Super junction MOS device with improved avalanche tolerance and preparation method and chip
By setting high doping concentration doping regions and dielectric layers in superjunction MOS devices, uniformizing the electric field and current distribution, the problems of poor reverse recovery performance and insufficient breakdown voltage in the prior art are solved, and the device is improved Avalanche tolerance and reverse recovery performance.
Patent Information
- Application Number
- CN202411339007.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-25
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-09-25
AI Technical Summary
The existing superjunction MOS devices have large reverse recovery peak current and poor reverse recovery performance when reverse conduction, which limits their application in higher frequency systems and insufficient breakdown voltage and avalanche withstand capacity.
By providing a gate dielectric layer and a gate polysilicon layer on the third N column, and a first N column with a high doping concentration is provided between the third N column and the second P column, the third N column and the third N column and the third N column are provided. A second N column with a high doping concentration is provided between the P columns, a second P column with a high doping concentration is provided between the first P column and the first N column, and between the second N column and the fourth P column. A third P column with a high doping concentration is provided so that the electric field in the device is more uniform and the current distribution is evenly distributed, thereby improving the breakdown voltage and avalanche withstand capacity.
It significantly improves the breakdown voltage and avalanche withstand capacity of the device, improves the reverse recovery performance, reduces the reverse recovery time and reverse recovery charge, and is suitable for higher frequency systems.
Smart Images

Figure CN118866943B_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of power devices, and in particular, relates to a super junction MOS device with improved avalanche tolerance, a preparation method, and a chip. Background Art
[0002] Superjunction MOS devices have broken the "silicon limit" relationship between the on-voltage and resistance of conventional power MOSFETs, and have lower switching losses. They have been widely used in automotive electronics, consumer electronics, power supplies, aerospace and other fields. In the current research trend, the relationship between the specific on-resistance and breakdown voltage of superjunction MOS devices is constantly being optimized, and it is usually hoped that a higher breakdown voltage can be achieved at the same specific on-resistance. Summary of the invention
[0003] In order to solve the above technical problems, the embodiments of the present application provide a super junction MOS device with improved avalanche resistance, a preparation method, and a chip, aiming to improve the breakdown voltage and avalanche resistance of current super junction MOS devices.
[0004] A first aspect of an embodiment of the present application provides a super junction MOS device with improved avalanche tolerance, comprising:
[0005] N-type substrate;
[0006] A first N column, a second N column and a third N column are arranged on the N-type substrate, and the third N column is arranged between the first N column and the second N column; wherein the doping concentration of the first N column and the second N column is greater than the doping concentration of the third N column;
[0007] A first P column, a second P column, a third P column and a fourth P column are arranged on the N-type substrate, and the second P column is arranged between the first P column and the first N column, and the third P column is arranged between the second N column and the fourth P column; the doping concentration of the second P column is greater than the doping concentration of the first P column, and the doping concentration of the third P column is greater than the doping concentration of the fourth P column;
[0008] A first P-type base region is formed on the first P column, the second P column and the first N column;
[0009] A second P-type base region is formed on the third P column, the fourth P column and the second N column;
[0010] a gate dielectric layer and a gate polysilicon layer, wherein the gate dielectric layer is formed on the third N column and is located between the first P-type base region and the second P-type base region, wherein the gate polysilicon layer is wrapped by the gate dielectric layer;
[0011] A first P-type source region and a first N-type source region, formed on the first P-type base region;
[0012] A second P-type source region and a second N-type source region, formed on the second P-type base region;
[0013] a source layer, contacting the first P-type source region, the first N-type source region, the second P-type source region, and the second N-type source region;
[0014] a gate layer, contacting the gate polysilicon layer;
[0015] The drain layer is formed on the back side of the N-type substrate.
[0016] In some embodiments, N-type doping regions are disposed in the first P column and the fourth P column.
[0017] In some embodiments, the super junction MOS device further comprises:
[0018] The first transverse P column is disposed between the first P-type base region and the first P column and the second P column.
[0019] In some embodiments, the super junction MOS device further comprises:
[0020] The second transverse P column is disposed between the second P-type base region and the third P column and the fourth P column.
[0021] In some embodiments, the width of the first P-pillar is greater than the width of the second P-pillar; and / or
[0022] The width of the fourth P-pillar is greater than the width of the third P-pillar.
[0023] In some embodiments, a width of the third N pillar is greater than widths of the first N pillar and the second N pillar.
[0024] In some embodiments, the width of the third N column is the same as the width of the gate dielectric layer.
[0025] In some embodiments, the width of the second P column is the same as the width of the first N column; and / or,
[0026] The width of the third P column is the same as the width of the second N column.
[0027] A second aspect of the present application also provides a method for preparing a super junction MOS device with improved avalanche tolerance, the method comprising:
[0028] Epitaxially generating an N-type drift region on the front side of the N-type substrate, and after etching a trench in a partial area of the N-type drift region, filling it with P-type material to form a third N column, a first P column, and a fourth P column;
[0029] Etching grooves multiple times on partial areas of the first P column and the fourth P column, and filling P-type material and N-type material to form a first N column, a second N column, a second P column and a third P column; wherein the third N column is arranged between the first N column and the second N column, the second P column is arranged between the first P column and the first N column, the third P column is arranged between the second N column and the fourth P column, and the doping concentrations of the first N column and the second N column are greater than the doping concentration of the third N column; the doping concentration of the second P column is greater than the doping concentration of the first P column, and the doping concentration of the third P column is greater than the doping concentration of the fourth P column;
[0030] Continue to epitaxially grow the N-type epitaxial material and perform an ion implantation process to form a first P-type base region on the first P column, the second P column and the first N column, and to form a second P-type base region on the third P column, the fourth P column and the second N column;
[0031] Sequentially implanting N-type doping ions and P-type doping ions into the first P-type base region and the second P-type base region to form a first P-type source region and a first N-type source region on the first P-type base region, and forming a second P-type source region and a second N-type source region on the second P-type base region;
[0032] A trench is formed by etching between the first P-type base region and the second P-type base region, and a gate dielectric layer and a gate polysilicon layer are formed, wherein the gate dielectric layer is formed on the third N column and is located between the first P-type base region and the second P-type base region; wherein the gate polysilicon layer is wrapped by the gate dielectric layer;
[0033] A source layer in contact with the first P-type source region, the first N-type source region, the second P-type source region and the second N-type source region, a gate layer in contact with the gate polysilicon layer, and a drain layer in contact with the back side of the N-type substrate are formed.
[0034] A third aspect of the embodiments of the present application further provides a chip, comprising a super junction MOS device as described in any of the above embodiments.
[0035] The beneficial effects of the embodiments of the present application are as follows: by setting a gate dielectric layer and a gate polysilicon layer on the third N column, and setting a first N column with a higher doping concentration between the third N column and the second P column, setting a second N column with a higher doping concentration between the third N column and the third P column, setting a second P column with a higher doping concentration between the first P column and the first N column, and setting a third P column with a higher doping concentration between the second N column and the fourth P column, the electric field in the device is more uniform, and when the device breaks down, the current distribution in the device can be more uniform, thereby improving the breakdown voltage and avalanche tolerance of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1a A schematic diagram of the structure of a super junction MOS device provided in an embodiment of the present application;
[0037] Figure 1b A second structural diagram of a super junction MOS device provided in an embodiment of the present application;
[0038] Figure 1c A third structural diagram of a super junction MOS device provided in an embodiment of the present application;
[0039] Figure 1d Schematic diagram of the structure of the super junction MOS device provided in the embodiment of the present application Figure 4 ;
[0040] Figure 2a Graph showing simulation results of breakdown voltages of conventional super junction MOSFET and super junction MOS device in the embodiment of the present application;
[0041] Figure 2b Graph showing simulation results of output characteristic curves of a conventional super junction MOSFET and a super junction MOS device in an embodiment of the present application;
[0042] Figure 2c Graph showing simulation results of transfer characteristic curves of a conventional super junction MOSFET and a super junction MOS device in an embodiment of the present application;
[0043] Figure 2d Graph showing simulation results of reverse recovery characteristic curves of a conventional super junction MOSFET and a super junction MOS device in an embodiment of the present application;
[0044] Figure 3a This is the current density simulation result diagram of the traditional super junction MOSFET device;
[0045] Figure 3b In the embodiment of this application Figure 1a The current density simulation result diagram of the super junction MOS device shown;
[0046] Figure 4 Graph showing the electric field distribution simulation results of a conventional planar super junction MOSFET and a super junction MOS device in an embodiment of the present application;
[0047] Figure 5a Schematic diagram of the relationship between the breakdown voltage of the super junction MOS device and the doping concentration of the N column in the embodiment of the present application;
[0048] Figure 5b Schematic diagram of the relationship between the output characteristic curve of the super junction MOS device and the doping concentration of the N column in the embodiment of the present application;
[0049] Figure 5cA schematic diagram showing the relationship between the output characteristic curve of the super junction MOS device in the application embodiment and the distance between the N column and the P column;
[0050] Figure 5d A schematic diagram of the relationship between the output characteristic curve of the super junction MOS device in the embodiment of the present application and the concentration of the N-type doping point region;
[0051] Figure 6 A schematic diagram of a process for preparing a super junction MOS device provided in an embodiment of the present application;
[0052] Figure 7 It is a schematic diagram of forming an N-type drift region on the front side of an N-type substrate in an embodiment of the present application;
[0053] Figure 8 It is a schematic diagram of forming a third N column, a first P column, and a fourth P column on the front surface of an N-type substrate in an embodiment of the present application;
[0054] Figure 9a is a schematic diagram of forming a first N column, a second N column, a second P column, and a third P column on the front side of an N-type substrate in an embodiment of the present application;
[0055] Figure 9b is a schematic diagram of forming an N-type doping point region in the first P column and the fourth P column in an embodiment of the present application;
[0056] Fig.10 is a schematic diagram of forming a first P-type base region, a second P-type base region, a first P-type source region, a second P-type source region, a first N-type source region, and a second N-type source region in an embodiment of the present application;
[0057] Fig.11 It is a schematic diagram of forming a gate dielectric layer and a gate polysilicon layer in an embodiment of the present application. DETAILED DESCRIPTION
[0058] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0059] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.
[0060] It should be understood that the orientation or position relationship indicated by terms such as "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0061] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, "plurality" means one or more, unless otherwise clearly and specifically defined.
[0062] When the superjunction MOS device is reverse-conducting, minority carrier charges are injected by the body diode, resulting in a large reverse recovery peak current and poor reverse recovery performance, which limits its application in higher frequency systems.
[0063] In order to solve the above technical problems, the present application embodiment provides a super junction MOS device with improved avalanche tolerance, see Figure 1a As shown, the super junction MOS device in this embodiment includes: an N-type substrate 110, a first N-column 121, a second N-column 122, a third N-column 120, a first P-column 131, a second P-column 133, a third P-column 134, a fourth P-column 132, a first P-type base region 141, a second P-type base region 142, a gate dielectric layer 171, a gate polysilicon layer 172, a first P-type source region 151, a first N-type source region 161, a second P-type source region 152, a second N-type source region 162, a source layer 173, a gate layer 174 and a drain layer 180.
[0064] The first N column 121, the second N column 122 and the third N column 120 are disposed on the N-type substrate 110, and the third N column 120 is disposed between the first N column 121 and the second N column 122; wherein the doping concentration of the first N column 121 and the second N column 122 is greater than the doping concentration of the third N column 120. The first P column 131, the second P column 133, the third P column 134 and the fourth P column 132 are disposed on the N-type substrate 110, and the second P column 133 is disposed between the first P column 131 and the first N column 121, and the third P column 134 is disposed between the second N column 122 and the fourth P column 132; the doping concentration of the second P column 133 is greater than the doping concentration of the first P column 131, and the doping concentration of the third P column 134 is greater than the doping concentration of the fourth P column 132. The first P-type base region 141 is formed on the first P-pillar 131, the second P-pillar 133 and the first N-pillar 121; the second P-type base region 142 is formed on the third P-pillar 134, the fourth P-pillar 132 and the second N-pillar 122. The gate dielectric layer 171 is formed on the third N-pillar 120 and is located between the first P-type base region 141 and the second P-type base region 142, wherein the gate polysilicon layer 172 is wrapped by the gate dielectric layer 171. The first P-type source region 151 and the first N-type source region 161 are formed on the first P-type base region 141; the second P-type source region 152 and the second N-type source region 162 are formed on the second P-type base region 142; the source layer 173 is in contact with the first P-type source region 151, the first N-type source region 161, the second P-type source region 152, and the second N-type source region 162; the gate layer 174 is in contact with the gate polysilicon layer 172; and the drain layer 180 is formed on the back side of the N-type substrate 110.
[0065] In this embodiment, a gate dielectric layer 171 and a gate polysilicon layer 172 are arranged on the third N column 120, and a first N column 121 with a higher doping concentration is arranged between the third N column 120 and the second P column 133, a second N column 122 with a higher doping concentration is arranged between the third N column 120 and the third P column 134, a second P column 133 with a higher doping concentration is arranged between the first P column 131 and the first N column 121, and a third P column 134 with a higher doping concentration is arranged between the second N column 122 and the fourth P column 132, so that the electric field in the device is more uniform, and when the device breaks down, the current distribution in the device can be more uniform, thereby improving the breakdown voltage and avalanche tolerance of the device.
[0066] Combination Figure 1b As shown, in some embodiments, N-type doping dot regions (N-dot) may be disposed in the first P column 131 and the fourth P column 132 .
[0067] In this embodiment, a first N-type doping point region 123 is provided in the first P column 131, and a second N-type doping point region 124 is provided in the fourth P column 132. This design can change the resistance of the first P column 131 and the fourth P column 132, thereby affecting the extraction speed of holes in the device, improving the softness of the reverse recovery of the device, reducing the reverse recovery time and reverse recovery charge of the device, thereby improving the reverse recovery performance of the device. In addition, this design makes the electric field in the device more uniform. When the device breaks down, the current distribution in the device can be more uniform, thereby improving the breakdown voltage of the device.
[0068] In the embodiment of the present application, the first N-type doping point region 123 may be located in the first P column 131 at one end close to the first P-type base region 141, and may not contact the first P-type base region 141. The second N-type doping point region 124 may be located in the fourth P column 132 at one end close to the second P-type base region 142, and may not contact the second P-type base region 142.
[0069] The following Table 1 compares the conventional super junction MOS device and the embodiment of the present application. Figure 1a The super junction MOS device (excluding N-Dot) shown in the embodiment of the present application Figure 1b The static characteristics of the three structures of super junction MOS devices (including N-Dot) and their reverse recovery related parameters are shown.
[0070] Among them, the V (BR)DSS is the drain-source breakdown voltage, R DS(ON) is the on-resistance, I D is the source-drain saturation current, V th is the threshold voltage, t rr is the body diode reverse recovery time, Q rr is the body diode reverse recovery charge, I RRM Reverse recovery current, V GS (Right now, V gs ) is the turn-on voltage, I DS (Right now, I ds ) is the drain current, VDD is the power supply voltage, and di / dt is the current.
[0071] Table 1:
[0072]
[0073] In addition, combined Figure 2a , Figure 2b , Figure 2c as well as Figure 2d As shown in Figure 2, when the reverse peak current of the superjunction MOS device is lower and the reverse recovery time is smaller, its reverse recovery charge is lower and the reverse recovery characteristic is better. Figure 2a , Figure 2b , Figure 2c , Figure 2d as well as Figure 4 Curve 1 in the figure is a simulation result diagram of a conventional super junction MOSFET device, and curve 2 is a simulation result diagram of a conventional super junction MOSFET device provided in the embodiment of the present application. Figure 1a The simulation result diagram of the super junction MOS device (excluding N-Dot) shown in FIG. 3 is provided in the embodiment of the present application. Figure 1b The simulation results of the super junction MOS device (including N-Dot) are shown. Figure 1a The super junction MOS device shown does not include N-Dot (the first N-type doping dot region 123 and the second N-type doping dot region 124). Figures 2a to 5d In the figure, Id is the drain current, Vds is the voltage between the drain and the source, and Ids is the current between the drain and the source.
[0074] Combined with Table 1, Figure 2a , Figure 2b , Figure 2c , Figure 2d , Figure 3a as well as Figure 3b As shown, the on-resistance, saturation current and threshold voltage of the three devices are basically the same. The present application sets a gate dielectric layer 171 and a gate polysilicon layer 172 on the third N column 120, sets a first N column 121 with a higher doping concentration between the third N column 120 and the second P column 133, sets a second N column 122 with a higher doping concentration between the third N column 120 and the third P column 134, sets a second P column 133 with a higher doping concentration between the first P column 131 and the first N column 121, and sets a third P column 134 with a higher doping concentration between the second N column 122 and the fourth P column 132, so that when the device breaks down, the current distribution is more uniform, the breakdown voltage of the device is increased by improving the current distribution, and the avalanche tolerance of the device is improved. Among them, Figure 3a as well as Figure 3b The X in the figure represents the depth coordinate of the device, and the Y represents the width coordinate of the device.
[0075] Combination Figure 4It can be seen that by setting the first N-type doping point area 123 in the first P column 131 and the second N-type doping point area 124 in the fourth P column 132, the resistance of the first P column 131 and the fourth P column 132 is changed, thereby affecting the extraction speed of holes in the device, improving the softness of the reverse recovery of the device, and making the electric field in the device more uniform. When the device breaks down, the current distribution in the device can be more uniform, thereby improving the breakdown voltage of the device. Figure 4 Curve 1 in the figure is a simulation result diagram of a conventional super junction MOSFET device, and curve 2 is a simulation result diagram of a conventional super junction MOSFET device provided in the embodiment of the present application. Figure 1a The simulation result diagram of the super junction MOS device (excluding N-Dot) shown in FIG. 2 is provided in the embodiment of the present application. Figure 1b The simulation results of the super junction MOS device (including N-Dot) shown in the figure. Figure 4 The abscissa X in represents the depth coordinate of the device.
[0076] Keep Figure 1a The overall charge of the device structure shown is the same as that of the conventional superjunction MOS device structure. Figure 5a As shown, the doping concentration of the second P column 133, the first N column 121, the third P column 134 and the second N column 122 is increased. When the concentration is less than 1.8e16 cm -3 When the concentration exceeds 1.8e16 cm -3 When the breakdown voltage drops significantly. Figure 5b As shown, when the concentration is greater than 1.2e16 cm -3 When the forward resistance increases significantly.
[0077] Combination Figure 5c As shown, keep Figure 1a When the overall charge of the device structure shown is the same as that of the traditional super junction MOS device structure, the distance between the third N column 120 and the first P column 131 (i.e., the sum of the widths of the second P column 133 and the first N column 121), and the distance between the third N column 120 and the fourth P column 132 (i.e., the sum of the widths of the third P column 134 and the second N column 122) are changed. When the distance between the third N column 120 and the first P column 131 and the distance between the third N column 120 and the fourth P column 132 are larger, the breakdown voltage of the device is lower, and the distance between the third N column 120 and the first P column 131 and the distance between the third N column 120 and the fourth P column 132 have substantially no effect on the output characteristic curve of the device.
[0078] In some embodiments, the doping concentrations of the first N column 121 and the second N column 122 may be the same.
[0079] In some embodiments, the doping concentration of the first N column 121 and the second N column 122 may be 7.2e15 cm -3 .
[0080] In some embodiments, the doping concentrations of the second P column 133 and the third P column 134 may be the same.
[0081] In some embodiments, the doping concentrations of the second P column 133 and the third P column 134 are the same as the doping concentrations of the first N column 121 and the second N column 122 .
[0082] In some embodiments, the doping concentration of the second P column 133 and the third P column 134 may be 7.2e15 cm -3 .
[0083] In some embodiments, the doping concentration of the third N column 120 may be 5.4e15 cm -3 .
[0084] In some embodiments, the doping concentration of the first P column 131 and the fourth P column 132 may be 5.4e15 cm -3 .
[0085] In some embodiments, the doping concentration of the first N-type doping region 123 and the second N-type doping region 124 may be 9e15 cm -3 .
[0086] In some embodiments, the distance between the first N-type doping point region 123 and the first N-type source region 161 is 5 um, and the distance between the second N-type doping point region 124 and the second N-type source region 162 is 5 um.
[0087] In some embodiments, in combination Figure 1c As shown, the super junction MOS device further includes a first lateral P column 213 , which is disposed between the first P-type base region 141 and the first P column 131 , and between the first P-type base region 141 and the second P column 133 .
[0088] In this embodiment, one end of the first lateral P column 213 contacts one end of the second P column 133, and the other end of the second P column 133 contacts the N-type substrate 110. This design can adjust the charge balance above the first N column 121 (close to the source), while reducing some hole injection and improving the reverse recovery characteristics of the device.
[0089] In some embodiments, in combination Figure 1c As shown, the super junction MOS device further includes a second lateral P column 214 , which is disposed between the second P-type base region 142 and the third P column 134 , and between the second P-type base region 142 and the fourth P column 132 .
[0090] In this embodiment, one end of the second lateral P column 214 contacts one end of the third P column 134, and the other end of the third P column 134 contacts the N-type substrate 110. This design can adjust the charge balance above the second N column 122 (close to the source), while reducing some hole injection and improving the reverse recovery characteristics of the device.
[0091] In some embodiments, the width of the first P-pillar 131 is greater than the width of the second P-pillar 133 .
[0092] In some embodiments, the width of the fourth P-pillar 132 is greater than the width of the third P-pillar 134 .
[0093] In some embodiments, in combination Figure 1c As shown, a first N-type doping region 211 is disposed between the first lateral P column 213 and the gate dielectric layer 171 , and a second N-type doping region 212 is disposed between the second lateral P column 214 and the gate dielectric layer 171 .
[0094] In this embodiment, by providing the first N-type doping region 211 and the second N-type doping region 212 , the charges in the contact region between the first N-type doping region 211 and the second N-type doping region 212 can be balanced, and the minority carrier lifetime can be reduced, thereby improving the reverse recovery charge.
[0095] In some embodiments, the doping concentration of the first N-type doping region 211 is greater than the doping concentration of the first N column 121 , and the doping concentration of the second N-type doping region 212 is greater than the doping concentration of the second N column 122 , thereby reducing the minority carrier lifetime and improving the reverse recovery charge of the device.
[0096] In some embodiments, the width of the third N column 120 is greater than the widths of the first N column 121 and the second N column 122 .
[0097] In some embodiments, the width of the third N column 120 is the same as the width of the gate dielectric layer 171 .
[0098] In some embodiments, the width of the second P column 133 is the same as the width of the first N column 121 .
[0099] In some embodiments, the width of the third P column 134 is the same as the width of the second N column 122 .
[0100] In this embodiment, the doping concentrations of the second P column 133 and the first N column 121 between the first P column 131 and the third N column 120 are relatively high, and the doping concentrations of the second N column 122 and the third P column 134 between the third N column 120 and the fourth P column 132 are relatively high, so that the first P column 131 and the third N column 120 are highly doped, and the third N column 120 and the fourth P column 132 are highly doped. In addition, the width of the second P column 133 is the same as that of the first N column 121, and the width of the third P column 134 is the same as that of the second N column 122. This design can make the current distribution in the device more uniform when the device breaks down, thereby improving the breakdown voltage of the device.
[0101] In some embodiments, the concentration of N-type dopant ions in the first N column 121 and the second N column 122 is at least 100 times the doping concentration of N-type dopant ions in the third N column 120 .
[0102] In some embodiments, the concentration of the P-type dopant ions in the second P column 133 is at least 100 times the doping concentration of the P-type dopant ions in the first P column 131 .
[0103] In some embodiments, the concentration of the P-type dopant ions in the third P column 134 is at least 100 times the doping concentration of the P-type dopant ions in the fourth P column 132 .
[0104] In some embodiments, since the thickness of the N-type drift region generated by the front epitaxial growth of the N-type substrate 110 is relatively large, during ion implantation, a higher concentration of N-type doped ions will be injected into the side of the N-type drift region away from the N-type substrate 110. Therefore, in order to balance the electric field in the N-type drift region, the doping concentration of the N-type doped ions in the first N column 121 and the second N column 122 gradually increases in the direction from the N-type substrate 110 to the P-type base region. Similarly, the concentration of the P-type doped ions in the second P column 133 and the third P column 134 gradually increases in the direction from the N-type substrate 110 to the P-type base region.
[0105] In some embodiments, in combination Figure 1d As shown, a plurality of first N-type doping point regions 123 are provided in the first P column 131, a plurality of second N-type doping point regions 124 are provided in the fourth P column 132, the plurality of first N-type doping point regions 123 are arranged in parallel and spaced apart, and the closer to the second P column 133, the smaller the spacing between adjacent first N-type doping point regions 123; the plurality of second N-type doping point regions 124 are arranged in parallel and spaced apart, and the closer to the third P column 134, the smaller the spacing between adjacent second N-type doping point regions 124.
[0106] In this embodiment, the current distribution between the N-type substrate 110 and the first P-type base region 141 can be adjusted through multiple first N-type doping point regions 123, and the current distribution between the N-type substrate 110 and the second P-type base region 142 can be adjusted through multiple second N-type doping point regions 124. In this way, the resistance of the first P column 131 and the fourth P column 132 can be adjusted, thereby balancing the extraction speed of holes in the device, improving the softness of the reverse recovery of the device, and making the electric field in the device more uniform. When the device breaks down, the current distribution in the device can be more uniform.
[0107] Combination Figure 5d As shown, the positions of the first N-type doping point region 123 and the second N-type doping point region 124 have little effect on the output characteristics of the device. When the first N-type doping point region 123 and the second N-type doping point region 124 are closer to the source, the breakdown voltage can be improved to a certain extent. When they are closer to the drain, the breakdown voltage will be deteriorated to a certain extent, but the overall impact is small. In addition, the concentrations of the first N-type doping point region 123 and the second N-type doping point region 124 have little effect on the output characteristics of the device. When the doping concentrations of the first N-type doping point region 123 and the second N-type doping point region 124 are greater than 1.2e16 cm -3 The breakdown voltage of the device drops significantly.
[0108] The present application also provides a method for preparing a super junction MOS device with improved avalanche resistance, see Figure 6 As shown, the preparation method in this embodiment includes steps S100 to S600.
[0109] In step S100 , an N-type drift region 120 ′ is epitaxially grown on the front side of the N-type substrate 110 , and a trench is etched in a portion of the N-type drift region 120 ′ and then filled with P-type material to form a third N column 120 , a first P column 131 , and a fourth P column 132 .
[0110] Combination Figure 7 and Figure 8 As shown, the first P column 131 and the fourth P column 132 are respectively located on both sides of the third N column 120. Moreover, the widths of the first P column 131 and the fourth P column 132 are smaller than the width of the third N column 120. The first P column 131, the fourth P column 132 and the third N column 120 are in contact with the N-type substrate 110.
[0111] In step S200 , trenches are etched multiple times in partial regions of the first P column 131 and the fourth P column 132 , and filled with P-type material and N-type material to form the first N column 121 , the second N column 122 , the second P column 133 , and the third P column 134 .
[0112] Combination Figure 9aAs shown, in this embodiment, the third N column 120 is disposed between the first N column 121 and the second N column 122, the second P column 133 is disposed between the first P column 131 and the first N column 121, and the third P column 134 is disposed between the second N column 122 and the fourth P column 132. The doping concentrations of the first N column 121 and the second N column 122 are greater than the doping concentration of the third N column 120. The doping concentration of the second P column 133 is greater than the doping concentration of the first P column 131, and the doping concentration of the third P column 134 is greater than the doping concentration of the fourth P column 132.
[0113] Combination Figure 9b As shown, in one embodiment, in the above step S200, N-type doping point regions may be formed in the first P column 131 and the fourth P column 132 by etching trenches and ion filling.
[0114] In this embodiment, combined with Figure 1b As shown, a first N-type doping point region 123 is provided in the first P column 131, and a second N-type doping point region 124 is provided in the fourth P column 132. This design can change the resistance of the first P column 131 and the fourth P column 132, thereby affecting the extraction speed of holes in the device, improving the softness of the reverse recovery of the device, and making the electric field in the device more uniform. When the device breaks down, the current distribution in the device can be more uniform.
[0115] In some embodiments, in combination Figure 1d As shown, a plurality of first N-type doping point regions 123 may be provided in the first P column 131, a plurality of second N-type doping point regions 124 may be provided in the fourth P column 132, the plurality of first N-type doping point regions 123 are arranged in parallel and spaced apart, the closer to the second P column 133, the smaller the spacing between adjacent first N-type doping point regions 123, the plurality of second N-type doping point regions 124 are arranged in parallel and spaced apart, the closer to the third P column 134, the smaller the spacing between adjacent second N-type doping point regions 124.
[0116] In this embodiment, the current distribution between the N-type substrate 110 and the first P-type base region 141 can be adjusted through multiple first N-type doping point regions 123, and the current distribution between the N-type substrate 110 and the second P-type base region 142 can be adjusted through multiple second N-type doping point regions 124. In this way, the resistance of the first P column 131 and the fourth P column 132 can be adjusted, thereby balancing the extraction speed of holes in the device, improving the softness of the reverse recovery of the device, and making the electric field in the device more uniform. When the device breaks down, the current distribution in the device can be more uniform.
[0117] In step S300 , the N-type epitaxial material is continuously grown and an ion implantation process is performed to form a first P-type base region 141 on the first P column 131 , the second P column 133 , and the first N column 121 , and a second P-type base region 142 on the third P column 134 , the fourth P column 132 , and the second N column 122 .
[0118] In step S400, N-type dopant ions and P-type dopant ions are sequentially implanted into the first P-type base region 141 and the second P-type base region 142 to form a first P-type source region 151 and a first N-type source region 161 on the first P-type base region 141, and a second P-type source region 152 and a second N-type source region 162 on the second P-type base region 142;
[0119] See also Fig.10 As shown, in some embodiments, the thickness of the first P-type base region 141 is greater than the thickness of the first P-type source region 151 and the first N-type source region 161, and the thickness of the first P-type source region 151 is the same as the thickness of the first N-type source region 161. The thickness of the second P-type base region 142 is greater than the thickness of the second P-type source region 152 and the second N-type source region 162, and the thickness of the second P-type source region 152 is the same as the thickness of the second N-type source region 162.
[0120] In some embodiments, the first P-type source region 151 and the first N-type source region 161 have the same width, and the second P-type source region 152 and the second N-type source region 162 have the same width.
[0121] In step S500, a trench is formed by etching between the first P-type base region 141 and the second P-type base region 142, and a gate dielectric layer 171 and a gate polysilicon layer 172 are formed. The gate dielectric layer 171 is formed on the third N column 120 and is located between the first P-type base region 141 and the second P-type base region 142.
[0122] In this embodiment, the gate polysilicon layer 172 is wrapped by the gate dielectric layer 171 .
[0123] See also Fig.11 As shown, in one embodiment, the gate dielectric layer 171 is located between the first N column 121 and the second N column 122, and contacts the first N column 121 and the second N column 122, the depth of the third N column 120 is less than the depth of the first N column 121 and the second N column 122, and the depths of the first N column 121 and the second N column 122 are the same.
[0124] In step S600, a source layer 173 is formed in contact with the first P-type source region 151, the first N-type source region 161, the second P-type source region 152 and the second N-type source region 162, a gate layer 174 is formed in contact with the gate polysilicon layer 172, and a drain layer 180 is formed in contact with the back side of the N-type substrate 110.
[0125] See also Figure 1a and Figure 1b As shown, the gate dielectric layer 171 is in a concave structure, and the gate polysilicon layer 172 is filled in the concave structure of the gate dielectric layer 171 and is in contact with the gate layer 174 .
[0126] In this embodiment, a gate dielectric layer 171 and a gate polysilicon layer 172 are provided on the third N column 120, and a first N column 121 with a higher doping concentration is provided between the third N column 120 and the second P column 133, a second N column 122 with a higher doping concentration is provided between the third N column 120 and the third P column 134, a second P column 133 with a higher doping concentration is provided between the first P column 131 and the first N column 121, and a third P column 134 with a higher doping concentration is provided between the second N column 122 and the fourth P column 132, thereby reducing the reverse peak current of the device, reducing the reverse recovery time and reverse recovery charge of the device, and improving the reverse recovery performance of the device.
[0127] In one embodiment of the present application, Figure 1c As shown, in the above step S300, before generating the first P-type base region and the second P-type base region, the first lateral P column 213 and the second lateral P column 214 may be formed first, so that the first lateral P column 213 is disposed between the first P-type base region 141 and the first P column 131, and between the first P-type base region 141 and the second P column 133, and the second lateral P column 214 is disposed between the second P-type base region 142 and the third P column 134, and between the second P-type base region 142 and the fourth P column 132. In addition, a first N-type doping region 211 is disposed between the first lateral P column 213 and the gate dielectric layer 171, and a second N-type doping region 212 is disposed between the second lateral P column 214 and the gate dielectric layer 171.
[0128] In this embodiment, one end of the first transverse P column 213 contacts one end of the second P column 133, and the other end of the second P column 133 contacts the N-type substrate 110. This design can adjust the charge balance above the first N column 121 (in the direction close to the source), while reducing some hole injection, and improving the reverse recovery characteristics of the device. One end of the second transverse P column 214 contacts one end of the third P column 134, and the other end of the third P column 134 contacts the N-type substrate 110. This design can adjust the charge balance above the second N column 122 (in the direction close to the source), while reducing some hole injection, and improving the reverse recovery characteristics of the device. By providing the first N-type doping region 211 and the second N-type doping region 212, the charges in the contact area between the first N-type doping region 211 and the second N-type doping region 212 can be balanced, and the minority carrier lifetime can be reduced, thereby improving the reverse recovery charge.
[0129] An embodiment of the present application also provides a chip, comprising a super junction MOS device as described in any of the above embodiments.
[0130] In this embodiment, the chip includes a chip substrate, on which one or more super junction MOS devices are arranged. The super junction MOS device can be prepared by the preparation method in any of the above embodiments, or the super junction MOS device in any of the above embodiments can be arranged on the chip substrate.
[0131] In a specific application embodiment, other related semiconductor devices may be integrated on the chip substrate and form an integrated circuit with the super junction MOS device in any of the above embodiments.
[0132] In a specific application embodiment, the chip may be a switch chip or a driver chip.
[0133] The beneficial effects of the embodiments of the present application are as follows: by setting a gate dielectric layer 171 and a gate polysilicon layer 172 on the third N column 120, and setting a first N column 121 with a higher doping concentration between the third N column 120 and the second P column 133, setting a second N column 122 with a higher doping concentration between the third N column 120 and the third P column 134, setting a second P column 133 with a higher doping concentration between the first P column 131 and the first N column 121, and setting a third P column 134 with a higher doping concentration between the second N column 122 and the fourth P column 132, the electric field in the device is more uniform, and when the device breaks down, the current distribution in the device can be more uniform, thereby improving the breakdown voltage and avalanche tolerance of the device.
[0134] Those skilled in the art can clearly understand that for the convenience and simplicity of description, only the division of the above-mentioned doping regions and devices is used as an example for illustration. In actual applications, the above-mentioned functions can be assigned to different doping regions and devices as needed, that is, the internal structure of the device is divided into different doping regions to complete all or part of the functions described above. The doping regions and devices in the embodiments can be integrated into one unit, or each unit can exist physically separately, or two or more units can be integrated into one unit.
[0135] In addition, the specific names of the doping regions and devices are only for the convenience of distinguishing each other and are not used to limit the scope of protection of the present application.
[0136] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described or recorded in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.
[0137] In addition, each doping region in each embodiment of the present application may be integrated into one unit, or each unit may exist physically separately, or two or more units may be integrated into one unit.
[0138] The above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. These modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application, and should all be included in the protection scope of the present application.
Claims
1. A super junction MOS device with improved avalanche withstand, characterized in that: include: N-type substrate; A first N column, a second N column and a third N column are arranged on the N-type substrate, and the third N column is arranged between the first N column and the second N column; wherein the doping concentration of the first N column and the second N column is greater than the doping concentration of the third N column; A first P column, a second P column, a third P column and a fourth P column are arranged on the N-type substrate, and the second P column is arranged between the first P column and the first N column, and the third P column is arranged between the second N column and the fourth P column; the doping concentration of the second P column is greater than the doping concentration of the first P column, and the doping concentration of the third P column is greater than the doping concentration of the fourth P column; A first P-type base region is formed on the first P column, the second P column and the first N column; A second P-type base region is formed on the third P column, the fourth P column and the second N column; a gate dielectric layer and a gate polysilicon layer, wherein the gate dielectric layer is formed on the third N column and is located between the first P-type base region and the second P-type base region, wherein the gate polysilicon layer is wrapped by the gate dielectric layer; A first P-type source region and a first N-type source region, formed on the first P-type base region; A second P-type source region and a second N-type source region, formed on the second P-type base region; a source layer, contacting the first P-type source region, the first N-type source region, the second P-type source region, and the second N-type source region; a gate layer, contacting the gate polysilicon layer; The drain layer is formed on the back side of the N-type substrate.
2. The super junction MOS device according to claim 1, characterized in that: N-type doping point regions are disposed in the first P column and the fourth P column.
3. The super junction MOS device according to claim 1, characterized in that: The super junction MOS device further comprises: The first transverse P column is disposed between the first P-type base region and the first P column, and between the first P-type base region and the second P column.
4. The super junction MOS device according to claim 1, characterized in that: The super junction MOS device further comprises: The second transverse P column is disposed between the second P-type base region and the third P column, and between the second P-type base region and the fourth P column.
5. The super junction MOS device according to any one of claims 1 to 4, characterized in that: The width of the first P-pillar is greater than the width of the second P-pillar; and / or, The width of the fourth P-pillar is greater than the width of the third P-pillar.
6. The super junction MOS device according to any one of claims 1 to 4, characterized in that: The width of the third N pillars is greater than the widths of the first N pillars and the second N pillars.
7. The super junction MOS device according to any one of claims 1 to 4, characterized in that: The width of the third N column is the same as the width of the gate dielectric layer.
8. The super junction MOS device according to any one of claims 1 to 4, characterized in that: The width of the second P column is the same as the width of the first N column; and / or, The width of the third P column is the same as the width of the second N column.
9. A method for preparing a super junction MOS device with improved avalanche tolerance, characterized in that: The preparation method comprises: Epitaxially generating an N-type drift region on the front side of the N-type substrate, and after etching a trench in a partial area of the N-type drift region, filling it with P-type material to form a third N column, a first P column, and a fourth P column; Etching grooves multiple times on partial areas of the first P column and the fourth P column, and filling P-type material and N-type material to form a first N column, a second N column, a second P column and a third P column; wherein the third N column is arranged between the first N column and the second N column, the second P column is arranged between the first P column and the first N column, the third P column is arranged between the second N column and the fourth P column, and the doping concentrations of the first N column and the second N column are greater than the doping concentration of the third N column; the doping concentration of the second P column is greater than the doping concentration of the first P column, and the doping concentration of the third P column is greater than the doping concentration of the fourth P column; Continue to epitaxially grow the N-type epitaxial material and perform an ion implantation process to form a first P-type base region on the first P column, the second P column and the first N column, and to form a second P-type base region on the third P column, the fourth P column and the second N column; Sequentially implanting N-type doping ions and P-type doping ions into the first P-type base region and the second P-type base region to form a first P-type source region and a first N-type source region on the first P-type base region, and forming a second P-type source region and a second N-type source region on the second P-type base region; A trench is formed by etching between the first P-type base region and the second P-type base region, and a gate dielectric layer and a gate polysilicon layer are formed, wherein the gate dielectric layer is formed on the third N column and is located between the first P-type base region and the second P-type base region; wherein the gate polysilicon layer is wrapped by the gate dielectric layer; A source layer in contact with the first P-type source region, the first N-type source region, the second P-type source region and the second N-type source region, a gate layer in contact with the gate polysilicon layer, and a drain layer in contact with the back side of the N-type substrate are formed.
10. A chip, characterized in that: Comprising a super junction MOS device as claimed in any one of claims 1 to 8.
Citation Information
Patent Citations
Super junction structure, preparation method of super junction structure and semiconductor device
CN104241376A
Power device capable of improving avalanche tolerance of super junction structure and preparation method
CN117423723A