Processing method of catalytic diesel oil

Through the combined process of reacting catalytic diesel with hydrogen and then mixing it with alkali metal, the problem of over-saturation of aromatic hydrocarbons and large loss of extraction solvent in catalytic diesel is solved, and the effect of improving BTX yield and fuel oil quality is achieved.

CN118853232AActive Publication Date: 2024-10-29CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202310458342.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-26
Publication Date
2024-10-29
Estimated Expiration
2043-04-26

AI Technical Summary

Technical Problem

In existing catalytic diesel processing methods, aromatic hydrocarbons are oversaturated and extraction solvents are lost, leading to problems such as reduced fuel oil quality and low yield.

Method used

The hydrorefining, alkali metal treatment and hydrocracking processes are combined to catalyze the reaction of diesel with hydrogen and then mix it with alkali metal for separation and hydrocracking to avoid over-saturation of aromatic hydrocarbons and increase the BTX yield.

Benefits of technology

It effectively avoids oversaturation of aromatic hydrocarbons, increases the yield of BTX, reduces the operating conditions of the hydrotreating unit, and improves the quality of fuel oil.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118853232A_ABST
    Figure CN118853232A_ABST
Patent Text Reader

Abstract

The invention discloses a processing method of catalytic diesel oil, which comprises the following steps: (1) mixing the catalytic diesel oil with hydrogen, feeding into a hydrofining reaction zone, and contacting with a hydrofining catalyst for reaction to obtain a hydrofining reaction effluent; (2) in the presence of hydrogen, the hydrofining reaction effluent in the step (1) is mixed with alkali metal, and the mixture enters an alkali metal treatment reaction zone for reaction; (3) carrying out separation treatment on the alkali metal treatment effluent obtained in the step (2) to obtain an alkali metal treatment liquid phase product; and (4) enabling the alkali metal treatment liquid phase product in the step (3) to enter a hydrocracking reaction zone, sequentially carrying out gas-liquid separation and fractionation on the reaction effluent to obtain gas, light naphtha, heavy naphtha and tail oil, and enabling the heavy naphtha to enter an aromatic hydrocarbon extraction device to obtain BTX. According to the method, hydrofining, alkali metal treatment and hydrocracking processes are combined to process the catalytic diesel oil, so that aromatic hydrocarbon oversaturation can be effectively avoided, and the BTX yield is increased.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for processing catalytic diesel, in particular to a method for processing catalytic diesel to produce more BTX. Background Art

[0002] Catalytic cracking diesel is one of the products of catalytic cracking unit. It has a high sulfur content and is rich in a large amount of aromatics. The aromatic content in catalytic diesel can be as high as 70-90%, mainly monocyclic, bicyclic and tricyclic aromatics. Monocyclic aromatics are mainly indane and tetralin, and polycyclic aromatics are mainly naphthalene and acenaphthene. Taking the catalytic diesel of a refinery as an example, monocyclic aromatics are mainly concentrated in the lighter fraction section of <260℃, while bicyclic aromatics are mainly concentrated in the heavier fraction section (>260℃). Hydrogenation technology is currently the main technical means for processing catalytic diesel. Although traditional hydrorefining technology can remove sulfur and nitrogen impurities in catalytic diesel, the hydrogen consumption in the hydrogenation process is high, and the deep desulfurization process will cause the problem of over-saturation of aromatics, reducing the quality of fuel oil.

[0003] CN106047404A discloses a combined process method for increasing the production of high-octane gasoline from inferior catalytic cracking diesel. The method firstly passes inferior catalytic cracking diesel through a hydrofining reactor under a hydrogen atmosphere and relatively mild refining conditions to carry out selective hydrogenation and desulfurization of condensed aromatics, and the refined liquid product enters a lightening reactor equipped with a precious metal catalyst for hydrogenation and lightening, thereby finally achieving the purpose of producing more high-octane gasoline. The above method uses conventional hydrofining agents. In order to achieve the purpose of deep impurity removal, the reaction conditions are harsh and there is a problem of oversaturation of aromatics.

[0004] CN103897731A discloses a catalytic cracking diesel and C 10 + The method for producing light aromatics by mixing distillate oils comprises the following steps: firstly mixing catalytic cracking diesel, C 10 + The distillate oil is mixed with hydrogen and subjected to a hydrorefining reaction to remove sulfur and nitrogen, saturate olefins and properly saturate aromatics; the hydrorefining product is then extracted with an extraction solvent to obtain an extracted oil rich in aromatics and a raffinate oil rich in alkanes; the raffinate oil is used as a clean diesel blending component, and the extracted oil is separated by distillation to obtain an aromatic extracted oil; the aromatic extracted oil is subjected to a hydrocracking reaction, and the hydrocracking product is then cut and separated, wherein the distillate oil product with a temperature of >195°C is used as a clean diesel blending component; the distillate oil with a temperature of <195°C is used as an aromatic raw material and enters an aromatic processing unit to obtain a light aromatic product and a clean gasoline blending component. The above method has the problem of large loss of extraction solvent and poor extraction effect. Summary of the invention

[0005] In view of the shortcomings of the prior art, the present invention provides a method for processing catalytic diesel, which combines hydrorefining, alkali metal treatment and hydrocracking processes to process catalytic diesel, which can effectively avoid oversaturation of aromatics and improve BTX yield.

[0006] A method for processing catalytic diesel, the method comprising the following steps: (1) Catalytic diesel and hydrogen are mixed and enter the hydrotreating reaction zone, where they are contacted with the hydrotreating catalyst to react and obtain a hydrotreating reaction effluent; (2) In the presence of hydrogen, the effluent from the hydrotreating reaction in step (1) is mixed with an alkali metal and enters an alkali metal treatment reaction zone for reaction; (3) separating and treating the alkali metal treatment effluent obtained in step (2) to obtain an alkali metal treatment liquid phase product; (4) The alkali metal treated liquid product in step (3) enters the hydrocracking reaction zone, and the reaction effluent is subjected to gas-liquid separation and fractionation in sequence to obtain gas and light naphtha, heavy naphtha and tail oil. The heavy naphtha enters the aromatics extraction unit to obtain BTX.

[0007] In the method of the present invention, the catalytic diesel in step (1) is one of the main products of the catalytic cracking unit; the catalytic diesel is the 160°C-370°C fraction in the catalytic cracking full fraction product, preferably the 220°C-340°C fraction; the density of the catalytic diesel is generally 0.90 g / cm -3 -0.99 g / cm -3 The sulfur content is generally 200 μg / g-8000 μg / g, the nitrogen content is generally 100 μg / g-2000 μg / g, and the aromatic hydrocarbon content is generally 50wt%-90wt%, preferably 60wt%-85wt%.

[0008] In the method of the present invention, the catalytic diesel in step (1) is cut to obtain light distillate oil and heavy distillate oil, and the heavy distillate oil is mixed with hydrogen and enters the hydrotreating reaction zone; the cutting point is 250°C-300°C, preferably 260°C-275°C; the content of monocyclic aromatic hydrocarbons in the heavy distillate oil is 0.1 wt.%-10wt.%, preferably 0.2 wt.%-5wt.%, and more preferably 0.5 wt.%-2wt.%.

[0009] In the method of the present invention, the hydrotreating catalyst in step (1) comprises a carrier and an active metal, wherein the carrier may be alumina or / and amorphous silicon aluminum, and the content thereof is 45-90 wt% by mass; the active metal comprises a main active metal and an auxiliary metal; the main active metal is a Group VIB metal component, such as tungsten or / and molybdenum, and the content thereof is 5-50 wt% by mass of the metal oxide; the auxiliary metal is a Group VIB metal component, such as cobalt or / and nickel, and the content thereof is 2-30 wt% by mass of the metal oxide.

[0010] In the method of the present invention, in step (1), the sulfur content of the hydrotreating effluent is controlled to be 50 μg / g-1000 μg / g, preferably 150 μg / g-850 μg / g, and more preferably 200 μg / g-500 μg / g; the nitrogen content is controlled to be 50 μg / g-800 μg / g, preferably 100 μg / g-500 μg / g, and more preferably 120 μg / g-200 μg / g. Specifically in the present invention, the sulfur content of the hydrotreating effluent is controlled to be 50μg / g-1000μg / g, preferably 150μg / g-850μg / g, and more preferably 200μg / g-500μg / g; the nitrogen content is controlled to be 50μg / g-800μg / g, preferably 100μg / g-500μg / g, and more preferably 120μg / g-200μg / g by controlling the operating conditions of the hydrotreating reactor.

[0011] In the method of the present invention, the process conditions of the hydrofining reaction zone in step (1) are compared with the process conditions of the conventional hydrofining reaction zone, and the reaction pressure is 0.5MPa-5.0MPa lower, the average reaction temperature is 10°C-40°C lower, and the volume space velocity is 0.5-3.0 h higher. -1 Preferably, the reaction pressure is 1.0MPa-2.5MPa lower, the average reaction temperature is 15℃-25℃ lower, and the volume space velocity is 0.8-2.0 h higher. -1 The process conditions of the conventional hydrofining reaction zone are generally: reaction pressure of 3.0 MPa-15.0 MPa, average reaction temperature of 300℃-450℃, volume space velocity of 0.5-10.0h -1 The preferred reaction pressure is 5.0 MPa-12.0 MPa, the average reaction temperature is 350°C-400°C, and the volume space velocity is 1.0-5.0 h -1 .

[0012] In the method of the present invention, the hydrogen-oil volume ratio in the hydrofining reaction zone in step (1) is 300 Nm 3 / m 3 -1500Nm 3 / m 3 , preferably 400Nm3 / m 3 -1200Nm 3 / m 3 .

[0013] In the method of the present invention, step (2) also introduces a light distillate oil obtained by cutting the catalytic diesel, and the light distillate oil is mixed with the hydrotreating reaction effluent in step (1) and an alkali metal and enters the alkali metal treatment reaction zone for reaction. During the research process, it was found that when the catalytic diesel is cut at a cutting point of 260-275°C, the monocyclic aromatic hydrocarbons are mainly concentrated in the lighter fraction segment, while the dicyclic and higher aromatic hydrocarbons are mainly concentrated in the heavier fraction segment. The present invention cuts the catalytic diesel according to the distribution law of monocyclic aromatic hydrocarbons and dicyclic and higher aromatic hydrocarbons in the catalytic diesel, and the light fraction rich in monocyclic aromatic hydrocarbons directly enters the alkali metal treatment device for desulfurization and denitrogenation reactions, thereby avoiding the hydrogenation saturation reaction of monocyclic aromatic hydrocarbons in the hydrotreating device.

[0014] In the method of the present invention, the alkali metal in step (2) is at least one of lithium, sodium, potassium, rubidium, cesium and francium, preferably lithium, sodium or potassium, and more preferably sodium; the mass ratio of the alkali metal to the hydrotreating reaction effluent is (0.1-5.0):100, preferably (0.5-2.5):100.

[0015] In the method of the present invention, the reactor used in the alkali metal treatment reaction zone in step (2) is one or more of a kettle reactor, a pipeline reactor and a tower reactor, preferably a kettle reactor.

[0016] In the method of the present invention, the process conditions of the alkali metal treatment reaction zone in step (2) are generally as follows: reaction temperature 200°C-380°C, hydrogen partial pressure 0.5MPa-15.0MPa, reaction time or residence time 0.1h-2.0h, hydrogen to oil volume ratio 100Nm 3 / m 3 -1000Nm 3 / m 3 Preferably, the reaction temperature is 280°C-340°C, the hydrogen partial pressure is 2.0MPa-8.0MPa, the reaction time or residence time is 0.5h-1.0h, and the hydrogen-to-oil volume ratio is 350Nm 3 / m 3 -750Nm 3 / m 3 .

[0017] In the method of the present invention, the separation treatment in step (3) is a solid-liquid separation treatment. There is no special regulation on the method of solid-liquid separation, and any of the existing solid-liquid separation methods in the art can be used. Specifically in the present invention, the solid-liquid separation method can be at least one of vacuum filtration, pressure filtration, filtration centrifugation, sedimentation centrifugation or membrane filtration.

[0018] In the method of the present invention, the acid value of the liquid phase stream obtained by the separation treatment in step (3) is less than 0.85 mgKOH / g, preferably less than 0.35 mgKOH / g; the solid content is 15-500 ppm, preferably 25-150 ppm.

[0019] In the method of the present invention, the separation process in step (3) is as follows: the alkali metal treatment effluent obtained in step (2) is subjected to a solid-liquid separation to obtain a first liquid phase stream; the first liquid phase stream is mixed with an auxiliary agent, and the mixed material is subjected to a second solid-liquid separation to obtain a second liquid phase stream, wherein the auxiliary agent is at least one of formic acid, acetic acid, phosphoric acid, hydrochloric acid and sulfuric acid; the mass ratio of the auxiliary agent to the first liquid phase stream is (1-10):100, preferably (3-7):100. The alkali value in the first liquid phase stream is controlled to be 15-30 mgKOH / g, preferably 11-20 mgKOH / g; the solid content is 500-2000 ppm, preferably 500-1000 ppm. The acid value in the second liquid phase stream is controlled to be less than 0.85 mgKOH / g, preferably less than 0.35 mgKOH / g, and the solid content is 15-500 ppm, preferably 25-150 ppm.

[0020] In the method of the present invention, in step (3), an acidic additive is optionally added under stirring at a suitable temperature, wherein the temperature is 100-300° C., preferably 150-250° C. The stirring rate is 100-1500 r / min, preferably 500-1000 r / min.

[0021] In the method of the present invention, the catalyst used in the hydrocracking reaction zone in step (4) includes a carrier and a metal active component; the carrier includes at least one of alumina, amorphous silica-alumina, and a molecular sieve, and the molecular sieve is usually a Y-type and / or a β-type molecular sieve; the metal active component is a metal of Group VI, Group VII, or Group VIII, a metal oxide, or a metal sulfide, preferably one or more of iron, chromium, molybdenum, tungsten, cobalt, or nickel. Based on the weight of the catalyst, the content of the metal active component in terms of oxide is generally 10-35wt%, and the content of the carrier in terms of mass is generally 60-85wt%.

[0022] In the method of the present invention, the process conditions of the hydrocracking reaction zone in step (4) are generally: reaction pressure of 3.0MPa-18.0MPa, average reaction temperature of 320℃-450℃, volume space velocity of 1.0-8.0h -1 , hydrogen to oil volume ratio is 300Nm 3 / m 3 -1500Nm 3 / m 3The preferred reaction pressure is 5.0 MPa-15.0 MPa, the average reaction temperature is 350°C-420°C, and the volume space velocity is 1.0-3.0 h -1 , hydrogen to oil volume ratio is 400Nm 3 / m 3 -1200Nm 3 / m 3 .

[0023] In the method of the present invention, the aromatics extraction in step (4) can adopt existing technologies, such as solvent liquid-liquid extraction method and extractive distillation method. Specifically in the present invention, the aromatics extraction adopts solvent liquid-liquid extraction method, and the solvent liquid-liquid extraction method includes Udex method (glycol solvent), Sulfolane method (cyclopentane solvent), Arosolvan method (N-methylpyrrolidone solvent), DMSO method (dimethyl sulfoxide solvent), Formex method (N-formylmorpholine solvent); the operating conditions of the aromatics extraction device are: the mass ratio of solvent to heavy naphtha is 1-10:1, the extraction temperature is 20-250°C, and the extraction pressure is 0.1-3MPa, preferably the mass ratio of solvent to heavy naphtha is 3-6:1, the extraction temperature is 80-150°C, and the extraction pressure is 0.5-1.0MPa.

[0024] In the method of the present invention, the tail oil in step (4) can be discharged from the device as a product, or can be recycled to the hydrotreating reaction zone.

[0025] Compared with the prior art, the advantages of the present invention are: (1) The method of the present invention organically combines hydrofining with an alkali metal treatment unit, controls the depth of desulfurization and denitrification reactions during the hydrofining process, and transfers the sulfur-containing compounds and nitrogen-containing compounds that are difficult to remove to the alkali metal treatment unit. On the one hand, it can give full play to the advantages of high selectivity of desulfurization and denitrification reactions of alkali metal treatment technology, and on the other hand, it can reduce the operating conditions of the hydrofining unit, especially the reaction pressure, to avoid oversaturation of aromatics, thereby further improving the yield of light aromatics.

[0026] (2) After being treated by the hydrotreating unit, the viscosity of the catalytic diesel is reduced, which is beneficial to the contact and reaction between the alkali metal and the catalytic diesel in the alkali metal treatment unit, thereby improving the reaction effect.

[0027] (3) Catalytic diesel is cut according to the distribution pattern of single-ring aromatic hydrocarbons and double-ring or higher aromatic hydrocarbons in the catalytic diesel. The light fraction rich in single-ring aromatic hydrocarbons directly enters the alkali metal treatment unit for desulfurization and denitrogenation reactions, thereby avoiding the hydrogenation saturation reaction of single-ring aromatic hydrocarbons in the hydrotreating unit. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1A schematic diagram of a catalytic diesel hydrogenation method used in an embodiment of the present invention.

[0029] Among them, 1 is catalytic diesel, 2 is hydrogen, 3 is hydrofining reaction zone, 4 is hydrofining reaction effluent, 5 is alkali metal, 6 is alkali metal treatment reaction zone, 7 is alkali metal treatment reaction effluent, 8 is a primary solid-liquid separation device, 9 is a solid phase product obtained by primary solid-liquid separation treatment, 10 is a first liquid phase feed stream, 11 is a purification treatment device, 12 is gas, 13 is a solid-liquid two-phase mixture obtained by purification treatment, 14 is an acidic additive, 15 is a secondary solid-liquid separation device, 16 is a second liquid phase feed stream, 17 is a solid phase product obtained by secondary solid-liquid separation treatment, 18 is a hydrocracking reaction zone, 19 is gas, 20 is light naphtha, 21 is heavy naphtha, and 22 is tail oil.

[0030] Figure 2 A schematic diagram of another catalytic diesel hydrogenation method used in an embodiment of the present invention.

[0031] Among them, 1 is catalytic diesel, 2 is a fractionation tower, 3 is a catalytic cracking diesel light fraction oil, 4 is a catalytic cracking diesel heavy fraction oil, 5 is hydrogen, 6 is a hydrotreating reaction zone, 7 is a hydrotreating reaction effluent, 8 is an alkali metal, 9 is an alkali metal treatment reaction zone, 10 is an alkali metal treatment reaction effluent, 11 is a primary solid-liquid separation device, 12 is a solid phase product obtained by a primary solid-liquid separation treatment, 13 is a first liquid phase feed stream, 14 is a purification treatment device, 15 is a gas, 16 is a solid-liquid two-phase mixture obtained by purification treatment, 17 is an acidic additive, 18 is a secondary solid-liquid separation device, 19 is a second liquid phase feed stream, 20 is a solid phase product obtained by a secondary solid-liquid separation treatment, 21 is a hydrocracking reaction zone, 22 is a gas, 23 is light naphtha, 24 is heavy naphtha, and 25 is tail oil. Implementation

[0032] The method provided by the present invention is described below in conjunction with the accompanying drawings.

[0033] like Figure 1As shown, catalytic diesel 1 is mixed with hydrogen 2 and enters hydrofining reaction zone 3 for reaction to obtain hydrofining effluent 4; hydrofining effluent 4 is mixed with alkali metal 5 and enters alkali metal treatment reaction zone 6 for reaction to obtain alkali metal treatment reaction effluent 7; alkali metal treatment reaction effluent 7 enters primary solid-liquid separation device 8 for primary separation to obtain solid phase product 9 and first liquid phase stream 10, first liquid phase stream 10 enters purification treatment device 11, and is mixed with acidic additive 14 for reaction to obtain gas phase products 12 such as hydrogen and hydrogen sulfide and solid-liquid two-phase mixture 13; solid-liquid two-phase mixture 13 enters secondary solid-liquid separation device 15 for separation to obtain second liquid phase stream 16 and solid phase products 17 such as alkali metal salt, and second liquid phase stream 16 enters hydrocracking reaction zone 18 for cracking reaction, and obtains gas 19 and light naphtha 20, heavy naphtha 21 and tail oil 22 through gas-liquid separation and fractionation, wherein heavy naphtha 21 enters aromatic extraction device.

[0034] like Figure 2 As shown, catalytic diesel 1 enters fractionation tower 2 for separation to obtain light distillate 3 and heavy distillate 4; heavy distillate 4 is mixed with hydrogen 5 and enters hydrofining reaction zone 6 for reaction to obtain hydrofining effluent 7; hydrofining effluent 7 and light distillate 3 are mixed with alkali metal 8 and enter alkali metal treatment reaction zone 9 for reaction to obtain alkali metal treatment reaction effluent 10; alkali metal treatment reaction effluent 10 enters primary solid-liquid separation device 11 for primary separation to obtain solid phase product 12 and first liquid phase feed stream 13, and first liquid phase feed stream 14 is separated into solid phase product 12 and first liquid phase feed stream 15. The stream 13 enters the purification treatment device 14, and is mixed with the acidic additive 17 to react to obtain gas phase products 15 such as hydrogen and hydrogen sulfide and a solid-liquid two-phase mixture 16; the solid-liquid two-phase mixture 16 enters the secondary solid-liquid separation device 18 to obtain a second liquid phase stream 19 and solid phase products 20 such as alkali metal salts after separation. The second liquid phase stream 19 enters the hydrocracking reaction zone 21 for cracking reaction, and after gas-liquid separation and fractionation, a gas 22 and light naphtha 23, heavy naphtha 24 and tail oil 25 are obtained, wherein the heavy naphtha 24 is removed from the aromatic extraction device.

[0035] The following examples will further illustrate the method provided by the present invention, but are not intended to limit the present invention.

[0036] The catalyst used in the hydrorefining reaction zone in the embodiments of the present invention and the comparative examples is the FF-66 hydrorefining catalyst produced by Sinopec Catalyst Co., Ltd.; the catalyst used in the hydrocracking reaction zone is the FC-70A hydrocracking catalyst produced by Sinopec Catalyst Co., Ltd.; the extraction solvent used in the aromatics extraction device is N-methylpyrrolidone, the mass ratio of N-methylpyrrolidone to heavy naphtha is 5:1, the extraction temperature is 100°C, and the extraction pressure is 0.5MPa.

[0037] In the embodiment of the present invention, the alkali metal used in the alkali metal treatment reaction zone is sodium; the auxiliary agent used in the separation treatment process is a mixture of acetic acid and phosphoric acid, and the mass ratio of acetic acid to phosphoric acid is 2:1.

[0038] Example 1 This embodiment adopts Figure 1 The process flow is shown.

[0039] (1) Catalytic diesel and hydrogen are mixed and enter the hydrotreating reaction zone, where they are contacted with the hydrotreating catalyst to react and obtain a hydrotreating reaction effluent; (2) In the presence of hydrogen, the effluent from the hydrotreating reaction in step (1) is mixed with an alkali metal and enters an alkali metal treatment reaction zone for reaction; (3) The alkali metal treatment effluent obtained in step (2) is subjected to separation treatment to obtain an alkali metal treatment liquid phase product; the separation treatment process is as follows: the alkali metal treatment effluent is subjected to a solid-liquid separation to obtain a first liquid phase stream; the first liquid phase stream is mixed with an auxiliary agent, and the mixed material is subjected to a second solid-liquid separation to obtain a second liquid phase stream; (4) The alkali metal treated liquid product in step (3) enters the hydrocracking reaction zone, and the reaction effluent is subjected to gas-liquid separation and fractionation in sequence to obtain gas and light naphtha, heavy naphtha and tail oil. The heavy naphtha enters the aromatics extraction unit for treatment to obtain BTX.

[0040] Example 2 The process flow of this embodiment is the same as that of embodiment 1.

[0041] Example 3 The process flow of this embodiment is the same as that of embodiment 1.

[0042] Example 4 This embodiment adopts Figure 2 The process flow is shown.

[0043] (1) Light distillate oil and heavy distillate oil are obtained by cutting catalytic diesel, and the heavy distillate oil is mixed with hydrogen and enters the hydrotreating reaction zone to contact with the hydrotreating catalyst for reaction to obtain a hydrotreating reaction effluent; (2) In the presence of hydrogen, the hydrotreating reaction effluent in step (2) and the light distillate oil in step (1) are mixed with an alkali metal and enter an alkali metal treatment reaction zone for reaction; (3) The alkali metal treatment effluent obtained in step (3) is subjected to separation treatment to obtain an alkali metal treatment liquid phase product; the separation treatment process is as follows: the alkali metal treatment effluent is subjected to a solid-liquid separation to obtain a first liquid phase stream; the first liquid phase stream is mixed with an auxiliary agent, and the mixed material is subjected to a second solid-liquid separation to obtain a second liquid phase stream; (4) The alkali metal treated liquid product in step (4) enters the hydrocracking reaction zone, and the reaction effluent is subjected to gas-liquid separation and fractionation in sequence to obtain gas and light naphtha, heavy naphtha and tail oil. The heavy naphtha enters the aromatics extraction unit for treatment to obtain BTX.

[0044] Example 5 The process flow of this embodiment is the same as that of embodiment 4.

[0045] The properties of the catalytic diesel feedstock are shown in Table 1; the operating conditions of the hydrotreating, alkali metal treatment and hydrocracking reaction zones are shown in Table 2; the operating conditions of the separation treatment are shown in Table 3; and the product properties are shown in Table 4.

[0046] Table 1 Catalytic diesel feedstock properties

[0047] Table 2 Operating conditions of hydrotreating, alkali metal treatment and hydrocracking reaction zones

[0048] Table 3 Separation treatment operating conditions

[0049] Table 4 Product properties

[0050] Comparative Example 1 The catalytic diesel first enters the hydrofining reaction zone for hydrogenation saturation reaction, and the effluent of the hydrofining reaction zone enters the hydrocracking reaction zone for hydrocracking reaction. The reaction effluent is sequentially separated by gas-liquid separation and fractionation to obtain gas and light naphtha, heavy naphtha and tail oil. The heavy naphtha enters the aromatics extraction unit for treatment to obtain BTX. The operating conditions and reaction results are shown in Table 5.

[0051] Table 5 Operating conditions and reaction results of Comparative Example 1

[0052] It can be seen from the test results of the embodiments and comparative examples that the processing method of the catalytic diesel of the present invention can effectively increase the heavy naphtha yield and the light aromatics content, and improve the BTX yield.

Claims

1. A method for processing catalytic diesel, characterized in that: The method comprises the following steps: (1) Catalytic diesel and hydrogen are mixed and enter the hydrotreating reaction zone, where they are contacted with the hydrotreating catalyst to react and obtain a hydrotreating reaction effluent; (2) In the presence of hydrogen, the effluent from the hydrotreating reaction in step (1) is mixed with an alkali metal and enters an alkali metal treatment reaction zone for reaction; (3) separating and treating the alkali metal treatment effluent obtained in step (2) to obtain an alkali metal treatment liquid phase product; (4) The alkali metal treated liquid product in step (3) enters the hydrocracking reaction zone, and the reaction effluent is subjected to gas-liquid separation and fractionation in sequence to obtain gas and light naphtha, heavy naphtha and tail oil. The heavy naphtha enters the aromatics extraction unit to obtain BTX.

2. The method according to claim 1, characterized in that: The catalytic diesel in step (1) is the 160°C-370°C fraction in the catalytic cracking full fraction product, preferably the 220°C-340°C fraction; the catalytic diesel has a density of 0.90 g / cm -3 -0.99g / cm -3 , the sulfur content is 200 μg / g-8000 μg / g, the nitrogen content is 100 μg / g-2000 μg / g, and the aromatic hydrocarbon content is 50 wt%-90 wt%, preferably 60 wt%-85 wt%.

3. The method according to claim 1, characterized in that: In step (1), the catalytic diesel is cut to obtain light distillate oil and heavy distillate oil, and the heavy distillate oil is mixed with hydrogen and enters the hydrotreating reaction zone; the cutting point is 250°C-300°C, preferably 260°C-275°C.

4. The method according to claim 3, characterized in that: The content of monocyclic aromatic hydrocarbons in the heavy distillate oil is 0.1 wt.%-10 wt.%, preferably 0.2 wt.%-5 wt.%, and more preferably 0.5 wt.%-2 wt.%.

5. The method according to claim 1 or 3, characterized in that: In step (1), the sulfur content of the hydrotreating effluent is controlled to be 50 μg / g-1000 μg / g, preferably 150 μg / g-850 μg / g, and more preferably 200 μg / g-500 μg / g; the nitrogen content is controlled to be 50 μg / g-800 μg / g, preferably 100 μg / g-500 μg / g, and more preferably 120 μg / g-200 μg / g.

6. The method according to claim 1 or 3, characterized in that: Compared with the conventional hydrofining reaction zone process conditions, the reaction pressure in the hydrofining reaction zone in step (1) is 0.5MPa-5.0MPa lower, the average reaction temperature is 10℃-40℃ lower, and the volume space velocity is 0.5-3.0h higher. -1 Preferably, the reaction pressure is 1.0MPa-2.5MPa lower, the average reaction temperature is 15℃-25℃ lower, and the volume space velocity is 0.8-2.0 h higher. -1 .

7. The method according to claim 6, characterized in that: The process conditions of the conventional hydrofining reaction zone are: reaction pressure of 3.0 MPa-15.0 MPa, average reaction temperature of 300°C-450°C, volume space velocity of 0.5-10.0 h -1 The preferred reaction pressure is 5.0 MPa-12.0 MPa, the average reaction temperature is 350°C-400°C, and the volume space velocity is 1.0-5.0 h -1 .

8. The method according to claim 3, characterized in that: In the method of the present invention, step (2) also introduces light distillate oil obtained by cutting catalytic diesel, and the light distillate oil is mixed with the hydrotreating reaction effluent in step (1) and alkali metal and enters the alkali metal treatment reaction zone for reaction.

9. The method according to claim 1, characterized in that: The alkali metal in step (2) is at least one of lithium, sodium, potassium, rubidium, cesium and francium, preferably lithium, sodium or potassium, and more preferably sodium; the mass ratio of the alkali metal to the hydrotreating reaction effluent is (0.1-5.0):100, preferably (0.5-2.5):

100.

10. The method according to claim 1, characterized in that: The reactor used in the alkali metal treatment reaction zone in step (2) is one or more of a kettle reactor, a pipeline reactor and a tower reactor, preferably a kettle reactor.

11. The method according to claim 1, characterized in that: The process conditions of the alkali metal treatment reaction zone in step (2) are: reaction temperature 200°C-380°C, hydrogen partial pressure 0.5MPa-15.0MPa, reaction time or residence time 0.1h-2.0h, hydrogen to oil volume ratio 100Nm 3 / m 3 -1000Nm 3 / m 3 Preferably, the reaction temperature is 280°C-340°C, the hydrogen partial pressure is 2.0MPa-8.0MPa, the reaction time or residence time is 0.5h-1.0h, and the hydrogen-to-oil volume ratio is 350Nm 3 / m 3 -750Nm 3 / m 3 .

12. The method according to claim 1, characterized in that: The catalyst used in the hydrocracking reaction zone in step (4) comprises a carrier and a metal active component; the carrier comprises at least one of alumina, amorphous silica-alumina and a molecular sieve, and the molecular sieve is a Y-type and / or a β-type molecular sieve; the metal active component is a metal of Group VI, Group VII or Group VIII, a metal oxide or a metal sulfide, preferably one or more of iron, chromium, molybdenum, tungsten, cobalt or nickel; based on the weight of the catalyst, the content of the metal active component in terms of oxide is 10-35wt%, and the content of the carrier in terms of mass is 60-85wt%.

13. The method according to claim 1, characterized in that: The process conditions of the hydrocracking reaction zone in step (4) are: reaction pressure of 3.0 MPa-18.0 MPa, average reaction temperature of 320°C-450°C, volume space velocity of 1.0-8.0 h -1 , hydrogen to oil volume ratio is 300Nm 3 / m 3 -1500Nm 3 / m 3 The preferred reaction pressure is 5.0 MPa-15.0 MPa, the average reaction temperature is 350°C-420°C, and the volume space velocity is 1.0-3.0 h -1 , hydrogen to oil volume ratio is 400Nm 3 / m 3 -1200Nm 3 / m 3 .

14. The method according to claim 1, characterized in that: The aromatics extraction in step (4) is a solvent liquid-liquid extraction method and / or an extractive distillation method.

15. The method according to claim 1, characterized in that: The aromatics extraction adopts a solvent liquid-liquid extraction method; the operating conditions are: the mass ratio of solvent to heavy naphtha is 1-10:1, the extraction temperature is 20-250°C, and the extraction pressure is 0.1-3MPa. Preferably, the mass ratio of solvent to heavy naphtha is 3-6:1, the extraction temperature is 80-150°C, and the extraction pressure is 0.5-1.0MPa.

16. The method according to claim 1, characterized in that: The tail oil in step (4) is circulated to the hydrotreating reaction zone.

Citation Information

Patent Citations

  • Hydrocracking method for producing low-sulfur heavy naphtha

    CN116004283A

  • Very Low Sulfur Heavy Crude oil and Porcess for the Production thereof

    US20090134059A1

  • Regeneration of alkali metal reagent

    US20110147274A1

  • Production of lubricating oils including hydrofining an extract

    US3702817A

  • Systems and methods of producing a crude product

    WO2005061664A2