A method for manufacturing a radio frequency coaxial cable

By setting up a sinusoidal bonding interface and shielding network during the manufacturing process of RF coaxial cables, the performance of the insulation layer and shielding layer is optimized, and the problem of poor flexibility of RF coaxial cables in frequent bending or deformation scenarios is solved, and its resistance is improved Bending and shielding performance.

CN118867632BActive Publication Date: 2024-11-26嘉兴翼波电子有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411327835.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-24
Publication Date
2024-11-26
Estimated Expiration
2044-09-24

AI Technical Summary

Technical Problem

Existing RF coaxial cables have poor flexibility in application scenarios where frequent bending or deformation are required, limiting their application in complex wiring environments.

Method used

During the manufacturing process of the radio frequency coaxial cable, a sinusoidal bonding interface between the first insulating layer and the second insulating layer is provided, with a hardness less than the second insulating layer, and a shielding net is provided outside the second insulating layer to combine the insulating packet. Cover the eigenvalue and deformation interference eigenvalue for verification, and optimize the cable preparation process to improve bending and shielding performance.

Benefits of technology

Improves the flexibility and bending resistance of RF coaxial cables, enhances shielding performance, and improves preparation stability and efficiency through standardized control and precise adjustment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118867632B_ABST
    Figure CN118867632B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical field of cable manufacturing, and in particular to a manufacturing method of a radio frequency coaxial cable, comprising: obtaining a core wire, and cleaning and drying the core wire; cooling and shaping after completing the coating of a first insulating layer; completing the coating of the first insulating layer with a second insulating layer and shaping it to obtain a cable to be braided; when it is determined that the preparation of the cable to be braided does not meet the preset standard, determining the reason why the preparation of the cable to be braided does not meet the preset standard according to an insulation separation angle, or reducing the traction speed of the second insulating layer coating; obtaining a braided cable; performing a bending rebound test on the braided cable to obtain a deformation interference characteristic value; when it is determined that the preparation of the braided cable does not meet the preset standard, reducing the coating force of the shielding net, or increasing the frequency of change of the sinusoidal extrusion force of the first insulating layer; extruding an outer sheath of the braided cable that meets the preset standard to obtain a radio frequency coaxial cable, thereby improving the bending resistance and shielding performance of the radio frequency coaxial cable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of cable manufacturing, and in particular to a method for manufacturing a radio frequency coaxial cable. Background Art

[0002] RF coaxial cable is a special cable used to transmit high-frequency signals. It consists of an inner conductor, an insulating layer, an outer conductor and an outer sheath, and has good shielding performance and low loss characteristics. RF coaxial cable is widely used in communications, broadcasting, television, radar, radio equipment and computer networks, providing a reliable medium for signal transmission. Among them, bendability is crucial for the application of RF coaxial cable in complex wiring environments.

[0003] Chinese patent publication number: CN115910473A, discloses a super flexible RF coaxial cable, the super flexible RF coaxial cable adopts 3 / 8 RF coaxial cable, the super flexible RF coaxial cable comprises: a flexible inner conductor, and a low attenuation insulation layer, a high shielding outer conductor and a low bending radius sheath layer are arranged in sequence from the inside to the outside on the outer circumference of the flexible inner conductor. It can be seen that the above technical solution adopts the design of corrugating the thin-walled copper tube to form wrinkles in the shielding layer, and the steel tube has high rigidity and poor flexibility, which limits the RF coaxial cable in application scenarios that require frequent bending or deformation. Summary of the invention

[0004] To this end, the present invention provides a method for manufacturing a radio frequency coaxial cable, so as to overcome the problem in the prior art that the cable is limited in application scenarios requiring frequent bending or deformation.

[0005] To achieve the above object, the present invention provides a method for manufacturing a radio frequency coaxial cable, comprising:

[0006] Obtaining a core wire, and cleaning and drying the core wire to complete pretreatment of the core wire;

[0007] Using an extruder and based on a sinusoidal extrusion force to coat the first insulating layer, followed by cooling and shaping;

[0008] Using the extruder and completing the coating of the first insulating layer with the second insulating layer based on constant pressure and then shaping it to obtain the cable to be braided;

[0009] When obtaining the insulation coating characteristic value of the cable to be braided and determining that the preparation of the cable to be braided does not meet the preset standard according to the insulation coating characteristic value, determining the reason why the preparation of the cable to be braided does not meet the preset standard according to the insulation separation angle, or reducing the pulling speed of the second insulation layer coating;

[0010] Weaving a shielding mesh on the cable to be braided that meets the preset standard to obtain a braided cable;

[0011] Performing a bending rebound test on the braided cable to obtain a deformation interference characteristic value;

[0012] When it is determined according to the deformation interference characteristic value that the preparation of the braided cable does not meet the preset standard, reducing the covering force of the shielding net, or increasing the frequency of change of the sinusoidal extrusion force of the first insulating layer;

[0013] The braided cable that meets the preset standard is passed through the extruder to extrude the outer sheath to obtain a radio frequency coaxial cable.

[0014] Further, the process of determining that the preparation of the cable to be braided does not meet the preset standard according to the insulation coating characteristic value includes:

[0015] Comparing the insulation coating characteristic value with the first preset coating characteristic value and the second preset coating characteristic value respectively;

[0016] If the insulation coating characteristic value is greater than or equal to the first preset coating characteristic value and less than the second preset coating characteristic value, it is determined that the preparation of the cable to be braided does not meet the preset standard, and the reason why the preparation of the cable to be braided does not meet the preset standard is determined according to the insulation separation angle;

[0017] If the insulation coating characteristic value is greater than or equal to the second preset coating characteristic value, it is determined that the preparation of the cable to be braided does not meet the preset standard, and the traction speed of the second insulation layer coating is reduced according to the difference between the insulation coating characteristic value and the second preset coating characteristic value.

[0018] Furthermore, the insulation coating characteristic value is determined based on an average value of the difference between the maximum diameter and the minimum diameter of several sections of the cable to be braided.

[0019] Furthermore, several speed adjustment methods are provided for reducing the pulling speed of the second insulating layer coating, and each speed adjustment method reduces the pulling speed of the second insulating layer coating by a different degree.

[0020] Further, the reason why the preparation of the cable to be braided does not meet the preset standard is determined according to the insulation separation angle, wherein:

[0021] If the insulation separation angle is less than the preset insulation separation angle, it is determined that the reason why the preparation of the to-be-braided cable does not meet the preset standard is that the cooling rate of the second insulation layer is not up to standard, and the setting temperature of the second insulation layer is reduced according to the difference between the preset insulation separation angle and the insulation separation angle;

[0022] If the insulation separation angle is greater than or equal to the preset insulation separation angle, it is determined that the reason why the preparation of the cable to be braided does not meet the preset standard is that the coating temperature of the second insulation layer does not meet the standard, and the coating temperature of the second insulation layer is reduced according to the difference between the insulation separation angle and the preset insulation separation angle;

[0023] The insulation separation angle is a bending angle at which the first insulation layer and the second insulation layer are separated when the cable to be braided is bent.

[0024] Furthermore, the reduction range of the coating temperature is positively correlated with the insulation separation angle difference, wherein the insulation separation angle difference is the difference between the insulation separation angle and the preset insulation separation angle.

[0025] Further, the process of determining that the preparation of the braided cable does not meet the preset standard according to the deformation interference characteristic value includes:

[0026] Comparing the deformation interference characteristic value with the first preset deformation interference characteristic value and the second preset deformation interference characteristic value respectively;

[0027] If the deformation interference characteristic value is greater than or equal to the first preset deformation interference characteristic value and less than the second preset deformation interference characteristic value, it is determined that the preparation of the braided cable does not meet the preset standard, and the covering force of the shielding net is reduced according to the difference between the deformation interference characteristic value and the first preset deformation interference characteristic value;

[0028] If the deformation interference characteristic value is greater than or equal to the second preset deformation interference characteristic value, it is determined that the preparation of the braided cable does not meet the preset standard, and the frequency of change of the sinusoidal extrusion force of the first insulating layer is increased according to the difference between the deformation interference characteristic value and the second preset deformation interference characteristic value.

[0029] Furthermore, the process of performing a bending rebound test on the braided cable to obtain the deformation interference characteristic value includes:

[0030] Fixing the braided cable horizontally on a cable bending test machine;

[0031] Acquire an initial image of a braided space within a preset distance from a preset bending point of the braided cable;

[0032] applying a preset bending force to one end of the braided cable;

[0033] Based on the preset bending point, one end of the braided cable is bent according to a preset bending angle, and the other end of the braided cable is kept in a horizontal fixed state;

[0034] Return the bent braided cable to a horizontal state;

[0035] Acquire a deformed image of a braided space within a preset distance from a preset bending point of the braided cable;

[0036] Obtaining the absolute value of the area deformation of each of the weaving spaces within the preset distance;

[0037] The average of the absolute values ​​of the area deformation amounts of the weaving spaces within the preset distance is recorded as the deformation interference characteristic value.

[0038] Furthermore, a plurality of frequency adjustment modes are provided for the frequency variation of the sinusoidal extrusion pressure of the first insulating layer, and each frequency adjustment mode increases the frequency variation of the sinusoidal extrusion pressure of the first insulating layer by a different amount.

[0039] Furthermore, under the first preset condition, several correction methods are provided for correcting the changing frequency of the sinusoidal extrusion pressure of the first insulating layer, and each correction method has a different correction amplitude for the changing frequency of the sinusoidal extrusion pressure of the first insulating layer; the first preset condition is that the changing frequency of the sinusoidal extrusion pressure of the first insulating layer completes the increasing adjustment and the insulation separation angle of the cable to be braided after adjustment is greater than or equal to the preset insulation separation angle.

[0040] Compared with the prior art, the beneficial effect of the present invention lies in that a sinusoidal bonding interface is set between the first insulating layer and the second insulating layer, wherein the hardness of the first insulating layer is less than that of the second insulating layer, and a shielding net is set on the outside of the second insulating layer. At the same time, the cable performance before and after braiding is verified in turn through the insulation coating characteristic value and the deformation interference characteristic value, thereby improving the bending resistance and shielding performance of the RF coaxial cable.

[0041] Furthermore, the present invention uses an extruder and completes the coating and cooling of the core wire by the first insulating layer based on a sinusoidal extrusion force; uses the extruder and completes the coating and shaping of the first insulating layer by the second insulating layer based on a constant pressure to obtain a cable to be braided, thereby enhancing the flexibility and insulation performance of the cable.

[0042] Furthermore, the present invention improves the preparation stability of the cable to be braided by setting the insulation coating characteristic value of the cable to be braided and determining whether the preparation of the cable to be braided meets the preset standard.

[0043] Furthermore, the present invention provides a quantitative index by setting the insulation coating characteristic value, thereby achieving standardized control of the preparation process of the braided cable.

[0044] Furthermore, the present invention provides several speed reduction methods for reducing the traction speed of the second insulation layer coating, and each speed reduction method reduces the traction speed of the second insulation layer coating by a different degree, thereby achieving precise control of the reduction degree of the traction speed of the second insulation layer coating.

[0045] Furthermore, the present invention optimizes the preparation process of the cable to be braided by determining the reason for not meeting the preset standard according to the insulation separation angle.

[0046] Furthermore, the present invention realizes dynamic regulation of the reduction range of the coating temperature by setting the reduction range of the coating temperature to be positively correlated with the insulation separation angle difference.

[0047] Furthermore, the present invention improves the preparation efficiency of the braided cable by determining whether the preparation of the braided cable meets preset standards based on the deformation interference characteristic value. BRIEF DESCRIPTION OF THE DRAWINGS

[0048] Figure 1 is a flow chart of a method for manufacturing a radio frequency coaxial cable according to an embodiment of the present invention;

[0049] Figure 2 A flow chart of an embodiment of the present invention for determining whether the preparation of the cable to be braided meets a preset standard;

[0050] Figure 3 A flow chart for determining the reason why the preparation of the cable to be braided does not meet the preset standard according to an embodiment of the present invention;

[0051] Figure 4 The present invention is a flowchart for determining whether the preparation of the braided cable meets the preset standard. DETAILED DESCRIPTION

[0052] In order to make the objects and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0053] It should be pointed out that the data in this embodiment are obtained by comprehensive analysis and evaluation of the historical test data of the present invention three months before this test and the corresponding historical test results. It can be understood by those skilled in the art that the method of the present invention can determine the above parameters for a single item by selecting the value with the highest proportion as the preset standard parameter according to the data distribution, using weighted summation to use the obtained value as the preset standard parameter, substituting each historical data into a specific formula and using the value obtained by the formula as the preset standard parameter or other selection methods, as long as the method of the present invention can clearly define the different specific situations in the single determination process through the obtained values.

[0054] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.

[0055] See also Figure 1 , Figure 2 , Figure 3 as well as Figure 4 As shown, they are respectively a flow chart of a method for manufacturing a radio frequency coaxial cable according to an embodiment of the present invention; a flow chart of determining whether the preparation of the cable to be braided meets the preset standard according to an embodiment of the present invention; a flow chart of determining the reason why the preparation of the cable to be braided does not meet the preset standard according to an embodiment of the present invention; a flow chart of determining whether the preparation of the braided cable meets the preset standard according to an embodiment of the present invention.

[0056] A method for manufacturing a radio frequency coaxial cable according to an embodiment of the present invention includes:

[0057] Step S1, obtaining a core wire, and cleaning and drying the core wire to complete pretreatment of the core wire;

[0058] Step S2, using an extruder to coat the first insulating layer based on a sinusoidal extrusion force and then cooling and shaping;

[0059] Step S3, using the extruder and completing the coating of the first insulating layer with the second insulating layer based on a constant pressure and then shaping it to obtain a cable to be braided;

[0060] Step S4, when obtaining the insulation coating characteristic value of the cable to be braided and determining that the preparation of the cable to be braided does not meet the preset standard according to the insulation coating characteristic value, determining the reason why the preparation of the cable to be braided does not meet the preset standard according to the insulation separation angle, or reducing the pulling speed of the second insulation layer coating;

[0061] Step S5, weaving a shielding mesh on the cable to be braided that meets the preset standard to obtain a braided cable;

[0062] Step S6, performing a bending rebound test on the braided cable to obtain a deformation interference characteristic value;

[0063] Step S7, when it is determined according to the deformation interference characteristic value that the preparation of the braided cable does not meet the preset standard, reducing the covering force of the shielding net, or increasing the frequency of change of the sinusoidal extrusion force of the first insulating layer;

[0064] Step S8, extruding the outer sheath of the braided cable that meets the preset standard through the extruder to obtain a radio frequency coaxial cable.

[0065] Specifically, the core wire is made of a single copper wire; the first insulating layer is made of polyethylene material; the second insulating layer is made of polytetrafluoroethylene material; the shielding net is set as a multi-strand copper wire textile layer; and the outer sheath is made of silicone rubber material.

[0066] Specifically, the radio frequency coaxial cable can be obtained by, for example, an SJ65 extruder or a TZ-032 extruder, without any specific limitation, as long as the preparation requirements are met.

[0067] Specifically, the sinusoidal extrusion pressure means that the extruder forms the first insulation layer by applying a sinusoidal extrusion pressure to coat the core wire. After the first insulation layer is cooled and formed, the outer contour shape of the cross section along the cable is sinusoidal. The amplitude and frequency of the sinusoidal waveform are not limited, and it only needs to meet the preparation requirements of the extruder.

[0068] Specifically, whether the preparation of the cable to be braided meets the preset standard is determined according to the insulation coating characteristic value, wherein:

[0069] If the insulation coating characteristic value is less than the first preset coating characteristic value of 0.028 mm, it is determined that the preparation of the cable to be braided meets the preset standard, and the cable to be braided that meets the preset standard is braided into a shielding mesh to obtain a braided cable;

[0070] If the insulation coating characteristic value is greater than or equal to the first preset coating characteristic value and less than the second preset coating characteristic value of 0.069 mm, it is determined that the preparation of the cable to be braided does not meet the preset standard, and the reason why the preparation of the cable to be braided does not meet the preset standard is determined according to the insulation separation angle;

[0071] If the insulation coating characteristic value is greater than or equal to the second preset coating characteristic value, it is determined that the preparation of the cable to be braided does not meet the preset standard, and the traction speed of the second insulation layer coating is reduced according to the difference between the insulation coating characteristic value and the second preset coating characteristic value.

[0072] Specifically, the insulation coating characteristic value is calculated by the following formula:

[0073] ;

[0074] In the formula, A represents the insulation coating characteristic value; Dimax represents the maximum diameter of the i-th unit segment of the cable to be braided; Dimin represents the minimum diameter of the i-th unit segment of the cable to be braided, where i=1,2...n, and n represents the total number of unit segments into which the cable to be braided is evenly divided.

[0075] Specifically, several speed adjustment methods are provided for reducing the pulling speed of the second insulating layer coating, wherein:

[0076] If the coating characteristic difference is less than the first preset coating characteristic difference of 0.01 mm, the pulling speed of the second insulating layer coating is reduced by using the first preset speed adjustment coefficient of 0.98;

[0077] If the coating characteristic difference is greater than or equal to the first preset coating characteristic difference and less than the second preset coating characteristic difference of 0.02 mm, the pulling speed of the second insulating layer coating is reduced by using the second preset speed adjustment coefficient of 0.93;

[0078] If the coating characteristic difference is greater than or equal to the second preset coating characteristic difference, the pulling speed of the second insulating layer coating is reduced by using a third preset speed adjustment coefficient of 0.88;

[0079] The coating characteristic difference is the difference between the insulating coating characteristic value and the second preset coating characteristic value.

[0080] Specifically, the reason why the preparation of the cable to be braided does not meet the preset standard is determined according to the insulation separation angle, wherein:

[0081] If the insulation separation angle is less than the preset insulation separation angle of 105°, it is determined that the reason why the preparation of the cable to be braided does not meet the preset standard is that the cooling rate of the second insulation layer is not up to standard, and the setting temperature of the second insulation layer is reduced according to the difference between the preset insulation separation angle and the insulation separation angle;

[0082] If the insulation separation angle is greater than or equal to the preset insulation separation angle, it is determined that the reason why the preparation of the cable to be braided does not meet the preset standard is that the coating temperature of the second insulation layer does not meet the standard, and the coating temperature of the second insulation layer is reduced according to the difference between the insulation separation angle and the preset insulation separation angle;

[0083] The insulation separation angle is a bending angle at which the first insulation layer and the second insulation layer are separated when the cable to be braided is bent.

[0084] Specifically, the reduction amplitude of the coating temperature is positively correlated with the insulation separation angle difference. For example, the reduction amplitude of the coating temperature is set to △D, and the insulation separation angle difference is set to △Φ, then △D=α×△Φ, α is the amplitude adjustment coefficient, and α is set to 1.02. It can be understood that the greater the insulation separation angle difference, the greater the reduction amplitude of the coating temperature, wherein the insulation separation angle difference is the difference between the insulation separation angle and the preset insulation separation angle.

[0085] Specifically, whether the preparation of the braided cable meets the preset standard is determined according to the deformation interference characteristic value, wherein:

[0086] If the deformation interference characteristic value is less than the first preset deformation interference characteristic value of 0.017 mm 2 , it is determined that the preparation of the braided cable meets the preset standard, and the braided cable meeting the preset standard is extruded through the extruder to obtain an RF coaxial cable;

[0087] If the deformation interference characteristic value is greater than or equal to the first preset deformation interference characteristic value and less than the second preset deformation interference characteristic value 0.029 mm 2 , it is determined that the preparation of the braided cable does not meet the preset standard, and the covering force of the shielding net is reduced according to the difference between the deformation interference characteristic value and the first preset deformation interference characteristic value;

[0088] If the deformation interference characteristic value is greater than or equal to the second preset deformation interference characteristic value, it is determined that the preparation of the braided cable does not meet the preset standard, and the frequency of change of the sinusoidal extrusion force of the first insulating layer is increased according to the difference between the deformation interference characteristic value and the second preset deformation interference characteristic value.

[0089] Specifically, the process of performing a bending rebound test on the braided cable to obtain the deformation interference characteristic value includes:

[0090] Fixing the braided cable horizontally on a cable bending test machine;

[0091] Acquire an initial image of a braided space within a preset distance of 30 cm from a preset bending point of the braided cable;

[0092] Applying a preset bending force of 600N to one end of the braided cable;

[0093] Based on the preset bending point, one end of the braided cable is bent at a preset bending angle of 110°, and the other end of the braided cable is kept in a horizontal fixed state;

[0094] Return the bent braided cable to a horizontal state;

[0095] Acquire a deformed image of a braided space within a preset distance from a preset bending point of the braided cable;

[0096] Obtaining the absolute value of the area deformation of each of the weaving spaces within the preset distance;

[0097] The average of the absolute values ​​of the area deformation amounts of the weaving spaces within the preset distance is recorded as the deformation interference characteristic value.

[0098] Specifically, several frequency increasing modes are provided for the frequency variation of the sinusoidal extrusion force of the first insulating layer, wherein:

[0099] If the interference characteristic difference is less than the first preset interference characteristic difference of 0.011 mm 2 , then use the first preset speed frequency adjustment coefficient 1.03 to increase the frequency of change of the sinusoidal extrusion force of the first insulating layer;

[0100] If the interference characteristic difference is greater than or equal to the first preset interference characteristic difference and less than the second preset interference characteristic difference 0.023 mm 2 , then use the second preset speed frequency adjustment coefficient of 1.07 to increase the frequency of change of the sinusoidal extrusion force of the first insulating layer;

[0101] If the interference characteristic difference is greater than or equal to the second preset interference characteristic difference, using a third preset speed adjustment coefficient of 1.13 to increase the frequency of change of the sinusoidal extrusion force of the first insulating layer;

[0102] The interference feature difference is the difference between the deformation interference feature value and the second preset deformation interference feature value.

[0103] Specifically, under the first preset condition, several correction methods are provided for correcting the frequency change of the sinusoidal extrusion force of the first insulating layer, wherein:

[0104] If the correction difference is less than the first preset correction difference of 8.4°, the frequency of change of the sinusoidal extrusion force of the first insulating layer is corrected to a corresponding value using the first preset correction coefficient of 0.96;

[0105] If the correction difference is greater than or equal to the first preset correction difference and less than the second preset correction difference of 10.6°, the frequency of change of the sinusoidal extrusion force of the first insulating layer is corrected to a corresponding value using the second preset correction coefficient of 0.92;

[0106] If the correction difference is greater than or equal to the second preset correction difference, the frequency of change of the sinusoidal extrusion force of the first insulating layer is corrected to a corresponding value using a third preset correction coefficient of 0.89;

[0107] The correction difference is the difference between the adjusted insulation separation angle of the cable to be braided and the preset insulation separation angle;

[0108] The first preset condition is that the frequency of the change of the sinusoidal extrusion pressure of the first insulating layer completes the increase adjustment and the insulation separation angle of the cable to be braided after adjustment is greater than or equal to the preset insulation separation angle of 105°.

[0109] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.

[0110] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for manufacturing a radio frequency coaxial cable, characterized in that: include: Obtaining a core wire, and cleaning and drying the core wire to complete pretreatment of the core wire; Using an extruder and based on a sinusoidal extrusion force to coat the first insulating layer, followed by cooling and shaping; Using the extruder and completing the coating of the first insulating layer with the second insulating layer based on constant pressure and then shaping it to obtain the cable to be braided; When obtaining the insulation coating characteristic value of the cable to be braided and determining that the preparation of the cable to be braided does not meet the preset standard according to the insulation coating characteristic value, determining the reason why the preparation of the cable to be braided does not meet the preset standard according to the insulation separation angle, or reducing the pulling speed of the second insulation layer coating; Weaving a shielding mesh on the cable to be braided that meets the preset standard to obtain a braided cable; Performing a bending rebound test on the braided cable to obtain a deformation interference characteristic value; When it is determined according to the deformation interference characteristic value that the preparation of the braided cable does not meet the preset standard, reducing the covering force of the shielding net, or increasing the frequency of change of the sinusoidal extrusion force of the first insulating layer; Extruding the outer sheath of the braided cable that meets the preset standard through the extruder to obtain a radio frequency coaxial cable; The insulation coating characteristic value is determined according to the average value of the difference between the maximum diameter and the minimum diameter of several sections of the cable to be braided; The insulation separation angle is a bending angle at which the first insulation layer and the second insulation layer are separated when the cable to be braided is bent; The process of performing a bending rebound test on the braided cable to obtain the deformation interference characteristic value includes: Fixing the braided cable horizontally on a cable bending test machine; Acquire an initial image of a braided space within a preset distance from a preset bending point of the braided cable; applying a preset bending force to one end of the braided cable; Based on the preset bending point, one end of the braided cable is bent according to a preset bending angle, and the other end of the braided cable is kept in a horizontal fixed state; Return the bent braided cable to a horizontal state; Acquire a deformed image of a braided space within a preset distance from a preset bending point of the braided cable; Obtaining the absolute value of the area deformation of each of the weaving spaces within the preset distance; The average of the absolute values ​​of the area deformation amounts of the weaving spaces within the preset distance is recorded as the deformation interference characteristic value.

2. The method for manufacturing a radio frequency coaxial cable according to claim 1, characterized in that: The process of determining, according to the insulation coating characteristic value, that the preparation of the cable to be braided does not meet the preset standard comprises: Comparing the insulation coating characteristic value with the first preset coating characteristic value and the second preset coating characteristic value respectively; If the insulation coating characteristic value is greater than or equal to the first preset coating characteristic value and less than the second preset coating characteristic value, it is determined that the preparation of the cable to be braided does not meet the preset standard, and the reason why the preparation of the cable to be braided does not meet the preset standard is determined according to the insulation separation angle; If the insulation coating characteristic value is greater than or equal to the second preset coating characteristic value, it is determined that the preparation of the cable to be braided does not meet the preset standard, and the traction speed of the second insulation layer coating is reduced according to the difference between the insulation coating characteristic value and the second preset coating characteristic value.

3. The method for manufacturing a radio frequency coaxial cable according to claim 2, characterized in that: Several speed adjustment methods are provided for reducing the pulling speed of the second insulating layer sheath, and each speed adjustment method reduces the pulling speed of the second insulating layer sheath by a different degree.

4. The method for manufacturing a radio frequency coaxial cable according to claim 3, characterized in that: The reason why the preparation of the cable to be braided does not meet the preset standard is determined according to the insulation separation angle, wherein: If the insulation separation angle is less than the preset insulation separation angle, it is determined that the reason why the preparation of the braided cable does not meet the preset standard is that the cooling rate of the second insulation layer is not up to standard, and the setting temperature of the second insulation layer is reduced according to the difference between the preset insulation separation angle and the insulation separation angle; If the insulation separation angle is greater than or equal to the preset insulation separation angle, it is determined that the reason why the preparation of the braided cable does not meet the preset standard is that the coating temperature of the second insulation layer does not meet the standard, and the coating temperature of the second insulation layer is reduced according to the difference between the insulation separation angle and the preset insulation separation angle.

5. The method for manufacturing a radio frequency coaxial cable according to claim 4, characterized in that: The reduction range of the coating temperature is positively correlated with the insulation separation angle difference, wherein the insulation separation angle difference is the difference between the insulation separation angle and the preset insulation separation angle.

6. The method for manufacturing a radio frequency coaxial cable according to claim 5, characterized in that: The process of determining, according to the deformation interference characteristic value, that the preparation of the braided cable does not meet the preset standard comprises: Comparing the deformation interference characteristic value with a first preset deformation interference characteristic value and a second preset deformation interference characteristic value respectively; If the deformation interference characteristic value is greater than or equal to the first preset deformation interference characteristic value and less than the second preset deformation interference characteristic value, it is determined that the preparation of the braided cable does not meet the preset standard, and the covering force of the shielding net is reduced according to the difference between the deformation interference characteristic value and the first preset deformation interference characteristic value; If the deformation interference characteristic value is greater than or equal to the second preset deformation interference characteristic value, it is determined that the preparation of the braided cable does not meet the preset standard, and the frequency of change of the sinusoidal extrusion force of the first insulating layer is increased according to the difference between the deformation interference characteristic value and the second preset deformation interference characteristic value.

7. The method for manufacturing a radio frequency coaxial cable according to claim 6, characterized in that: Several frequency adjustment methods are provided for the frequency variation of the sinusoidal extrusion pressure of the first insulating layer, and each frequency adjustment method has a different increase range for the frequency variation of the sinusoidal extrusion pressure of the first insulating layer.

8. The method for manufacturing a radio frequency coaxial cable according to claim 7, characterized in that: Under the first preset condition, several correction methods are set for correcting the changing frequency of the sinusoidal extrusion pressure of the first insulating layer, and each correction method has a different correction amplitude for the changing frequency of the sinusoidal extrusion pressure of the first insulating layer; the first preset condition is that the changing frequency of the sinusoidal extrusion pressure of the first insulating layer completes the increasing adjustment and the insulation separation angle of the cable to be braided after adjustment is greater than or equal to the preset insulation separation angle.