N atoms from two C3N2H4 ligands and two [AsMo 10 O 35 ] 7- The two O atoms of the anion are coordinated.

[0011] Preferably, the space group of the arsenomolybdate-based rare earth derivative is Pnnm, and a is b is c is α is 90°, β is 90°, γ is 90°, Z is 2; the unit cell volume is

[0012] The present invention also provides a method for preparing the arsenomolybdate-based rare earth derivatives described in the above technical solution, comprising the following steps:

[0013] NaAsO2 and (NH4)6Mo7O 24The mixed solution and the first pH value adjusting agent are first mixed to obtain an arsenic molybdenum oxy-cluster solution; the pH value of the system after the first mixing is 1.0 to 1.5;

[0014] The arsenic molybdenum oxy-cluster solution is mixed with praseodymium chloride, imidazole and a second pH value regulator for a second time and then self-assembled in situ to obtain the arsenic molybdate-based rare earth derivative; the pH value of the system after the second mixing is 4.0-4.5.

[0015] Preferably, the second mixed system contains NaAsO2, (NH4)6Mo7O 24 , praseodymium chloride and imidazole in a molar ratio of 0.269:0.404:0.281:1.469;

[0016] The first pH value adjusting agent is a hydrochloric acid solution; the second pH value adjusting agent is an ammonia solution;

[0017] The temperature of the in-situ self-assembly is 60° C. to 80° C., and the time is 30 to 40 minutes.

[0018] Preferably, the molar concentration of the hydrochloric acid solution is 3 to 5 mol / L, and the molar concentration of the ammonia solution is 0.5 to 1.5 mol / L.

[0019] The present invention also provides a modified composite of an arsenomolybdate-based rare earth derivative, comprising an arsenomolybdate-based rare earth derivative and a carboxylated multi-walled carbon nanotube, wherein the carboxylated multi-walled carbon nanotube is combined with the arsenomolybdate-based rare earth derivative by intermolecular forces;

[0020] The arsenomolybdate-based rare earth derivative is the arsenomolybdate-based rare earth derivative described in the above technical solution or the arsenomolybdate-based rare earth derivative prepared by the preparation method described in the above technical solution.

[0021] Preferably, the carboxylated multi-walled carbon nanotubes have an inner diameter of 5 to 8 nm, an outer diameter of 10 to 15 nm, a length of 2 to 8 μm, a carboxyl content of 1.0 to 2.0 mmol / g, and a specific surface area of ​​≥190 m 2 / g;

[0022] The mass ratio of the arsenomolybdate-based rare earth derivative to the carboxylated multi-walled carbon nanotube is 1:0.8-1.2.

[0023] The present invention also provides a method for preparing the modified composite of the arsenomolybdate-based rare earth derivative described in the above technical solution, comprising the following steps:

[0024] The arsenomolybdate-based rare earth derivative and the carboxylated multi-walled carbon nanotube are ground and mixed to obtain the modified composite of the arsenomolybdate-based rare earth derivative.

[0025] The present invention also provides a modified electrode, comprising a substrate and a coating coated on the surface of the substrate, wherein the coating is formed by film-forming a dispersion of a modified composite of an arsenomolybdate-based rare earth derivative;

[0026] The method for preparing the dispersion of the modified composite of the arsenomolybdate-based rare earth derivative comprises the following steps: mixing the modified composite of the arsenomolybdate-based rare earth derivative, ethanol, a perfluorosulfonic acid type polymer solution and water to obtain the dispersion of the modified composite of the arsenomolybdate-based rare earth derivative;

[0027] The modified compound of arsenomolybdate-based rare earth derivative is the modified compound of arsenomolybdate-based rare earth derivative described in the above technical solution or the modified compound of arsenomolybdate-based rare earth derivative prepared by the preparation method described in the above technical solution.

[0028] The present invention also provides the application of the modified electrode described in the above technical solution in electrochemical detection.

[0029] The present invention provides an arsenomolybdate-based rare earth derivative having a chemical formula shown in Formula 1: H4(NH4)2(C3N2H5) 16 [Na(C3N2H4)]2[Pr 0.5 Na 0.5 (H2O)3]2[AsMo 10 O 35 ]4·32H2O Formula 1; the arsenomolybdate-based rare earth derivative is composed of 4 [AsMo 10 O 35 ] 7- Anion, 4 [H + ], 16 [C3N2H5] + cation, 2 [Pr 0.5 Na 0.5 (H2O)3] 2+ unit and 2 [Na(C3N2H4)2] + unit and 32 crystal water molecules; the [AsMo 10 O 35 ] 7- The Mo-O bond length in the anion is The [AsMo 10 O 35 ] 7- The As-O bond length in the anion is 4 [AsMo 10 O 35 ] 7- The anion is formed by the interaction with two [Pr 0.5 Na 0.5 (H2O)3] 2+unit and 2 [Na(C3N2H4)2] + The units are connected by coordination to form a ring structure; the [C3N2H5] + Cations and crystal water molecules fill the space between adjacent ring structures; the [Na(C3N2H4)2] + Na in unit + With two N atoms from two C3N2H4 ligands and two [AsMo 10 O 35 ] 7- The two O atoms of the anion are coordinated. The present invention uses sodium arsenite, ammonium molybdate, praseodymium chloride and imidazole as starting materials, and adopts an in-situ self-assembly method to successfully synthesize a new type of arsenomolybdate-based rare earth derivative. The synthesized arsenomolybdate-based rare earth derivative has excellent electrocatalytic activity for nitrite; the arsenomolybdate-based rare earth derivative / COOH-MCNTs composite material prepared by compounding it with carboxylated multi-walled carbon nanotubes (COOH-MCNTs) can achieve sensitive electrochemical detection of nitrite under the synergistic signal amplification effect of the arsenomolybdate-based rare earth derivative and the carboxylated multi-walled carbon nanotubes. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 To {B-β-AsMo9O 33} structure of two {Mo3O 13 {AsMo} is derived by inserting a {MoO6} octahedron into the cavity between the units. 10 O 35}Schematic diagram of the cluster;

[0031] Figure 2 For 4 [AsMo 10 O 35 ] 7- The anion is formed by the interaction with two [Pr 0.5 Na 0.5 (H2O)3] 2+ unit and 2 [Na(C3N2H4)2] + Schematic diagram of the ring structure formed by the coordination connection of the units, where (a) is a schematic diagram of the mixed polyhedral structure of the ring structure, and (b) is a ball-and-stick model of the ring structure, where brown is As, purple is Mo, pink is Pr, green is Na, gray is C, blue is N, and white is O;

[0032] Figure 3 For [Pr 0.5 Na 0.5 (H2O)3] 2+ Polyhedral model of unit coordination geometry, where pink is Pr 0.5 Na 0.5 , white is O;

[0033] Figure 4 [Na(C3N2H4)2] + Ball-and-stick model of the unit, with green for Na, grey for C, blue for N, and white for O;

[0034] Figure 5 is protonated imidazole [C3N2H5] + Cation and [AsMo 10 O 35 ] 7- Schematic diagram of the structure where the surface oxygen atoms of the anion form multi-point hydrogen bonds to form a three-dimensional framework;

[0035] Figure 6 The XRD spectrum of the arsenomolybdate-based rare earth derivative prepared in Example 1;

[0036] Figure 7 The infrared spectra of the arsenomolybdate-based rare earth derivatives prepared in Example 1 and Comparative Example 1;

[0037] Figure 8 This is a thermogravimetric curve of the arsenomolybdate-based rare earth derivative prepared in Example 1;

[0038] Fig. 9 This is the UV-visible absorption spectrum of the arsenomolybdate-based rare earth derivative prepared in Example 1;

[0039] Fig.10 The SEM image and SEM-mapping spectrum of the arsenomolybdate-based rare earth derivative prepared in Example 1;

[0040] Fig.11 This is an energy dispersion spectrum of the arsenomolybdate-based rare earth derivative prepared in Example 1;

[0041] Fig.12 The cyclic voltammetry curve of arsenomolybdate-based rare earth derivative / COOH-MCNTs / GCE prepared in Example 1;

[0042] Fig.13 Comparison of cyclic voltammetry curves of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE prepared in Example 1 at different scan rates;

[0043] Fig.14 Comparison of cyclic voltammetry curves of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE prepared in Example 1 at different times;

[0044] Fig.15This is a comparison diagram of cyclic voltammetry curves of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE prepared in Example 1 under different concentrations of nitrite;

[0045] Fig.16 The current-time response curve of the arsenomolybdate-based rare earth derivative / COOH-MCNTs / GCE prepared in Example 1 to different concentrations of nitrite;

[0046] Fig.17 This is a linear relationship diagram between the current response signal of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE and nitrite concentration. DETAILED DESCRIPTION

[0047] The present invention provides an arsenomolybdate-based rare earth derivative having a chemical formula shown in Formula 1:

[0048] H4(NH4)2(C3N2H5) 16 [Na(C3N2H4)]2[Pr 0.5 Na 0.5 (H2O)3]2[AsMo 10 O 35 ]4·32H2O Formula 1.

[0049] In the present invention, the arsenomolybdate-based rare earth derivative is composed of 4 [AsMo 10 O 35 ] 7- Anion, 4 [H + ], 16 [C3N2H5] + cation, 2 [Pr 0.5 Na 0.5 (H2O)3] 2+ unit and 2 [Na(C3N2H4)2] + The unit is composed of 32 crystal water molecules.

[0050] In the present invention, {AsMo 10 O 35 The cluster prefers to pass to the triple-vacancy {B-β-AsMo9O 33 Two trimetallic clusters {Mo3O 13} is derived by inserting a {MoO6} octahedron into the hole between them; Figure 1 is a schematic diagram of the derivation, wherein the brown is As and the purple octahedron is {MoO6}. 10 O 35 ] 7- Mo in anion VI The atom is in a six-coordinate mode. In the present invention, the [AsMo10 O 35 ] 7- The Mo-O bond length in the anion is In the present invention, the [AsMo 10 O 35 ] 7- The As atoms in the anion are located in the {AsO3} pyramidal geometry. 10 O 35 ] 7- The As-O bond length in the anion is

[0051] In the present invention, 4 [AsMo 10 O 35 ] 7- The anion is formed by the interaction with two [Pr 0.5 Na 0.5 (H2O)3] 2+ unit and 2 [Na(C3N2H4)2] + The units are connected by coordination to form a ring structure; the schematic diagram of the ring structure is as follows Figure 2 As shown, (a) is a schematic diagram of the mixed polyhedron structure of the ring structure, and (b) is a ball-and-stick model of the ring structure, where brown is As, purple is Mo, pink is Pr, green is Na, gray is C, blue is N, and white is O. Figure 3 For [Pr 0.5 Na 0.5 (H2O)3] 2+ Polyhedral model of unit coordination geometry, where pink is Pr 0.5 Na 0.5 , white is O; Figure 4 [Na(C3N2H4)2] + A ball-and-stick model of a cell, with Na in green, C in grey, N in blue, and O in white.

[0052] In the present invention, the [Pr 0.5 Na 0.5 (H2O)3] 2+ The Pr and Na atoms (0.5 each) in the unit both present a five-coordinate environment, with five oxygen atoms coming from three water molecules and two [AsMo 10 O 35 ] 7- Anion.

[0053] In the present invention, C3N2H4 is used as a monodentate ligand to bind to Na + Ion coordination forms a mononuclear [Na(C3N2H4)2] + Unit. [Na(C3N2H4)2] +The unit has a small volume and steric hindrance, which is conducive to the reaction with [AsMo 10 O 35 ] 7- In the present invention, the [Na(C3N2H4)2] + Na in unit + Adopting a four-coordinate tetrahedral configuration, the [Na(C3N2H4)2] + Na in unit + With two N atoms from two C3N2H4 ligands and two [AsMo 10 O 35 ] 7- The two O atoms of the anion are coordinated. In the present invention, the [Na(C3N2H4)2] + Na in unit + The Na-N bond length formed by the coordination of two N atoms from two C3N2H4 ligands is preferably [Na(C3N2H4)2] + Na in unit + With the two [AsMo 10 O 35 ] 7- The Na-O bond length formed by the coordination of the two O atoms of the anion is preferably

[0054] In the present invention, the [C3N2H5] + The cations and crystal water molecules fill the spaces between adjacent ring structures. In the present invention, the protonated imidazole [C3N2H5] + Cation and [AsMo 10 O 35 ] 7- The surface oxygen atoms of the anions form multi-point hydrogen bonds to form a three-dimensional framework, as shown in the schematic diagram. Figure 5 In the present invention, the hydrogen bond preferably includes OH···O POM and NH···O POM In the present invention, the OH···O POM The bond length is preferably The NH···O POM The bond length is preferably

[0055] In the present invention, the space group of the arsenomolybdate-based rare earth derivative is preferably Pnnm, and a is preferably b is preferably c is preferably α is preferably 90°, β is preferably 90°, γ is preferably 90°, Z is preferably 2; the unit cell volume is preferably

[0056] In the present invention, the arsenomolybdate-based rare earth derivative is preferably a light green crystal. In the present invention, the crystal system of the arsenomolybdate-based rare earth derivative is an orthorhombic system.

[0057] The present invention also provides a method for preparing the arsenomolybdate-based rare earth derivatives described in the above technical solution, comprising the following steps:

[0058] NaAsO2 and (NH4)6Mo7O 24 The mixed solution and the first pH value adjusting agent are first mixed to obtain an arsenic molybdenum oxy-cluster solution; the pH value of the system after the first mixing is 1.0 to 1.5;

[0059] The arsenic molybdenum oxy-cluster solution is mixed with praseodymium chloride, imidazole and a second pH value regulator for a second time and then self-assembled in situ to obtain the arsenic molybdate-based rare earth derivative; the pH value of the system after the second mixing is 4.0-4.5.

[0060] The present invention combines NaAsO2 and (NH4)6Mo7O 24 The mixed solution and the first pH value adjusting agent are first mixed to obtain an arsenic molybdenum oxycarbon cluster solution. In the present invention, the NaAsO2 and (NH4)6Mo7O 24 The mixed solution preferably contains NaAsO2 and (NH4)6Mo7O 24 Dissolve in water to obtain (NH4)6Mo7O 24 Preferably (NH4)6Mo7O 24 ·4H2O. The present invention has no special requirements for the dissolution, as long as it can be completely dissolved. The present invention uses (NH4)6Mo7O 24 Arsenomolybdate-based rare earth derivative crystals were prepared as the initial raw material. If Na2MoO4·2H2O was used to replace (NH4)6Mo7O 24 The product prepared by using 4H2O as raw material is a light green powder, not a crystal. III O3 3- The anion has a trigonal pyramidal configuration, As III The steric effect of the lone pair of electrons on the atom can effectively avoid the formation of saturated arsenic, molybdenum, and oxygen clusters and easily produce vacant arsenic, molybdenum, and oxygen cluster fragments, thus providing an effective synthetic strategy for capturing rare earth ions to construct arsenic, molybdenum, and oxygen clusters.

[0061] In the present invention, the first pH regulator is preferably a hydrochloric acid solution, and the molar concentration of the hydrochloric acid solution is preferably 3-5 mol / L, more preferably 4 mol / L. In the present invention, the pH value of the first mixed system is 1.0-1.5, preferably 1.0. The present invention has no special limitation on the amount of the first pH regulator, as long as the pH value of the first mixed system can meet the requirements. The purpose of adjusting the pH value by the first pH regulator in the present invention is to first generate arsenic molybdenum oxygen clusters with a saturated structure.

[0062] The present invention has no special requirements for the first mixing, as long as the mixing can be uniform.

[0063] After obtaining the arsenic molybdenum oxy-cluster solution, the present invention performs in-situ self-assembly after the arsenic molybdenum oxy-cluster solution is mixed with praseodymium chloride, imidazole, and a second pH regulator to obtain the arsenic molybdenum salt-based rare earth derivative. In the present invention, the second pH regulator is preferably an ammonia solution, and the molar concentration of the ammonia solution is preferably 0.5-1.5 mol / L, and more preferably 1 mol / L. In the present invention, the pH value of the second mixed system is 4.0-4.5, preferably 4.0. The present invention has no special limitation on the amount of the second pH regulator, as long as the pH value of the second mixed system can meet the requirements. The present invention limits the pH value of the second mixed system to be within the above range, which is conducive to the formation of arsenic molybdenum salt-based rare earth derivative crystals, and the yield is the highest when the pH value is 4.0; if the pH value is less than 3.5 or greater than 4.5, crystals cannot be obtained.

[0064] The present invention has no special requirements for the second mixing, as long as the mixing can be uniform.

[0065] In the present invention, the second mixed system contains NaAsO2, (NH4)6Mo7O 24 The molar ratio of praseodymium chloride to imidazole is preferably 0.269:0.404:0.281:1.469. The present invention uses imidazole as an organic ligand to prepare arsenomolybdate-based rare earth derivatives; imidazole has a variety of coordination modes and a strong ability to bind transition metal ions, and is an effective linker for the coordination assembly of arsenomolybdate-based rare earth derivatives. In addition, protonated imidazole [C3N2H5] + As a counter cation, it forms hydrogen bonds with arsenomolybdate-based rare earth derivatives, thereby stabilizing the crystal structure and facilitating crystallization.

[0066] In the present invention, the temperature of the in-situ self-assembly is preferably 60-80° C., more preferably 60-70° C.; the time of the in-situ self-assembly is preferably 30-40 min, more preferably 30-35 min.

[0067] In the present invention, after the in-situ self-assembly, it is preferred that the method further includes: filtering the system after the in-situ self-assembly, cooling, standing and solid-liquid separation are performed in sequence to obtain the arsenomolybdate-based rare earth derivative. The present invention has no special requirements for the filtration, and the conventional method in the art can be used. In the present invention, the temperature after cooling is preferably room temperature, and the temperature of the room temperature is preferably 20 to 35°C, more preferably 25 to 30°C. In the present invention, the standing time is preferably 6 to 8 days, more preferably 7 days. In the present invention, the standing process is the process of precipitating crystals. The present invention has no special requirements for the solid-liquid separation, as long as the crystals can be separated.

[0068] The present invention also provides a modified composite of an arsenomolybdate-based rare earth derivative, comprising an arsenomolybdate-based rare earth derivative and a carboxylated multi-walled carbon nanotube, wherein the carboxylated multi-walled carbon nanotube is combined with the arsenomolybdate-based rare earth derivative by intermolecular forces;

[0069] The arsenomolybdate-based rare earth derivative is the arsenomolybdate-based rare earth derivative described in the above technical solution or the arsenomolybdate-based rare earth derivative prepared by the preparation method described in the above technical solution.

[0070] In the present invention, the inner diameter of the carboxylated multi-walled carbon nanotubes (COOH-MCNTs) is preferably 5 to 8 nm, more preferably 6 to 7 nm; the outer diameter of the carboxylated multi-walled carbon nanotubes is preferably 10 to 15 nm, more preferably 12 to 14 nm; the length of the carboxylated multi-walled carbon nanotubes is preferably 2 to 8 μm, more preferably 3 to 7 μm; the carboxyl content of the carboxylated multi-walled carbon nanotubes is preferably 1.0 to 2.0 mmol / g, more preferably 1.0 to 1.5 mmol / g; the specific surface area of ​​the carboxylated multi-walled carbon nanotubes is preferably ≥ 190 m 2 / g, more preferably 190 to 210 m 2 / g.

[0071] In the present invention, the mass ratio of the arsenomolybdate-based rare earth derivative to the carboxylated multi-walled carbon nanotube is preferably 1:0.8-1.2, more preferably 1:1.

[0072] In the present invention, the method for preparing the modified composite of arsenomolybdate-based rare earth derivatives described in the above technical solution comprises the following steps:

[0073] The arsenomolybdate-based rare earth derivative and the carboxylated multi-walled carbon nanotube are ground and mixed to obtain the modified composite of the arsenomolybdate-based rare earth derivative.

[0074] In the present invention, the grinding and mixing time is preferably 4 to 6 minutes, more preferably 5 minutes; the grinding is preferably carried out in an agate mortar; the grinding speed is preferably 60 to 90 r / min, more preferably 70 to 80 r / min.

[0075] In the present invention, the carboxylated multi-walled carbon nanotubes are combined with the arsenomolybdate-based rare earth derivatives through intermolecular forces during the grinding and mixing process, and the intermolecular forces include hydrogen bonds or electrostatic attraction.

[0076] In the present invention, carboxylated multi-walled carbon nanotubes have a large specific surface area and excellent electron transfer performance. Compounding them with arsenomolybdate-based rare earth derivatives can enhance the dispersion and conductivity of arsenomolybdate-based rare earth derivatives on the electrode surface, further improve the electrocatalytic activity of arsenomolybdate-based rare earth derivatives, synergistically expand the current detection signal, and improve the electrochemical detection sensitivity. The modified composite of arsenomolybdate-based rare earth derivatives provided by the present invention has excellent electrocatalytic activity, can be used as an electrode modification material, effectively improve the detection sensitivity of electrochemical sensors, and achieve highly sensitive electrochemical detection of nitrite.

[0077] The present invention also provides a modified electrode, comprising a substrate and a coating coated on the surface of the substrate, wherein the coating is formed by film-forming a dispersion of a modified composite of an arsenomolybdate-based rare earth derivative;

[0078] The method for preparing the dispersion of the modified composite of the arsenomolybdate-based rare earth derivative comprises the following steps: mixing the modified composite of the arsenomolybdate-based rare earth derivative, ethanol, a perfluorosulfonic acid type polymer solution and water to obtain the dispersion of the modified composite of the arsenomolybdate-based rare earth derivative;

[0079] The modified compound of arsenomolybdate-based rare earth derivative is the modified compound of arsenomolybdate-based rare earth derivative described in the above technical solution or the modified compound of arsenomolybdate-based rare earth derivative prepared by the preparation method described in the above technical solution.

[0080] In the present invention, the substrate preferably includes a glassy carbon electrode (GCE).

[0081] In the present invention, the ethanol is preferably anhydrous ethanol; the mass concentration of the perfluorosulfonic acid polymer (Nafion) solution is preferably 4-6%, more preferably 5%. In the present invention, the volume ratio of the ethanol, perfluorosulfonic acid polymer solution and water is preferably 760-800:18-22:180-220, more preferably 780:20:200. In the present invention, the mass ratio of the modified complex of the arsenomolybdate-based rare earth derivative and the volume ratio of ethanol is preferably 8-12mg:760-800mL, more preferably 10mg:780mL. In the present invention, the mixing of the modified complex of the arsenomolybdate-based rare earth derivative, ethanol, perfluorosulfonic acid polymer solution and water is preferably carried out under ultrasonic conditions, and the ultrasonic time is preferably 35-45min, more preferably 40min. The present invention has no special requirements for the power of the ultrasound, as long as it can be evenly dispersed.

[0082] The present invention preferably drips the dispersion of the modified complex of the arsenomolybdate-based rare earth derivative onto the surface of the substrate and then dries to obtain the modified electrode. The present invention has no special requirements for the drip coating, and a conventional method in the art can be used. In the present invention, the drying is preferably carried out under an infrared lamp, and the drying time is preferably 1.8 to 2.2 hours, more preferably 2 hours.

[0083] In the present invention, the thickness of the coating is preferably 0.2 to 0.5 mm, more preferably 0.3 to 0.4 mm.

[0084] In the present invention, arsenomolybdate-based rare earth derivatives have good redox ability and catalytic activity, and carboxylated multi-walled carbon nanotubes have a large specific surface area; the modified complex of arsenomolybdate-based rare earth derivatives not only has good catalytic performance, but also has strong adhesion ability on the electrode surface, thereby amplifying the electrochemical signal of the detected nitrite, thereby improving the electrochemical detection sensitivity.

[0085] The modified electrode provided by the present invention shows excellent electrochemical detection performance for nitrite detection, including a wide linear range of 20 to 220 μM and a high sensitivity of 0.027 μA·μM -1 and a low detection limit of 3.34 μM.

[0086] The present invention also provides the application of the modified electrode in electrochemical detection. In the present invention, the application of the modified electrode in electrochemical detection is preferably to use the modified electrode as an electrochemical sensor for nitrite detection. In the present invention, the nitrite is preferably sodium nitrite.

[0087] In order to further illustrate the present invention, the technical solutions provided by the present invention are described in detail below in conjunction with embodiments, but they should not be construed as limiting the protection scope of the present invention.

[0088] Example 1

[0089] 0.035 g NaAsO2 (0.269 mmol) and 0.5 g (NH4)6Mo7O 24 4H2O (0.404mmol) was dissolved in 20mL water to obtain NaAsO2 and (NH4)6Mo7O 24 Mixed solution; NaAsO2 and (NH4)6Mo7O 24 The mixed solution and a 4 mol / L HCl solution are mixed to adjust the pH value of the system to 1.0 to obtain an arsenic molybdenum oxy-cluster solution;

[0090] The arsenomolybdenum oxy-cluster solution, 0.1 g PrCl3·6H2O (0.695 mmol), 0.1 g imidazole (1.469 mmol), and an ammonia solution with a molar concentration of 1 mol / L were mixed to adjust the pH value of the system to 4.0, and then in-situ self-assembled for 30 min at 60° C.; the system after in-situ self-assembled was filtered, cooled to 30° C., and allowed to stand for 7 days, and solid-liquid separation was performed to obtain a light green crystalline arsenomolybdate-based rare earth derivative.

[0091] 5 mg of arsenomolybdate-based rare earth derivatives and 5 mg of carboxylated multi-walled carbon nanotubes (COOH-MCNTs, inner diameter of 7 nm, outer diameter of 13 nm, length of 6 μm, carboxyl content of 1 mmol / g, specific surface area of ​​200 m 2 / g) were ground and mixed in an agate mortar at a rotation speed of 90r / min for 5min to obtain a modified composite of arsenomolybdate-based rare earth derivatives.

[0092] 10 mg of the modified composite of the arsenomolybdate-based rare earth derivative, 200 μL of water, 780 μL of ethanol and 20 μL of a Nafion solution with a mass concentration of 5 wt% were ultrasonically dispersed for 40 min to obtain a dispersion of the modified composite of the arsenomolybdate-based rare earth derivative;

[0093] The dispersion was transferred with a pipette, 3 μL was drop-coated on the surface of the glassy carbon electrode, and dried under an infrared lamp for 2 h to obtain a modified electrode (arsenomolybdate-based rare earth derivative / COOH-MCNTs / GCE) with a coating thickness of 0.5 mm.

[0094] Comparative Example 1

[0095] Arsenomolybdate-based rare earth derivatives were prepared according to the method of Example 1, except that Na2MoO4·2H2O was used instead of (NH4)6Mo7O 24 ·4H2O raw material, the product prepared is light green powder instead of crystal.

[0096] Detection of arsenomolybdate-based rare earth derivatives:

[0097] The arsenomolybdate-based rare earth derivative prepared in Example 1 was subjected to X-ray powder diffraction (XRD) test, and the XRD spectrum was obtained as follows: Figure 6 As shown. Figure 6 The XRD pattern of the arsenomolybdate-based rare earth derivative prepared in Example 1 observed in the experiment is basically consistent with the main peak position in the simulation spectrum (theory), thereby verifying the high purity of the arsenic molybdenum oxygen cluster complex.

[0098] The arsenomolybdate-based rare earth derivatives prepared in Example 1 and Comparative Example 1 were subjected to infrared detection to obtain infrared spectra, such as Figure 7 shown. Figure 7 Example 1 at 893 cm -1 、801cm -1 、730cm -1 、610cm -1 and 544cm -1 The five characteristic peaks at 10 O 35 ] 7- Anion υ(As-O), υ(Mo=O t ),υ(Mo-O b -Mo) and υ(Mo-O c -Mo) stretching vibration. 2977~1053cm -1 The peaks in the region correspond to the characteristic vibration peaks of imidazole ligands. -1 and 2840cm -1 The band at 1575-1053cm is attributed to υ(CH) stretching vibration. -1 The strong absorption peak at 421 cm-1 is attributed to the δ(NH) and δ(CH) bending vibrations, υ(C=C) and υ(C=N) stretching vibrations of the imidazole ring. -1 The band at is attributed to the stretching vibration of υ(Na-N), indicating that Na + Coordination between ions and imidazole ligands. 3141cm -1 The broad band at is the υ(OH) stretching vibration of the lattice water molecules. Figure 7 It is shown that the infrared absorption peak of Comparative Example 1 is significantly different from that of Example 1, indicating that the products prepared in Comparative Example 1 and Example 1 have different structures.

[0099] The arsenomolybdate-based rare earth derivative prepared in Example 1 was subjected to thermogravimetric analysis to obtain a thermogravimetric curve. Figure 8 shown. Figure 8It shows a three-step weight loss process in the temperature range of 35 to 800°C. The first weight loss is 8.52% (calculated value is 8.47%), which occurs between 35 and 324°C. The reason is the release of 32 lattice water molecules, 2 ammonia molecules and 6 coordinated water molecules. In the temperature range of 324 to 538°C, the second weight loss is 14.49%, which is because 18 imidazole molecules are removed (calculated value is 14.43%). When heated to 800°C, the third weight loss is 6.68% (calculated value is 6.58%), which is due to the escape of As2O3 and H2O produced by the decomposition of the POM framework, and the final product is a mixed metal oxide. The total weight loss of 29.69% is basically consistent with the theoretical value of 29.48%.

[0100] The arsenomolybdate-based rare earth derivative prepared in Example 1 was subjected to ultraviolet-visible light detection in an aqueous solution with a pH value of 4.0 to obtain an ultraviolet-visible absorption spectrum, as shown in FIG. Fig. 9 shown. Fig. 9 In the wavelength range of 200-400 nm, two characteristic peaks appeared at 203 nm and 232 nm, belonging to O b,c →Mo and O d →Mo charge transfer transition. The five broad peaks at 449nm, 474nm, 489nm, 589nm and 598nm can be attributed to Pr 3+ Ionic 3 H4→ 3 P2, 3 H4→ 3 P1, 3 H4→ 3 P0 and 3 H4→ 1 D2 transition.

[0101] The arsenomolybdate-based rare earth derivative prepared in Example 1 was observed using a scanning electron microscope (SEM) to obtain a SEM image and a SEM-mapping map. Fig.10 As shown. Fig.10 It can be seen that the arsenomolybdate-based rare earth derivatives have a rectangular flake structure with a smooth surface, clear edges, and a size between 5 and 20 μm.

[0102] The arsenomolybdate-based rare earth derivative prepared in Example 1 was subjected to energy dispersion spectroscopy (EDS) testing to obtain an energy dispersion spectrum as shown in the following figure: Fig.11 The presence of As, Mo, Pr, Na, C, N and O in arsenomolybdate-based rare earth derivatives was confirmed by combining energy dispersive spectroscopy and SEM-mapping.

[0103] The results of the above XRD detection, infrared detection, thermogravimetric decomposition, ultraviolet detection, SEM detection and EDS detection prove that the arsenomolybdate-based rare earth derivative prepared in Example 1 has the molecular formula shown in Formula 1. The crystallographic data of the arsenomolybdate-based rare earth derivative prepared in Example 1 are shown in Table 1.

[0104] Table 1 Crystallographic data of arsenomolybdate-based rare earth derivatives

[0105]

[0106]

[0107] a R1=∑|F o |-|F c | / ∑|F c |;wR2=[∑w(F o 2 -F c 2 ) 2 / ∑w(F o 2 ) 2 ] 1 / 2

[0108] Performance test of modified electrode:

[0109] In a mixed solution of H2SO4 with a molar concentration of 0.1 mol / L and Na2SO4 with a molar concentration of 0.1 mol / L, in the potential range of -0.8 to +0.6 V, at a scanning rate of 100 mV / s, the cyclic voltammetry (CV) behavior of the arsenomolybdate-based rare earth derivative / COOH-MCNTs / GCE prepared in Example 1 was tested using a three-electrode system, and a cyclic voltammetry curve was obtained, as shown in FIG. Fig.12 shown. Fig.12 The cyclic voltammetry curve shows three pairs of reversible redox peaks with an average peak potential of E 1 / 2 =(E pa +E pc ) / 2 is -0.586V(II′), -0.372V(II-II′) and -0.226V(III-III′), which is attributed to Mo VI Central redox process.

[0110] The CV curves of the arsenomolybdate-based rare earth derivative / COOH-MCNTs / GCE prepared in Example 1 were tested according to the above method, except that the scanning rates were 40 mV·s -1 , 70mV·s -1 , 100mV·s -1, 130mV·s -1 , 160mV·s -1 and 190mV·s -1 ; The cyclic voltammetry curves obtained at different scan rates are as follows: Fig.13 As shown. Fig.13 It can be seen from 40mV·s -1 Increase to 190mV·s -1 The current intensity of the CV curve gradually increases when the scanning rate increases. The peak current of II-II′ shows a good linear relationship with the scanning rate, which indicates that the redox process of arsenomolybdate-based rare earth derivatives is a surface-controlled process.

[0111] The CV behavior of the arsenomolybdate-based rare earth derivative / COOH-MCNTs / GCE prepared in Example 1 was tested according to the above method, with a scan rate of 100 mV·s -1 , and obtain the cyclic voltammetry curves at different times, such as Fig.14 The stability of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE was evaluated by measuring the cyclic voltammetry curves at different times. Fig.14 It shows that the position and current intensity of the redox peak have basically not changed after scanning for 48 hours, indicating that arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE have good stability in a mixed solution of H2SO4 with a molar concentration of 0.1 mol / L and Na2SO4 with a molar concentration of 0.1 mol / L.

[0112] Fig.15 The CV curves of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE in a mixed solution of H2SO4 (0.1mol / L) and Na2SO4 (0.1mol / L) containing different concentrations of sodium nitrite (0mmol / L, 1mmol / L, 2mmol / L, 3mmol / L and 4mmol / L) were obtained by three-electrode system detection in the potential range of -0.8 to +0.6V and the scanning rate of 100mV / s. After adding 1mmol / L sodium nitrite, the reduction peak currents of I, II and III increased significantly, but the oxidation peak currents of I', II' and III' decreased accordingly, indicating that the reducing species of Mo center in the framework of arsenomolybdate-based rare earth derivatives have obvious electrocatalytic reduction activity for sodium nitrite.

[0113] The electrocatalytic properties of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE indicate that it has potential sensing properties for detecting nitrite. The present invention further evaluates the detection sensitivity of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE using chronoamperometry, and sets -0.5V as the working potential. Fig.16 The amperometric current response curve is shown in a mixed solution (electrolyte) of H2SO4 (0.1 mol / L) and Na2SO4 (0.1 mol / L) when 30 μmol / L sodium nitrite is added to the electrolyte solution every 30 seconds. Fig.16 It can be seen that the current response of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE gradually increases with the increase of sodium nitrite concentration, and the response time to reach 95% steady-state current is less than 3s, indicating that sodium nitrite undergoes a rapid reduction process on arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE. In the range of 30 to 270 μM, the current response of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE shows a good linear relationship with nitrite concentration.

[0114] According to the linear relationship fitted by the current response signal of arsenomolybdate-based rare earth derivatives / COOH-MCNTs / GCE and the detection results of sodium nitrite concentration, the linear regression equation is I 亚硝酸钠 =0.1329C 亚硝酸钠 +5.089(R 2 =0.996), the linear curve is as follows Fig.17 As shown. Fig.17 It can be seen that the sensitivity is 0.1329μA·μM -1 , the detection limit was calculated to be 2.24 μM (S / N=3).

[0115] Although the above embodiment describes the present invention in detail, it is only a part of the embodiments of the present invention, not all of the embodiments. People can also obtain other embodiments based on this embodiment without creativity, and these embodiments all fall within the protection scope of the present invention.

Claims

1. An arsenomolybdate-based rare earth derivative, characterized in that: It has the chemical formula shown in Formula 1: H4(NH4)2(C3N2H5) 16 [Na(C3N2H4)]2[Pr 0.5 Na 0.5 (H2O)3]2[AsMo 10 O 35 ]4·32H2O Formula 1; The arsenomolybdate-based rare earth derivatives are composed of 4 [AsMo 10 O 35 ] 7- Anion, 4 [H + ], 16 [C3N2H5] + cation, 2 [Pr 0.5 Na 0.5 (H2O)3] 2+ unit and 2 [Na(C3N2H4)2] + The unit is composed of 32 crystal water molecules; The [AsMo 10 O 35 ] 7- The Mo-O bond length in the anion is The [AsMo 10 O 35 ] 7- The As-O bond length in the anion is 4 [AsMo 10 O 35 ] 7- The anion is formed by the interaction with two [Pr 0.5 Na 0.5 (H2O)3] 2+ unit and 2 [Na(C3N2H4)2] + The units are connected by coordination to form a ring structure; [C3N2H5] + Cations and crystal water molecules fill the spaces between adjacent ring structures; [Na(C3N2H4)2] + Na in unit + With two N atoms from two C3N2H4 ligands and two [AsMo 10 O 35 ] 7- The two O atoms of the anion are coordinated.

2. The arsenomolybdate-based rare earth derivative according to claim 1, characterized in that: The space group of the arsenomolybdate-based rare earth derivative is Pnnm, and a is b is c is α is 90°, β is 90°, γ is 90°, Z is 2; the unit cell volume is 3. The method for preparing the arsenomolybdate-based rare earth derivative according to claim 1 or 2, characterized in that: The following steps are involved: NaAsO2 and (NH4)6Mo7O 24 The mixed solution and the first pH value adjusting agent are first mixed to obtain an arsenic molybdenum oxy-cluster solution; the pH value of the system after the first mixing is 1.0 to 1.5; The arsenic molybdenum oxy-cluster solution is mixed with praseodymium chloride, imidazole and a second pH value regulator for a second time and then self-assembled in situ to obtain the arsenic molybdate-based rare earth derivative; the pH value of the system after the second mixing is 4.0-4.

5.

4. The preparation method according to claim 3, characterized in that: The second mixed system contains NaAsO2, (NH4)6Mo7O 24 , praseodymium chloride and imidazole in a molar ratio of 0.269:0.404:0.281:1.469; The first pH value adjusting agent is a hydrochloric acid solution; the second pH value adjusting agent is an ammonia solution; The temperature of the in-situ self-assembly is 60° C. to 80° C., and the time is 30 to 40 minutes.

5. The preparation method according to claim 4, characterized in that: The molar concentration of the hydrochloric acid solution is 3-5 mol / L, and the molar concentration of the ammonia solution is 0.5-1.5 mol / L.

6. A modified composite of an arsenomolybdate-based rare earth derivative, characterized in that: It comprises an arsenomolybdate-based rare earth derivative and a carboxylated multi-walled carbon nanotube, wherein the carboxylated multi-walled carbon nanotube is combined with the arsenomolybdate-based rare earth derivative by intermolecular forces; The arsenomolybdate-based rare earth derivative is the arsenomolybdate-based rare earth derivative according to claim 1 or 2 or the arsenomolybdate-based rare earth derivative prepared by the preparation method according to any one of claims 3 to 5.

7. The modified composite of arsenomolybdate-based rare earth derivatives according to claim 6, characterized in that: The carboxylated multi-walled carbon nanotube has an inner diameter of 5 to 8 nm, an outer diameter of 10 to 15 nm, a length of 2 to 8 μm, a carboxyl content of 1.0 to 2.0 mmol / g, and a specific surface area of ​​190 m 2 / g; The mass ratio of the arsenomolybdate-based rare earth derivative to the carboxylated multi-walled carbon nanotube is 1:0.8-1.

2.

8. The method for preparing the modified composite of arsenomolybdate-based rare earth derivatives according to claim 6 or 7, comprising the following steps: The arsenomolybdate-based rare earth derivative and the carboxylated multi-walled carbon nanotube are ground and mixed to obtain the modified composite of the arsenomolybdate-based rare earth derivative.

9. A modified electrode, characterized in that: The invention comprises a substrate and a coating coated on the surface of the substrate, wherein the coating is formed by forming a film from a dispersion of a modified composite of an arsenomolybdate-based rare earth derivative; The method for preparing the dispersion of the modified composite of the arsenomolybdate-based rare earth derivative comprises the following steps: mixing the modified composite of the arsenomolybdate-based rare earth derivative, ethanol, a perfluorosulfonic acid type polymer solution and water to obtain the dispersion of the modified composite of the arsenomolybdate-based rare earth derivative; The modified compound of the arsenomolybdate-based rare earth derivative is the modified compound of the arsenomolybdate-based rare earth derivative according to claim 6 or 7 or the modified compound of the arsenomolybdate-based rare earth derivative prepared by the preparation method according to claim 8.

10. Use of the modified electrode according to claim 9 in electrochemical detection.

Citation Information

Cited By

  • Rare earth-polyacid-based compound and preparation method and application thereof

    CN119874560A